A dental implant structure and a method for manufacturing the same
By introducing a braided carbon fiber buffer layer and a titanium alloy bearing layer into the dental implant structure, combining multiple layers of carbon fiber and titanium composite connecting layer, the problem of traditional dental implants being subjected to force during vigorous occlusal is solved, and the service life and wear of dental implants are improved. Comfort.
Patent Information
- Application Number
- CN202011446836.6
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2020-12-11
- Publication Date
- 2024-11-08
- Estimated Expiration
- 2040-12-11
AI Technical Summary
When traditional dental implants have single or multiple powerful occlusals, the occlusal force is transmitted to the implant through a force conduction effect, which may lead to a broken neck of the implant or a broken crown. The existing technology is difficult to effectively solve this problem.
Design a dental implant structure, including a crown, abutment and implant, the abutment consists of a buffer layer and a bearing layer. The buffer layer is a braided carbon fiber buffer layer and a crown connected to the crown. The bearing layer is titanium or titanium alloy material, and is implanted The body is connected, and the connecting layer is provided in the middle of the composite material of multi-layer carbon fiber and titanium. It is manufactured through 3D printing technology to achieve buffering effect.
The energy absorption effect of the buffer layer disperses the stress between the crown and the implant, improves the service life of the implant and the crown, reduces weight, and improves the wear comfort of the patient.
Smart Images

Figure CN112618069B_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the technical field of dental implants, and in particular to a dental implant structure and a manufacturing method thereof. Background Art
[0002] Currently, dental implants are usually divided into three parts: implant, abutment and crown. The implant is used to be implanted in the jawbone below the gums to play a load-bearing role, usually made of metal or ceramic materials. The abutment is connected to the implant through a slot and reinforced with screws, usually made of metal materials. The crown is a structure that performs the chewing function and is bonded to the top of the abutment with resin cement, usually made of ceramic, resin or metal materials. The crown of a traditional dental implant is directly connected to the abutment, and a bite force is generated during a single or multiple strong bites or chewing. This force will be transmitted to the implant through the force conduction effect and cause great pressure on the implant, and may cause the neck of the implant to break or cause loss of adjacent teeth. Therefore, the strength of the crown needs to be continuously improved to increase its lifespan. Summary of the invention
[0003] One of the purposes of the present invention is to provide a dental implant structure to avoid the deficiencies in the prior art, solve the problem of damage to the implant or crown caused by multiple or single direct impacts in the prior art, and improve the phenomenon of implant breakage or crown collapse. Another purpose of the present invention is to provide a method for manufacturing a dental implant structure, which can manufacture a dental implant structure with a buffering effect.
[0004] One of the purposes of the present invention is achieved through the following technical solutions:
[0005] A dental implant structure comprises a crown, a base and an implant, wherein the base comprises a buffer layer and a bearing layer, the buffer layer is a woven carbon fiber buffer layer and is connected to the crown, and the bearing layer is connected to the implant.
[0006] Furthermore, the braided carbon fiber buffer layer is a multi-layer structure, and the thickness of the braided carbon fiber buffer layer is 20%-30% of the thickness of the base.
[0007] Furthermore, the buffer layer is provided with a first clamping block, the dental crown is provided with a first clamping groove matching the first clamping block, the bearing layer is provided with a second clamping block, and the implant is provided with a second clamping groove matching the second clamping block.
[0008] Furthermore, a first buffer component and a second buffer component are respectively disposed outside the first clamping block and the second clamping block, and the first buffer component and the second buffer component are one or more of springs, foams and sponges.
[0009] Furthermore, the bearing layer is a titanium or titanium alloy material layer, and the thickness of the bearing layer is 20%-30% of the thickness of the base.
[0010] Furthermore, a connecting layer is provided between the buffer layer and the bearing layer, and the connecting layer is a composite material of multiple layers of carbon fiber and titanium or a composite material of multiple layers of carbon fiber and titanium alloy, and the thickness of the connecting layer is 40%-55% of the thickness of the base.
[0011] Furthermore, the carbon fiber content in the connecting layer decreases gradually, and the titanium or titanium alloy content in the connecting layer increases gradually.
[0012] Furthermore, the woven carbon fiber buffer layer, connecting layer and bearing layer are all multi-layer structures, the single layer thickness of the woven carbon fiber buffer layer is 50μm-100μm, the single layer thickness of the connecting layer is 100μm-200μm, and the single layer thickness of the bearing layer is 100μm-200μm.
[0013] The second object of the present invention is achieved by the following technical solutions:
[0014] A method for manufacturing a dental implant structure comprises the following steps:
[0015] S1. Crown production: through 3D scanning and modeling in 3Shape;
[0016] S2. Buffer layer production: The buffer layer is a braided carbon fiber buffer layer. The braided carbon fiber buffer layer is three-dimensionally modeled by matching the inner surface of the crown, and is manufactured layer by layer through 3D printing. The carbon fiber material is manufactured by a three-dimensional multi-directional braiding method. The angle between the braided structures is 45° to 135°. The thickness of the braided carbon fiber buffer layer is 20%-30% of the thickness of the base.
[0017] S3. Bearing layer production: The bearing layer is a dense structure layer of titanium or titanium alloy material, which is manufactured layer by layer through 3D printing technology. The thickness of the bearing layer is 20%-30% of the thickness of the base.
[0018] S4. Preparation of connecting layer: The connecting layer is a composite material of multiple layers of carbon fiber material and titanium or a composite material layer of multiple layers of carbon fiber and titanium alloy. The carbon fiber material is sprayed or extruded from a nozzle, and the titanium or titanium alloy material is sprayed or extruded from another nozzle. The carbon fiber content decreases in a gradient, and the titanium or titanium alloy content increases in a gradient. The thickness of the connecting layer is 40%-55% of the thickness of the base.
[0019] Furthermore, the connecting layer in step S4 is normally embedded between the woven carbon fiber buffer layer and the bearing layer.
[0020] It can be seen from the above scheme that the present invention has the following beneficial effects: the base in a dental implant structure of the present invention includes a buffer layer and a bearing layer, the buffer layer provides a buffer for the crown and the implant, and disperses the force on the crown and the implant, the buffer layer is a woven carbon fiber buffer layer, and the energy absorption effect of the woven carbon fiber buffer layer reduces the force on the implant and increases the service life of the implant, and the woven carbon fiber material is light, which makes the weight of the dental implant structure lighter.
[0021] Furthermore, a method for manufacturing a dental implant structure of the present invention is based on the existing 3D printing technology and can produce a dental implant structure with a buffering effect. The buffer layer reduces the force between the dental implant and the crown, thereby increasing the service life of the dental implant structure; it disperses the force on the dental implant structure and improves the wearing comfort of the patient. BRIEF DESCRIPTION OF THE DRAWINGS
[0022] The invention is further described using the accompanying drawings, but the embodiments in the accompanying drawings do not constitute any limitation to the invention. A person skilled in the art can obtain other drawings based on the following drawings without creative work.
[0023] Figure 1 This is an exploded view of a dental implant structure provided by the present invention.
[0024] Figure 2 yes Figure 1 Schematic diagram of the structure of the base.
[0025] Figure 3 It is an assembly diagram of a dental implant structure provided by the present invention.
[0026] The reference numerals are as follows:
[0027] 1. Crown; 2. Abutment; 3. Implant; 21. First clamping block; 22. Buffer layer; 23. Connecting layer; 24. Bearing layer; 211. First buffer member; 241. Second clamping block; 2411. Second buffer member. DETAILED DESCRIPTION
[0028] In order to enable those skilled in the art to better understand the scheme of the present invention, the technical scheme in the embodiments of the present invention will be clearly and completely described below in conjunction with the drawings in the embodiments of the present invention. Obviously, the described embodiments are only embodiments of a part of the present invention, rather than all embodiments.
[0029] like Figure 1 and Figure 3As shown, a dental implant structure of this embodiment includes a crown 1, a base 2 and an implant 3, wherein the base 2 includes a buffer layer 22 and a bearing layer 24, the buffer layer 22 is a woven carbon fiber buffer layer and is connected to the crown 1, and the bearing layer 24 is connected to the implant 3.
[0030] In this embodiment, a woven carbon fiber buffer layer is provided. The energy absorption effect of the woven carbon fiber buffer layer reduces the force on the implant 3 and increases the service life of the implant 3. In addition, the breakage of the crown 1 due to excessive stress is reduced, thereby increasing the service life of the crown 1.
[0031] Specifically, Figure 2 As shown, the thickness of the woven carbon fiber buffer layer is 20%-30% of the thickness of the base 2, the buffer layer 22 is provided with a first clamping block 21, and the crown 1 is provided with a first clamping groove matching the first clamping block 21, and the depth of the first clamping groove is slightly greater than the height of the first clamping block 21. The connection between the buffer layer 22 and the crown 1 is achieved through the cooperation of the first clamping block 21 and the first clamping groove. Furthermore, a first buffer component 211 is provided on the outside of the first clamping block 21, and the first buffer component 211 is one or more of a spring, foam and sponge.
[0032] Furthermore, the first clamping block 21 is made of the same carbon fiber material as the braided carbon fiber buffer layer and is integrally formed during manufacturing.
[0033] In this embodiment, if Figure 2 As shown, the bearing layer 24 is a titanium or titanium alloy material layer, and the thickness of the bearing layer 24 is 20%-30% of the thickness of the base 2. The bearing layer 24 is provided with a second clamping block 241, and the upper surface of the implant 3 is provided with a second clamping groove matching the second clamping block 241. The depth of the second clamping groove is slightly greater than the height of the second clamping block 241. The outside of the second clamping block 241 is also provided with a second buffer 2411. In this embodiment, the second buffer 2411 is also one or more of a spring, foam and sponge. The second clamping block 241 and the bearing layer 24 are integrally formed.
[0034] like Figure 2 As shown, in this embodiment, a connecting layer 23 is provided between the buffer layer 22 and the bearing layer 24. The connecting layer 23 is a composite material of multiple layers of carbon fiber and titanium or a composite material of multiple layers of carbon fiber and titanium alloy. The thickness of the connecting layer 23 is 40%-55% of the thickness of the base 2. The connecting layer 23 can prevent the buffer layer 22 and the bearing layer 24 from falling off, thereby achieving a firm connection between the buffer layer 22 and the bearing layer 24.
[0035] Furthermore, the carbon fiber content in the connecting layer 23 decreases gradually, and the titanium or titanium alloy content in the connecting layer 23 increases gradually. For example, the carbon fiber material content decreases from 100% to 0% layer by layer, and at the same time, the titanium or titanium alloy material content increases from 0% to 100% layer by layer. The gradient changes of the two materials can achieve better fusion and play a good transition role.
[0036] like Figure 2 As shown, the buffer layer 22, the connecting layer 23 and the bearing layer 24 are all multi-layer structures, the single layer thickness of the buffer layer 22 is 50μm-100μm, the single layer thickness of the connecting layer 23 is 100μm-200μm, and the single layer thickness of the bearing layer 24 is 100μm-200μm. The woven carbon fiber buffer layer can be stretched and deformed along the normal direction and can be restored to the original woven state.
[0037] Another aspect of the present invention provides a method for manufacturing a dental implant structure, comprising the following steps:
[0038] S1. Crown 1 production: through 3D scanning and modeling in 3Shape;
[0039] S2. Preparation of buffer layer 22: The buffer layer 22 is a braided carbon fiber buffer layer. The braided carbon fiber buffer layer is three-dimensionally modeled by matching the inner surface of the crown 1, and is manufactured layer by layer through 3D printing. The carbon fiber material is manufactured by a three-dimensional multi-directional braiding method. The angle between the braided structures is 45° to 135°. The thickness of the braided carbon fiber buffer layer is 20%-30% of the thickness of the base 2.
[0040] S3, manufacturing of the bearing layer 24: the bearing layer 24 is a dense structure layer of titanium or titanium alloy material, which is manufactured layer by layer by 3D printing technology. The thickness of the bearing layer 24 is 20%-30% of the thickness of the base;
[0041] S4. Preparation of connecting layer 23: The connecting layer 23 is a composite material of multiple layers of carbon fiber material and titanium or a composite material layer of multiple layers of carbon fiber and titanium alloy. The carbon fiber material is sprayed or extruded from a nozzle, and the titanium or titanium alloy material is sprayed or extruded from another nozzle. The carbon fiber content decreases in a gradient, and the titanium or titanium alloy content increases in a gradient. The thickness of the connecting layer 23 is 40%-55% of the thickness of the base.
[0042] Furthermore, the connection layer 13 in step S4 is normally embedded between the buffer layer 22 and the bearing layer 24, which effectively avoids possible slippage and other phenomena and achieves a firm connection.
[0043] The present invention provides a method for manufacturing a dental implant structure based on the existing 3D printing technology, and can manufacture a dental implant structure with a buffering effect. The buffer layer reduces the force between the dental implant and the crown, thereby increasing the service life of the dental implant structure; the force on the dental implant structure is dispersed, thereby improving the wearing comfort of the patient.
[0044] Finally, it should be noted that the above embodiments are only used to illustrate the technical solution of the present invention, rather than to limit the scope of protection of the present invention. Although the present invention has been described in detail with reference to the preferred embodiments, those skilled in the art should understand that the technical solution of the present invention can be modified or replaced by equivalents without departing from the essence and scope of the technical solution of the present invention.
Claims
1. A dental implant structure, comprising a crown, an abutment and an implant, characterized in that: The base includes a buffer layer and a bearing layer, the buffer layer is a woven carbon fiber buffer layer and is connected to the tooth crown, and the bearing layer is connected to the implant; the thickness of the woven carbon fiber buffer layer is 20%-30% of the thickness of the base; a connecting layer is provided between the buffer layer and the bearing layer, the connecting layer is a composite material of multiple layers of carbon fiber and titanium or a composite material of multiple layers of carbon fiber and titanium alloy, and the thickness of the connecting layer is 40%-55% of the thickness of the base; the carbon fiber content in the connecting layer decreases gradually, and the titanium or titanium alloy content in the connecting layer increases gradually; the woven carbon fiber buffer layer, the connecting layer and the bearing layer are all multi-layer structures, the single layer thickness of the woven carbon fiber buffer layer is 50μm-100μm, the single layer thickness of the connecting layer is 100μm-200μm, and the single layer thickness of the bearing layer is 100μm-200μm.
2. A dental implant structure according to claim 1, characterized in that: The buffer layer is provided with a first clamping block, and the dental crown is provided with a first clamping groove matching the first clamping block; the bearing layer is provided with a second clamping block, and the implant is provided with a second clamping groove matching the second clamping block.
3. A dental implant structure according to claim 2, characterized in that: A first buffer component and a second buffer component are respectively disposed outside the first clamping block and the second clamping block. The first buffer component and the second buffer component are one or more of springs, foams and sponges.
4. A dental implant structure according to claim 1, characterized in that: The bearing layer is a titanium or titanium alloy material layer, and the thickness of the bearing layer is 20%-30% of the thickness of the base.
5. A method for manufacturing a dental implant structure, characterized in that: Used to make a dental implant structure as claimed in any one of claims 1 to 4, comprising the following steps: S1. Crown production: through 3D scanning and modeling in 3Shape; S2. Buffer layer production: The buffer layer is a braided carbon fiber buffer layer. The braided carbon fiber buffer layer is three-dimensionally modeled by matching the inner surface of the crown, and is manufactured layer by layer through 3D printing. The carbon fiber material is manufactured by a three-dimensional multi-directional braiding method. The angle between the braided structures is 45° to 135°. The thickness of the braided carbon fiber buffer layer is 20%-30% of the thickness of the base. S3. Bearing layer production: The bearing layer is a dense structure layer of titanium or titanium alloy material, which is manufactured layer by layer through 3D printing technology. The thickness of the bearing layer is 20%-30% of the thickness of the base. S4. Preparation of connecting layer: The connecting layer is a composite material of multiple layers of carbon fiber material and titanium or a composite material layer of multiple layers of carbon fiber and titanium alloy. The carbon fiber material is sprayed or extruded from a nozzle, and the titanium or titanium alloy material is sprayed or extruded from another nozzle. The carbon fiber content decreases in a gradient, and the titanium or titanium alloy content increases in a gradient. The thickness of the connecting layer is 40%-55% of the thickness of the base.
6. The method for manufacturing a dental implant structure according to claim 5, characterized in that: The connecting layer in step S4 is normally embedded between the woven carbon fiber buffer layer and the bearing layer.