Chopped carbon fiber composite material barrel material forming method

By using a molding method for short-cut carbon fiber and resin composite materials, the problems of high-temperature brittleness and difficulty in preparing shapes in existing thermal insulation materials have been solved, resulting in high-strength carbon fiber composite barrels with good appearance quality, suitable for mass production.

CN118993754APending Publication Date: 2024-11-22INDAF ADVANCED MATERIALS (SUZHOU) CO LTD
View PDF 3 Cites 0 Cited by

Patent Information

Application Number
CN202411070876.3
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-06
Publication Date
2024-11-22

AI Technical Summary

Technical Problem

Existing insulation materials have low operating temperatures, become brittle at high temperatures, have short service lives, and are not easy to be made into specific shapes, making it difficult to meet the requirements of high efficiency and energy saving.

Method used

Short-cut carbon fibers are combined with resin and then processed through steps such as stirring, vacuum dehydration, spraying adhesive, winding into a mold, and curing in an oven to form a carbon fiber composite barrel. The fiber length and resin ratio are controlled to ensure uniform distribution and tight bonding.

Benefits of technology

This composite material achieves high strength and good appearance quality, is suitable for barrels of different sizes, is easy to machine, and is suitable for mass production.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118993754A_ABST
    Figure CN118993754A_ABST
Patent Text Reader

Abstract

The invention provides a chopped carbon fiber composite material barrel material forming method which comprises the following steps: cutting carbon fibers or graphite fibers into chopped fibers, then putting resin powder and the chopped fibers into a stirrer, adding a solvent and a suspending agent, stirring into uniform suspension slurry, conveying the suspension slurry to a conveyor belt by using a pump, and carrying out vacuum decompression dehydration to obtain the chopped carbon fiber composite material barrel material. The preparation method comprises the following steps: preparing a wet felt, uniformly spraying a binder on the wet felt, drying to gelatinize a resin glue solution, winding the gelatinized wet felt on a cylindrical mold, controlling the tension of the cylindrical mold to be within a certain range, and pressing the cylindrical mold in an outer mold; and then putting into a drying oven for curing, and then carbonizing and graphitizing to form the barrel material. The fiber and the resin are uniformly distributed, the interlayer combination is tight, the fiber length is adjustable, the size of a formed body can be accurately controlled, the machining operation is simple, and the method is suitable for preparing barrel materials with different sizes.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the technical field of heat insulation material preparation, and specifically relates to a method for forming a barrel material of chopped carbon fiber composite material. Background Art

[0002] As the level of human industrialization continues to improve, the crisis of energy shortage and even depletion has gradually emerged. In order to more effectively solve the problem of energy consumption, it has become particularly urgent to develop and apply energy-saving technologies. Therefore, the development and use of environmentally friendly thermal insulation materials will be the direction of future development. Carbon fiber-based composite insulation products have a series of advantages such as high strength, high modulus, low density, good dimensional stability, small thermal expansion coefficient, ablation resistance, and good oxidation resistance, and have become a hot topic for researchers at home and abroad. Most of the thermal insulation materials currently used are felt-type thermal insulation materials, which have the disadvantages of low operating temperature, becoming brittle at high temperatures, short service life, and being difficult to be made into a specific shape. Short-cut carbon fibers have good interface properties with the matrix resin, have very good fluidity in the resin, and are evenly dispersed, so that the composite material has high mechanical strength and good appearance quality. Therefore, by using short-cut carbon fibers and resin composites, materials with specific shapes can be prepared through a molding process, thereby obtaining excellent performance. Therefore, technicians in this field are committed to developing a method for molding short-cut carbon fiber composite barrel materials to expand the technology for preparing thermal insulation materials with specific shapes. Summary of the invention

[0003] Technical problems to be solved: In view of the above technical problems, the purpose of the present invention is to provide a method for forming a short-cut carbon fiber composite barrel material, which includes the following steps: cutting carbon fiber or graphite fiber into short-cut fibers, then putting resin powder and short-cut fibers into a blender, adding solvent and suspending agent, stirring into a uniform suspension slurry, pumping to a conveyor belt, dehydrating by vacuum decompression to form a wet felt, spraying a binder evenly on it, and gelling the resin glue after drying, winding the gelled wet felt on a cylindrical mold, controlling it within a certain tension, and then placing it in an external mold for pressing; then putting it in an oven for curing, and then carbonizing and graphitizing it to form a barrel material. The fiber and resin of the present invention are evenly distributed, the interlayer bonding is tight, the fiber length is adjustable, the size of the molded body can be accurately controlled, the machining operation is simple, and it is suitable for preparing barrel materials of different sizes.

[0004] Technical solution: A method for forming a chopped carbon fiber composite barrel material, comprising the following steps: Step 1: Cut carbon fiber or graphite fiber into chopped fibers; Step 2: Mix 100-300 parts of resin powder and 50-100 parts of chopped fibers, add 500-1000 parts of solvent and 0-50 parts of suspending agent, stir evenly, and prepare a suspension slurry; Step 3: Use a pump to transport the slurry to a conveyor belt, and dehydrate it under vacuum pressure at a vacuum degree of -0.05 to -0.1 MPa to form a wet felt; Step 4: spray the adhesive evenly on the wet felt, dry it, and gel the resin glue to obtain a gelled wet felt; Step 5: Winding the gelled wet felt on a cylindrical mold, and then placing an outer mold for pressing to obtain pressed wet felt; Step 6: Put the pressed wet felt into an oven for curing, carbonization, and graphitization to form a barrel material. Furthermore, in step 1, the length of the chopped fibers is 6 to 25 mm. Furthermore, the resin powder in step 2 is one or more of phenolic modified epoxy resin powder, condensed polynuclear aromatic resin powder, furfural resin powder, phenolic resin powder, and boron phenolic resin powder. Furthermore, in step 2, the solvent is one or more of water and a mixture of water and ethanol; and the suspending agent is one or more of methyl cellulose, hydroxypropyl methyl cellulose, carboxymethyl cellulose, and polyvinyl alcohol. Furthermore, in step 2, the stirring speed is 1000 to 5000 rpm. Furthermore, the binder in step 4 is one or more of furfural resin binder, phenolic resin binder, polyimide binder, urea-formaldehyde resin binder and acrylic resin binder. Furthermore, the thickness of the gelled wet felt in step 4 is 1.5 to 6.5 mm. Furthermore, the outer mold pressing in step 5 is specifically as follows: the wet felt is wrapped by splicing a plurality of small mold pieces together, and then tied tightly with elastic ropes, and then pressed into shape by a pressing roller. Furthermore, in step 6, the oven temperature is 80-150°C. Beneficial effects: 1. The present invention cuts carbon fiber or graphite fiber into short fibers, and the fiber length is adjustable, so the size of the molded body can be accurately controlled to prepare barrel materials of different sizes, thus broadening the scope of application; 2. The present invention mixes chopped fibers and resin powder to prepare a composite material. The chopped fibers and the matrix resin have good interface properties, and the chopped fibers have very good fluidity in the resin, can be evenly dispersed in the resin matrix, and the density is controllable; the appropriate amount of resin content will also affect the quality of the barrel material. Too much resin will cause the weight of the barrel material to increase and the performance to decrease, while too little resin will affect the strength and toughness of the barrel material. Therefore, the chopped fibers and the resin powder are mixed within a reasonable range. The prepared composite material has high mechanical properties and good appearance quality. The material with a specific shape can be prepared through a molding process, thereby obtaining excellent performance; 3. The present invention winds the gelled wet felt on a cylindrical mold and then places an outer mold for pressing, so that the layers are tightly bonded and the molding is fast. At the same time, it also avoids the occurrence of uneven component distribution caused by directly pouring the slurry into the molding mold; 4. The machining operation of the present invention is simple and convenient, and the forming is rapid, and the high-efficiency and high-quality batch production of barrel materials can be realized. BRIEF DESCRIPTION OF THE DRAWINGS Figure 1 This is a process flow chart of carbon fiber composite barrel molding; Figure 2 is the effect of suspending agent on fiber dispersion uniformity, where a means adding suspending agent and b means not adding suspending agent. DETAILED DESCRIPTION The present invention is further described below in conjunction with the accompanying drawings and embodiments. The following embodiments are explanations of the present invention and the present invention is not limited to the following embodiments: Example 1 A method for forming a chopped carbon fiber composite barrel material comprises the following steps: Step 1: Cut carbon fiber or graphite fiber into 10 mm chopped fibers; Step 2: Put 100 parts of phenolic resin powder and 50 parts of chopped fibers into a blender, add 1000 parts of water and 50 parts of hydroxypropyl methylcellulose suspending agent, and stir at a speed of 3000 rpm to prepare a uniform suspension slurry; Step 3: Use a pump to transport the slurry to a fine conveyor belt, and under a vacuum degree of -0.05MPa, dehydrate it through vacuum decompression to form wet felt; Step 4: Evenly spray phenolic resin binder on it, and after drying, gel the resin glue liquid, and the thickness of the gelled wet felt is 3mm; Step 5: Wrap the gelled wet felt around a cylindrical mold, control it within a certain tension, and then place it in an outer mold for pressing; Step 6: Place it in an oven at 100°C for curing, then carbonize and graphitize to form a barrel material. Example 2 A method for forming a chopped carbon fiber composite barrel material comprises the following steps: Step 1: Cut carbon fiber or graphite fiber into 10 mm chopped fibers; Step 2: Put 100 parts of phenolic modified epoxy resin powder and 50 parts of chopped fibers into a blender, add 1000 parts of water and 50 parts of hydroxypropyl methylcellulose suspending agent, and stir at a speed of 3000 rpm to prepare a uniform suspension slurry; Step 3: Use a pump to transport the slurry to a fine conveyor belt, and under a vacuum degree of -0.05MPa, dehydrate it through vacuum decompression to form wet felt; Step 4: Evenly spray phenolic resin binder on it, and after drying, gel the resin glue liquid, and the thickness of the gelled wet felt is 3mm; Step 5: Wrap the gelled wet felt around a cylindrical mold, control it within a certain tension, and then place it in an outer mold for pressing; Step 6: Place it in an oven at 100°C for curing, then carbonize and graphitize to form a barrel material. Example 3 A method for forming a chopped carbon fiber composite barrel material comprises the following steps: Step 1: Cut carbon fiber or graphite fiber into 10 mm chopped fibers; Step 2: Put 100 parts of condensed polynuclear aromatic resin powder and 50 parts of chopped fibers into a blender, add 1000 parts of water and 50 parts of hydroxypropyl methylcellulose suspending agent, and stir at a speed of 3000 rpm to prepare a uniform suspension slurry; Step 3: Use a pump to transport the slurry to a fine conveyor belt, and under a vacuum degree of -0.05MPa, dehydrate it through vacuum decompression to form wet felt; Step 4: Evenly spray phenolic resin binder on it, and after drying, gel the resin glue liquid, and the thickness of the gelled wet felt is 3mm; Step 5: Wrap the gelled wet felt around a cylindrical mold, control it within a certain tension, and then place it in an outer mold for pressing; Step 6: Place it in an oven at 100°C for curing, then carbonize and graphitize to form a barrel material. Example 4 A method for forming a chopped carbon fiber composite barrel material comprises the following steps: Step 1: Cut carbon fiber or graphite fiber into 10 mm chopped fibers; Step 2: Put 100 parts of furfural resin powder and 50 parts of chopped fibers into a blender, add 1000 parts of water and 50 parts of hydroxypropyl methylcellulose suspending agent, and stir at a speed of 3000 rpm to prepare a uniform suspension slurry; Step 3: Use a pump to transport the slurry to a fine conveyor belt, and under a vacuum degree of -0.05MPa, dehydrate it through vacuum decompression to form wet felt; Step 4: Evenly spray phenolic resin binder on it, and after drying, gel the resin glue liquid, and the thickness of the gelled wet felt is 3mm; Step 5: Wrap the gelled wet felt around a cylindrical mold, control it within a certain tension, and then place it in an outer mold for pressing; Step 6: Place it in an oven at 100°C for curing, then carbonize and graphitize to form a barrel material. Example 5 A method for forming a chopped carbon fiber composite barrel material comprises the following steps: Step 1: Cut carbon fiber or graphite fiber into 10 mm chopped fibers; Step 2: Put 100 parts of boron phenolic resin powder and 50 parts of chopped fibers into a blender, add 1000 parts of water and 50 parts of hydroxypropyl methylcellulose suspending agent, and stir at a speed of 3000 rpm to prepare a uniform suspension slurry; Step 3: Use a pump to transport the slurry to a fine conveyor belt, and under a vacuum degree of -0.05MPa, dehydrate it through vacuum decompression to form wet felt; Step 4: Evenly spray phenolic resin binder on it, and after drying, gel the resin glue liquid, and the thickness of the gelled wet felt is 3mm; Step 5: Wrap the gelled wet felt around a cylindrical mold, control it within a certain tension, and then place it in an outer mold for pressing; Step 6: Place it in an oven at 100°C for curing, then carbonize and graphitize to form a barrel material. Example 6 A method for forming a chopped carbon fiber composite barrel material comprises the following steps: Step 1: Cut carbon fiber or graphite fiber into 6mm chopped fibers; Step 2: Put 200 parts of phenolic resin powder and 50 parts of chopped fibers into a blender, add 500 parts of water and 10 parts of hydroxypropyl methylcellulose suspending agent, and stir at a speed of 1000 rpm to prepare a uniform suspension slurry; Step 3: Use a pump to transport the slurry to a fine conveyor belt, and under a vacuum degree of -0.05MPa, dehydrate it through vacuum decompression to form wet felt; Step 4: Evenly spray phenolic resin binder on it, and after drying, gel the resin glue liquid, and the thickness of the gelled wet felt is 1.5mm; Step 5: Wrap the gelled wet felt around a cylindrical mold, control it within a certain tension, and then place it in an outer mold for pressing; Step 6: Place it in an oven at 80°C for curing, then carbonize and graphitize to form a barrel material. Example 7 A method for forming a chopped carbon fiber composite barrel material comprises the following steps: Step 1: Cut carbon fiber or graphite fiber into 15 mm chopped fibers; Step 2: Put 250 parts of phenolic resin powder and 80 parts of chopped fibers into a blender, add 600 parts of water and 20 parts of hydroxypropyl methylcellulose suspending agent, and stir at a speed of 2000 rpm to prepare a uniform suspension slurry; Step 3: Use a pump to transport the slurry to a fine conveyor belt, and under the condition of a vacuum degree of -0.05MPa, it is dehydrated by vacuum decompression to form a wet felt; Step 4: Evenly spray phenolic resin binder on it, and after drying, gel the resin glue liquid, and the thickness of the gelled wet felt is 5mm; Step 5: Wrap the gelled wet felt around a cylindrical mold, control it within a certain tension, and then place it in an outer mold for pressing; Step 6: Place it in an oven at 100°C for curing, then carbonize and graphitize to form a barrel material. Example 8 A method for forming a chopped carbon fiber composite barrel material comprises the following steps: Step 1: Cut carbon fiber or graphite fiber into 25mm chopped fibers; Step 2: Put 300 parts of phenolic resin powder and 100 parts of chopped fibers into a blender, add 800 parts of water and 40 parts of hydroxypropyl methylcellulose suspending agent, and stir at a speed of 5000 rpm to prepare a uniform suspension slurry; Step 3: Use a pump to transport the slurry to a fine conveyor belt, and under the condition of a vacuum degree of -0.05MPa, it is dehydrated by vacuum decompression to form a wet felt; Step 4: Evenly spray phenolic resin binder on it, and then dry it to gel the resin glue. The thickness of the gelled wet felt is 6.5mm; Step 5: Wrap the gelled wet felt around a cylindrical mold, control it within a certain tension, and then place it in an outer mold for pressing; Step 6: Place it in an oven at 150°C for curing, then carbonize and graphitize to form a barrel material. Comparative Example 1 The difference between this comparative example and Example 1 is that the barrel material is prepared directly by pouring, as follows: A method for forming a chopped carbon fiber composite barrel material comprises the following steps: Step 1: Cut carbon fiber or graphite fiber into 10 mm chopped fibers; Step 2: Put 100 parts of phenolic resin powder and 50 parts of chopped fibers into a blender, add 1000 parts of water and 50 parts of hydroxypropyl methylcellulose suspending agent, and stir at a speed of 3000 rpm to prepare a uniform suspension slurry; Step 3: Add phenolic resin binder to the slurry and mix evenly to obtain a mixed material; Step 4: Pour the mixture into the mold, put it into an oven at 100°C for curing, and then carbonize and graphitize it to form a barrel material. Comparative Example 2 The difference between this comparative example and Example 1 is that the length of the chopped fibers is 4 mm, as follows: A method for forming a chopped carbon fiber composite barrel material comprises the following steps: Step 1: Cut carbon fiber or graphite fiber into 4 mm chopped fibers; Step 2: Put 100 parts of phenolic resin powder and 50 parts of chopped fibers into a blender, add 1000 parts of water and 50 parts of hydroxypropyl methylcellulose suspending agent, and stir at a speed of 3000 rpm to prepare a uniform suspension slurry; Step 3: Use a pump to transport the slurry to a fine conveyor belt, and under a vacuum degree of -0.05MPa, dehydrate it through vacuum decompression to form wet felt; Step 4: Evenly spray phenolic resin binder on it, and after drying, gel the resin glue liquid, and the thickness of the gelled wet felt is 3mm; Step 5: Wrap the gelled wet felt around a cylindrical mold, control it within a certain tension, and then place it in an outer mold for pressing; Step 6: Place it in an oven at 100°C for curing, then carbonize and graphitize to form a barrel material. Comparative Example 3 The difference between this comparative example and Example 1 is that the length of the short-cut fibers is 30 mm, as follows: A method for forming a chopped carbon fiber composite barrel material comprises the following steps: Step 1: Cut carbon fiber or graphite fiber into 30mm chopped fibers; Step 2: Put 100 parts of phenolic resin powder and 50 parts of chopped fibers into a blender, add 1000 parts of water and 50 parts of hydroxypropyl methylcellulose suspending agent, and stir at a speed of 3000 rpm to prepare a uniform suspension slurry; Step 3: Use a pump to transport the slurry to a fine conveyor belt, and under the condition of a vacuum degree of -0.05MPa, it is dehydrated by vacuum decompression to form a wet felt; Step 4: Evenly spray phenolic resin binder on it, and after drying, gel the resin glue liquid, and the thickness of the gelled wet felt is 3mm; Step 5: Wrap the gelled wet felt around a cylindrical mold, control it within a certain tension, and then place it in an outer mold for pressing; Step 6: Place it in an oven at 100°C for curing, then carbonize and graphitize to form a barrel material. Comparative Example 4 The difference between this comparative example and Example 1 is that a smaller amount of resin powder is used, as follows: A method for forming a chopped carbon fiber composite barrel material comprises the following steps: Step 1: Cut carbon fiber or graphite fiber into 10 mm chopped fibers; Step 2: Put 80 parts of phenolic resin powder and 50 parts of chopped fibers into a blender, add 1000 parts of water and 50 parts of hydroxypropyl methylcellulose suspending agent, and stir at a speed of 3000 rpm to prepare a uniform suspension slurry; Step 3: Use a pump to transport the slurry to a fine conveyor belt, and under the condition of a vacuum degree of -0.05MPa, it is dehydrated by vacuum decompression to form a wet felt; Step 4: Evenly spray phenolic resin binder on it, and after drying, gel the resin glue liquid, and the thickness of the gelled wet felt is 3mm; Step 5: Wrap the gelled wet felt around a cylindrical mold, control it within a certain tension, and then place it in an outer mold for pressing; Step 6: Place it in an oven at 100°C for curing, then carbonize and graphitize to form a barrel material. Comparative Example 5 The difference between this comparative example and Example 1 is that a larger amount of resin powder is used, as follows: A method for forming a chopped carbon fiber composite barrel material comprises the following steps: Step 1: Cut carbon fiber or graphite fiber into 10 mm chopped fibers; Step 2: 350 parts of phenolic resin powder and 50 parts of chopped fibers were placed in a blender, and 1000 parts of water and 50 parts of hydroxypropyl methylcellulose suspension agent were added, and the mixture was stirred at a speed of 3000 rpm to prepare a uniform suspension slurry; Step 3: Use a pump to transport the slurry to a fine conveyor belt, and under the condition of a vacuum degree of -0.05MPa, it is dehydrated by vacuum decompression to form a wet felt; Step 4: Evenly spray phenolic resin binder on it, and after drying, gel the resin glue liquid, and the thickness of the gelled wet felt is 3mm; Step 5: Wrap the gelled wet felt around a cylindrical mold, control it within a certain tension, and then place it in an outer mold for pressing; Step 6: Place it in an oven at 100°C for curing, then carbonize and graphitize to form a barrel material. Performance Testing: (1) Fiber dispersion uniformity Mix the resin powder and chopped fibers, add the solvent and suspending agent, stir evenly to make a suspension slurry. Take a certain volume of slurry and slowly pour it into a transparent beaker, and use a digital camera to record the actual dispersion. Observe the dispersion of the fiber in the resin liquid through the picture to evaluate the uniformity and dispersion of the fiber. like Figure 2 As shown, by observing the slurry picture, it can be seen that the chopped fibers are evenly dispersed in the resin matrix with the suspending agent added. This is because the chopped fibers and the matrix resin have good interface properties, and the chopped fibers have very good fluidity in the resin and can be evenly dispersed in the resin matrix. (2) Mechanical properties The compression performance and bending performance of the samples prepared in Examples 1 to 8 of the present invention and Comparative Examples 1 to 5 are tested below. The specific sample performance testing method is: the compression performance of the sample is tested according to the standard test method of ASTM D3410; the bending performance of the sample is tested with reference to ISO 14125. The test results are shown in Table 1 below. Table 1 Compressive strength and bending strength of barrel materials prepared in various embodiments and comparative examples sample Compressive strength(MPa) Bending strength(MPa) Example 1 0.8 0.7 Example 2 0.7 0.7 Example 3 0.8 0.6 Example 4 0.7 0.5 Example 5 0.7 0.6 Example 6 0.7 0.6 Example 7 0.8 0.5 Example 8 0.7 0.6 Comparative Example 1 0.6 0.5 Comparative Example 2 0.9 0.7 Comparative Example 3 0.3 0.4 Comparative Example 4 0.6 0.5 Comparative Example 5 1.1 0.9 It can be seen from the data shown in Table 1 that the composite barrel material prepared by the preparation method of the present invention has excellent mechanical properties. Compared with Example 1, the molding method, the length of the short-cut fiber and the amount of resin added of the composite materials of Comparative Examples 1, 2, 3, 4 and 5 will affect their mechanical properties. The above is only a preferred embodiment of the present invention and does not limit the present invention in any form. Any technician familiar with the art can make many possible changes and modifications to the technical solution of the present invention by using the above disclosed methods and technical contents without departing from the spirit and technical solution of the present invention, or modify it into an equivalent embodiment of equivalent changes. Therefore, any simple modification, equivalent replacement, equivalent change and modification made to the above embodiments according to the technical essence of the present invention without departing from the content of the technical solution of the present invention still falls within the scope of protection of the technical solution of the present invention.

Claims

1. A method for forming a barrel material of chopped carbon fiber composite material, characterized in that: The following steps are involved: Step 1: Cut carbon fiber or graphite fiber into chopped fibers; Step 2: Mix 100-300 parts of resin powder and 50-100 parts of chopped fibers, add 500-1000 parts of solvent and 0-50 parts of suspending agent, stir evenly, and prepare a suspension slurry; Step 3: Use a pump to transport the slurry to a conveyor belt, and dehydrate it under vacuum pressure at a vacuum degree of -0.05 to -0.1 MPa to form a wet felt; Step 4: spray the adhesive evenly on the wet felt, dry it, and gel the resin glue to obtain a gelled wet felt; Step 5: Winding the gelled wet felt on a cylindrical mold, and then placing an outer mold for pressing to obtain pressed wet felt; Step 6: Put the pressed wet felt into an oven for curing, carbonization, and graphitization to form a barrel material.

2. The method for forming a chopped carbon fiber composite barrel material according to claim 1, characterized in that: The length of the chopped fibers in step 1 is 6 to 25 mm.

3. The method for forming a chopped carbon fiber composite barrel material according to claim 1, characterized in that: The resin powder in step 2 is one or more of phenolic modified epoxy resin powder, condensed polynuclear aromatic resin powder, furfural resin powder, phenolic resin powder, and boron phenolic resin powder.

4. The method for forming a chopped carbon fiber composite barrel material according to claim 1, characterized in that: In step 2, the solvent is one or more of water and a mixture of water and ethanol; the suspending agent is one or more of methyl cellulose, hydroxypropyl methyl cellulose, carboxymethyl cellulose, and polyvinyl alcohol.

5. The method for forming a chopped carbon fiber composite barrel material according to claim 1, characterized in that: The stirring speed in step 2 is 1000-5000 rpm.

6. The method for forming a chopped carbon fiber composite barrel material according to claim 1, characterized in that: In step 4, the binder is one or more of furfural resin binder, phenolic resin binder, polyimide binder, urea-formaldehyde resin binder and acrylic resin binder.

7. The method for forming a chopped carbon fiber composite barrel material according to claim 1, characterized in that: The thickness of the gelled wet felt in step 4 is 1.5 to 6.5 mm.

8. The method for forming a chopped carbon fiber composite barrel material according to claim 1, characterized in that: The outer mold pressing in step 5 is specifically as follows: the wet felt is wrapped by splicing a plurality of small mold pieces together, and then tied tightly with elastic ropes, and then pressed into shape by a pressing roller.

9. The method for forming a chopped carbon fiber composite barrel material according to claim 1, characterized in that: The oven temperature in step 6 is 80-150°C.

Citation Information

Patent Citations

  • Pitch-based carbon fiber non-woven felt heat-insulating cylinder and preparation method thereof

    CN104261853A

  • Basalt fiber surfacing mat and preparation method thereof

    CN107268179A

  • Carbon fiber drum composite material and preparation method thereof

    CN116041081A