A micro-nano fiber, electrospinning technology, applied in spinning solution preparation, fiber processing, textiles and papermaking, etc., can solve the problem that it is difficult to use conventional surgical dressing and treatment methods, wound peripheral protection does not play a good role, and Unable to effectively control wound infection and other problems, to achieve the effect of convenient dressing change, convenient observation of wound condition, and good biocompatibility
Patent Information
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Publication Date
- 2013-03-13
- Estimated Expiration
- Not applicable · inactive patent
Abstract
Description
Technical field:
[0001] The invention belongs to the technical field of electrospinning, and relates to the application of a novel portable hand-held electrospinning device, a new process for preparing a fiber film capable of covering injured skin wounds by using electrospinning technology, in particular to an electrospinning process A method for preparing micro-nano fiber film by silk method. Background technique:
[0002] At present, burns or skin injuries are common accidental traumas that seriously endanger human health. People are threatened by fires and traffic accidents from nature and humans all the time. Especially with the development of science, People's daily life and production are surrounded by combustible materials. The fire hazard is very serious. Burn patients are often scarred and unrecognizable. In severe cases, they will cause permanent disabilities or even life-threatening; Necrosis, vascular embolism, and poor local blood supply cannot effectively cont...
Examples
Embodiment
[0012] This embodiment includes three process steps of spinning solution preparation, spinning device installation and electrospinning micro-nano fiber film:
[0013] Spinning solution preparation: The prepared spinning solution is an ethanol solution of polyvinylpyrrolidone (PVP, molecular weight 1.3 million) mixed with epidermal growth factor (epidermal growth factor, EGF) with a mass fraction of 13 wt%. Mix 1.3 grams of polyvinylpyrrolidone (PVP) powder with 8.7 grams of absolute ethanol, then add 0.02 grams of epidermal growth factor (EGF), and stir magnetically at room temperature for 2 hours to fully disperse the EGF and then let it stand for 0.5 hours to obtain a uniform A precursor electrospinning solution for transparent electrospinning;
[0014] Spinning device installation: extract the prepared electrospinning solution with a sterilized injection needle in a sterile room, then install the needle on the syringe as a spinning nozzle, and then install the syringe on a ...