Parallel formation device, parallel formation equipment and lithium ion battery

By using the combined technology of multi-layered clamping mechanisms and pressure-adjusting telescopic parts during the battery formation process, the time-consuming and labor-intensive problem of battery formation is solved, the battery is quickly fixed and the gas is discharged, and the formation efficiency and qualification rate are improved. The stability and consistency of the battery are ensured.

CN112490512BActive Publication Date: 2024-10-22HUIZHOU HENGTAI TECH
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202011476915.1
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2020-12-15
Publication Date
2024-10-22
Estimated Expiration
2040-12-15

AI Technical Summary

Technical Problem

The battery formation process needs to be clamped one by one, which is time-consuming and labor-intensive, increases labor costs and reduces the formation efficiency. It is also easy for the air inside the battery to bulge and affect the stability of the solid electrolyte interface membrane, resulting in a low qualification rate.

Method used

At least two stacked clamping mechanisms are used to clamp the battery, and the pressure-adjusting telescopic member is used to quickly fix the battery and discharge gas, combined with a horizontal straightener to ensure uniform formation pressure.

Benefits of technology

It improves the efficiency and qualification rate of battery formation, reduces the formation time, enhances the stability of the solid electrolyte interface film, and ensures the production efficiency and consistency of the battery.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN112490512B_ABST
    Figure CN112490512B_ABST
Patent Text Reader

Abstract

The present application provides a parallel formation device, parallel formation equipment and lithium-ion battery. The above-mentioned parallel formation device includes at least two clamping mechanisms arranged in a stacked manner, and the two clamping mechanisms are used together to clamp the battery. When the transmission group drives the sliding block to slide along a first direction relative to the mounting plate, the two adjacent mounting plates approach each other, and the pressure regulating telescopic member contracts; when the transmission group drives the sliding block to slide along a second direction relative to the mounting plate, the two adjacent mounting plates move away from each other, and the pressure regulating telescopic member extends. The above-mentioned parallel formation device improves the production efficiency of the battery and the qualified rate of the battery formation.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the technical field of batteries, and in particular to a parallel formation device, parallel formation equipment and a lithium ion battery. Background Art

[0002] Battery formation is an essential step in the battery preparation process and is also a key step affecting the performance of various batteries. Battery formation refers to a small current charge and discharge process of the prepared battery to generate a stable solid electrolyte interface film inside the battery.

[0003] During the battery formation, the batteries need to be clamped one by one to ensure that the positive and negative electrodes of the batteries are stably connected to the positive and negative terminals. The formation operation of such batteries is not only time-consuming and labor-intensive, but also increases the labor cost required for the formation operation, while reducing the battery formation efficiency. In addition, during the formation process, the battery is prone to bulging shells due to gas swells, which has a great influence on the stability of the interface film of the solid electrolyte formed by the formation, thereby resulting in a low battery qualification rate. Summary of the invention

[0004] The purpose of the present invention is to overcome the shortcomings of the prior art and provide a parallel formation device, parallel formation equipment and lithium ion battery which can improve the production efficiency of batteries, reduce the formation time and improve the qualified rate of battery formation.

[0005] The objective of the present invention is achieved through the following technical solutions:

[0006] A parallel formation device comprises at least two stacked clamping mechanisms, the two clamping mechanisms are used together to clamp a battery, and each of the clamping mechanisms comprises:

[0007] A mounting plate, wherein the mounting plates of two adjacent clamping mechanisms are stacked, wherein a mounting cavity, a conducting groove and a sliding groove are provided in the mounting plate, wherein the mounting cavity is communicated with the conducting groove, and wherein a plurality of telescopic grooves are provided in the mounting plate, wherein the extension direction of each telescopic groove is the same as the extension direction of the conducting groove, and the opening direction of each telescopic groove is the same as the opening direction of the conducting groove;

[0008] 14. The electrical connector of claim 13, wherein the first and second clamping members are configured to engage a first electrode and a second electrode, wherein the first electrode and the second clamping member are configured to engage a first electrode and a second electrode, and wherein the first electrode and the second electrode ...

[0009] A pressure regulating component, the pressure regulating component includes a pressure regulating telescopic member and a lifting regulating member, the pressure regulating telescopic member is located in the mounting cavity and is elastically connected to the mounting plate, the pressure regulating telescopic member partially protrudes from the periphery of the mounting plate through the conducting groove, the pressure regulating telescopic member is also slidably connected to the mounting plate, the sliding direction of the pressure regulating telescopic member is the same as the extension direction of the conducting groove, the pressure regulating telescopic member includes an elastic member and a pressure block, the elastic member is arranged in the mounting cavity, the pressure block is located in the mounting cavity, and the pressure block partially protrudes from the conducting groove , one end of the elastic member is connected to the pressure block, the other end of the elastic member is connected to the inner wall of the mounting cavity, and the pressure block is slidably connected to the mounting plate; the lifting and lowering adjustment member includes a sliding block and a transmission group, the sliding block is arranged at the sliding groove and is slidably connected to the mounting plate, and the sliding block is connected to another stacked mounting plate, the transmission group is installed on the mounting plate, and the power output end of the transmission group is connected to the sliding block, the transmission group drives the sliding block to slide relative to the mounting plate, and the sliding direction of the sliding block is the same as the extension direction of the conducting groove;

[0010] Among them, when the transmission group drives the sliding block to slide along the first direction relative to the mounting plate, the two adjacent mounting plates approach each other and the pressure regulating telescopic part contracts; when the transmission group drives the sliding block to slide along the second direction relative to the mounting plate, the two adjacent mounting plates move away from each other and the pressure regulating telescopic part extends.

[0011] In one embodiment, the transmission group includes a motor, a first pulley, a second pulley, a transmission belt and a screw pair. The motor is mounted on the mounting plate, the first pulley is sleeved on the power output end of the motor, the second pulley is sleeved on the screw pair, the transmission belt is passed through the mounting plate and respectively sleeved on the first pulley and the second pulley, and the screw pair is rotatably connected to the sliding block.

[0012] In one embodiment, the pressure block includes a clamping portion and an abutting portion, the clamping portion is clamped in the mounting cavity and is slidably connected to the mounting plate, the clamping portion is connected to the abutting portion, the abutting portion is located in the conducting groove, and the abutting portion partially protrudes from the conducting groove, and the abutting portion is arranged corresponding to the second clamping member of each clamping assembly.

[0013] In one embodiment, the clamping portion and the abutting portion are an integrally formed structure.

[0014] In one embodiment, the number of the conducting grooves and the abutment portions are both plural, the abutment portions are arranged one-to-one in the conducting grooves, the abutment portions are all connected to the clamping portions, and the abutment portions are arranged one-to-one with the second clamping members of the clamping assemblies.

[0015] In one of the embodiments, the first clamping member of each clamping assembly further includes an insulator, and the insulator of the first clamping member of each clamping assembly is clamped between the corresponding positive electrode column and the corresponding negative electrode column.

[0016] A parallel formation device comprises a horizontal corrector, a shell and the parallel formation device described in any of the above embodiments, at least two stacked clamping mechanisms and the horizontal corrector are arranged in the shell, the horizontal corrector is connected to the mounting plate of any of the clamping mechanisms, and the horizontal corrector is used to adjust the horizontality of the mounting plate.

[0017] A lithium ion battery is formed by using the parallel formation equipment described in any of the above embodiments.

[0018] Compared with the prior art, the present invention has at least the following advantages:

[0019] 1. In the parallel formation device of the present invention, at least two stacked clamping mechanisms are used to clamp the battery, which avoids the need to use a clamp to fix the batteries one by one during battery formation, which is time-consuming and labor-intensive, resulting in increased labor costs and reduced formation efficiency. Specifically, the battery is placed near the first clamping member of the clamping mechanism, and the positive and negative pole ears are abutted against the first clamping member, and then the second clamping member of another clamping mechanism is connected to the first clamping member accordingly, and the pressure regulating telescopic member is abutted against the battery. On the one hand, the pressure regulating telescopic member plays a role in fixing the battery, and is used in conjunction with the first clamping member and the second clamping member to improve the battery. The production efficiency of the battery is improved and the battery formation time is reduced; on the other hand, the pressure regulating telescopic member plays a role in squeezing the battery and assisting in discharging the gas in the battery. When the transmission group drives the sliding block to slide relative to the mounting plate along the first direction, the two adjacent mounting plates are close to each other, and the pressure regulating telescopic member is contracted, so that the pressure on the battery is increased; when the transmission group drives the sliding block to slide relative to the mounting plate along the second direction, the two adjacent mounting plates are away from each other, and the pressure regulating telescopic member is extended, so that the pressure on the battery is reduced, thereby realizing the pressure regulation during the battery formation, reducing the degree of gas bulging in the battery shell during the formation process, and thus improving the qualified rate of the battery formation;

[0020] 2. In the parallel formation equipment of the present invention, at least two stacked clamping mechanisms in the parallel formation device are used to realize the rapid fixation of the battery and the adjustment of the battery formation pressure, and a horizontal corrector is added to make each parallel formation device in a horizontal state, avoiding the parallel formation device from tilting, resulting in uneven formation pressure of each battery, and causing the parallel formation device to adjust the formation pressure of each battery inaccurately, thereby reducing the consistency of the battery after formation, and even causing poor contact between the positive and negative ears of the battery and leakage of electrolyte during the battery formation process, thereby reducing the problem of battery formation qualification rate, improving the consistency of the battery after formation and improving the battery formation qualification rate. BRIEF DESCRIPTION OF THE DRAWINGS

[0021] In order to more clearly illustrate the technical solutions of the embodiments of the present invention, the drawings required for use in the embodiments are briefly introduced below. It should be understood that the following drawings only show certain embodiments of the present invention and therefore should not be regarded as limiting the scope. For ordinary technicians in this field, other related drawings can be obtained based on these drawings without creative work.

[0022] Figure 1 It is a schematic structural diagram of a parallel formation device according to one embodiment of the present invention;

[0023] Figure 2 for Figure 1 A partial enlarged view of the parallel formation device shown;

[0024] Figure 3 for Figure 1 Another structural schematic diagram of the parallel formation device shown;

[0025] Figure 4 for Figure 3 A partial enlarged view of the parallel formation device shown;

[0026] Figure 5 for Figure 1 A cross-sectional view of the parallel formation device shown;

[0027] Figure 6 for Figure 4 A partial enlarged view of the parallel formation device shown;

[0028] Figure 7 It is a structural schematic diagram of a parallel formation device according to one embodiment of the present invention;

[0029] Figure 8 The figure is a formation flow chart of the lithium ion battery of the present invention. DETAILED DESCRIPTION

[0030] In order to facilitate the understanding of the present invention, the present invention will be described more fully below with reference to the relevant drawings. The preferred embodiments of the present invention are given in the drawings. However, the present invention can be implemented in many different forms and is not limited to the embodiments described herein. On the contrary, the purpose of providing these embodiments is to make the disclosure of the present invention more thoroughly understood.

[0031] It should be noted that when an element is referred to as being "fixed to" another element, it may be directly on the other element or there may be a central element. When an element is considered to be "connected to" another element, it may be directly connected to the other element or there may be a central element at the same time. The terms "vertical", "horizontal", "left", "right" and similar expressions used herein are for illustrative purposes only and do not represent the only implementation method.

[0032] Unless otherwise defined, all technical and scientific terms used herein have the same meaning as those commonly understood by those skilled in the art of the present invention. The terms used herein in the specification of the present invention are only for the purpose of describing specific embodiments and are not intended to limit the present invention. The term "and / or" used herein includes any and all combinations of one or more related listed items.

[0033] The present application provides a parallel formation device. The above-mentioned parallel formation device includes at least two clamping mechanisms arranged in a stacked manner, and the two clamping mechanisms are used together to clamp the battery. Each clamping mechanism includes a mounting plate, a plurality of clamping assemblies and a pressure regulating assembly. The mounting plates of two adjacent clamping mechanisms are stacked, and a mounting cavity, a conducting groove and a sliding groove are provided in the mounting plate, and the mounting cavity is connected to the conducting groove. Each clamping assembly includes a first clamping member and a second clamping member, and the first clamping member and the second clamping member are relatively arranged on both sides of the mounting plate, and each first clamping member includes a positive pole and a negative pole, and the positive pole and the negative pole are both installed on the mounting plate, and the second clamping member is slidably connected to the mounting plate, and the sliding direction of the second clamping member is the same as the extension direction of the conducting groove, and the opening direction of the conducting groove is toward the side of the mounting plate where the second clamping member is arranged. The pressure regulating assembly includes a pressure regulating telescopic member and a lifting regulating member. The pressure regulating telescopic member is located in the mounting cavity and is elastically connected to the mounting plate. The pressure regulating telescopic member partially protrudes from the periphery of the mounting plate through the conducting groove. The pressure regulating telescopic member is also slidably connected to the mounting plate. The sliding direction of the pressure regulating telescopic member is the same as the extension direction of the conducting groove. The lifting regulating member includes a sliding block and a transmission group. The sliding block is arranged at the sliding groove and is slidably connected to the mounting plate, and the sliding block is connected to another stacked mounting plate. The transmission group is installed on the mounting plate, and the power output end of the transmission group is connected to the sliding block. The transmission group drives the sliding block to slide relative to the mounting plate, and the sliding direction of the sliding block is the same as the extension direction of the conducting groove. When the transmission group drives the sliding block to slide relative to the mounting plate in a first direction, two adjacent mounting plates approach each other, and the pressure regulating telescopic member contracts; when the transmission group drives the sliding block to slide relative to the mounting plate in a second direction, two adjacent mounting plates move away from each other, and the pressure regulating telescopic member extends.

[0034] In the above-mentioned parallel formation device, at least two stacked clamping mechanisms are used to clamp the battery, which avoids the need to use a clamp to fix the batteries one by one during battery formation, which is time-consuming and labor-intensive, resulting in increased labor costs and reduced formation efficiency. Specifically, a plurality of clamping assemblies are provided in the parallel formation device, wherein the battery is placed at a first clamping member close to the clamping mechanism, and the positive and negative pole ears are abutted against the first clamping member, and then the second clamping member of another clamping mechanism is correspondingly connected to the first clamping member, that is, the effect of clamping multiple batteries at one time is achieved, the time for fixing the battery during formation is reduced, and the battery formation efficiency is improved, and the pressure regulating telescopic member is abutted against the battery. On the one hand, the pressure regulating telescopic member plays a role in fixing the battery, When used in conjunction with the first clamping member and the second clamping member, the fixing reliability of the battery is improved, the rapid fixing of the battery is achieved, the production efficiency of the battery is improved, and the battery formation time is reduced; on the other hand, the pressure regulating telescopic member plays a role in squeezing the battery and assisting in discharging the gas in the battery. When the transmission group drives the sliding block to slide along the first direction relative to the mounting plate, the two adjacent mounting plates approach each other, and the pressure regulating telescopic member contracts, so that the pressure on the battery increases; when the transmission group drives the sliding block to slide along the second direction relative to the mounting plate, the two adjacent mounting plates move away from each other, and the pressure regulating telescopic member extends, so that the pressure on the battery is reduced, thereby achieving pressure regulation during battery formation, reducing the degree of gas bulging in the battery shell during the formation process, and thus improving the qualified rate of battery formation.

[0035] In order to better understand the parallel formation device 10 of the present invention, the parallel formation device 10 of the present invention is further explained below.

[0036] Please also read Figure 1 , Figure 4 and Figure 5The parallel formation device 10 of one embodiment includes at least two stacked clamping mechanisms 10a, and the two clamping mechanisms 10a are used to clamp the battery. Each clamping mechanism 10a includes a mounting plate 100, a plurality of clamping components 200, and a pressure regulating component 300. The mounting plates 100 of two adjacent clamping mechanisms 10a are stacked, and a mounting cavity 110, a conducting groove 120, and a sliding groove 130 are provided in the mounting plate 100, and the mounting cavity 110 is connected to the conducting groove 120. Each clamping assembly 200 includes a first clamping member 210 and a second clamping member 220, and the first clamping member 210 and the second clamping member 220 are relatively arranged on both sides of the mounting plate 100, and each first clamping member 210 includes a positive pole column 211 and a negative pole column 212, and the positive pole column 211 and the negative pole column 212 are both installed on the mounting plate 100, and the second clamping member 220 is slidably connected to the mounting plate 100, and the sliding direction of the second clamping member 220 is the same as the extension direction of the conductive groove 120, and the opening direction of the conductive groove 120 is toward the side of the mounting plate 100 where the second clamping member 220 is set. The pressure regulating assembly 300 includes a pressure regulating telescopic member 310 and a lifting and lowering regulating member 320. The pressure regulating telescopic member 310 is located in the mounting cavity 110 and is elastically connected to the mounting plate 100. The pressure regulating telescopic member 310 partially protrudes from the periphery of the mounting plate 100 through the conducting groove 120. The pressure regulating telescopic member 310 is also slidably connected to the mounting plate 100, and the sliding direction of the pressure regulating telescopic member 310 is the same as the extension direction of the conducting groove 120; the lifting and lowering regulating member 320 includes a sliding block 321 and a transmission group 322. The sliding block 321 is arranged at the sliding groove 130 and is slidably connected to the mounting plate 100, and the sliding block 321 is connected to another stacked mounting plate 100. The transmission group 322 is installed on the mounting plate 100, and the power output end of the transmission group 322 is connected to the sliding block 321. The transmission group 322 drives the sliding block 321 to slide relative to the mounting plate 100, and the sliding direction of the sliding block 321 is the same as the extension direction of the conducting groove 120. Among them, when the transmission group 322 drives the sliding block 321 to slide along the first direction relative to the mounting plate 100, that is, when the transmission group 322 drives the sliding block 321 to slide along the A direction relative to the mounting plate 100, the two adjacent mounting plates 100 approach each other, and the pressure regulating telescopic member 310 contracts; when the transmission group 322 drives the sliding block 321 to slide along the second direction relative to the mounting plate 100, that is, when the transmission group 322 drives the sliding block 321 to slide along the B direction relative to the mounting plate 100, the two adjacent mounting plates 100 move away from each other, and the pressure regulating telescopic member 310 extends.

[0037] In the above-mentioned parallel formation device 10, at least two stacked clamping mechanisms 10a are used to clamp the battery, which avoids the need to use a clamp to fix the batteries one by one during battery formation, which is time-consuming and labor-intensive, resulting in increased labor costs and reduced formation efficiency. Specifically, the battery is placed at a first clamping member 210 close to the clamping mechanism 10a, and the positive and negative pole ears are abutted against the first clamping member 210, and then the second clamping member 220 of another clamping mechanism 10a is correspondingly connected to the first clamping member 210, and the pressure regulating telescopic member 310 is abutted against the battery. On the one hand, the pressure regulating telescopic member 310 plays a role in fixing the battery, and is used in conjunction with the first clamping member 210 and the second clamping member 220 to improve the battery. On the other hand, the pressure regulating telescopic member 310 plays a role in squeezing the battery and assisting in discharging the gas in the battery. When the transmission group 322 drives the sliding block 321 to slide along a first direction relative to the mounting plate 100, two adjacent mounting plates 100 approach each other, and the pressure regulating telescopic member 310 contracts, so that the pressure on the battery increases; when the transmission group 322 drives the sliding block 321 to slide along a second direction relative to the mounting plate 100, two adjacent mounting plates 100 move away from each other, and the pressure regulating telescopic member 310 extends, so that the pressure on the battery is reduced, thereby realizing the pressure regulation during the battery formation, reducing the degree of gas bulging of the battery shell during the formation process, and thus improving the qualified rate of the battery formation.

[0038] It should be noted that the second clamping member 220 and the pressure regulating telescopic member 310 are arranged on the same side of the mounting plate 100. Specifically, the opening direction of the conducting groove 120 is toward the second clamping member 220, and the sliding direction of the second clamping member 220 is the same as the extension direction of the conducting groove 120, and the sliding direction of the pressure regulating telescopic member 310 is the same as the extension direction of the conducting groove 120, that is, the sliding direction of the second clamping member 220 and the pressure regulating telescopic member 310 is the same, that is, when the pressure regulating telescopic member 310 shrinks and slides toward the mounting cavity 110, the second clamping member 220 slides toward the mounting plate 100; when the transmission group 322 drives the sliding block 321 to slide along the first direction A relative to the mounting plate 100, the two adjacent mounting plates 100 approach each other, and the pressure regulating telescopic member 310 shrinks, thereby realizing the abutment between the pressure regulating telescopic member 310 and the battery, and realizing the regulation of the battery formation pressure during the extension and contraction of the pressure regulating telescopic member 310. It can also be understood that if the first clamping member 210 is slidably connected to the mounting plate 100 and the sliding direction is the same as the extending direction of the conducting groove 120, and the second clamping member 220 is fixedly connected to the mounting plate 100, when the positive and negative ears of the battery are abutted against the first clamping member 210, the protruding length of the first clamping member 210 is larger, and then the second clamping member 220 is connected to the first clamping member 210, and in the process of adjusting the battery formation pressure, the first clamping member 210 will be relatively loose relative to the mounting plate 100. During the sliding process, the first clamping member 210 and the second clamping member 220 clamp the positive and negative poles of the battery and stretch or squeeze the positive and negative poles of the battery, causing damage to the positive and negative poles of the battery and destroying the structure of the battery. Therefore, in the parallel formation device of the present application, the first clamping member 210 is fixedly connected to the mounting plate 100 to ensure that the positive and negative poles of the battery are not damaged during the formation process, thereby improving the qualified rate of the battery formation.

[0039] It should also be noted that the first clamping member 210 includes a positive electrode column 211 and a negative electrode column 212, the positive electrode column 211 is connected to the positive electrode ear of the battery, the negative electrode column 212 is connected to the negative electrode ear of the battery, and each first clamping member 210 is connected in parallel with the power supply, thereby realizing the parallel connection of each battery, improving the current consistency of the battery formation, and thus improving the consistency of the battery formation.

[0040] It can be understood that the sliding block 321 is a connection structure between the mounting plate 100 containing the sliding block 321 and another stacked mounting plate 100, and the first direction is that the stacked mounting plate 100 vertically points to the mounting plate 100 containing the sliding block 321; the second direction is that the mounting plate 100 containing the sliding block 321 vertically points to the stacked mounting plate 100, thereby ensuring the adjustment of the distance between the mounting plates 100 and further ensuring the pressure adjustment on the battery surface.

[0041] It can also be understood that the sliding block 321 is the contact part of two stacked clamping mechanisms 10a. When the sliding block 321 of one of the clamping mechanisms 10a is adjusted to slide along the first direction, two adjacent mounting plates 100 are close to each other, and the pressure regulating telescopic member 310 is contracted, so that the elastic deformation of the pressure regulating telescopic member 310 becomes larger, thereby increasing the formation pressure of the battery, and realizing the regulation of the battery formation pressure; when the transmission group 322 drives the sliding block 321 to slide along the second direction relative to the mounting plate 100, the two adjacent mounting plates 100 are away from each other, and the pressure regulating telescopic member 310 is extended, so that the elastic deformation of the pressure regulating telescopic member 310 becomes smaller, thereby reducing the formation pressure of the battery. It can also be understood that the transmission group 322 is installed on the mounting plate 100 and is connected to the sliding block 321 in transmission, realizing the controllability of the sliding adjustment of the sliding block 321, thereby improving the controllability of the formation pressure in the battery formation process.

[0042] Please also read Figure 1 , Figure 2 and Figure 6 In one embodiment, the sliding block 321 is an "L"-shaped or "T"-shaped sliding block, which improves the connection reliability between the sliding block 321 and another stacked mounting plate 100, that is, improves the connection stability between the mounting plate 100 containing the sliding block 321 and another stacked mounting plate 100.

[0043] Please also read Figure 1 , Figure 3 and Figure 5 In one embodiment, the number of lifting and adjusting members 320 is two, and the two lifting and adjusting members 320 are respectively arranged at the two ends of the mounting plate 100, thereby ensuring the controllability of the distance between the mounting plates 100 and 100, thereby improving the controllability of the formation pressure during the battery formation process. It can also be understood that in other embodiments, the number of lifting and adjusting members 320 is multiple, and the multiple lifting and adjusting members 320 are evenly distributed on the mounting plate 100, thereby better ensuring the controllability of the distance between the mounting plates 100 and 100, thereby improving the controllability of the formation pressure during the battery formation process.

[0044] Please also read Figure 2 , Figure 5 and Figure 6In one embodiment, the transmission group 322 includes a motor 3221, a first pulley 3224, a second pulley 3225, a transmission belt 3222 and a screw pair 3223. The motor 3221 is installed on the mounting plate 100, the first pulley 3224 is sleeved on the power output end of the motor 3221, the second pulley 3225 is sleeved on the screw pair 3223, the transmission belt 3222 is passed through the mounting plate 100 and is respectively sleeved on the first pulley 3224 and the second pulley 3225, and the screw pair 3223 is rotatably connected to the sliding block 321. It can be understood that the transmission belt 3222 is respectively mounted on the first pulley 3224 and the second pulley 3225, so that the motor 3221 indirectly drives the screw pair 3223 to rotate, and the screw pair 3223 is connected to the sliding block 321. In the process of the motor 3221 driving the screw pair 3223 to rotate, the screw pair 3223 also drives the sliding block 321 to slide relative to the mounting plate 100. Through the precise control of the motor 3221 and the screw pair 3223, the sliding controllability of the sliding block 321 is improved, thereby improving the controllability of the formation pressure during the battery formation process.

[0045] Please also read Figure 5 and Figure 6 In one embodiment, the pressure regulating telescopic member 310 includes an elastic member 311 and a pressing block 312, the elastic member 311 is arranged in the mounting cavity 110, the pressing block 312 is located in the mounting cavity 110, and the pressing block 312 partially protrudes from the conducting groove 120, one end of the elastic member 311 is connected to the pressing block 312, the other end of the elastic member 311 is connected to the inner wall of the mounting cavity 110, and the pressing block 312 is slidably connected to the mounting plate 100. It can be understood that the elastic member 311 realizes the telescopic performance of the pressure regulating telescopic member 310, and in the process of the elastic member 311 being extended and retracted, the change of elastic deformation causes the pressure of the pressing block 312 in contact with the battery to change, thereby realizing the controllability of the formation pressure during the battery formation process, and the contact area between the pressing block 312 and the battery is large, ensuring that the pressure received at various places during the battery formation process is consistent, avoiding the problem of uneven pressure received during the battery formation process, resulting in local bulging of the battery shell, and improving the consistency and qualified rate of the battery formation.

[0046] In one embodiment, the elastic member is welded to the inner wall of the pressing block and the mounting plate respectively, thereby improving the connection stability between the elastic member and the pressing block, and between the elastic member and the mounting plate.

[0047] In one embodiment, the elastic member abuts against the inner wall of the pressing block and the mounting plate respectively, thereby improving the connection stability between the elastic member and the pressing block, and between the elastic member and the mounting plate.

[0048] In one embodiment, the elastic member is glued to the inner wall of the pressing block and the mounting plate respectively, thereby improving the connection stability between the elastic member and the pressing block, and between the elastic member and the mounting plate.

[0049] In one of the embodiments, the pressing block is a silicone pressing block, which avoids the problem of the pressing block damaging the battery packaging shell.

[0050] In one embodiment, the mounting plate further comprises a first limiting body, which is arranged in the mounting cavity, and the elastic member is sleeved on the first limiting body. The pressing block comprises a second limiting body, which is arranged in the mounting cavity, and the elastic member is sleeved on the second limiting body. The first limiting body and the second limiting body are arranged alternately, thereby improving the connection stability between the elastic member and the pressing block, and between the elastic member and the mounting plate.

[0051] In one embodiment, the elastic body is a coil spring, one end of the coil spring is connected to the inner wall of the mounting cavity, and the other end of the coil spring is connected to the pressure, thereby ensuring the sliding connection between the pressure block and the mounting plate.

[0052] In one embodiment, the elastic body is an elastic rubber column, one end of the elastic rubber column is connected to the inner wall of the installation cavity, and the other end of the elastic rubber column is connected to the pressure, thereby ensuring the sliding connection between the pressure block and the installation plate.

[0053] Please also read Figure 5 and Figure 6 In one embodiment, the pressing block 312 includes a clamping portion 3121 and an abutting portion 3122. The clamping portion 3121 is clamped in the mounting cavity 110 and slidably connected to the mounting plate 100, and the clamping portion 3121 is connected to the abutting portion 3122. The abutting portion 3122 is located in the conducting groove 120, and the abutting portion 3122 partially protrudes from the conducting groove 120. The abutting portion 3122 is arranged corresponding to the second clamping member 220 of each clamping assembly 200. It can be understood that the clamping portion 3121 is clamped on the mounting plate 100 and connected to the abutting portion 3122, so that the pressing block 312 is installed on the mounting plate 100 and avoids the problem of the pressing block 312 slipping off the mounting plate 100, thereby improving the connection stability between the pressing block 312 and the mounting plate 100.

[0054] In one of the embodiments, the clamping portion 3121 and the abutting portion 3122 are an integrally formed structure, so that the clamping portion 3121 and the abutting portion 3122 are firmly connected, which is conducive to the rapid processing and forming of the pressing block 312, reduces the processing steps of the pressing block 312, increases the structural stability of the pressing block 312, and makes the structure of the pressing block 312 more compact.

[0055] Please also read Figure 5 and Figure 6In one embodiment, the number of the conducting grooves 120 and the abutting portions 3122 are both multiple, and the multiple abutting portions 3122 are arranged in a one-to-one correspondence in the multiple conducting grooves 120, and the multiple abutting portions 3122 are all connected to the clamping portion 3121, and the multiple abutting portions 3122 are arranged in a one-to-one correspondence with the second clamping members 220 of the multiple clamping assemblies 200. It can be understood that the multiple abutting portions 3122 are arranged in a one-to-one correspondence with the multiple conducting grooves 120, so that the sliding of the pressing block 312 is realized, and the multiple abutting portions 3122 are connected to the clamping portion 3121, which improves the consistency of the pressure on each battery during the battery formation process, thereby improving the consistency and qualified rate of the battery formation.

[0056] It should be noted that if the number of the pressing block 312 and the elastic member 311 are both multiple, and the multiple pressing blocks 312 are independent of each other, then when the elastic force generated by the elastic deformation of the elastic member 311 of the pressing block 312 is inconsistent, the formation pressure consistency of each battery during the battery formation process is poor, thereby causing the battery formation consistency to be poor. Therefore, in the parallel formation device of the present application, the pressing block 312 includes a clamping portion 3121 and an abutting portion 3122, so that the abutting portion 3122 is arranged in the mounting cavity 110 and is slidably connected to the mounting plate 100, so that the force of the elastic deformation of the elastic member 311 is uniformly applied to the clamping portion 3121, and pressure is applied to the battery through multiple abutting portions 3122 connected to the clamping portion 3121, thereby improving the consistency of the pressure received by each battery during the battery formation process, thereby improving the consistency and qualified rate of the battery formation.

[0057] In one of the embodiments, the area of ​​the side of the pressing block 312 that abuts against the battery is larger than the area of ​​the side of the battery that abuts against the pressing block 312, further ensuring that the pressure at various locations during the battery formation process remains consistent, avoiding uneven pressure during the battery formation process, which may cause local bulging of the battery shell, and improving the consistency and pass rate of the battery formation.

[0058] Please also read Figure 5 and Figure 6In one embodiment, a plurality of telescopic slots 140 are further provided on the mounting plate 100, and the extension direction of each telescopic slot 140 is the same as the extension direction of the conducting slot 120, and the opening direction of each telescopic slot 140 is the same as the opening direction of the conducting slot 120. In this embodiment, the second clamping member 220 of each clamping assembly 200 includes a clamping block 221 and a telescopic member 222, and one end of the clamping block 221 of the second clamping member 220 of each clamping assembly 200 is clamped in the corresponding telescopic slot 140 and slidably connected with the mounting plate 100, and the telescopic member 222 of the second clamping member 220 of each clamping assembly 200 is disposed in the corresponding telescopic slot 140, and the telescopic member 222 of the second clamping member 220 of each clamping assembly 200 is clamped between the mounting plate 100 and the corresponding clamping block 221. It can be understood that one end of the clamping block 221 of the second clamping member 220 is clamped in the corresponding telescopic groove 140, which avoids the problem of the second clamping member 220 detaching from the mounting plate 100, improves the connection stability between the second clamping member 220 and the mounting plate 100, and realizes the sliding of the second clamping member 220 through the telescopic member 222, avoids the mechanical interference of the second clamping member 220 on the pressure regulating telescopic member 310, and ensures the controllability of the pressure regulating telescopic member 310 on the formation pressure of the battery.

[0059] It can be understood that the second clamping member 220 is an insulating clamping body, which reduces the probability of battery short circuit during battery formation and improves the battery formation qualification rate.

[0060] In one embodiment, the telescopic member 222 is welded to the inner wall of the clamping block 221 and the telescopic slot 140 , respectively, which improves the connection stability between the telescopic member 222 and the clamping block 221 , and between the telescopic member 222 and the mounting plate 100 .

[0061] In one embodiment, the telescopic member 222 abuts against the inner wall of the clamping block 221 and the telescopic slot 140 , respectively, thereby improving the connection stability between the telescopic member 222 and the clamping block 221 , and between the telescopic member 222 and the mounting plate 100 .

[0062] In one embodiment, the telescopic member 222 is glued to the clamping block 221 and the inner wall of the telescopic slot 140 respectively, which improves the connection stability between the telescopic member 222 and the clamping block 221 , and between the telescopic member 222 and the mounting plate 100 .

[0063] In one embodiment, the telescopic member 222 is a coil spring, one end of which is connected to the inner wall of the telescopic slot, and the other end of which is connected to the clamping block 221 , thereby ensuring a sliding connection between the clamping block 221 and the mounting plate 100 .

[0064] In one embodiment, the telescopic member 222 is an elastic rubber column, one end of which is connected to the inner wall of the telescopic groove, and the other end of which is connected to the clamping block 221, thereby ensuring a sliding connection between the clamping block 221 and the mounting plate 100.

[0065] In one embodiment, the clamping block 221 is a silicone clamping block, which avoids the problem of the pressing block 312 damaging the positive and negative terminals of the battery.

[0066] In one embodiment, the mounting plate 100 further includes a third limiting body, which is disposed in the telescopic groove 140, and the telescopic member 222 is sleeved on the third limiting body. The clamping block 221 includes a fourth limiting body, which is disposed in the telescopic groove 140, and the telescopic member 222 is sleeved on the fourth limiting body. The first limiting body and the second limiting body are staggered, thereby improving the connection stability between the telescopic member 222 and the clamping block 221, and between the telescopic member 222 and the mounting plate 100.

[0067] Please also read Figure 4 In one embodiment, the first clamping member 210 of each clamping assembly 200 also includes an insulator 213. The insulator 213 of the first clamping member 210 of each clamping assembly 200 is clamped between the corresponding positive electrode column 211 and the corresponding negative electrode column 212, thereby reducing the probability of battery short circuit during battery formation and improving the battery formation qualification rate.

[0068] See also Figure 7 The present application also provides a parallel formation device, comprising a level corrector, a housing 20 and a parallel formation device 10 of any of the above embodiments, wherein at least two stacked clamping mechanisms 10a and the level corrector are both arranged in the housing 20, and the level corrector is connected to a mounting plate 100 of any clamping mechanism 10a, and the level corrector is used to adjust the levelness of the mounting plate 100. Please refer to Figure 1 , Figure 3 and Figure 5In this embodiment, the parallel formation device 10 includes at least two stacked clamping mechanisms 10a, and the two clamping mechanisms 10a are used to clamp the battery. Each clamping mechanism 10a includes a mounting plate 100, a plurality of clamping components 200 and a pressure regulating component 300. The mounting plates 100 of two adjacent clamping mechanisms 10a are stacked, and the mounting plates 100 are provided with a mounting cavity 110, a conducting groove 120 and a sliding groove 130, and the mounting cavity 110 is connected to the conducting groove 120. Each clamping assembly 200 includes a first clamping member 210 and a second clamping member 220, and the first clamping member 210 and the second clamping member 220 are relatively arranged on both sides of the mounting plate 100, and each first clamping member 210 includes a positive pole column 211 and a negative pole column 212, and the positive pole column 211 and the negative pole column 212 are both installed on the mounting plate 100, and the second clamping member 220 is slidably connected to the mounting plate 100, and the sliding direction of the second clamping member 220 is the same as the extension direction of the conductive groove 120, and the opening direction of the conductive groove 120 is toward the side of the mounting plate 100 where the second clamping member 220 is set. The pressure regulating assembly 300 includes a pressure regulating telescopic member 310 and a lifting and lowering regulating member 320. The pressure regulating telescopic member 310 is located in the mounting cavity 110 and is elastically connected to the mounting plate 100. The pressure regulating telescopic member 310 partially protrudes from the periphery of the mounting plate 100 through the conducting groove 120. The pressure regulating telescopic member 310 is also slidably connected to the mounting plate 100, and the sliding direction of the pressure regulating telescopic member 310 is the same as the extension direction of the conducting groove 120; the lifting and lowering regulating member 320 includes a sliding block 321 and a transmission group 322. The sliding block 321 is arranged at the sliding groove 130 and is slidably connected to the mounting plate 100, and the sliding block 321 is connected to another stacked mounting plate 100. The transmission group 322 is installed on the mounting plate 100, and the power output end of the transmission group 322 is connected to the sliding block 321. The transmission group 322 drives the sliding block 321 to slide relative to the mounting plate 100, and the sliding direction of the sliding block 321 is the same as the extension direction of the conducting groove 120. Among them, when the transmission group 322 drives the sliding block 321 to slide along the first direction relative to the mounting plate 100, that is, when the transmission group 322 drives the sliding block 321 to slide along the A direction relative to the mounting plate 100, the two adjacent mounting plates 100 approach each other, and the pressure regulating telescopic member 310 contracts; when the transmission group 322 drives the sliding block 321 to slide along the second direction relative to the mounting plate 100, that is, when the transmission group 322 drives the sliding block 321 to slide along the B direction relative to the mounting plate 100, the two adjacent mounting plates 100 move away from each other, and the pressure regulating telescopic member 310 extends.

[0069] In the above-mentioned parallel formation equipment, at least two stacked clamping mechanisms 10a in the parallel formation device 10 are used to realize the rapid fixation of the battery and the adjustment of the battery formation pressure, and a horizontal corrector is added to make each parallel formation device 10 in a horizontal state, avoiding the parallel formation device 10 from tilting, resulting in uneven formation pressure of each battery, and causing the parallel formation device 10 to adjust the formation pressure of each battery inaccurately, reducing the consistency of the battery after formation, and even causing poor contact between the positive and negative ears of the battery and leakage of electrolyte during the battery formation process, reducing the problem of battery formation qualification rate, improving the consistency of the battery after formation and improving the battery formation qualification rate.

[0070] It should be noted that the level corrector is used to detect the level of the clamping mechanism 10a and adjust the level of the holding mechanism so that the clamping mechanism 10a is in a horizontal state.

[0071] The present application also provides a lithium-ion battery, which is formed by using the parallel formation equipment of any of the above embodiments. Figure 7 In this embodiment, the parallel formation equipment includes a horizontal corrector, a shell 20 and the parallel formation device 10 of any of the above embodiments, at least two stacked clamping mechanisms 10a and the horizontal corrector are arranged in the shell 20, the horizontal corrector is connected to the mounting plate 100 of the clamping mechanism 10a, and the horizontal corrector is used to adjust the horizontality of the mounting plate 100.

[0072] In the above-mentioned lithium-ion battery, rapid fixation of the battery and adjustment of the battery formation pressure are achieved through at least two stacked clamping mechanisms 10a in the parallel formation equipment, and a horizontal corrector is added to make each parallel formation device 10 in a horizontal state, avoiding the parallel formation device 10 from tilting, resulting in uneven formation pressure of each battery, and causing the parallel formation device 10 to adjust the formation pressure of each battery inaccurately, thereby reducing the consistency of the battery after formation, and even causing poor contact between the positive and negative ears of the battery and leakage of electrolyte during the battery formation process, thereby reducing the problem of battery formation qualification rate and improving the consistency of the battery after formation.

[0073] In order to better understand the lithium ion battery of the present invention, the lithium ion battery of the present invention is further explained below. In one embodiment, the lithium ion battery is formed by using the parallel formation equipment described in any of the above embodiments. Please refer to Figure 7 , the formation of the lithium ion battery comprises the following steps:

[0074] S100, obtain the battery cell after the injection. It can be understood that the operation object in the lithium-ion battery formation process is the battery cell after the injection. The electrolyte injected into the battery cell will react with the electrode in the battery cell. The type and amount of the electrolyte are related to the active material in the electrode. Therefore, the electrolyte injected into the obtained battery cell is an electrolyte compatible with the electrode of the battery cell, and the battery cell after the injection is the battery cell with the same electrolyte injection time, which improves the consistency of the internal resistance of the battery cell after the injection, makes the current passing through the static battery cell in the parallel circuit closer, reduces the difficulty of parameter control, and better realizes the feasibility of the static battery cell in the parallel circuit. The efficiency of lithium-ion battery formation is improved.

[0075] S200, inkjet the battery cells. It is understandable that in the process of forming the lithium-ion battery, the formation is not performed on a single cell or a small number of battery cells, but on a large number of battery cells. The operator may miss or mishandle the battery cells with a small probability by relying on memory or simple marking, which makes it difficult to ensure the consistency of the infiltration degree of the battery cells, resulting in different internal resistances of the battery cells at the beginning of the formation, and thus making it difficult to control the current of the battery cells under each parallel circuit, making the consistency of the battery cells after the formation of the same batch poor, and making it impossible to effectively control the battery capacity and cycle performance of the lithium-ion battery after the formation. Therefore, by inkjet printing the battery cells, each battery cell has its own corresponding information system, and after screening the information system, the battery cells have the same time from the completion of the injection to the inkjet printing, which ensures the full infiltration of the battery cells before the formation and the consistency of the battery cells before the formation.

[0076] S300, the battery cells after the coding treatment are put aside to obtain the static battery cells. It can be understood that the battery cells after the coding treatment have their own corresponding information systems to measure the operation time of the battery cell shelving operation respectively. The information system screens all the battery cells that have reached the preset length of the static time, displays the location of each battery cell, and then the operator picks it out to proceed to the next step of formation. The foolproof operation is designed to avoid the small probability of battery cell leakage or processing errors, improve the consistency of the lithium-ion battery after formation, make the current passing through the static battery cells in the parallel circuit relatively similar, reduce the difficulty of parameter control, better realize the feasibility of static battery cells in the parallel circuit formation, and thus improve the efficiency of lithium-ion battery formation.

[0077] S400, the static cells are connected in parallel to obtain a cell group. It is understood that the voltages of the static cells connected in parallel are the same, and under the premise of ensuring the consistency of the internal resistance of the static cells, the consistency of the current passing through the static cells is better. Therefore, when controlling the current through the static cells in parallel, the current set at both ends of the power supply is the sum of the static cells, which reduces the control difficulty of the lithium ion battery formation, better realizes the feasibility of the static cells in the parallel circuit formation, and then improves the efficiency of the lithium ion battery formation. In the present embodiment, the static cells are connected in parallel using a parallel formation device. It is also understood that the parallel formation device realizes the fast fixed connection of the static cells, and improves the connection stability of the static cells.

[0078] S500, using a predetermined current to perform a staged formation operation on the battery group to obtain a lithium-ion battery. It can be understood that the stationary batteries are connected in parallel, and the predetermined current is used to perform a staged formation operation on the battery group while ensuring the consistency of the wetting of the stationary batteries, which improves the consistency of the lithium-ion battery formation, effectively reduces the formation time of the lithium-ion battery and improves the conductivity of the lithium-ion battery, thereby improving the formation efficiency of the lithium-ion battery and the cycle performance of the battery, avoiding the problem of a long formation time required for the battery group under a small current state and a fast cycle decay of the battery group under a large current state.

[0079] In the above-mentioned lithium-ion battery parallel formation method, the battery cells are subjected to coding treatment so that each battery cell has a corresponding coding time, and the battery cells after coding treatment are subjected to static operation so that each battery cell has a corresponding static operation time, so that an operator can select static batteries with the same static operation time, thereby ensuring the wetting consistency of the static batteries, making the currents passing through the static batteries in the parallel circuit closer, reducing the difficulty of parameter control, and better realizing the feasibility of forming the static batteries in the parallel circuit, thereby improving the efficiency of lithium-ion battery formation. The stationary cells are connected in parallel, and a predetermined current is used to perform a staged formation operation on the cell group while ensuring the wetting consistency of the stationary cells. This improves the consistency of the formation of the lithium-ion battery, effectively reduces the formation time of the lithium-ion battery and improves the conductivity of the lithium-ion battery, thereby improving the formation efficiency of the lithium-ion battery and the cycle performance of the lithium-ion battery, avoiding the problem of a long formation time required for the cell group under a small current state and a fast cycle attenuation of the cell group under a large current state.

[0080] In one embodiment, before obtaining the stationary battery cell and after the battery cell after the coding treatment is placed, the following step is also included: obtaining the qualified standing time X of the stationary battery cell. It can be understood that the qualified time X is determined based on the average time interval of the battery cell after injection obtained by detecting the degree of electrolyte infiltration of the battery cell after injection, wherein the object of the average time interval of complete infiltration is the battery cell after injection prepared using the electrolyte of the same material and the battery cell of the same material, ensuring that the battery cell after injection is completely infiltrated, and improving the battery capacity of the lithium-ion battery.

[0081] Furthermore, the battery cells that have been processed by inkjet coding are scanned to obtain the resting time x of the battery cells. It can be understood that the battery cells that have been processed by inkjet coding have their own corresponding information systems to measure the operation time of the battery cell shelving operation respectively. The information system will perform corresponding real-time measurement of the operation time of the battery cell shelving operation. After the measured resting time x reaches the qualified resting time X, a corresponding prompt will be given to designate the battery cell. However, the operator may still make accidental operations and confuse the battery cells that have been coded with other battery cells that have been coded. Therefore, when confirming the designated battery cell, it is necessary to further scan the designated battery cell for confirmation. Setting two fool-proof operations of inkjet coding and scanning further ensures that the selected battery cell after liquid injection does have enough resting time, thereby improving the consistency of the lithium-ion battery and increasing the battery capacity of the lithium-ion battery.

[0082] Furthermore, the battery cell is judged as a qualified static battery cell, and a static battery cell can be obtained if X=x; if X>x, the battery cell is judged as an unqualified static battery cell, and the shelving operation is repeated. It can be understood that the information system performs corresponding real-time measurement of the operation time of the battery cell shelving operation, and gives a corresponding prompt after the measured static time x reaches the qualified static time X, and the designated battery cell meets the requirements of the static battery cell, and then the designated battery cell is further scanned for confirmation. If X=x after scanning the code, the battery cell is judged as a qualified static battery cell, and a static battery cell can be obtained. If X>x after scanning the code, the battery cell is judged as an unqualified static battery cell, and the shelving operation is repeated. By setting two foolproof operations of spraying and scanning, it is further ensured that the selected battery cell after injection does have sufficient static time, thereby improving the consistency of the lithium-ion battery and increasing the battery capacity of the lithium-ion battery.

[0083] It can be understood that by inkjet coding the battery cells after injection, an information system corresponding to the battery cells themselves is established, so that the operation time of the shelving operation of each battery cell can be quantified, avoiding the problem of a small probability of missing or mishandling the battery cells after injection due to the operator's memory or simple marking. After the information system prompts that the standing time x of the battery cells after injection meets the requirement of standing time X, the information is further confirmed to be correct by scanning the code. Through the two fool-proof operations of inkjet coding and scanning the code, it is further ensured that the selected battery cells after injection do have sufficient standing time, thereby improving the consistency of the lithium-ion battery and increasing the battery capacity of the lithium-ion battery.

[0084] In one of the embodiments, the qualified standing time X is 18 hours to 35 hours, which ensures that the positive and negative electrodes of the battery cell are completely soaked in the electrolyte.

[0085] In one of the embodiments, the battery cell after the coding treatment is placed on hold under high temperature conditions, thereby increasing the speed at which the electrodes in the battery cell after the coding treatment are infiltrated by the electrolyte.

[0086] In one embodiment, the staged formation operation includes a first stage formation operation, a second stage formation operation, a third stage formation operation and a fourth stage formation operation performed sequentially. In the staged formation operation, the formation current used by the battery cell group first increases and then decreases as the stages increase, thereby avoiding the problem of a long formation time required for the battery cell group under a small current state and a fast cycle attenuation of the battery cell group under a large current state, thereby improving the formation efficiency and cycle performance of the lithium ion battery.

[0087] In one embodiment, the formation current used by the battery cell group in the third stage formation operation is greater than the formation current used by the battery cell group in the second stage formation operation, and the formation current used by the battery cell group in the third stage formation operation is greater than the formation current used by the battery cell group in the fourth stage formation operation, thereby ensuring the formation of a stable solid electrolyte interface film during the formation process of the lithium ion battery and improving the formation efficiency of the lithium ion battery.

[0088] In one embodiment, the staged formation operation comprises the following steps:

[0089] The first stage formation operation of the battery cell group is performed with a constant current of 0.2C to 0.3C to obtain the first battery cell. It can be understood that in the initial stage of the formation of the battery cell group with an external current, a solid electrolyte interface membrane has not yet been formed in the battery cell group. If a large external current is applied, the produced solid electrolyte interface membrane will be fluffy and unstable. Therefore, in the initial stage of the formation of the battery cell group, that is, in the first stage formation operation, a constant current of 0.2C to 0.3C is used to form the battery cell group, which improves the stability of the solid electrolyte interface membrane formed by the first battery cell, reduces the consumption of conductive materials in the positive and negative electrodes, and ensures the battery capacity of the first battery cell.

[0090] Further, a second stage formation operation is performed on the first battery cell with a constant current of 0.4C to 0.5C to obtain a second battery cell. It can be understood that after the initial stage of formation of the battery cell group, if the first battery cell is continuously formed with an external small current, the solid electrolyte interface film formed by the first battery cell will be more compact and increased, thereby affecting the rate and cycle performance of the lithium-ion battery. Therefore, after the initial stage of formation of the battery cell group, that is, in the second stage formation operation of the first battery cell, a constant current of 0.4C to 0.5C is used to form the first battery cell, so that the solid electrolyte interface film formed has better bulkiness on one side facing the electrolyte, and then the solid electrolyte interface film can be infiltrated with more electrolyte, thereby improving the ionic conductivity of the second battery cell.

[0091] Furthermore, a 0.6C-0.7C constant current is used to perform a third-stage formation operation on the second battery cell to obtain a third battery cell. It can be understood that after the battery cell group is formed in the first two stages, in order to increase the formation efficiency of the lithium-ion battery, the applied current is further increased to perform the third-stage formation operation on the second battery cell, but the increase in current is too large, so that the movement speed of lithium ions cannot keep up with the movement speed of electrons, causing serious polarization of the second battery cell. Therefore, a 0.6C-0.7C constant current is used to form the second battery cell, which reduces the polarization degree of the third battery cell. However, in order to further reduce the polarization degree of the third battery cell, the temperature, pressure and charging time should be adjusted at the same time to assist in reducing the polarization degree of the third battery cell under a larger current.

[0092] Furthermore, the third battery cell is subjected to the fourth stage formation operation using a constant current of 0.2C to 0.4C to obtain a lithium-ion battery. It can be understood that after the battery cell group has been subjected to the first three stages of formation, the battery has been basically formed, and the solid electrolyte interface membrane has also been basically formed. At this stage, the third battery cell is subjected to the fourth stage formation operation using a constant current of 0.2C to 0.4C, so that the density of the solid electrolyte interface membrane facing the electrolyte is increased, the completion of the formation is promoted, the efficiency of the battery formation is further improved, and the stability of the solid electrolyte interface membrane is further improved.

[0093] It can be understood that by connecting the stationary cells in parallel, while ensuring the wetting consistency of the stationary cells, the cell group is subjected to staged formation operation using constant currents of 0.2C-0.3C, 0.4C-0.5C, 0.6C-0.7C and 0.2C-0.4C respectively, which improves the consistency of the formation of the lithium-ion battery, effectively reduces the formation time of the lithium-ion battery and improves the conductivity of the lithium-ion battery, thereby improving the formation efficiency of the lithium-ion battery and the cycle performance of the battery, avoiding the problem of a long formation time required for the cell group under a small current state and a faster cycle attenuation of the cell group under a large current state.

[0094] It should be noted that the above 0.2-0.3, 0.4-0.5, 0.6-0.7 and 0.2-0.4 are rate range values, and C represents the capacity value of each group of lithium-ion batteries.

[0095] In one embodiment, in the staged formation operation, the first stage formation operation is performed at a temperature of 40°C to 50°C. It can be understood that in the first stage of the formation of the battery group by the applied current, the solid electrolyte interface membrane has not yet been formed in the battery group, and the battery group is formed by a constant current of 0.2C to 0.3C to ensure the stability of the solid electrolyte interface membrane formed by the first battery, and under the condition of a temperature of 40°C to 50°C, the ionic conductivity of the electrolyte is increased, which is conducive to the formation of the solid electrolyte interface membrane, but if the temperature is too low, the desired effect cannot be achieved; if the temperature is too high, the compactness of the generated solid electrolyte interface membrane will be destroyed, resulting in the generated solid electrolyte interface membrane being porous and fluffy, therefore, the battery group is formed by a constant current of 0.2C to 0.3C at a temperature of 40°C to 50°C to further ensure the stability of the solid electrolyte interface membrane formed by the first battery.

[0096] Further, the second stage formation operation is performed at a temperature of 60°C to 70°C. It can be understood that after the initial stage of the formation of the battery group, the first battery is formed with a constant current of 0.4C to 0.5C to ensure that the solid electrolyte interface membrane formed has a better bulkiness on the side facing the electrolyte, but in the process of increasing the current for formation, it is easy to cause the polarization degree of the lithium ion battery to increase, and under the condition of a temperature of 60°C to 70°C, the movement speed of lithium ions in the electrolyte is accelerated, so that the movement speed of lithium ions at this time is closer to the movement speed of electrons at this time, effectively reducing the polarization degree of the second battery, and the use of 0.4C to 0.5C constant current formation aids the second stage formation operation at a temperature of 60°C to 70°C, so that the solid electrolyte interface membrane formed has a better bulkiness on the side facing the electrolyte, thereby improving the ionic conductivity of the second battery.

[0097] Furthermore, the third stage formation operation is performed at a temperature of 70°C to 80°C. It can be understood that after the first two stages of formation of the battery group, the second battery is formed using a constant current of 0.6C to 0.7C to increase the formation efficiency of the lithium-ion battery, but in the process of further increasing the current for formation, it is easy to cause the polarization degree of the lithium-ion battery to further increase, and under the condition of a temperature of 70°C to 80°C, the movement speed of lithium ions in the electrolyte is further accelerated, so that the movement speed of lithium ions at this time is closer to the movement speed of electrons at this time, effectively reducing the polarization degree of the third battery, and the use of a constant current formation aid of 0.6C to 0.7C to perform the third stage formation operation at a temperature of 70°C to 80°C further increases the bulkiness of the solid electrolyte interface film on one side facing the electrolyte, thereby improving the ionic conductivity of the second battery. It can also be understood that if the temperature is too high during the battery formation process, the formed solid electrolyte interface film will be destroyed, causing the solid electrolyte interface film to dissolve, resulting in irreversible capacity loss of the lithium-ion battery, and will increase the side reactions inside the battery, causing bulging on the surface of the lithium-ion battery; and if the temperature is too low, the movement speed of lithium ions in the electrolyte of the lithium-ion battery will not keep up with the movement speed of electrons, so that increasing the temperature cannot achieve the effect of reducing polarization. Therefore, in the third stage formation operation, the temperature is controlled at 70°C to 80°C, which, on the one hand, reduces the damage to the formed solid electrolyte interface film and increases the battery capacity and charge and discharge rate of the lithium-ion battery; on the other hand, it increases the movement speed of lithium ions in the electrolyte and reduces the polarization of the lithium-ion battery.

[0098] Furthermore, the fourth stage formation operation is performed at a temperature of 35°C to 45°C. It can be understood that after the first three stages of formation of the battery cell group, the battery has basically completed the formation, and the solid electrolyte interface film has also been basically formed. At this time, the fourth stage formation operation is performed on the third battery cell at a constant current of 0.2C to 0.4C, which reduces the movement rate of electrons. Therefore, the temperature is lowered to reduce the movement speed of ions in the lithium-ion battery, and the temperature is lowered to reduce the damage to the formed solid electrolyte interface film, making the formed solid electrolyte interface film more compact, thereby making the formed solid electrolyte interface film more stable, promoting the completion of the formation, thereby improving the efficiency of the battery formation, and improving the stability of the solid electrolyte interface film.

[0099] It can be understood that the cell group is subjected to staged formation operation at temperatures of 40°C to 50°C, 60°C to 70°C, 70°C to 80°C and 35°C to 45°C, respectively, and the cell group is subjected to staged formation operation at constant currents of 0.2C to 0.3C, 0.4C to 0.5C, 0.6C to 0.7C and 0.2C to 0.4C correspondingly, which increases the formation speed of the cell, thereby improving the formation efficiency of the lithium-ion battery; and reduces the polarization problem in the formation process of the lithium-ion battery, and also makes the formed solid electrolyte interface film more stable and has higher conductivity, thereby improving the charge and discharge performance and cycle performance of the lithium-ion battery.

[0100] In one embodiment, in the staged formation operation, the operation time of the first stage formation operation is 3min to 5min. It can be understood that in the first stage formation operation, a solid electrolyte interface film is initially formed on the surface of the pole piece. At this time, the solid electrolyte interface film is greatly affected by the temperature of the electrolyte, which easily causes the generated solid electrolyte interface film to be rapidly and irreversibly destroyed, thereby reducing the formation efficiency of the lithium ion battery and reducing the battery capacity of the lithium ion battery after formation. Therefore, in the first stage formation operation, a smaller current and a lower temperature are used to form the battery core. If the time of the first stage operation is too long, the speed of the lithium ion battery formation is affected, and the impedance of the solid electrolyte interface film is increased, affecting the charge and discharge performance of the lithium ion battery; if the time of the first stage operation is too short, the stability of the generated solid electrolyte interface film is poor, affecting the battery capacity and cycle performance of the lithium ion battery. Therefore, the operation time of the first stage formation operation is 3min to 5min, which increases the formation speed of the lithium ion battery and increases the stability of the solid electrolyte interface film in the lithium ion battery. A constant current of 0.2C to 0.3C, a temperature of 40°C to 50°C and an operation time of 3min to 5min are used. At this time, the formation current is small, so that the formed solid electrolyte interface film is denser, and a lower temperature is used to reduce the degree of damage to the generated solid electrolyte interface film.

[0101] Further, the operation time of the second stage formation operation is 6min to 10min. It can be understood that in the second stage formation operation, a relatively dense solid electrolyte interface film has been initially formed on the surface of the pole piece, but the solid electrolyte interface film is still greatly affected by the electrolyte temperature. In order to further increase the formation speed of the battery cell, the current is relatively increased in the second stage formation operation, that is, a 0.4C to 0.5C constant current is used to form the battery cell. Further, the temperature of the second stage formation operation is adjusted to reduce the degree of damage to the solid electrolyte interface film, that is, a temperature of 60°C to 70°C is used to form the battery cell, which increases the formation speed of the battery cell and reduces the polarization degree of the lithium-ion battery, so that the operation time of the second stage formation operation is 6min to 10min, ensuring that the degree of damage to the solid electrolyte interface film is reduced while increasing the formation speed of the battery cell.

[0102] Furthermore, the operation time of the third stage formation operation is 15min to 25min. It can be understood that in the third stage formation operation, a relatively stable solid electrolyte interface film has been formed on the surface of the pole piece. In order to further increase the formation speed of the battery cell, the current is further increased in the third stage formation operation, that is, a 0.6C to 0.7C constant current is used to form the battery cell. Further, the temperature of the third stage formation operation is adjusted, that is, a temperature of 60°C to 70°C is used to form the battery cell, which increases the formation speed of the battery cell and reduces the polarization degree of the lithium-ion battery. The operation time of the third stage formation operation is 15min to 25min, ensuring the formation of a stable solid electrolyte interface film. It can also be understood that if a constant current higher than 0.4C to 0.5C and a temperature higher than 60°C to 70°C are directly used to perform a formation operation on the battery core in the second stage formation operation, the solid electrolyte interface film generated in the first stage formation operation is severely damaged, making it difficult for the electrode surface of the lithium ion battery to further form a stable solid electrolyte interface film, and seriously reducing the battery capacity of lithium ions, affecting the use of the lithium ion battery after formation. Therefore, in the second stage formation operation, a constant current of 0.4C to 0.5C and a temperature of 60°C to 70°C are first used to perform a formation operation on the battery core, so that a relatively stable solid electrolyte interface film is further generated, and then the current and temperature are further increased to further improve the formation speed of the lithium ion battery, that is, in the third stage formation operation, a constant current of 0.6C to 0.7C and a temperature of 60°C to 70°C are used to perform a second stage formation operation on the battery core for 6min to 10min, ensuring that the degree of damage to the generated solid electrolyte interface film is reduced while improving the formation speed of the lithium ion battery.

[0103] Furthermore, the operation time of the fourth stage formation operation is 35min to 45min. It can be understood that in the fourth stage formation operation, the battery has basically completed the formation, and the solid electrolyte interface film has basically been formed, but the side of the generated solid electrolyte interface film facing the electrolyte is relatively fluffy and is easily destroyed during the charging and discharging process of the lithium ion battery. Therefore, in the fourth stage formation operation, a 0.2C to 0.4C constant current and a temperature of 35°C to 45°C are used to perform the fourth stage formation operation on the third battery cell, which improves the compactness of the side of the generated solid electrolyte interface film facing the electrolyte, thereby improving the stability of the solid electrolyte interface film generated in the lithium ion battery after formation, so that the operation time of the fourth stage formation operation is 35min to 45min, ensuring the formation of a stable solid electrolyte interface film.

[0104] It is understandable that the formation time of lithium ion batteries is generally 5 to 7 days of static formation, and the parallel formation method of lithium ion batteries of the present invention adopts temperatures of 40°C to 50°C, 60°C to 70°C, 70°C to 80°C and 35°C to 45°C respectively, and one-to-one correspondence is matched with 0.2C to 0.3C, 0.4C to 0.5C, 0.6C to 0.7C and 0.2C to 0.4C constant currents, and one-to-one correspondence is matched with 3min to 5min, 6min to 10min, 15min to 25min and 35min to 45min operation time to perform staged formation operation on the battery cell group, which increases the formation speed of the battery cell, thereby improving the formation efficiency of the lithium ion battery, and makes the formed solid electrolyte interface film more stable and has higher conductivity, thereby improving the charge and discharge performance and cycle performance of the lithium ion battery.

[0105] In one embodiment, the parallel connection operation step includes the following steps: using parallel formation equipment to fix the stationary battery cells, thereby ensuring the rapid fixation and fixation reliability of each battery cell.

[0106] Furthermore, the stationary cells after the fixing treatment are connected in parallel in the circuit. It can be understood that the stationary cells with the same stationary time, that is, the stationary cells with better consistency of infiltration degree, are formed in the same parallel circuit, which ensures the consistency of the voltage and current passing through each stationary cell in the cell group, and improves the consistency of the performance of the lithium-ion battery after formation.

[0107] In the above-mentioned parallel connection operation, the stationary cells that have been fixed are connected in parallel in the circuit to ensure the connectivity stability of the stationary cells in the circuit, and the stationary cells with good consistency in the degree of wetting are formed in the same parallel circuit, ensuring the consistency of the voltage and current passing through each stationary cell in the cell group, thereby improving the consistency of the performance of the lithium-ion battery after formation.

[0108] In one embodiment, before the step of staged formation operation and after the step of parallel connection operation, the parallel formation method of lithium ion batteries also includes the following steps: performing horizontal correction operation on the battery group. It can be understood that if the pressure of the static cells in the battery group is controlled one by one, the difficulty of controlling the consistency of the pressure on each static cell is increased, so that there is an error in the pressure on each static cell, thereby reducing the consistency of the lithium ion battery after formation. Therefore, in order to ensure the consistency of the pressure on each static cell in the battery group, each static cell in the battery group is subjected to the pressure applied by the same substance, and in order to further ensure the consistency of the pressure on each static cell in the battery group, before applying pressure, the battery group is horizontally corrected to ensure that each static cell in the battery group is located at the same horizontal plane, so that the pressure applied by the same substance acts evenly on each static cell in the battery group, ensuring the consistency of the pressure on each static cell in the battery group, thereby improving the consistency of the lithium ion battery after formation.

[0109] In one embodiment, before the step of obtaining the lithium-ion battery and after the step of the staged formation operation, the lithium-ion battery parallel formation method further includes the following step: performing a gas extraction operation on the battery cell group. It is understood that during the formation process of the lithium-ion battery, a side reaction will occur to generate gas, which will destroy the generated solid electrolyte interface film and affect the performance of the lithium-ion battery. Therefore, after the lithium-ion battery is formed, the gas generated during the formation process needs to be extracted to ensure the performance of the lithium-ion battery.

[0110] It can also be understood that in the process of extracting gas, moisture in the external environment will further promote the generation of gas in the lithium-ion battery, thereby destroying the generated solid electrolyte interface film and electrode structure, affecting the charging rate and cycle performance of the lithium-ion battery. Therefore, in one of the embodiments, the battery cell group is evacuated under dry conditions to reduce the impact of moisture on the lithium-ion battery after formation.

[0111] In one embodiment, before the step of obtaining the lithium-ion battery and after the step of evacuating the gas, the lithium-ion battery parallel formation method further includes the following step: sealing the battery cell group. It is understandable that after the lithium-ion battery is formed, the gas in the lithium-ion battery needs to be extracted, and after the gas is extracted, the lithium-ion battery needs to be packaged, that is, the battery cell group needs to be sealed to isolate the contact between the inside of the lithium-ion battery and the outside world, thereby ensuring the performance of the lithium-ion battery.

[0112] It can also be understood that in the process of packaging the lithium-ion battery, there is a certain contact between the interior of the lithium-ion battery and the outside world. The moisture in the external environment will further promote the generation of gas in the lithium-ion battery, thereby destroying the generated solid electrolyte interface film and electrode structure, affecting the charging rate and cycle performance of the lithium-ion battery. Therefore, in one of the embodiments, the battery cell group is sealed under dry conditions to reduce the impact of moisture on the lithium-ion battery after formation.

[0113] It is understood that the battery will generate gas during the formation process. If the gas is not removed in time during the formation process, it will affect the formation of the solid electrolyte interface film of the lithium-ion battery and the structural stability of the lithium-ion battery electrode. Therefore, in one embodiment, in the staged formation operation, the pressure applied to the battery pack is 2.0N / cm 2 ~3.7N / cm 2 , reducing the amount of moisture in the external environment entering the battery cell group, effectively reducing the impact on the formation of the solid electrolyte interface film of the lithium-ion battery, and effectively improving the battery capacity and battery cycle performance of the lithium-ion battery.

[0114] In one embodiment, at a pressure of 2.0 N / cm 2 ~2.4N / cm 2 It can be understood that in the first stage of the formation operation, the battery cell is formed by using a constant current of 0.2C to 0.3C, a temperature of 40°C to 50°C, and an operation time of 3min to 5min. At this time, the amount of gas in the battery cell is small, so 2.0N / cm 2 ~2.4N / cm 2 The pressure is applied to the battery cell group, ensuring that the electrolyte in the battery cell group is not pressed out, and effectively discharging the gas in each battery cell of the battery cell group out of the battery cell, reducing the moisture in the external environment from entering the battery cell group, thereby improving the battery capacity and battery cycle performance of the lithium-ion battery.

[0115] Furthermore, at a pressure of 2.7 N / cm 2 ~3.1N / cm 2 It can be understood that in the second stage of the formation operation, the battery cell is subjected to a formation operation for 6min to 10min at a constant current of 0.4C to 0.5C and a temperature of 60℃ to 70℃. At this time, the growth rate of the amount of gas in the battery cell gradually increases, and the temperature of 2.0N / cm is still used. 2 ~2.4N / cm 2 The pressure applied to the battery pack cannot discharge the gas in the battery in time, so 2.7N / cm 2 ~3.1N / cm2 The pressure is applied to the battery cell group, ensuring that the electrolyte in the battery cell group is not pressed out, and effectively discharging the gas in each battery cell of the battery cell group out of the battery cell, reducing the moisture in the external environment from entering the battery cell group, thereby improving the battery capacity and battery cycle performance of the lithium-ion battery.

[0116] Furthermore, at a pressure of 3.2 N / cm 2 ~3.7N / cm 2 It can be understood that in the third stage of the formation operation, the battery cell is subjected to a 15-25 minute formation operation using a constant current of 0.4C-0.5C and a temperature of 60°C-70°C. The increase in current and temperature enhances the interaction between substances in the electrolyte, thereby further increasing the growth rate of the amount of gas in the battery cell. The 2.7N / cm 2 ~3.1N / cm 2 The pressure applied to the battery pack cannot discharge the gas in the battery in time, so 3.2N / cm 2 ~3.7N / cm 2 The pressure is applied to the battery cell group, ensuring that the electrolyte in the battery cell group is not pressed out, and effectively discharging the gas in each battery cell of the battery cell group out of the battery cell, reducing the moisture in the external environment from entering the battery cell group, thereby improving the battery capacity and battery cycle performance of the lithium-ion battery.

[0117] Furthermore, at a pressure of 2.0 N / cm 2 ~2.4N / cm 2 It can be understood that in the fourth stage of the formation operation, the battery has basically completed the formation, and the solid electrolyte interface film has basically been formed. The third battery cell is subjected to the formation operation for 35min to 45min at a constant current of 0.2C to 0.4C and a temperature of 35℃ to 45℃. At this time, the amount of gas generated is small, so 2.0N / cm 2 ~2.4N / cm 2 The pressure is applied to the battery cell group, ensuring that the electrolyte in the battery cell group is not pressed out, and effectively discharging the gas in each battery cell of the battery cell group out of the battery cell, reducing the moisture in the external environment from entering the battery cell group, thereby improving the battery capacity and battery cycle performance of the lithium-ion battery.

[0118] In one embodiment, performing a staged formation operation under vacuum conditions is beneficial for discharging the gas in each battery cell of the battery cell group out of the battery cell, reducing the amount of moisture in the external environment that enters the battery cell group, thereby improving the battery capacity and battery cycle performance of the lithium-ion battery.

[0119] In one of the embodiments, in the staged formation operation, a short-circuit monitoring device and a circuit-break monitoring device are used to monitor the short circuit and circuit-break of the parallel circuit, thereby avoiding the problem that when the parallel circuit of the battery cell group is short-circuited or open-circuited, the current in the parallel circuit changes, resulting in the formation of the solid electrolyte interface film of each stationary battery cell in the battery cell group being affected, thereby ensuring the stability and conductivity of the formed solid electrolyte interface film and improving the charge and discharge performance and cycle performance of the lithium-ion battery.

[0120] It can be understood that the wetting degree of the stationary cells is made the same, so that the consistency of the internal resistance of each stationary cell in the cell group is better, but the factors affecting the internal resistance of the stationary cells are not limited to the wetting degree of the stationary cells. In order to further improve the consistency of the internal resistance of each stationary cell in the cell group, in one embodiment, in the staged formation operation, a resistance adjustment device is used to adjust the current of the parallel circuit. By adjusting the current of the parallel circuit through the resistance adjustment device, the consistency of the current of each stationary cell in the cell group is improved, thereby improving the consistency of the lithium-ion battery after formation.

[0121] Compared with the prior art, the present invention has at least the following advantages:

[0122] 1. In the parallel formation device of the present invention, at least two stacked clamping mechanisms are used to clamp the battery, which avoids the need to use a clamp to fix the batteries one by one during battery formation, which is time-consuming and labor-intensive, resulting in increased labor costs and reduced formation efficiency. Specifically, the battery is placed near the first clamping member of the clamping mechanism, and the positive and negative pole ears are abutted against the first clamping member, and then the second clamping member of another clamping mechanism is connected to the first clamping member accordingly, and the pressure regulating telescopic member is abutted against the battery. On the one hand, the pressure regulating telescopic member plays a role in fixing the battery, and is used in conjunction with the first clamping member and the second clamping member to improve the battery. The production efficiency of the battery is improved and the battery formation time is reduced; on the other hand, the pressure regulating telescopic member plays a role in squeezing the battery and assisting in discharging the gas in the battery. When the transmission group drives the sliding block to slide relative to the mounting plate along the first direction, the two adjacent mounting plates are close to each other, and the pressure regulating telescopic member is contracted, so that the pressure on the battery is increased; when the transmission group drives the sliding block to slide relative to the mounting plate along the second direction, the two adjacent mounting plates are away from each other, and the pressure regulating telescopic member is extended, so that the pressure on the battery is reduced, thereby realizing the pressure regulation during the battery formation, reducing the degree of gas bulging in the battery shell during the formation process, and thus improving the qualified rate of the battery formation;

[0123] 2. In the parallel formation equipment of the present invention, at least two stacked clamping mechanisms in the parallel formation device are used to realize the rapid fixation of the battery and the adjustment of the battery formation pressure, and a horizontal corrector is added to make each parallel formation device in a horizontal state, avoiding the parallel formation device from tilting, resulting in uneven formation pressure of each battery, and causing the parallel formation device to adjust the formation pressure of each battery inaccurately, thereby reducing the consistency of the battery after formation, and even causing poor contact between the positive and negative ears of the battery and leakage of electrolyte during the battery formation process, thereby reducing the problem of battery formation qualification rate, improving the consistency of the battery after formation and improving the battery formation qualification rate.

[0124] The above embodiments only express several implementation methods of the present invention, and the descriptions thereof are relatively specific and detailed, but they cannot be understood as limiting the scope of the invention patent. It should be pointed out that, for those of ordinary skill in the art, several variations and improvements can be made without departing from the concept of the present invention, and these all belong to the protection scope of the present invention. Therefore, the protection scope of the patent of the present invention shall be subject to the attached claims.

Claims

1. A parallel formation device, characterized in that: It comprises at least two stacked clamping mechanisms, the two clamping mechanisms are used together to clamp the battery, and each of the clamping mechanisms comprises: A mounting plate, wherein the mounting plates of two adjacent clamping mechanisms are stacked, wherein a mounting cavity, a conducting groove and a sliding groove are provided in the mounting plate, wherein the mounting cavity is communicated with the conducting groove, and wherein a plurality of telescopic grooves are provided in the mounting plate, wherein the extension direction of each telescopic groove is the same as the extension direction of the conducting groove, and the opening direction of each telescopic groove is the same as the opening direction of the conducting groove; 14. The electrical connector of claim 13, wherein the first and second clamping members are configured to engage a first electrode and a second electrode, wherein the first electrode and the second clamping member are configured to engage a first electrode and a second electrode, and wherein the first electrode and the second electrode ... A pressure regulating component, the pressure regulating component includes a pressure regulating telescopic member and a lifting regulating member, the pressure regulating telescopic member is located in the mounting cavity and is elastically connected to the mounting plate, the pressure regulating telescopic member partially protrudes from the periphery of the mounting plate through the conducting groove, the pressure regulating telescopic member is also slidably connected to the mounting plate, the sliding direction of the pressure regulating telescopic member is the same as the extension direction of the conducting groove, the pressure regulating telescopic member includes an elastic member and a pressure block, the elastic member is arranged in the mounting cavity, the pressure block is located in the mounting cavity, and the pressure block partially protrudes from the conducting groove , one end of the elastic member is connected to the pressure block, the other end of the elastic member is connected to the inner wall of the mounting cavity, and the pressure block is slidably connected to the mounting plate; the lifting and lowering adjustment member includes a sliding block and a transmission group, the sliding block is arranged at the sliding groove and is slidably connected to the mounting plate, and the sliding block is connected to another stacked mounting plate, the transmission group is installed on the mounting plate, and the power output end of the transmission group is connected to the sliding block, the transmission group drives the sliding block to slide relative to the mounting plate, and the sliding direction of the sliding block is the same as the extension direction of the conducting groove; Among them, when the transmission group drives the sliding block to slide along the first direction relative to the mounting plate, the two adjacent mounting plates approach each other and the pressure regulating telescopic part contracts; when the transmission group drives the sliding block to slide along the second direction relative to the mounting plate, the two adjacent mounting plates move away from each other and the pressure regulating telescopic part extends.

2. The parallel formation device according to claim 1, characterized in that: The transmission group includes a motor, a first pulley, a second pulley, a transmission belt and a screw pair. The motor is mounted on the mounting plate, the first pulley is sleeved on the power output end of the motor, the second pulley is sleeved on the screw pair, the transmission belt is passed through the mounting plate and sleeved on the first pulley and the second pulley respectively, and the screw pair is rotatably connected to the sliding block.

3. The parallel formation device according to claim 1, characterized in that: The pressing block includes a clamping portion and an abutting portion, the clamping portion is clamped in the mounting cavity and slidably connected to the mounting plate, the clamping portion is connected to the abutting portion, the abutting portion is located in the conducting groove, and the abutting portion partially protrudes from the conducting groove, and the abutting portion is arranged corresponding to the second clamping piece of each clamping assembly.

4. The parallel formation device according to claim 3, characterized in that: The clamping portion and the abutting portion are an integrally formed structure.

5. The parallel formation device according to claim 4, characterized in that: The number of the conducting grooves and the abutting parts are both multiple, and the multiple abutting parts are arranged in a one-to-one correspondence in the multiple conducting grooves. The multiple abutting parts are all connected to the clamping parts, and the multiple abutting parts are arranged in a one-to-one correspondence with the second clamping members of the multiple clamping assemblies.

6. The parallel formation device according to any one of claims 1 to 5, characterized in that: The first clamping member of each clamping assembly further includes an insulator, and the insulator of the first clamping member of each clamping assembly is clamped between the corresponding positive electrode column and the corresponding negative electrode column.

7. A parallel formation device, characterized in that: It comprises a horizontal corrector, a shell and a parallel formation device as described in any one of claims 1 to 6, at least two stacked clamping mechanisms and the horizontal corrector are arranged in the shell, the horizontal corrector is connected to the mounting plate of any one of the clamping mechanisms, and the horizontal corrector is used to adjust the horizontality of the mounting plate.

8. A lithium ion battery, characterized in that: The product is obtained by using the parallel formation equipment described in claim 7.