A metal diffusion barrier layer structure and a method for forming the same

By adopting a three-dimensional molybdenum disulfide barrier layer structure in semiconductor integrated circuits, the copper interconnect reliability and electromigration problems are solved, the barrier layer thickness and resistance are reduced, and process compatibility is improved.

CN112133675BActive Publication Date: 2024-12-06SHANGHAI INTEGRATED CIRCUIT RESEARCH & DEVELOPMENT CENTER CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202010865178.8
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2020-08-25
Publication Date
2024-12-06
Estimated Expiration
2040-08-25

AI Technical Summary

Technical Problem

In advanced semiconductor integrated circuit processes, the reliability problems of copper interconnection are serious. High current density leads to a reduced electromigration life of copper, and copper is prone to diffusing into Low-k medium, resulting in short circuits. The thickness of traditional TaN/Ta diffusion barrier layer Unsustainable reduction leads to high resistance problems.

Method used

The structure from the outside to the inside is adopted, including an adhesion layer, a molybdenum disulfide barrier layer and a wire layer, wherein the molybdenum disulfide barrier layer is formed by infiltration of sulfur into the copper-molybdenum alloy layer, and a multi-layer film with a three-dimensional structure and a coral-like accumulation. Structure, low-temperature ionic sulfur permeability process forms a uniformly covered molybdenum disulfide barrier layer.

Benefits of technology

It effectively reduces the thickness of the barrier layer, improves the metal proportion and conductivity of the wire, improves the electromigration resistance of copper wires, and solves the coverage and process compatibility problems of two-dimensional materials in complex structures.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN112133675B_ABST
    Figure CN112133675B_ABST
Patent Text Reader

Abstract

The present invention discloses a metal diffusion barrier layer structure, including an adhesion layer, a molybdenum disulfide barrier layer, a seed layer and a conductor layer, which are sequentially formed in a groove or hole from the outside to the inside; wherein the molybdenum disulfide barrier layer is formed by infiltrating sulfur into a copper-molybdenum alloy seed layer and reacting with the molybdenum therein. The present invention replaces the traditional tantalum nitride as a metal diffusion barrier layer with a three-dimensional molybdenum disulfide layer, which can greatly reduce the thickness of the barrier layer, increase the proportion of conductor metal, and has good conductivity, thereby greatly reducing the metal interconnection resistance overall, improving the anti-electromigration ability of the copper conductor, and effectively overcoming the problems of groove coverage and process compatibility when introducing two-dimensional materials in the back-end process.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the field of semiconductor integrated circuit process technology, and in particular to a metal diffusion barrier layer structure and a forming method thereof that can be used in back-end interconnection technology. Background Art

[0002] In advanced semiconductor integrated circuit process technology, copper (Cu) is widely used as the conductor connection material and Low-k dielectric is used as the interlayer dielectric to reduce the transmission delay (RC delay) phenomenon in the back-end interconnection. However, with the continuous miniaturization of wire size, the reliability problem of copper interconnection is becoming more and more serious: high current density leads to a decrease in the electromigration (EM) life of copper, and copper easily diffuses into the Low-k dielectric during the process, resulting in device short circuit.

[0003] In order to alleviate the reliability problem of copper interconnection, it is generally necessary to pre-deposit a barrier layer in the metal wire slots and through holes to prevent copper diffusion. Currently, TaN / Ta is mainly used as the diffusion barrier layer. But at the same time, in advanced technology nodes, the thickness of the barrier layer cannot be continuously reduced, otherwise it will not achieve the purpose of preventing copper diffusion. As a result, the proportion of the high-resistance barrier layer in the entire wire increases rapidly, resulting in an increase in the overall back-end resistance. Therefore, it is necessary to introduce new diffusion barrier layer materials.

[0004] Two-dimensional materials such as graphene, molybdenum disulfide and WS2, which are atomically thin and highly conductive, have great potential for interconnect applications and can replace TaN / Ta as diffusion barrier materials. However, there are still many process issues that need to be solved when using these materials, including:

[0005] (1) Two-dimensional materials have a low coverage problem in three-dimensional grooves and through holes in complex structures.

[0006] (2) The traditional two-dimensional material preparation process requires a higher deposition temperature, which leads to incompatibility with the subsequent thermal budget. Summary of the invention

[0007] The purpose of the present invention is to overcome the above-mentioned defects in the prior art and to provide a metal diffusion barrier layer structure and a method for forming the same.

[0008] To achieve the above object, the technical solution of the present invention is as follows:

[0009] A metal diffusion barrier layer structure comprises an adhesion layer, a molybdenum disulfide barrier layer, a seed crystal layer and a conductor layer which are sequentially formed in a groove or a hole from the outside to the inside.

[0010] Furthermore, the seed layer includes a copper-molybdenum alloy layer.

[0011] Furthermore, the molybdenum disulfide barrier layer is formed by infiltrating sulfur into the copper-molybdenum alloy layer and reacting with molybdenum therein.

[0012] Furthermore, the molybdenum disulfide barrier layer has a three-dimensional structure.

[0013] Furthermore, the molybdenum disulfide barrier layer is a coral-like stacked multilayer film structure.

[0014] Further, the groove comprises an interconnection groove, and the hole comprises a through hole.

[0015] A method for forming a metal diffusion barrier layer structure comprises the following steps:

[0016] Step 1: providing a substrate, forming a dielectric layer on the substrate, and forming grooves or holes on the dielectric layer;

[0017] Step 2: forming an adhesive layer on the inner wall surface of the groove or hole;

[0018] Step 3: forming a copper-molybdenum alloy layer as a seed layer on the adhesion layer;

[0019] Step 4: infiltrating sulfur into the copper-molybdenum alloy layer and reacting with molybdenum therein to form a molybdenum disulfide barrier layer between the adhesion layer and the seed crystal layer;

[0020] Step 5: Continue to fill the conductor layer in the groove or hole and planarize it.

[0021] Furthermore, in step three, copper and molybdenum are solid-phase sintered in a certain proportion to form a target material, and the copper-molybdenum alloy layer is deposited on the adhesion layer by a PVD process to form a seed layer.

[0022] Furthermore, in step four, sulfur is infiltrated into the copper-molybdenum alloy layer through a low-temperature ion sulfurization process, and a reducing atmosphere is used for protection. After a certain insulation time, a molybdenum disulfide barrier layer with uniform coverage and a three-dimensional structure is formed between the adhesion layer and the seed crystal layer.

[0023] Furthermore, the sulfurization temperature when sulfur is infiltrated into the copper-molybdenum alloy layer is 200°C to 300°C.

[0024] It can be seen from the above technical solution that the present invention replaces the traditional TaN as a metal diffusion barrier layer with a three-dimensional molybdenum disulfide (MoS2) layer. On the one hand, it can greatly reduce the thickness of the barrier layer and increase the proportion of wire metal. On the other hand, the three-dimensional molybdenum disulfide layer as a barrier layer has good conductivity, which can greatly reduce the metal interconnection resistance overall. At the same time, wrapping the three-dimensional molybdenum disulfide layer at the interface of the interconnected metal copper can improve the anti-electromigration ability of the copper wire. Moreover, from the perspective of process integration, the total process steps have not increased, and the problems of groove coverage and process compatibility existing in the introduction of two-dimensional materials in the back-end process have been effectively overcome. BRIEF DESCRIPTION OF THE DRAWINGS

[0025] Figure 1-Figure 7 It is a schematic diagram of the process steps of manufacturing a metal diffusion barrier layer structure according to a method for forming a metal diffusion barrier layer structure of the present invention in a preferred embodiment of the present invention.

[0026] In the figure, 101. back-end interconnect dielectric layer, 102. interlayer separation layer, 103. interconnect metal, 104. metal cap layer, 201. interconnect wire slot, 202. dielectric layer, 203. adhesion layer, 204. seed layer, 205. molybdenum disulfide barrier layer, 206. interconnect wire layer. DETAILED DESCRIPTION

[0027] The specific implementation modes of the present invention will be further described in detail below in conjunction with the accompanying drawings.

[0028] It should be noted that in the following specific embodiments, when describing the embodiments of the present invention in detail, in order to clearly represent the structure of the present invention for the convenience of explanation, the structures in the accompanying drawings are not drawn according to general proportions, and are partially enlarged, deformed and simplified. Therefore, it should be avoided to understand this as a limitation of the present invention.

[0029] In the following specific embodiments of the present invention, please refer to Figure 7 , Figure 7 In a preferred embodiment of the present invention, a metal diffusion barrier layer structure is manufactured according to a method for forming a metal diffusion barrier layer structure according to the present invention. Figure 7 As shown, a metal diffusion barrier layer structure of the present invention includes an adhesion layer 203, a molybdenum disulfide barrier layer 205 and a seed layer 204 sequentially covering the inner wall surface of the interconnection line slot 201 from the outside to the inside.

[0030] Furthermore, the interconnection groove 201 within the seed layer 204 is also filled with a conductor layer 206 .

[0031] As an optional implementation, the interconnection wire slot 201 may also be replaced by a through hole. The interconnection wire slot 201 is taken as an example for description, but is not limited thereto.

[0032] As an optional implementation, the adhesion layer 203 may include a tantalum (Ta) film 203; and the wire layer 206 may include a copper wire layer 206. But the invention is not limited thereto.

[0033] As a preferred embodiment, the seed layer 204 may include a copper-molybdenum alloy layer. The molybdenum disulfide barrier layer 205 may be formed by infiltrating sulfur into the copper-molybdenum alloy layer 204 and reacting the sulfur with the molybdenum in the copper-molybdenum alloy layer 204 .

[0034] Furthermore, the molybdenum disulfide barrier layer 205 may have a three-dimensional structure. For example, the molybdenum disulfide barrier layer 205 may be a coral-like stacked multilayer film structure uniformly covering the tantalum film 203 and the copper-molybdenum alloy layer 204 .

[0035] The above-mentioned metal diffusion barrier layer structure of the present invention can be established on a semiconductor substrate chip. The chip structure involved may include: a back-end interconnect dielectric layer 101, a layer separation layer 102, an interconnect metal 103, and a metal cap layer 104 arranged on a semiconductor silicon substrate, all of which are manufactured using a standard CMOS back-end interconnect process and have all the characteristics of the CMOS back-end interconnect process of the technology node. In addition, a circuit module with a specific function can be formed through a subsequent interconnect process.

[0036] Please refer to Figure 7 A dielectric layer 202 is provided on the interlayer separation layer 102 of the chip structure; and an interconnection line groove 201 is formed on the dielectric layer 202 .

[0037] The dielectric layer 202 may involve dielectric layers such as isolation, passivation and etch stop layers, including but not limited to at least one of a low-K (dielectric constant) material layer, a silicon dioxide layer, a silicon nitride layer, a silicon carbide layer, an aluminum oxide layer and an aluminum nitride layer. That is, the dielectric layer 202 material of the present invention includes but is not limited to at least one of a low-K value material, silicon dioxide, silicon nitride, silicon carbide, aluminum oxide and aluminum nitride. The dielectric layer 202 film thickness may be 5nm to 500nm.

[0038] In the above-mentioned metal diffusion barrier layer structure of the present invention, the total thickness of the Ta adhesion layer 203, the three-dimensional molybdenum disulfide barrier layer 205 and the copper-molybdenum alloy seed layer 204 is not more than 5nm. In addition, the metal materials involved include but are not limited to tantalum (Ta), copper (Cu), etc., and may also include compounds containing all or part of the above elements formed for specific properties.

[0039] Taking tantalum film as adhesion layer 203 and copper-molybdenum alloy film as seed layer 204 as an example, the thickness of tantalum film 203 can be within 1 nm, and the sum of the thickness of three-dimensional molybdenum disulfide barrier layer 205 and copper-molybdenum alloy seed layer 204 does not exceed 4 nm.

[0040] The following is a specific implementation method and combined with the attached Figure 1-Figure 7 , a method for forming a metal diffusion barrier layer structure of the present invention is described in detail.

[0041] Please refer to Figure 1-Figure 7 , Figure 1-Figure 7 This is a schematic diagram of the process steps for making a metal diffusion barrier layer structure according to a method for forming a metal diffusion barrier layer structure according to a preferred embodiment of the present invention. Figure 1-Figure 7 As shown, a method for forming a metal diffusion barrier structure of the present invention can be used to manufacture the above Figure 7 A metal diffusion barrier layer structure as shown in FIG. 1 may include the following steps:

[0042] Step 1: providing a substrate, forming a dielectric layer 202 on the substrate, and forming an interconnection line groove 201 on the dielectric layer 202 .

[0043] Please refer to Figure 1 A semiconductor back-end interconnect substrate may be used, and a dielectric layer 202 may be further deposited on the interlayer separation layer 102 of the substrate. The chip structure involved may include a back-end interconnect dielectric layer 101, an interlayer separation layer 102, an interconnect metal 103, a metal cap layer 104, etc., which may all be manufactured using a standard CMOS back-end interconnect process and have all the features of the CMOS back-end interconnect process of the technology node. Through subsequent interconnect processes, a circuit module with specific functions may be formed.

[0044] Please refer to Figure 2 Then, a standard back-end interconnection photolithography and etching process is performed to form an interconnection line groove 201 on the dielectric layer 202 .

[0045] Step 2: forming an adhesive layer 203 on the inner wall surface of the interconnection wire slot 201 .

[0046] Please refer to Figure 3 In the interconnection line groove 202, a metal tantalum film 203 may be deposited on the dielectric layer 202 and the inner wall surface of the interconnection line groove 201 by using a process such as PVD or ALD, and the thickness may be about 1 nm.

[0047] Step three: forming a copper-molybdenum alloy layer 204 as a seed layer on the adhesion layer 203 .

[0048] Please refer to Figure 4 Next, a Cu / Mo seed layer 204 thin film may be deposited on the Ta adhesion layer 203 by using a PVD process. The PVD target used is formed by solid-phase sintering of a certain proportion of Cu and Mo metals, wherein the atomic percentage of Mo metal may be in the range of 10% to 50%.

[0049] Step 4: Sulfur is infiltrated into the copper-molybdenum alloy layer 204 and reacts with the molybdenum therein to form a molybdenum disulfide barrier layer 205 between the adhesion layer 203 and the seed layer 204 .

[0050] Please refer to Figure 5 Then, a low temperature ion sulfurization process may be used to form a three-dimensional MoS 2 barrier layer 205 between the Ta adhesion layer 203 and the Cu / Mo seed layer 204 .

[0051] The gaseous sulfur source used in this step can be solid sulfur vapor, carbon disulfide vapor or hydrogen sulfide gas and other sulfur sources. The process temperature can be 200°C to 300°C, and the commonly used reducing gas combination Ar-H2 can be used as the sulfurizing atmosphere. The cathode glow discharge voltage can be 100V to 500V, and the sulfurizing holding time can be 1min to 30min.

[0052] During the above-mentioned sulfurization process, a reducing atmosphere is used to protect and control the rate of the sulfurization reaction, so that the sulfur oxidation reaction of the exposed portion of the Cu / Mo seed crystal layer 204 facing the inner side of the interconnection line groove 201 is suppressed, making it easier to form a three-dimensional MoS2 barrier layer 205 between the Ta adhesion layer 203 and the Cu / Mo seed crystal layer 204.

[0053] As a result of the low temperature ion sulfurization, sulfur ions diffuse into the Cu / Mo seed crystal layer 204 and react with the Mo metal therein, thereby forming a uniformly covered three-dimensional MoS2 barrier layer between the Ta adhesion layer 203 and the Cu / Mo seed crystal layer 204.

[0054] Step 5: Continue to fill the interconnection wire layer 206 in the interconnection wire groove 201 and planarize it.

[0055] Please refer to Figure 6 The interconnection wire layer 206 may be deposited and filled in the interconnection wire groove 201 by electroplating or chemical plating process.

[0056] Please refer to Figure 7 Finally, a chemical planarization process may be used to remove excess copper, copper-molybdenum alloy, molybdenum disulfide, tantalum and other metals outside the interconnection line slot 201 to form the metal diffusion barrier layer structure of the present invention.

[0057] In summary, the present invention replaces the traditional TaN as a metal diffusion barrier layer with a three-dimensional molybdenum disulfide (MoS2) layer. On the one hand, the thickness of the barrier layer can be greatly reduced and the proportion of wire metal can be increased. On the other hand, the three-dimensional molybdenum disulfide layer as a barrier layer has good conductivity, which can greatly reduce the metal interconnection resistance overall. At the same time, wrapping the three-dimensional molybdenum disulfide layer at the interface of the interconnected metal copper can improve the anti-electromigration ability of the copper wire. Moreover, from the perspective of process integration, the total process steps have not increased, and the problems of groove coverage and process compatibility existing in the introduction of two-dimensional materials in the back-end process have been effectively overcome.

[0058] The above are only preferred embodiments of the present invention, and the embodiments are not intended to limit the protection scope of the present invention. Therefore, all equivalent structural changes made using the description and drawings of the present invention should be included in the protection scope of the present invention.

Claims

1. A metal diffusion barrier layer structure, characterized in that: It includes an adhesion layer, a molybdenum disulfide barrier layer, a seed layer and a conductor layer which are sequentially formed in a groove or a hole from the outside to the inside; the seed layer includes a copper-molybdenum alloy layer; the molybdenum disulfide barrier layer is formed by infiltrating sulfur into the copper-molybdenum alloy layer and reacting with molybdenum therein; the molybdenum disulfide barrier layer has a three-dimensional structure.

2. The metal diffusion barrier layer structure according to claim 1, characterized in that: The molybdenum disulfide barrier layer is a coral-like stacked multilayer film structure.

3. The metal diffusion barrier layer structure according to claim 1, characterized in that: The slots include interconnection slots, and the holes include through holes.

4. A method for forming a metal diffusion barrier structure, characterized in that: The following steps are involved: Step 1: providing a substrate, forming a dielectric layer on the substrate, and forming grooves or holes on the dielectric layer; Step 2: forming an adhesive layer on the inner wall surface of the groove or hole; Step 3: solid-phase sintering copper and molybdenum in a certain ratio to form a target material, and depositing a copper-molybdenum alloy layer as a seed layer on the adhesion layer through a PVD process; Step 4: sulfur is infiltrated into the copper-molybdenum alloy layer through a low-temperature ion sulfurization process, and a reducing atmosphere is used for protection. After a certain insulation time, a molybdenum disulfide barrier layer with uniform coverage and a three-dimensional structure is formed between the adhesion layer and the seed crystal layer; Step 5: Continue to fill the conductor layer in the groove or hole and planarize it.

5. The method for forming a metal diffusion barrier structure according to claim 4, characterized in that: The sulfurization temperature when sulfur is infiltrated into the copper-molybdenum alloy layer is 200°C to 300°C.