Terahertz metasurface sensor applied to prochloraz detection and preparation method of terahertz metasurface sensor
By introducing ring dipole resonator arrays and graphene integrated designs into terahertz metasurface sensors, the problem of detection of low-concentration organic molecules in the existing technology is solved, and high-sensitivity pesticide residue detection is achieved, which promotes food safety and the environment The development of rapid testing.
Patent Information
- Application Number
- CN202411201769.X
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-29
- Publication Date
- 2024-12-06
AI Technical Summary
The prior art is complex and time-consuming to detect pesticide residues, making it difficult to achieve rapid detection of low-concentration organic molecules, especially in the rapid detection of food safety and environmental conditions.
Using terahertz metasurface sensors, including amethyst quartz glass base layer, lower polyimide dielectric layer, ring dipole array layer and graphene layer, ring dipole is constructed through micro-nano processing and graphene suspension transfer technology. Sub-resonator arrays to improve detection sensitivity and performance.
It has achieved high sensitivity detection of low-concentration organic molecules, promoted the popularization of pesticide residue detection technology, and improved the ability of food safety and rapid environmental detection.
Smart Images

Figure CN119086483A_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the field of terahertz technology, and in particular to a terahertz supersurface sensor used for prochloraz detection and a preparation method thereof. Background Art
[0002] The agricultural field widely uses the pesticide prochloraz to prevent diseases caused by ascomycetes and imperfect fungi on field crops, fruits and vegetables. However, the irregular use and abuse of pesticides lead to excessive pesticide residues, which endanger the health of consumers and aggravate environmental pollution. Therefore, accurate detection of pesticide residues has become an important task to ensure food safety. At present, common pesticide residue detection methods mainly include chromatographic techniques such as gas chromatography, gas chromatography-mass spectrometry, high performance liquid chromatography and liquid chromatography-mass spectrometry. Although these methods can detect trace amounts of residues, problems such as complex operation and long time consumption limit their application in rapid detection of pesticide residues.
[0003] Terahertz waves are electromagnetic waves with a frequency range of 0.1THz to 10THz, corresponding to wavelengths between 30μm and 3mm, between microwaves and infrared light in the electromagnetic spectrum. Terahertz wave photons have low energy and strong penetration into non-polar substances. Most molecules, especially organic molecules, have rotational and vibrational transitions in this frequency band, showing optical specificity, and therefore have great potential in food safety testing. However, natural materials in nature have weak electromagnetic responses in the terahertz frequency band, resulting in a "terahertz blank", which cannot meet the needs of high-sensitivity and rapid detection of low-concentration biochemical molecules. Traditional terahertz sensors based on metasurfaces only use biochemical molecules combined with electromagnetic metasurfaces to change the surface refractive index of the device, causing changes in the optical response and spectral information of the device, making it difficult to meet the needs of low-concentration organic molecule detection. Summary of the invention
[0004] In view of this, the present invention provides a terahertz metasurface sensor for the detection of prochloraz and a preparation method thereof, so as to improve the sensitivity and performance of sensor detection, realize the detection needs of low-concentration organic molecules, play a greater role in food safety and rapid environmental detection, and promote the popularization of pesticide residue detection technology.
[0005] In a first aspect, the present invention provides a terahertz metasurface sensor for detecting prochloraz, the terahertz metasurface sensor comprising:
[0006] Amethyst glass base layer;
[0007] a lower polyimide dielectric layer;
[0008] The ring dipole resonator array layer is generated by magnetron sputtering of a ring dipole resonator pattern, the array material is metal gold, and is grown on the upper surface of the lower polyimide dielectric layer;
[0009] An upper polyimide layer is disposed on the upper surface of the ring dipole resonator array layer;
[0010] The graphene layer is arranged on the upper surface of the upper polyimide layer.
[0011] In a second aspect, the present invention provides a method for preparing a terahertz supersurface sensor for detecting prochloraz, the method comprising:
[0012] Step 1, cleaning the purple quartz glass substrate;
[0013] Step 2: Coat a 10 μm thick layer of polyimide on the cleaned purple quartz glass substrate as a lower dielectric layer to provide basic support and insulation performance for the sample;
[0014] Step 3, coating a layer of AZ5214 photoresist on the lower polyimide dielectric layer by spin coating technology, and curing it by drying;
[0015] Step 4: using the prepared mask to expose the area coated on the surface of the photoresist to form the desired ring dipole resonator array structure pattern;
[0016] Step 5, placing the sample in a developer for development, and then drying it on a hot plate to remove unexposed photoresist;
[0017] Step 6: Using evaporation technology, a 200 nm thick layer of metal gold is evaporated on the surface of the AZ5214 photoresist that has been developed to form a ring dipole resonator array structure;
[0018] Step 7, immersing the prepared sample in an acetone solution to remove the photoresist with metal gold, thereby exposing the lower polyimide dielectric layer and the ring dipole resonator array layer;
[0019] Step 8, cutting the sample into a predetermined size of 1.35 cm×1.35 cm to obtain the required sample size;
[0020] Step 9, spin coating a 5 μm thick upper polyimide layer on the ring dipole resonator array layer;
[0021] Step 10: Transfer a layer of graphene onto the surface of the upper polyimide layer to form a desired multilayer structure.
[0022] Optionally, step 1 includes:
[0023] A 500 μm thick 4-inch purple quartz glass substrate was cleaned by ultrasonic cleaning with acetone and alcohol for 15 minutes each, and then rinsed with deionized water for 3-5 times to remove organic pollutants on the surface and ensure the cleanliness of the polished surface of the substrate.
[0024] Optionally, the step 2 includes:
[0025] A polyimide solution with a viscosity of 3600 centipoise is evenly coated on a cleaned purple quartz glass substrate by spin coating; after coating, a staged curing treatment is performed, first, the substrate is heated to 120°C and maintained for 1 hour, then the temperature is raised to 200°C and maintained for 1 hour, and then the temperature is further raised to 230°C and maintained for 1 hour; after completing these three stages of curing, the temperature is raised to 250°C and baked at 250°C for 2 hours; after curing is completed, the heating device is turned off and the sample is allowed to cool naturally to room temperature; after the sample is completely cooled, the cured polyimide coated substrate is taken out of the oven.
[0026] Optionally, step 3 includes:
[0027] A reverse photoresist AZ5214 with a thickness of 1 μm was spin-coated on the lower polyimide dielectric layer and then baked at 95° C. for 90 seconds.
[0028] Optionally, step 4 includes:
[0029] The purple quartz glass substrate was tightly fitted to the mask, the light intensity was set to 9.8, and the exposure time was 4.5 seconds; after the exposure was completed, reverse baking was performed at 110°C for 1 minute, and then exposure without a mask was performed for 45 seconds.
[0030] Optionally, step 5 includes:
[0031] The developer was used for development for 45 seconds. After development, the film was rinsed with deionized water for three times and dried with nitrogen gas.
[0032] Optionally, step 7 includes:
[0033] The sample with the metal layer evaporated was placed in an acetone solution for ultrasonication for 30 minutes, and then cleaned with isopropyl alcohol and deionized water.
[0034] Optionally, the step 10 includes:
[0035] Move graphene to the sensor surface in deionized water and air-dry it for 30 minutes. Then place the sensor on a baking tray, heat it to 100 degrees, and bake it for 30 minutes. Then take out the sensor and let it cool at room temperature for 5 minutes. Then soak the sensor in pure acetone for 10 minutes. Finally, replace it with clean pure acetone and soak it again for half an hour.
[0036] In the technical solution provided by the present invention, the terahertz supersurface sensor includes a purple quartz glass substrate layer; a lower polyimide dielectric layer; a ring dipole resonator array layer, which is generated by magnetron sputtering of a ring dipole resonant pattern, and the array material is metal gold, which is grown on the upper surface of the lower polyimide dielectric layer; an upper polyimide layer, which is arranged on the upper surface of the ring dipole resonator array layer; and a graphene layer, which is arranged on the upper surface of the upper polyimide layer. The terahertz supersurface sensor introduces a design scheme of integrating a ring dipole resonator array and graphene, adopts a micro-nano processing method to construct a ring dipole resonator array, and adopts a graphene suspension transfer technology, thereby improving the sensitivity and performance of sensor detection, meeting the needs of low-concentration organic molecule detection, playing a greater role in food safety and rapid environmental detection, and promoting the popularization of pesticide residue detection technology. BRIEF DESCRIPTION OF THE DRAWINGS
[0037] In order to more clearly illustrate the technical solutions of the embodiments of the present invention, the drawings required for use in the embodiments will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present invention. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative work.
[0038] Figure 1 A side schematic diagram of a terahertz metasurface sensor unit structure provided by an embodiment of the present invention;
[0039] Figure 2 A schematic top view of a terahertz metasurface sensor unit structure provided by an embodiment of the present invention;
[0040] Figure 3 A schematic diagram of an array arrangement of ring dipole resonators of a terahertz metasurface sensor provided by an embodiment of the present invention;
[0041] Figure 4 Transmission spectrum curves at different prochloraz concentrations provided by the embodiments of the present invention;
[0042] Figure 5 A graph showing changes in amplitude at the resonance frequency of a transmission spectrum at different prochloraz concentrations provided in an embodiment of the present invention;
[0043] Figure 6 A schematic diagram of the effective transmission area of the transmission spectrum at different prochloraz concentrations provided by an embodiment of the present invention;
[0044] Figure 7 A schematic diagram of effective transmission area of a transmission spectrum at different prochloraz concentrations provided by an embodiment of the present invention;
[0045] Figure 8A schematic diagram of the change in effective transmission area of a transmission spectrum at different prochloraz concentrations provided in an embodiment of the present invention.
[0046] Reference numerals:
[0047] 1-purple quartz glass substrate layer, 2-lower polyimide dielectric layer, 3-ring dipole resonator array layer, 4-upper polyimide layer, 5-graphene layer. DETAILED DESCRIPTION
[0048] In order to make the purpose, technical solution and advantages of the embodiments of the present invention clearer, the technical solution in the embodiments of the present invention will be clearly and completely described below in conjunction with the drawings in the embodiments of the present invention. Obviously, the described embodiments are part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0049] It should be clear that the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0050] The terms used in the embodiments of the present invention are only for the purpose of describing specific embodiments, and are not intended to limit the present invention. The singular forms "a", "said" and "the" used in the embodiments of the present invention are also intended to include plural forms, unless the context clearly indicates other meanings.
[0051] It should be understood that the term "and / or" used in this article is only a description of the association relationship of associated objects, indicating that there can be three relationships. For example, A and / or B can represent: A exists alone, A and B exist at the same time, and B exists alone. In addition, the character " / " in this article generally indicates that the associated objects before and after are in an "or" relationship.
[0052] The word "if" as used herein may be interpreted as "at the time of" or "when" or "in response to determining" or "in response to detecting", depending on the context. Similarly, the phrases "if it is determined" or "if (stated condition or event) is detected" may be interpreted as "when it is determined" or "in response to determining" or "when detecting (stated condition or event)" or "in response to detecting (stated condition or event)", depending on the context.
[0053] The present invention provides a terahertz supersurface sensor for detecting prochloraz, such as Figure 1 As shown, the terahertz metasurface sensor includes:
[0054] Amethyst glass substrate layer 1;
[0055] A lower polyimide dielectric layer 2;
[0056] The ring dipole resonator array layer 3 is generated by magnetron sputtering of a ring dipole resonator pattern, the array material is metal gold, and is grown on the upper surface of the lower polyimide dielectric layer 2;
[0057] An upper polyimide layer 4 is arranged on the upper surface of the ring dipole resonator array layer 3;
[0058] The graphene layer 5 is disposed on the upper surface of the upper polyimide layer 4 .
[0059] In the embodiment of the present invention, the lower polyimide layer 2 is used as the flexible substrate.
[0060] In the embodiment of the present invention, Figure 1 As shown, the terahertz metasurface sensor structure is divided into five layers: the first layer is a purple quartz glass substrate layer 1, above which is a lower polyimide dielectric layer 2, a ring dipole resonator array layer 3 is arranged on the upper surface of the lower polyimide dielectric layer 2, above which is an upper polyimide dielectric layer 4, and the top is a single-layer graphene layer 5. The thickness of the lower polyimide dielectric layer 2 is 10 μm, the ring dipole resonator array layer 3 is gold with a thickness of 200 nm, and a layer of graphene is transferred after a 5 μm thick upper polyimide layer is spin-coated on the upper surface of the ring dipole resonator array layer 3.
[0061] In the embodiment of the present invention, Figure 2 and Figure 3 As shown, the relevant parameters of the ring dipole resonator array layer 3 are as follows: Px=55μm, Py=27.5μm, the outer length of the resonator U-shaped metal structure x=30μm, the outer width of the resonator U-shaped metal structure 2y=40μm, the inner length of the resonator U-shaped metal structure q=25μm, the inner width of the resonator U-shaped metal structure p=30μm, the outer length of the resonator I-shaped metal structure 2w=28μm, the inner length of the resonator I-shaped metal structure n=12μm, and the gap between the resonator U-shaped metal structure and the I-shaped metal structure m=5μm.
[0062] The present invention provides a method for preparing a terahertz supersurface sensor for detecting prochloraz, the method comprising:
[0063] Step 1, cleaning the purple quartz glass substrate;
[0064] In the embodiment of the present invention, step 1 includes:
[0065] A 500 μm thick 4-inch purple quartz glass substrate was cleaned by ultrasonic cleaning with acetone and alcohol for 15 minutes each, and then rinsed with deionized water for 3-5 times to remove organic pollutants on the surface and ensure the cleanliness of the polished surface of the substrate.
[0066] Step 2: Coat a 10 μm thick layer of polyimide on the cleaned purple quartz glass substrate as a lower dielectric layer to provide basic support and insulation performance for the sample;
[0067] In the embodiment of the present invention, step 2 includes:
[0068] A polyimide solution with a viscosity of 3600 centipoise is evenly coated on a cleaned purple quartz glass substrate by spin coating; after coating, a staged curing treatment is performed, first, the substrate is heated to 120°C and maintained for 1 hour, then the temperature is raised to 200°C and maintained for 1 hour, and then the temperature is further raised to 230°C and maintained for 1 hour; after completing these three stages of curing, the temperature is raised to 250°C and baked at 250°C for 2 hours; after curing is completed, the heating device is turned off and the sample is allowed to cool naturally to room temperature; after the sample is completely cooled, the cured polyimide coated substrate is taken out of the oven.
[0069] Step 3, coating a layer of AZ5214 photoresist on the lower polyimide dielectric layer by spin coating technology, and curing it by drying;
[0070] In the embodiment of the present invention, step 3 includes:
[0071] A reverse photoresist AZ5214 with a thickness of 1 μm was spin-coated on the lower polyimide dielectric layer and then baked at 95° C. for 90 seconds.
[0072] Step 4: using the prepared mask to expose the area coated on the surface of the photoresist to form the desired ring dipole resonator array structure pattern;
[0073] In the embodiment of the present invention, step 4 includes:
[0074] The purple quartz glass substrate was tightly fitted to the mask, the light intensity was set to 9.8, and the exposure time was 4.5 seconds; after the exposure was completed, reverse baking was performed at 110°C for 1 minute, and then exposure without a mask was performed for 45 seconds.
[0075] Step 5, placing the sample in a developer for development, and then drying it on a hot plate to remove unexposed photoresist;
[0076] In the embodiment of the present invention, step 5 includes:
[0077] The developer was used for development for 45 seconds. After development, the film was rinsed with deionized water for three times and dried with nitrogen gas.
[0078] Step 6: Using evaporation technology, a 200 nm thick layer of metal gold is evaporated on the surface of the AZ5214 photoresist that has been developed to form a ring dipole resonator array structure;
[0079] Step 7, immersing the prepared sample in an acetone solution to remove the photoresist with metal gold, thereby exposing the lower polyimide dielectric layer and the ring dipole resonator array layer;
[0080] In the embodiment of the present invention, step 7 includes:
[0081] The sample with the metal layer evaporated was placed in an acetone solution for ultrasonication for 30 minutes, and then cleaned with isopropyl alcohol and deionized water.
[0082] Step 8, cutting the sample into a predetermined size of 1.35 cm×1.35 cm to obtain the required sample size;
[0083] Step 9, spin coating a 5 μm thick upper polyimide layer on the ring dipole resonator array layer;
[0084] Step 10: Transfer a layer of graphene onto the surface of the upper polyimide layer to form a desired multilayer structure.
[0085] In the embodiment of the present invention, step 10 includes:
[0086] Move graphene to the sensor surface in deionized water and air-dry it for 30 minutes. Then place the sensor on a baking tray, heat it to 100 degrees, and bake it for 30 minutes. Then take out the sensor and let it cool at room temperature for 5 minutes. Then soak the sensor in pure acetone for 10 minutes. Finally, replace it with clean pure acetone and soak it again for half an hour.
[0087] In the present invention, the prepared terahertz metasurface sensor for prochloraz detection generates a ring dipole resonance response when reacted with terahertz waves, a prochloraz solution is dripped onto the sensor surface using a pipette, and after it is dried at room temperature, a terahertz time-domain spectroscopy system is used to measure the transmission spectrum of the device, and the above steps are repeated to obtain the transmission spectrum of the sensor when different prochloraz solution concentrations are dripped. Figure 4 As shown in FIG. 1 , after adding prochloraz solution of different concentrations, the transmission spectrum of the terahertz metasurface sensor of this example is obtained using a terahertz time-domain spectrometer. Figure 4 It can be seen that the resonance peak at 1.02THz gradually increases with the increase of prochloraz concentration. Figure 5As shown in the peak change curve at the resonance frequency of 1.02THz (i.e. f1), when the concentration of prochloraz is 100pg / ml, 300pg / ml, 500pg / ml, 700pg / ml and 800pg / ml, the transmission peak amplitude changes are 25.90%, 27.55%, 29.32%, 31.30% and 32.07% respectively. Figure 5 , Figure 6 , Figure 7 and Figure 8 They are respectively the peak change curve at frequency f1, the effective transmission region and its area, and the effective transmission area change curve. When the concentrations of prochloraz are 100pg / ml, 300pg / ml, 500pg / ml, 700pg / ml and 800pg / ml, the effective transmission areas are 9.41, 10.13, 10.52, 10.98, 11.45 and 11.66, respectively. The above data show that the concentration of prochloraz changes linearly with the peak value of the transmission spectrum and the effective transmission area. It can be seen that by changing the concentration of the added prochloraz solution, the Fermi level of CVD graphene moves to the Dirac point, the ring dipole resonance intensity is enhanced, thereby improving the detection performance of the sensor and realizing ultra-sensitive detection of THz biochemical sensors.
[0088] In an embodiment of the present invention, the detection method adopted is to drip a solution of prochloraz onto the upper surface of a graphene layer and detect the transmission spectrum of the device. The detection parameter is the increase or decrease in the amplitude of the sensor transmission spectrum to which prochloraz of different concentrations is dripped. A biochemical sensor dripped with prochloraz of different concentrations is placed at the detection position of a spectrometer. During the detection process, a terahertz beam is incident from the transmitting end of the instrument, passes through the graphene layer of the sensor, and then is emitted from the purple quartz substrate layer, and is finally received by the detection end. By recording the change of the terahertz beam from the incident to the emitted one, a transmission spectrum can be obtained. The transmission spectrum contains the transmission intensity and phase change information of the terahertz beam under the influence of different concentrations of prochloraz.
[0089] The terahertz supersurface sensor designed by the present invention can be used to measure the concentration of prochloraz, and the detection process includes:
[0090] (1) Different concentrations of prochloraz solution were dripped onto the graphene layer of the terahertz metasurface sensor, with the dripping concentrations being 100 pg / ml, 300 pg / ml, 500 pg / ml, 700 pg / ml and 800 pg / ml respectively. After being fully dried, the transmission spectrum of the biochemical sensor was detected using a terahertz time-domain spectrometer. The terahertz beam was first incident from the graphene layer dripped with different concentrations of prochloraz, and then emitted from the quartz substrate. Figure 4 As shown, the transmission spectrum change curve of prochloraz concentration detected in a nitrogen environment at room temperature (humidity less than 4%).
[0091] (2) Figure 5The change of the transmission spectrum peak under different prochloraz concentrations is shown. Among the four prochloraz samples with different concentrations, the different prochloraz concentrations and the transmission spectrum peak show a linear change law of y=0.0001046x+0.2407.
[0092] (3) Figure 7 The effective transmission area under different myclobutanil concentrations was shown. The effective transmission areas of six myclobutanil samples with different concentrations were 9.49, 10.13, 10.52, 10.98, 11.45 and 11.66, respectively. With the increase of the concentration of myclobutanil solution, the effective transmission area of the biochemical sensor showed a linear increase trend.
[0093] (4) Figure 8 The change of effective transmission area under different myclobutanil concentrations is shown. The effective transmission area of six myclobutanil samples with different concentrations shows a linear change of y=0.002581x+9.659.
[0094] The transmission spectrum of the biochemical sensor with different concentrations of prochloraz was detected by using a terahertz time-domain spectrometer. During the detection process, the terahertz beam incident from the graphene layer with different concentrations of prochloraz and then emitted from the purple quartz substrate layer was detected to obtain the transmission spectrum of the biochemical sensor for prochloraz concentration detection. In the THz frequency band, the electromagnetic wave and the terahertz sensor produce a ring dipole resonance response. When the concentration of the prochloraz solution is changed, the Fermi level of the CVD graphene moves to the Dirac point, and the ring dipole resonance intensity is enhanced. The transmission spectrum of the terahertz sensor is detected by a THz time-domain spectrometer to achieve label-free and highly sensitive detection of picogram-level prochloraz concentrations.
[0095] By transferring graphene onto the ring dipole resonator array structure, the highly sensitive ring dipole resonance response characteristics of the metasurface are combined with the property that the initial Fermi level of graphene slightly deviates from the Dirac point, thus preparing a highly sensitive terahertz metasurface biochemical sensor.
[0096] In the embodiment of the present invention, the sample type detected is prochloraz. The prepared prochloraz solutions of different concentrations are respectively dripped on the metasurface ring dipole resonator array to which the monolayer graphene has been transferred. When dripping, ensure that the dripping amount of each solution is equal and the droplets are evenly distributed on the sensor surface to ensure the accuracy and repeatability of subsequent detection.
[0097] The present invention adopts a micro-nano processing method to construct a ring dipole resonator array, and adopts a graphene suspension transfer technology to prepare a terahertz supersurface biochemical sensor. In combination with a terahertz time-domain spectroscopy system, the transmission spectrum of the device is detected and analyzed, thereby achieving ultra-sensitive detection of picogram-level prochloraz substances.
[0098] Focusing on the ultra-sensitive and rapid detection of trace-level organic molecules based on electromagnetic metasurface terahertz sensors, on the one hand, a metasurface sensor with a strong electromagnetic resonance response is designed. The ring dipole resonance response describes the specific frequency response phenomenon of the electric dipole in the ring structure. When the ring dipole is near its resonance frequency, its absorption or radiation efficiency increases significantly, forming an obvious frequency peak or valley. On the other hand, as a single-atom-layer two-dimensional optoelectronic material, graphene has a Brillouin zone K and K′ points in the band structure composed of two conical energy bands with linear dispersion relations, and the equivalent dielectric constant and equivalent magnetic permeability at the central intersection Dirac point are both zero. However, the initial Fermi level of graphene prepared by chemical vapor deposition (CVD) is slightly deviated from the Dirac point and is in the valence band (p-type doping). Only very weak external stimulation is needed to move the initial Fermi level from the valence band to the Dirac point. Therefore, by utilizing the unique Dirac point characteristics of CVD graphene and integrating graphene with electromagnetic metasurfaces, terahertz sensors for high-sensitivity detection of trace-level organic molecules are prepared, which can play a greater role in food safety and rapid environmental detection and promote the popularization of pesticide residue detection technology.
[0099] In the technical solution provided by the present invention, the terahertz supersurface sensor includes a purple quartz glass substrate layer; a lower polyimide dielectric layer; a ring dipole resonator array layer, which is generated by magnetron sputtering of a ring dipole resonant pattern, and the array material is metal gold, which is grown on the upper surface of the lower polyimide dielectric layer; an upper polyimide layer, which is arranged on the upper surface of the ring dipole resonator array layer; and a graphene layer, which is arranged on the upper surface of the upper polyimide layer. The terahertz supersurface sensor introduces a design scheme of integrating a ring dipole resonator array and graphene, adopts a micro-nano processing method to construct a ring dipole resonator array, and adopts a graphene suspension transfer technology, thereby improving the sensitivity and performance of sensor detection, meeting the needs of low-concentration organic molecule detection, playing a greater role in food safety and rapid environmental detection, and promoting the popularization of pesticide residue detection technology.
[0100] Those skilled in the art can clearly understand that, for the convenience and brevity of description, the specific working processes of the systems, devices and units described above can refer to the corresponding processes in the aforementioned method embodiments and will not be repeated here.
[0101] The above description is only a preferred embodiment of the present invention and is not intended to limit the present invention. Any modifications, equivalent substitutions, improvements, etc. made within the spirit and principles of the present invention should be included in the scope of protection of the present invention.
Claims
1. A terahertz metasurface sensor for detecting prochloraz, characterized in that: The terahertz metasurface sensor comprises: Amethyst glass substrate (1); A lower polyimide dielectric layer (2); A ring dipole resonator array layer (3), which is generated by magnetron sputtering of a ring dipole resonator pattern, and the array material is metal gold, and is grown on the upper surface of the lower polyimide dielectric layer (2); An upper polyimide layer (4) is arranged on the upper surface of the ring dipole resonator array layer (3); The graphene layer (5) is arranged on the upper surface of the upper polyimide layer (4).
2. A method for preparing a terahertz supersurface sensor for prochloraz detection, characterized in that: The method comprises: Step 1, cleaning the purple quartz glass substrate; Step 2: Coat a 10 μm thick layer of polyimide on the cleaned purple quartz glass substrate as a lower dielectric layer to provide basic support and insulation performance for the sample; Step 3, coating a layer of AZ5214 photoresist on the lower polyimide dielectric layer by spin coating technology, and curing it by drying; Step 4: using the prepared mask to expose the area coated on the surface of the photoresist to form the desired ring dipole resonator array structure pattern; Step 5, placing the sample in a developer for development, and then drying it on a hot plate to remove unexposed photoresist; Step 6: Using evaporation technology, a 200 nm thick layer of metal gold is evaporated on the surface of the AZ5214 photoresist that has been developed to form a ring dipole resonator array structure; Step 7, immersing the prepared sample in an acetone solution to remove the photoresist with metal gold, thereby exposing the lower polyimide dielectric layer and the ring dipole resonator array layer; Step 8, cutting the sample into a predetermined size of 1.35 cm×1.35 cm to obtain the required sample size; Step 9, spin coating a 5 μm thick upper polyimide layer on the ring dipole resonator array layer; Step 10: Transfer a layer of graphene onto the surface of the upper polyimide layer to form a desired multilayer structure.
3. The method according to claim 2, characterized in that The step 1 comprises: A 500 μm thick 4-inch purple quartz glass substrate was cleaned by ultrasonic cleaning with acetone and alcohol for 15 minutes each, and then rinsed with deionized water for 3-5 times to remove organic pollutants on the surface and ensure the cleanliness of the polished surface of the substrate.
4. The method according to claim 2, characterized in that: The step 2 comprises: A polyimide solution with a viscosity of 3600 centipoise is evenly coated on a cleaned purple quartz glass substrate by spin coating; after coating, a staged curing treatment is performed, first, the substrate is heated to 120°C and maintained for 1 hour, then the temperature is raised to 200°C and maintained for 1 hour, and then the temperature is further raised to 230°C and maintained for 1 hour; after completing these three stages of curing, the temperature is raised to 250°C and baked at 250°C for 2 hours; after curing is completed, the heating device is turned off and the sample is allowed to cool naturally to room temperature; after the sample is completely cooled, the cured polyimide coated substrate is taken out of the oven.
5. The method according to claim 2, characterized in that: The step 3 comprises: A reverse photoresist AZ5214 with a thickness of 1 μm was spin-coated on the lower polyimide dielectric layer and then baked at 95° C. for 90 seconds.
6. The method according to claim 2, characterized in that The step 4 comprises: The purple quartz glass substrate was tightly fitted to the mask, the light intensity was set to 9.8, and the exposure time was 4.5 seconds; after the exposure was completed, reverse baking was performed at 110°C for 1 minute, and then exposure without a mask was performed for 45 seconds.
7. The method according to claim 2, characterized in that The step 5 comprises: The developer was used for development for 45 seconds. After development, the film was rinsed with deionized water for three times and dried with nitrogen gas.
8. The method according to claim 2, characterized in that: The step 7 comprises: The sample with the metal layer evaporated was placed in an acetone solution for ultrasonication for 30 minutes, and then cleaned with isopropyl alcohol and deionized water.
9. The method according to claim 2, characterized in that: The step 10 comprises: Transfer graphene to the sensor surface in deionized water and air-dry it for 30 minutes. Then place the sensor on a baking tray, heat it to 100 degrees, and bake it for 30 minutes. Then take out the sensor and let it cool at room temperature for 5 minutes. Then soak the sensor in pure acetone for 10 minutes. Finally, replace it with clean pure acetone and soak it again for half an hour.
Citation Information
Patent Citations
Metasurface sensor and preparation method and application thereof
CN117589712A
Rugby-shaped terahertz biochemical sensor based on graphene and preparation method of rugby-shaped terahertz biochemical sensor
CN119086482A
Cited By
Graphene terahertz metasurface sensor and application thereof in pesticide residue detection
CN121324302A
Graphene terahertz metasurface sensor and its application in pesticide residue detection
CN121324302B