A fiber reinforced buckle and its forming process
Through the winding and molding process of fiber reinforced materials, lightweight and high-strength buckles are prepared, which solves the problems of heavy metal buckles and insufficient strength of plastic buckles, and provides a better skin-friendly experience and high-strength performance.
Patent Information
- Application Number
- CN201911203159.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2019-11-29
- Publication Date
- 2024-10-29
- Estimated Expiration
- 2039-11-29
AI Technical Summary
Existing metal buckles are heavy and have poor skin-friendly feel, while plastic buckles are not strong enough to meet the needs of high-intensity use.
Fiber-reinforced materials are used to prepare buckles. By preparing continuous long fiber winding tapes, selecting appropriate fibers and resins, pre-impregnating, winding and heating molding, a buckle with low density, small thermal conductivity coefficient and high strength is formed.
The buckle is lightweight and skin-friendly, and its strength is close to that of stainless steel, far exceeding that of plastic buckles, making it suitable for applications requiring high strength.
Abstract
Description
Technical Field
[0001] The present invention relates to the technical field of fasteners, and in particular to a fiber fastener and a molding process thereof. Background Art
[0002] Common webbing buckles in the prior art include plastic buckles and metal buckles. Plastic buckles do not require high strength and are produced using plastic injection molding. Most plastic buckles include male buckles and female buckles. The male buckle and female buckle connected to two different webbings are combined to facilitate free connection and fix the webbing at both ends. This buckle is widely used in the buckling of helmets, backpacks or shoe laces. Common metal buckles are made of various metals, such as belt buckles or male buckles and female buckles with larger load-bearing capacity.
[0003] Existing metal buckles are heavy and have poor skin-friendly feel when used in places that need to contact the skin, especially in winter, the cold metal texture will irritate the user, and the experience is poor. The strength of plastic buckles cannot meet the high-strength usage requirements. Summary of the invention
[0004] The purpose of the present invention is to overcome the deficiencies of the prior art and provide a fiber-reinforced buckle and a molding process thereof which has high strength, light weight and good skin-friendly effect.
[0005] In order to achieve the above object, the solution of the present invention is:
[0006] A molding process of a fiber reinforced buckle, comprising the following steps:
[0007] Step A: preparing a continuous filament winding tape; specifically comprising the following steps:
[0008] Step A1 Fiber preparation: Select appropriate fiber yarn, cloth (tube cloth) or felt according to product functional requirements.
[0009] Step A2: Resin preparation: Select and mix appropriate resin according to product functional requirements.
[0010] Step A3 Fiber pre-impregnation: The fiber yarn, cloth (tube cloth) or felt fabric is pre-impregnated with the prepared resin and pre-baked at medium to low temperature (about 50-90°C). If dry yarn is used, no pre-impregnation operation is required, and the resin can be directly poured or injected with necessary heating and molding. If thermoplastic resin is used, it can also be injected in a similar way. And the resin content can be controlled according to the needs.
[0011] Step B: Wrap the wrapping tape in step A on the wrapping jig. The wrapping needs to be done in a preset direction according to the design of the product, and the number of wrapping turns is controlled according to the set wrapping amount. When wrapping, wrap the wrapping tape longitudinally along the axial direction of the product ribs. It can be done manually or with equipment or equipment assistance.
[0012] Step C: placing the winding jig wrapped with the winding tape into a mold of the product and heating and forming it;
[0013] Step D: After molding, the fiber-reinforced fastener is demoulded to obtain the fiber-reinforced fastener.
[0014] Further, step A comprises the following steps:
[0015] Step A1: Select fiber raw materials according to product functional requirements and cut them into required axial fibers;
[0016] Step A2: Select and prepare the resin according to the functional requirements of the product, and the content of the resin accounts for more than 20% of the long fiber winding tape;
[0017] Step A3: The selected fiber raw material is pre-impregnated with the prepared resin and pre-baked at a medium-low temperature of 50 to 90 degrees to obtain the continuous long fiber winding tape.
[0018] Further, step A may also include the following steps:
[0019] Step A1: Select dry yarn as fiber raw material and cut it into desired axial fibers;
[0020] Step A2: Select and prepare the resin according to the product functional requirements;
[0021] Step A3: pouring or injecting the axial fibers of step A1 and the resin of step A2, and heating and molding.
[0022] Furthermore, in step A1, the fiber raw material is any one or any combination of fiber yarn, fiber cloth, fiber tube cloth or fiber felt.
[0023] Furthermore, in the step A2, the content of the resin is 30% to 50%, and the most preferred content is 35%.
[0024] Furthermore, in the step B, the amount of fibers in the long fiber winding tape in the radial and axial directions exceeds 50%, and the amount of fibers at an angle to the winding direction does not exceed 50%. The percentage here refers to the percentage of fiber content in the winding tape, and also refers to the winding amount of the fiber tape at the winding position;
[0025] Furthermore, the molding process of the fiber reinforced fastener includes the following steps after step D:
[0026] Step E: affixing the pre-prepared film-like resin material to the product surface of the fiber-reinforced fastener in step D.
[0027] Furthermore, in step C, a pre-prepared film-like resin material is attached to the mold, so that the surface of the fiber-reinforced fastener in step D is formed with a pattern of the film-like resin material.
[0028] Furthermore, in step D, the heating molding includes any one of compression molding, bag pressing molding, heating molding after wrapping with a heat shrinkable film, or injection molding.
[0029] The present invention also provides a fiber reinforced buckle prepared by using the molding process.
[0030] After adopting the above structure, the present invention uses a fiber-reinforced material to make a buckle. Because its density is much lower than the metal that can be used for buckles, its mass is only one-third to one-fifth of that of ordinary metal buckles. In addition, its thermal conductivity is also much lower than that of metal, and its skin-friendly experience is much higher than that of metal buckles. In addition, compared with plastic buckles, the strength of the fiber-reinforced buckle of the present invention far exceeds that of plastic buckles, and is even close to the strength of stainless steel metal buckles. DETAILED DESCRIPTION
[0031] In order to further explain the technical solution of the present invention, the present invention is described in detail below through specific embodiments.
[0032] The present invention discloses a molding process of a fiber reinforced buckle, which comprises the following steps:
[0033] Step A: preparing a continuous filament winding tape;
[0034] The preparation of the fiber winding tape includes the following steps:
[0035] Step A1: Fiber preparation, select appropriate fiber yarn, fiber cloth, fiber tube cloth, fiber felt or dry yarn according to product functional requirements. The fiber winding tape can be made of pre-impregnated fiber material, or dry yarn, cloth, tube cloth or felt and other fabrics and their pre-impregnated materials.
[0036] Step A2: Resin preparation. Select and mix appropriate resin according to product functional requirements. The resin content of the buckle product of the present invention is above 20%, and the optimal range is around 35%. The resin involved can be a thermosetting resin formed by reaction or a thermoplastic resin formed by non-chemical reaction.
[0037] Step A3: Fiber pre-impregnation, the fiber yarn, fiber cloth, fiber tube cloth or fiber felt fabrics are pre-impregnated with the resin prepared in step A2, and pre-baked at medium and low temperature (about 50-90°C). If dry yarn is used, no pre-impregnation operation is required, and the resin can be directly poured or injected with necessary heating and molding. If thermoplastic resin is used, it can also be injected in a similar way, and the resin content can be controlled according to the needs.
[0038] Step B: Winding operation, winding the winding tape in step A on a winding jig. The winding needs to be performed in a pre-set direction according to the design of the product, and the number of winding turns is controlled according to the set winding amount. The winding is performed on a winding jig, and the jig is designed according to the shape of the product. During winding, the amount of fiber in the direction of the product diameter / axis (referring to the force direction of each position of the product) exceeds 50%, and the amount of fiber at an angle to the winding direction should not exceed 50%. After the continuous long fiber is laid in the diameter / axial direction, the fiber can withstand external force to the maximum extent, giving full play to the strength advantage of carbon fiber composite materials, and ultimately optimizing the strength of the product using the present invention.
[0039] Step C: Molding operation, put the wrapping jig wrapped with wrapping tape into the mold of the product for heating and molding; the molding method can be mold pressing and heating molding, bag pressing and heating molding, or heating molding after wrapping with heat shrink film, etc. Because the jig is designed according to the shape of the product, it can also be used as a part of the mold during molding. After completing step B, put it directly into the mold for pressure heating and molding, and then take it out.
[0040] Step D: After molding, the fiber-reinforced fastener is demoulded to obtain the fiber-reinforced fastener.
[0041] Step E: Product appearance processing. In order to simplify the subsequent processing of the product and achieve environmental protection, in-mold decoration and / or the addition of appearance improvement film can be used during molding to achieve the elimination of the subsequent spraying process. The main method is to use a pre-prepared film-like resin material (the film-like material can also be printed with the required pattern in advance using printing technology such as silk screen printing) to stick it on the pre-wrapped product or directly stick it in the mold and then mold it together with the pre-wrapped product. In this way, the appearance of the molded product can be free of the spraying process of the commonly used technology.
[0042] The present invention adopts the fiber winding method to make the annular buckle, which is suitable for single-hole or multi-hole annular products, and is also suitable for non-closed annular buckles or other products; the buckle made of fiber-reinforced material of the present invention has a density far lower than that of metal that can be used for buckles, so the mass is only one-third to one-fifth of that of ordinary metal buckles; in addition, its thermal conductivity coefficient is also far lower than that of metal, and the skin-friendly experience is far better than that of metal buckles. Compared with plastic buckles, the strength of the buckle of the present invention far exceeds that of plastic buckles, and is even close to the strength of stainless steel metal buckles.
[0043] The above embodiments do not limit the product form and style of the present invention. Any appropriate changes or modifications made by ordinary technicians in the relevant technical field should be deemed to be within the patent scope of the present invention.
Claims
1. A molding process for a fiber-reinforced buckle, characterized in that: The following steps are involved: Step A: preparing a continuous long fiber winding tape; Step B: winding the winding tape in step A on a winding jig, the winding needs to be wound in a pre-set direction according to the design of the product, and the number of winding turns is controlled according to the set winding amount; Step C: placing the winding jig wrapped with the winding tape into a mold of the product for heating and molding; Step D: demolding after molding to obtain a fiber reinforced fastener; The step A comprises the following steps: step A1: selecting fiber raw materials according to product functional requirements; step A2: selecting and preparing resin according to product functional requirements, wherein the content of the resin accounts for more than 20% of the long fiber winding tape; step A3: pre-impregnating the selected fiber raw materials with the prepared resin, and pre-baking at a medium-low temperature of 50 to 90 degrees to obtain the continuous long fiber winding tape, and cutting it into the desired axial fibers.
2. A fiber reinforced buckle molding process as claimed in claim 1, characterized in that: In the step A1, the fiber raw material is any one or any combination of fiber yarn, fiber cloth, fiber tube cloth or fiber felt.
3. A fiber reinforced buckle molding process as claimed in claim 1, characterized in that: The step A comprises the following steps: step A1: selecting dry yarn as the fiber raw material and cutting it into the desired axial fibers; step A2: selecting and mixing the resin according to the functional requirements of the product; step A3: pouring or injecting the axial fibers of step A1 and the resin of step A2, and heating and molding them.
4. A fiber reinforced buckle molding process as claimed in claim 1 or 3, characterized in that: In the step A2, the content of the resin is 30% to 50%.
5. A fiber reinforced buckle molding process as claimed in claim 1, characterized in that: The method also includes the following steps after step D: step E: attaching the pre-prepared film-like resin material to the product surface of the fiber-reinforced fastener in step D.
6. A fiber reinforced buckle molding process as claimed in claim 1, characterized in that: In step C, a pre-prepared film-like resin material is attached to the mold, so that the surface of the fiber-reinforced fastener in step D is formed with a pattern of the film-like resin material.
7. A fiber reinforced buckle molding process as claimed in claim 1, characterized in that: In step D, the heating molding includes any one of compression molding, bag pressing molding, heating molding after wrapping with a heat shrinkable film, or injection molding.
8. A fiber-reinforced fastener prepared using the molding process as claimed in any one of claims 1 to 7.
Citation Information
Patent Citations
Novel safe knot
CN204888938U
Belt clasp is made from carbon fibre reinforced plastics as buckle, hook or coupling lock with no metal parts