Preparation method of 300-series stainless steel symmetric longitudinal division wide cold plate
Through the preparation method of symmetrical vertical and wide-width cold plates, including rolling, solid solution, pickling, flattening and pulling treatment, the problem of controlling the thickness and unevenness of the cold plate of 300 series stainless steel is solved, and high-quality product production is achieved .
Patent Information
- Application Number
- CN202411143863.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-20
- Publication Date
- 2024-11-22
AI Technical Summary
When producing 300 series stainless steel cold plates, the thickness of the wide-width cold plates is difficult to control the difference in the thickness of the horizontal plate and the unevenness of the plate shape, resulting in unqualified product quality and affecting customer use.
The preparation method of symmetrical vertical and wide-width cold plates includes rolling, solid solution treatment, pickling treatment, leveling treatment and bending straightening treatment after obtaining raw materials. By designing the intermediate roll structure and optimizing the rolling process, the rolling is controlled. The thickness of the back steel belt is 0~0.8% different from the plate and the unevenness of the plate is less than or equal to 10mm/m, and the thickness is flattened and pulled in the cold line process.
The preparation of symmetrical vertical and wide-width cold plate of 300 series stainless steel was successfully achieved, with a difference of lateral thickness of the same plate as the plate, and a plate unevenness of the plate was ≤8mm/m, which improved product quality and production efficiency.
Smart Images

Figure CN118988975A_ABST
Abstract
Description
Technical Field
[0001] The invention belongs to the field of stainless steel strip preparation, and relates to a method for preparing a 300 series stainless steel symmetrical longitudinally divided wide-width cold plate. Background Art
[0002] 300 series stainless steel cold plate is a special variety developed by TISCO. It has the characteristics of good surface quality, high dimensional accuracy, excellent welding performance, etc. It is widely used in the manufacture of deep-drawn parts, acid pipelines, containers, etc. Customers have high requirements on the thickness and plate shape of this product. The horizontal thickness difference of the same plate is ≤1%, and the plate shape unevenness requirement is ≤10mm / m.
[0003] In order to improve production efficiency and product cost competitiveness, a symmetrical longitudinal division method is adopted to produce 300 series stainless steel cold plates with a width of 900-1050mm. That is, a roll of steel coil with a width of 1800-2100mm is directly and symmetrically divided longitudinally into two rolls of steel coils with a width of 900-1050mm. This production mode will put forward higher requirements on the process quality control of wide-width cold plate products with a width of 1800-2100mm, and bring challenges to the quality control level of production enterprises.
[0004] The wide cold plate is rolled by SUNDWING S6-High 2100mm 18-roller rolling mill with multi-pass reversible rolling. After rolling, it is annealed, pickled, leveled, straightened and curled in the cold line process. Finally, it is symmetrically divided into two narrow-width steel coils in the finishing process. During the production process, problems such as the transverse thickness difference of more than 1% and edge wave shape defects occur, which seriously affect customer use. It is urgent to propose a method that is easy to operate on site to quickly and effectively solve this problem. Summary of the invention
[0005] In order to overcome the defects in the above-mentioned related technologies, the present invention proposes a method for preparing a 300 series stainless steel symmetrical longitudinally divided wide cold plate.
[0006] Some embodiments of the present invention provide a method for preparing a 300 series stainless steel symmetrical longitudinally divided wide cold plate, the method comprising: Obtaining raw materials, the raw materials comprising 300 series stainless steel strips, the thickness of the 300 series stainless steel strips having a transverse convexity C40=(0-1%)*H0 and a wedge-shaped amount W40=(-0.5%-0.5%)*H0; Rolling the 300 series stainless steel strip to obtain the rolled stainless steel strip, and making the thickness difference of the rolled stainless steel strip in the transverse direction be 0-0.8% and the plate unevenness be less than or equal to 10 mm / m; The rolled stainless steel strip is subjected to solution treatment, pickling treatment, flattening treatment and bending and straightening treatment; The rolled stainless steel strip is symmetrically longitudinally stripped; Among them, the C40 is the difference between the midpoint thickness of the 300 series stainless steel strip in the width direction and the thickness at 40 mm from the edge, the W40 is the difference between the thickness at 40 mm from the edge on the operating side and the thickness at 40 mm from the edge on the transmission side, and H0 is the nominal thickness of the 300 series stainless steel strip.
[0007] The method of rolling the 300 series stainless steel strip and obtaining the rolled stainless steel strip, and making the thickness difference of the rolled stainless steel strip in the transverse direction be 0-0.8% and the plate unevenness be less than or equal to 10 mm / m, comprises: The structure of the intermediate roller for rolling the 300 series stainless steel strip is designed, the cone length of the intermediate roller is 600 mm, the intermediate roller is a straight cone from 0 to 540 mm, and the ratio of the cone length to the cone height of the straight cone is 1:0.001 to 2:0.002; The line segment of the intermediate roller intersecting with the vertical plane passing through the center line at 540mm~600mm is a sine curve, the half angle of the sine curve is 60°~80°, and the cone length:cone height of the intermediate roller of 540mm~600mm is 1:0.0004~1:0.0006.
[0008] The method of rolling the 300 series stainless steel strip and obtaining the rolled stainless steel strip, and making the thickness difference of the rolled stainless steel strip in the transverse direction be 0-0.8% and the plate unevenness be less than or equal to 10 mm / m, further comprises: The total number of rolling passes is 5 to 7, the deformation rate of the first pass is 12 to 18%, the deformation rate from the second pass to the pass before the finished product decreases successively, and the deformation rate of the finished product pass is 3 to 7%. The target curve of the plate shape for the first, second and third rolling passes is an arc with an opening upward, the actual stress deviation value of the edge plate shape is in the range of 40 to 100 N / mm2, and the actual stress deviation value of the middle plate shape is in the range of -30 to 0 N / mm2; the target curve of the plate shape from the fourth rolling pass to the finished product pass is a wave shape, the actual stress deviation value of the edge plate shape is controlled in the range of 10 to 40 N / mm2, and the actual stress deviation value of the middle plate shape is controlled in the range of 10 to 40 N / mm2. The total deformation rate is controlled at 40~50%.
[0009] During the leveling treatment, the leveling roller convexity is 20 to 30 passes, the tension used for the leveling treatment is 20 to 35 tons, the elongation is 0.3 to 1.0%, the stretching tension of the stretching straightening treatment is 40 to 100 tons, the elongation is 0.5% to 2.0%, and the stretching straightening unit has three groups of stretching straightening rollers, and the reduction amounts are 30 to 40 mm, 20 to 30 mm and 10 to 30 mm respectively.
[0010] The beneficial effects of the present invention are: By designing the raw material thickness parameters, raw materials with appropriate thickness requirements can be provided for the cold rolling process. After rolling in the cold rolling process, the convexity and wedge shape of the raw material are fully improved.
[0011] Through the roll system design and process optimization of the rolling process, we can provide intermediate rolls with sufficient taper and reasonable processes to achieve the matching of the rolling process and the target plate shape curve, eliminate the lateral thickness difference, and ensure the straightness of the strip shape after rolling.
[0012] Through the standardization of cold line leveling and straightening process, the physical plate shape after annealing can be improved to the greatest extent, and the plate shape unevenness can reach ≤10mm / m.
[0013] After adopting the method of the present invention, 300 series stainless steel symmetrical longitudinally divided wide cold plates were successfully prepared, the transverse thickness difference between the same plates reached ≤0.05%, and the plate shape unevenness reached ≤8mm / m. BRIEF DESCRIPTION OF THE DRAWINGS
[0014] In order to more clearly illustrate the technical solutions in the embodiments of the present invention or related technologies, the drawings required for use in the embodiments or related technical descriptions are briefly introduced below. Obviously, the drawings described below are only some embodiments of the present invention. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative work.
[0015] Figure 1 The target curve of the cold rolling 1st to 3rd pass of the present invention; Figure 2 It is the target curve of the cold-rolled 4th-finished pass plate shape of the present invention. DETAILED DESCRIPTION
[0016] In order to make the above-mentioned purposes, features and advantages of the present invention more obvious and easy to understand, the technical scheme in the embodiments of the present invention will be clearly and completely described below in conjunction with the drawings in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work belong to the scope of protection of the present invention.
[0017] In the description of the present invention, it should be understood that the terms "center", "up", "down", "front", "back", "left", "right", "vertical", "horizontal", "top", "bottom", "inside", "outside", etc., indicating the orientation or position relationship are based on the orientation or position relationship shown in the drawings, and are only for the convenience of describing the present invention and simplifying the description, rather than indicating or implying that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore cannot be understood as a limitation on the present invention.
[0018] The terms "first" and "second" are used for descriptive purposes only and should not be understood as indicating or implying relative importance or implicitly indicating the number of the indicated technical features. Thus, a feature defined as "first" or "second" may explicitly or implicitly include one or more of the features. In the description of the present invention, unless otherwise specified, "plurality" means two or more.
[0019] Some embodiments of the present invention provide a method for preparing a 300 series stainless steel symmetrical longitudinally divided wide cold plate, the method comprising: Obtaining raw materials, the raw materials comprising 300 series stainless steel strips, the thickness of the 300 series stainless steel strips having a transverse convexity C40=(0-1%)*H0 and a wedge-shaped amount W40=(-0.5%-0.5%)*H0; Rolling the 300 series stainless steel strip to obtain the rolled stainless steel strip, and making the thickness difference of the rolled stainless steel strip in the transverse direction be 0-0.8% and the plate unevenness be less than or equal to 10 mm / m; The rolled stainless steel strip is subjected to solution treatment, pickling treatment, flattening treatment and bending and straightening treatment; The rolled stainless steel strip is symmetrically longitudinally stripped; Among them, the C40 is the difference between the midpoint thickness of the 300 series stainless steel strip in the width direction and the thickness at 40 mm from the edge, the W40 is the difference between the thickness at 40 mm from the edge on the operating side and the thickness at 40 mm from the edge on the transmission side, and H0 is the nominal thickness of the 300 series stainless steel strip.
[0020] The method of rolling the 300 series stainless steel strip and obtaining the rolled stainless steel strip, and making the thickness difference of the rolled stainless steel strip in the transverse direction be 0-0.8% and the plate unevenness be less than or equal to 10 mm / m, comprises: The structure of the intermediate roller for rolling the 300 series stainless steel strip is designed, the cone length of the intermediate roller is 600 mm, the intermediate roller is a straight cone from 0 to 540 mm, and the ratio of the cone length to the cone height of the straight cone is 1:0.001 to 2:0.002; The line segment of the intermediate roller intersecting with the vertical plane passing through the center line at 540mm~600mm is a sine curve, the half angle of the sine curve is 60°~80°, and the cone length:cone height of the intermediate roller of 540mm~600mm is 1:0.0004~1:0.0006.
[0021] The method of rolling the 300 series stainless steel strip and obtaining the rolled stainless steel strip, and making the thickness difference of the rolled stainless steel strip in the transverse direction be 0-0.8% and the plate unevenness be less than or equal to 10 mm / m, further comprises: The total number of rolling passes is 5 to 7, the deformation rate of the first pass is 12 to 18%, and the deformation rates of the second pass to the final product pass decrease successively, and the deformation rate of the final product pass is 3 to 7%. The target curve of the plate shape of the first, second and third rolling passes is an arc with an opening upward, such as Figure 1 As shown in the figure, the actual stress deviation of the edge plate shape is within the range of 40~100N / mm2, and the actual stress deviation of the middle plate shape is within the range of -30~0N / mm2; the plate shape target curve from the 4th rolling pass to the finished product pass is wavy, as shown in the figure. Figure 2 As shown in the figure, the actual stress deviation value of the edge plate shape is controlled within the range of 10~40N / mm2, and the actual stress deviation value of the middle plate shape is controlled within the range of 10~40N / mm2. The total deformation rate is controlled at 40~50%.
[0022] During the leveling treatment, the leveling roller convexity is 20 to 30 passes, the tension used for the leveling treatment is 20 to 35 tons, the elongation is 0.3 to 1.0%, the stretching tension of the stretching straightening treatment is 40 to 100 tons, the elongation is 0.5% to 2.0%, and the stretching straightening unit has three groups of stretching straightening rollers, and the reduction amounts are 30 to 40 mm, 20 to 30 mm and 10 to 30 mm respectively.
[0023] In the description of this specification, specific features, structures, materials or characteristics may be combined in an appropriate manner in any one or more embodiments or examples.
[0024] The above are only specific embodiments of the present invention, but the protection scope of the present invention is not limited thereto. Any changes or substitutions that can be easily thought of by a person skilled in the art within the technical scope disclosed by the present invention should be included in the protection scope of the present invention. Therefore, the protection scope of the present invention should be based on the protection scope of the claims.
Claims
1. A method for preparing a 300 series stainless steel symmetrical longitudinally divided wide cold plate, characterized in that: include: Obtaining raw materials, the raw materials comprising 300 series stainless steel strips, the thickness of the 300 series stainless steel strips having a transverse convexity C40=(0-1%)*H0 and a wedge-shaped amount W40=(-0.5%-0.5%)*H0; Rolling the 300 series stainless steel strip to obtain the rolled stainless steel strip, and making the thickness difference of the rolled stainless steel strip in the transverse direction be 0-0.8% and the plate unevenness be less than or equal to 10 mm / m; The rolled stainless steel strip is subjected to solution treatment, pickling treatment, flattening treatment and bending and straightening treatment; The rolled stainless steel strip is symmetrically divided into longitudinal strips; Among them, the C40 is the difference between the midpoint thickness of the 300 series stainless steel strip in the width direction and the thickness at 40 mm from the edge, the W40 is the difference between the thickness at 40 mm from the edge on the operating side and the thickness at 40 mm from the edge on the transmission side, and H0 is the nominal thickness of the 300 series stainless steel strip.
2. The method for preparing a 300 series stainless steel symmetrical longitudinally divided wide cold plate according to claim 1, characterized in that: The method of rolling the 300 series stainless steel strip and obtaining the rolled stainless steel strip, and making the thickness difference of the rolled stainless steel strip in the transverse direction be 0-0.8% and the plate unevenness be less than or equal to 10 mm / m, comprises: The structure of the intermediate roller for rolling the 300 series stainless steel strip is designed, the cone length of the intermediate roller is 600 mm, the intermediate roller is a straight cone from 0 to 540 mm, and the ratio of the cone length to the cone height of the straight cone is 1:0.001 to 2:0.002; The line segment of the intermediate roller intersecting with the vertical plane passing through the center line at 540mm~600mm is a sine curve, the half angle of the sine curve is 60°~80°, and the cone length:cone height of the intermediate roller of 540mm~600mm is 1:0.0004~1:0.0006.
3. The method for preparing a 300 series stainless steel symmetrical longitudinally divided wide cold plate according to claim 2, characterized in that: The method of rolling the 300 series stainless steel strip and obtaining the rolled stainless steel strip, and making the thickness difference of the rolled stainless steel strip in the transverse direction be 0-0.8% and the plate unevenness be less than or equal to 10 mm / m, further comprises: The total number of rolling passes is 5 to 7, the deformation rate of the first pass is 12 to 18%, the deformation rate from the second pass to the pass before the finished product decreases successively, and the deformation rate of the finished product pass is 3 to 7%. The target curve of the plate shape for the first, second and third rolling passes is an arc with an opening upward, the actual stress deviation value of the edge plate shape is in the range of 40 to 100 N / mm2, and the actual stress deviation value of the middle plate shape is in the range of -30 to 0 N / mm2; the target curve of the plate shape from the fourth rolling pass to the finished product pass is a wave shape, the actual stress deviation value of the edge plate shape is controlled in the range of 10 to 40 N / mm2, and the actual stress deviation value of the middle plate shape is controlled in the range of 10 to 40 N / mm2. The total deformation rate is controlled at 40~50%.
4. The method for preparing a 300 series stainless steel symmetrical longitudinally divided wide cold plate according to claim 3, characterized in that: During the leveling treatment, the leveling roller convexity is 20 to 30 passes, the tension used for the leveling treatment is 20 to 35 tons, the elongation is 0.3 to 1.0%, the stretching tension of the stretching straightening treatment is 40 to 100 tons, the elongation is 0.5% to 2.0%, and the stretching straightening unit has three groups of stretching straightening rollers, and the reduction amounts are 30 to 40 mm, 20 to 30 mm and 10 to 30 mm respectively.
Citation Information
Patent Citations
Stainless steel cold-rolled strip steel production device
CN108906888A
300-series stainless steel wide and thick cold plate shape control method
CN112355061A
Method for improving flatness of stainless steel cold-rolled sheet of lining of low-temperature liquid container
CN114472525A
Stainless steel wide cold plate rolling plate shape control method
CN115121622A
Method for controlling dirty marks on surface of 301-series stainless steel wide panel
CN115921539A
Cited By
Thickness hit rate control method for stainless steel wide and thick cold plate
CN119747384A
A method for controlling the thickness hit rate of a stainless steel wide and thick cold plate
CN119747384B
Narrow and thick stainless steel cold plate and preparation method thereof
CN120961594A