Substrate manufacturing method and metasurface lens
By forming grooves and dielectric layers with larger line widths on the substrate, and removing parts to form protrusions with smaller line widths, the problem that the substrate cannot prepare a small line width structure in the prior art is solved, and a metasurface lens is realized High precision and mass production adaptability in the field.
Patent Information
- Application Number
- CN202310567147.8
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2023-05-19
- Publication Date
- 2024-11-22
AI Technical Summary
The prior art cannot effectively prepare substrates with smaller line width structures, and the substrate production process is difficult to meet mass production needs, especially under the high accuracy requirements of metasurface lenses.
By forming a first groove with a larger line width on the substrate, and forming the first film layer and the second dielectric layer sequentially, the first film layer portion is removed by utilizing the filling property and etch resistance of the second dielectric layer to remove the first film layer portion to A second film layer protrusion with a smaller line width is formed, and a first substrate protrusion with a smaller line width is formed on the substrate.
It further reduces the line width based on the existing technology, is suitable for mass production of devices, and improves the fineness and complexity of the substrate, and supports higher computing and control scenarios.
Smart Images

Figure CN119001934A_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the field of optoelectronic technology, and in particular to a substrate manufacturing method and a super-surface lens. Background Art
[0002] Nowadays, in order to expand the functions of optical devices or semiconductor devices, lithography technology is usually used to transfer ideal patterns on the substrate, so as to further prepare optical devices or semiconductor devices using the substrate containing the ideal pattern. With the increasing demand for the computing power and efficiency of optical devices or semiconductor devices, it is urgent to reduce the line width of the structure on the substrate to meet the needs of improving the computing power of metasurface lenses.
[0003] In the prior art, a photolithography machine is usually used to form a pattern on a substrate, but the minimum line width that can be achieved by the photolithography machine is above 150nm, which is difficult to meet the requirements of preparing high-precision optical devices or semiconductor devices including metasurface lenses. Some prior arts simply adjust the photoresist material to achieve exposure and development of smaller line width structures, but this brings with it an increase in the cost of special photoresists and process limitations that prevent batch transfer of patterns, making it difficult to apply to mass production of devices. Summary of the invention
[0004] One of the purposes of the present invention is to provide a substrate manufacturing method to solve the technical problems that the prior art cannot prepare a substrate with a smaller line width structure and the substrate manufacturing process cannot be adapted to mass production.
[0005] One of the objects of the present invention is to provide a metasurface lens.
[0006] To achieve one of the above-mentioned purposes of the invention, an embodiment of the present invention provides a substrate manufacturing method, comprising: providing a substrate; forming a first groove having a first width on the substrate; forming a first film layer and a second dielectric layer in sequence at least at the first groove; wherein the portion of the first film layer in the first groove is retracted inwardly to form a second groove, and the second dielectric layer forms a second dielectric body having a second width in the second groove; the second width is smaller than the first width; removing the first film layer portion located on both sides of the second dielectric body to obtain a first film layer protrusion; wherein the first film layer protrusion has the second width; forming a first substrate protrusion at the substrate along the first film layer protrusion; wherein the first substrate protrusion has the second width.
[0007] As a further improvement of an embodiment of the present invention, the "forming a first groove having a first width on the substrate" specifically includes: forming a first dielectric layer on the substrate; and photolithographically forming an epitaxial structure matching a preset pattern and including the first groove at the first dielectric layer.
[0008] As a further improvement of an embodiment of the present invention, the material of the first dielectric layer is different from the material of the second dielectric layer; the first dielectric layer includes ultraviolet photoresist and has high resolution.
[0009] As a further improvement of an embodiment of the present invention, the "forming a first film layer and a second dielectric layer in sequence at least at the first groove" specifically includes: forming the first film layer on the side of the first groove away from the substrate; wherein the first groove is formed at the first dielectric layer on the substrate; and forming the second dielectric layer on the side of the first film layer away from the first dielectric layer.
[0010] As a further improvement of one embodiment of the present invention, the "forming the first film layer" specifically includes: using an atomic layer deposition method to uniformly cover the bottom and side walls of the first groove with a first film layer; wherein the first film layer is configured as a metal mask material; the "forming the second dielectric layer" specifically includes forming the second dielectric layer by a spin coating method; wherein the material of the second dielectric layer is different from that of the first dielectric layer; the second dielectric layer is configured as a photoresist mask material and has good filling and etching resistance.
[0011] As a further improvement of an embodiment of the present invention, after "forming the second dielectric layer on the side of the first film layer away from the first dielectric layer", the method further includes: etching and removing the portion of the second dielectric layer located on the side of the second dielectric body away from the first film layer by oxygen plasma, and retaining at least a portion of the second dielectric body; wherein, compared with the first film layer, the retained portion of the second dielectric body is away from the surface of the side of the substrate and closer to the substrate.
[0012] As a further improvement of one embodiment of the present invention, the "removing the first film layer portion located on both sides of the second dielectric body to obtain the first film layer protrusion" specifically includes: removing at least a portion of the first film layer located on both sides of the second dielectric body, retaining at least a portion of the second groove, so that the side surface of the second dielectric body is at least partially exposed outside the retained portion of the second groove; using the second dielectric body as a mask, removing the portion of the second groove that exceeds the side surface of the second dielectric body, to obtain the first film layer protrusion.
[0013] As a further improvement of an embodiment of the present invention, the “removing at least part of the first film layer located on both sides of the second dielectric body, retaining at least part of the second groove, so that the side of the second dielectric body is at least partially exposed outside the retained part of the second groove” specifically includes: etching and removing the parts of the first film layer located on both sides of the second dielectric body and located on the side of the first groove away from the substrate, retaining at least part of the second groove, so that the side of the second dielectric body is at least partially exposed outside the retained part of the second groove; wherein, the first groove is formed at the first dielectric layer on the substrate, and compared with the first dielectric layer, the retained part of the second groove is away from the surface of the side of the substrate and is closer to the substrate; the “using the second dielectric body as a mask to remove the part of the second groove that exceeds the side of the second dielectric body to obtain the first film layer protrusion” specifically includes: using the second dielectric body and the first dielectric layer as masks at the same time, and etching and removing the first film layer part of the second groove located at the gap between the two by inductively coupled plasma, to obtain the first film layer protrusion located on the side of the second dielectric body close to the substrate.
[0014] As a further improvement of an embodiment of the present invention, the first groove is formed at the first dielectric layer on the substrate; the "forming a first substrate protrusion at the substrate along the first film layer protrusion" specifically includes: removing the first dielectric layer and the second dielectric body; wherein the first dielectric layer and the second dielectric body are photoresist; using the first film layer protrusion as a mask, etching the substrate to form the first substrate protrusion; removing the first film layer protrusion.
[0015] To achieve one of the above-mentioned purposes of the invention, one embodiment of the present invention provides a metasurface lens, comprising a substrate; the substrate is prepared by the substrate manufacturing method described in any one of the above-mentioned technical solutions.
[0016] Compared with the prior art, the substrate manufacturing method provided by the present invention uses the first groove with a larger line width on the substrate as a "negative mold" to form a second dielectric body and a second film layer protrusion corresponding to the first groove and having a smaller line width, so as to achieve the effect of processing the first substrate protrusion on the substrate corresponding to the second film layer protrusion. Since the first substrate protrusion corresponds to the second film layer protrusion, it has the same smaller line width. In this way, on the basis of the existing groove forming technology, a structure with a smaller line width can be further formed on the substrate, and the demand for materials is weakened, which can be suitable for mass production of devices. BRIEF DESCRIPTION OF THE DRAWINGS
[0017] Figure 1 1 is a flow chart of the steps of a method for manufacturing a substrate in one embodiment of the present invention.
[0018] Figure 21 is a flowchart of the steps of a first embodiment of a method for manufacturing a substrate in one embodiment of the present invention.
[0019] Figure 3 1 is a flow chart of the steps of a second embodiment of a method for manufacturing a substrate in one embodiment of the present invention.
[0020] Figure 4 1 is a flowchart of a third embodiment of a method for manufacturing a substrate according to an embodiment of the present invention.
[0021] Figure 5 1 is a flow chart of the steps of a fourth embodiment of a method for manufacturing a substrate in one embodiment of the present invention.
[0022] Figures 6 to 16 It is a structural schematic diagram of a substrate manufacturing method implemented in one embodiment of the present invention. DETAILED DESCRIPTION
[0023] The present invention will be described in detail below in conjunction with the specific embodiments shown in the accompanying drawings. However, these embodiments do not limit the present invention, and any structural, methodological, or functional changes made by a person skilled in the art based on these embodiments are all within the scope of protection of the present invention.
[0024] It should be noted that the term "comprises" or any other variation thereof is intended to cover non-exclusive inclusion, so that a process, method, article or device that includes a series of elements includes not only those elements, but also includes other elements not explicitly listed, or also includes elements inherent to such process, method, article or device. In addition, the terms "first", "second", "third", "fourth", etc. are used for descriptive purposes only and cannot be understood as indicating or implying relative importance.
[0025] One embodiment of the present invention provides a metasurface lens. As a nano-optical device, a metasurface lens (Metalens) has the ability to replace traditional lenses. Generally, a metasurface lens includes a metasurface layer, on which a two-dimensional array structure is arranged to control the propagation and focusing of light and realize optical imaging and other functions. The metasurface lens provided by the present invention includes a substrate prepared by implementing a substrate manufacturing method. On the one hand, the substrate can be used to prepare the metasurface layer, and the pattern formed on the substrate by the substrate protrusions can be used to constitute a two-dimensional array structure or other structure of the metasurface layer. On the other hand, the substrate can be prepared by the substrate manufacturing method described in any of the technical solutions provided below.
[0026] Metasurface lenses can be used to focus incident light or change its propagation direction. The above functions can be achieved by adjusting the two-dimensional array structure on the metasurface layer, etc., by controlling the phase and amplitude of light, thereby achieving efficient manipulation of light. Metasurface lenses can be used in imaging, optical communications, laser focusing, optical sensors, and optical computers. In one embodiment, the metasurface lens provided by the present invention can be used to construct a neural network based on its ability to form a pattern with a smaller line width on the metasurface layer, and the computing speed is faster than that of a traditional electronic neural network.
[0027] The metasurface layer is composed of a series of tiny nanostructures, which can be called primitives. The primitives can be formed by forming substrate protrusions on the substrate. The metasurface lens provided by the present invention, based on the included substrate prepared by the substrate manufacturing method provided below, can achieve a line width configuration as low as about 80nm, and even a line width configuration of about 50nm, and can generate more complex patterns in a limited area to support more precise and complex calculations or control scenarios.
[0028] One embodiment of the present invention provides a substrate manufacturing method, which can be implemented in any of the above-mentioned processes for preparing the metasurface lens, metasurface layer, or the substrate contained therein. Figure 1 In this embodiment, the substrate manufacturing method includes the following steps.
[0029] Step S1, providing a substrate.
[0030] The substrate has at least one bearing surface, which can be used to attach other material layers to achieve corresponding functions, or based on the bearing surface, one side of the substrate can be etched to prepare corresponding devices using the substrate itself. Figures 7 to 14 In the structure shown, the integrity of the substrate 100 itself is maintained and a plurality of hierarchical structures are arranged on a certain bearing surface thereof, so that a functional unit can be prepared; in a specific example, an integrated circuit chip can be formed by arranging metal wiring on the bearing surface. For another example, Figure 15 to Figure 16 In the structure shown, by etching or other operations on the substrate 100, structures such as the first substrate protrusion 11 can be formed, which can be used to form primitives on the super surface layer and participate in the process of adjusting the light and its propagation path. The smaller the volume of the structure formed on the substrate bearing surface, the more and more complex the functions it usually supports, and the higher the integration.
[0031] The substrate is not limited to having only one bearing surface. When the substrate is configured as a sheet, the two oppositely arranged extensions thereof can both serve as the bearing surfaces of the substrate.
[0032] The materials used to prepare the substrate include, but are not limited to, polymers and oxides. Specifically, it can be a silicon-based material, such as amorphous silicon, silicon nitride, etc. When the substrate manufacturing method provided by the present invention is applied to the preparation process of the metasurface lens, the substrate can specifically be titanium dioxide.
[0033] Step S2, forming a first groove having a first width on the substrate.
[0034] On the one hand, the first groove can be formed by photolithography, dry etching or wet etching.
[0035] On the other hand, the term "formed on a substrate" includes forming on the substrate and forming on a certain hierarchical structure on the substrate. The former means etching a certain bearing surface of the substrate toward one side of the substrate to form the first groove in the substrate; the latter means coating a certain hierarchical structure on a certain bearing surface of the substrate and forming the first groove in the hierarchical structure. Figures 6 to 8 The latter may specifically be coating a glue layer on the supporting surface relatively above the substrate 100 and forming a first groove 21 on the glue layer.
[0036] The first groove may be in the shape of a blind hole or a channel, with an opening facing away from the substrate. The first width may be the width of the first groove in the extending direction of the groove bottom, and preferably, the first width may be the narrowest width of the first groove.
[0037] In one embodiment, the first width may be the minimum width that can be formed on a conventional material using conventional means such as a photolithography machine. In this embodiment, since the substrate formed by the substrate manufacturing method provided by the present invention can produce a first substrate protrusion with a line width smaller than the first width, its superior performance relative to conventional means is more prominent.
[0038] Step S3, forming a first film layer and a second dielectric layer in sequence at least at the first groove.
[0039] The material of the first film layer can be different from that of the second dielectric layer to prevent mutual interference and removal of parts that should not be removed when the substrate and the packaging structure composed of the hierarchical structures thereon are processed as a whole. Preferably, the material of the first film layer can be a metal material, and the second dielectric layer can be an insulating material; therefore, the two will not react with each other, and the properties presented in response to different patterning processes and etching processes are different. In one embodiment, the material of the first film layer is chromium, which has good stripping properties; in one embodiment, the second dielectric layer is photoresist.
[0040] The portion of the first film layer in the first groove is indented inward to form a second groove, and the second dielectric layer forms a second dielectric body with a second width in the second groove; the second width is smaller than the first width.
[0041] Combination Figures 8 to 10 As shown, the first film layer 300 is at least arranged in the first groove 21. Since the first film layer 300 has a thickness, when the first film layer 300 is arranged on the side wall of the first groove 21 or the groove bottom close to the substrate 100, it will enclose a space smaller than the first groove 21 due to its own thickness, and the structure enclosing the space can be defined as the second groove 31; it can be understood that the second groove 31 is composed of the first film layer 300, especially the part of the first film layer 300 located at the first groove 21.
[0042] On the one hand, the “inward retraction” at least includes retraction along the width direction of the bottom of the first groove 21, so that when the second dielectric layer 400 forms the second dielectric body 41 in the second groove 31, the second dielectric body 41 can have a second width b that is smaller than the first width a. In one embodiment, the first film layer 300 can be arranged at least on the side wall of the first groove 21.
[0043] On the other hand, the first film layer 300 is not limited to being disposed only in the first groove 21. During actual preparation, the first groove 21 (or the structure used to form the first groove 21 together with the substrate 100, such as the first dielectric layer 200 described below) and the substrate 100 together constitute a package body, and the first film layer 300 can be arranged as a whole on the surface of the package body located on the side of the first groove 21 away from the substrate 100.
[0044] Similarly, the second dielectric layer 400 may only fill the space surrounded by the second groove 31, such as Fig.11 The second dielectric layer 400 may also be disposed on the surface of the package body formed by the first groove 21, the substrate 100 and the first film layer 300, for example, it may be arranged as a whole on the surface of the package body located on the side of the second groove 31 away from the substrate 100.
[0045] When the second dielectric layer 400 is at least partially and uniformly filled in the second groove 31 and can cover the groove bottom of the second groove 31 along the width direction, the portion of the second dielectric layer 400 located in the second groove 31 can be the second dielectric body 41. In this embodiment, the second dielectric body 41 and the second groove 31 both have a second width b, and the extension direction of the second dielectric body 41 is consistent with the extension direction of the second groove 31. Of course, the present invention is not limited to this embodiment, and technical solutions that can prepare a second dielectric body 41 with a width smaller than the first groove 21 in the second groove 31 are all within the protection scope of the present invention.
[0046] It can be understood that the second dielectric body 41 is formed by the second dielectric layer 400 , so the material of the second dielectric body 41 can be the same as that of the second dielectric layer 400 ; in one embodiment, it can be photoresist.
[0047] Step S4, removing the first film layer portion located on both sides of the second dielectric body to obtain a first film layer protrusion.
[0048] Wherein, the first film layer protrusion has the second width.
[0049] like Figures 10 to 13 , a portion of the first film layer 300 located in a direction away from the second dielectric body 41 can be removed along at least one of the two side surfaces spaced apart along the width direction of the second dielectric body 41, thereby "cutting" the second groove 31 (or, the portion of the first film layer 300 used to form the second groove 31) to form a structure with the same width as the second dielectric body 41, that is, forming the first film layer protrusion 32.
[0050] On the one hand, the "convex" of the first film layer protrusion 32 means that it protrudes toward the side away from the substrate 100 relative to the bearing surface of the substrate 100. The "obtaining the first film layer protrusion" can be interpreted as forming the first film layer protrusion 32 between the second dielectric body 41 and the substrate 100. In other words, the second dielectric body 41 can be retained after the first film layer protrusion 32 is formed by "cutting". Of course, the "obtaining the first film layer protrusion" can also be interpreted as removing other structures other than the first film layer protrusion 32 and the substrate 100 after the first film layer protrusion 32 is formed by "cutting".
[0051] On the other hand, since the first film layer 300 and the second dielectric layer 400 are formed sequentially in step S3, the first film layer protrusion 32 can be directly formed on the surface of the substrate 100, the bottom of the first groove 21, or at least closer to the substrate 100 than the second dielectric body 41. In this way, in one specific example, a pattern or wiring can be directly formed on one side of the substrate 100, and in another specific example, it can be used as a mask to more accurately implement photolithography, etching and other processes on the substrate 100, or on other structures between the substrate 100 and the first film layer protrusion 32. Regardless of the above specific examples, since the first film layer protrusion 32 has a smaller second width, it is possible to prepare a substrate that supports a smaller line width.
[0052] Step S5, forming a first substrate protrusion on the substrate along the first film layer protrusion.
[0053] Wherein, the first substrate protrusion has the second width.
[0054] In this embodiment, combined with Figures 13 to 16As shown, at least one of the two side surfaces spaced apart along the width direction of the first film layer protrusion 32 can be removed in the thickness direction of the substrate 100 from the portion of the substrate 100 that is located in the plane where the side surface is located and that is away from the first film layer protrusion 32, thereby "cutting" the substrate 100 to form a structure with the same width as the first film layer protrusion 32 (or the second dielectric body 41, or the second groove 31), that is, forming the first substrate protrusion 11.
[0055] Of course, similar to the above, when the first substrate protrusion 11 (or the first film layer protrusion 32) is used to form a pattern on the substrate 100, the above-mentioned "cutting" operation does not indicate that all parts of the substrate 100 located in the above-mentioned direction are removed; the specific extent of removal is determined by the actual pattern structure. In addition, when executing step S5, the "cutting" operation in the thickness direction of the substrate 100, in other words, when the etching process is used to implement step S5, the degree of etching in the thickness direction of the substrate 100 is determined by the thickness of the substrate 100 at this point; that is, the thickness of the first substrate protrusion 11 is less than the thickness of the substrate 100 at the corresponding position.
[0056] In this way, the substrate manufacturing method provided by the present invention can be generally applicable to various existing processes and materials, and can achieve the effect of further reducing the line width based on the existing line width; in addition, because the substrate manufacturing method provided by the present invention superimposes a hierarchical structure on the substrate and processes it sequentially, it can adapt to mass production conditions and quickly form a more precise pattern or wiring on the substrate.
[0057] like Figure 2 The present invention provides a first embodiment of a substrate manufacturing method, which includes the following steps.
[0058] Step S1, providing a substrate.
[0059] Step S21, forming a first dielectric layer on the substrate.
[0060] Step S22: photolithographically forming an epitaxial structure matching a preset pattern and including a first groove on the first dielectric layer.
[0061] Step S3, forming a first film layer and a second dielectric layer in sequence at least at the first groove.
[0062] Step S4, removing the first film layer portion located on both sides of the second dielectric body to obtain a first film layer protrusion.
[0063] Step S5, forming a first substrate protrusion on the substrate along the first film layer protrusion.
[0064] Combination Figures 6 to 8In order to maintain the original thickness of the substrate 100 before forming the first substrate protrusion 11 and prevent the process difficulty of forming the first substrate protrusion 11 from increasing and the thickness from being too small, the present invention preferably adopts a solution in which the first dielectric layer 200 and the substrate 100 jointly form the first groove 21.
[0065] In one embodiment, for step S21, a first dielectric layer 200 may be deposited or coated on a bearing surface of the first substrate 100. The first dielectric layer 200 may be a photoresist, preferably a positive photoresist with high resolution to replicate the preset pattern; in one embodiment, the first dielectric layer 200 may be an ultraviolet photoresist.
[0066] In one embodiment, for step S22, an epitaxial structure including a first groove can be formed at the first dielectric layer 200 by exposure and development. In other words, when the preset pattern is replicated at the first dielectric layer 200, at least a first groove will be formed to form an epitaxial structure. In one embodiment, the exposure and development method can be implemented by DUV (Deep Ultraviolet Lithography). Preferably, the first width a can be the minimum line width that can be achieved by DUV or other exposure and development methods to form a structure. As an additional explanation, the minimum line width supported by DUV can be about 150nm.
[0067] In one embodiment, the first dielectric layer 200 and the second dielectric layer 400 are made of different materials. In one embodiment, both can be insulating material layers, but exhibit different properties when performing photolithography and etching. In one embodiment, both can be photoresists, but one of them is configured as a positive resist and the other is configured as a secondary resist. In any embodiment provided by the present invention, the first dielectric layer 200 can have a higher resolution than the second dielectric layer 400.
[0068] Among them, when the substrate 100 is used to prepare a metasurface lens, the epitaxial structure can be used to form or directly serve as a number of nanostructures on the metasurface layer, and is specifically used to form control over the phase, amplitude, etc. of the incident light.
[0069] like Figure 3 The present invention provides a second embodiment of a substrate manufacturing method, which includes the following steps.
[0070] Step S1, providing a substrate.
[0071] Step S2, forming a groove having a first width on the substrate.
[0072] Step S31 , forming a first film layer on a side of the first groove away from the substrate.
[0073] Step S32, forming a second dielectric layer on a side of the first film layer away from the first dielectric layer.
[0074] Step S4, removing the first film layer portion located on both sides of the second dielectric body to obtain a first film layer protrusion.
[0075] Step S5, forming a first substrate protrusion on the substrate along the first film layer protrusion.
[0076] Wherein, the first groove is formed at the first dielectric layer on the substrate.
[0077] Combination Figures 8 to 11 In order to simplify the manufacturing process and better adapt to mass production and the formation of complex patterns, the present invention adopts a solution of sequentially arranging film layers and dielectric layers on a package body formed by a substrate 100 and other hierarchical structures.
[0078] In one embodiment, for step S31, the first film layer 300 may be formed as a whole on the side of the first groove 21 away from the substrate 100, and is not limited to being formed only on the inner wall of the first groove 21. In other words, the first groove 21 (or the first dielectric layer 200 used to form the first groove 21) and the substrate 100 constitute a package, and the first film layer 300 is formed on the side of the package located on the side of the first groove 21 away from the substrate 100; that is, the relatively upper side in the figure. At this time, the first film layer 300 is not only formed on the side wall (composed of the first dielectric layer 200) and the groove bottom (which may be composed of the first dielectric layer 200, preferably composed of the substrate 100) of the first groove 21, but can also be arranged on other parts of the first dielectric layer 200 on the side away from the substrate 100.
[0079] In one embodiment, the “forming a first film layer” in step S31 may include any of the following solutions:
[0080] (1) depositing the first film layer by ALD (Atomic Layer Deposition);
[0081] (2) Depositing the first film layer by EBE (Electron Beam Evaporation).
[0082] Among them, ALD has the advantages of high precision, high uniformity, and can adapt to the deposition of complex patterns; EBE has the advantages of fast deposition speed and low equipment cost. During operation, you can choose to configure one of them or mix the two according to the actual situation.
[0083] Preferably, the present invention adopts ALD, and specifically configures the "forming a first film layer" in step S31 to include: using an atomic layer deposition method to uniformly coat the bottom and sidewalls of the first groove with the first film layer. Figures 8 to 10 , it is possible to accurately control the extent of "shrinking" of the first film layer 300 in the width direction and / or thickness direction at the first groove 21, and thus accurately adjust the second width b to achieve the preparation of the target small line width structure.
[0084] In addition, combined Figures 8 to 16 Since the first film layer 300 is uniformly deposited on at least the left and right side walls of the first groove 21, the positional deviation of the second dielectric body 41, the first film layer protrusion 32 and the first substrate protrusion 11 formed subsequently in the width direction can be avoided; similarly, since the first film layer 300 is uniformly deposited on the groove bottom and side walls of the first groove 21, the positions of the second dielectric body 41, the first film layer protrusion 32 and the first substrate protrusion 11 in the thickness direction can be controlled. The above configuration has more significant advantages with the participation of ALD.
[0085] In one embodiment, the first film layer 300 can be configured as a metal mask material. As a mask material, it can facilitate subsequent etching operations; as a metal material, especially when configured as chromium, it has a better stripping property than other structural materials used in the preparation process.
[0086] In one embodiment, for step S31, the second dielectric layer 400 may be formed as a whole on the side of the first film layer 300 away from the first dielectric layer 200 (or away from the first groove 21). In other words, the first film layer 300 (or the second groove 31), the first dielectric layer 200 (or the first groove 21) and the substrate 100 constitute a package, and the second dielectric layer 400 is formed and located on the side of the first film layer 300 away from the first dielectric layer 200 (or away from the substrate 100); that is, relatively above in the figure. At this time, the first film layer is not only formed in the space enclosed by the second groove 31, but can also be arranged at other parts of the first film layer 300 away from the first dielectric layer 200.
[0087] In one embodiment, the "forming the second dielectric layer" in step S32 may include: forming the second dielectric layer by spin coating. In this way, the second dielectric layer can be made more uniform, which facilitates subsequent etching and photolithography of the second dielectric body formed by the second dielectric layer, and can improve the accuracy of subsequent steps.
[0088] Preferably, the second dielectric layer is configured with a material having good filling properties, so that it can be more and more fully filled in the second groove 31. Of course, the present invention does not exclude the use of CVD (Chemical Vapor Deposition) or ALD and other processes.
[0089] In one embodiment, the second dielectric layer 300 can be configured as a photoresist mask material. As a grinding material, it can facilitate subsequent etching operations; as a photoresist material, especially when configured as a secondary resist, it has photosensitivity and leaves the exposed part while dissolving the exposed part during development, thereby preventing it from being affected by other steps in the substrate manufacturing process.
[0090] Preferably, the second dielectric layer 300 may be configured as a material with good filling and etching resistance to avoid being affected by other process flows.
[0091] In one embodiment, the first dielectric layer 200 and the second dielectric layer 400 are made of different materials. In any embodiment provided by the present invention, the second dielectric layer 400 may have better filling property and etching resistance than the first dielectric layer 200 .
[0092] If, when executing step S3 or step S32, it is ensured that the second dielectric layer is only filled in the second groove, or it is ensured that all or most of the second dielectric layer is used to form the second dielectric body (equivalent to directly generating the second dielectric body after executing the above steps), Fig.11 If the structure shown in FIG. 1 is not shown in FIG. 1 , step S4 is directly executed, which can simplify the process flow and improve the structural accuracy.
[0093] If, due to process difficulty, the second dielectric layer is inevitably arranged at other parts of the first film layer except the second groove when executing step S3 or step S32, especially arranged at the side of the first film layer away from the first dielectric layer (or substrate) at the other parts of the first film layer, the substrate manufacturing method provided by the present invention can also achieve the effect of forming a protrusion of the first film layer by removing the excess part of the second dielectric layer and part of the first film layer.
[0094] Specifically, in one embodiment, before implementing step S4 (removing the first film layer portion located on both sides of the second dielectric body to obtain the first film layer protrusion) or its derivative steps; after implementing step S3 or its derivative step S32 (forming the second dielectric layer on the side of the first film layer away from the first dielectric layer), the substrate manufacturing method may further include:
[0095] Step S33: etching and removing the portion of the second dielectric layer located on the side of the second dielectric body away from the first film layer by oxygen plasma, and retaining at least a portion of the second dielectric body.
[0096] refer to Figure 10 to Figure 11 When the portion of the second dielectric layer 400 that is not used to form the second dielectric body 41 is attached to the first film layer 300 , the excess portion of the second dielectric layer 400 can be etched away before processing the first film layer 300 , thereby facilitating subsequent processing of the first film layer 300 .
[0097] On the one hand, the process of etching using the "oxygen plasma" can be interpreted as implementing oxygen plasma etching, which is an efficient dry etching technology that can effectively and quickly remove organic materials. Of course, when there are other configuration schemes for the second dielectric layer 400, other etching or photolithography methods can also be used instead.
[0098] On the one hand, the “portion of the second dielectric layer located on the side of the second dielectric body away from the first film layer” can be interpreted as defining a hierarchical structure between the first film layer 300 and the substrate 100 to constitute a package, and removing other portions of the second dielectric layer 400 on the second dielectric body 41 away from the side of the package through step S33; or it can be interpreted as the portion of the second dielectric layer 400 located outside the second groove 31 (or its enclosed space); or it can be interpreted as the portion of the second dielectric layer 400 that is not used to form the second dielectric body 41.
[0099] On the other hand, “retaining at least part of the second dielectric body” can be interpreted as: retaining the entire second dielectric body 41 (ie, retaining the entire part of the second dielectric layer 400 located in the second groove 31 ), or retaining part of the second dielectric body 41 .
[0100] Preferably, compared with the first film layer, the retained portion of the second dielectric body is away from the surface of the substrate and closer to the substrate. Fig.11 As shown, the surface of the retained portion of the second dielectric body 41 on the side facing away from the substrate 100 is shorter in height than the surface of the first film layer 300 on the side facing away from the substrate 100. In this way, the portion of the second dielectric body 41 close to the plane where the surface of the first film layer 300 on the side facing away from the substrate 100 is located is removed at the same time, and the portion of the second dielectric body 41 is retained; it is equivalent to deepening the etching of the redundant portion of the second dielectric layer 400. Based on the difference in materials between the second dielectric layer 400 and the first film layer 300, the second dielectric layer 400 attached to the first film layer 300 can be completely removed without affecting the first film layer 300, so as to facilitate the implementation of subsequent steps.
[0101] For step S4, the present invention can provide a process method based on Fig.10 or Fig.11In the embodiment shown in the structure, the first film layer 300 and the first dielectric layer 200 (if any) located on the plane of the two sides of the first dielectric body 41 away from the first dielectric body 41 can be removed together, and the step S4 can be directly performed to form a Fig.14 As shown (or Fig.14 A second dielectric body is provided on top of the structure.
[0102] However, in a scenario where conventional process flow is applicable and all of them cannot be removed at once, a similar effect can be achieved by implementing the third embodiment provided below to overcome the technical barriers.
[0103] like Figure 4 The present invention provides a third embodiment of a substrate manufacturing method, which includes the following steps.
[0104] Step S1, providing a substrate.
[0105] Step S2, forming a groove having a first width on the substrate.
[0106] Step S3, forming a first film layer and a second dielectric layer in sequence at least at the first groove.
[0107] Step S41 , removing at least a portion of the first film layer located on both sides of the second dielectric body, retaining at least a portion of the second groove, so that the side surface of the second dielectric body is at least exposed outside the retained portion of the second groove.
[0108] Step S42 , using the second dielectric body as a mask, removing the portion of the second groove that exceeds the side surface of the second dielectric body, to obtain a first film layer protrusion.
[0109] Step S5, forming a first substrate protrusion on the substrate along the first film layer protrusion.
[0110] Combination Figure 11 to Figure 12 For step S41, the “at least part of the first film layer located on both sides of the second dielectric body” can be interpreted as removing all the first film layer 300 located on both sides of the second dielectric body 41, or can be interpreted as partially removing the above-mentioned part of the first film layer 300.
[0111] In one embodiment, the portion of the first film layer 300 that is not used to form the second groove 31 may be removed; in one embodiment, the portion of the first film layer 300 that is outside the first groove 21 may be removed.
[0112] Retaining at least part of the second groove 31 can, on the one hand, avoid over-etching of the first film layer 300 and affect the width of the subsequent first film layer protrusion 32; on the other hand, it can increase the margin of the first film layer 300 before etching to form the first film layer protrusion 32, thereby preventing low equipment precision from causing further etching to fail to form the first film layer protrusion 32.
[0113] By making the side surface of the second dielectric body 41 at least exposed outside the reserved portion of the second groove 31, on the one hand, it is possible to release at least part of the coverage of the side surface of the second dielectric body 41 by the first film layer 300, so that the second dielectric body 41 can be used as a mask for subsequent etching; on the other hand, when the thickness of the first dielectric layer 200 (or the depth of the first groove 21) is less than the sum of the thickness of the reserved portion of the second dielectric body 41 and the thickness of the portion of the first film layer 300 located between the second dielectric body 41 and the substrate 100 (or the first dielectric layer 400), the second dielectric body 41 can be exposed in the height direction, thereby facilitating the process operation.
[0114] Preferably, the step S41 may include:
[0115] Step S411, etching and removing portions of the first film layer located on both sides of the second dielectric body and on the side of the first groove away from the substrate, retaining at least a portion of the second groove, so that a side surface of the second dielectric body is at least partially exposed outside the retained portion of the second groove.
[0116] The first groove is formed at the first dielectric layer on the substrate, and compared with the first dielectric layer, the reserved portion of the second groove is away from the surface of one side of the substrate and is closer to the substrate.
[0117] Combination Figure 11 to Figure 12 , which is equivalent to etching away part of the first film layer 300 located on both sides of the second dielectric body 41 and above the first dielectric layer 200, so as to retain the second groove 31 and expose the side of the second dielectric body 41. At this time, it is equivalent to etching with the side of the second dielectric body 41 and the upper surface of the first dielectric layer 200 as reference at the same time, which can reduce the difficulty of the process.
[0118] In addition, the upper surface of the reserved portion of the second groove 31 is lower than the upper surface of the first dielectric layer 200 , which can effectively remove the first film layer 300 attached to the first dielectric layer 200 , and does not affect the first dielectric layer 200 when the first dielectric layer 200 and the first film layer 300 are configured with different materials.
[0119] It can be understood that the relationship between the second groove 31 and the first film layer 300, and the relationship between the first dielectric layer 200 and the first groove 21 can be referred to in the previous text, and will not be described in detail here. The directional words such as "upper" and "lower" defined in the present invention can be understood with reference to the accompanying drawings, but do not mean that the relevant structures provided by the present invention are limited to the placement states shown in the accompanying drawings.
[0120] In addition, the etching and removing process of part of the first film layer 300 proposed in step S41 may adopt dry etching or wet etching, which is not limited in the present invention.
[0121] Combination Figure 12 to Figure 13 For step S42, the “removing the portion of the second groove that exceeds the side of the second dielectric body” can be interpreted as removing the portion of the second groove 31 that exceeds the plane where the side of the second dielectric body 41 is located in the width direction, or can be interpreted as removing the portion of the second groove 31 that is outside the projection of the second dielectric body 41 formed thereon with a width of the second width b.
[0122] In one embodiment, the portion of the retained portion of the second groove 31 located on the plane where the side surface of the second dielectric body 41 and the side wall of the first groove 21 (or the side wall of the first dielectric layer 200 close to the second dielectric body 41) are located can be removed; in one implementation manner, the portion of the retained portion of the second groove 31 located outside the second dielectric body 41 can be removed.
[0123] By using the second dielectric body 41 as a mask, the formed first film layer protrusion 32 can be strictly aligned with the outer edge of the second dielectric body 41 , thereby accurately obtaining the first film layer protrusion 32 with the second width b.
[0124] It can be understood that the first film layer protrusion 32 is formed by etching the first film layer 300 , and thus the first film layer protrusion 32 may have the same material configuration as the first film layer 300 .
[0125] Preferably, the step S42 may include:
[0126] Step S421 , using the second dielectric body and the first dielectric layer as masks, etching and removing the first film layer portion of the second groove located at the gap between the second dielectric body and the first dielectric layer by inductively coupled plasma, to obtain a first film layer protrusion located at a side of the second dielectric body close to the substrate.
[0127] Combination Figure 12 to Figure 13, which is equivalent to partially removing the first film layer 300 located at the gap between the first dielectric layer 200 and the second dielectric body 41 in the retained portion of the second groove 31, and jointly forming a restriction on the etching operation by the two dielectric layers so that the portion that cannot be used to form the first film layer protrusion 32 is completely removed, thereby improving the width accuracy of the second film layer protrusion 32 and indirectly improving the width accuracy of the first substrate protrusion 11 that is finally formed.
[0128] Although step S421 indicates that after obtaining the first film layer protrusion 32, the second dielectric body 41 is still retained, it is understandable that in step S42 or other embodiments derived from step S4, the second dielectric body 41 and / or the first dielectric layer 200 can also be removed in this step to directly generate Fig.14 The structure shown.
[0129] The process of using the "inductively coupled plasma" etching can be interpreted as implementing inductively coupled plasma etching (ICP Etching), which is a high-precision dry etching technology that can strictly ensure that the width of the first film layer protrusion 32 meets expectations and can be suitable for manufacturing micro-nano structures. Of course, when there are other configuration schemes for the first film layer 300, other etching or photolithography methods can also be implemented instead.
[0130] like Figure 5 The present invention provides a fourth embodiment of a substrate manufacturing method, which includes the following steps.
[0131] Step S1, providing a substrate.
[0132] Step S2, forming a groove having a first width on the substrate.
[0133] Step S3, forming a first film layer and a second dielectric layer in sequence at least at the first groove.
[0134] Step S4, removing the first film layer portion located on both sides of the second dielectric body to obtain a first film layer protrusion.
[0135] Step S51, removing the first dielectric layer and the second dielectric body.
[0136] Step S52, using the first film layer protrusion as a mask, etching the substrate to form a first substrate protrusion.
[0137] Wherein, the first groove is formed at the first dielectric layer on the substrate. Wherein, the first dielectric layer and the second dielectric body are photoresist.
[0138] Combination Figures 13 to 15When the first dielectric layer 200 and the second dielectric body 41 (or the second dielectric layer 400) are both photoresists, they can be removed together regardless of whether they present different optical properties, thereby saving operation time and quickly obtaining a package body including only the first film layer protrusion 32 and the substrate 100.
[0139] Preferably, step S51 may be specifically implemented by oxygen plasma etching, or other wet degumming methods, such as using acetone, N-methylpyrrolidone (N-Methyl-2-pyrrolidone, NMP), N, N-dimethylformamide (Dimethylformamide, DMF) and other reagents. Of course, the first dielectric layer 200 and the second dielectric body 41 (second dielectric layer 400) may also be removed in sequence.
[0140] Since after step S51, the substrate 100 only carries the first film layer protrusions 32 of the second width b, when combined with step S22, it is equivalent to that the preset pattern has been transferred to the substrate 100 and is composed of the first film layer protrusions 32, and a smaller line width arrangement is achieved. At this time, Fig.14 The structure shown can be used directly to form a predetermined pattern of wiring; Fig.14 The structure shown can be used as a substrate assembly (package) finally manufactured by the present invention.
[0141] Furthermore, the first film layer protrusion 32 can be used as a mask to further etch the first substrate protrusion 11, thereby realizing the arrangement of a smaller line width structure on the substrate 100. Preferably, the preset pattern can be transferred to the substrate 100 body, so as to facilitate the use of the substrate 100 to prepare optical devices such as metasurface lenses or other semiconductor devices.
[0142] In one embodiment, the first substrate protrusion 11 and the first film layer protrusion 32 work together, so that: Fig.15 The structure shown can be used as another substrate assembly (package) finally manufactured by the present invention.
[0143] In a preferred embodiment, step S5 may further include:
[0144] Step S53, removing the first film layer protrusions.
[0145] Combination Figure 15 to Figure 16 , the first substrate protrusion 11 with the second line width b can be formed, and the substrate 100 formed in this way itself realizes the formation of a smaller line width structure, and preferably the preset pattern can also be transferred. Therefore, Fig.16 The structure shown can be used as another substrate finally manufactured by the present invention.
[0146] The line width described in this article can be interpreted as a critical dimension (CD). The two terms only differ in expression in the solution provided by the present invention and are not used to limit the present invention.
[0147] The above four embodiments provided by the present invention, as well as other implementation modes, embodiments or specific examples, etc., can be combined or separated with each other. The steps of the substrate manufacturing method provided by the present invention can be exchanged in sequence, and the technical effects produced after the sequence exchange are what can be expected by those skilled in the art under the inspiration of the above description of the present invention.
[0148] In summary, the substrate manufacturing method and metasurface lens provided by the present invention use the first groove with a larger line width on the substrate as a "negative mold" to form a second dielectric body and a second film layer protrusion corresponding to the first groove and having a smaller line width, so as to achieve the effect of processing the first substrate protrusion at the substrate corresponding to the second film layer protrusion. Since the first substrate protrusion corresponds to the second film layer protrusion, it has the same smaller line width. In this way, on the basis of the existing groove formation technology, a structure with a smaller line width can be further formed on the substrate, and the demand for materials is weakened, which can be suitable for mass production of devices.
[0149] It should be understood that although this specification is described according to implementation modes, not every implementation mode contains only one independent technical solution. This description of the specification is only for the sake of clarity. Those skilled in the art should regard the specification as a whole. The technical solutions in each implementation mode may also be appropriately combined to form other implementation modes that can be understood by those skilled in the art.
[0150] The series of detailed descriptions listed above are only specific descriptions of feasible implementation methods of the present invention. They are not intended to limit the scope of protection of the present invention. Any equivalent implementation methods or changes that do not deviate from the technical spirit of the present invention should be included in the scope of protection of the present invention.
Claims
1. A method for manufacturing a substrate, characterized in that: include: providing a substrate; forming a first groove having a first width on the substrate; A first film layer and a second dielectric layer are sequentially formed at least at the first groove; wherein the portion of the first film layer in the first groove is indented inwardly to form a second groove, and the second dielectric layer forms a second dielectric body having a second width in the second groove; the second width is smaller than the first width; Removing the first film layer portion located on both sides of the second dielectric body to obtain a first film layer protrusion; wherein the first film layer protrusion has the second width; A first substrate protrusion is formed on the substrate along the first film layer protrusion; wherein the first substrate protrusion has the second width.
2. The method for manufacturing a substrate according to claim 1, characterized in that: The “forming a first groove having a first width on the substrate” specifically includes: forming a first dielectric layer on the substrate; On the first dielectric layer, an epitaxial structure matching a preset pattern and including the first groove is formed by photolithography.
3. The method for manufacturing a substrate according to claim 2, characterized in that: The material of the first dielectric layer is different from that of the second dielectric layer; the first dielectric layer includes ultraviolet photoresist and has high resolution.
4. The method for manufacturing a substrate according to claim 1, wherein: The “forming a first film layer and a second dielectric layer in sequence at least at the first groove” specifically includes: Forming the first film layer on the side of the first groove away from the substrate; wherein the first groove is formed at the first dielectric layer on the substrate; The second dielectric layer is formed on a side of the first film layer away from the first dielectric layer.
5. The method for manufacturing a substrate according to claim 4, characterized in that: The “forming the first film layer” specifically includes: using an atomic layer deposition method to uniformly cover the bottom and sidewalls of the first groove with the first film layer; wherein the first film layer is configured as a metal mask material; The "forming the second dielectric layer" specifically includes forming the second dielectric layer by spin coating; wherein the material of the second dielectric layer is different from that of the first dielectric layer; the second dielectric layer is configured as a photoresist mask material and has good filling and etching resistance.
6. The method for manufacturing a substrate according to claim 4, characterized in that: After “forming the second dielectric layer on the side of the first film layer away from the first dielectric layer”, the method further includes: The second dielectric layer portion located on the side of the second dielectric body away from the first film layer is etched away by oxygen plasma, and at least a portion of the second dielectric body is retained; wherein, compared with the first film layer, the retained portion of the second dielectric body is away from the surface of the substrate side and closer to the substrate.
7. The method for manufacturing a substrate according to claim 1, characterized in that: The “removing the first film layer portion located on both sides of the second dielectric body to obtain the first film layer protrusion” specifically includes: removing at least a portion of the first film layer located on both sides of the second dielectric body, retaining at least a portion of the second groove, so that at least a portion of the side surface of the second dielectric body is exposed outside the retained portion of the second groove; The second dielectric body is used as a mask to remove the portion of the second groove that exceeds the side surface of the second dielectric body to obtain the first film layer protrusion.
8. The method for manufacturing a substrate according to claim 7, characterized in that: The “removing at least a portion of the first film layer located on both sides of the second dielectric body, retaining at least a portion of the second groove, so that the side surface of the second dielectric body is at least partially exposed outside the retained portion of the second groove” specifically includes: Etching and removing the portions of the first film layer located on both sides of the second dielectric body and on the side of the first groove away from the substrate, leaving at least a portion of the second groove, so that the side surface of the second dielectric body is at least partially exposed outside the remaining portion of the second groove; wherein the first groove is formed at the first dielectric layer on the substrate, and compared with the first dielectric layer, the remaining portion of the second groove is away from the surface of the side of the substrate and closer to the substrate; The “using the second dielectric body as a mask to remove the portion of the second groove that exceeds the side surface of the second dielectric body to obtain the first film layer protrusion” specifically includes: At the same time, the second dielectric body and the first dielectric layer are used as masks, and the first film layer portion where the second groove is located in the gap between the two is etched away by inductively coupled plasma to obtain a first film layer protrusion located on the second dielectric body near the substrate.
9. The method for manufacturing a substrate according to claim 1, characterized in that: The first groove is formed at the first dielectric layer on the substrate; and the “forming a first substrate protrusion at the substrate along the first film layer protrusion” specifically includes: removing the first dielectric layer and the second dielectric body; wherein the first dielectric layer and the second dielectric body are photoresists; Using the first film layer protrusion as a mask, etching the substrate to form the first substrate protrusion; The first film layer protrusion is removed.
10. A metasurface lens, characterized in that: It comprises a substrate; the substrate is prepared by the substrate manufacturing method according to any one of claims 1 to 9.