C-shaped channel semiconductor device, manufacturing method thereof, and electronic device including the same

By adopting C-shaped nanosheets or nanowire channel sections in semiconductor devices and forming a gate stack around them, the limitations of device performance and density improvement in the prior art are solved, and high-performance and high-density semiconductor devices are achieved.

CN111261700BActive Publication Date: 2024-11-19INST OF MICROELECTRONICS CHINESE ACAD OF SCI LTD
View PDF 7 Cites 0 Cited by

Patent Information

Application Number
CN202010072948.3
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2020-01-21
Publication Date
2024-11-19
Estimated Expiration
2040-01-21

AI Technical Summary

Technical Problem

Existing semiconductor devices have limitations in increasing integration density and enhancing device performance, especially the difficulty in controlling the thickness and diameter of nanosheets or nanowires due to process fluctuations.

Method used

Semiconductor devices using C-shaped nanosheets or nanowire channel sections are used to determine the channel by forming multiple C-shaped curved nanosheets or nanowire channels on the substrate and forming a gate stack around their periphery. Dimensions and gate lengths avoid uncertainty in etching and lithography.

Benefits of technology

High-performance and high-density semiconductor devices are achieved, and the channel thickness and gate length are accurately controlled through epitaxial growth processes, improving the current driving capability and performance stability of the device.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN111261700B_ABST
    Figure CN111261700B_ABST
Patent Text Reader

Abstract

Disclosed are a C-shaped channel semiconductor device, a manufacturing method thereof, and an electronic device including the semiconductor device. According to an embodiment, the semiconductor device may include: a channel on a substrate, the channel including two or more curved nanosheets or nanowires spaced apart from each other in a lateral direction relative to the substrate and each having a C-shaped cross section; source / drain portions located at upper and lower ends of the channel relative to the substrate; and a gate stack surrounding the periphery of each nanosheet or nanowire in the channel.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present disclosure relates to the field of semiconductors, and more particularly, to a semiconductor device having a C-shaped nanosheet or nanowire channel portion, a method for manufacturing the same, and an electronic device including the semiconductor device. Background Art

[0002] With the continuous miniaturization of semiconductor devices, various devices with different structures have been proposed, such as fin field effect transistors (FinFETs), multi-bridge channel field effect transistors (MBCFETs), etc. However, due to the limitations of the device structure, the room for improvement of these devices in increasing integration density and enhancing device performance still cannot meet the requirements.

[0003] In addition, due to fluctuations in processes such as lithography and etching, it is difficult to control the thickness or diameter of vertical nanosheets or nanowires such as metal oxide semiconductor field effect transistors (MOSFETs). Summary of the invention

[0004] In view of the above, an object of the present disclosure is at least partially to provide a semiconductor device having a C-shaped nanosheet or nanowire channel portion, a method for manufacturing the same, and an electronic device including the semiconductor device.

[0005] According to one aspect of the present disclosure, a semiconductor device is provided, comprising: a channel portion on a substrate, the channel portion comprising two or more curved nanosheets or nanowires spaced apart from each other in a lateral direction relative to the substrate and each having a C-shaped cross-section; source / drain portions located at the upper and lower ends of the channel portion respectively relative to the substrate; and a gate stack surrounding the periphery of each nanosheet or nanowire in the channel portion.

[0006] According to another aspect of the present disclosure, a method for manufacturing a semiconductor device is provided, comprising: arranging a stack of a first material layer, a second material layer, and a third material layer on a substrate; composing the stack into a strip structure extending along a first direction; making the sidewalls of the second material layer laterally recessed relative to the sidewalls of the first material layer and the third material layer on opposite sides of the strip structure in a second direction intersecting the first direction, thereby defining a first recessed portion; forming a first channel layer on the sidewalls of the second material layer exposed by the first recessed portion; forming a first position holding layer in the remaining space of the first recessed portion; forming a source / drain portion in the first material layer and the third material layer; separating the strip structure into several segments in the first direction; forming an isolation layer on the substrate; removing the second material layer and the first position holding layer; and forming a gate stack around the first channel layer on the isolation layer.

[0007] According to another aspect of the present disclosure, an electronic device is provided, comprising the above-mentioned semiconductor device.

[0008] According to the embodiments of the present disclosure, a semiconductor device with a novel structure is proposed, which can have the advantages of high performance and high density. BRIEF DESCRIPTION OF THE DRAWINGS

[0009] The above and other objects, features and advantages of the present disclosure will become more apparent through the following description of the embodiments of the present disclosure with reference to the accompanying drawings, in which:

[0010] Figures 1 to 24(c) Some stages in the process of manufacturing a semiconductor device according to an embodiment of the present disclosure are schematically shown;

[0011] Fig.25 schematically illustrates a stacking configuration of a channel layer according to another embodiment of the present disclosure;

[0012] Figures 26 to 29 Some stages in a process of manufacturing a semiconductor device according to another embodiment of the present disclosure are schematically shown, wherein:

[0013] Figure 1 , 2 , 3(a), 4 to 9, 10(a), 10(b), 11, 12, 13(a), 13(b), 16(a), 17(a), 18(a), 19(a), 21(a), 22(a), 23(a), 24(a), 26 to 29 are cross-sectional views along line AA′;

[0014] Figure 3(b) , 3(c) , 14(a), 14(b), 15(a), 19(d), 20, 24(c) are top views;

[0015] Figure 15(b) , 16(b) , 16(c), 17(b), 17(c), 18(b), 19(b), 21(b), 22(b), 23(b), 24(b) are cross-sectional views along line BB′;

[0016] Figure 18(c) , 19(c) , 21(c), 22(c), and 23(c) are cross-sectional views along line CC′;

[0017] Fig.25 It is a partial cross-sectional view along line AA′.

[0018] Throughout the drawings, the same or similar reference numerals refer to the same or similar parts. DETAILED DESCRIPTION

[0019] Hereinafter, embodiments of the present disclosure will be described with reference to the accompanying drawings. However, it should be understood that these descriptions are exemplary only and are not intended to limit the scope of the present disclosure. In addition, in the following description, descriptions of well-known structures and technologies are omitted to avoid unnecessary confusion of the concepts of the present disclosure.

[0020] Various structural schematic diagrams according to embodiments of the present disclosure are shown in the accompanying drawings. These figures are not drawn to scale, and some details are magnified and some details may be omitted for the purpose of clear expression. The shapes of various regions and layers shown in the figures and the relative sizes and positional relationships therebetween are only exemplary, and may deviate in practice due to manufacturing tolerances or technical limitations, and those skilled in the art may further design regions / layers with different shapes, sizes, and relative positions according to actual needs.

[0021] In the context of the present disclosure, when a layer / element is referred to as being "on" another layer / element, the layer / element may be directly on the other layer / element or an intervening layer / element may exist therebetween. In addition, if a layer / element is "on" another layer / element in one orientation, the layer / element may be "below" the other layer / element when the orientation is reversed.

[0022] According to an embodiment of the present disclosure, a vertical semiconductor device is provided, having an active area arranged vertically on a substrate (for example, in a direction substantially perpendicular to the surface of the substrate). The channel portion may include two or more curved nanosheets or nanowires that are spaced apart from each other in a lateral direction relative to the substrate (for example, the second direction described below) and each of which has a C-shaped cross-section (for example, a cross-section perpendicular to the surface of the substrate, which may also be perpendicular to the first direction described below), so that such a device may be referred to as a multi-C-channel field effect transistor (C-Channel FET), i.e., mCCFET. The channel portion includes a plurality of nanosheets or nanowires, which may enhance the current driving capability of the device. As described below, each nanosheet or nanowire may be formed by epitaxial growth, and thus may be an integrated monolithic piece and may have a substantially uniform thickness.

[0023] At least some of the nanosheets or nanowires included in the semiconductor device may differ in at least one of thickness, material, and doping concentration to adjust device performance. The number of nanosheets or nanowires included in the channel portion may differ between different semiconductor devices on the substrate. Similarly, the nanosheets or nanowires may differ in at least one of thickness, material, and doping concentration between different semiconductor devices.

[0024] At least some of the nanosheets or nanowires in the channel portion may include a plurality of sub-nanosheets or sub-nanowires stacked in sequence in the second direction and each having a C-shaped cross section (e.g., a cross section perpendicular to the substrate surface, which may also be perpendicular to the first direction). Here, the sub-nanosheets or sub-nanowires may be identical or similar to the nanosheets or nanowires in physical configuration, except that the sub-nanosheets or sub-nanowires may be closely aligned side by side to form a single "nanosheet or nanowire". Therefore, the contents described herein regarding nanosheets or nanowires may also be applicable to sub-nanosheets or sub-nanowires.

[0025] At least some of the multiple sub-nanosheets or sub-nanowires included in the same nanosheet or nanowire may have different characteristics to optimize device performance. For example, the multiple sub-nanosheets or sub-nanowires may include a first sub-nanosheet or sub-nanowire and a second sub-nanosheet or sub-nanowire respectively located on both sides of the corresponding nanosheet or nanowire in the second direction, and a third sub-nanosheet or sub-nanowire located between the first sub-nanosheet or sub-nanowire and the second sub-nanosheet or sub-nanowire. The first sub-nanosheet or sub-nanowire and the second sub-nanosheet or sub-nanowire may have improved interface quality with the gate stack, while the third sub-nanosheet or sub-nanowire may have high carrier mobility. Additionally or alternatively, the first sub-nanosheet or sub-nanowire and the second sub-nanosheet or sub-nanowire may have high carrier mobility, while the third sub-nanosheet or sub-nanowire may optimize carrier distribution. Additionally or alternatively, the third sub-nanosheet or sub-nanowire may confine carriers in the first sub-nanosheet or sub-nanowire and / or the second sub-nanosheet or sub-nanowire. For example, for an n-type device, the lowest energy level of the conduction band of the third sub-nanosheet or sub-nanowire can be higher than the lowest energy level of the conduction band of the first sub-nanosheet or sub-nanowire and / or the second sub-nanosheet or sub-nanowire; for a p-type device, the highest energy level of the valence band of the third sub-nanosheet or sub-nanowire can be lower than the highest energy level of the valence band of the first sub-nanosheet or sub-nanowire and / or the second sub-nanosheet or sub-nanowire.

[0026] The number of sub-nanosheets or sub-nanowires included in different nanosheets or nanowires may be different. In addition, the number of sub-nanosheets or sub-nanowires in a stack of sub-nanosheets or sub-nanowires may be different between different devices on a substrate.

[0027] The semiconductor device may also include source / drain portions respectively arranged at the upper and lower ends of the channel portion. The size of the source / drain portion in the lateral direction relative to the substrate may be larger than the size of the channel portion in the corresponding direction to ensure that the upper and lower ends of the channel portion are connected to the source / drain portion. The source / drain portion may have a certain doping. For example, for a p-type device, the source / drain portion may have a p-type doping; for an n-type device, the source / drain portion may have an n-type doping. The channel portion may have a certain doping to adjust the threshold voltage of the device. Alternatively, the semiconductor device may be a junctionless device, in which the channel portion and the source / drain portion may have the same conductivity type of doping. Alternatively, the semiconductor device may be a tunneling device, in which the source / drain portions at both ends of the channel portion may have opposite doping types to each other.

[0028] The source / drain portion may be disposed in the corresponding semiconductor layer. For example, the source / drain portion may be a doped region in the corresponding semiconductor layer. The source / drain portion may be a portion or the entirety of the corresponding semiconductor layer. In the case where the source / drain portion is a portion of the corresponding semiconductor layer, a doping concentration interface may exist between the source / drain portion and the remaining portion in the corresponding semiconductor layer. As described below, the source / drain portion may be formed by diffusion doping. In this case, the doping concentration interface may be substantially along a vertical direction relative to the substrate.

[0029] The channel portion may include a single crystal semiconductor material. Of course, the source / drain portion or the semiconductor layer in which they are formed may also include a single crystal semiconductor material. For example, they may be formed by epitaxial growth.

[0030] The semiconductor device may also include a gate stack surrounding the periphery of the channel portion, more specifically surrounding the periphery of each channel layer in the channel portion. Therefore, the semiconductor device according to an embodiment of the present disclosure may be a gate-enclosed device. According to an embodiment of the present disclosure, the gate stack may be self-aligned to the channel portion. For example, at least a portion of the gate stack adjacent to the channel portion may be substantially coplanar with the channel portion, for example, the portion of the gate stack and the upper surface and / or lower surface of the channel portion are substantially coplanar with each other.

[0031] Such a semiconductor device can be manufactured, for example, as follows.

[0032] According to an embodiment, a stack of a first material layer, a second material layer, and a third material layer may be provided on a substrate. The first material layer may define the position of a lower source / drain portion, the second material layer may define the position of a gate stack, and the third material layer may define the position of an upper source / drain portion. The first material layer may be provided by a substrate, such as an upper portion of a substrate, and the second material layer and the third material layer may be sequentially formed on the first material layer by, for example, epitaxial growth. Alternatively, the first material layer, the second material layer, and the third material layer may be sequentially formed on the substrate by, for example, epitaxial growth. The first material layer and the third material layer may be in-situ doped while epitaxially growing to form a source / drain portion therein.

[0033] The stack may be patterned into a strip-like structure extending in a first direction. The sidewalls of the second material layer may be laterally recessed relative to the sidewalls of the first material layer and the third material layer on opposite sides of the strip-like structure in a second direction intersecting (e.g., perpendicular) to the first direction, thereby defining a first recessed portion. The first recessed portion may have a curved surface recessed toward the inner side of the strip-like structure.

[0034] A channel portion may be formed on the sidewall of the first recess (i.e., the sidewall of the second material layer exposed in the first recess). For example, a first active layer may be formed by epitaxial growth on the exposed surface of the strip structure, and the portion of the first active layer located on the surface of the first recess may be used as a channel portion (may also be referred to as a "(first) channel layer"). Two first channel layers may be formed based on the first active layer on the opposite sidewalls of the strip structure. Thus, a multi-channel device may be formed. A first position holding layer may be formed in the first recess having the first channel layer formed on the surface.

[0035] After defining the first recessed portion and before forming the first active layer, the exposed surface of the strip structure may be etched back by a certain amount, for example, approximately the thickness of the first active layer to be formed. This helps to ensure that the gate stack formed subsequently has substantially equal gate lengths on opposite sides of the channel layer obtained from the first active layer.

[0036] To achieve more channel layers, similar treatments can be performed. For example, the sidewalls of the first position-maintaining layer can be laterally recessed relative to the sidewalls of the first material layer and the third material layer on opposite sides of the strip structure in the second direction, thereby defining a second recessed portion. The second recessed portion can have a curved surface recessed toward the inner side of the strip structure. A second channel layer can be formed on the sidewalls of the second recessed portion (i.e., the sidewalls of the first position-maintaining layer exposed in the second recessed portion), for example, by epitaxial growth. To achieve epitaxial growth, the first position-maintaining layer can be formed by epitaxial growth. A second position-maintaining layer formed in a second recessed portion having a second channel layer formed on the surface.

[0037] Similarly, after defining the second recessed portion and before forming the second channel layer, an etch-back operation may also be performed, and the etch-back amount is, for example, substantially equal to the thickness of the second channel layer.

[0038] Through this recess-growth process, more channel layers can be realized.

[0039] The source / drain portion may be formed in the first material layer and the third material layer. For example, the source / drain portion may be formed by doping the first material layer and the third material layer (particularly when they are not doped when formed). Such doping may be achieved through a solid phase dopant source layer.

[0040] An opening may be formed in the strip structure (e.g., extending along the second direction) to separate the strip structure into a plurality of segments in the first direction (respectively used as active regions of devices adjacent to each other in the first direction). The opening may extend substantially along the second direction. Through the opening, the second material layer and the inner position holding layer may be exposed.

[0041] The second material layer and each position holding layer may be replaced with a gate stack by a replacement gate process, thereby forming a gate stack surrounding each channel layer in the channel portion.

[0042] According to other embodiments of the present disclosure, another opening (e.g., extending along the first direction) may be formed in the strip-like structure to separate the strip-like structure into, for example, two parts in the second direction. The opening may be in the middle of the strip-like structure extending along the first direction, so that the two parts may be substantially symmetrical with respect to each other.

[0043] According to an embodiment of the present disclosure, the thickness and gate length of the nanosheet or nanowire used as the channel portion and possible sub-nanosheets or sub-nanowires are mainly determined by epitaxial growth rather than by etching or lithography, so that good channel size / thickness and gate length control can be achieved.

[0044] The present disclosure may be presented in various forms, some examples of which are described below. In the following description, various material selections are involved. In addition to considering its function (for example, semiconductor materials are used to form active areas and dielectric materials are used to form electrical isolation), the selection of materials also takes into account etching selectivity. In the following description, the required etching selectivity may or may not be indicated. It should be clear to those skilled in the art that when the following mentions etching a certain material layer, if it is not mentioned that other layers are also etched or it is not shown in the figure that other layers are also etched, then such etching can be selective, and the material layer can have etching selectivity relative to other layers exposed to the same etching recipe.

[0045] Figures 1 to 24(c) Some stages in a process of manufacturing a semiconductor device according to an embodiment of the present disclosure are schematically shown.

[0046] like Figure 1 As shown, a substrate 1001 is provided (the upper part of which may constitute the first material layer mentioned above). The substrate 1001 may be a substrate of various forms, including but not limited to a bulk semiconductor material substrate such as a bulk Si substrate, a semiconductor on insulator (SOI) substrate, a compound semiconductor substrate such as a SiGe substrate, etc. In the following description, for convenience of explanation, a bulk Si substrate is taken as an example. Here, a silicon wafer is provided as the substrate 1001.

[0047] In the substrate 1001, a well region may be formed. If a p-type device is to be formed, the well region may be an n-type well; if an n-type device is to be formed, the well region may be a p-type well. The well region may be formed, for example, by injecting a corresponding conductive type dopant (a p-type dopant such as B or In, or an n-type dopant such as As or P) into the substrate 1001 and then performing thermal annealing. There are many ways to set such a well region in the art, which will not be described in detail here.

[0048] In this example, a p-type device and an n-type device are formed simultaneously, and the p-type device and the n-type device are adjacent to each other (a complementary metal oxide semiconductor (CMOS) configuration may be formed later), thereby forming an adjacent n-type well and a p-type well. However, the present disclosure is not limited thereto. For example, devices of the same conductivity type may be formed. Alternatively, devices of different conductivity types may be formed, but the p-type device is formed in a certain region and the n-type device is formed in another region.

[0049] On the substrate 1001, a second material layer 1003 and a third material layer 1005 may be formed by, for example, epitaxial growth. The second material layer 1003 may be used to define the position of the gate stack, and the thickness may be, for example, about 20 nm to 50 nm. The third material layer 1005 may be used to define the position of the upper source / drain portion, and the thickness may be, for example, about 20 nm to 200 nm.

[0050] The substrate 1001 and the adjacent layers of the above layers formed thereon may have etching selectivity relative to each other. For example, when the substrate 1001 is a silicon wafer, the second material layer 1003 may include SiGe (for example, Ge atomic percentage is about 10%-30%), and the third material layer 1005 may include Si.

[0051] To facilitate composition, Figure 2 As shown, a hard mask layer 1009 may be formed on the third material layer 1005 by, for example, deposition. For example, the hard mask layer 1009 may include nitride (e.g., silicon nitride) with a thickness of about 30 nm-100 nm. In addition, for better etching control, an etch stop layer 1007 may be formed first by, for example, deposition. For example, the etch stop layer 1007 may include oxide (e.g., silicon oxide) with a thickness of about 1 nm-10 nm.

[0052] The hard mask layer 1009 may be used to pattern the active area.

[0053] For example, Figure 3(a) and 3(b)As shown, a photoresist 1011 can be formed on the hard mask layer 1009 and patterned into a strip extending along a first direction (a direction perpendicular to the paper in FIG. 3 (a), and a vertical direction within the paper in FIG. 3 (b)) by photolithography. The photoresist 1011 can be used as an etching mask, and the hard mask layer 1013 can be selectively etched by, for example, reactive ion etching (RIE), and the pattern of the photoresist can be transferred to the hard mask layer 1013. The etching can be stopped at the etching stop layer 1009. Then, the layers below can be selectively etched in sequence by, for example, RIE. The etching can be carried out into the substrate 1001, especially the well region therein.

[0054] Therefore, in the p-type device area (the area above the n-type well area) and the n-type device area (the area above the p-type well area), the third material layer 1005, the second material layer 1003 and the upper part of the substrate 1001 (the first material layer) are composed into strip structures R1 and R2, respectively.

[0055] In this example, the strip structure R1 on the p-type device region is wider than the strip structure R2 on the n-type device region because a greater number of channel layers are formed for the p-type device in this example. However, the present disclosure is not limited thereto, and the widths of the strip structures R1 and R2 may be adjusted according to the number of channel layers to be formed. Figure 3(a) and 3(b) Horizontal dimensions within the paper).

[0056] In addition, in the example shown in FIG3(b), the strip structures R1 and R2 extend continuously along the first direction (corresponding to the active regions of several devices and then separated). Note that FIG3(b) only shows a local area on the wafer, so the upper and lower ends in FIG3(b) may not be the true ends of the strip structures R1 and R2, and the strip structures R1 and R2 may extend in the first direction beyond the range shown in FIG3(b).

[0057] Figure 3(c) shows the end of the strip structures R1 and R2. As described below, the channel layer may be formed at the end of the strip structures R1 and R2. In order to make the channel layer extend continuously and smoothly, the end of the strip structures R1 and R2 may be rounded.

[0058] In the following, for convenience, the situation shown in FIG. 3( b ) is mainly described as an example.

[0059] In this example, the depth of etching into the well region is not great, so that a contact region for the lower source / drain portion is subsequently formed around the lower source / drain portion. According to an embodiment of the present disclosure, the substrate 1001 may be further etched around the contact region to form a groove in the substrate 1001. Isolation, such as shallow trench isolation (STI), may then be formed in the formed groove.

[0060] According to the embodiments of the present disclosure, a region where a contact region for a lower source / drain portion is to be formed may be defined in a self-aligned manner.

[0061] For example, Figure 4 As shown, partition walls 1013 may be formed on the sidewalls of the strip structures R1 and R2, particularly on the opposite sidewalls in a second direction intersecting (e.g., perpendicular) to the first direction. For example, a layer of oxide may be deposited in a substantially conformal manner (the thickness of which may be adjusted according to the size of the contact region to be formed), and then the deposited oxide layer may be anisotropically etched in a vertical direction, such as by RIE, to remove its lateral extension portion and leave its vertical extension portion, thereby obtaining the partition walls 1013.

[0062] The substrate 1001 can be selectively etched, such as RIE, using the hard mask layer 1009 and the partition wall 1013 as etching masks, thereby forming grooves for isolation in the substrate 1001. These grooves are also self-aligned with the strip structures R1 and R2 and formed around the strip structures R1 and R2, which helps to save area.

[0063] Here, the groove between the p-type device region and the n-type device region passes through the pn junction between the n-type well and the p-type well.

[0064] The STI can be formed by filling the groove with a dielectric material such as oxide. Figure 5 As shown, an oxide may be formed on the substrate by, for example, deposition. The deposited oxide may be planarized, such as by chemical mechanical polishing (CMP) (may stop at the hard mask layer 1009), and then etched back. The etch back may be performed until the surface of the substrate 1001 originally blocked by the partition wall 1013 is exposed to form an isolation layer 1015. During the etch back, the partition wall 1013, which is also an oxide, may be removed.

[0065] Afterwards, source / drain doping can be performed.

[0066] like Figure 6 As shown, a solid-phase dopant source layer can be formed on the sidewalls of the strip structures R1 and R2 by, for example, deposition. Here, solid-phase dopant source layers for p-type devices and n-type devices can be formed respectively. For example, a solid-phase dopant source layer 1017p for a p-type device can be formed, and the solid-phase dopant source layer 1017p can be positioned in the p-type device region by photolithography, especially covering the strip structure R1 therein. Similarly, a solid-phase dopant source layer 1017n for an n-type device can be formed, and the solid-phase dopant source layer 1017n can be positioned in the n-type device region by photolithography, especially covering the strip structure R2 therein.

[0067] The solid-phase dopant source layers 1017p and 1017n may be formed in a substantially conformal manner. For example, the solid-phase dopant source layers 1017p and 1017n may be oxides containing dopants with a thickness of about 1 nm to 5 nm. The dopants contained in the solid-phase dopant source layers 1017p and 1017n may be used to dope the source / drain portion (and optionally, the exposed surface of the substrate 1001), and thus may have the same conductivity type as the source / drain portion to be formed. For example, for a p-type device, the solid-phase dopant source layer 1017p may contain a p-type dopant such as B or 1n; for an n-type device, the solid-phase dopant source layer 1017n may contain an n-type dopant such as P or As. The concentration of the dopant in the solid-phase dopant source layer 1029 may be about 0.1% to 5%.

[0068] By annealing, the dopants in the solid phase dopant source layers 1017p and 1017n can be driven into the first material layer and the third material layer to form a source / drain portion S / Dp for a p-type device and a source / drain portion S / Dn for an n-type device (and optionally, can be driven into the exposed surface of the substrate 1001 to form respective contact regions of the source / drain portions at the lower ends of the two devices), as shown in FIG. Figure 7 The concentration of the dopant in the source / drain region may be about 1E18-1E21 cm -3 Thereafter, the solid phase dopant source layers 1017p, 1017n may be removed.

[0069] exist Figure 7 In FIG. 1 , the regions where the dopants are driven in are schematically shown with diagonal hatching. In the following figures, these diagonal hatchings are no longer shown for the sake of simplicity.

[0070] In this example, the first material layer is provided through the upper portion of the substrate 1001. However, the present disclosure is not limited thereto. For example, the first material layer may also be an epitaxial layer on the substrate 1001. In this case, the first material layer and the third material layer may be doped in situ during epitaxy, rather than being doped using a solid phase dopant source layer.

[0071] Next, the channel layer may be fabricated.

[0072] In this example, the channel layers for the p-type device and the n-type device are different (in at least one aspect such as quantity, material, thickness, doping, etc.), so the p-type device and the n-type device can be processed separately. Figure 8 As shown, a shielding layer 1019 may be formed on the p-type device region by, for example, deposition and etching. For example, the shielding layer 1019 may include SiC.

[0073] In addition, before forming the shielding layer 1019, the thickness of the isolation layer 1015 may be increased. For example, the thickness of the isolation layer 1015 may be increased so as to shield the contact region for the lower source / drain portion (to prevent the channel layer from growing on the contact region later). Of course, the top surface of the isolation layer 1015 after the increase may not exceed the bottom surface of the second material layer so as not to affect the formation of the channel layer on the sidewall of the second material layer. The increase of the isolation layer 1015 may be achieved by depositing oxide, planarizing the deposited oxide, and then etching back the oxide.

[0074] According to an embodiment of the present disclosure, in order to form a gate stack surrounding the channel portion, a space for the gate stack may be reserved on the side of the strip structure R2, especially on both sides in the second direction. Fig. 9 As shown, the second material layer 1003 can be selectively etched so that its sidewalls in the second direction are relatively concave. In order to better control the amount of etching, atomic layer etching (ALE) can be used. For example, the amount of etching can be about 10nm-40nm. Depending on the characteristics of the etching, such as the etching selectivity of the second material layer 1003 relative to the substrate 1001 and the third material layer 1005, the sidewalls of the second material layer 1003 after etching can present different shapes. Fig. 9 , it is shown that the sidewall of the second material layer 1003 after etching is a C-shape that is concave inward. However, the present disclosure is not limited to this. For example, when the etching selectivity is good, the sidewall of the second material layer 1003 after etching can be close to vertical. Here, the etching can be isotropic, especially when a large etching amount is required. The C-shape formed on both sides can be symmetrical with respect to each other, for example, symmetrical about the center plane of the strip structure R2. Typically, the C-shaped sidewall of the second material layer 1003 has a larger curvature at the upper and lower ends, and a smaller curvature at the waist or middle.

[0075] A first channel layer for an n-type device may be formed on the sidewalls of the strip structure R2 to define a channel portion later. In order to keep the gate lengths (e.g., along a direction perpendicular to the substrate surface) substantially equal when gate stacks are subsequently formed on the left and right sides of the C-shaped channel layer, as shown in FIG. Fig. 9As shown, the strip structure R2 (specifically, the exposed surfaces of the first material layer, the second material layer, and the third material layer) can be etched back so that the peripheral sidewall thereof is laterally recessed relative to the peripheral sidewall of the hard mask layer 1009. In order to better control the amount of etch back, ALE can be used. The amount of etch back can be substantially equal to the thickness of the first channel layer to be grown subsequently, for example, about 5nm-15nm. Then, a first channel layer 1021n for an n-type device can be formed on the sidewall of the strip structure R2 by, for example, selective epitaxial growth. Due to the selective epitaxial growth, the first channel layer 1021n for an n-type device may not be formed on the surface of the isolation layer 1015. The first channel layer 1021n for an n-type device can then define a channel portion, and the thickness is, for example, about 3nm-15nm. According to an embodiment of the present disclosure, the thickness of the first channel layer 1021n for an n-type device (subsequently used as a channel portion) can be determined by an epitaxial growth process, so the thickness of the channel portion can be better controlled.

[0076] exist Fig. 9 , the sidewalls of the first channel layer 1021n for n-type devices on the sidewalls of the first material layer and the third material layer are shown to be substantially flush with the sidewalls of the hard mask layer 1009. This can be achieved by controlling the etch-back amount and the epitaxial growth thickness to be substantially the same. However, the present disclosure is not limited thereto. For example, the sidewalls of the first channel layer 1021n for n-type devices on the sidewalls of the first material layer and the third material layer may be recessed relative to the sidewalls of the hard mask layer 1009, or may even protrude.

[0077] Here, the above-mentioned etch-back can etch the upper end and the lower end of the recessed portion upward and downward, respectively, so that after the first channel layer 1021n is grown, the height t1 of the recessed portion and the thickness t2 of the second material layer 1003 can be substantially the same. In this way, the gate stacks subsequently formed on the left and right sides of the first channel layer 1021n can have substantially equal gate lengths. However, the present disclosure is not limited thereto. According to an embodiment of the present disclosure, the gate length outside the first channel layer 1021n can also be changed by adjusting the etch-back amount, thereby changing the ratio of the gate lengths on both sides, so as to optimize the impact of the different morphologies on the left and right sides of the C-shaped channel portion on the device performance.

[0078] The material of the first channel layer 1021n for the n-type device can be appropriately selected according to the performance requirements of the device in the design. For example, the first channel layer 1021n for the n-type device can include various semiconductor materials, such as Si, Ge, SiGe, InP, GaAs, InGaAs, etc. In this example, the first channel layer 1021n for the n-type device can include the same material as the first material layer and the third material layer, such as Si. In addition, as needed, the first channel layer 1021n for the n-type device can be in-situ doped when it is grown to adjust the threshold voltage of the n-type device.

[0079] Next, the p-type device region can be processed similarly. As shown in FIG. 10( a), a shielding layer 1023 can be formed on the n-type device region by, for example, deposition and etching. For example, the shielding layer 1023 can include SiC. When etching the shielding layer 1023, the shielding layer 1019 on the p-type device region can be removed. In addition, the shielding layer 1023 can enter the recess of the strip structure R2 to form a position holding layer to maintain space for subsequently forming a gate stack.

[0080] In this example, the position-keeping layer and the shielding layer are formed together. However, the present disclosure is not limited thereto. According to other embodiments of the present disclosure, the position-keeping layer may be formed separately. For example, as shown in FIG. 10( b), a position-keeping layer 1023 a may be formed in the recess of the strip structure R2, and then a shielding layer 1023 b may be formed to shield the n-type device region. In order to be removed together with the second material layer 1003 in the following replacement gate process, the position-keeping layer 1023 a may include the same material as the second material layer 1003, such as SiGe. The position-keeping layer 1023 a may be formed by epitaxially growing SiGe and then selectively etching the epitaxially grown SiGe, such as RIE (for example, with the hard mask layer 1009 as an etching mask). The concentration of Ge in the SiGe included in the position-keeping layer 1023 a may be substantially the same as the concentration of Ge in the second material layer 1003, and may be in-situ doped during growth to be substantially the same as the doping concentration in the second material layer 1003 (doped when forming the source / drain portion). Thus, in the subsequent replacement gate process, the position maintaining layer 1023 a and the second material layer 1003 may be removed at substantially the same etching rate.

[0081] Similarly, space for gate stacking may be reserved on the sides of the strip structure R1, especially on both sides in the second direction. Figure 10(a) and 10(b) As shown, the second material layer 1003 can be selectively etched so that its sidewalls in the second direction are relatively concave. In order to better control the amount of etching, ALE can be used. For example, the amount of etching is large (because the number of channel layers to be formed is large), which can be about 20nm-60nm. Depending on the characteristics of the etching, such as the etching selectivity of the second material layer 1003 relative to the substrate 1001 and the third material layer 1005, the sidewalls of the second material layer 1003 after etching can present different shapes. Figure 10(a) and 10(b), it is shown that the sidewall of the second material layer 1003 after etching is a C-shape that is concave inward. However, the present disclosure is not limited to this. For example, when the etching selectivity is good, the sidewall of the second material layer 1003 after etching can be close to vertical. Here, the etching can be isotropic, especially when a large etching amount is required. The C-shape formed on both sides can be symmetrical with respect to each other, for example, symmetrical about the center plane of the strip structure R1. Typically, the C-shaped sidewall of the second material layer 1003 has a larger curvature at the upper and lower ends, and a smaller curvature at the waist or middle.

[0082] A first channel layer for a p-type device may be formed on the sidewall of the strip structure R1 so as to subsequently define a channel portion. In order to keep their gate lengths (e.g., in a direction perpendicular to the substrate surface) substantially equal when gate stacks are subsequently formed on the left and right sides of the C-shaped channel layer, the strip structure R1 (specifically, the exposed surfaces of the first material layer, the second material layer, and the third material layer) may be etched back so that its peripheral sidewalls are laterally recessed relative to the peripheral sidewalls of the hard mask layer 1009. In order to better control the amount of etch-back, ALE may be used. The amount of etch-back may be substantially equal to the thickness of the first channel layer to be grown subsequently, for example, about 5nm-15nm. Then, a first channel layer 1021p-1 for a p-type device may be formed on the sidewall of the strip structure R1 by, for example, selective epitaxial growth. Due to the selective epitaxial growth, the first channel layer 1021p-1 for a p-type device may not be formed on the surface of the isolation layer 1015. The first channel layer 1021p-1 for the p-type device may then define a channel portion, and may have a thickness of, for example, about 3nm-15nm. According to an embodiment of the present disclosure, the thickness of the first channel layer 1021p-1 for the p-type device (later used as the channel portion) may be determined by an epitaxial growth process, and thus the thickness of the channel portion may be better controlled.

[0083] exist Figure 10(a) and 10(b) , the sidewalls of the first channel layer 1021p-1 for a p-type device on the sidewalls of the first material layer and the third material layer are shown to be substantially flush with the sidewalls of the hard mask layer 1009. This can be achieved by controlling the etch-back amount and the epitaxial growth thickness to be substantially the same. However, the present disclosure is not limited thereto. For example, the sidewalls of the first channel layer 1021p-1 for a p-type device on the sidewalls of the first material layer and the third material layer may be recessed relative to the sidewalls of the hard mask layer 1009, or may even protrude.

[0084] Similarly, the above-mentioned etch back can etch the upper end and the lower end of the recessed portion upward and downward, respectively, so that after the first channel layer 1021p-1 is grown, the height of the recessed portion and the thickness of the second material layer 1003 can be substantially the same. In this way, the gate stacks subsequently formed on the left and right sides of the first channel layer 1021p-1 can have substantially equal gate lengths. However, the present disclosure is not limited thereto. According to an embodiment of the present disclosure, the gate length outside the first channel layer 1021p-1 can also be changed by adjusting the etch back amount, thereby changing the ratio of the gate lengths on both sides, so as to optimize the impact of the different morphologies on the left and right sides of the C-shaped channel portion on the device performance.

[0085] The material of the first channel layer 1021p-1 for the p-type device can be appropriately selected according to the performance requirements of the device in the design. For example, the first channel layer 1021p-1 for the p-type device can include various semiconductor materials, such as Si, Ge, SiGe, InP, GaAs, InGaAs, etc. In this example, the first channel layer 1021p-1 for the p-type device can include the same material as the first material layer and the third material layer, such as Si. In addition, as needed, the first channel layer 1021p-1 for the p-type device can be in-situ doped when it is grown to adjust the threshold voltage of the p-type device.

[0086] In this example, the first channel layer formed on the p-type device region and the n-type device region may have substantially the same features (e.g., material, size, etc.). However, the present disclosure is not limited thereto. According to the design performance requirements for the two devices, the first channel layer formed on the p-type device region and the n-type device region may have different features, such as thickness, material, and doping concentration. For example, for a p-type device, the first channel layer 1021p-1 may include SiGe, Ge, etc.; for an n-type device, the first channel layer 1021n may include InGaAs, InP, or other III-V compound semiconductors, etc. Since the first channel layer grows thinner and the stress can be released in the up and down directions, the quality of the film is relatively less affected by the lattice constant mismatch, and the film quality is better.

[0087] Similar to the position retaining layer 1023 a , a position retaining layer 1025 a may be formed in the recess of the strip structure R1 . The position retaining layer 1025 a may include the same material as the second material layer 1003 .

[0088] Similar to the formation of the first channel layer 1021p-1, a second channel layer 1021p-2 for a p-type device may be formed on the sidewall of the strip structure R1. Fig.12As shown. For example, the position holding layer 1025a can be selectively etched so that its sidewall in the second direction is relatively concave. In order to better control the amount of etching, ALE can be used. For example, the amount of etching is about 10nm-30nm. As described above, in order to keep their gate lengths substantially equal when the gate stacks are subsequently formed on the left and right sides of the C-shaped channel layer, the strip structure R1 can be etched back (more specifically, the surface of the strip structure R1 is currently covered by the position holding layer 1025a and the first channel layer 1021p-1, so the position holding layer 1025a and the first channel layer 1021p-1 can be etched back, and the first channel layer 1021p-1 is thin and may be etched back), and the amount of etching back can be substantially equal to the thickness of the second channel layer to be grown subsequently, for example, about 5nm-15nm. Of course, the ratio of the gate lengths on both sides can also be changed by adjusting the amount of etching back as described above. Then, a second channel layer 1021p-2 for a p-type device may be formed on the sidewalls of the strip structure R1 and the position holding layer 1025a by, for example, selective epitaxial growth. The second channel layer 1021p-2 for a p-type device may then define a channel portion, and may have a thickness of, for example, about 3nm-15nm. According to an embodiment of the present disclosure, the thickness of the second channel layer 1021p-2 for a p-type device (later used as a channel portion) may be determined by an epitaxial growth process, and thus the thickness of the channel portion may be better controlled.

[0089] The material of the second channel layer 1021p-2 for the p-type device can be appropriately selected according to the performance requirements of the device in the design. For example, the second channel layer 1021p-2 for the p-type device can include various semiconductor materials, such as Si, Ge, SiGe, InP, GaAs, InGaAs, etc. In this example, the second channel layer 1021p-2 for the p-type device can include the same material as the first material layer and the third material layer, such as Si. In addition, as needed, the second channel layer 1021p-2 for the p-type device can be in-situ doped when it is grown to adjust the threshold voltage of the p-type device.

[0090] Note that the first channel layer 1021p-1 and the second channel layer 1021p-2 for the p-type device may be different in at least one aspect, such as material, thickness, and doping concentration.

[0091] FIG13(a) shows the case where position-keeping layers 1023p and 1023n of a dielectric such as SiC are formed, and FIG13(b) shows the case where position-keeping layers 1023a and 1025b of the same material as the second material layer 1003 are formed.

[0092] So far, the active region including the source / drain portion and the channel portion has been defined. Currently, the active region is continuous in the first direction. The strip structure can be separated into several sections in the first direction, thereby defining the active region for each individual device respectively.

[0093] For example, as shown in Figure 14(a), a photoresist 1027 can be formed and patterned by photolithography to shield the active regions of each individual device and expose the active regions between the individual devices. Figure 14(b) shows the situation at the end of the stripe structure.

[0094] Then, if Figure 15(a) and 15(b) As shown, the photoresist 1027 can be used as an etching mask, and the third material layer 1005 (upper source / drain portion), the second material layer 1003 (channel portion) and the first material layer (lower source / drain portion) can be cut off in sequence by selective etching such as RIE, so as to separate the active area in the first direction. It should be noted that, according to the device layout design, the lower source / drain portions of some individual devices can remain connected. Afterwards, the photoresist 1027 can be removed.

[0095] Figures 16(a) to 16(c) Figure 2 shows the situation at the end of the strip structure. Figure 16(b) and 16(c) As shown, the channel layer may extend to the end of the strip structure. That is, for a segment separated from the strip structure and including the end of the strip structure, the channel layer may extend continuously between the two sides of the segment in the second direction and one end connecting the two sides (note that the other end of the segment previously did not have a channel layer because it was continuously extended with the adjacent segment, and was exposed to the outside through the above separation process), so that it may be U-shaped in a cross-sectional view parallel to the substrate surface. Figure 16(b) and 16(c) The situations shown differ in the position-keeping layers.

[0096] Due to the separation of active areas between individual devices, an isolation layer can be formed between the active areas of the individual devices. The isolation layer can be formed by depositing oxide, planarizing the deposited oxide and then etching back the oxide. The isolation layer formed in this way is still shown as 1015 together with the isolation layer formed previously. The top surface of the isolation layer 1015 can be near the bottom surface of the original second material layer (the top surface of the first material layer), preferably not higher than the bottom surface of the second material layer to avoid covering the channel portion.

[0097] Next, a replacement gate process may be performed to form a gate stack.

[0098] like Figures 17(a) to 17(c)As shown, each position holding layer can be removed by selective etching. Oxidation treatment can be performed as needed to make the corners of the C-shaped channel portion smooth, thereby improving device performance and reliability. In the case of oxidation treatment, the oxide formed by the oxidation treatment can be removed by selective etching. FIG. 17( b) shows the situation of the segment at the end of the non-strip structure, while FIG. 17( c) shows the situation of the segment at the end of the strip structure.

[0099] Then, if Figures 18(a) to 18(c) As shown, a gate stack can be formed on the isolation layer 1015. For example, a gate dielectric layer 1029 can be formed in a roughly conformal manner by deposition, and a gate conductor layer 1031 can be formed on the gate dielectric layer 1029. The gate conductor layer 1031 can fill the space between the active areas. The gate conductor layer 1031 can be planarized such as by CMP, and the CMP can stop at the hard mask layer 1009. Then, the gate conductor layer 1031 can be etched back, and the top surface of the gate conductor layer 1031 after etching back is preferably higher than the top surface of the original second material layer (or the bottom surface of the third material layer) to ensure that the end of the C-shaped channel portion can be covered by the gate conductor layer, otherwise the end of the C-shaped channel portion may undergo a local threshold voltage change. In this way, the end of the formed gate stack is embedded in the space where the previous position holding layers were located, surrounding the channel portion.

[0100] For example, the gate dielectric layer 1029 may include a high-k gate dielectric such as HfO 2 , with a thickness of, for example, about 1 nm-5 nm. Before forming the high-k gate dielectric, an interface layer may also be formed, such as an oxide formed by an oxidation process or deposition such as atomic layer deposition (ALD), with a thickness of about 0.3 nm-1.5 nm. Here, the gate conductor layer 1031 may be used for a p-type device, and thus may include a work function adjustment metal for a p-type device such as TiN, TaN, etc. and a gate conductive metal such as W, etc.

[0101] As shown in FIG. 18( a ), the gate stack surrounds the channel portion. It can be seen that the channel portion includes a C-shaped curved nanosheet (when the nanosheet is narrow, it can become a nanowire). Due to the high etching selectivity of the second material layer 1003 (SiGe) relative to the channel layer (Si), the thickness of the channel portion (in the case of nanowires, the thickness, or the diameter) is basically determined by the selective growth process of the channel layer. This has a huge advantage over the technology that only uses etching methods or photolithography methods to determine the thickness, because compared to etching or photolithography, the epitaxial growth process has much better process control.

[0102] According to an embodiment of the present disclosure, before forming a gate stack, an annealing treatment may be performed to drive the dopants in the source / drain portion closer to the C-type channel portion, and even a small portion of the dopants may enter both ends of the C-type channel portion to reduce external resistance and improve device performance.

[0103] The gate conductor layer 1031 for the p-type device is currently also formed in the n-type device region. The gate conductor layer 1031 in the n-type device region can be removed, and the landing pad of the gate contact can also be patterned.

[0104] like Figures 19(a) to 19(d) As shown, a photoresist 1033 may be formed and patterned to mask regions where landing pads for gate contacts are to be formed, while exposing other regions. Fig. 20 The situation at the end of the strip structure is shown. Fig. 20 For the sake of convenience, the gate dielectric layer is not shown.

[0105] Then, if Figures 21(a) to 21(c) As shown, the photoresist 1033 (and the hard mask layer 1009) can be used as a mask to selectively etch the gate conductor layer 1031, such as by RIE, and the RIE can stop at the gate dielectric layer 1029. Afterwards, the photoresist 1033 can be removed.

[0106] Thus, the gate conductor layer 1031 substantially remains and is self-aligned under the hard mask layer 1009 , except for a portion protruding at one side (upper side in a top view) of the hard mask layer 1009 to serve as a landing pad.

[0107] Currently, the gate conductor layer 1031 for the p-type device is still left in the n-type device region and can be removed. Figures 22(a) to 22(c) As shown, a shielding layer (e.g., photoresist, not shown) can be formed and patterned to shield the p-type device region and expose the n-type device region. Then, the gate conductor layer 1031 in the n-type device region can be removed by selective etching. Afterwards, the shielding layer can be removed.

[0108] Then, a gate conductor layer 1035 for n-type devices may be formed in a similar manner to the gate conductor layer 1031. The gate conductor layer 1035 may include a work function adjustment metal for n-type devices such as TiN, TaN, TiAlC, etc. and a gate conductive metal such as W, etc.

[0109] Currently, the gate stacks of the two devices are connected to each other as a whole. According to the device design, the gate conductor layer 1035 can be disconnected between the two devices by, for example, photolithography, and the landing pad of the gate contact can also be patterned. This can be done by referring to the above Figures 19(a) to 21(c) The processing described is performed as Figures 23(a) to 23(c) shown.

[0110] Thus, in the p-type device region, the gate conductor layer 1031 substantially remains and self-aligns under the hard mask layer 1009, except for a portion protruding on one side (upper side in top view) of the hard mask layer 1009 to serve as a landing pad. The gate conductor layer 1031 is combined with the gate dielectric layer 1029 to define a gate stack for the p-type device. Similarly, in the n-type device region, the gate conductor layer 1035 substantially remains and self-aligns under the hard mask layer 1009, except for a portion protruding on one side (upper side in top view) of the hard mask layer 1009 to serve as a landing pad. The gate conductor layer 1035 is combined with the gate dielectric layer 1029 to define a gate stack for the p-type device.

[0111] In this example, the p-type device and the n-type device have the same gate dielectric layer 1029. However, the present disclosure is not limited thereto. For example, the p-type device and the n-type device may have different gate dielectric layers. When different materials are used for different types of devices, they may be processed separately. As described above, when processing one type of device, a shielding layer may be used to shield the area where another type of device is located. The processing order thereof may be interchanged.

[0112] At this point, the fabrication of the device infrastructure is complete, and then various contacts, interconnect structures, etc. can be fabricated.

[0113] For example, Figures 24(a) to 24(c) As shown, a dielectric layer 1037 can be formed on the substrate by, for example, deposition and then planarization. Then, a contact hole can be formed, and a conductive material such as metal can be filled in the contact hole to form a contact portion 1039. The contact portion 1039 can include a contact portion penetrating the hard mask layer 1009 and the etch stop layer 1007 to connect to the upper source / drain portion, a contact portion penetrating the dielectric layer 1037 and the isolation layer 1015 to connect to the contact area of ​​the lower source / drain portion, and a contact portion penetrating the dielectric layer 1037 to connect to the landing pad of the gate conductor layer. As shown in FIG. 24(a), the contact portions to the contact area of ​​the lower source / drain portion of each of the two adjacent devices can be located on opposite sides (left and right in the figure) of the active area.

[0114] In the above embodiments, the channel layer is a single-layer structure. However, the present disclosure is not limited thereto. According to other embodiments of the present disclosure, one or more channel layers may include a structure in which multiple sub-layers are stacked.

[0115] For example, Fig.25 As shown, the channel layer (eg, the first channel layer and / or the second channel layer described above) may include a first sublayer 1021-1, a second sublayer 1021-2, and a third sublayer 1021-3 stacked in sequence.

[0116] According to an embodiment of the present disclosure, at least some of the first sub-layer 1021 - 1 , the second sub-layer 1021 - 2 , and the third sub-layer 1021 - 3 may have different characteristics to optimize device performance.

[0117] For example, the second sublayer 1021-2 may include (relative to the first sublayer 1021-1 and the third sublayer 1021-3) a material with high carrier mobility, such as SiGe (for example, Ge atomic percentage is about 30%-100%, and becomes Ge when Ge atomic percentage is 100%), to improve the current capability of the device. However, the interface quality between SiGe and the gate dielectric layer formed subsequently may be poor (for example, the interface state charge density is large, the surface roughness is high, the carrier scattering is large or the channel resistance is large, etc.). For this reason, the first sublayer 1021-1 and the third sublayer 1021-3 may include a material with good interface quality with the gate dielectric layer, such as Si.

[0118] As another example, the first sublayer 1021 - 1 and the third sublayer 1021 - 3 may include materials having high carrier mobility (relative to the second sublayer 1021 - 2 ), and the second sublayer 1021 - 2 may include a material capable of optimizing carrier distribution.

[0119] For another example, the second sublayer 1021-2 can confine carriers in the first sublayer 1021-1 and / or the third sublayer 1021-3, so as to be closer to the gate dielectric layer, which is beneficial to improving the short channel effect and reducing the leakage current. For example, for an n-type device, the lowest energy level of the conduction band of the second sublayer 1021-2 can be higher than the lowest energy level of the conduction band of the first sublayer 1021-1 and / or the third sublayer 1021-3; for a p-type device, the highest energy level of the valence band of the second sublayer 1021-2 can be lower than the highest energy level of the valence band of the first sublayer 1021-1 and / or the third sublayer 1021-3.

[0120] The number of sub-layers included in each channel layer may be different, and the sub-layer stacking structure in different devices may also be different.

[0121] In the above embodiments, source / drain doping is performed through a solid phase dopant source layer. However, the present disclosure is not limited thereto.

[0122] like Fig.26 As shown, on the substrate 1001, the n-type device region can be shielded by photoresist 1041, and the p-type device region can be exposed. In the p-type device region, an n-type well (the concentration of the n-type impurity can be, for example, about 1E17-5E18cm -3 ), and a source / drain region S / Dp for a p-type device can be formed in the n-type well (the concentration of the p-type impurity can be, for example, about 1E19-1E21cm -3According to an embodiment, the concentration of p-type impurities at the top surface may be lower than the concentration of p-type impurities at lower positions to reduce adverse effects on subsequent epitaxial growth.

[0123] The n-type device region can be processed similarly. Fig. 27 As shown, the p-type device region can be shielded by photoresist 1043, and the n-type device region can be exposed. In the n-type device region, a p-type well (the concentration of the p-type impurity can be, for example, about 1E17-5E18cm -3 ), and a source / drain region S / Dn for an n-type device can be formed in the p-type well (the concentration of the n-type impurity can be, for example, about 1E19-1E21cm -3 According to an embodiment, the concentration of n-type impurities at the top surface may be lower than the concentration of n-type impurities at lower positions to reduce adverse effects on subsequent epitaxial growth.

[0124] Then, if Fig.28 As shown, a second material layer 1003 and a third material layer 1005 may be formed on the substrate 1001. For this, please refer to the above description, which will not be repeated here.

[0125] like Fig.29 As shown, it can be combined with Fig.26 and 27 Similar to the process described above, a source / drain region S / Dp for a p-type device is formed in the third material layer 1005 (the concentration of the p-type impurity may be, for example, about 1E19-1E21 cm -3 ) and source / drain regions S / Dn for n-type devices (the concentration of n-type impurities may be, for example, about 1E19-1E21 cm -3 ).

[0126] In this case, the above combination Figure 6 and 7 The described processing can be omitted. Figures 18(a) to 18(c) The annealing process described above (driving the dopants in the source / drain region close to or even into the C-channel region) can still be used, or can be changed to be combined with Figure 15(a) and 15(b) After separating the active regions of the individual devices and combining Figures 17(a) to 17(c) This can reduce the annealing effect on Figures 17(a) to 17(c) Destruction of the less supported structure is shown.

[0127] The semiconductor device according to the embodiment of the present disclosure can be applied to various electronic devices. For example, an integrated circuit (IC) can be formed based on such a semiconductor device, and an electronic device can be constructed therefrom. Therefore, the present disclosure also provides an electronic device including the above-mentioned semiconductor device. The electronic device may also include a display screen that cooperates with the integrated circuit and components such as a wireless transceiver that cooperates with the integrated circuit. Such electronic devices include, for example, smart phones, computers, tablet computers (PCs), wearable smart devices, mobile power supplies, and the like.

[0128] According to an embodiment of the present disclosure, a method for manufacturing a chip system (SoC) is also provided. The method may include the above method. Specifically, multiple devices may be integrated on the chip, at least some of which are manufactured according to the method of the present disclosure.

[0129] In the above description, the technical details of the patterning and etching of each layer are not described in detail. However, those skilled in the art should understand that various technical means can be used to form layers, regions, etc. of desired shapes. In addition, in order to form the same structure, those skilled in the art can also design methods that are not completely the same as the methods described above. In addition, although the various embodiments are described above separately, this does not mean that the measures in the various embodiments cannot be used in combination to advantage.

[0130] The embodiments of the present disclosure are described above. However, these embodiments are for illustrative purposes only and are not intended to limit the scope of the present disclosure. The scope of the present disclosure is defined by the appended claims and their equivalents. Without departing from the scope of the present disclosure, a person skilled in the art may make a variety of substitutions and modifications, which should all fall within the scope of the present disclosure.

Claims

1. A semiconductor device, include: A channel portion on a substrate, the channel portion comprising two or more curved nanosheets or nanowires spaced apart from each other in a lateral direction relative to the substrate and each having a C-shaped cross section; The two or more nanosheets or nanowires are connected to the same source / drain portion at the upper end of the channel portion and to the same source / drain portion at the lower end of the channel portion relative to the source / drain portion of the substrate at the upper and lower ends of the channel portion; as well as A gate stack surrounds a periphery of each of the two or more nanosheets or nanowires in the channel portion, the gate stack including a portion between adjacent nanosheets or nanowires of the two or more nanosheets or nanowires.

2. The semiconductor device according to claim 1, in, At least one of the two or more nanosheets or nanowires includes a plurality of sub-nanosheets or sub-nanowires which are sequentially stacked in the lateral direction and each of which has a C-shaped cross section.

3. The semiconductor device according to claim 2, in, At least some of the plurality of sub-nanosheets or sub-nanowires have different properties.

4. The semiconductor device according to claim 3, in, The multiple sub-nanosheets or sub-nanowires include a first sub-nanosheet or sub-nanowire and a second sub-nanosheet or sub-nanowire, which are respectively located on both sides of the corresponding nanosheet or nanowire in the lateral direction and have improved interface quality with the gate stack, and a third sub-nanosheet or sub-nanowire, which is located between the first sub-nanosheet or sub-nanowire and the second sub-nanosheet or sub-nanowire and has high carrier mobility.

5. The semiconductor device according to claim 3, in, The multiple sub-nanosheets or sub-nanowires include a first sub-nanosheet or sub-nanowire and a second sub-nanosheet or sub-nanowire respectively located on both sides of the corresponding nanosheet or nanowire in the lateral direction and having high carrier mobility, and a third sub-nanosheet or sub-nanowire located between the first sub-nanosheet or sub-nanowire and the second sub-nanosheet or sub-nanowire and capable of optimizing carrier distribution.

6. The semiconductor device according to claim 3, in, The plurality of sub-nanosheets or sub-nanowires include a first sub-nanosheet or sub-nanowire and a second sub-nanosheet or sub-nanowire located at both sides of the corresponding nanosheet or nanowire in the lateral direction, and a third sub-nanosheet or sub-nanowire located between the first sub-nanosheet or sub-nanowire and the second sub-nanosheet or sub-nanowire, Wherein, for an n-type semiconductor device, the lowest energy level of the conduction band of the third sub-nanosheet or sub-nanowire is higher than the lowest energy level of the conduction band of the first sub-nanosheet or sub-nanowire and / or the second sub-nanosheet or sub-nanowire; or For a p-type semiconductor device, the highest energy level of the valence band of the third sub-nanosheet or sub-nanowire is lower than the highest energy level of the valence band of the first sub-nanosheet or sub-nanowire and / or the second sub-nanosheet or sub-nanowire.

7. The semiconductor device according to claim 2, in, The at least one is two or more, wherein the stack of sub-nanosheets or sub-nanowires included in at least one nanosheet or nanowire is different from the stack of sub-nanosheets or sub-nanowires included in at least another nanosheet or nanowire.

8. The semiconductor device according to claim 2, in, The substrate has a plurality of the semiconductor devices thereon, wherein the stack of sub-nanosheets or sub-nanowires included in at least one nanosheet or nanowire in at least one semiconductor device is different from the stack of sub-nanosheets or sub-nanowires included in at least one nanosheet or nanowire in at least another semiconductor device.

9. The semiconductor device according to claim 1, in, At least some of the two or more nanosheets or nanowires differ in at least one of thickness, material, and doping concentration.

10. The semiconductor device according to claim 1, Among them, the substrate There are a plurality of the semiconductor devices, wherein at least one nanosheet or nanowire in at least one semiconductor device is different from at least one nanosheet or nanowire in at least another semiconductor device in at least one aspect of thickness, material, and doping concentration.

11. The semiconductor device according to claim 1, in, The two or more nanosheets or nanowires include one or more pairs of nanosheets or nanowires that are symmetrical about a plane extending in a vertical direction relative to the substrate.

12. The semiconductor device according to claim 1, in, A plurality of the semiconductor devices are provided on a substrate, wherein at least some of the semiconductor devices have different numbers of nanosheets or nanowires included in the channel portions.

13. The semiconductor device according to claim 12, in, The plurality of semiconductor devices include n-type semiconductor devices and p-type semiconductor devices, wherein the number of nanosheets or nanowires included in a channel portion of the p-type semiconductor device is twice the number of nanosheets or nanowires included in a channel portion of the n-type semiconductor device.

14. The semiconductor device according to claim 1, in, Each of the two or more nanosheets or nanowires has a substantially uniform thickness.

15. The semiconductor device according to claim 2, in, Each of the plurality of sub-nanosheets or sub-nanowires has a substantially uniform thickness.

16. The semiconductor device according to claim 1, in, At least a portion of the gate stack adjacent to the channel portion is substantially coplanar with the channel portion.

17. The semiconductor device according to claim 11, in, The plane is a center plane of the source / drain portion at an upper end of the channel portion.

18. The semiconductor device according to claim 1, in, At least a portion of the periphery of the gate stack extends along a corresponding periphery of the source / drain portion at an upper end of the channel portion.

19. The semiconductor device according to claim 1, in, The highest surface of the gate conductor layer in the gate stack is higher than the top surface of the channel portion.

20. The semiconductor device according to claim 1, in, The channel portion and / or the source / drain portion include a single crystalline semiconductor material.

21. The semiconductor device according to claim 11, in, The substrate has a plurality of the semiconductor devices thereon, wherein the channel portions of at least some of the semiconductor devices are substantially coplanar.

22. The semiconductor device according to claim 21, in, The upper source / drain portions of at least some of the semiconductor devices are substantially coplanar, and the lower source / drain portions of at least some of the semiconductor devices are substantially coplanar.

23. The semiconductor device according to claim 1, in, In a cross-section extending laterally relative to the substrate, the two or more nanosheets or nanowires extend substantially parallel.

24. The semiconductor device according to claim 1, in, In a cross-section extending laterally relative to the substrate, each of the two or more nanosheets or nanowires is U-shaped.

25. The semiconductor device according to claim 1, in, At two opposite sides of at least one of the two or more curved nanosheets or nanowires in the lateral direction, the gate lengths of the gate stacks are substantially equal.

26. A method of manufacturing a semiconductor device, include: Disposing a stack of a first material layer, a second material layer, and a third material layer on a substrate; Patterning the stack into a strip-like structure extending along a first direction; forming source / drain portions in the first material layer and the third material layer; At opposite sides of the strip structure in a second direction intersecting the first direction, the sidewalls of the second material layer are laterally recessed relative to the sidewalls of the first material layer and the third material layer, thereby defining a first recessed portion; forming a first channel layer by epitaxial growth on the sidewall of the second material layer exposed by the first recessed portion; forming a first position holding layer in a remaining space of the first recessed portion; At opposite sides of the strip structure in the second direction, the sidewalls of the first position maintaining layer are laterally recessed relative to the sidewalls of the first material layer and the third material layer, thereby defining a second recessed portion; forming a second channel layer by epitaxial growth on the side wall of the first position holding layer exposed by the second recessed portion; forming a second position holding layer in a remaining space of the second recessed portion; Separating the strip structure into a plurality of segments in the first direction; forming an isolation layer on the substrate; removing the second material layer, the first position holding layer, and the second position holding layer; and A gate stack is formed on the isolation layer around the first channel layer.

27. The method according to claim 26, in, The strip-shaped structure has an end in the first direction, and the recessing operation is also directed to the end, so that the recessed portion obtained thereby also extends to the end.

28. The method according to claim 26, in, A plurality of semiconductor devices are formed on a substrate, wherein the second channel layer is formed only for a portion of the semiconductor devices.

29. The method according to claim 26, in, Forming the first position maintaining layer includes epitaxially growing the first position maintaining layer on the first channel layer.

30. The method according to claim 26, in, The first material layer is an upper portion of the substrate, or is an epitaxial layer on the substrate.

31. The method according to claim 26, in, The second material layer has an etching selectivity relative to the first material layer and the third material layer.

32. The method according to claim 26, in, Recessing the sidewalls of the second material layer includes isotropic etching.

33. The method according to claim 26, in, Forming the first channel layer includes selective epitaxial growth.

34. The method according to claim 26, in, Forming the source / drain portion includes: forming a dopant source layer on the sidewalls of the stripe structure; and Dopants in the dopant source layer are driven into the first material layer and the third material layer.

35. The method according to claim 26, in, After defining the first recessed portion and before forming the first channel layer, the method further includes: The exposed surface of the stripe structure is etched back to a thickness substantially the same as a thickness of a first channel layer to be formed.

36. An electronic device comprising the semiconductor device according to any one of claims 1 to 25.

37. The electronic device according to claim 36 comprises a smart phone, a computer, a tablet computer, a wearable smart device, an artificial intelligence device, and a mobile power supply.

Citation Information

Patent Citations

  • Semiconductor device and forming method thereof

    CN105448723A

  • Semiconductor device and manufacturing method thereof and electronic equipment comprising semiconductor device

    CN106298778A

  • Semiconductor device, manufacturing method thereof and electronic device comprising device

    CN107887440A

  • Semiconductor device, manufacturing method thereof and electronic device comprising device

    CN107887444A

  • Phosphorous doping methods of manufacturing field effect transistors having multiple stacked channels

    CN1702843A