Production distribution method of medium-thickness plate production line
By optimizing the heating furnace and rolling mill process of the medium and thick plate production line, ensuring their production capacity matching, the problem of mismatch between the heating furnace and rolling mill capacity in the existing technology is solved, and the overall efficiency and rhythm of the production line are improved.
Patent Information
- Application Number
- CN202411378738.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-09-30
- Publication Date
- 2024-12-06
- Estimated Expiration
- 2044-09-30
AI Technical Summary
When the prior art improves the production efficiency of medium and thick plate production lines, it unilaterally improves the heating capacity of the heating furnace or the rolling mill capacity, resulting in a mismatch between the heating furnace and the rolling mill capacity, affecting the rhythm and output of the entire production line.
By optimizing the process of heating furnace and rolling mill, we ensure that the production capacity of the heating furnace matches the capacity of the rolling mill. The combination of multiple heating furnaces and dual-stack rolling mills is adopted to adjust the process parameters of the heating furnace and rolling mill to make their production capacity per unit time Matching the output, a 5-stage heating and insulation process and instant cooling device are used to optimize the heating and rolling rhythm of the blank.
It effectively avoids the situation of empty rolling mills and waiting for blanks to be released, improves the production efficiency of the production line, reduces the rolling time and waiting time, improves the rolling efficiency, and matches the rhythm of the heating furnace and the rolling mill.
Smart Images

Figure CN119076614A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of medium and thick plate rolling, and in particular provides a production allocation method for a medium and thick plate production line. Background Art
[0002] There are many factors that affect the production efficiency of medium and thick plate production lines in the prior art, such as the heating capacity of the heating furnace, the rolling capacity of the rolling mill, etc. Currently, many patents only propose to improve the heating capacity of the heating furnace, or to improve the rolling capacity of the rolling mill, but no effective method is given to improve the production efficiency of the entire medium and thick plate production line.
[0003] As for the prior art, there are many patents that optimize the heating efficiency of the heating furnace by optimizing the heating distribution method, such as patents CN102747216B, CN102435072A, CN107475507A, etc., by controlling the gap between the steel billets in the heating furnace, laying out the slabs in multiple layers, or using a walking beam heating furnace and a pusher heating furnace to share the slabs, etc.;
[0004] Some patents also improve production efficiency by optimizing the rolling process, such as patent CN101658870A, which uses a variable rolling process to improve the rolling mill rhythm, such as patent CN102896148B, which uses a method to optimize the double-stand rolling load distribution to improve the rolling rhythm.
[0005] The technical solutions disclosed in the above patent documents for improving the heating efficiency of the heating furnace or improving the rolling rhythm of the rolling mill only improve the efficiency unilaterally from the heating furnace or the rolling rhythm, without considering the overall medium and thick plate production line. The production efficiency of the medium and thick plate production line is jointly determined by the heating capacity of the heating furnace and the rolling capacity of the rolling mill. Improving the heating capacity of the heating furnace or the rolling capacity of the rolling mill alone will cause a mismatch between the heating furnace and the rolling mill, affecting the rhythm and output of the entire production line. Summary of the invention
[0006] In view of the above problems, the present invention provides a process optimization scheme for the medium and thick plate production line taking into account the overall process. The scheme can match the heating furnace capacity with the rolling mill capacity, and can also optimize the heating furnace process and the rolling mill process respectively. The specific scheme is as follows:
[0007] A production allocation method for a medium and thick plate production line, comprising:
[0008] S1, heating process;
[0009] S2, rolling process, wherein:
[0010] In the step S1, the total amount of the blank heated by the heating process in a unit time by multiple heating furnaces is N1;
[0011] In the step S2, the total amount of steel plates that can be rolled by the double-stand rolling mill in a unit time is N2;
[0012] The relationship between N1 and N2 complies with the formula N2-2<N1<N2+3.
[0013] Furthermore, there are three heating furnaces, namely, two first heating furnaces F1 and F2 and one second heating furnace F3. The first heating furnace is provided with two parallel walking beams; the second heating furnace is provided with three parallel walking beams; the total amount of the blanks heated by the three heating furnaces per unit time is:
[0014] N1=N F1 +N F2 +N F3 =(2A1+2A2+2n+m+A3) / t;
[0015] Wherein, A1 is the number of rows of billets in the first heating furnace F1, A2 is the number of rows of billets in the first heating furnace F2; A3 is the number of rows of billets in the second heating furnace F3; t is the heating time in hours;
[0016] n is the number of rows in the second heating furnace of the a-type material distribution method, in which three blanks arranged side by side are fed in each time through three rows of walking beams;
[0017] m is the number of rows in the second heating furnace of type b distribution method. Type b distribution method is to feed two side-by-side blanks each time through three rows of walking beams, and the length of at least one blank needs to be erected by two rows of walking beams.
[0018] Furthermore, the blank includes two sizes with a thickness of 220 mm or 320 mm.
[0019] Furthermore, the heating steps of the three heating furnaces in step S1 for heating the blank with a thickness of 320 mm include:
[0020] H1, preheating temperature ≤ 950℃, residence time ≥ 60min;
[0021] H2, heating section temperature is 950~980℃, residence time is ≥60min;
[0022] H3, the temperature of the heating section is 1080~1110, and the residence time is ≥60min;
[0023] H4, heating section temperature is 1150~1180℃, residence time is ≥90min;
[0024] H5, the temperature of the soaking section is 1160~1200℃, and the residence time is ≥50min;
[0025] Total time ≥320min;
[0026] The heating steps for a billet thickness of 220 mm include:
[0027] B1. Preheating temperature ≤ 950℃, residence time ≥ 40min;
[0028] B2, the temperature of the heating section is 950~980℃, and the residence time is ≥40min;
[0029] B3, the temperature of the heating section is 1080~1110, and the residence time is ≥40min;
[0030] B4, the temperature of the heating section is 1150~1180℃, and the residence time is ≥70min;
[0031] B5. The temperature of the soaking section is 1160~1200℃, and the residence time is ≥30min;
[0032] Total time in the furnace ≥ 220min.
[0033] Furthermore, in step S2, the double-stand rolling mill includes a roughing mill and a finishing mill, wherein the roughing mill and the finishing mill have odd number of passes.
[0034] Furthermore, in the step S2, the rolling force of the roughing mill and the finishing mill passes is ≥ rated rolling force × 70%, or the torque of the roughing mill and the finishing mill passes is ≥ rated torque × 70%.
[0035] Furthermore, in the step S2, an instant cooling device is used to cool the intermediate billet between the roughing mill and the finishing mill.
[0036] Furthermore, in step S2, after the intermediate billet is finished in the roughing mill, the intermediate billet passes through the instant cooling system of the roughing mill. After cooling, the intermediate billet is transported to the instant cooling system of the finishing mill. During the transportation process, the intermediate billet is self-tempered and finally enters the instant cooling system of the roughing mill for cooling again.
[0037] Compared with the prior art, the advantages of the present invention are as follows:
[0038] 1. The present invention controls the heating quantity per unit time of the three heating furnaces to match the rolling quantity per unit time of the double-stand rolling mill, thereby avoiding the situation where the rolling mill is idle and waiting for the billet to be discharged from the furnace, thereby improving the production efficiency of the production line.
[0039] 2. The present invention adjusts the width value of the billet in the furnace and the number of rows heated by the two first heating furnaces, thereby adjusting the amount of billets heated per unit time in the two first heating furnaces; and adjusts the total number of billets heated in the third heating furnace by controlling the number of rows of the three distribution methods, thereby adjusting the amount of billets heated per unit time in the third heating furnace. By adjusting the amount of billets heated per unit time in the three heating furnaces, it is matched with the production capacity rhythm of the double-stand rolling mill.
[0040] 3. The present invention implements a five-stage heating and heat preservation process for billets of two specifications, 220 mm and 320 mm, in the walking beam type continuous heating furnace. By selecting the specifications of billet thickness, the residence time of the billets in multiple walking beam type continuous heating furnaces is controlled, so that the discharge rhythm of the multiple walking beam type continuous heating furnaces matches the rolling rhythm of the double-stand rolling mill.
[0041] 4. The present invention adopts the method of reducing the rolling time of each pass, reducing the total number of billet rolling passes, reducing the waiting time of the roughing mill and the finishing mill, and reducing the waiting time of the intermediate billet, thereby greatly improving the rolling rhythm and the rolling efficiency. BRIEF DESCRIPTION OF THE DRAWINGS
[0042] Figure 1 It is a top view schematic diagram of the material distribution method of the first walking beam type continuous heating furnace and the second walking beam type continuous heating furnace of the present invention. DETAILED DESCRIPTION
[0043] The technical solution of the invention will be described clearly and completely below. Obviously, the described embodiments are only part of the embodiments of the invention, rather than all of the embodiments.
[0044] Based on the embodiments of the invention, all other embodiments obtained by ordinary technicians in this field without making any creative work shall fall within the scope of protection of the invention.
[0045] In the description of the invention, it should be noted that the terms "center", "upper", "lower", "left", "right", "vertical", "horizontal", "inner", "outer", etc., indicating the orientation or positional relationship, are based on the orientation or positional relationship shown in the drawings, and are only for the convenience of describing the invention and simplifying the description, rather than indicating or implying that the device or element referred to has a specific orientation, is constructed and operated in a specific orientation, and therefore cannot be understood as limiting the invention. In addition, the terms "first", "second", and "third" are used for descriptive purposes only, and cannot be understood as indicating or implying relative importance.
[0046] In the description of the invention, it should be noted that, unless otherwise clearly specified and limited, the terms "installed", "connected", and "connected" should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection or an electrical connection; it can be a direct connection, or it can be indirectly connected through an intermediate medium, or it can be the internal communication of two components. For ordinary technicians in this field, the specific meanings of the above terms in the invention can be understood according to specific circumstances.
[0047] Example 1
[0048] A production allocation method for a medium and thick plate production line, comprising:
[0049] Three heating furnaces, namely two first heating furnaces F1 and F2 and one second heating furnace F3, the first heating furnaces are provided with two parallel walking beams, and the second heating furnace is provided with three parallel walking beams;
[0050] The length of the first heating furnace and the second heating furnace are both L, and the maximum width of the blank is l max , the minimum width is l min , the number of rows of billets in the heating furnace is: L / l min ≧A≧L / l max , A takes the minimum value of integers;
[0051] Then, let the number of rows of billets in the first heating furnace F1 be A1, the number of rows of billets in the first heating furnace F2 be A2, and the number of rows of billets in the second heating furnace F3 be A3;
[0052] The heating time of the two first heating furnaces F1 and F2 and the second heating furnace F3 is constant at t, where t is the heating time in hours.
[0053] Since two rows of walking beams are arranged in the first heating furnace, two side-by-side blanks can be fed in each time, and the number of blanks that can be heated by the first heating furnace each time is 2A; the heating quantities per unit time of the two first heating furnaces are: N F1 =2A1 / t and N F2 =2A2 / t;
[0054] There are three rows of walking beams in the second heating furnace, and the feeding methods of the blanks are as follows:
[0055] a. Three parallel blanks are fed in each time through three rows of walking beams;
[0056] b. Feed two side-by-side blanks at a time through three rows of walking beams, and the length of at least one blank needs to be set up by two rows of walking beams;
[0057] c. Feed one piece of blank each time through three rows of walking beams;
[0058] Assume that there are n rows of a type of material distribution, m rows of b type of material distribution, and f rows of c type of material distribution in the second heating furnace, f = A3-mn, then the number of blanks heated in the second heating furnace is 3n+2m+(A3-nm)=2n+m+A3, and the number of heats per unit time in the second walking beam continuous heating furnace is: N F3 =(2n+m+A3) / t;
[0059] Then the total amount of blanks heated by multiple heating furnaces per unit time is N1 = N F1 +N F2 +N F3 =(2A1+2A2+2n+m+A3) / t, where t is the heating time in hours.
[0060] Preferably, each time, two billets U1 and U2 are respectively sent into the first heating furnace for heating side by side through two rows of walking beams. The length range of the two billets U1 and U2 is between 2600 and 4800 mm, preferably 3300 mm, and the interval between the two billets is 300 to 600 mm; the width of the billets S1 and S2 can be selected from the values of 1865, 2265, and 2665 mm, preferably 2265 mm, and each batch of the furnace can be loaded with 20 rows, with an error of ±1 row, for a total of 40±2 pieces. The time in the furnace for a billet with a thickness of 220 mm is 220 minutes, that is, 10.9±2 pieces can be taken out per hour; the time in the furnace for a billet with a thickness of 320 mm is 320 minutes, that is, 7.5±2 pieces can be taken out per hour.
[0061] The second step heating furnace is equipped with three parallel walking beams, and its distribution method includes:
[0062] a. Each time, three billets A1, A2, A3 are respectively sent into the furnace for heating in parallel through three rows of walking beams. Each of billets A1, A2, A3 uses one row of walking beams. The length range of A1, A2, A3 is between 2600 and 3300 mm, and the length is preferably 3300 mm; the interval between each row of billets is 300 to 600 mm; the width of billets A1, A2, A3 can be selected from 1865, 2265, and 2665 mm, and the preferred width is 2265 mm;
[0063] b1. Two blanks V1 and V2 are sent into the furnace for heating side by side through three rows of walking beams. The lengths of the blanks V1 and V2 cannot be transported by one walking beam. The two blanks V1 and V2 are placed on the two outer walking beams respectively. The adjacent ends of the blanks V1 and V2 are both mounted on the middle walking beam. The lengths of V1 and V2 are both between 4800 and 5000 mm.
[0064] b2. Two billets C1 and C2 are fed into the furnace for heating in parallel through three rows of walking beams. Billet C1 is twice as long as billet C2. During heating and transportation, C1 is placed on two adjacent rows of walking beams, and C2 is placed on another walking beam. The length of C1 is 5001-6599 mm, and the length of C2 is 2600-3300 mm. If billets C1 and C2 are fed continuously, the positions of C1 and C2 need to be exchanged when they are fed next time.
[0065] d. Send a piece of billet D with a length that requires three rows of walking beams to be erected into the furnace for heating. The length of D is 6600~10000mm;.
[0066] Table 1: Loading status of walking beam continuous heating furnace
[0067]
[0068] The processing technology for blank thickness of 320mm includes:
[0069] The processing technology for the blank with a thickness of 320mm includes: H1, preheating section temperature ≤ 950℃, residence time ≥ 60min; H2, heating section temperature 950~980℃, residence time ≥ 60min; H3, heating section temperature 1080~1110, residence time ≥ 60min; H4, heating section temperature 1150~1180℃, residence time ≥ 90min; H5, soaking section temperature 1160~1200℃, residence time ≥ 50min; total time ≥ 320min;
[0070] The processing technology for the billet with a thickness of 220mm includes: B1, preheating section temperature ≤ 950℃, residence time ≥ 40min; B2, heating section temperature is 950-980℃, residence time ≥ 40min; B3, heating section temperature is 1080-1110, residence time ≥ 40min; B4, heating section temperature is 1150-1180℃, residence time ≥ 70min; B5, soaking section temperature is 1160-1200℃, residence time ≥ 30min; total time in the furnace ≥ 220min.
[0071] The total amount of billets heated per unit time by the multiple walking beam type continuous heating furnaces is N1, and the residence time of the billets in the multiple walking beam type continuous heating furnaces can be controlled by selecting the specifications of the billet thickness.
[0072] Double-stand rolling mill: the total amount of steel plates that can be rolled per unit time is N2;
[0073] The rolling process of the double-stand rolling mill is as follows: the steel biting speed of the roughing mill and the finishing mill are both ≥2.0m / s, and the acceleration is ≥1.5m / s 2The rolling speed of the roughing mill is 2-3 m / s, the rolling speed of the finishing mill is 3-6 m / s, the throwing distance of the roughing mill and the finishing mill is ≤1.0 m; the rolling force of the roughing mill and the finishing mill pass is ≥ the rated rolling force of the mill × 70%, or the torque of the roughing mill and the finishing mill pass is ≥ the rated torque of the mill × 70%; the number of passes of the roughing mill and the finishing mill are both odd, and there are no empty passes; an instant cooling device is used between the passes of the roughing mill and the finishing mill to cool the intermediate billet to reduce the waiting time; the thickness of the steel plate after rolling the 220 mm billet is 10-100 mm, the thickness of the steel plate after rolling the 320 mm billet is 30-160 mm, and the thickness of 90% of the steel plates after rolling is between 15 and 100 mm.
[0074] The intermediate billet is cooled by an instant cooling device between the roughing mill and the finishing mill. The cooling method is as follows: after the roughing mill is finished, the intermediate billet passes through the instant cooling system of the roughing mill at a speed of 0.5m / s to 5m / s. The instant cooling device of the roughing mill is 6400mm long and 3500mm wide, with 8 sets of headers on the upper and lower sides. During cooling, the instant cooling water pressure is 0.5MPa, the water volume of the upper header is 60 to 120m3 / h, the water volume of the lower header is 120 to 240m3 / h, and the lower-upper water ratio is ≥2; after cooling, the intermediate billet is transported to the instant cooling system of the finishing mill at a speed of 0.5m / s to 5m / s, and the intermediate billet is self-tempered during the transportation process. Before being transported to the instant cooling system of the finishing mill, the intermediate billet passes through the instant cooling system of the finishing mill at a speed of 0.5m / s to 5m / s. The instant cooling device of the finishing mill is 4800mm long and 3500mm wide, with 6 sets of headers on the upper and lower sides. During cooling, the instant cooling water pressure is 0.5MPa, and the water volume of the upper header is 60 to 120m 3 / h, the water volume of the lower header is 120~240m 3 / h, the lower and upper water ratio is ≥ 2. After the intermediate billet is cooled by the instant cooling device, the waiting time can be reduced and the rolling efficiency can be improved.
[0075] The above rolling process can reduce the rolling time of each pass, reduce the total number of billet rolling passes, reduce the idle time of the roughing mill and the finishing mill waiting for each other, and reduce the waiting time of the intermediate billet, thereby greatly improving the rolling rhythm and improving the rolling efficiency.
[0076] The relationship between N1 and N2 complies with the formula N2-2<N1<N2+3, so that the heating energy rhythm of multiple walking beam continuous heating furnaces matches the rolling rhythm of the double-stand rolling mill.
[0077] Example 2
[0078] Based on the scheme of Example 1, taking batches 1 to 18 as an example, the present invention can achieve maximum production efficiency by complying with the formula N2-2<N1<N2+3, so that the heating energy rhythm of multiple walking beam continuous heating furnaces is matched with the rolling rhythm of the double-stand rolling mill.
[0079] The feeding methods, billet thickness, heating furnace discharge amount N1 and double-stand rolling mill rolling amount N2 of two first stepping beam type continuous heating furnaces F1 and F2 and one second stepping beam type continuous heating furnace F3 are shown in Table 2.
[0080] Table 2 Heating furnace charging method, heating output and rolling mill rolling output
[0081]
[0082]
[0083] In batches 1 to 9, the relationship between the total heated output N1 and the total rolling amount N2 conforms to the formula N2-2<N1<N2+3. The heating capacity of the heating furnace matches the rolling capacity of the rolling mill, and the production efficiency of the production line is maximized.
[0084] In batches 10 to 12, the charging methods, billet thickness, heating furnace discharge amount N1 and double-stand rolling mill rolling amount N2 of F1, F2 and F3 are shown in Table 3.
[0085] Table 3 Heating furnace charging method, heating output and rolling mill rolling output
[0086]
[0087] In batches 10 to 12, the relationship between the output of the heating furnace N1 and the rolling output of the rolling mill N2 is N1<N2-2, which means that the heating capacity of the heating furnace is less than the rolling capacity of the rolling mill. The heating capacity of the heating furnace is insufficient, and the double-stand rolling mill needs to wait and be idle during the rolling process. The heating capacity of the heating furnace does not match the production capacity rhythm of the double-stand rolling mill.
[0088] In batches 13 to 18, the charging methods of F1, F2 and F3, the billet thickness, the heating furnace discharge amount N1 and the rolling amount N2 of the rolling mill are shown in Table 4.
[0089] Table 4 Heating furnace charging method, heating output and rolling mill rolling output
[0090]
[0091]
[0092] In batches 13 to 18, the relationship between the total output N1 of the heating furnace and the total rolling output N2 is N1>N2+3, which means that the heating capacity of the heating furnace is much greater than the rolling capacity of the double-stand rolling mill, and the heating furnace heats excessively, which does not match the rolling capacity of the double-stand rolling mill.
[0093] The embodiments described above are only used to illustrate the technical solutions of the present invention, rather than to limit them. Although the present invention has been described in detail with reference to the aforementioned embodiments, those skilled in the art should understand that the technical solutions described in the aforementioned embodiments may still be modified, or some of the technical features may be replaced by equivalents. Such modifications or replacements will not cause the essence of the corresponding technical solutions to deviate from the spirit and scope of the technical solutions of the various embodiments of the present invention.
Claims
1. A production allocation method for a medium and thick plate production line, comprising: S1, heating process; S2, rolling process, wherein: In the step S1, the total amount of the blank heated by the heating process in a unit time by multiple heating furnaces is N1; In the step S2, the total amount of steel plates that can be rolled by the double-stand rolling mill in a unit time is N2; It is characterized in that The relationship between N1 and N2 complies with the formula N2-2<N1<N2+3.
2. The production allocation method of a medium and thick plate production line according to claim 1, characterized in that: There are three heating furnaces, namely two first heating furnaces F1 and F2 and one second heating furnace F3. The first heating furnace is provided with two parallel walking beams; the second heating furnace is provided with three parallel walking beams; the total amount of blanks heated by the three heating furnaces per unit time is: <h2 style=";text-align:left;direction:ltr">N1=N<h2 style=";text-align:left;direction:ltr"> F1 <h2 style=";text-align:left;direction:ltr"> +N<h2 style=";text-align:left;direction:ltr"> F2 <h2 style=";text-align:left;direction:ltr"> +N<h2 style=";text-align:left;direction:ltr"> F3 <h2 style=";text-align:left;direction:ltr"> =(2A1+2A2+2n+m+A3) / t Wherein, A1 is the number of rows of billets in the first heating furnace F1, A2 is the number of rows of billets in the first heating furnace F2; A3 is the number of rows of billets in the second heating furnace F3; t is the heating time in hours; n is the number of rows in the second heating furnace of the a-type material distribution method, in which three blanks arranged side by side are fed in each time through three rows of walking beams; m is the number of rows in the second heating furnace of type b distribution method. Type b distribution method is to feed two side-by-side blanks each time through three rows of walking beams, and the length of at least one blank needs to be erected by two rows of walking beams.
3. The production allocation method of the medium and thick plate production line according to claim 2 is characterized in that: The blanks include two sizes of thickness: 220 mm or 320 mm.
4. The production allocation method of a medium and thick plate production line according to claim 3, characterized in that: The heating steps of the three heating furnaces in step S1 for the blank with a thickness of 320 mm include: H1, preheating temperature ≤ 950℃, residence time ≥ 60min; H2, heating section temperature is 950~980℃, residence time is ≥60min; H3, the temperature of the heating section is 1080~1110, and the residence time is ≥60min; H4, heating section temperature is 1150~1180℃, residence time is ≥90min; H5, the temperature of the soaking section is 1160~1200℃, and the residence time is ≥50min; Total time ≥320min; The heating steps for a billet thickness of 220 mm include: B1. Preheating temperature ≤ 950℃, residence time ≥ 40min; B2, the temperature of the heating section is 950~980℃, and the residence time is ≥40min; B3, the temperature of the heating section is 1080~1110, and the residence time is ≥40min; B4, the temperature of the heating section is 1150~1180℃, and the residence time is ≥70min; B5. The temperature of the soaking section is 1160~1200℃, and the residence time is ≥30min; Total time in the furnace ≥ 220min.
5. The production allocation method of a medium and thick plate production line according to claim 1, characterized in that: In the step S2, the double-stand rolling mill includes a roughing mill and a finishing mill, wherein the roughing mill and the finishing mill both have odd-numbered passes.
6. The production allocation method of a medium and thick plate production line according to claim 5, characterized in that: In the step S2, the rolling force of the roughing mill and the finishing mill passes is ≥ the rated rolling force×70%, or the torque of the roughing mill and the finishing mill passes is ≥ the rated torque×70%.
7. The production allocation method of a medium and thick plate production line according to claim 6, characterized in that: In the step S2, an instant cooling device is used to cool the intermediate billet between the roughing mill and the finishing mill.
8. The production allocation method of a medium and thick plate production line according to claim 7, characterized in that: In step S2, after the intermediate billet is finished at the roughing mill, the intermediate billet passes through the instant cooling system of the roughing mill. After cooling, the intermediate billet is transported to the instant cooling system of the finishing mill. During the transportation process, the intermediate billet is self-tempered and finally enters the instant cooling system of the roughing mill for further cooling.
Citation Information
Patent Citations
Thick steel plate and rolling method thereof
CN110280589A
Continuous heating furnace arrangement mode for thick plate production and steel pumping method through same
CN112575176A
Stepping type heating furnace with double movable supporting devices for fast-paced production and machining method of stepping type heating furnace
CN112595104A
Method and system for guiding production rhythm based on medium plate heating process
CN114921632A
Time-bitmap analysis method for rolling rhythm of medium plate
CN116174493A