Semiconductor structure and method for forming the same
By using sidewall anti-punch-through regions and source-drain doping regions that are different from the doping ions in the semiconductor structure, the problem of short channel effect is solved and the electrical performance of the semiconductor structure is improved.
Patent Information
- Application Number
- CN201910459891.X
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2019-05-30
- Publication Date
- 2024-10-29
- Estimated Expiration
- 2039-05-30
AI Technical Summary
In semiconductor manufacturing, as the device channel length shortens, the gate structure's ability to control the channel decreases, making the short channel effect more likely to occur and affecting the electrical performance of the semiconductor structure.
In the semiconductor structure, a sidewall anti-punchthrough region is formed on the sidewall near the top of the fin. The sidewall antipunchthrough region contains second-type ions that are different from the doping ions of the first-type transistor, and forms a gate across the fin. The electrode structure and the source and drain doped regions contain first-type ions to improve the electrical performance.
Through the design of the sidewall anti-punch-through area, the probability of punch-through of the source and drain is reduced, the electrical performance of the semiconductor structure is improved, and the gate's ability to control the channel is enhanced.
Smart Images

Figure CN112018163B_ABST
Abstract
Description
Technical Field
[0001] The embodiments of the present invention relate to the field of semiconductor manufacturing, and in particular to a semiconductor structure and a method for forming the same. Background Art
[0002] In semiconductor manufacturing, with the development trend of ultra-large-scale integrated circuits, the feature size of integrated circuits continues to decrease. In order to adapt to smaller feature sizes, the channel length of metal-oxide-semiconductor field-effect transistors (MOSFETs) is also shortened accordingly. However, as the channel length of the device shortens, the distance between the source and drain of the device also shortens, so the control ability of the gate structure over the channel becomes worse, and the difficulty of pinching off the channel by the gate voltage becomes increasingly greater, making subthreshold leakage, the so-called short-channel effects (SCE), more likely to occur.
[0003] Therefore, in order to better adapt to the reduction of feature size, semiconductor processes have gradually begun to transition from planar MOSFET to three-dimensional transistors with higher power efficiency, such as fin field effect transistors (FinFET). In FinFET, the gate structure can control the ultra-thin body (fin) from at least two sides. Compared with planar MOSFET, the gate structure has stronger control over the channel and can effectively suppress the short channel effect; and FinFET has better compatibility with existing integrated circuit manufacturing than other devices. Summary of the invention
[0004] The problem solved by the embodiments of the present invention is to provide a semiconductor structure and a method for forming the same, so as to optimize the electrical performance of the semiconductor structure.
[0005] To solve the above problems, an embodiment of the present invention provides a method for forming a semiconductor structure, which is used to form a first-type transistor, including: providing a substrate; etching the substrate to form a substrate and a fin located on the substrate, wherein a sidewall anti-punchthrough region is formed on the sidewall of the fin near the top of the fin, and the sidewall anti-punchthrough region contains second-type ions, which are different from the doping ions of the first-type transistor; forming a gate structure spanning the fin, the gate structure covering part of the sidewall of the sidewall anti-punchthrough region; forming source-drain doping regions in the fin on both sides of the gate structure, and the first-type ions are formed in the source-drain doping regions.
[0006] Correspondingly, an embodiment of the present invention also provides a semiconductor structure, which is a first-type transistor, comprising: a substrate; a fin, located on the substrate; a sidewall anti-punchthrough region, located on the sidewall of the fin near the top of the fin, the sidewall anti-punchthrough region containing second-type ions, and the second-type ions are different from the doping ions of the first-type transistor; a gate structure, spanning multiple fins, and the gate structure covers part of the sidewall of the sidewall anti-punchthrough region; a source-drain doping region, located in the fin on both sides of the gate structure, the source-drain doping region is doped with the first-type ions.
[0007] Compared with the prior art, the technical solution of the embodiment of the present invention has the following advantages:
[0008] In an embodiment of the present invention, a sidewall anti-punchthrough region is formed on the sidewall of the fin near the top of the fin, and the sidewall anti-punchthrough region contains second-type ions. The second-type ion type is different from the doping ions of the first-type transistor, that is, different from the doping ion type in the source and drain doping region. Compared with the case where no sidewall anti-punchthrough region is formed on the sidewall of the fin, the depletion layer of the source and drain in the source and drain doping region is not easy to expand on the sidewall of the fin, thereby reducing the probability of punch-through of the source and drain, which is beneficial to improving the electrical performance of the semiconductor structure. BRIEF DESCRIPTION OF THE DRAWINGS
[0009] Figures 1 to 3 It is a schematic structural diagram corresponding to each step in a method for forming a semiconductor structure;
[0010] Figures 4 to 11 is a schematic structural diagram corresponding to each step in a first embodiment of a method for forming a semiconductor structure according to an embodiment of the present invention;
[0011] Figures 12 to 16 It is a schematic structural diagram corresponding to each step in the second embodiment of the method for forming a semiconductor structure according to an embodiment of the present invention. DETAILED DESCRIPTION
[0012] As can be seen from the background technology, the devices currently formed still have the problem of poor performance. The reasons for the poor performance of the devices are now analyzed in combination with a method for forming a semiconductor structure.
[0013] refer to Figures 1 to 3 , showing a structural schematic diagram corresponding to each step in a method for forming a semiconductor structure.
[0014] refer to Figure 1 , providing a base, the base comprising a substrate 1 and a fin 2 located on the substrate 1; forming an isolation material layer 3 on the substrate 1 where the fin 2 is exposed, the isolation material layer 3 covering the side wall of the fin 2, and the top surface of the isolation material layer 3 is flush with the top surface of the fin 2.
[0015] refer to Figure 2 , ion implantation is performed on the fin 2 to form an anti-punch-through region 4 in the fin 2 .
[0016] refer to Figure 3 , partially etching back the isolation material layer 3 to form an isolation layer 5; after forming the isolation layer 5, a gate structure 6 spanning the fin 2 is formed, and the gate structure 6 covers a portion of the top and a portion of the side wall of the fin 2.
[0017] Subsequently, source-drain doped regions are formed in the fin 2 on both sides of the gate structure 6. When the semiconductor structure is working, the fin 2 covered by the gate structure 6 between the source and the drain of the source-drain doped region serves as a channel, and the anti-punch-through region 4 makes it difficult for the area below the channel to be punched through. However, the depletion layers of the source and the drain in the source-drain doped region are easy to expand on the sidewalls of the fin 2, causing the source and the drain to be easily punched through on the sidewalls of the fin 2, resulting in poor electrical performance of the semiconductor structure.
[0018] In order to solve the technical problem, an embodiment of the present invention provides a method for forming a semiconductor structure, which is used to form a first-type transistor, including: providing a substrate; etching the substrate to form a substrate and a fin located on the substrate, wherein a sidewall anti-punchthrough region is formed on the sidewall of the fin near the top of the fin, and the sidewall anti-punchthrough region contains second-type ions, which are different from the doping ions of the first-type transistor; forming a gate structure spanning the fin, the gate structure covering part of the sidewall of the sidewall anti-punchthrough region; forming source-drain doping regions in the fin on both sides of the gate structure, and the first-type ions are formed in the source-drain doping regions.
[0019] In an embodiment of the present invention, a sidewall anti-punchthrough region is formed on the sidewall of the fin near the top of the fin, and the sidewall anti-punchthrough region contains second-type ions. The second-type ion type is different from the doping ions of the first-type transistor, that is, different from the doping ion type in the source and drain doping region. Compared with the case where no sidewall anti-punchthrough region is formed on the sidewall of the fin, the depletion layer of the source and drain in the source and drain doping region is not easy to expand on the sidewall of the fin, thereby reducing the probability of punch-through of the source and drain, which is beneficial to improving the electrical performance of the semiconductor structure.
[0020] In order to make the above-mentioned purposes, features and advantages of the embodiments of the present invention more obvious and easy to understand, specific embodiments of the embodiments of the present invention are described in detail below with reference to the accompanying drawings.
[0021] Figures 4 to 11 It is a schematic structural diagram corresponding to each step in the first embodiment of the method for forming a semiconductor structure of the present invention.
[0022] refer to Figure 4, providing a substrate 100.
[0023] The substrate 100 provides a process platform for subsequently forming a semiconductor structure. The semiconductor structure formed subsequently is a first-type transistor, which includes a source-drain doping region doped with first-type ions.
[0024] In this embodiment, the material of the substrate 100 is silicon. In other embodiments, the material of the substrate may also be germanium, silicon carbide, gallium arsenide or indium gallium, and the substrate may also be a silicon substrate on an insulator or a germanium substrate on an insulator. An interface layer may also be formed on the surface of the substrate 100, and the material of the interface layer may be silicon oxide, silicon nitride or silicon oxynitride.
[0025] A mask layer 102 is formed on the substrate 100. The mask layer 102 can be used as a mask for subsequently etching the substrate 100 to form a fin.
[0026] Specifically, the material of the mask layer 102 includes one or more materials selected from silicon nitride, silicon carbonitride, silicon carbon nitride oxide, silicon nitride oxide, boron nitride and boron carbonitride. In this embodiment, the material of the mask layer 102 is silicon nitride.
[0027] It should be noted that the thermal expansion coefficients of the material of the mask layer 102 and the material of the substrate 100 are quite different. If the mask layer 102 is directly formed on the substrate 100, the mask layer 102 is prone to cracks or even fall off, so that it cannot serve as a mask. Therefore, a buffer layer 101 is formed between the mask layer 102 and the substrate 100, and the buffer layer 101 serves as a buffer.
[0028] In this embodiment, the material of the buffer layer 101 is silicon oxide.
[0029] refer to Figures 5 to 7 , etching the base 100 to form a substrate 103 (such as Figure 7 ) and the fin 104 located on the substrate 103 (as shown Figure 7 A sidewall anti-punch-through region 105 is formed on the sidewall of the fin 104 near the top of the fin 104 (as shown in FIG. Figure 7 As shown), the sidewall anti-punch-through region 105 contains second-type ions, and the second-type ions are different from the doping ions of the first-type transistor.
[0030] In this embodiment, the second type ions are different from the doping ions of the first type transistor, which means that the second type ions are different from the doping ions in the subsequently formed source and drain doping regions.
[0031] In an embodiment of the present invention, a sidewall anti-punchthrough region 105 is formed on the sidewall of the fin 104 near the top of the fin 104. The sidewall anti-punchthrough region 105 contains doped ions. The type of doped ions in the sidewall anti-punchthrough region 105 is different from the type of doped ions in the subsequently formed source and drain doped regions. Compared with the case where the sidewall anti-punchthrough region 105 is not formed on the sidewall of the fin 104, the depletion layer of the source and the drain in the source and drain doped regions is not easy to expand on the sidewall of the fin 104, thereby reducing the probability of punch-through of the source and the drain, which is beneficial to improving the electrical performance of the semiconductor structure.
[0032] Specifically, the steps of forming the substrate 103 and the fin 104 include:
[0033] like Figure 5 As shown, the substrate 100 is etched using the mask layer 102 as a mask (eg Figure 4 As shown), an initial substrate 106 and an initial fin 107 located on the initial substrate 106 are formed.
[0034] After the initial fin 107 is formed, preparation is made for subsequently forming a doped region on the initial fin 107 and the initial substrate 106 exposed by the initial fin 107 .
[0035] In this embodiment, the mask layer 102 is used as a mask and a dry etching process is used to etch the substrate 100 to form an initial substrate 106 and an initial fin 107. The dry etching process is an anisotropic etching process and has good controllability of the etching profile, which is conducive to making the morphology of the initial fin 107 meet the process requirements, and is conducive to accurately controlling the formation height of the initial substrate 106 and reducing damage to other film layer structures.
[0036] It should be noted that the initial fin 107 should not be too high or too low. If the initial fin 107 is too high, the area of the doped region subsequently formed on the side wall of the initial fin 107 and the initial substrate 106 will be too large. Accordingly, the process time spent is too long, the process defects are difficult to control, and it is not easy to improve the formation quality of the semiconductor structure. When the semiconductor structure is working, the sidewall anti-punchthrough region is used to prevent the depletion layer of the source and drain of the subsequently formed source and drain doped regions from expanding on the side wall of the fin. If the initial fin 107 is too low, it is easy to cause the height of the sidewall anti-punchthrough region subsequently formed on the side wall of the fin to be too small, and the bottom of the gate structure subsequently formed is too lower than the bottom of the sidewall anti-punchthrough region, which in turn causes the source and drain doped regions to easily punch through the side wall of the fin below the subsequently formed sidewall anti-punchthrough region. In this embodiment, the height of the initial fin 107 accounts for one-third to one-half of the height of the fin formed subsequently.
[0037] like Figure 6As shown, with the mask layer 102 as a mask, doping is performed on the sidewalls of the initial fin 107 and the initial substrate 106 exposed by the initial fin 107 to form a doped region 108 .
[0038] Subsequently, the initial substrate 106 is etched using the mask layer 102 as a mask to form a substrate and a fin located on the substrate. In the process of forming the fin, the doped region 108 on the initial substrate 106 is removed, and the remaining doped region 108 located on the fin serves as a sidewall anti-punch-through region. Therefore, the doped region 108 is prepared for the subsequent formation of the sidewall anti-punch-through region.
[0039] In this embodiment, ion implantation is used to dope the sidewalls of the initial fin 107 and the initial substrate 106 exposed by the initial fin 107 with second-type ions to form a doped region 108 .
[0040] In this embodiment, when the first-type transistor is NMOS, the second-type ions are P-type ions, and the second-type ions include boron ions, gallium ions or indium ions.
[0041] It should be noted that the implantation dose of the second type ion should not be too large or too small. If the implantation dose of the second type ion is too large, it is easy to cause the doping concentration of the second type ion in the doped region 108 to be too large, and the doped ions are easy to diffuse into the area used as the channel in the subsequent fin. When the semiconductor structure is working, it is easy to cause the scattering of carriers, and then the migration rate of carriers is not high. If the implantation dose of the second type ion is too small, it is easy to cause the doping concentration of the second type ion in the doped region 108 to be too small, and then the doping concentration of the second type ion in the sidewall anti-punch-through region formed subsequently is too small. When the semiconductor structure is working, the sidewall anti-punch-through region is not easy to prevent the depletion layer of the source and drain formed subsequently from expanding on the sidewall of the fin, and then it is easy to cause the punch-through of the source and drain. In this embodiment, the implantation dose of the ion is 3E12 atoms per square centimeter to 3E13 atoms per square centimeter.
[0042] It should be noted that the injection energy of the second type ions should not be too large or too small. If the injection energy of the second type ions is too large, it is easy to cause large lattice damage to the initial fin 107 in the process of forming the doped region 108, and the subsequent annealing process is difficult to repair. Moreover, because the initial fin 101 is used as a channel region in the subsequent process, the carrier migration rate in the channel is not high when the semiconductor structure is working. If the injection energy of the second type ions is too small, it is easy to cause the second type ions to be difficult to enter the bottom of the initial fin 107, which in turn causes the second type ion doping concentration at the bottom of the subsequently formed sidewall anti-punch-through region 105 to be too low. When the semiconductor structure is working, the sidewall anti-punch-through region is not easy to prevent the depletion layer of the source and drain of the subsequently formed source and drain doping region from expanding on the side wall of the fin, which is easy to cause the punch-through of the source and drain. In this embodiment, the ion implantation energy is 0.5Kev to 1Kev.
[0043] It should be noted that the angle between the injection direction of the second type ions and the surface normal of the initial substrate 106 should not be too large. If the angle is too large, it is easy to cause the doped ions to enter too much into the region of the fin used as the channel. When the semiconductor structure is working, the channel is prone to carrier scattering problems, resulting in low electrical performance of the semiconductor structure. In this embodiment, the angle between the injection direction of the second type ions and the surface normal of the initial substrate 106 is 0 to 5 degrees.
[0044] In other embodiments, when the first-type transistor is PMOS, the process parameters of the ion implantation include: the second-type ions are N-type ions, and the second-type ions include phosphorus ions, arsenic ions or antimony ions; the second-type ion implantation energy is 0.5Kev to 1Kev; the implantation dose of the second-type ions is 3E12 atoms per square centimeter to 3E13 atoms per square centimeter; the angle between the implantation direction and the normal line of the initial substrate surface is 0 degrees to 5 degrees.
[0045] like Figure 7 As shown, the doped region 108 (such as Figure 6 After that, the mask layer 102 is used as a mask to remove a portion of the initial substrate 106 (as shown in FIG. Figure 6 As shown), a substrate 103 and a fin 104 located on the substrate 103 are formed, and the remaining doped region 108 located on the sidewall of the fin 104 serves as a sidewall anti-punch-through region 105.
[0046] In this embodiment, the process parameters for etching the substrate 100 to form the initial fin 107 are the same as the process parameters for etching the initial substrate 106 to form the fin 104, so that in the process of etching the initial substrate 106 to form the fin 104, the etched track of the initial substrate 106 is the same as the extension direction of the initial fin 107, and the doped region 108 on the side wall of the initial fin 107 is not easy to be mistakenly etched, and then in the extension direction perpendicular to the fin 104, the thickness of the formed side wall anti-punch-through region 105 is not easy to be too small. When the semiconductor structure is working, the subsequent source and drain depletion layers are not easy to expand on the side wall of the fin 104, thereby reducing the probability of the source and drain punching through on the side wall of the fin 104, which is conducive to improving the electrical performance of the semiconductor structure.
[0047] It should be noted that, in the direction perpendicular to the extension of the fin 104, the size of the sidewall anti-punchthrough area 105 should not be too large or too small. If the size is too large, the width of the channel region is too small in the direction perpendicular to the extension of the fin 104, which may easily lead to a too low carrier migration rate when the semiconductor structure is working. If the size is too small, the sidewall anti-punchthrough area 105 will not easily prevent the depletion layer of the source and drain from expanding on the sidewall of the fin 104, causing the source and drain to be easily punched through. In this embodiment, in the direction perpendicular to the extension of the fin 104, the size of the sidewall anti-punchthrough area 105 is 1 nanometer to 3 nanometers.
[0048] The method for forming the semiconductor structure further includes: forming the doped region 108 (such as Figure 6 After that, the initial substrate 106 (as shown) is etched Figure 6 As shown) to form the fin 104 (as shown Figure 7 As shown in FIG. 1 , the doped region 108 is annealed.
[0049] The annealing process is used to activate the doping ions in the doping region 108 and repair the lattice defects.
[0050] In this embodiment, spike annealing or laser annealing is used for annealing. Because the spike annealing or laser annealing has a short time, the ions in the doping region 108 are not easy to diffuse into the channel region below the gate structure formed subsequently, so that the carriers in the channel are not easy to scatter during the subsequent semiconductor operation, thereby improving the carrier migration rate.
[0051] refer to Figures 8 to 11 , forming a gate structure 111 (such as Fig.11 As shown), the gate structure 111 covers a portion of the sidewall of the sidewall anti-punch-through region 105.
[0052] When the semiconductor structure is working, the gate structure 111 is used to open or close the channel.
[0053] In this embodiment, the gate structure 111 includes a gate oxide layer (not shown in the figure) and a gate layer (not shown in the figure) located on the gate oxide layer.
[0054] In this embodiment, the material of the gate oxide layer is silicon oxide. In other embodiments, the material of the gate oxide layer may also be silicon oxynitride.
[0055] In this embodiment, the material of the gate layer is polysilicon. In other embodiments, the material of the gate layer may also be amorphous carbon.
[0056] like Figure 8 and Fig. 9 As shown, the method for forming the semiconductor structure further includes: after forming the sidewall anti-punch-through region 105 and before forming the gate structure 111, doping the fin 104 below the sidewall anti-punch-through region 105 to form a bottom anti-punch-through region 110 (such as Fig. 9 shown).
[0057] The bottom anti-punch-through region 110 and the sidewall anti-punch-through region 105 have the same doping ion type, both of which are second-type ions. When the semiconductor structure is working, the bottom anti-punch-through region 110 and the sidewall anti-punch-through region 105 make it difficult for the depletion layer of the source and the drain to expand from the bottom surface and the side wall of the channel respectively, thereby making it difficult for the source and the drain of the source-drain doping region to be punched through.
[0058] In this embodiment, the top surface of the bottom anti-punchthrough region 110 is higher than the bottom surface of the sidewall anti-punchthrough region 105 or is flush with the bottom surface of the sidewall anti-punchthrough region 105. Compared with the case where the top surface of the bottom anti-punchthrough region 110 is lower than the sidewall anti-punchthrough region 105, when the semiconductor structure is working, the embodiment of the present invention makes it difficult for the depletion layer of the source and the drain to expand between the sidewall anti-punchthrough region 105 and the bottom anti-punchthrough region 110, thereby making it difficult for the source and the drain of the source and drain doping regions to be punched through.
[0059] It should be noted that the bottom surface of the gate structure 111 should not be too high or too low above the top surface of the bottom anti-punch-through region 110. If the bottom surface of the gate structure 111 is too high above the top surface of the bottom anti-punch-through region 110, that is, when the semiconductor structure is working, the channel is too far away from the bottom anti-punch-through region 110, and the depletion layer of the source and drain of the source-drain doping region is likely to expand at the bottom of the channel, resulting in the punch-through of the source and drain of the source-drain doping region. If the bottom surface of the gate structure 111 is too low above the top surface of the bottom anti-punch-through region 110, that is, when the semiconductor structure is working, the bottom anti-punch-through region 110 of partial thickness acts as a channel, which is likely to cause carrier scattering, thereby resulting in a low carrier migration rate. In this embodiment, the bottom surface of the gate structure 111 is not lower than the top surface of the bottom anti-punch-through region 110 by 10 nanometers, and the bottom surface of the gate structure 111 is not higher than the top surface of the bottom anti-punch-through region 110 by 5 nanometers.
[0060] Specifically, the process of forming the bottom anti-punch-through area 110 is as follows:
[0061] like Figure 8 As shown, after the sidewall anti-punch-through region 105 is formed, an isolation material layer 109 is formed on the substrate 103 where the fin 104 is exposed.
[0062] A part of the bottom anti-punch-through region is formed by the second type ions moving in the fin 104 and staying in the fin 104, and another part is formed by the second type ions passing through the isolation material layer 109 and staying in the fin 104. The isolation material layer 109, in the process of forming the bottom anti-punch-through region, hinders the movement of the second type ions, so that the speed of the second type ions is reduced, so that the speed attenuation of the second type ions doped in the isolation material layer 109 is similar to the speed attenuation of the second type ions doped in the fin 104, and finally the position consistency of the formed bottom anti-punch-through region in the fin 104 is good, which is conducive to improving the uniformity of device performance.
[0063] In this embodiment, the isolation material layer 109 is made of dielectric material.
[0064] Specifically, the material of the isolation material layer 109 includes one or more of silicon oxide, silicon nitride, silicon carbonitride, silicon carbon nitride oxide, silicon nitride oxide, boron nitride and boron carbonitride. In this embodiment, the material of the isolation material layer 109 is silicon oxide.
[0065] The step of forming the isolation material layer 109 includes: forming an isolation material film (not shown in the figure) covering the fin 104; planarizing the isolation material film until the mask layer 102 is exposed, and etching back a portion of the thickness of the isolation material film to form the isolation material layer 109, and the top surface of the isolation material layer 109 is not higher than the top surface of the buffer layer 102.
[0066] It should be noted that the top surface of the isolation material layer 109 is not higher than the top surface of the buffer layer 102 , in preparation for the subsequent removal of the mask layer 102 .
[0067] Continue to refer Figure 8 After forming the isolation material layer 109, the mask layer 102 (eg Figure 7 shown).
[0068] The mask layer 102 is removed to prepare for the subsequent doping of the fin 104 below the sidewall anti-punch-through region 105 to form a bottom anti-punch-through region.
[0069] In this embodiment, a wet etching process is used to remove the mask layer 102. Compared with the case where the top surface of the isolation material layer 109 is higher than the top surface of the buffer layer 102, the top surface of the isolation material layer 109 is not higher than the top surface of the buffer layer 102. In the process of removing the mask layer 102 by the wet etching process, the removal rate of the mask layer 102 is faster and it is not easy to leave residue. The wet etching process is isotropic etching, which has a high etching rate, simple operation and low process cost. In other embodiments, a dry etching process can also be used to remove the mask layer.
[0070] In this embodiment, the material of the mask layer 102 is silicon nitride, and accordingly, a phosphoric acid solution is used to remove the mask layer 102 .
[0071] like Fig. 9 As shown, after the isolation material layer 109 is formed, the bottom anti-punch-through region 110 is formed in the fin 104 by ion implantation.
[0072] In this embodiment, the angle between the ion implantation direction and the surface normal of the substrate 103 is 0 degrees. In the process of doping the fin 104 below the sidewall anti-punch-through region 105, the top surface of the formed bottom anti-punch-through region 110 has good height consistency, and the second type ions are not easily located in the channel region of the fin 104 through appropriate implantation energy. When the semiconductor structure is working, the probability of carrier scattering in the channel is reduced, the carrier mobility is improved, and the electrical performance of the semiconductor structure is further optimized.
[0073] like Fig.10 and Fig.11After forming the bottom anti-punch-through region 110 , a portion of the thickness of the isolation material layer 109 is etched back to form an isolation layer 112 .
[0074] The isolation layer 112 is used to electrically isolate the adjacent fins 104. The isolation layer 112 is also used to determine the height of the gate structure covering the fins 104, and accordingly, determines the magnitude of the driving current in the channel of the fins 104.
[0075] It should be noted that, in the process of etching back the isolation material layer 109 to form the isolation layer 112 , the buffer layer 101 on the top of the fin 104 is removed.
[0076] The method for forming the semiconductor structure further includes: forming source-drain doping regions (not shown in the figure) in the fins 104 on both sides of the gate structure 111 , wherein first type ions are formed in the source-drain doping regions.
[0077] The source-drain doped regions are used to provide stress to the channel and increase the migration rate of carriers.
[0078] In this embodiment, the first-type transistor is an NMOS (Negative channel Metal Oxide Semiconductor), and the source and drain doping regions are silicon carbide or silicon phosphide doped with first-type ions. In this embodiment, the first-type ions are N-type ions, and the first-type ions include: phosphorus ions, arsenic ions or antimony ions.
[0079] In other embodiments, the first-type transistor is a PMOS (Positive Channel Metal Oxide Semiconductor). The source and drain doping regions are silicon germanium doped with first-type ions. In this embodiment, the first-type ions are P-type ions, and the first-type ions include boron ions, gallium ions, or indium ions.
[0080] It should be noted that the method for forming the semiconductor structure also includes: after forming the source and drain doping regions, forming an interlayer dielectric layer (not shown in the figure) covering the source and drain doping regions, the interlayer dielectric layer covers the side walls of the gate structure 111, and the interlayer dielectric layer exposes the top of the gate structure 111; removing the gate structure 111 to form an opening; and forming a metal gate structure (not shown in the figure) in the opening.
[0081] Figures 12 to 16 It is a schematic structural diagram corresponding to each step in the second embodiment of the method for forming a semiconductor structure of the present invention.
[0082] refer to Fig.12 , providing a substrate 200.
[0083] The substrate 200 provides a process platform for subsequently forming a semiconductor structure.
[0084] The semiconductor structure formed subsequently is a first-type transistor, wherein the first-type transistor includes source-drain doping regions, and the source-drain doping regions are doped with first-type ions.
[0085] In this embodiment, the material of the substrate 200 is silicon. In other embodiments, the material of the substrate may also be germanium, silicon carbide, gallium arsenide or indium gallium, and the substrate may also be a silicon substrate on an insulator or a germanium substrate on an insulator. An interface layer may also be formed on the surface of the substrate 200, and the material of the interface layer may be silicon oxide, silicon nitride or silicon oxynitride.
[0086] Continue to refer Fig.12 , a mask layer 202 is formed on the substrate 200 .
[0087] The mask layer 202 can be used as a mask for subsequent etching of the substrate 200 to form a fin, and can also be used as an implantation mask for forming a sidewall anti-punch-through region.
[0088] Specifically, the material of the mask layer 202 includes one or more materials selected from silicon nitride, silicon carbonitride, silicon carbon nitride oxide, silicon nitride oxide, boron nitride and boron carbonitride. In this embodiment, the material of the mask layer 202 is silicon nitride.
[0089] It should be noted that the thermal expansion coefficients of the material of the mask layer 202 and the material of the substrate 200 are quite different. If the mask layer 202 is directly formed on the substrate 200, the mask layer 202 is prone to cracks or even fall off, so that it cannot serve as a mask. Therefore, a buffer layer 201 is formed between the mask layer 202 and the substrate 200, and the buffer layer 201 serves as a buffer.
[0090] In this embodiment, the material of the buffer layer 201 is silicon oxide.
[0091] refer to Fig.13 , etching the base 200 to form a substrate 203 and a fin 204 located on the substrate 203, a sidewall anti-punchthrough region 205 is formed on the sidewall of the fin 204 near the top of the fin 204, and the sidewall anti-punchthrough region 205 contains second type ions, and the second type ions are different from the doping ions of the first type transistor.
[0092] In this embodiment, the second type ions are different from the doping ions of the first type transistor, which means that the second type ions are different from the doping ions in the subsequently formed source and drain doping regions.
[0093] In an embodiment of the present invention, a sidewall anti-punchthrough region 205 is formed on the sidewall of the fin 204 near the top of the fin 204. The sidewall anti-punchthrough region 205 contains second-type ions, and the second-type ions are different from the doping ion type in the subsequently formed source and drain doping region. Compared with the case where the sidewall anti-punchthrough region 205 is not formed on the sidewall of the fin 204, the depletion layer of the source and drain in the source and drain doping region is not easy to expand on the sidewall of the fin 204, thereby reducing the probability of source and drain punching through, which is beneficial to improving the electrical performance of the semiconductor structure.
[0094] In this embodiment, the base 200 is etched using the mask layer 202 as a mask to form a substrate 203 and a fin 204 located on the substrate 203 .
[0095] In this embodiment, the base 200 is etched by a dry etching process to form a substrate 203 and a fin 204 located on the substrate 203. The dry etching process is an anisotropic etching process, which has good controllability of the etching profile, is conducive to making the morphology of the fin 204 meet the process requirements, and is conducive to accurately controlling the formation height of the fin 204, reducing damage to other film structures.
[0096] After the fin 204 is formed, the mask layer 202 is used as a doping mask to dope the sidewall of the fin 204 near the top of the fin 204 to form the sidewall anti-punch-through region 205 .
[0097] In this embodiment, ion implantation is used to dope the sidewalls of the fin 204 near the top of the fin 204 to form the sidewall anti-punch-through region 205. During the ion implantation process, the second-type ion implantation direction forms a certain angle with the normal line of the surface of the substrate 203, and part of the second-type ions are blocked by the mask layer 202, which acts as an implantation mask. The position of the sidewall anti-punch-through region 205 on the fin 204 can be controlled by adjusting the angle between the second-type ion implantation direction and the normal line of the surface of the substrate 203.
[0098] When the first-type transistor is NMOS, the process parameters of the ion implantation include: the second-type ions are P-type ions, and the doped ions include: boron, gallium or indium.
[0099] It should be noted that the implantation dose of the second type ion should not be too large or too small. If the implantation dose of the second type ion is too large, it is easy to cause the doping concentration of the second type ion in the formed sidewall anti-punch-through area 205 to be too large, and the doped ions are easy to diffuse into the area of the fin 204 that is subsequently used as a channel. When the semiconductor structure is working, it is easy to cause the scattering of carriers, and then the migration rate of carriers is not high. If the implantation dose of the second type ion is too small, it is easy to cause the doping concentration of the second type ion in the sidewall anti-punch-through area 205 to be too small. When the semiconductor structure is working, the sidewall anti-punch-through area 205 is not easy to prevent the depletion layer of the source and drain from expanding on the sidewall of the fin 204, and then it is easy to cause the source and drain to punch through. In this embodiment, the implantation dose of the ion is 3E12 atoms per square centimeter to 3E13 atoms per square centimeter.
[0100] It should be noted that the injection energy of the second type ions should not be too large or too small. If the injection energy of the second type ions is too large, in the process of forming the sidewall anti-punchthrough area 205, the second type ions are easy to enter the area used as the channel in the fin 204, which is easy to cause carrier scattering when the semiconductor structure is working, and thus the carrier migration rate is not high. If the injection energy of the second type ions is too small, the width of the sidewall anti-punchthrough area 205 is small in the extension direction perpendicular to the fin 204. When the semiconductor structure is working, the sidewall anti-punchthrough area 205 is not easy to prevent the depletion layer of the source and drain from expanding on the sidewall of the fin 204, which is easy to cause the punch-through of the source and drain. In this embodiment, the injection energy is 0.5Kev to 1Kev.
[0101] It should be noted that the angle between the second-type ion implantation direction and the surface normal of the substrate 203 should not be too large or too small. If the angle is too small, the height of the sidewall anti-punchthrough area 205 formed on the sidewall of the fin 204 is too large. Accordingly, too much process time is spent, process defects cannot be controlled, and it is not easy to improve the formation efficiency of the semiconductor structure. If the angle is too large, it is easy to cause the height of the sidewall anti-punchthrough area 205 formed on the sidewall of the fin 204 to be too small, so that the bottom of the gate structure formed subsequently is too lower than the bottom of the sidewall anti-punchthrough area 205. When the semiconductor is working, the depletion layer of the source and drain of the source and drain doping regions expands on the sidewall of the fin 204, and the source and drain are easy to penetrate on the sidewall of the fin 204. In this embodiment, the angle between the second-type ion implantation direction and the surface normal of the substrate 203 is 3 degrees to 10 degrees.
[0102] The fin 204 is formed by etching the substrate 200 using the mask layer 202 as a mask by dry etching. Fig.11The polymer impurities generated during the etching process are not removed in time and accumulate at the bottom, which hinders the dry etching process, so that the side wall of the fin 204 formed by etching forms a certain angle with the normal line of the substrate 203. In this embodiment, the angle between the second type ion implantation direction and the normal line of the substrate 203 is 3 degrees to 10 degrees, so that the thickness uniformity of the side wall anti-punch-through region 205 formed on the side wall of the fin 204 is better. Accordingly, when the semiconductor structure is working, the side wall anti-punch-through region 205 can better prevent the depletion layer of the source and drain from expanding on the side wall of the fin 204, so that the source and drain are not easy to punch through.
[0103] In other embodiments, when the first type transistor is PMOS, the process parameters of the ion implantation include: doping ions include: phosphorus, arsenic or antimony; the implantation energy is 0.5Kev to 1Kev; the ion implantation dose is 3E12 atoms per square centimeter to 3E13 atoms per square centimeter; the angle between the implantation direction and the normal of the substrate 203 is 3 degrees to 10 degrees.
[0104] refer to Figures 14 to 16 , forming a gate structure 211 (such as Fig.16 As shown), the gate structure 211 covers a portion of the sidewall of the sidewall anti-punch-through region 205.
[0105] When the semiconductor structure is working, the gate structure 211 is used to control the opening and closing of the channel.
[0106] The method for forming the semiconductor structure includes: after forming the sidewall anti-punch-through region 205 and before forming the gate structure 211, doping the fin 204 below the sidewall anti-punch-through region 205 to form a bottom anti-punch-through region 210 (such as Fig.15 shown).
[0107] In this embodiment, the advantages of the bottom anti-punch-through region 210 and the detailed description of the positional relationship between the gate structure 211 and the bottom anti-punch-through region 210 can refer to the first embodiment.
[0108] like Fig.14 As shown, the method for forming the semiconductor structure also includes: after forming the sidewall anti-punch-through region 205 and before forming the sidewall anti-punch-through region 205, forming an isolation structure 206 on the substrate 203 exposed by the fin 204, and the isolation structure 206 covers a partial thickness of the sidewall anti-punch-through region 205.
[0109] In this embodiment, ions are subsequently doped in the isolation structure 206, and the doped ions diffuse into the fin 204 to form the bottom anti-punchthrough region. The isolation structure 206 covers a portion of the thickness of the sidewall anti-punchthrough region 205, preparing for the bottom anti-punchthrough region 210 formed after the second type ions in the isolation structure 206 diffuse into the fin 204 to contact the sidewall anti-punchthrough region 205. When the semiconductor structure is working, the contact between the bottom anti-punchthrough region 210 and the sidewall anti-punchthrough region 205 can better prevent the depletion layer of the source and drain from expanding in the fin 204, so that the source and drain are not easy to punch through.
[0110] like Fig.15 As shown, the step of forming the bottom anti-punch-through region 210 includes: using the mask layer 202 as an ion implantation mask, doping ions in the isolation structure 206 by ion implantation, and diffusing the doped ions into the fin 204 to form the bottom anti-punch-through region 210 .
[0111] In the present embodiment, the material of the mask layer 202 is silicon nitride, which has a high density. In the process of forming the bottom penetration region 210 by ion implantation, the second type ions are not easy to pass through the mask layer 202. Therefore, the second type ions are not easy to be located in the area used as the channel region in the fin 204. When the semiconductor structure is working, carrier scattering is not easy to occur in the channel, which is beneficial to improving the formation quality of the channel region, thereby making the migration rate of carriers in the channel higher when the subsequent semiconductor structure is working.
[0112] It should be noted that after the bottom anti-punch-through region 210 is formed, the mask layer 202 and the buffer layer 201 below the mask layer 202 are removed to prepare for forming a gate structure.
[0113] It should be noted that, in the present embodiment, the bottom anti-punch-through region 210 is formed by doping ions in the isolation structure 206 , and the doped ions diffuse into the fin 204 .
[0114] In the present embodiment, in the extension direction perpendicular to the fin 204 , the second type ions have not completely doped the fin 204 at the bottom of the side wall anti-punch-through region 205 , that is, there is an undoped fin 204 region between the bottom anti-punch-through region 210 on the two side walls of the fin 204 , and correspondingly, there is an area under the channel region that is not doped with the second type ions, so that the second type ions are not easily diffused into the channel region of the fin 204 .
[0115] It should also be noted that, in this embodiment, in the direction perpendicular to the extension direction of the fin 204, the size of the bottom anti-punchthrough region 210 is larger than the size of the sidewall anti-punchthrough region 205. When the semiconductor structure is working, the depletion layer of the source and drain in the subsequently formed source-drain doped region is not easy to expand at the bottom of the fin 204.
[0116] Therefore, the bottom anti-punch-through region 210 makes it difficult for the depletion layers of the source and drain in the subsequently formed source-drain doping region to expand at the bottom of the fin 204, and also makes it difficult for the second type ions in the bottom anti-punch-through region 210 to diffuse into the channel region of the fin 204, so that when the semiconductor structure is working, carrier scattering is unlikely to occur in the channel, so that the migration rate of carriers in the channel is higher when the subsequent semiconductor structure is working.
[0117] like Fig.16 As shown, for the specific description of the method for forming the gate structure 211 , reference may be made to the relevant description of the first embodiment, which will not be repeated in this embodiment.
[0118] Accordingly, an embodiment of the present invention further provides a semiconductor structure. Fig.11 , showing a schematic structural diagram of a first embodiment of a semiconductor structure of the present invention.
[0119] The semiconductor structure is used to form a first-type transistor, including: a substrate 100; a fin 104, located on the substrate 100; a sidewall anti-punchthrough region 105, located on the sidewall of the fin 104 near the top of the fin 104, the sidewall anti-punchthrough region 105 contains second-type ions, and the second-type ions are different from the doping ions of the first-type transistor; a gate structure 111, spanning multiple fins 104, and the gate structure 111 covers part of the sidewall of the sidewall anti-punchthrough region 105; a source-drain doping region (not shown in the figure), located in the fin 104 on both sides of the gate structure 111, and the source-drain doping region is doped with the first-type ions.
[0120] In this embodiment, the second type ions are different from the doping ions of the first type transistor, which means that the second type ions are different from the doping ions in the source and drain doping regions.
[0121] In the embodiment of the present invention, a sidewall anti-punchthrough region 105 is provided on the sidewall of the fin 104 near the top of the fin 104, and the sidewall anti-punchthrough region 105 contains doped ions. The type of doped ions in the sidewall anti-punchthrough region 105 is different from the type of doped ions in the source and drain doping regions. Compared with the case where the sidewall anti-punchthrough region 105 does not exist on the sidewall of the fin 104, the depletion layer of the source and the drain in the source and drain doping regions is not easy to expand on the sidewall of the fin 104, thereby reducing the probability of punch-through of the source and the drain, which is beneficial to improving the electrical performance of the semiconductor structure.
[0122] In this embodiment, the material of the substrate 103 is silicon. In other embodiments, the material of the substrate may also be germanium, silicon carbide, gallium arsenide or indium gallium, and the substrate may also be a silicon substrate on an insulator or a germanium substrate on an insulator. An interface layer may also be formed on the surface of the substrate 103, and the material of the interface layer may be silicon oxide, silicon nitride or silicon oxynitride.
[0123] In this embodiment, the material of the fin 104 is the same as that of the substrate 103 .
[0124] The semiconductor structure further includes an isolation layer 112 for electrically isolating adjacent fins 104 .
[0125] In this embodiment, the material of the isolation layer 112 is a dielectric material. Specifically, the material of the isolation layer 112 includes one or more of silicon oxide, silicon nitride, silicon carbonitride, silicon carbonitride oxide, silicon nitride oxide, boron nitride and boron carbonitride. In this embodiment, the material of the isolation layer 112 is silicon oxide.
[0126] It should be noted that the sidewall anti-punchthrough region 105 should not be too high or too low. If the sidewall anti-punchthrough region 105 is too high, the process time for forming the sidewall anti-punchthrough region 105 is too long, process defects are difficult to control, and it is not easy to improve the formation quality of the semiconductor structure. When the semiconductor structure is working, the sidewall anti-punchthrough region 105 is used to prevent the depletion layer of the source and drain of the source and drain doping regions from expanding on the sidewalls of the fins. If the sidewall anti-punchthrough region 105 is too low, the bottom of the gate structure is too much lower than the bottom of the sidewall anti-punchthrough region 105, which makes it easy for the source and drain doping regions to punch through the sidewalls of the fins 104 below the sidewall anti-punchthrough region 105. In this embodiment, the height of the sidewall anti-punchthrough region 105 accounts for one-third to one-half of the height of the fin 104.
[0127] In this embodiment, when the first-type transistor is NMOS, the second-type ions are P-type ions, and the P-type ions include boron, gallium or indium.
[0128] It should be noted that the doping concentration in the sidewall anti-punchthrough region 105 should not be too high or too low. If the doping concentration of the second type ions in the sidewall anti-punchthrough region 105 is too high, it is easy to cause the second type ions in the sidewall anti-punchthrough region 105 to diffuse into the channel region, which is easy to cause carrier scattering when the semiconductor structure is working, and thus cause the carrier migration rate to be low. If the doping concentration of the second type ions in the sidewall anti-punchthrough region 105 is too low, when the semiconductor structure is working, it is not easy for the sidewall anti-punchthrough region 105 to prevent the depletion layer of the source and drain of the source and drain doping region from expanding on the sidewall of the fin 104, which is easy to cause the punch-through of the source and drain. In this embodiment, the doping concentration in the sidewall anti-punchthrough region 105 is 3E17 atoms per cubic centimeter to 3E18 atoms per cubic centimeter.
[0129] In other embodiments, when the first-type transistor is PMOS, the second-type ions are N-type ions, and the N-type ions include phosphorus, arsenic or antimony; the doping concentration in the sidewall anti-punch-through region 105 is 3E17 atoms per cubic centimeter to 3E18 atoms per cubic centimeter.
[0130] It should be noted that, in the direction perpendicular to the extension of the fin 104, the size of the sidewall anti-punchthrough region 105 should not be too large or too small. If the size is too large, the width of the channel region is too small in the direction perpendicular to the extension of the fin 104, which may easily lead to a too low carrier migration rate when the semiconductor structure is working. If the size is too small, the sidewall anti-punchthrough region 105 will not easily prevent the depletion layer of the source and drain in the source-drain doping region from expanding on the sidewall of the fin 104, causing the source and drain to be easily punched through. In this embodiment, in the direction perpendicular to the extension of the fin 104, the width of the sidewall anti-punchthrough region 105 is 1 nanometer to 3 nanometers.
[0131] When the semiconductor structure is working, the gate structure 111 is used to open or close the channel.
[0132] In this embodiment, the gate structure 111 includes a gate oxide layer (not shown in the figure) and a gate layer (not shown in the figure) located on the gate oxide layer.
[0133] In this embodiment, the material of the gate oxide layer is silicon oxide. In other embodiments, the material of the gate oxide layer may also be silicon oxynitride. In this embodiment, the material of the gate layer is polysilicon. In other embodiments, the material of the gate layer may also be amorphous carbon.
[0134] In other embodiments, the gate structure is a metal gate structure, and the metal gate structure includes a gate dielectric layer (not shown in the figure) and a metal gate layer (not shown in the figure) located on the gate dielectric layer.
[0135] The source-drain doped regions are used to provide stress to the channel and increase the migration rate of carriers.
[0136] In this embodiment, the first-type transistor is NMOS, and the source and drain doping regions are silicon carbide or silicon phosphide doped with first-type ions. In this embodiment, the first-type ions include: phosphorus, arsenic or antimony.
[0137] In other embodiments, the first-type transistor is a PMOS. The source and drain doping regions are silicon germanium doped with first-type ions. In this embodiment, the first-type ions include boron, gallium or indium.
[0138] The semiconductor structure further includes a bottom anti-punch-through region 110 located in the fin 104 below the sidewall anti-punch-through region 105 .
[0139] The doping ion type of the bottom anti-punchthrough region 110 is the same as the doping ion type of the sidewall anti-punchthrough region 105, both of which are second-type ions. When the semiconductor structure is working, the bottom anti-punchthrough region 110 and the sidewall anti-punchthrough region 105 respectively make it difficult for the depletion layer of the source and the drain to expand from the bottom surface and the side wall of the channel, thereby making it difficult for the source and the drain of the source-drain doping region to be punched through.
[0140] In this embodiment, the top surface of the bottom anti-punchthrough region 110 is higher than the bottom surface of the sidewall anti-punchthrough region 105 or is flush with the bottom surface of the sidewall anti-punchthrough region 105. Compared with the case where the top surface of the bottom anti-punchthrough region 110 is lower than the sidewall anti-punchthrough region 105, when the semiconductor structure is working, this embodiment makes it difficult for the depletion layer of the source and the drain to expand between the sidewall anti-punchthrough region 105 and the bottom anti-punchthrough region 110, thereby making it difficult for the source and the drain of the source and drain doping regions to be punched through.
[0141] It should be noted that the bottom surface of the gate structure 111 should not be too high or too low above the top surface of the bottom anti-punch-through region 110. If the bottom surface of the gate structure 111 is too high above the top surface of the bottom anti-punch-through region 110, that is, when the semiconductor structure is working, the channel is too far away from the bottom anti-punch-through region 110, and the depletion layer of the source and drain of the source-drain doping region is likely to expand at the bottom of the channel, resulting in the punch-through of the source and drain of the source-drain doping region. If the bottom surface of the gate structure 111 is too low above the top surface of the bottom anti-punch-through region 110, that is, when the semiconductor structure is working, the bottom anti-punch-through region 110 of partial thickness acts as a channel, which is likely to cause carrier scattering, thereby resulting in a low carrier migration rate. In this embodiment, the bottom surface of the gate structure 111 is not lower than the top surface of the bottom anti-punch-through region 110 by 10 nanometers, and the bottom surface of the gate structure 111 is not higher than the top surface of the bottom anti-punch-through region 110 by 5 nanometers.
[0142] It should be noted that, in other embodiments, the bottom anti-punchthrough zone is located on the side wall of the fin, and in the direction perpendicular to the extension direction of the fin, the size of the bottom anti-punchthrough zone is larger than the size of the side wall anti-punchthrough zone, and there is an undoped fin area between the bottom anti-punchthrough zone on the two side walls of the fin, that is, there is an area under the channel area that is not doped with the second type of ions.
[0143] When the semiconductor structure is working, the bottom anti-punchthrough region is located below the channel region, and in the direction perpendicular to the extension of the fin, the size of the bottom anti-punchthrough region is larger than the size of the sidewall anti-punchthrough region, so that the depletion layer of the source and drain in the subsequently formed source-drain doping region is not easy to expand at the bottom of the fin. There is an area below the channel region that is not doped with the second type of ions, so that the second type of ions in the bottom anti-punchthrough region are not easy to diffuse into the channel region of the fin, so that when the semiconductor structure is working, carrier scattering is not easy to occur in the channel, so that the migration rate of carriers in the channel is high when the semiconductor structure is working later.
[0144] The semiconductor structure can be formed by the formation method described in the above embodiment, or by other formation methods. For the specific description of the semiconductor structure described in this embodiment, reference can be made to the corresponding description in the above embodiment, and this embodiment will not be repeated here.
[0145] Although the embodiments of the present invention are disclosed above, the embodiments of the present invention are not limited thereto. Any person skilled in the art may make various changes and modifications without departing from the spirit and scope of the embodiments of the present invention. Therefore, the protection scope of the embodiments of the present invention shall be subject to the scope defined by the claims.
Claims
1. A method for forming a semiconductor structure, for forming a first-type transistor, characterized in that: include: providing a substrate; Etching the base to form a substrate and a fin located on the substrate, wherein a sidewall anti-punchthrough region is formed on a sidewall of the fin near a top of the fin, the sidewall anti-punchthrough region is formed on a sidewall parallel to an extending direction of the fin, and the sidewall anti-punchthrough region contains second-type ions, which are different from doping ions of the first-type transistor; After providing a substrate, before etching the substrate, the method further includes: forming a mask layer on the substrate; the step of forming a substrate and a fin located on the substrate includes: etching the substrate using the mask layer as a mask to form an initial substrate and an initial fin located on the initial substrate; using the mask layer as a mask, doping the sidewalls of the initial fin and the initial substrate exposed by the initial fin to form a doped region; after forming the doped region, removing a portion of the thickness of the initial substrate using the mask layer as a mask to form a substrate and a fin located on the substrate, wherein the doped region located on the sidewalls of the fin serves as a sidewall anti-punch-through region; forming a gate structure across the fin, wherein the gate structure covers a portion of the sidewall of the sidewall anti-punch-through region; Source and drain doping regions are formed in the fins at both sides of the gate structure, and first type ions are formed in the source and drain doping regions.
2. The method for forming a semiconductor structure according to claim 1, wherein: Ion implantation is used to perform doping on the sidewalls of the initial fin and the initial substrate exposed by the initial fin to form a doped region.
3. The method for forming a semiconductor structure according to claim 2, wherein: When the first-type transistor is NMOS, the process parameters of the second-type ion implantation include: the second-type ions are P-type ions, and the P-type ions include boron ions, gallium ions or indium ions; the second-type ion implantation energy is 0.5Kev to 1Kev; the second-type ion implantation dose is 3E12 atoms per square centimeter to 3E13 atoms per square centimeter, and the angle between the implantation direction and the substrate surface normal is 0 degrees to 5 degrees; When the first-type transistor is PMOS, the process parameters of the second-type ion implantation include: the second-type ions are N-type ions, and the N-type ions include phosphorus ions, arsenic ions or antimony ions; the second-type ion implantation energy is 0.5Kev to 1Kev; the implantation dose of the second-type ions is 3E12 atoms per square centimeter to 3E13 atoms per square centimeter; the angle between the implantation direction and the normal to the substrate surface is 0 degrees to 5 degrees.
4. The method for forming a semiconductor structure according to claim 2, wherein: The process parameters for etching the base to form the initial fin are the same as the process parameters for etching the initial substrate to form the fin.
5. The method for forming a semiconductor structure according to claim 1, wherein: After forming the doped region, before etching the initial substrate to form the fin, the method further includes: performing annealing treatment on the doped region.
6. The method for forming a semiconductor structure according to claim 1, wherein: The height of the sidewall anti-punch-through area accounts for one third to one half of the height of the fin.
7. The method for forming a semiconductor structure according to claim 1, wherein: In a direction perpendicular to the extension direction of the fin, a size of the sidewall anti-punch-through region is 1 nanometer to 3 nanometers.
8. A semiconductor structure, which is a first-type transistor, characterized in that: The semiconductor structure is formed by the method for forming a semiconductor structure according to any one of claims 1 to 7, comprising: A substrate; a fin located on the substrate; a sidewall anti-punchthrough region located on a sidewall of the fin near a top of the fin, the sidewall anti-punchthrough region being formed on a sidewall parallel to an extension direction of the fin, the sidewall anti-punchthrough region containing second-type ions, the second-type ions being different from doping ions of a first-type transistor; a gate structure spanning across a plurality of the fins, the gate structure covering a portion of the sidewalls of the sidewall anti-punchthrough region; and a source-drain doping region located in the fins on both sides of the gate structure, the source-drain doping region being doped with first-type ions.
9. The semiconductor structure according to claim 8, characterized in that The height of the sidewall anti-punch-through area accounts for one third to one half of the height of the fin.
10. The semiconductor structure according to claim 8, wherein: In a direction perpendicular to the extension direction of the fin, the width of the sidewall anti-punch-through region is 1 nanometer to 3 nanometers.
11. The semiconductor structure according to claim 8, wherein: The semiconductor structure is NMOS, the second-type ions are P-type ions, and the P-type ions include boron ions, gallium ions or indium ions; the doping concentration of the second-type ions in the sidewall anti-punch-through region is 3E17 atoms per cubic centimeter to 3E18 atoms per cubic centimeter; The semiconductor structure is PMOS, the second-type ions are N-type ions, and the N-type ions include phosphorus ions, arsenic ions or antimony ions; the second-type ion doping concentration in the sidewall anti-punch-through region is 3E17 atoms per cubic centimeter to 3E18 atoms per cubic centimeter.
12. The semiconductor structure according to claim 8, wherein: The semiconductor structure further includes a bottom anti-punch-through region located in the fin portion below the sidewall anti-punch-through region.
13. The semiconductor structure according to claim 12, wherein: The top surface of the bottom anti-punch-through region is higher than the bottom surface of the sidewall anti-punch-through region or is flush with the bottom surface of the sidewall anti-punch-through region.
14. The semiconductor structure according to claim 12, wherein: The bottom surface of the gate structure is not lower than the top surface of the bottom anti-punch-through region by 10 nanometers, and the bottom surface of the gate structure is not higher than the top surface of the bottom anti-punch-through region by 5 nanometers.
Citation Information
Patent Citations
FinFET channel doping method
CN103515205A
Fin type field effect transistor and formation method thereof
CN108573869A