How to recycle waste

LAP113AUndetermined Publication Date: 2025-09-19QIHUI LIAN
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
LAP113
Authority / Receiving Office
LA · LA
Patent Type
Applications
Current Assignee / Owner
Priority Date
2007-07-25
Filing Date
2008-07-21
Publication Date
2025-09-19

AI Technical Summary

Technical Problem

Existing domestic waste treatment methods cannot effectively solve the pollution problems of soil, water and atmosphere, and it is difficult to achieve complete recycling and resource treatment of waste, resulting in environmental pollution and economic losses.

Method used

Through steps such as drying, classification, crushing, high-pressure molding, and high-temperature carbonization or firing, the garbage is converted into charcoal or building bricks to achieve complete recycling of garbage, reduce environmental pollution, and generate economic value.

Benefits of technology

It achieves the thorough recycling of domestic waste, reduces environmental pollution, reduces processing costs, and converts waste into fuel or building materials with economic value.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure 00000000_0000_ABST
    Figure 00000000_0000_ABST
  • Figure 00000000_0001_ABST
    Figure 00000000_0001_ABST
Patent Text Reader

Abstract

The recycling method of waste disposal consists of the following steps: separating, crushing, drying, high-pressure pressing and shaping, making charcoal and burning waste that cannot be burned at high temperatures, and then cooling it to obtain bricks and boards for construction. This method can reuse waste. This method can make bricks and boards for construction. This method is simple and low-cost.
Need to check novelty before this filing date? Find Prior Art

Description

[0001] Methods for the complete recycling of solid waste

[0002] Technical Field

[0003] This invention relates to a method for treating municipal solid waste, and more particularly to a method for treating solid waste that can be completely recycled, belonging to the field of environmental protection technology.

[0004] Background Technology

[0005] Municipal solid waste is not only a major public nuisance jeopardizing sustainable socio-economic development, but also the only potential resource on Earth that is increasing. How to scientifically and effectively treat municipal solid waste that pollutes soil, water, and air, damages environmental quality, and harms human health, and how to rationally utilize recyclable or renewable resources within the waste to achieve the goals of reducing, rendering harmless, and recycling municipal solid waste, are key environmental issues of great concern and research worldwide. To protect the human living environment and ecological environment, waste management is becoming increasingly important. In recent years, with rapid economic development and the improvement of people's material and cultural living standards, municipal solid waste has undergone significant changes in both quality and quantity. In the past, waste mainly consisted of food and organic waste, but now it includes a large amount of paper and difficult-to-decompose plastic products. Currently, the main methods for municipal solid waste treatment include landfill, incineration, and recycling. The disadvantages of landfilling are that it involves piling up, crushing, burying, and covering garbage, which requires a large amount of land. Since plastic waste accounts for a large proportion of various urban household waste and cannot decompose for many years, land that has been landfilled generally cannot be used as arable land. Incineration extracts heat energy, but the residual waste after combustion must be treated. Recycling is a more ideal waste treatment method, such as generating biogas from household waste or making fertilizer through composting, but it still produces residual waste, which can easily cause secondary pollution of the environment in the long run, damaging the quality of the ecological environment and human health.

[0006] Summary of the Invention

[0007] The purpose of this invention is to provide a method for treating solid waste that can completely recycle and utilize waste, protect the human living environment, resolve the contradiction between human life and survival, effectively treat household waste, process solid waste into useful materials, turn waste into raw materials to produce and sell goods, thus turning waste into treasure, and both protecting the environment and obtaining economic benefits.

[0008] The objective of this invention is achieved through the following main steps:

[0009] (1) Drying: The waste is dried separately;

[0010] (2) High-pressure molding: The waste is pressed into blocks of various shapes under high pressure; (3) High-temperature carbonization or firing: The combustible part of the waste is carbonized at high temperature to form coal, and the non-combustible part of the waste is fired at high temperature to form bricks or boards for building. After cooling, the finished product is obtained.

[0011] A further improvement of the invention is that the waste is dehydrated before any of the steps of sorting, crushing, or drying.

[0012] Another improvement of the present invention is that the method for treating municipal solid waste involves high-pressure molding of the waste while simultaneously heating it at high temperature.

[0013] The drying temperature is 100-500°C, and the drying time is 0.5-30 minutes.

[0014] The high-pressure condition mentioned is a pressure of 1 cm. 2 The pressure is 1-30 kg and the temperature is 100-500°C.

[0015] The high-temperature carbonization temperature is 300-300°C, and the time is 5 seconds to 18 minutes.

[0016] The high-temperature firing temperature is 700-1200°C, and the time is 1-10 hours.

[0017] The objective of this invention can be achieved through the following main steps:

[0018] (1) Classification: Separate the waste into combustible and non-combustible parts;

[0019] (2) Crushing: The waste is crushed separately using a crusher;

[0020] (3) Drying: Dry the waste separately;

[0021] (4) High-pressure molding: The waste is compressed into blocks of various shapes under high pressure;

[0022] (5) High-temperature carbonization or firing: The combustible part of the waste is carbonized at high temperature to form coal, and the non-combustible part of the waste is fired at high temperature to form bricks or boards for building. The finished product is obtained after cooling.

[0023] The objective of this invention can also be achieved in the following main steps: (1) Classification: The waste is divided into combustible and non-combustible parts;

[0024] (2) Crushing: The two types of waste are placed in a crusher for crushing;

[0025] (3) High-pressure molding: The waste is pressed into blocks of various shapes under high pressure;

[0026] (4) High-temperature carbonization or firing: The combustible part of the waste is carbonized at high temperature to form coal, and the non-combustible part of the waste is fired at high temperature to form bricks or boards for building. The finished product is obtained after cooling.

[0027] The high-pressure condition mentioned is a pressure of 1 cm. 2 The pressure is 1-30 kg; the high-temperature carbonization temperature is 300-1300 °C, and the time is 5 seconds to 18 minutes; the high-temperature firing temperature is 700-1200 °C, and the time is 1-10 hours.

[0028] The advantages of this invention are: by completely converting household waste into coal or building bricks or boards for reuse, it achieves thorough recycling of household waste, especially its solid components, thus solving environmental pollution. Simultaneously, it transforms waste into economically valuable fuel or building materials, with fewer steps, a simpler process, and easily manufactured equipment, resulting in lower processing costs. Detailed Implementation

[0029] Example 1

[0030] In this invention, the waste is dried using an oven at 500°C for 0.5 minutes. Alternatively, it can be dried using sunlight or other drying equipment. The drying time decreases as the temperature increases. Under high temperature and high pressure conditions, the pressure is 1 cm. 2 (Referring to cross-sectional area), pressure is 10 kg, temperature is 300°C, and the higher the pressure, the better the quality. A press is used to compress waste into various shapes, such as cubes, cakes, or strips. This is because high-temperature heating is used, with a temperature of 300°C and a pressure of 1 cm. 2The weight is 10 kg because combustible waste is quite sticky, and this is to prevent the waste from sticking to the press (non-combustible waste can also be processed in the same way; due to its low stickiness, high-temperature conditions are not required during molding, only high-temperature firing is needed). Finally, the formed blocky waste is carbonized at 450°C for 6 minutes to form charcoal. The higher the carbonization temperature, the shorter the time required. The required temperature and carbonization time vary depending on the composition of the waste and the thickness of the product. After cooling, coal blocks, briquettes, or coal of different shapes that can be used as fuel are obtained. The resulting charcoal has good combustibility, high calorific value, and low sulfide content, significantly reducing air pollution compared to ordinary coal.

[0031] Example 2

[0032] In this invention, the first step is to classify the collected household waste, separating it into combustible and non-combustible components manually or mechanically. At this stage, high-value metal waste should be separated for sale. The combustible waste is then dehydrated using a dehydrator. Next, the waste is pulverized into granules, preferably powder, using a shredder. The waste is then dried in an oven at 100°C for 30 minutes. Alternatively, it can be dried using sunlight or other drying equipment. The drying time decreases as the temperature increases. Under high temperature and pressure conditions, the drying time is reduced per 1 cm³. 2 (Referring to cross-sectional area) The pressure is 1 kg, the temperature is 100°C, and the garbage is pressed into various shapes of blocks, such as cubes, cakes, or strips, using a press. The reason for this high-temperature heating is 100°C, per 1 cm³. 2 The pressure is 1 kg. Due to the high viscosity of combustible waste, this is to prevent the waste from sticking to the press. Finally, the formed lumps of waste are carbonized at 300°C for 18 minutes to form charcoal. The higher the carbonization temperature, the shorter the time required. Furthermore, the required temperature and carbonization time vary depending on the composition of the waste and the thickness of the product. After cooling, coal lumps, briquettes, or coal of different shapes suitable for fuel are obtained. The resulting charcoal has good combustibility, high calorific value, and low sulfide content, significantly reducing air pollution compared to ordinary coal.

[0033] Example 3

[0034] The waste treatment method of this invention first involves classifying the collected household waste, and then sorting the waste manually or mechanically. The waste is sorted into combustible and non-combustible components. At this stage, high-value metal waste should be separated and sold. The combustible waste is then dehydrated using a dehydrator, followed by pulverization using a crusher until it becomes granular, preferably powdered. The waste is then dried in an oven at 500°C for 0.5 minutes. Alternatively, it can be dried using sunlight or other drying equipment. The drying time decreases with increasing temperature. Under high temperature and pressure conditions, the drying time per 1 cm³... 2 (Referring to cross-sectional area) The pressure is 30 kg, and the temperature is 50°C. Higher pressure results in better quality. The waste is pressed into various shapes, such as cubes, cakes, or strips, using a press. High-temperature heating is used here, at 500°C, per 1 cm³... 2 The pressure is 30 kg because the combustible waste is quite sticky, and this is to prevent the waste from sticking to the press. Finally, the formed lumps of waste are carbonized at a high temperature of 1300°C for 5 seconds to form charcoal. The higher the carbonization temperature, the shorter the time required. Furthermore, the required temperature and carbonization time vary depending on the composition of the waste and the thickness of the product. After cooling, coal lumps, briquettes, or coal of different shapes that can be used as fuel are obtained. The resulting charcoal has good combustibility, high calorific value, and low sulfide content, significantly reducing air pollution compared to ordinary coal.

[0035] Example 4

[0036] This invention begins by sorting collected household waste into combustible and non-combustible components, either manually or mechanically. High-value metal waste is prioritized for sale. The combustible waste is then dehydrated using a dehydrator, followed by pulverization using a crusher to produce granules, preferably powder. The waste is then dried using an oven, or alternatively, through sunlight or other drying equipment. Finally, under high temperature and pressure conditions, each 1 cm³ of waste is dried... 2 (Referring to cross-sectional area) The pressure is 20 kg, and the temperature is 35°C. Higher pressure results in better quality. The waste is pressed into various shapes, such as cubes, discs, or strips, using a press. High-temperature heating is used here, at 350°C, with a pressure of 1 cm³. 2The initial weight is 20 kg, chosen because the combustible waste is quite sticky, and this is to prevent the waste from sticking to the press. Finally, the formed lumps of waste are carbonized at 650°C for 9 minutes to form charcoal. The higher the carbonization temperature, the shorter the time required. Furthermore, the required temperature and carbonization time vary depending on the composition of the waste and the thickness of the product. After cooling, coal lumps, briquettes, or coal of different shapes can be obtained for fuel. The resulting charcoal has good combustibility, high calorific value, and low sulfide content, significantly reducing air pollution compared to ordinary coal.

[0037] Example 5

[0038] This embodiment describes the treatment of non-combustible waste. The sorting, dehydration, crushing, and drying steps are the same as in embodiments two, three, and four, except that the particle size doesn't necessarily need to be as fine during crushing. Then, during high-pressure molding, because the non-combustible waste has low viscosity, clay is added to increase its viscosity. The waste is then compressed under high pressure using a press. Various shapes of blocky materials, such as squares, plates, or columns, can be formed without high-temperature conditions. Finally, the formed blocky waste is fired at a high temperature of 700°C for 10 hours to sinter it into building materials with sufficient hardness and strength. After cooling, bricks or boards that can be used for construction can be obtained.

[0039] Example 6

[0040] This embodiment describes the treatment of non-combustible waste. The sorting, dehydration, crushing, and drying steps are the same as in embodiments two, three, and four, except that the particle size does not necessarily need to be as fine during crushing. Then, during high-pressure molding, since the non-combustible waste has low viscosity, clay is added to increase its viscosity. The waste is then pressed into various shapes of blocks, such as cubes, plates, or columns, using a high-pressure press. High-temperature molding is not required. Finally, the formed blocks are fired at 1200°C for one hour to sinter them into building materials with sufficient hardness and strength. After cooling, bricks or slabs suitable for construction are obtained.

[0041] Example 7

[0042] This embodiment describes the treatment of non-combustible waste. The sorting, dehydration, crushing, and drying steps are the same as in embodiments two, three, and four, except that the particle size doesn't necessarily need to be as fine during crushing. Then, during high-pressure molding, because the non-combustible waste has low viscosity, clay is added to increase its viscosity. The waste is then pressed into blocks of various shapes using a high-pressure press.

Claims

Claims 1. A method for the complete recycling of solid waste, characterized in that... The process includes the following steps: (1) Drying: Dry the waste separately; (2) High-pressure molding: The waste is pressed into blocks of various shapes under high pressure; (3) High-temperature carbonization or firing: The combustible part of the waste is carbonized at high temperature to form coal, and the non-combustible part of the waste is fired at high temperature to form bricks or boards for building. The finished product is obtained after cooling.

2. The processing method according to claim 1, characterized in that... It also includes the following steps - (1) Sorting: Separating the waste into combustible and non-combustible parts; (2) Crushing: The two types of waste are placed in a crusher for crushing.

3. The processing method according to claim 1 or 2, characterized in that, The waste is also dehydrated before any of the steps of sorting, crushing, or drying.

4. The processing method according to claim 1, 2, or 3, characterized in that, The waste is subjected to high-pressure molding and high-temperature heating at the same time.

5. The processing method according to claim 1, characterized in that, The drying process, wherein the drying temperature is 100~ 500 °C, for 0.5 to 30 minutes.

6. The processing method according to claim 4, characterized in that, The high-pressure conditions are: pressure 1 cm2, pressure 1-30 kg, and temperature 100-500°C.

7. The processing method according to claim 1, characterized in that, The high-temperature carbonization temperature is 300-1300°C, and the time is 5 seconds to 18 minutes.

8. The processing method according to claim 1, characterized in that, The high-temperature firing temperature is 700-1200 °C, and the time is 1-10 hours.

9. A method for the complete recycling of solid waste, characterized in that... The steps include: (1) Sorting: Separating the waste into combustible and non-combustible parts; (2) Crushing: The waste is crushed separately using a crusher; (3) High-pressure molding: The waste is pressed into blocks of various shapes under high pressure conditions; (4) High-temperature carbonization or firing: The combustible part of the waste is carbonized at high temperature to form coal, and the non-combustible part of the waste is fired at high temperature to form bricks or boards for building. The finished product is obtained after cooling.

10. The processing method according to claim 9, characterized in that: The high-pressure condition is a pressure of 1 cm2, and the pressure is 1-30 kg; the high-temperature carbonization temperature is 300-1300°C, and the time is 5 seconds to 18 minutes; the high-temperature firing temperature is 700-1200°C, and the time is 1-10 hours.