A method for producing NLDMOS device and NLDMOS device

By adopting a low-resistance P+ substrate and Pwell layer structure in NLDMOS devices, the gate, drain and source regions are formed, and boron elements are injected at the bottom of the Pwell layer, thereby drawing out the Body electrode, which solves the large area and size of traditional NLDMOS devices. The problem of low reliability has achieved the reduction of device area and the improvement of reliability, meeting the requirements of high density and high reliability.

CN112510095BActive Publication Date: 2024-11-19PRIOSEMI TECH LTD CO
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202011384126.5
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2020-12-01
Publication Date
2024-11-19
Estimated Expiration
2040-12-01

AI Technical Summary

Technical Problem

Traditional NLDMOS devices have large areas and cannot meet the requirements for device density and area in high reliability applications, and the sampling resistance affects the standby time.

Method used

A low-resistance P+ type substrate is used to form an STI region and a Pwell layer, generate a gate, drain and source region, and inject boron elements into the bottom of the Pwell layer, thereby guiding the Body electrode out, reducing device area and improving reliability.

Benefits of technology

The area of ​​NLDMOS devices produced by this method is significantly reduced, which improves the reliability of the device, meets the requirements of high density and small area, and enhances the integration capability of current detection functions.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN112510095B_ABST
    Figure CN112510095B_ABST
Patent Text Reader

Abstract

The present invention provides a method for producing an NLDMOS device, and also provides an NLDMOS device obtained by the method. The method comprises first providing a P+ type substrate; then forming an STI region and a Pwell layer on both sides of the low-resistance P+ type substrate; then generating a gate region above the Pwell layer; then generating a drain region and a source region between the STI regions; finally, injecting a boron element at the bottom of the Pwell layer, then leading the electrode of the Body from the bottom of the Pwell layer, and forming a Body region; the area of ​​the NLDMOS device obtained by the method provided by the present invention is greatly reduced, so that the device with current detection function can be integrated.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the field of lithium battery protection, and in particular to a method for producing an NLDMOS device, and an NLDMOS device. Background Art

[0002] In the traditional CMOS and NMOS structures, the Body region is generally led out from the top of the device. In more and more high-reliability application scenarios, the lead-out density of the Body is also getting higher and higher. Therefore, how to achieve the ever-increasing density requirements for devices and reduce the area of ​​devices, provide devices that meet the requirements and methods for producing the devices are the problems that the present invention needs to solve. Summary of the invention

[0003] The invention provides a device for lithium battery protection, which solves the problem in the prior art that the resistance value of the sampling resistor affects the total resistance value in the loop, thereby causing the standby time of the whole device to decrease.

[0004] In order to solve the above technical problems, a technical solution adopted by the present invention is to provide a method for producing an NLDMOS device, comprising:

[0005] First, a low-resistance P+ substrate is provided;

[0006] Forming an STI region and a Pwell layer on both sides of the low-resistance P+ type substrate;

[0007] Generating a gate region above the Pwell layer;

[0008] generating a drain region and a source region between the STI regions;

[0009] Boron element is implanted at the bottom of the Pwell layer, and then the electrode of the Body is led out from the bottom of the Pwell layer to form a Body region.

[0010] Furthermore, the step of forming the STI region and the Pwell layer on both sides of the low-resistance P+ type substrate includes:

[0011] Etching STI regions at both sides of the low-resistance P+ substrate;

[0012] Filling the STI area and performing CMP polishing;

[0013] Pwell is injected into the low-resistance P+ substrate, and diffused through a thermal process to form a Pwell layer.

[0014] Furthermore, in the step of injecting Pwell into the low-resistance P+ substrate, the dose of Pwell injected is X / cm 2, the value of X is: 1e12≦X≦1e14.

[0015] Furthermore, the step of generating a gate region above the Pwell layer includes:

[0016] Growing a gate oxide on the upper surface of the P+ type substrate, wherein the thickness of the gate oxide is about 100 Å-150 Å;

[0017] Polysilicon is then deposited on the gate oxide, and the polysilicon is etched using a gate photomask to form the final gate.

[0018] Furthermore, the step of generating a drain region and a source region between the STI regions includes:

[0019] Implanting N+ on both sides of the STI region and the region between the gate to form N+ regions respectively;

[0020] The N+ region is subjected to a thermal process to diffuse and form an NDD structure;

[0021] N+ is implanted again, and then activated through a short RTA process to form the active area N+ region.

[0022] Furthermore, the step of injecting N+ between the STI region and the gate to form an N+ region includes:

[0023] Select phosphorus element to implant N+ between the STI region and the gate, with an implantation dose of K / cm 2 , the value of K is: 1e12≦K≦1e14.

[0024] Further, the step of injecting N+ again and then undergoing a short RTA process for activation to form an active area N+ region includes:

[0025] Arsenic is selected to be injected into N+ again, with an injection dose of N / cm 2 , the value of N is 1e14≦N≦1e15;

[0026] Then it undergoes a short RTA process to activate and form the active area N+ region.

[0027] Furthermore, the step of injecting boron into the bottom of the Pwell layer, and then leading the electrode of the Body out from the bottom of the Pwell layer to form the Body region includes:

[0028] Boron is injected into the bottom of the Pwell layer at a dose of M / cm 2 , the value of M is 1e13≦M≦1e15;

[0029] The electrode of the Body is led out from the bottom of the Pwell layer to form a Body region.

[0030] In order to solve the above technical problems, another technical solution adopted by the present invention is to provide an NLDMOS device, which is produced according to the above method for producing the NLDMOS device, and the NLDMOS device comprises:

[0031] Low resistance P+ type substrate;

[0032] A gate, a source electrode and a drain electrode respectively located on both sides of the gate;

[0033] The Body region is located at the bottom of the low-resistance P+ substrate;

[0034] The gate, the source and the drain are led out from the top of the low-resistance P+ type substrate; and the body region is led out from the bottom of the low-resistance P+ type substrate.

[0035] Furthermore, the current of the NLDMOS device flows in from the drain, passes through the body region, and then flows out from the source.

[0036] The beneficial effects of the present invention are as follows: the present invention provides a method for producing an NLDMOS device, and also provides an NLDMOS device obtained by the method. The method comprises first providing a low-resistance P+ type substrate; then forming an STI region and a Pwell layer on both sides of the low-resistance P+ type substrate; then generating a gate region above the Pwell layer; then generating a drain region and a source region between the STI regions; finally, injecting boron elements at the bottom of the Pwell layer, then leading the electrode of the Body out from the bottom of the Pwell layer, and forming a Body region; the area of ​​the NLDMOS device produced by the method provided by the present invention is greatly reduced, so that the device with current detection function can be integrated. BRIEF DESCRIPTION OF THE DRAWINGS

[0037] Figure 1 It is a schematic diagram of the structure of a traditional NLDMOS device;

[0038] Figures 2 to 7 It is a schematic diagram of the structure of the NLDMOS device presented in each step of the method for producing the NLDMOS device of the present invention;

[0039] Figure 8 It is a schematic diagram of the structure of the NLDMOS device in the present invention. DETAILED DESCRIPTION

[0040] In order to facilitate the understanding of the present invention, the present invention is described in more detail below in conjunction with the accompanying drawings and specific embodiments. Preferred embodiments of the present invention are provided in the accompanying drawings. However, the present invention can be implemented in many different forms and is not limited to the embodiments described in this specification. On the contrary, the purpose of providing these embodiments is to make the understanding of the disclosure of the present invention more thorough and comprehensive.

[0041] It should be noted that, unless otherwise defined, all technical and scientific terms used in this specification have the same meaning as those commonly understood by those skilled in the art of the present invention. The terms used in the specification of the present invention are only for the purpose of describing specific embodiments and are not intended to limit the present invention. The term "and / or" used in this specification includes any and all combinations of one or more related listed items.

[0042] like Figure 1 As shown, Figure 1 This is a schematic diagram of the structure of a traditional NLDMOS device. In the traditional NLDMOS device structure, Pwell is used as the substrate, and the gate, source, drain, and body are all drawn out from the surface of the NLDMOS device. The source and drain are located on both sides of the gate, and the other side of the source and drain are drawn out from the body. The body is drawn out from the P+ contact area of ​​the Pwell substrate, and the drain and gate are drawn out from the N+ contact area of ​​the Pwell substrate. The N+ contact area is located in the N-type well area. Shallow trench isolation (STI) areas are set between the P+ contact area and the N-type well area on both sides.

[0043] Traditional NLDMOS devices have large area and low reliability, and cannot meet the increasing requirements for NLDMOS devices. This embodiment provides a method for producing NLDMOS devices. The NLDMOS devices produced by this method have greatly reduced area and enhanced reliability, which can meet the high requirements for NLDMOS devices.

[0044] See also Figures 2 to 7 , which is a schematic diagram of the structure of the NLDMOS device presented in each step of the method for producing the NLDMOS device in this embodiment.

[0045] exist Figure 2 In the process, a low-resistance P+ substrate wafer is first provided as a substrate.

[0046] Then, an STI region and a Pwell layer are formed on the low-resistance P+ substrate. Specifically, the STI region is first etched on both sides of the low-resistance P+ substrate, and then the STI region is filled and CMP polished; then Pwell is injected into the aforementioned low-resistance P+ substrate, and diffused through a thermal process to form the final Pwell layer; wherein, in the step of injecting Pwell into the low-resistance P+ substrate, the dose of the injected Pwell is X / cm 2 , and the value of X is in the range of 1e12≦X≦1e14. The final device structure is as follows Figure 3 shown.

[0047] exist Figure 3 On the basis of the gate region, a gate region is generated. Specifically, a gate oxide is grown on the surface of the aforementioned low-resistance P+ substrate, wherein the thickness of the gate oxide is about 100A-150A; polysilicon is then deposited on the gate oxide, and finally the polysilicon is etched using a gate photomask to form the final gate. The final device structure is as follows Figure 4 shown.

[0048] exist Figure 4 Based on this, N+ is injected on both sides of the STI region and the region between the gate. In this embodiment, phosphorus is selected to inject N+, and no photomask is required. The injection dose is K / cm 2 , the value of K is: 1e12≦K≦1e14, forming an N+ region; when phosphorus is injected, it is doped with the gate polysilicon. The final device structure is as follows Figure 5 shown.

[0049] exist Figure 5 Based on this, phosphorus is injected into N+ to undergo a thermal process and diffuse to form an NDD structure; and N+ is injected again. This time, arsenic is selected for N+ injection, and the injection dose is N / cm 2 , the value of N is 1e14≦N≦1e15, and after a short RTA process, it is activated to form the active area N+ region. The final device structure is as follows Figure 6 shown.

[0050] exist Figure 6 On the basis of the active area N+ region, a hole is drilled, and a metal is deposited and etched to form a contact, and the drain and source are respectively led out from both sides. A large dose of boron is injected into the bottom of the Pwell layer to reduce the lead-out resistance. The injection dose is M, and the value of M ranges from 1e13≦M≦1e15; then the Body electrode is led out from the bottom of the Pwell layer to form the Body region, which is set at the bottom of the device. Figure 7 As shown, the structure of the NLDMOS device in the present invention is formed.

[0051] A method for producing an NLDMOS device provided in this embodiment provides a P+ type substrate, forms an STI region and a Pwell layer on both sides of the low-resistance P+ type substrate, generates a gate region above the Pwell layer, and generates a drain region and a source region between the STI regions, and finally injects boron elements at the bottom of the Pwell layer, and then leads the Body electrode from the bottom of the Pwell layer to form a Body region; the NLDMOS device finally produced has the Body lead-out at the bottom of the device, and the gate and drain are led out at the top of the device, which improves the reliability of the device on the one hand and reduces the area of ​​the device on the other hand, meeting the requirements of high-standard NLDMOS devices.

[0052] like Figure 8 As shown, a novel NLDMOS device proposed by the present invention is produced by the method for producing the NLDMOS device in the aforementioned embodiment. The NLDMOS device in this embodiment includes a low-resistance P+ type substrate, a gate, a source and a drain led out from the top of the low-resistance P+ type substrate, wherein the source and the drain are located on both sides of the gate; the Body region is located at the bottom of the low-resistance P+ type substrate, and the Body region is led out from the bottom of the low-resistance P+ type substrate. The Body region is led out at the bottom of the low-resistance P+ type substrate, while the source and the drain are led out at the top of the low-resistance P+ type substrate, which improves the reliability of the device on the one hand and reduces the area of ​​the device on the other hand.

[0053] Furthermore, the NLDMOS device in this embodiment includes a first N-type well region 101 and a second N-type well region 102, wherein the first N-type well region is provided with a first N+ contact region 103, and the second N-type well region is provided with a second N+ contact region 104; wherein the drain is led out from the first N+ contact region 103, and the source is led out from the second N+ contact region 104.

[0054] The NLDMO device further includes a first STI region 105 and a second STI region 106 , wherein the first STI region 105 is located on the other side of the first N-type well region 101 , and the second STI region 106 is located on the other side of the second N-type well region 102 .

[0055] The current flow path in the NLDMO device is as follows: the current flows into the Drain end of each device, passes downward through the Body area, and then flows upward from the Source end.

[0056] The NLDMOS device in this embodiment changes the Body region from being led out from the top of the low-resistance P+ substrate to being led out from the bottom of the low-resistance P+ substrate, and the Body region is flush with the edges of both sides of the low-resistance P+ substrate, and the source and drain are led out at the top of the low-resistance P+ substrate. This not only improves the reliability of the NLDMOS device, but also reduces the area of ​​the device, thereby providing conditions for the integration of multiple NLDMOS devices.

[0057] The above descriptions are merely embodiments of the present invention and are not intended to limit the patent scope of the present invention. Any equivalent structural transformations made using the contents of the present invention's specification and drawings, or directly or indirectly applied in other related technical fields, are also included in the patent protection scope of the present invention.

Claims

1. A method for producing an NLDMOS device, It is characterized in that The method comprises: First, a low-resistance P+ substrate is provided; Forming STI regions and Pwel l layers on both sides of the low-resistance P+ type substrate; Generating a gate region above the Pwell layer; Generating a drain region and a source region between the STI region and the gate region by two N+ implantations; Injecting boron element into the bottom of the Pwel 1 layer, and then leading the Body electrode out from the bottom of the Pwel 1 layer to form a Body region; The gate, the source and the drain are led out from the top of the low-resistance P+ type substrate; and the body region is led out from the bottom of the low-resistance P+ type substrate.

2. The method according to claim 1, It is characterized in that The step of forming the STI region and the Pwel l layer on both sides of the low-resistance P+ type substrate comprises: Etching STI regions at both sides of the low-resistance P+ substrate; Filling the STI area and performing CMP polishing; Pwel l is injected into the low-resistance P+ type substrate, and diffused through a thermal process to form a Pwel l layer.

3. The method according to claim 2, It is characterized in that The step of injecting Pwel l into the low-resistance P+ substrate is performed with a dose of X / cm 2 , the value of X is: 1e12≦X≦1e14.

4. The method according to claim 1, It is characterized in that The step of generating a gate region above the Pwell 1 layer comprises: Growing a gate oxide on the upper surface of the P+ type substrate, wherein the thickness of the gate oxide is 100 angstroms to 150 angstroms; Polysilicon is then deposited on the gate oxide, and the polysilicon is etched using a gate photomask to form the final gate.

5. The method according to claim 4, It is characterized in that The step of generating a drain region and a source region between the STI region and the gate region by two N+ implantations comprises: Implanting N+ on both sides of the STI region and the region between the gate to form N+ regions respectively; The N+ region is subjected to a thermal process to diffuse and form an NDD structure; N+ is implanted again, and then activated through a short RTA process to form the active area N+ region.

6. The method according to claim 5, It is characterized in that The step of implanting N+ between the STI region and the gate to form an N+ region comprises: Select phosphorus element to implant N+ between the STI region and the gate, with an implantation dose of K / cm 2 , the value of K is: 1e12≦K≦1e14.

7. The method according to claim 6, It is characterized in that The steps of injecting N+ again and then activating by a short RTA process to form an active area N+ region include: Arsenic is selected to be injected into N+ again, with an injection dose of N / cm 2 , the value of N is 1e14≦N≦1e15; Then it undergoes a short RTA process to activate and form the active area N+ region.

8. The method according to claim 1, It is characterized in that The step of injecting boron element into the bottom of the Pwel 1 layer, then leading the electrode of the Body out from the bottom of the Pwel 1 layer, and forming the Body region includes: Boron is injected into the bottom of the Pwel l layer at a dose of M / cm 2 , the value of M is 1e13≦M≦1e15; The Body electrode is led out from the bottom of the Pwel l layer to form a Body region.

9. An NLDMOS device, It is characterized in that The NLDMOS device is produced by any one of the production methods described in claim 1 to claim 8, and the NLDMOS device comprises: Low resistance P+ type substrate; A gate, a source electrode and a drain electrode respectively located on both sides of the gate; The Body region is located at the bottom of the low-resistance P+ substrate; The gate, the source and the drain are led out from the top of the low-resistance P+ type substrate; and the body region is led out from the bottom of the low-resistance P+ type substrate.

10. The NLDMOS device according to claim 9, It is characterized in that The current of the NLDMOS device flows in from the drain, passes through the body region, and then flows out from the source.