A ring forming device and a method of using the same
By using an annular forming device of multiple stamping molds and central bearing components, the joint marks during splicing of piezoelectric ceramic sheets are reduced, the molding accuracy and quality are improved, the problems of joint marks and misalignment in the prior art are solved, and the problem of joint marks and dislocations in the prior art is realized. Better imaging results.
Patent Information
- Application Number
- CN201811544411.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2018-12-17
- Publication Date
- 2024-12-03
- Estimated Expiration
- 2038-12-17
AI Technical Summary
In the existing annular forming methods, joint marks are prone to occur when splicing piezoelectric ceramic sheets, which affects the consistency of array elements and tissue imaging effect, and the splicing is prone to misalignment, resulting in a decrease in the quality of piezoelectric ceramic ring.
Using an annular forming device including multiple stamping dies and central bearing components, the annular cavity is formed through the combination of the central bearing pipe, the center rod and the buffer sleeve, which reduces joint marks and improves the molding accuracy, and ensures that the shrinkage structure and buffer sleeve are used. The inner surface is flat and the disassembled design is easy to remove.
Reduce joint marks, avoid misalignment of piezoelectric ceramic sheets, and improve the molding quality and use effect of piezoelectric ceramic rings.
Smart Images

Figure CN109473540B_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the technical field of ultrasonic equipment, and in particular to a ring-shaped forming device and a use method thereof. Background Art
[0002] Based on the widespread application of ultrasonic transducers in medical imaging, in order to obtain image documents of tubular tissues such as the digestive tract, nasal cavity, and blood vessels and arteries, the transducer is usually made into a ring shape or a single-element transducer is rotated to obtain a complete image.
[0003] The existing ring forming method is to splice two piezoelectric ceramic sheets with arc-shaped cross-sections into a completed ring. The disadvantage of this method is that two joint marks will appear in the middle of the two piezoelectric ceramic sheets spliced together. During use, one of the joint marks cannot be avoided. This joint mark causes the connection, spacing, and consistency between the transducer array elements to change, which is bound to affect the imaging effect of the tissue facing the joint mark. In addition, the two piezoelectric ceramic sheets are easily misaligned when spliced, thereby generating steps in the radial direction and / or axial direction, affecting the quality of the piezoelectric ceramic ring. Summary of the invention
[0004] In view of this, the first object of the present invention is to provide a ring-shaped forming device to facilitate the manufacture of piezoelectric ceramic rings and reduce joint marks during the forming of piezoelectric ceramic rings; the second object of the present invention is to provide a method for using the above-mentioned ring-shaped forming device.
[0005] To achieve the above first object, the present invention provides the following technical solutions:
[0006] A ring-shaped forming device, comprising:
[0007] A molding assembly, comprising a plurality of dies, each of which can cooperate with each other to enclose a cavity;
[0008] A center bearing assembly, comprising a center bearing tube, a center rod and a buffer sleeve, wherein the center bearing tube comprises a contraction structure, wherein the contraction structure comprises a plurality of contraction seams opened along the length direction of the center bearing tube and distributed circumferentially, wherein the center rod is detachably inserted into the center bearing tube and tightens the contraction structure, and the buffer sleeve is detachably clamped outside the contraction structure;
[0009] When the molding assembly is molded, the gaps between each of the pressing dies and the buffer sleeve form an annular cavity.
[0010] Preferably, the middle support pipe is threadably matched with the center rod.
[0011] Preferably, the center support pipe includes a connecting pipe section and a shrinking pipe section connected to each other, the shrinking seam is opened in the shrinking pipe section, and the center rod includes a threaded section for cooperating with the connecting pipe section and a bare rod section for cooperating with the shrinking pipe section.
[0012] Preferably, the middle supporting pipe also includes a tapered tube section, the large end of the tapered tube section is connected to the contraction tube section, the small end of the tapered tube section is connected to the connecting tube section, and the center rod includes a tapered rod section connected between the threaded section and the smooth rod section, the small end of the tapered rod section is connected to the threaded section, and the large end of the tapered tube section is connected to the smooth rod section.
[0013] Preferably, an operating handle is provided at one end of the central rod.
[0014] Preferably, a positioning step surface is formed on the side wall of the cavity, and the positioning step surface is perpendicular to the axis of the annular cavity.
[0015] Preferably, two adjacent dies are locked by threaded fasteners.
[0016] Preferably, at least one of the die surfaces is provided with a die opening groove, and the die opening groove has an exposed opening after the molding assembly is molded.
[0017] Preferably, the buffer sleeve is a rubber sleeve.
[0018] Preferably, the length of the shrinkage seam is greater than the length of the buffer sleeve.
[0019] To achieve the above second object, the present invention provides a method for using an annular forming device, comprising the steps of:
[0020] A mold release agent is applied to the side walls of each die for enclosing a cavity, one of the die is a static die, and the other die are dynamic die, and each dynamic die moves toward the static die to achieve mold closing;
[0021] Preheating the piezoelectric ceramic sheet until it softens, and placing the piezoelectric ceramic sheet on a static mold forming surface;
[0022] Press the assembled center bearing assembly onto the piezoelectric ceramic sheet so that the piezoelectric ceramic sheet fits the static mold forming surface;
[0023] Each movable mold moves toward the static mold to close the mold and press the piezoelectric ceramic sheet into a piezoelectric ceramic ring;
[0024] After the piezoelectric ceramic ring has cooled, the center rod, the center bearing tube and the buffer sleeve of the center bearing assembly are removed in sequence.
[0025] Preferably, after taking out the middle bearing assembly, the method further comprises the following steps:
[0026] Filling a backing material into a piezoelectric ceramic ring to prepare a ring transducer;
[0027] After the backing material has cooled, the individual dies of the molding assembly are disassembled.
[0028] In summary, the present invention provides an annular forming device comprising a forming component and a middle bearing component, wherein the forming component comprises a plurality of dies, each of which can cooperate with each other to form a cavity; the middle bearing component comprises a middle bearing tube, a center rod and a buffer sleeve, the middle bearing tube comprises a contraction structure, the contraction structure comprises a plurality of contraction seams opened along the length direction of the middle bearing tube and distributed circumferentially, the center rod can be detachably inserted into the middle bearing tube and tighten the contraction structure, that is, when the center rod is pulled out of the middle bearing tube, due to the loss of support, the contraction structure of the middle bearing tube can be contracted toward the axis direction of the middle bearing tube for easy demoulding, the buffer sleeve is used to isolate the piezoelectric ceramic sheet from the contraction seam, so that the product forms a flat and smooth inner surface, and provides buffer protection for the product when demolding, and the buffer sleeve is detachably clamped outside the contraction structure; when the forming component is molded, the gap between each die and the buffer sleeve constitutes an annular cavity for molding the product;
[0029] When in use, firstly, a release agent is applied on the side walls of each die used to enclose the cavity to facilitate demolding, the piezoelectric ceramic sheet is heated until it softens, and then the piezoelectric ceramic sheet is placed on the molding surface of one of the dies coated with the release agent, and then the assembled middle bearing component is pressed on the piezoelectric ceramic sheet to make the piezoelectric ceramic sheet fit the molding surface; the remaining dies are brought together to close the mold to press the piezoelectric ceramic sheet on the middle bearing component to form a piezoelectric ceramic ring; after the piezoelectric ceramic ring is cooled, the center rod, middle bearing tube and buffer sleeve of the middle bearing component are removed in turn; it can be seen that when using the above-mentioned annular forming device, a plurality of dies are closed around the middle bearing component, so that a piece of piezoelectric ceramic sheet can be pressed into an annular structure, thereby reducing a joint mark compared to the existing manufacturing method, ensuring the use effect of the piezoelectric ceramic ring, and at the same time, pressing a piece of piezoelectric ceramic sheet to form a piezoelectric ceramic ring is not easy to be dislocated, which helps to improve the quality of the piezoelectric ceramic ring. BRIEF DESCRIPTION OF THE DRAWINGS
[0030] In order to more clearly illustrate the embodiments of the present invention or the technical solutions in the prior art, the drawings required for use in the embodiments or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present invention. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative work.
[0031] Figure 1 An axonometric view of the annular forming device provided by an embodiment of the present invention when the mold is closed;
[0032] Figure 2 An exploded view of a ring-shaped forming device provided in an embodiment of the present invention;
[0033] Figure 3 An axonometric view of a center bearing assembly provided in an embodiment of the present invention;
[0034] Figure 4 An axonometric view of a center bearing pipe of a center bearing assembly provided in an embodiment of the present invention;
[0035] Figure 5 An axonometric view of a center rod of a center bearing assembly provided in an embodiment of the present invention;
[0036] Figure 6 A schematic diagram of a middle bearing assembly pressing a piezoelectric ceramic sheet toward one of the dies in a method for using the annular forming device provided in an embodiment of the present invention;
[0037] Figure 7 A schematic diagram of a middle bearing assembly pressing a piezoelectric ceramic sheet onto a molding surface of one of the dies in a method for using the annular molding device provided in an embodiment of the present invention;
[0038] Figure 8 A schematic diagram of the structure after mold closing in the method for using the annular forming device provided by an embodiment of the present invention;
[0039] Fig. 9 A schematic diagram of the structure after the central rod is removed in the method for using the annular forming device provided by an embodiment of the present invention;
[0040] Fig.10 A schematic diagram of the structure after the middle support pipe is removed in the method for using the annular forming device provided in an embodiment of the present invention;
[0041] Fig.11 A schematic diagram of the structure after the buffer sleeve is removed in the method for using the annular forming device provided in an embodiment of the present invention.
[0042] Among them, 1 is a molding component; 100 is a mold opening groove; 110 is an upper die; 111 is an upper molding cavity; 112 is a first step groove; 113 is a threaded hole; 120 is a lower die; 121 is a lower molding cavity; 122 is a second step groove; 123 is a second arc-shaped step surface; 2 is a middle bearing component; 210 is a center rod; 211 is an operating handle; 212 is a bare rod section; 213 is a threaded section; 214 is a tapered rod section; 220 is a middle bearing pipe; 221 is a shrinkage pipe section; 222 is a connecting pipe section; 223 is a shrinkage seam; 224 is a tapered pipe section; 230 is a buffer sleeve. DETAILED DESCRIPTION
[0043] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0044] See also Figure 1-Figure 3 , Figure 1 This is an axonometric view of the annular forming device provided by an embodiment of the present invention when the mold is closed. Figure 2 An exploded view of a ring-shaped forming device provided in an embodiment of the present invention, Figure 3 An axonometric view of a center bearing assembly provided in an embodiment of the present invention.
[0045] An embodiment of the present invention provides an annular forming device, including a forming component 1 and a middle bearing component 2.
[0046] Among them, the molding component 1 includes multiple dies, each of which can cooperate with each other to form a cavity; the middle bearing component 2 includes a middle bearing tube 220, a center rod 210 and a buffer sleeve 230, the middle bearing tube 220 includes a shrinkage structure, the shrinkage structure includes multiple shrinkage seams 223 opened along the length direction of the middle bearing tube 220 and distributed circumferentially, the center rod 210 can be detachably inserted into the middle bearing tube 220 and tighten the shrinkage structure, that is, when the center rod 210 is pulled out of the middle bearing tube 220, due to the loss of support, the shrinkage structure of the middle bearing tube 220 can shrink toward the axial direction of the middle bearing tube 220 to facilitate demolding, the buffer sleeve 230 is used to isolate the piezoelectric ceramic sheet from the shrinkage seam 223, so that the product forms a flat and smooth inner surface, and provides buffer protection for the product when the mold is removed, and the buffer sleeve 230 can be detachably clamped outside the shrinkage structure; when the molding component 1 is molded, the gap between each die and the buffer sleeve 230 constitutes an annular cavity for molding the product.
[0047] To sum up, compared with the prior art, when an annular forming device provided in an embodiment of the present invention is used, first, a release agent is applied on the side walls of each die used to enclose a cavity to facilitate demolding, the piezoelectric ceramic sheet is heated until it softens, and then the piezoelectric ceramic sheet is placed on the molding surface of one of the dies coated with the release agent, and then the assembled middle bearing component 2 is pressed on the piezoelectric ceramic sheet to make the piezoelectric ceramic sheet fit the molding surface; the remaining dies are brought together to close the mold to press the piezoelectric ceramic sheet on the middle bearing component 2 to form a piezoelectric ceramic ring; after the piezoelectric ceramic ring is cooled, the center rod 210, the middle bearing tube 220 and the buffer sleeve 230 of the middle bearing component 2 are removed in turn; it can be seen that when using the above-mentioned annular forming device, a plurality of dies are closed around the middle bearing component 2, so that a piece of piezoelectric ceramic sheet can be pressed into an annular structure, thereby reducing a joint mark compared to the existing manufacturing method, ensuring the use effect of the piezoelectric ceramic ring, and at the same time, pressing a piece of piezoelectric ceramic sheet to form a piezoelectric ceramic ring is not easy to be dislocated, which helps to improve the quality of the piezoelectric ceramic ring.
[0048] exist Figure 1-Figure 3 In the illustrated embodiment, the cavity of the molding component 1 is cylindrical, and the outer surface of the center support component 2 is also cylindrical, and the cross-section of the product formed by the cooperation of the two is circular. In other embodiments, other shapes such as square, elliptical, etc. may also be used, and the inner cavity shape of the center support component 2 may be the same as or different from the contour shape of the center support component 2.
[0049] The middle support tube 220 and the center rod 210 can be plug-fitted, but it is understandable that when the mold is closed and pressed, the plug-fitted middle support tube 220 and the center rod 210 are difficult to separate, and forming a pressed ceramic ring is only a step in manufacturing the annular transducer. Later, it is necessary to pour backing material into the pressed ceramic ring without removing the mold. Therefore, if the above-mentioned method of pouring backing material without removing the mold is adopted in the production process, the middle support tube 220 and the center rod 210 generally do not adopt a plug-fitting method, but a threaded method. The threaded cooperation between the middle support tube 220 and the center rod 210 can ensure the close cooperation between the middle support tube 220 and the center rod 210 on the one hand, and on the other hand, after the piezoelectric ceramic ring is formed and cooled, by rotating the center rod 210, the middle support tube 220 can be withdrawn with the help of the thrust of the threaded cooperation between the center rod 210 and the middle support tube 220, so as to facilitate the removal of the middle support component 2 without removing the mold.
[0050] Preferably, see Figure 4 The middle support pipe 220 includes a connecting pipe section 222 and a shrink pipe section 221 connected to each other, and a shrinkage seam 223 is opened in the shrinkage pipe section 221. The center rod 210 includes a threaded section 213 and a bare rod section 212, wherein the threaded section 213 is used to cooperate with the connecting pipe section 222, and the bare rod section 212 is used to cooperate with the shrinkage pipe section 221. Figure 4In the illustrated embodiment, the threaded section 213 is provided with external threads, and the connecting pipe section 222 is provided with internal threads. In other embodiments, the threaded section 213 may be provided with internal threads, and the connecting pipe section 222 may be provided with external threads.
[0051] Further optimize the above technical solution, such as Figure 4 and Figure 5 As shown, the middle supporting pipe 220 also includes a tapered tube section 224, the large end of the tapered tube section 224 is connected to the shrinkage tube section 221, the shrinkage seam 223 on the shrinkage tube section 221 extends to the tapered tube section 224, the small end of the tapered tube section 224 is connected to the connecting tube section 222, and the center rod 210 includes a tapered rod section 214 connected between the threaded section 213 and the smooth rod section 212, the small end of the tapered rod section 214 is connected to the threaded section 213, and the large end of the tapered tube section 224 is connected to the smooth rod section 212. When in use, the tapered surface between the tapered rod section 214 and the tapered tube section 224 can ensure that the center rod 210 tightens the shrinkage tube section 221. This tapered surface tightening method has lower requirements on precision and better effects.
[0052] To facilitate the disassembly of the middle bearing assembly 2, Figure 5 As shown, an operating handle 211 is provided at one end of the central rod 210 .
[0053] Preferably, a positioning step surface is formed on the side wall of the cavity of the molding component 1, and the positioning step surface is perpendicular to the axis of the annular cavity. Figure 1 and Figure 2 As shown, in a specific embodiment of the present invention, the molding component 1 includes an upper die 110 and a lower die 120. A first arcuate step surface (not shown in the figure) is arranged in the upper molding cavity 111 of the upper die 110, and a second arcuate step surface 123 is arranged in the lower molding cavity 121 of the lower die 120. The upper molding cavity 111 and the lower molding cavity 121 form a cavity. The first arcuate step surface and the second arcuate step surface 123 are connected to form a positioning step surface for positioning the piezoelectric ceramic ring. When the middle bearing tube 220 of the middle bearing component 2 is removed, the positioning step surface can position the piezoelectric ceramic ring to prevent it from shifting.
[0054] The dies in the molding assembly 1 can be relatively fixed by means of a clamping connection or by means of a connecting piece. In the present invention, it is preferred to use a threaded fastener to lock two adjacent dies. Specifically, Figure 1 and Figure 2As shown, the upper die 110 and the lower die 120 are respectively provided with threaded holes 113 at corresponding positions, and the threaded fasteners cooperate with the threaded holes 113 of the upper die 110 and the lower die 120 to lock the upper die 110 and the lower die 120. Furthermore, at least two threaded holes 113 are respectively provided on the upper die 110 and the lower die 120, and at least two threaded holes 113 on the same die are symmetrically distributed on both sides of the cavity.
[0055] To further optimize the above technical solution, in order to facilitate demolding, a mold opening groove 100 can be provided on the mold surface of at least one die, and the mold opening groove 100 has an exposed opening after the molding component 1 is molded, and the opening is used to insert a tool such as a screwdriver to disassemble two adjacent dies. Figure 2 As shown, a first step groove 112 is provided on the mold surface of the upper mold 110, and a second step groove 122 is provided on the mold surface of the lower mold 120. When the upper mold 110 and the lower mold 120 are molded together, the first step groove 112 and the second step groove 122 cooperate with each other to form a mold opening groove 100.
[0056] It is understandable that in order to play a role of buffering and facilitating demoulding, the buffer sleeve 230 should be made of a material with a certain elasticity. In a specific embodiment of the present invention, the buffer sleeve 230 is a rubber sleeve.
[0057] To further optimize the above technical solution, in a specific embodiment of the present invention, the length of the contraction seam 223 is greater than the length of the buffer sleeve 230 .
[0058] To achieve the second objective, the present invention provides a method for using the annular forming device, the method comprising the steps of:
[0059] S101: applying a mold release agent on the side walls of each die for enclosing a cavity, wherein one die is a static die and the other dies are dynamic die, and each dynamic die moves toward the static die to achieve mold closing;
[0060] In the embodiment of the present invention, the mold release agent is wax. When in use, each mold is first heated, and then a wax block is placed on the molding surface thereof, and the wax block is evenly applied after liquefaction. Of course, wax is only a preferred embodiment provided in the embodiment of the present invention, and is not limited thereto. Other mold release agents may also be used, which is not limited here. In the embodiment of the present invention, Figure 6 As shown, the lower die 120 is used as a static die, and the upper die 110 is used as a dynamic die.
[0061] S102: preheating the piezoelectric ceramic sheet until the piezoelectric ceramic sheet softens, and placing the piezoelectric ceramic sheet on a static mold forming surface;
[0062] In order to facilitate the bending of the piezoelectric ceramic sheet, it is necessary to heat it to soften it and then place it on the forming surface of the static mold.
[0063] S103: Pressing the assembled center bearing assembly 2 onto the piezoelectric ceramic sheet so that the piezoelectric ceramic sheet fits the static mold molding surface;
[0064] The assembled center bearing assembly 2 refers to the center rod 210 and the center bearing tube 220 are closely matched to tighten the center bearing tube 220, and the buffer sleeve 230 is sleeved on the shrink pipe section 221 of the center bearing tube 220 to play the role of isolation and buffering. Figure 7 shown.
[0065] S104: The movable molds are brought close to the static molds to close the molds and press the piezoelectric ceramic sheets into piezoelectric ceramic rings;
[0066] like Figure 8 As shown, the upper pressing die 110 and the lower pressing die 120 are closed together to press the piezoelectric ceramic sheet onto the buffer sleeve 230 of the middle bearing component 2, so that the piezoelectric ceramic sheet forms a ring shape.
[0067] S105: After the piezoelectric ceramic ring is cooled, the central rod 210, the middle bearing tube 220 and the buffer sleeve 230 of the middle bearing assembly 2 are removed in sequence.
[0068] like Figure 9-11 shown.
[0069] Further optimizing the above technical solution, after taking out the middle bearing assembly 2, the following steps are further included:
[0070] S106: pouring a backing material into the piezoelectric ceramic ring to prepare a ring transducer;
[0071] S107: After the backing material is cooled, the respective dies of the molding assembly 1 are disassembled.
[0072] The above method can realize the pouring of the backing without removing the mold, which is convenient for the production of the annular transducer.
[0073] The various embodiments in this specification are described in a progressive manner, and each embodiment focuses on the differences from other embodiments. The same or similar parts between the various embodiments can be referenced to each other.
[0074] The above description of the disclosed embodiments enables one skilled in the art to implement or use the present invention. Various modifications to these embodiments will be apparent to one skilled in the art, and the general principles defined herein may be implemented in other embodiments without departing from the spirit or scope of the present invention. Therefore, the present invention will not be limited to the embodiments shown herein, but rather to the widest scope consistent with the principles and novel features disclosed herein.
Claims
1. A ring forming device, characterized in that: include: A molding assembly, comprising a plurality of dies, each of which can cooperate with each other to enclose a cavity; A center bearing assembly, comprising a center bearing tube, a center rod and a buffer sleeve, wherein the center bearing tube comprises a contraction structure, wherein the contraction structure comprises a plurality of contraction seams opened along the length direction of the center bearing tube and distributed circumferentially, wherein the center rod is detachably inserted into the center bearing tube and tightens the contraction structure, and the buffer sleeve is detachably clamped outside the contraction structure; When the molding assembly is molded, the gaps between each of the pressing dies and the buffer sleeve form an annular cavity; The middle support pipe is threadedly matched with the center rod; The center support pipe includes a connecting pipe section and a shrinking pipe section connected to each other, the shrinking seam is opened in the shrinking pipe section, and the center rod includes a threaded section for cooperating with the connecting pipe section and a polished rod section for cooperating with the shrinking pipe section; The center supporting pipe also includes a tapered tube section, the large end of which is connected to the contraction tube section, and the small end of which is connected to the connecting tube section. The center rod includes a tapered rod section connected between the threaded section and the smooth rod section, the small end of which is connected to the threaded section, and the large end of which is connected to the smooth rod section.
2. The annular forming device according to claim 1, characterized in that: An operating handle is arranged at one end of the central rod.
3. The annular forming device according to claim 1, characterized in that: A positioning step surface is formed on the side wall of the cavity, and the positioning step surface is perpendicular to the axis of the annular cavity.
4. The annular forming device according to claim 1, characterized in that: Two adjacent pressing dies are locked by threaded fasteners.
5. The annular forming device according to claim 1, characterized in that: A die opening groove is arranged on the die closing surface of at least one of the pressing dies, and the die opening groove has an exposed opening after the molding assembly is molded.
6. The annular forming device according to claim 1, characterized in that: The buffer sleeve is a rubber sleeve.
7. The annular forming device according to claim 1, characterized in that: The length of the shrinkage seam is greater than the length of the buffer sleeve.
8. A method for using a ring-shaped forming device, characterized in that: The annular forming device according to any one of claims 1 to 7 comprises the steps of: A mold release agent is applied to the side walls of each die for enclosing a cavity, one of the die is a static die, and the other die are dynamic die, and each dynamic die moves toward the static die to achieve mold closing; Preheating the piezoelectric ceramic sheet until it softens, and placing the piezoelectric ceramic sheet on a static mold forming surface; Press the assembled center bearing assembly onto the piezoelectric ceramic sheet so that the piezoelectric ceramic sheet fits the static mold forming surface; Each movable mold moves toward the static mold to close the mold and press the piezoelectric ceramic sheet into a piezoelectric ceramic ring; After the piezoelectric ceramic ring has cooled, the center rod, the center bearing tube and the buffer sleeve of the center bearing assembly are removed in sequence.
9. The method for using the annular forming device according to claim 8, characterized in that: After taking out the middle bearing assembly, the following steps are also included: Filling a backing material into a piezoelectric ceramic ring to prepare a ring transducer; After the backing material has cooled, the individual dies of the molding assembly are disassembled.