Technology for preparing potash fertilizer from potassium feldspar-decomposed mother liquor employing adsorption method

A technology for decomposing mother liquor and potassium feldspar, applied in the directions of potash fertilizer, inorganic fertilizer, fertilization device, etc., can solve the problems of inability to obtain industrial application, limitation of development and utilization of potassium feldspar, and high process energy consumption, and achieves low production cost, The effect of reducing energy consumption and shortening the process flow

CN103864472AInactive Publication Date: 2014-06-18CHANGSHA DESIGN & RES INST OF CHEM IND MIN
7 Cites 0 Cited by

Patent Information

Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Publication Date
2014-06-18
Estimated Expiration
Not applicable · inactive patent
Patent Text Reader

Abstract

The invention discloses a technology for preparing a potash fertilizer from potassium feldspar-decomposed mother liquor employing an adsorption method. The technology comprises the following steps: (1) grinding the potassium feldspar into -100 to -400 meshes; (2) evenly mixing with a strong alkali liquid after grinding potassium feldspar minerals, and then carrying out hydrothermal reaction inside a high-pressure container; (3) adding water to leach, agitating for 0.5-24 hours and carrying out solid-liquid separation; (4) adding zeolite which is equal to 0.2-1fold of the mass of the potassium feldspar, and agitating for 0.5-4 hours, so as to separate out potassium ions by zeolite adsorption; (5) adding the zeolite adsorbed with the potassium ions in the step (4) to an inorganic acid or a sodium salt liquid, agitating for 1-24 hours, and then carrying out solid-liquid separation; (6) cleaning a solid phase by clean water twice, and baking at 100-300 DEG C for 0.5-4 hours to recycle; and (7) evaporating and crystallizing the liquid phase obtained in the step (5), so as to prepare a qualified potash fertilizer. By adopting the technology, the potassium feldspar is decomposed at a high temperature, energy consumption is reduced, and the technology is short in technological process, simple in equipment, low in investment and low in production cost.
Need to check novelty before this filing date? Find Prior Art

Description

technical field

[0001] The invention relates to a process for preparing potassium fertilizer from potassium feldspar decomposing mother liquor, in particular to a process for preparing potassium fertilizer from potassium feldspar decomposing mother liquor by an adsorption method. Background technique

[0002] Potassium salt resources in my country are poor, but potassium feldspar resources are abundant, widely distributed, large reserves, and high potassium content, generally greater than 10% (calculated as potassium oxide), is an ideal raw material for comprehensive utilization of potassium salt production. Potassium feldspar is a Si~AL~O framework structure, and its molecular formula is K[AlSi 3 o 8 ], its composition is a network structure, extremely stable, and is hardly decomposed by acid and alkali under normal temperature and pressure. Therefore, the development and utilization of potassium feldspar is limited.

[0003] At present, a large number of literatures have...

Examples

Embodiment 1

[0022] This embodiment includes the following steps:

[0023] Grind potassium feldspar ore to -100 mesh; after grinding potassium feldspar mineral, mix it with sodium hydroxide solution with a mass concentration of 20wt% according to the ratio of potassium feldspar: strong alkali solution mass ratio of 1:0.5 , and then carry out hydrothermal reaction in a high-pressure container, the reaction temperature is 100 ° C, the pressure is 2 MPa, and the reaction time is 4 hours; add water equivalent to 0.5 times the mass of the original potassium feldspar powder to the material obtained from the reaction for leaching, Stir for 0.5h; obtain the material for solid-liquid separation, add zeolite equivalent to 0.2 times the quality of the raw material potassium feldspar to the obtained liquid phase, and stir for 4 hours to make the zeolite fully adsorb potassium ions and precipitate; solid-liquid separation, the obtained adsorbed potassium Ionic zeolite, add hydrochloric acid with a mass...

Embodiment 2

[0026] This embodiment includes the following steps:

[0027] Grind the potassium feldspar ore to -100 mesh, grind the potassium feldspar mineral finely, and mix it with a sodium hydroxide solution with a mass concentration of 40wt% according to the ratio of potassium feldspar: strong alkali solution mass ratio of 1:1.5 , and then carry out hydrothermal reaction in a high-pressure container, the reaction temperature is 200 ° C, the pressure is 4 MPa, and the reaction time is 1 h; the material obtained by the reaction is added to the material obtained by the reaction. 5h; obtain the material for solid-liquid separation, add zeolite equivalent to 0.6 times the quality of raw material potassium feldspar to the liquid phase, stir for 2h, make the zeolite adsorb potassium ions and separate out; 1 times the mass of sulfuric acid solution with a mass concentration of 49wt% was mixed, stirred for 12 hours, filtered and separated, the filtrate was evaporated and crystallized, and dried...

Embodiment 3

[0030] This embodiment includes the following steps:

[0031] Grind the potassium feldspar ore to -200 mesh, grind the potassium feldspar mineral finely, and mix it with sodium hydroxide solution with a mass concentration of 60wt% according to the ratio of potassium feldspar: strong alkali solution mass ratio of 1:2.5 , and then carry out hydrothermal reaction in a high-pressure container, the reaction temperature is 300 ° C, the pressure is 6 MPa, and the reaction time is 24 hours; add water equivalent to 10 times the mass of the original potassium feldspar powder to the material obtained from the reaction for leaching , stirred for 0.5h; the obtained material was subjected to solid-liquid separation, and zeolite equivalent to 0.8 times the quality of the raw material potassium feldspar was added to the obtained liquid phase, and stirred for 0.5h, so that the zeolite fully adsorbed potassium ions and precipitated; solid-liquid separation, the obtained adsorption The zeolite c...