Inner ring undercut injection molding demoulding structure
By designing the inner peripheral ring inverted injection molding and releasing structure, using the cooperation of the inclined guide column and slider, the problem of poor mold release effect of the inverted injection mold in the prior art is solved, and the smooth mold release and cost of injection molded parts are achieved reduce.
Patent Information
- Application Number
- CN202011011961.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2020-09-23
- Publication Date
- 2024-11-22
- Estimated Expiration
- 2040-09-23
Smart Images

Figure CN112092311B_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of undercut injection molding, in particular to an inner circumference undercut injection molding demoulding structure. Background Art
[0002] Injection molded products are usually more complicated when the mold involves an undercut structure. Especially when there are undercuts on all sides, the mold needs to have sliders for demolding, which is difficult to design. Usually, a hydraulic cylinder with a slider is used for demolding, or a large slider structure is used, which is very complicated, costly, and the demolding effect is not very good.
[0003] Therefore, providing an inner ring undercut injection molding demolding structure with good demolding effect has become an important technical problem to be solved by those skilled in the art. Summary of the invention
[0004] The object of the present invention is to provide an inner circumferential ring undercut injection molding demoulding structure to alleviate the technical problem of poor demoulding effect in the prior art.
[0005] In a first aspect, an embodiment of the present invention provides an inner circumferential ring undercut injection molding demolding structure, comprising a first fixed plate, a lower mold plate, an upper mold plate, a second fixed plate, a front mold core, and a rear mold core;
[0006] The lower template is arranged between the first fixing plate and the upper template, and the upper template is arranged between the lower template and the second fixing plate;
[0007] The front mold core is arranged on the lower mold plate, and the rear mold core is arranged on the upper mold plate;
[0008] The lower mold plate and the front mold core are both provided with inclined guide pillars;
[0009] The upper template is slidably provided with a plurality of outer sliding blocks, and the plurality of outer sliding blocks are all connected to the inclined guide pillars, so that the inclined guide pillars can drive the outer sliding blocks to slide on the upper template;
[0010] A first inner slider and a second inner slider are slidably disposed in the rear mold core, the first inner slider is connected to the inclined guide column so that the inclined guide column can drive the first inner slider to slide on the rear mold core, and a driving member for driving the second inner slider is disposed on the upper mold plate;
[0011] An inclined wedge shovel is fixedly arranged on the first fixed plate, and a front mold slider is arranged on the inclined wedge shovel. When the lower mold plate is away from the first fixed plate, the front mold slider is away from the injection molded part.
[0012] In combination with the first aspect, an embodiment of the present invention provides a possible implementation of the first aspect, wherein one end of the above-mentioned inclined wedge shovel is fixedly arranged on the first fixed plate, and the other end is wedge-shaped, and a limiting slide rail is arranged at the wedge-shaped end of the inclined wedge shovel, and a limiting slide groove adapted to the limiting slide rail is opened on the front mold slide block, so that when the lower mold plate is away from the first fixed plate, the front mold slide block can be away from the injection molded part;
[0013] The front mold slider is provided with a molding surface for molding the inner side of the injection molded part.
[0014] In combination with the first aspect, an embodiment of the present invention provides a possible implementation of the first aspect, wherein the outer slider includes a first outer slider, a second outer slider and a third outer slider;
[0015] The first outer slider, the second outer slider and the third outer slider are all provided with guide post holes adapted to the oblique guide posts;
[0016] The first outer slider, the second outer slider and the third outer slider are all provided with molding surfaces for molding the outer side of the injection molded part.
[0017] In combination with the first aspect, an embodiment of the present invention provides a possible implementation of the first aspect, wherein a molding surface extending along a first direction is provided on one side of the first inner sliding block, an inclined top is inserted into the first inner sliding block, and the inclined top cooperates with the first inner sliding block to form a molding surface extending along a second direction, and the first direction intersects with the second direction;
[0018] A cavity is provided in the first inner sliding block, a slanted top seat is slidably provided in the cavity, the slanted top is slidably sleeved on the slanted top seat, and the slanted top can slide up and down in the vertical direction;
[0019] The first inner sliding block is provided with an inclined mounting hole for mounting the inclined top, and the inclined mounting hole is closer to the rear mold core as it is farther away from the inclined top seat.
[0020] In combination with the first aspect, an embodiment of the present invention provides a possible implementation of the first aspect, wherein a positioning piece is inserted on the inclined top seat, a first positioning arc groove adapted to the positioning piece is opened on the rear mold core, and a second positioning arc groove adapted to the positioning piece is opened in the cavity;
[0021] Before demoulding, the second positioning arc groove is closer to the molding surface than the first positioning arc groove;
[0022] Before demoulding, one end of the positioning member abuts against the inner wall of the cavity, and the other end is located in the first positioning arc groove.
[0023] In combination with the first aspect, an embodiment of the present invention provides a possible implementation of the first aspect, wherein a tilted top stopper is provided on the tilted top seat, and a tilted top stopper groove adapted to the tilted top stopper is provided on the rear mold core.
[0024] In combination with the first aspect, an embodiment of the present invention provides a possible implementation of the first aspect, wherein a lifting rod is provided on the outer wall of the upper template, a locking buckle is provided on the outer wall of the lower template, and an unlocking rod is provided on the first fixing plate;
[0025] A spring and a bolt plate are arranged in the lock buckle, and a slot for engaging with the bolt plate is provided on the lifting rod;
[0026] The unlocking rod is provided with an arc-shaped protrusion, and the lock tongue plate is provided with a lock head capable of abutting against the arc-shaped protrusion. When the arc-shaped protrusion abuts against the lock head, the lock tongue plate is disengaged from the slot.
[0027] In combination with the first aspect, an embodiment of the present invention provides a possible implementation of the first aspect, wherein a plurality of light holes are opened on the above-mentioned lower template, and limiting bolts are arranged in the light holes, and the limiting bolts are fixedly connected to the first fixing plate.
[0028] In combination with the first aspect, an embodiment of the present invention provides a possible implementation of the first aspect, wherein cooling pipelines are provided on the lower template and the upper template.
[0029] In combination with the first aspect, an embodiment of the present invention provides a possible implementation of the first aspect, wherein an injection molding pipeline is arranged on the second fixed plate, and the injection molding pipeline is connected to the upper mold plate.
[0030] Beneficial effects:
[0031] The embodiment of the present invention provides an inner circumferential undercut injection molding demolding structure, comprising a first fixed plate, a lower template, an upper template, a second fixed plate, a front mold core and a rear mold core; the lower template is arranged between the first fixed plate and the upper template, and the upper template is arranged between the lower template and the second fixed plate; the front mold core is arranged on the lower template, and the rear mold core is arranged on the upper template; inclined guide columns are arranged on the lower template and the front mold core; a plurality of outer sliding blocks are slidably arranged on the upper template, and the plurality of outer sliding blocks are connected to the inclined guide columns so that the inclined guide columns can drive the outer sliding blocks to slide on the upper template; a first inner sliding block and a second inner sliding block are slidably arranged in the rear mold core, and the first inner sliding block is connected to the inclined guide columns so that the inclined guide columns can drive the first inner sliding block to slide on the rear mold core, and a driving member for driving the second inner sliding block is arranged on the upper template; an inclined wedge shovel is fixedly arranged on the first fixed plate, and a front mold slider is arranged on the inclined wedge shovel, and when the lower template is away from the first fixed plate, the front mold slider is away from the injection molded part.
[0032] During specific use, the staff first lifts the lower template, at which time the inclined wedge shovel will drive the front mold slider to separate from the injection molded part, and then the staff separates the upper template from the lower template. In the process of the upper template moving away from the lower template, the inclined guide columns set on the lower template and the front mold core will drive the multiple outer sliders on the upper template to slide relative to the upper template, thereby making the multiple outer sliders move away from the injection molded part. At the same time, the inclined guide columns will also drive the first inner slider on the rear mold core away from the injection molded part, and finally drive the second inner slider away from the injection molded part through the driving member. Through such a setting, the injection molded part formed by the inner circumference undercut injection molding can be conveniently demolded. BRIEF DESCRIPTION OF THE DRAWINGS
[0033] In order to more clearly illustrate the specific implementation methods of the present invention or the technical solutions in the prior art, the drawings required for use in the specific implementation methods or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are some implementation methods of the present invention. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative work.
[0034] Figure 1 A schematic diagram of an inner ring undercut injection molding demoulding structure provided by an embodiment of the present invention;
[0035] Figure 2 A first cross-sectional view of a schematic diagram of an inner peripheral ring undercut injection molding demoulding structure provided by an embodiment of the present invention;
[0036] Figure 3 A second cross-sectional view of a schematic diagram of an inner peripheral ring undercut injection molding demoulding structure provided by an embodiment of the present invention;
[0037] Figure 4 A partial schematic diagram of an inner ring undercut injection molding demoulding structure provided by an embodiment of the present invention;
[0038] Figure 5 An internal schematic diagram of an inner peripheral ring undercut injection molding demoulding structure provided by an embodiment of the present invention;
[0039] Figure 6 A schematic diagram of an inclined wedge scraper in an inner ring undercut injection molding demoulding structure provided by an embodiment of the present invention;
[0040] Figure 7 A cross-sectional view of a first inner sliding block in an inner peripheral ring undercut injection molding demoulding structure provided by an embodiment of the present invention;
[0041] Figure 8 The product is produced by the inner circumference undercut injection molding demoulding structure provided in the embodiment of the present invention.
[0042] icon:
[0043] 100 - first fixed plate; 110 - inclined wedge shovel; 120 - front mold slide; 130 - limit slide rail;
[0044] 200 - lower template; 210 - inclined guide column; 220 - limit bolt;
[0045] 300 - upper template; 310 - first outer slider; 320 - second outer slider; 330 - third outer slider; 340 - guide post hole;
[0046] 400 - second fixing plate;
[0047] 500-front mold;
[0048] 600-rear mold core; 610-first inner slide; 611-tilted top; 612-tilted top seat; 613-inclined mounting hole; 614-positioning member; 615-first positioning arc groove; 616-second positioning arc groove; 617-tilted top limiting member; 618-tilted top limiting groove; 619-first through hole; 620-second inner slide; 630-driving member; 631-push rod;
[0049] 710 - lifting rod; 720 - unlocking rod; 721 - arc-shaped protrusion; 730 - spring; 740 - locking tongue plate; 741 - locking head. DETAILED DESCRIPTION
[0050] The technical solution of the present invention will be described clearly and completely below in conjunction with the accompanying drawings. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0051] In the description of the present invention, it should be understood that the terms "center", "longitudinal", "lateral", "length", "width", "thickness", "up", "down", "front", "back", "left", "right", "vertical", "horizontal", "top", "bottom", "inside", "outside", "clockwise", "counterclockwise", "axial", "radial", "circumferential" and the like indicate orientations or positional relationships based on the orientations or positional relationships shown in the accompanying drawings, and are only for the convenience of describing the present invention and simplifying the description, and do not indicate or imply that the referred device or element must have a specific orientation, be constructed and operated in a specific orientation, and therefore should not be understood as limiting the present invention.
[0052] In addition, the terms "first" and "second" are used for descriptive purposes only and should not be understood as indicating or implying relative importance or implicitly indicating the number of the indicated technical features. Therefore, the features defined as "first" and "second" may explicitly or implicitly include one or more of the features. In the description of the present invention, the meaning of "plurality" is two or more, unless otherwise clearly and specifically defined.
[0053] In the present invention, unless otherwise clearly specified and limited, the terms "installed", "connected", "connected", "fixed" and the like should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection or an electrical connection; it can be a direct connection or an indirect connection through an intermediate medium, it can be the internal connection of two elements or the interaction relationship between two elements. For ordinary technicians in this field, the specific meanings of the above terms in the present invention can be understood according to specific circumstances.
[0054] The present invention is further described in detail below through specific embodiments in conjunction with the accompanying drawings.
[0055] See also Figure 1 , Figure 2 , Figure 3 , Figure 4 , Figure 5 , Figure 6 , Figure 7 and Figure 8 As shown, the present embodiment provides an inner circumferential undercut injection molding demolding structure, comprising a first fixed plate 100, a lower template 200, an upper template 300, a second fixed plate 400, a front mold core 500 and a rear mold core 600; the lower template 200 is arranged between the first fixed plate 100 and the upper template 300, and the upper template 300 is arranged between the lower template 200 and the second fixed plate 400; the front mold core 500 is arranged on the lower template 200, and the rear mold core 600 is arranged on the upper template 300; the lower template 200 and the front mold core 500 are both provided with inclined guide columns 210; the upper template 300 is slidably provided with a plurality of outer sliders, and the plurality of outer sliders are all in contact with the inclined guide columns 210; The column 210 is connected so that the inclined guide column 210 can drive the outer slider to slide on the upper mold plate 300; the first inner slider 610 and the second inner slider 620 are slidably arranged in the rear mold core 600, and the first inner slider 610 is connected to the inclined guide column 210 so that the inclined guide column 210 can drive the first inner slider 610 to slide on the rear mold core 600, and the upper mold plate 300 is provided with a driving member 630 for driving the second inner slider 620; an inclined wedge shovel machine 110 is fixedly arranged on the first fixed plate 100, and a front mold slider 120 is arranged on the inclined wedge shovel machine 110, and when the lower mold plate 200 is away from the first fixed plate 100, the front mold slider 120 is away from the injection molded part.
[0056] When in use, the staff first lifts the lower template 200, at which time the inclined wedge shovel 110 drives the front mold slider 120 to separate from the injection molded part, and then the staff separates the upper template 300 from the lower template 200. In the process of the upper template 300 moving away from the lower template 200, the inclined guide pillars 210 set on the lower template 200 and the front mold core 500 will drive the multiple outer sliders on the upper template 300 to slide relative to the upper template 300, so that the multiple outer sliders are away from the injection molded part. At the same time, the inclined guide pillars 210 will also drive the first inner slider 610 on the rear mold core 600 away from the injection molded part, and finally drive the second inner slider 620 away from the injection molded part through the driving member 630. Through such a setting, the injection molded part formed by the inner circumference undercut injection molding can be easily demoulded. Among them, the driving member 630 is connected to the second inner slider 620 through the push rod 631.
[0057] Among them, the inclined guide column 210 is set on the lower template 200 and the front mold core 500. When the lower template 200 is separated from the upper template 300, the inclined guide column 210 can drive the outer slider on the upper template 300 and the first inner slider 610 and the second inner slider 620 on the rear mold core 600, so that the outer slider, the first inner slider 610 and the second inner slider 620 are separated from the injection molded part and away from the injection molded part, so that the injection molded part can be discharged smoothly.
[0058] It should be pointed out that when the inner circumferential inverted injection molding demolding structure provided in this embodiment is in use, the first fixed plate 100, the lower template 200, the upper template 300 and the second fixed plate 400 are in an upright state, the upper template 300 is not above the lower template 200, and the second fixed plate 400 is connected to the driving end of the injection molding equipment. Through the drive of the injection molding equipment, the second fixed plate 400 can drive the upper template 300 to move horizontally away from the lower template 200.
[0059] In addition, a lifting rod 710 is provided on the outer wall of the upper template 300, a lock is provided on the outer wall of the lower template 200, and an unlocking rod 720 is provided on the first fixed plate 100; a spring 730 and a lock plate 740 are provided in the lock, and a slot engaged with the lock plate 740 is provided on the lifting rod 710; an arc-shaped protrusion 721 is provided on the unlocking rod 720, and a lock head 741 capable of abutting against the arc-shaped protrusion 721 is provided on the lock plate 740. When the arc-shaped protrusion 721 abuts against the lock head 741, the lock plate 740 is disengaged from the slot. When the injection molding equipment drives the upper mold plate 300 away from the lower mold plate 200, due to the clamping connection between the lifting rod 710 and the lock buckle, the injection molding equipment will move the upper mold plate 300 and the lower mold plate 200 synchronously. At this time, the first fixed plate 100 is fixed to the injection molding equipment, so the lower mold plate 200 will be separated from the first fixed plate 100. At this time, the inclined wedge shovel 110 can drive the front mold slider 120 to demould, and the unlocking rod 710 fixed on the first fixed plate 100 is released when the lower mold plate 200 is away from the first fixed plate 100. When the upper template 200 moves to the set position, the arc-shaped protrusion 721 on the unlocking rod 720 can abut against the lock head 741, thereby exerting pressure on the lock head 741, so that the lock head 741 drives the lock tongue plate 740 to compress the spring 730. At this time, the lock tongue plate 740 is in contact with the lifting rod 710, and the upper template 300 can move away from the lower template 200, thereby continuing the demolding of the outer slider, the first inner slider 610 and the second inner slider 620.
[0060] In addition, a plurality of light holes are provided on the lower template 200, and limit bolts 220 are provided in the light holes, and the limit bolts 220 are fixedly connected to the first fixing plate 100. By setting the limit bolts 220, the lower template 200 is limited to the maximum position away from the first fixing plate 100, so as to prevent the lower template 200 from falling off.
[0061] See also Figure 1 - Figure 8 As shown, in an optional scheme of the present embodiment, one end of the inclined wedge shovel 110 is fixedly set on the first fixed plate 100, and the other end is wedge-shaped, and a limiting slide rail 130 is provided at the wedge-shaped end of the inclined wedge shovel 110, and a limiting slide groove adapted to the limiting slide rail 130 is provided on the front mold slider 120, so that when the lower mold plate 200 is away from the first fixed plate 100, the front mold slider 120 can be away from the injection molded part; the front mold slider 120 is provided with a molding surface for molding the inner side of the injection molded part.
[0062] Specifically, when the lower template 200 is away from the first fixed plate 100, the angled wedge shovel 110 is fixed on the first fixed plate 100, so the angled wedge shovel 110 will not move with the lower template 200, and the front mold slider 120 is located in the front mold core 500. Driven by the lower template 200, the front mold core 500 will drive the front mold slider 120 to move with the lower template 200. At this time, the front mold slider 120 will move along the limiting slide rail 130, thereby separating the front mold slider 120 from the injection molded part.
[0063] When the lower mold plate 200 moves away from the first fixed plate 100 , the angled wedge shovel 110 moves away from the front mold core 500 , and after moving away, the angled wedge shovel 110 provides space for the front mold slider 120 so that the front mold slider 120 can move in a direction away from the injection molded part.
[0064] See also Figure 1 - Figure 8 As shown, in an optional scheme of this embodiment, the outer slider includes a first outer slider 310, a second outer slider 320 and a third outer slider 330; the first outer slider 310, the second outer slider 320 and the third outer slider 330 are all provided with guide post holes adapted to the inclined guide post 210; the first outer slider 310, the second outer slider 320 and the third outer slider 330 are all provided with a molding surface for outer molding of the injection molded part.
[0065] Specifically, when the upper mold plate 300 is separated from the lower mold plate 200, the inclined guide pillars 210 on the lower mold plate 200 will drive the first outer slider 310, the second outer slider 320 and the third outer slider 330 to move away from the injection molded part, thereby completing the demoulding work.
[0066] See also Figure 1 - Figure 8 As shown, in an optional scheme of the present embodiment, a molding surface extending along a first direction is provided on one side of the slider, a slanted top 611 is inserted in the slider, the slanted top 611 cooperates with the slider to form a molding surface extending along a second direction, and the first direction intersects with the second direction; a cavity is provided in the slider, a slanted top seat 612 is slidably provided in the cavity, the slanted top 611 is slidably sleeved on the slanted top seat 612, and the slanted top 611 can slide up and down in a vertical direction; an inclined mounting hole 613 for mounting the slanted top 611 is provided on the slider, and the inclined mounting hole 613 is closer to the rear mold core 600 as it is farther away from the slanted top seat 612.
[0067] Specifically, during demoulding, the first inner slider 610 is driven by the inclined guide column 210 to move in a direction away from the injection molded part. During the movement, the first inner slider 610 is away from the injection molded part, so that the molding surface on the first inner slider 610 is separated from the injection molded part. At this time, the molding surface formed by the inclined top 611 and the first inner slider 610 is locked with the injection molded part, so that the inclined top 611 does not move with the first inner slider 610, so that the inclined top 611 is pulled out of the first inner slider 610, and the inclined top 611 is pulled out of the slider along the inclined mounting hole 613, and the inclined mounting hole 613 is pulled out of the slider. The farther away from the inclined top seat 612, the closer to the rear mold core 600 it is. Therefore, when the inclined top 611 is pulled out of the slider, it will move toward the rear mold core 600, so that the molding surface formed by the inclined top 611 and the slider is separated from the injection molded part. Because one end of the inclined top 611 is mounted on the inclined top seat 612, the inclined top 611 will not be pulled out from the first inner slider 610. When the first inner slider 610 moves to abut against the inclined top seat 612, the first inner slider 610 can drive the inclined top seat 612 to move, thereby moving the inclined top 611 away from the injection molded part. Such an arrangement can achieve demolding in two directions.
[0068] It should be noted that the above method can be used for injection molded parts with greater structural strength.
[0069] See also Figure 1 - Figure 8 As shown, in an optional scheme of the present embodiment, a positioning piece 614 is inserted on the inclined top seat 612, a first positioning arc groove 615 adapted to the positioning piece 614 is provided on the rear mold core 600, and a second positioning arc groove 616 adapted to the positioning piece 614 is provided in the cavity; before demolding, the second positioning arc groove 616 is closer to the molding surface than the first positioning arc groove 615; before demolding, one end of the positioning piece 614 abuts against the inner wall of the cavity, and the other end is located in the first positioning arc groove 615.
[0070] Specifically, during demolding, the first inner slide 610 moves in a direction away from the injection molded part. At this time, the positioning piece 614 on the inclined top seat 612 is positioned by the second positioning arc groove 616 on the rear mold core 600, and at this time, the inner wall of the slider is not in contact with the front wall of the inclined top seat 612, so the positioning piece 614 will not move. Since the positioning piece 614 does not move, the inclined top seat 612 is fixed, and the inclined top seat 612 will support the inclined top 611 and will not move with the first inner slide 610. Moreover, the inclined mounting hole 613 on the first inner slide 610 is farther away from the inclined top seat 612 and closer to the rear mold core 600. Therefore, when the inclined top 611 is pushed out of the first inner slide 610 by the inclined top seat 612, the inclined top 611 will move toward the rear mold core 600, so that the inclined top 611 can be separated from the injection molded part.
[0071] Among them, when the first inner sliding block 610 continues to move away from the injection molded part, the first positioning arc groove 615 of the first inner sliding block 610 will move to the positioning member 614. At this time, the upper part of the positioning member 614 is the first positioning arc groove 615, and the lower part is the second positioning arc groove 616. At this time, the inner wall of the first inner sliding block 610 can abut against the outer wall of the inclined top seat 612 on the side close to the injection molded part. When the first inner sliding block drives the inclined top seat 612 to move, the positioning member 614 is forced to separate from the second positioning arc groove 616, so that the first inner sliding block 610 can drive the inclined top seat 612 to move. At this time, the inclined top 611 is completely separated from the injection molded part.
[0072] Among them, by setting the positioning member 614, the injection molded part itself does not need to hold the inclined top 611, thereby improving the quality of the injection molded part after demoulding and reducing the probability of damage to the injection molded part.
[0073] Among them, when not demolded, one end of the positioning member 614 can abut against the inner wall of the first inner sliding block 610, and the other end passes through the first through hole 619 and connects with the second positioning arc groove 616 on the rear mold core 600, so that the inclined top seat 612 is fixed by the positioning member 614.
[0074] See also Figure 1 - Figure 8 As shown, in an optional solution of the present embodiment, a tilted top stopper 617 is provided on the tilted top seat 612 , and a tilted top stopper groove 618 adapted to the tilted top stopper 617 is provided on the rear mold core 600 .
[0075] Specifically, one end of the inclined top limiting member 617 is connected to the inclined top seat 612 , and the other end passes through the second through hole and cooperates with the inclined top limiting groove 618 .
[0076] See also Figure 1 - Figure 8 As shown, in an optional solution of this embodiment, cooling pipelines are provided on both the lower template 200 and the upper template 300 .
[0077] Specifically, the lower mold plate 200, the front mold core 500, the upper mold plate 300 and the rear mold core 600 are cooled by cooling pipelines to improve the quality of the injection molded parts.
[0078] See also Figure 1 - Figure 8 As shown, in an optional solution of this embodiment, an injection molding pipeline is provided on the second fixing plate 400 , and the injection molding pipeline is connected to the upper mold plate 300 .
[0079] Specifically, the injection material is injected between the outer slider, the first inner slider 610 , the second inner slider 620 and the front mold slider 120 through the injection pipeline.
[0080] Finally, it should be noted that the above embodiments are only used to illustrate the technical solutions of the present invention, rather than to limit it. Although the present invention has been described in detail with reference to the aforementioned embodiments, those skilled in the art should understand that they can still modify the technical solutions described in the aforementioned embodiments, or replace some or all of the technical features therein by equivalents. However, these modifications or replacements do not cause the essence of the corresponding technical solutions to deviate from the scope of the technical solutions of the embodiments of the present invention.
Claims
1. An inner ring undercut injection molding demoulding structure, characterized in that: include: A first fixed plate (100), a lower mold plate (200), an upper mold plate (300), a second fixed plate (400), a front mold core (500) and a rear mold core (600); The lower template (200) is arranged between the first fixing plate (100) and the upper template (300), and the upper template (300) is arranged between the lower template (200) and the second fixing plate (400); The front mold core (500) is arranged on the lower mold plate (200), and the rear mold core (600) is arranged on the upper mold plate (300); The lower mold plate (200) and the front mold core (500) are both provided with inclined guide pillars (210); A plurality of outer sliding blocks are slidably arranged on the upper template (300), and the plurality of outer sliding blocks are all connected to the inclined guide pillar (210), so that the inclined guide pillar (210) can drive the outer sliding blocks to slide on the upper template (300); A first inner slider (610) and a second inner slider (620) are slidably disposed in the rear mold core (600); the first inner slider (610) is connected to the inclined guide column (210) so that the inclined guide column (210) can drive the first inner slider (610) to slide on the rear mold core (600); and a driving member (630) for driving the second inner slider (620) is disposed on the upper mold plate (300); The first fixed plate (100) is fixedly provided with an inclined wedge shovel machine (110), and the inclined wedge shovel machine (110) is provided with a front mold slider (120). When the lower mold plate (200) is away from the first fixed plate (100), the front mold slider (120) is away from the injection molded part.
2. The inner ring undercut injection molding demoulding structure according to claim 1, characterized in that: One end of the inclined wedge shovel (110) is fixedly arranged on the first fixed plate (100), and the other end is wedge-shaped, and a limiting slide rail (130) is arranged on the wedge-shaped end of the inclined wedge shovel (110), and a limiting slide groove adapted to the limiting slide rail (130) is opened on the front mold slider (120), so that when the lower mold plate (200) is away from the first fixed plate (100), the front mold slider (120) can be away from the injection molded part; The front mold slider (120) is provided with a molding surface for molding the inner side of the injection molded part.
3. The inner ring undercut injection molding demoulding structure according to claim 1, characterized in that: The outer slider comprises a first outer slider (310), a second outer slider (320) and a third outer slider (330); The first outer slider (310), the second outer slider (320) and the third outer slider (330) are all provided with guide post holes adapted to the inclined guide posts (210); The first outer slider (310), the second outer slider (320) and the third outer slider (330) are all provided with molding surfaces for molding the outer side of the injection molded part.
4. The inner ring undercut injection molding demoulding structure according to claim 1, characterized in that: A molding surface extending along a first direction is provided on one side of the first inner sliding block (610), an inclined top (611) is inserted into the first inner sliding block (610), and the inclined top (611) cooperates with the first inner sliding block (610) to form a molding surface extending along a second direction, and the first direction intersects with the second direction; A cavity is provided in the first inner sliding block (610), an inclined top seat (612) is slidably provided in the cavity, the inclined top (611) is slidably sleeved on the inclined top seat (612), and the inclined top (611) can slide up and down in the vertical direction; The first inner sliding block (610) is provided with an inclined mounting hole (613) for mounting the inclined top (611), and the inclined mounting hole (613) is closer to the rear mold core (600) as it is farther away from the inclined top seat (612).
5. The inner circumferential ring undercut injection molding demoulding structure according to claim 4, characterized in that: A positioning piece (614) is inserted on the inclined top seat (612), a first positioning arc groove (615) adapted to the positioning piece (614) is opened on the rear mold core (600), and a second positioning arc groove (616) adapted to the positioning piece (614) is opened in the cavity; Before demoulding, the second positioning arc groove (616) is closer to the molding surface than the first positioning arc groove (615); Before demoulding, one end of the positioning member (614) abuts against the inner wall of the cavity, and the other end is located in the first positioning arc groove (615).
6. The inner ring undercut injection molding demoulding structure according to claim 5, characterized in that: The inclined top seat (612) is provided with an inclined top limiting member (617), and the rear mold core (600) is provided with an inclined top limiting groove (618) adapted to the inclined top limiting member (617).
7. The inner ring undercut injection molding demoulding structure according to any one of claims 1 to 6, characterized in that: The outer wall of the upper template (300) is provided with a lifting rod (710), the outer wall of the lower template (200) is provided with a locking buckle, and the first fixing plate (100) is provided with an unlocking rod (720); A spring (730) and a locking tongue plate (740) are arranged in the lock buckle, and a slot for locking with the locking tongue plate (740) is provided on the lifting rod (710); The unlocking rod (720) is provided with an arc-shaped protrusion (721), and the locking tongue plate (740) is provided with a locking head (741) capable of abutting against the arc-shaped protrusion (721). When the arc-shaped protrusion (721) abuts against the locking head (741), the locking tongue plate (740) is disengaged from the card slot.
8. The inner ring undercut injection molding demoulding structure according to any one of claims 1 to 6, characterized in that: The lower template (200) is provided with a plurality of light holes, and limit bolts (220) are arranged in the light holes. The limit bolts (220) are fixedly connected to the first fixing plate (100).
9. The inner ring undercut injection molding demoulding structure according to any one of claims 1 to 6, characterized in that: The lower mold plate (200) and the upper mold plate (300) are both provided with cooling pipelines.
10. The inner ring undercut injection molding demoulding structure according to any one of claims 1 to 6, characterized in that: An injection molding pipeline is arranged on the second fixing plate (400), and the injection molding pipeline is connected to the upper mold plate (300).