Preparation method of skin-friendly elastic thermal insulation fabric
Through the mixing and spinning process of natural fibers and elastic fibers, combined with woven and soft treatment, the existing elastic insulation fabrics are solved, and the comfort and durability of the fabrics are improved, ensuring that the fabrics are worn and used during the process of wearing and using the fabrics stability in.
Patent Information
- Application Number
- CN202411049342.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-01
- Publication Date
- 2024-11-19
AI Technical Summary
The existing elastic insulation fabrics are poorly skin-friendly, and they are prone to discomfort when worn and lack comfort.
The mechanical mix of natural fibers and elastic fibers is made into yarns through spinning and weaving them in a woven manner, combining soft and styling to enhance the comfort and durability of the fabric.
It improves the wear comfort, wrinkle resistance and easy care of the fabric, ensures that the fabric remains stable during use and is not easy to deform, and enhances the overall performance of the fabric.
Smart Images

Figure CN118979327A_ABST
Abstract
Description
Technical Field
[0001] The present application relates to the technical field of textile fabric preparation, and in particular to a method for preparing a skin-friendly, elastic and thermal insulation fabric. Background Art
[0002] At present, as people's requirements for clothing comfort and functionality continue to increase, skin-friendly, elastic and thermal insulation properties have become important characteristics of fabrics. Currently, elastic thermal insulation fabrics on the market are mostly made of synthetic fibers and rubber. Although they have certain elasticity and warmth retention, synthetic materials usually do not have the hygroscopicity of cotton or wool, and cannot effectively absorb moisture from the skin, which may cause the wearer to feel damp and uncomfortable, lack skin-friendly, and easily cause discomfort when wearing.
[0003] The above-mentioned existing technical solutions have the following defects: the existing elastic thermal insulation fabrics have poor skin affinity and are prone to discomfort when worn, so there is room for improvement. Summary of the invention
[0004] In order to improve the comfort of fabrics, the present application provides a method for preparing skin-friendly elastic thermal insulation fabrics.
[0005] The above-mentioned invention objective of the present application is achieved through the following technical solutions: A method for preparing a skin-friendly elastic thermal insulation fabric, characterized in that the method for preparing the skin-friendly elastic thermal insulation fabric comprises: Selecting natural fibers and elastic fibers, and mechanically mixing the natural fibers and the elastic fibers according to a preset ratio; The mixed fibers are made into yarn through a spinning process; The yarn is woven by machine to obtain a woven fabric; The woven fabric is softened by using a pre-proportioned softener to obtain the softened fabric, and the softened fabric is shaped to obtain a finished fabric product.
[0006] By adopting the above technical scheme, natural fibers and elastic fibers are selected, and the physical and chemical properties of different fibers can be combined by mixing, such as the air permeability and comfort of natural fibers, and the elasticity and durability of elastic fibers, so as to obtain mixed fibers with specific properties; the quality and characteristics of the yarn directly affect the quality and feel of the final fabric, and the mixed fibers are made into yarns through a spinning process, and the short fibers or filaments are processed into continuous yarns to provide basic materials for subsequent weaving; the yarns are interwoven together according to a certain rule by a weaving method, and the yarns are woven to obtain woven fabrics; the fabrics are softened by using chemical additives or physical methods to make the fabrics feel softer and improve the comfort of wearing. In addition, the softening treatment can also improve the drape, wrinkle resistance and easy care of the fabrics; the softened fabrics are subjected to a shaping treatment, and the fiber structure of the fabrics is fixed by heat treatment at high temperature and for a certain period of time, reducing deformation during washing and wearing. The shaping treatment can fix the shape and size of the fabrics, ensuring that the fabrics remain stable and not easily deformed during use, and the final fabric product is obtained after the shaping treatment.
[0007] In a preferred example, the present application may be further configured as follows: the selecting of natural fibers and elastic fibers, and mechanically mixing the natural fibers and the elastic fibers according to a preset ratio comprises: 40%-60% of organic cotton fiber and 40%-60% of spandex fiber are selected as raw materials, and 2%-5% of bamboo charcoal fiber is added to the raw materials. The organic cotton fiber and the spandex fiber are mixed in a fiber mixer to serve as the warp and weft of the fabric.
[0008] By adopting the above technical scheme, 40%-60% of organic cotton fiber and 40%-60% of spandex fiber are selected as raw materials. Organic cotton fiber is favored for its comfort, breathability and environmental protection characteristics, while spandex fiber provides the required elasticity and durability. The mixed ratio ensures that the fabric not only maintains the natural advantages of organic cotton, but also has the functionality of spandex. 2%-5% of bamboo charcoal fiber is added to the raw materials. Bamboo charcoal fiber is well-known for its adsorption and antibacterial properties, which can bring additional health and hygiene properties to the fabric to provide additional benefits without significantly changing the basic properties of the fabric. Finally, the organic cotton fiber and spandex fiber are mixed in a ratio as the warp and weft of the fabric, which helps to improve the comfort of the finished fabric.
[0009] In a preferred example, the present application can be further configured as follows: the step of spinning the mixed fibers into yarn comprises: Spinning the mixed fibers by ring spinning technology to obtain preliminarily treated yarns; The yarn is obtained by performing a secondary treatment on the preliminarily treated yarn using a double-sided brushing technique.
[0010] By adopting the above technical scheme, the mixed fibers are spun by ring spinning technology, the mixed raw materials of organic cotton, spandex and bamboo charcoal fibers are converted into yarns, the fibers are stretched, twisted and wound into yarns by high-speed rotating ring spindles to produce uniform, high-strength and smooth-surfaced yarns, and the preliminarily treated yarns are secondary treated by double-sided brushing technology. By applying mechanical action on the yarn surface, short fibers and impurities are removed, and the yarn surface is made smoother and tidier, which can improve the strength and wear resistance of the yarn, reduce the breakage phenomenon during weaving, thereby improving production efficiency and fabric quality, and the brushed yarns are softer to the touch, which helps to improve the wearing comfort of the fabric.
[0011] In a preferred example, the present application can be further configured as follows: the weaving method includes: The yarn is woven into a double-layer fabric using double-layer weaving technology, wherein the inner layer uses yarn containing bamboo charcoal fiber, and the outer layer uses yarn containing organic cotton fiber and spandex fiber; The plain weaving process used has a density of 200-300 threads / 10cm.
[0012] By adopting the above technical scheme, the yarn is woven into a double-layer fabric using double-layer weaving technology to create a composite fabric with different functional layers. The inner layer uses yarn containing bamboo charcoal fiber to give the fabric additional antibacterial, deodorizing and adsorption properties. At the same time, the thermal regulation function of the bamboo charcoal fiber can also provide better wearing comfort. The outer layer uses yarn of organic cotton fiber and spandex fiber, which not only ensures the softness and breathability of the fabric, but also increases the stretchability and recovery of the fabric through the elasticity of the spandex fiber. The plain weaving process density adopted is 200-300 yarns / 10cm. A higher density means more yarns per unit area, which usually makes the fabric stronger and more durable, and may also increase its weight and warmth. However, too high a density may affect the breathability and softness of the fabric. Therefore, the density range of 200-300 yarns / 10cm is selected to balance the durability, comfort and functionality of the fabric.
[0013] In a preferred example, the present application can be further configured as follows: nanoparticles are added during the weaving process so that the nanoparticles are embedded in the woven yarns.
[0014] By adopting the above technical solution, nanoparticles are added during the weaving process and embedded in the woven yarn. Due to their tiny size and high surface area, nanoparticles can bring a series of unique properties to the fabric, such as antibacterial properties, UV resistance, flame retardancy or enhanced wear resistance.
[0015] In a preferred example, the present application can be further configured as follows: before the woven fabric is softened by using a pre-proportioned softener, the method includes: Performing mechanical stretching treatment on the woven fabric; After the mechanical stretching treatment, the stretched fabric is subjected to antistatic treatment, using an antistatic agent not exceeding 0.5 g / L, the treatment temperature is maintained at 50-60°C, and the treatment time is 10-20 minutes.
[0016] By adopting the above technical scheme, the woven fabric is subjected to mechanical stretching treatment. Through the mechanical stretching treatment, the dimensional stability of the fabric is improved, the deformation during wearing and washing is reduced, and the feel and drape of the fabric can also be improved; after the mechanical stretching treatment, the stretched fabric is subjected to antistatic treatment. In order to reduce the problem of static electricity generated by the fabric during wearing or use, an antistatic agent of no more than 0.5g / L is used, which can reduce the friction coefficient between fibers and thus reduce the generation of static electricity. The treatment temperature is maintained at 50-60°C. This temperature range helps the antistatic agent to better penetrate and evenly distribute on the fabric. The treatment time is 10-20 minutes to ensure that the antistatic agent has enough time to combine with the fabric fibers and exert its effect. The physical properties of the fabric are improved through mechanical stretching treatment, and the antistatic treatment improves the wearing comfort and practicality of the fabric.
[0017] In a preferred example, the present application can be further configured as follows: the woven fabric is softened by using a pre-proportioned softener, and the softened fabric includes: The woven fabric is immersed in a softener solution containing natural plant extracts for 20 minutes, wherein the softener solution is obtained by mixing and stirring 1-2% of natural lavender extract, 1-2% of chamomile extract, 1-2% of aloe extract, 10-15% of quaternary ammonium salt, 5-10% of silicone softener, 5-8% of stearic acid, 0.5-1% of carboxymethyl cellulose, 0.1-0.2% of sodium benzoate and 59.8-76.4% of water; The soaked fabric is dried using a drum dryer to obtain the softened fabric.
[0018] By adopting the above technical solution, the woven fabric is immersed in a softener solution containing natural plant extracts and immersed for 20 minutes. In order to remove excess moisture in the fabric and ensure that the fabric is dry and uniform, a drum dryer is used to dry the immersed fabric. The drum dryer accelerates the evaporation of moisture through high temperature and mechanical action while maintaining the shape and size of the fabric. This drying method helps the fabric maintain its softness and comfort after softener treatment, while avoiding deformation or damage of the fabric due to uneven drying.
[0019] In a preferred example, the present application can be further configured as follows: the shaping treatment of the softened fabric to obtain a finished fabric product includes: Performing ultrasonic trimming on the softened fabric to remove fibers from the edge of the softened fabric to obtain trimmed fabric; The trimmed fabric is shaped within a temperature range of 120° C. to 150° C., and the time is controlled within a range of 15 minutes to 30 minutes, to finally obtain the finished fabric.
[0020] By adopting the above technical solution, the fabric after softening is subjected to ultrasonic trimming by using high-frequency acoustic energy cutting technology. Ultrasonic trimming can remove loose fibers at the edge of the fabric very accurately, thereby obtaining a clean and smooth edge. This treatment not only improves the appearance quality of the fabric, but also helps to prevent the edge fibers from falling off, thereby enhancing the durability of the fabric. In addition, ultrasonic trimming is a non-thermal cutting process, which can avoid damage to the fabric or affect the softness of the fabric due to high temperature. The trimmed fabric is shaped within a temperature range of 120°C to 150°C. Within this temperature range, the molecular structure of the fabric fiber will change, so that the fabric can maintain the set shape after cooling. The time is controlled within 15 minutes to 30 minutes. This time period is sufficient for the fabric fiber to be fully shaped, while avoiding damage or hardening of the fabric that may be caused by excessive heating. Through this shaping treatment, the dimensional stability of the finished fabric is guaranteed, and deformation during subsequent use and washing is reduced.
[0021] In summary, the present application includes at least one of the following beneficial technical effects: 1. Select natural fibers and elastic fibers. Mixing different fibers can combine their physical and chemical properties, such as the breathability and comfort of natural fibers, and the elasticity and durability of elastic fibers, to obtain mixed fibers with specific properties; the quality and characteristics of the yarn directly affect the quality and feel of the final fabric, and the mixed fibers are made into yarns through a spinning process, and short fibers or filaments are processed into continuous yarns to provide basic materials for subsequent weaving; 2. Use a weaving method to interweave the yarns according to a certain pattern, weave the yarns to obtain woven fabrics; soften the finished fabrics, use chemical additives or physical methods to make the fabrics feel softer and improve the wearing comfort. In addition, the softening treatment can also improve the drape, wrinkle resistance and easy care of the fabrics; the softened fabrics are subjected to a shaping treatment. Through high temperature and a certain period of heat treatment, the fiber structure of the fabrics is fixed, reducing deformation during washing and wearing. The shaping treatment can fix the shape and size of the fabrics, ensuring that the fabrics remain stable during use and are not easily deformed. After the shaping treatment, the final fabric product is obtained. BRIEF DESCRIPTION OF THE DRAWINGS
[0022] Figure 1 It is a flow chart of a method for preparing a skin-friendly elastic thermal insulation fabric in one embodiment of the present application; Figure 2 This is a flowchart for implementing step S10 in a method for preparing a skin-friendly elastic thermal insulation fabric in an embodiment of the present application; Figure 3 This is a flowchart for implementing step S20 in a method for preparing a skin-friendly elastic thermal insulation fabric in an embodiment of the present application; Figure 4 This is a flowchart for implementing step S30 in a method for preparing a skin-friendly elastic thermal insulation fabric in an embodiment of the present application; Figure 5 This is another implementation flow chart of step S40 in a method for preparing a skin-friendly elastic thermal insulation fabric in an embodiment of the present application; Figure 6 This is a flowchart for implementing step S40 in a method for preparing a skin-friendly elastic thermal insulation fabric in an embodiment of the present application; Figure 7 This is a flowchart for implementing step S40 in a method for preparing a skin-friendly, elastic and thermal insulation fabric in one embodiment of the present application. DETAILED DESCRIPTION
[0023] The present application is further described in detail below in conjunction with the accompanying drawings.
[0024] In one embodiment, if Figure 1 As shown, the present application discloses a method for preparing a skin-friendly elastic thermal insulation fabric, which specifically comprises the following steps: S10: selecting natural fibers and elastic fibers, and mechanically mixing the natural fibers and the elastic fibers according to a preset ratio.
[0025] Specifically, natural fibers and elastic fibers are selected: natural fibers such as cotton, wool, silk, etc., and elastic fibers such as spandex, polyester, etc., because the mixing ratio will affect the elasticity, strength, feel and other properties of the fabric. For example, increasing the proportion of elastic fibers can improve the elasticity of the fabric. Therefore, natural fibers and elastic fibers are mixed according to a pre-set ratio, and mechanical equipment is used to mix two or more fibers evenly. During the mixing process, the mechanical force will cause the fibers to tumble and disperse in the mixing chamber, thereby achieving a uniform mixing effect to create a mixed yarn with specific properties.
[0026] S20: The mixed fibers are made into yarns through a spinning process.
[0027] Specifically, the mixed fibers are subjected to processes such as opening, carding, drawing, stretching, and twisting to transform the fibers into yarns with a certain strength and uniformity, thus preparing them for subsequent weaving.
[0028] S30: The yarns are woven by machine to obtain woven fabrics.
[0029] Specifically, the yarn is wound on the weaving beam and the tension of the yarn is ensured to be uniform to avoid breakage or relaxation during the weaving process. The yarn is interwoven on the loom according to a certain weave structure, such as plain, twill, satin, etc., to form a fabric with a certain thickness, density and texture.
[0030] S40: softening the woven fabric with a pre-proportioned softener to obtain a softened fabric, and shaping the softened fabric to obtain a finished fabric.
[0031] Specifically, after weaving is completed, the fabric needs to undergo preliminary inspection and cleaning to remove impurities or residues that may be generated during the weaving process. In order to ensure the effective penetration and uniform distribution of the softener, the fabric needs to be softened at a specific temperature and pH value by immersing the fabric in a solution containing a softener. After softening, the fabric needs to be washed to remove excess softener and possible chemical residues, and then the moisture in the fabric is removed by centrifugation or extrusion. Hot air or a drying drum is used to remove the remaining moisture in the fabric and fix the softener in the fiber. The dried fabric is then set at high temperature. The fabric is stretched to the desired size, and then the fiber structure is fixed by heat setting to prevent shrinkage or deformation in subsequent use, and finally the finished fabric is produced.
[0032] By adopting the above technical scheme, natural fibers and elastic fibers are selected, and the physical and chemical properties of different fibers can be combined by mixing, such as the air permeability and comfort of natural fibers, and the elasticity and durability of elastic fibers, so as to obtain mixed fibers with specific properties; the quality and characteristics of the yarn directly affect the quality and feel of the final fabric, and the mixed fibers are made into yarns through a spinning process, and the short fibers or filaments are processed into continuous yarns to provide basic materials for subsequent weaving; the yarns are interwoven together according to a certain rule by a weaving method, and the yarns are woven to obtain woven fabrics; the fabrics are softened by using chemical additives or physical methods to make the fabrics feel softer and improve the comfort of wearing. In addition, the softening treatment can also improve the drape, wrinkle resistance and easy care of the fabrics; the softened fabrics are subjected to a shaping treatment, and the fiber structure of the fabrics is fixed by heat treatment at high temperature and for a certain period of time, reducing deformation during washing and wearing. The shaping treatment can fix the shape and size of the fabrics, ensuring that the fabrics remain stable and not easily deformed during use, and the final fabric product is obtained after the shaping treatment.
[0033] In one embodiment, if Figure 2 As shown, in step S10, natural fibers and elastic fibers are selected and mechanically mixed according to a preset ratio, specifically including: S11: 40%-60% organic cotton fiber and 40%-60% spandex fiber are selected as raw materials, and 2%-5% bamboo charcoal fiber is added to the raw materials. The organic cotton fiber and spandex fiber are mixed in a fiber mixer to form the warp and weft of the fabric.
[0034] Specifically, organic cotton fiber and spandex fiber are mixed at a ratio of 40%-60% organic cotton fiber and 40%-60% spandex fiber as raw materials, and 2%-5% bamboo charcoal fiber is added to the raw materials to improve the antibacterial property of the fabric. During the fiber mixing process, the two fibers are evenly distributed by using fiber mixing equipment to ensure the performance consistency of the fabric, and the mixed fibers will be used as the warp and weft of the fabric.
[0035] In one embodiment, if Figure 3 As shown, in step S20, the mixed fibers are made into yarn through a spinning process, which specifically includes: S21: The mixed fibers are spun using ring spinning technology to obtain preliminarily processed yarns.
[0036] Specifically, the fiber strips are fed into the ring spinning machine, stretched to make the fibers parallel, and then introduced through the rotation of the ring wire ring. The bobbin winding speed is faster than the wire ring, so that the cotton yarn is twisted and wound into yarn, and finally the preliminarily processed yarn is obtained.
[0037] S22: The yarn treated initially is subjected to secondary treatment using a double-sided brushing technique to obtain yarn.
[0038] Specifically, after being processed by the ring spinning technology, the preliminarily processed yarn is obtained, and the preliminarily processed yarn is brushed by two brush rollers in opposite directions to remove impurities and loose fibers on the surface of the yarn, making the yarn smoother and neater, and finally obtaining the textile yarn used for textile fabrics.
[0039] In one embodiment, if Figure 4 As shown, in step S30, the yarn is woven by weaving to obtain a woven fabric, which also includes: S31: Adding nanoparticles during the weaving process so that the nanoparticles are embedded in the woven yarn.
[0040] Specifically, in the process of using a loom to weave yarns into textiles according to a certain organizational structure, the yarns are immersed in a finishing liquid containing nanoparticles, the finishing liquid is squeezed into the fibers through mechanical force, and then dried or heat-treated to integrate the nanoparticles into the yarns. The nanoparticles are embedded in the woven yarns to increase the functionality of the fabrics. For example, by adding nanoparticles of silver (Ag), copper (Cu), zinc (Zn), and photocatalytic antibacterial agents such as nano-TiO2 and nano-ZnO, textiles with antibacterial functions can be developed; by adding nano-TiO2, nano-ZnO, nano-silicon-based oxides, etc., these nanoparticles can enhance the absorption of ultraviolet rays by textiles and provide anti-ultraviolet functions; for example, Al2O3, TiO2, SiO2 and Fe2O3, etc., these nanoparticles have strong absorption properties for mid-infrared rays and can be used to make textiles with thermal insulation functions.
[0041] In one embodiment, if Figure 5 As shown, before step S40, that is, before the woven fabric is softened to obtain the softened fabric, and the softened fabric is shaped to obtain the finished fabric, the process also includes: S401: Mechanically stretching the woven fabric.
[0042] Specifically, in order to improve the dimensional stability and shape of the fabric, the woven fabric is mechanically stretched so that the fabric is unfolded under a certain tension, usually in the weft and warp directions of the fabric to ensure that the fabric has uniform tension and dimensional stability in both directions. Mechanical stretching can make the fabric fibers more closely arranged, enhance their elasticity and wrinkle resistance. Through this treatment, the dimensional stability of the fabric is improved, and deformation during wearing and washing is reduced, while the feel and drape of the fabric can also be improved.
[0043] S402: After the mechanical stretching treatment, the stretched fabric is subjected to antistatic treatment, using an antistatic agent not exceeding 0.5 g / L, maintaining the treatment temperature at 50-60°C, and the treatment time is 10-20 minutes.
[0044] Specifically, after mechanical stretching treatment, the fabric may generate static electricity, so anti-static treatment is required. By using an anti-static agent not exceeding 0.5g / L and maintaining the treatment temperature at 50-60°C for 10-20 minutes, this temperature range helps the anti-static agent to be evenly distributed and penetrated on the fabric while avoiding thermal damage to the fabric. This time length ensures that the anti-static agent fully reacts with the fabric to achieve an ideal anti-static effect. Fabrics after anti-static treatment reduce the generation of static electricity and improve the wearing comfort and functionality of the fabric.
[0045] In one embodiment, if Figure 6 As shown, in step S40, the woven fabric is softened by using a pre-proportioned softener to obtain the softened fabric, which specifically includes: S41: Immerse the woven fabric in a softener solution containing natural plant extracts for 20 minutes. The softener solution is obtained by mixing and stirring 1-2% natural lavender extract, 1-2% chamomile extract, 1-2% aloe extract, 10-15% quaternary ammonium salt, 5-10% silicone softener, 5-8% stearic acid, 0.5-1% carboxymethyl cellulose, 0.1-0.2% sodium benzoate and 59.8-76.4% water.
[0046] Specifically, the woven fabric is immersed in a softener solution containing natural plant extracts and soaked for 20 minutes. The softener solution is obtained by mixing and stirring 1-2% natural lavender extract, 1-2% chamomile extract, 1-2% aloe extract, 10-15% quaternary ammonium salt, 5-10% silicone softener, 5-8% stearic acid, 0.5-1% carboxymethyl cellulose, 0.1-0.2% sodium benzoate and 59.8-76.4% water. The softener solution includes natural lavender extract, chamomile extract or aloe extract. Lavender, chamomile or aloe extract can not only provide a softening effect, but also have skin soothing, anti-inflammatory and moisturizing properties. Lavender extract usually has a calming and soothing effect, chamomile extract helps reduce skin irritation and inflammation, and aloe extract is known for its moisturizing and healing properties to provide a more environmentally friendly and gentle softening effect.
[0047] S42: Drying the soaked fabric using a drum dryer to obtain a softened fabric.
[0048] Specifically, the fabric after soaking treatment is dried using a drum dryer. The drum dryer evenly heats the fabric through internal hot air circulation to accelerate the evaporation of moisture. During the drum drying process, the fabric rolls inside the drum to ensure that every part of the fabric can be evenly exposed to the hot air, thereby achieving a uniform drying effect and ultimately obtaining a softened fabric.
[0049] In one embodiment, if Figure 7 As shown, in step S40, the softened fabric is subjected to shaping treatment to obtain a finished fabric product, which specifically includes: S43: performing ultrasonic trimming on the softened fabric to remove fibers at the edge of the softened fabric to obtain trimmed fabric.
[0050] Specifically, the fabric is first softened to obtain the softened fabric. In order to remove the fibers at the edge and make the fabric edge neater, the softened fabric needs to be trimmed. Therefore, the softened fabric is trimmed by using ultrasound, that is, the ultrasonic trimming machine generates high-frequency vibration through the vibrating blade to cut off the fibers at the edge of the fabric. Removing the fibers at the edge of the softened fabric helps to improve the appearance and durability of the fabric and avoid the falling off or scattering of the edge fibers.
[0051] S44: shaping the edge-cut fabric within a temperature range of 120° C. to 150° C. for a time period of 15 to 30 minutes, and finally obtaining a finished fabric product.
[0052] Specifically, different fabrics require different temperatures to achieve the best shaping effect. Therefore, the shaping treatment of the fabric after edge trimming is carried out at a high temperature of 120°C to 150°C. It is determined according to the characteristics of the fabric and the required shaping effect. The shaping process of the fabric needs to last for 15 minutes to 30 minutes. Through the control of high temperature and time, the shape and size of the fabric are stabilized to prevent the fabric from deformation or relaxation during use, thereby ensuring the quality and durability of the finished fabric.
[0053] It should be understood that the size of the serial numbers of the steps in the above embodiments does not mean the order of execution. The execution order of each process should be determined by its function and internal logic, and should not constitute any limitation on the implementation process of the embodiments of the present application.
[0054] Those skilled in the art can clearly understand that for the convenience and simplicity of description, only the division of the above-mentioned functional units and modules is used as an example. In actual applications, the above-mentioned functions can be distributed and completed by different functional units and modules as needed, that is, the internal structure of the device can be divided into different functional units or modules to complete all or part of the functions described above.
[0055] The embodiments described above are only used to illustrate the technical solutions of the present application, rather than to limit them. Although the present application has been described in detail with reference to the aforementioned embodiments, a person skilled in the art should understand that the technical solutions described in the aforementioned embodiments may still be modified, or some of the technical features may be replaced by equivalents. Such modifications or replacements do not deviate the essence of the corresponding technical solutions from the spirit and scope of the technical solutions of the embodiments of the present application, and should all be included in the protection scope of the present application.
Claims
1. A method for preparing a skin-friendly elastic thermal insulation fabric, It is characterized in that The preparation method of the skin-friendly elastic thermal insulation fabric comprises: Selecting natural fibers and elastic fibers, and mechanically mixing the natural fibers and the elastic fibers according to a preset ratio; The mixed fibers are made into yarn through a spinning process; The yarn is woven by machine to obtain a woven fabric; The woven fabric is softened by using a pre-proportioned softener to obtain the softened fabric, and the softened fabric is shaped to obtain a finished fabric product.
2. A method for preparing a skin-friendly elastic thermal insulation fabric according to claim 1, It is characterized in that The selecting of natural fibers and elastic fibers, and mechanically mixing the natural fibers and elastic fibers according to a preset ratio comprises: 40%-60% of organic cotton fiber and 40%-60% of spandex fiber are selected as raw materials, and 2%-5% of bamboo charcoal fiber is added to the raw materials. The organic cotton fiber and the spandex fiber are mixed in a fiber mixer to serve as the warp and weft of the fabric.
3. A method for preparing a skin-friendly elastic thermal insulation fabric according to claim 1, It is characterized in that The method of preparing the mixed fibers into yarn by a spinning process comprises: Spinning the mixed fibers by ring spinning technology to obtain preliminarily treated yarns; The yarn is obtained by performing a secondary treatment on the preliminarily treated yarn using a double-sided brushing technique.
4. A method for preparing a skin-friendly elastic thermal insulation fabric according to claim 1, It is characterized in that The weaving method includes: The yarn is woven into a double-layer fabric using double-layer weaving technology, wherein the inner layer uses yarn containing bamboo charcoal fiber, and the outer layer uses yarn containing organic cotton fiber and spandex fiber; The plain weaving process used has a density of 200-300 threads / 10cm.
5. A method for preparing a skin-friendly elastic thermal insulation fabric according to claim 1, It is characterized in that Nanoparticles are added during the weaving process so that the nanoparticles are embedded in the woven yarns.
6. A method for preparing a skin-friendly elastic thermal insulation fabric according to claim 1, It is characterized in that Before the woven fabric is softened by using a pre-proportioned softener, the method includes: Performing mechanical stretching treatment on the woven fabric; After the mechanical stretching treatment, the stretched fabric is subjected to antistatic treatment, using an antistatic agent not exceeding 0.5 g / L, the treatment temperature is maintained at 50-60°C, and the treatment time is 10-20 minutes.
7. A method for preparing a skin-friendly elastic thermal insulation fabric according to claim 1, It is characterized in that The woven fabric is softened by using a pre-proportioned softener to obtain the softened fabric, which comprises: The woven fabric is immersed in a softener solution containing natural plant extracts for 20-30 minutes at a soaking temperature of 40-60° C. The softener solution is obtained by mixing and stirring 1-2% of natural lavender extract, 1-2% of chamomile extract, 1-2% of aloe extract, 10-15% of quaternary ammonium salt, 5-10% of silicone softener, 5-8% of stearic acid, 0.5-1% of carboxymethyl cellulose, 0.1-0.2% of sodium benzoate and 59.8-76.4% of water; The soaked fabric is dried using a drum dryer to obtain the softened fabric.
8. The method for preparing the skin-friendly elastic thermal insulation fabric according to claim 1, It is characterized in that The fabric after the softening treatment is subjected to shaping treatment to obtain a finished fabric product, comprising: Performing ultrasonic trimming on the softened fabric to remove fibers from the edge of the softened fabric to obtain trimmed fabric; The trimmed fabric is shaped within a temperature range of 120° C. to 150° C., and the time is controlled within a range of 15 minutes to 30 minutes, to finally obtain the finished fabric.
Citation Information
Patent Citations
Hand-mouth baby wet tissue and preparation method thereof
CN103040688A
Efficient antibacterial deodorant fabric
CN103101276A
Aloe-extract-containing softener
CN106894228A
Clothing care agent
CN107780225A
Sweat-absorbing and odor-resistant sock and preparation method thereof
CN111642823A