Method for synthesizing granular acid ammonium fluoride salt from fluorine-containing waste concentrated sulfuric acid, product and application
By adding dehydrating agent, ammonium fluoride and iron sulfate to the fluorine-containing waste sulfuric acid reaction, granular acid ammonium salt is generated, which solves the resource utilization problem of by-product sulfuric acid and provides a more lasting oil-water well Relieve blocking effect.
Patent Information
- Application Number
- CN202411084747.X
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-08
- Publication Date
- 2024-11-22
- Estimated Expiration
- 2044-08-08
AI Technical Summary
The by-product sulfuric acid produced in the boron trifluoride production process contains high concentration of fluorine, which cannot directly neutralize emissions, and there are difficulties in its resource utilization, resulting in serious problems in tanking of waste acid.
By adding dehydrating agent, ammonium fluoride and iron sulfate to the fluorine-containing waste sulfuric acid, the insulation and stirring reaction at 90-120°C is carried out to form a granular acid ammonium salt, which is used for oil-water well deblocking agent.
The resource utilization of by-products is realized. The prepared acid ammonium salt has a more lasting acid-resolving and blocking effect as an oil-water well deblocking agent, which avoids formation corrosion and new blocking problems, and is easy to store and use.
Smart Images

Figure BDA0004984849540000041
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of oil and gas field chemical industry, and in particular to a method, product and application of synthesizing granular acidic ammonium fluoride salt from fluorine-containing waste concentrated sulfuric acid. Background Art
[0002] In the production process of boron trifluoride, a large amount of sulfuric acid (about 96%) is produced as a by-product. This sulfuric acid is not only highly concentrated, but also contains up to 16.8g / L of fluorine. It cannot be directly neutralized and discharged, and there are many obstacles to its direct resource utilization. The problem of factory waste acid tank stagnation is very serious, and there is an urgent need to provide a solution.
[0003] In view of this, the present invention is proposed. Summary of the invention
[0004] The purpose of the present invention is to provide a method, product and application of synthesizing granular acid ammonium fluoride salt from fluorine-containing waste concentrated sulfuric acid, so as to solve the problems existing in the above-mentioned prior art.
[0005] To achieve the above object, the present invention provides the following solutions:
[0006] One of the technical solutions of the present invention is to provide a method for synthesizing acidic ammonium salt from fluorine-containing waste concentrated sulfuric acid, comprising the following steps:
[0007] A dehydrating agent is added to the fluorine-containing waste concentrated sulfuric acid for dehydration, and then ammonium fluoride is added, and the mixture is kept warm and stirred at 90-120° C., and then ferric sulfate is added, and the mixture is stirred and reacted at 90-120° C. to obtain the acidic ammonium salt.
[0008] As a further preferred embodiment of the present invention, the dehydrating agent is anhydrous sodium sulfate.
[0009] As a further preferred embodiment of the present invention, the mass volume ratio of the ammonium fluoride, ferric sulfate and fluorine-containing waste concentrated sulfuric acid is 400-500kg:25-30kg:200L.
[0010] As a further preferred embodiment of the present invention, the fluorine-containing waste concentrated sulfuric acid is a by-product of producing boron trifluoride; and the fluorine content in the fluorine-containing waste concentrated sulfuric acid is 1.8-100 g / L.
[0011] As a further preferred embodiment of the present invention, the time of the heat preservation and stirring is 15-20 minutes; the time of the stirring reaction is 5-10 minutes.
[0012] The second technical solution of the present invention is to provide the acidic ammonium salt prepared by the above preparation method.
[0013] The third technical solution of the present invention is to provide the use of the above-mentioned acidic ammonium salt as an oil and water well plugging remover.
[0014] A fourth technical solution of the present invention is to provide an oil and water well plugging remover containing the above-mentioned acidic ammonium salt.
[0015] The acidic ammonium salt product prepared by the invention is in the form of crystal particles, white in color, and very easily soluble in water, with a solubility of about 70g / 100g in water, and a pH value of a saturated solution of 3-3.5.
[0016] The treatment of fluorine-containing waste concentrated sulfuric acid involves complex chemical reactions. The present invention has taken a series of measures to obtain a product with high hardness and easy crushing and processing at room temperature:
[0017] First, add an appropriate amount of dehydrating agent anhydrous sodium sulfate to the fluorine-containing waste concentrated sulfuric acid to prevent the sulfuric acid from boiling.
[0018] Secondly, a sufficient amount of ammonium fluoride powder is added to generate acid ammonium salt, but the product obtained by this treatment is not hard enough and is relatively soft, which is not conducive to crushing. At the same time, this step is an exothermic reaction and is accompanied by the release of some hydrogen fluoride, so protective measures need to be taken.
[0019] Finally, before the acidic ammonium salt is cooled, an appropriate amount of ferric sulfate is added to partially generate ammonium ferric alum crystal seeds, which increases the strength of the product after solidification and makes it easier to crush and grind.
[0020] In the prior art, when preparing an oil and water well unblocking agent, soil acid (usually containing 10%-15% hydrochloric acid and 3%-8% hydrofluoric acid) is used to remove mud blockage and improve the permeability of mud sandstone formations to facilitate water injection or oil production. The hydrochloric acid in the soil acid can dissolve carbonates and iron and aluminum compounds in the formation, while the hydrofluoric acid can dissolve clay and silicates in the formation. The acid ammonium salt prepared by the present invention can replace the key component soil acid in the unblocking agent. The acid ammonium salt has moderate strength and a pH value of about 3.0-3.5. The dissolution rate of carbonate is relatively slow, and the formation near the wellbore will not be eroded due to excessive corrosion, resulting in well wall collapse. There is no large-scale generation of calcium sulfate and calcium fluoride to cause new blockage problems; at the same time, the acid ammonium salt of the present invention has a longer range of influence, a more lasting acid unblocking effect, and obvious benefits of increased production and increased injection.
[0021] The present invention discloses the following technical effects:
[0022] The invention provides a method for synthesizing granular acidic ammonium fluoride salt by using fluorine-containing waste concentrated sulfuric acid as a raw material. The method realizes resource utilization of the byproduct fluorine-containing waste concentrated sulfuric acid. The prepared acidic ammonium salt can be used as an oil and water well unblocking agent for acid unblocking of oil and water wells.
[0023] The acidic ammonium salt prepared by the invention is convenient for storage, transportation and use, has good safety during use, has a slow corrosion rate of the formation near the wellbore, has a long affected distance, and has a better acidification and plugging removal effect. DETAILED DESCRIPTION
[0024] Various exemplary embodiments of the present invention will now be described in detail. This detailed description should not be considered as limiting the present invention, but should be understood as a more detailed description of certain aspects, features, and embodiments of the present invention.
[0025] It should be understood that the terms described in the present invention are only for describing a particular embodiment and are not intended to limit the present invention. In addition, for the numerical range in the present invention, it should be understood that each intermediate value between the upper and lower limits of the scope is also specifically disclosed. The intermediate value in any stated value or stated range, and each smaller range between any other stated value or intermediate value in the described range is also included in the present invention. The upper and lower limits of these smaller ranges can be independently included or excluded in the scope.
[0026] Unless otherwise indicated, all technical and scientific terms used herein have the same meanings as those generally understood by those skilled in the art. Although the present invention describes only preferred methods and materials, any methods and materials similar or equivalent to those described herein may also be used in the implementation or testing of the present invention. All documents mentioned in this specification are incorporated by reference to disclose and describe the methods and / or materials associated with the documents. In the event of a conflict with any incorporated document, the content of this specification shall prevail.
[0027] It will be apparent to those skilled in the art that various modifications and variations may be made to the specific embodiments of the present invention description without departing from the scope or spirit of the present invention. Other embodiments derived from the present invention description will be apparent to those skilled in the art. The present invention description and examples are exemplary only.
[0028] The words “include,” “including,” “have,” “contain,” etc. used in this document are open-ended terms, meaning including but not limited to.
[0029] In the following examples of the present invention, the fluorine-containing waste concentrated sulfuric acid comes from Shandong Wanbang Chemical Co., Ltd., and has the following composition: 95% H2SO4, 4% H2O and 1% HF, and the fluorine content is 16.8 g / L.
[0030] Example 1
[0031] 200L of fluorine-containing waste concentrated sulfuric acid was put into a fluoroplastic stirred atmospheric pressure reactor (the reflux condenser was turned on in advance, and the water cooling temperature was 25°C), and then 400kg of powdered ammonium fluoride was slowly and evenly fed, and stirred continuously. The feed port of the reactor was closed in time during the feeding interval and after the feeding was completed, and the reactor was kept warm and stirred at 110°C for 15 minutes. During the reaction, there was a boiling phenomenon. Due to the rapid increase in temperature caused by the exothermic reaction, the water in it boiled rapidly, and a large amount of hydrofluoric acid volatilized, which had great operational risks; finally, the material was discharged from the bottom of the reactor.
[0032] The pilot product in this batch solidifies quickly, and the discharged material sticks to the agitator. After cooling, the product has an average hardness, similar to that of Class I soil, and a firmness coefficient of 0.3, which is not conducive to crushing and grinding.
[0033] Example 2
[0034] Put 200L of fluorine-containing waste concentrated sulfuric acid into a fluoroplastic stirred atmospheric pressure reactor (turn on the reflux condenser in advance, the water cooling temperature is 25℃), add 25kg of powdered anhydrous sodium sulfate at one time, stir for 5min; then slowly add 400kg of powdered ammonium fluoride at a uniform speed, stir continuously, close the feed port of the reactor in time during the feeding interval and after the feeding is completed, and keep warm and stir at 110℃ for 15min. There is basically no boiling phenomenon during the reaction, and only a small amount of hydrofluoric acid volatilizes; finally, discharge the material from the bottom of the reactor.
[0035] The product of this batch of pilot test also has the phenomenon of sticking to the agitator. hardness It is slightly improved compared with Example 1, similar to Class II soil, with a firmness coefficient of 0.5. The product is still sticky and not easy to crush and grind.
[0036] Example 3
[0037] Put 200L of fluorine-containing waste concentrated sulfuric acid into a fluoroplastic stirred atmospheric pressure reactor (turn on the reflux condensation device in advance, and the water cooling temperature is 25℃), feed 25kg of powdered anhydrous sodium sulfate at one time, and stir for 5min; then slowly and evenly feed 400kg of powdered ammonium fluoride, stir continuously, close the feed port of the reactor in time during the feeding interval and after the feeding is completed, and keep stirring at 110℃ for 15min; then continue to feed 25kg of powdered ferric sulfate, continue to stir at 110℃ for 5min, and the viscosity of the reaction system will drop significantly; finally, discharge the material from the bottom of the reactor. The final product is basically non-sticky to the reactor and the stirrer, and the discharge is very convenient. The conveyor belt is used for uniform discharge, and the bottom is water-cooled to make it solidify quickly.
[0038] This batch of pilot products has fast solidification speed, high strength, similar to Class II soil, solidity coefficient of 0.8, easy to crush and grind, white powder, and not easy to condense into a mass again, and excellent water solubility, solubility of 70g / 100g, saturated solution pH value of 3.2. The product obtained from this production is used as the finalized product, code-named WB-F-01.
[0039] Effect verification example:
[0040] The acidic ammonium salt product prepared by the present invention was prepared into a 25wt.% aqueous solution (labeled as 25wt.% WB-F-01 aqueous solution), and the effect of dissolving potassium feldspar and calcite was compared with that of mud acid (12wt.% HCl+8wt.% HF). The results are shown in Table 1.
[0041] Table 1
[0042]
[0043] At present, the main agent for acidizing and unblocking oil and water wells is soil acid, and the configuration of soil acid must be strictly allocated according to the formation geology, because hydrochloric acid dissolves calcite in a targeted manner, but does not work on feldspar, and hydrofluoric acid can only dissolve feldspar in a targeted manner, and can only change the dosage according to the feldspar content, which brings difficulties to downhole operations. The acid ammonium salt of the present invention can solve this problem well. At the same time, the initial rate of acid ammonium salt dissolution of potassium feldspar is slower, but the later stage will slowly have a similar dissolution effect to soil acid, and the spread distance of acid will be farther, the acidizing and unblocking effect is more lasting, and the benefit of increasing production and injection is more obvious. Moreover, the acid ammonium salt of the present invention is slower to the calcite dissolution rate, which is beneficial to the unblocking of oil and water wells.
[0044] The embodiments described above are only descriptions of the preferred modes of the present invention, and are not intended to limit the scope of the present invention. Without departing from the design spirit of the present invention, various modifications and improvements made to the technical solutions of the present invention by ordinary technicians in this field should all fall within the protection scope determined by the claims of the present invention.
Claims
1. A method for synthesizing acidic ammonium salt from fluorine-containing waste concentrated sulfuric acid, characterized in that: The following steps are involved: A dehydrating agent is added to the fluorine-containing waste concentrated sulfuric acid for dehydration, and then ammonium fluoride is added, and the mixture is kept warm and stirred at 90-120° C., and then ferric sulfate is added, and the mixture is stirred and reacted at 90-120° C. to obtain the acidic ammonium salt.
2. The method according to claim 1, characterized in that The fluorine content in the fluorine-containing waste concentrated sulfuric acid is 1.8-100 g / L.
3. The method according to claim 1, characterized in that The dehydrating agent is anhydrous sodium sulfate.
4. The method according to claim 1, characterized in that: The mass volume ratio of the ammonium fluoride, ferric sulfate and fluorine-containing waste concentrated sulfuric acid is 400-500kg:25-30kg:200L.
5. The method according to claim 1, characterized in that The fluorine-containing waste concentrated sulfuric acid is a by-product of producing boron trifluoride.
6. The method according to claim 1, characterized in that The time of the heat preservation and stirring is 15-20 minutes; the time of the stirring reaction is 5-10 minutes.
7. The acidic ammonium salt prepared by the preparation method according to any one of claims 1 to 6.
8. Use of the acidic ammonium salt as claimed in claim 7 as an oil and water well plugging remover.
9. An oil and water well plugging remover, characterized in that: Containing the acid ammonium salt according to claim 7.
Citation Information
Patent Citations
Method for realizing continuous production of ammonium hydrogen fluoride
CN103435069A
Low-leak-off high-corrosion acidification unblocking liquid used in oil-water well and preparation method of low-leak-off high-corrosion acidification unblocking liquid
CN104232041A
Well flushing process for in-situ leaching uranium mining production well
CN111520107A
Method for preparing ammonium bifluoride from rare earth fluorine-containing waste acid in recycling manner
CN111977671A
System and method for generating ammonium bifluoride by using fluorine-containing waste acid
CN118026434A