Semiconductor device and manufacturing method

By forming a plurality of bumps on the semiconductor substrate and setting appropriate lens material openings, the problems of low semiconductor chip bonding efficiency and poor accuracy are solved, and efficient and accurate chip bonding are achieved and the heat treatment time is shortened.

CN112687712BActive Publication Date: 2024-11-15SONY GROUP CORP
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202011526090.X
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Priority Date
2015-03-05
Filing Date
2016-02-22
Publication Date
2024-11-15
Estimated Expiration
2036-02-22

AI Technical Summary

Technical Problem

In the prior art, bonding of semiconductor chips is difficult to achieve, especially in the presence of lens materials, resulting in low bonding efficiency and poor accuracy, and long heat treatment time, which affects production efficiency and equipment performance.

Method used

A plurality of bumps are formed on the semiconductor substrate, and openings are provided in the area of ​​the lens material around it, so that the distance between the lens material and the bump is greater than twice the diameter of the bump, ensuring solder embedding and shape accuracy, reducing the The influence of lens material improves bonding efficiency.

Benefits of technology

Through this method, efficient bonding of semiconductor chips is achieved, bonding time is shortened, heat treatment load is reduced, and the production efficiency and accuracy of the equipment are improved.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN112687712B_ABST
    Figure CN112687712B_ABST
Patent Text Reader

Abstract

The present invention provides a semiconductor device, comprising: a first semiconductor substrate having a rectangular shape; a second semiconductor substrate having a rectangular shape, wherein the area of ​​the second semiconductor substrate is smaller than that of the first semiconductor substrate, and at least a first edge region of the second semiconductor substrate is flush with at least a first edge region of the first semiconductor substrate; and a third semiconductor substrate having a rectangular shape, wherein the area of ​​the third semiconductor substrate is smaller than that of the first semiconductor substrate, and at least a first edge region of the third semiconductor substrate is flush with at least a second edge region of the first semiconductor substrate.
Need to check novelty before this filing date? Find Prior Art

Description

[0001] This application is a divisional application of patent application No. 201680005481.2, filed on February 22, 2016, with the invention name “Semiconductor device, manufacturing method and electronic device”.

[0002] CROSS-REFERENCE TO RELATED APPLICATIONS

[0003] This application claims the benefit of Japanese Priority Patent Application JP 2015-043553 filed on Mar. 5, 2015, which is hereby incorporated by reference herein in its entirety. Technical Field

[0004] The present disclosure relates to a semiconductor device, a manufacturing method, and an electronic device, and in particular, to a semiconductor device, a manufacturing method, and an electronic device that allow easy bonding of semiconductor chips. Background Art

[0005] A technology for electrically connecting semiconductor chips is designed, which allows a connection portion to have multiple pins and lower capacitance by flip-chip bonding using bumps, and improves the data exchange speed between semiconductor chips compared to connections using wire bonding in the prior art (for example, see PTL 1).

[0006] As an application of this technology, there is a technology for stacking a peripheral circuit on the light collecting surface side of a surface-type solid-state imaging device by flip-chip bonding. Flip-chip bonding on the light collecting surface side of a surface-type solid-state imaging device requires forming bumps on the light collecting surface. However, a light collecting structure called an on-chip lens is formed on the light collecting surface, and lens materials such as organic substances that form these on-chip lenses are stacked on the entire light collecting surface including the peripheral circuit area and the pixel area. Therefore, in order to connect the bump to the bump connection electrode pad formed on the semiconductor substrate, an opening is formed in the lens material, and a bump is formed on the opening.

[0007] In this case, the depth of the opening increases by the thickness of the lens material, which makes it difficult to form a high-precision bump. This applies not only to solid-state imaging devices but also to components using a resin such as polyimide as a protective film.

[0008] As described above, in the case where the lens material exists in the region where the bump is formed, bonding of the semiconductor chip cannot be easily performed.

[0009] On the other hand, there is a solid-state imaging device in which a first semiconductor chip and a second semiconductor chip are stacked so as to face each other and be bonded to each other via bumps, wherein a photoelectric conversion element and connecting electrodes are formed in the first semiconductor chip, and an A / D conversion circuit, a signal processing circuit, a logic operation circuit, etc. and a collecting electrode are formed in the second semiconductor chip.

[0010] The number of pixels of a solid-state imaging device used in a camera or the like is generally in the millions to tens of millions, and therefore a large number of connection electrodes are required; the connection electrodes are arranged at a high density of a pitch of several tens of micrometers.

[0011] In order to accurately connect connection electrodes arranged at a high density, it is necessary to arrange alignment marks on each of the first semiconductor chip and the second semiconductor chip, and perform bump bonding while performing accurate alignment based on the alignment marks.

[0012] Bump bonding methods include chip-on-chip bonding methods (for example, see PTL 2) and chip-on-wafer bonding methods (for example, see PTL 3). The chip-on-chip bonding method is a method of bonding semiconductor chips in units of semiconductor chips, which has low bonding efficiency and is not suitable for mass production.

[0013] The chip-on-wafer bonding method is a method of bonding a plurality of second semiconductor chips to a semiconductor wafer, wherein the first semiconductor chips are arranged in a matrix form on the semiconductor wafer. Although this method improves the bonding efficiency compared to the chip-on-chip bonding method, in the case where the second semiconductor chips are bonded to the semiconductor wafer one by one, the time taken for bonding each semiconductor wafer is extended in proportion to the number of second semiconductor chips to be bonded. This not only leads to a decrease in production volume, but also prolongs the time of the heat treatment required for bump bonding, thereby increasing the heat load on the semiconductor wafer.

[0014] In the case of bonding a plurality of second semiconductor chips together to a semiconductor wafer, although the number of bonding times per semiconductor wafer is reduced, and thus the time taken for bonding is shortened, a design restriction is imposed in advance that the semiconductor chip has a symmetry axis by mirror inversion (for example, see PTL 4 and 5). However, since the solid-state imaging device obtains an image signal from a lens image projected onto the first semiconductor chip, the physical configuration such as east, south, west, north, etc. cannot be easily changed. In other words, it is difficult to impose design restrictions such as mirror inversion. Therefore, the bonding of semiconductor chips cannot be easily performed.

[0015] [Citation List]

[0016] [Patent Document]

[0017] PTL 1: JP 2006-49361A

[0018] PTL 2: JP 2011-243612A

[0019] PTL 3: JP 2001-196528A

[0020] PTL 4: JP 2001-168383A

[0021] PTL 5: JP 2012-503884T Summary of the invention

[0022] [Technical issues]

[0023] As described above, bonding of semiconductor chips cannot be performed easily.

[0024] The present disclosure, which has been completed in view of such circumstances, enables easy bonding of semiconductor chips.

[0025] [Solution to the problem]

[0026] According to a first embodiment of the present disclosure, a semiconductor device is provided, comprising: a plurality of bumps on a first semiconductor substrate; and a lens material in an area outside the plurality of bumps on the first semiconductor substrate, wherein a distance between a side of a bump closest to the lens material closest to the lens material and a side of the lens material closest to the bump is greater than twice a diameter of the bump closest to the lens material, and wherein a distance between a side of a bump closest to the lens material closest to the lens material and a side of the lens material closest to the bump is greater than a minimum spacing between the bumps.

[0027] The electronic device according to the first embodiment of the present disclosure corresponds to the semiconductor device according to the first embodiment of the present disclosure.

[0028] According to a second embodiment of the present disclosure, a method for manufacturing a semiconductor device is provided, comprising: forming a plurality of bumps on a first semiconductor substrate, and forming a lens material in an area outside the plurality of bumps on the first semiconductor substrate, wherein a distance between a side of a bump closest to the lens material closest to the lens material and a side of the lens material closest to the bump is greater than twice a diameter of the bump closest to the lens material, and wherein a distance between a side of a bump closest to the lens material closest to the lens material and a side of the lens material closest to the bump is greater than a minimum spacing between the bumps.

[0029] According to a third embodiment of the present disclosure, a semiconductor device is provided, comprising: a first semiconductor substrate having a rectangular shape; a second semiconductor substrate having a rectangular shape, wherein the area of ​​the second semiconductor substrate is smaller than that of the first semiconductor substrate, and at least a portion of a first edge of the second semiconductor substrate is flush with at least a portion of a first edge of the first semiconductor substrate; and a third semiconductor substrate having a rectangular shape. The area of ​​the third semiconductor substrate is smaller than that of the first semiconductor substrate, and at least a portion of a first edge of the third semiconductor substrate is flush with at least a portion of a second edge of the first semiconductor substrate.

[0030] The electronic device according to the third embodiment of the present disclosure corresponds to the semiconductor device according to the third embodiment of the present disclosure.

[0031] In a third embodiment of the present disclosure, the first semiconductor substrate includes a pixel array, and the second semiconductor substrate and the third semiconductor substrate each include at least one logic circuit. Each of the first edge of the first semiconductor substrate and the first edge of the second semiconductor substrate corresponds to a scribe line forming a first edge of a stacked semiconductor device. Each of the second edge of the first semiconductor substrate and the first edge of the third semiconductor substrate corresponds to a scribe line forming a second edge of a stacked semiconductor device.

[0032] According to a fourth embodiment of the present disclosure, a method for manufacturing a semiconductor device is provided, the method comprising: bonding a first semiconductor substrate including a plurality of logic circuits to a second semiconductor substrate and a third semiconductor substrate arranged in an array in a semiconductor wafer, wherein each of the second semiconductor substrate and the third semiconductor substrate comprises a pixel array. The first semiconductor substrate spans the second semiconductor substrate and the third semiconductor substrate. The method further comprises cutting a first edge of the first semiconductor substrate and a first edge of the second semiconductor substrate so that the first edge of the first semiconductor substrate and the first edge of the second semiconductor substrate are flush with each other.

[0033] In a fourth embodiment of the present disclosure, a fourth semiconductor substrate including a plurality of logic circuits may be bonded to a second semiconductor substrate and a fifth semiconductor substrate, wherein the fourth semiconductor substrate spans the second semiconductor substrate and the fifth semiconductor substrate. The method may further include cutting a second edge of the second semiconductor substrate and a first edge of the fourth semiconductor substrate so that the second edge of the second semiconductor substrate and the first edge of the fourth semiconductor substrate are flush with each other. In this embodiment, a semiconductor device is formed in which the first edge of the first semiconductor substrate and the first edge of the second semiconductor substrate are flush with each other. In addition, the second edge of the second semiconductor substrate and the first edge of the fourth semiconductor substrate may be flush with each other.

[0034] [Beneficial Effects of the Invention]

[0035] According to the first and third embodiments of the present disclosure, bonding of semiconductor chips can be easily performed.

[0036] According to the second embodiment of the present disclosure, a semiconductor device that allows semiconductor chips to be easily bonded can be manufactured.

[0037] It should be noted that the effects described here are not necessarily restrictive, and any effects desired to be described in the present disclosure may be exhibited. BRIEF DESCRIPTION OF THE DRAWINGS

[0038] Figure 1 is a block diagram showing an example configuration of a first embodiment of a CMOS image sensor as a semiconductor device to which the present disclosure is applicable;

[0039] Figure 2 It shows Figure 1 A diagram of a first example structure of a CMOS image sensor;

[0040] Figure 3 Is a description Figure 2 An overview of a method for manufacturing a CMOS image sensor;

[0041] Figure 4 is a diagram describing details of a method for forming a bump;

[0042] Figure 5 is a diagram showing an example structure of a bump when a lens material is stacked on the entire surface of the light irradiation side of a semiconductor chip;

[0043] Figure 6 It shows Figure 1 A cross-sectional view of a second example structure of a CMOS image sensor;

[0044] Figure 7 It is schematically shown Figure 1 A cross-sectional view of a third example structure of a CMOS image sensor;

[0045] Figure 8 It is schematically shown Figure 1 A cross-sectional view of a fourth example structure of a CMOS image sensor;

[0046] Fig. 9 is a diagram illustrating an example of an opening region;

[0047] Fig.10 is a diagram illustrating another example of an opening region;

[0048] Fig.11 It shows Figure 7 A diagram of an example of the shape of a region;

[0049] Fig.12 It shows Figure 7 A diagram of another example of the shape of a region;

[0050] Fig.13 It shows Figure 7 A diagram showing another example of the shape of the region;

[0051] Fig.14 is an overview diagram showing an example configuration of a second embodiment of a CMOS image sensor to which the present disclosure is applied;

[0052] Fig.15 It shows Fig.14 A perspective view of an example configuration of a CMOS image sensor before dicing;

[0053] Fig.16 It is along Fig.15 The cross-section of AA in ;

[0054] Fig.17 is a diagram showing an example structure of a CMOS image sensor in which a north chip and a south chip are formed separately;

[0055] Fig.18 Is a description Fig.14 A perspective view of a method for manufacturing a CMOS image sensor;

[0056] Fig.19 is a block diagram showing an example configuration of an imaging device as an electronic device to which an embodiment of the present disclosure is applicable;

[0057] Fig. 20 FIG. 1 is a diagram showing an application example of the above-mentioned CMOS image sensor. DETAILED DESCRIPTION

[0058] Hereinafter, a mode for implementing the present disclosure (hereinafter referred to as an embodiment) will be described. The description will be made in the following order.

[0059] 1. First Implementation: CMOS Image Sensor ( Figure 1-13 )

[0060] 2. Second Implementation: CMOS Image Sensor ( Figure 14-18 )

[0061] 3. Third embodiment: Imaging device ( Fig.19 )

[0062] 4. Application examples of CMOS image sensors ( Fig. 20 )

[0063] <First embodiment>

[0064] (Example Configuration of First Embodiment of CMOS Image Sensor)

[0065] Figure 1 is a block diagram showing an example configuration of a first embodiment of a complementary metal oxide semiconductor (CMOS) image sensor as a semiconductor device to which the present disclosure is applicable.

[0066] The CMOS image sensor 10 includes a semiconductor chip 11 and a semiconductor chip 12 connected via bumps 13. The semiconductor chip 11 and the semiconductor chip 12 each include a semiconductor substrate (eg, a silicon substrate) and a metal wiring layer of Cu, Al, or the like.

[0067] A pixel region 21, a pixel driving line 22, a vertical signal line 23, a vertical driving unit 24, a column processing unit 25-1, and a system control unit 27 are formed on the semiconductor chip 11. A column processing unit 25-2, a horizontal driving unit 26, and a memory and signal processing unit 28 are formed on the semiconductor chip 12.

[0068] In the pixel region 21, pixels are arranged in a two-dimensional matrix form for imaging, and each pixel includes a photoelectric conversion element that generates a charge amount equivalent to the light amount of incident light and accumulates the charge inside. In addition, a pixel drive line 22 is formed in each pixel row in the matrix in the pixel region 21, and a vertical signal line 23 is formed in each pixel column.

[0069] The vertical driving unit 24 includes a shift register, an address decoder, and the like, and drives the pixels in the pixel area 21, for example, in units of rows. One terminal of the pixel driving line 22 is connected to an output terminal not shown, which corresponds to each row of the vertical driving unit 24. Although the specific structure of the vertical driving unit 24 is not shown, the vertical driving unit 24 includes two scanning systems, a readout scanning system and a sweep scanning system.

[0070] The readout scanning system sequentially selects each row, thereby sequentially reading out pixel signals from pixels in row units, and outputs a selection signal, etc. from an output terminal connected to the pixel drive line 22 of the selected row. Thus, an electric signal of the charge accumulated in the photoelectric conversion element of the pixel in the row selected by the readout scanning system is read out as a pixel signal and supplied to the vertical signal line 23.

[0071] The clean-up scanning system outputs a reset signal from the output terminal connected to the pixel drive line 22 of each row earlier than the scanning performed by the readout scanning system by a time period corresponding to the shutter speed, so as to clear (reset) unnecessary charges from the photoelectric conversion element. By this scanning performed by the clean-up scanning system, the so-called electronic shutter operation is performed sequentially row by row. Here, the electronic shutter operation refers to an operation of discharging the charge of the photoelectric conversion element and restarting exposure (starting to accumulate charge).

[0072] The column processing unit 25-1 is a part of the signal processing circuit provided for each column of the pixel area 21, and the column processing unit 25-2 is another part. The column processing unit 25-1 and the column processing unit 25-2 are connected to each other via the bump 13 to form a signal processing circuit provided for each column of the pixel area 21. Each signal processing circuit performs signal processing such as A / D conversion processing and correlated double sampling (CDS) processing on the pixel signal output from the pixel of the selected row through the vertical signal line 23. Each signal processing circuit temporarily retains the pixel signal after the signal processing.

[0073] The horizontal drive unit 26 includes a shift register and an address decoder, etc., and sequentially selects the signal processing circuit of each column. Through this selection scanning performed by the horizontal drive unit 26, the pixel signals that have undergone signal processing by each signal processing circuit are sequentially output to the memory and signal processing unit 28.

[0074] The system control unit 27 includes a timing generator that generates various timing signals, etc. The system control unit 27 generates control signals for controlling the vertical driving unit 24, the column processing unit 25-1, the column processing unit 25-2, and the horizontal driving unit 26 based on the various timing signals generated by the timing generator.

[0075] The system control unit 27 supplies a control signal for controlling the vertical driving unit 24 to the vertical driving unit 24, and supplies a control signal for controlling the column processing unit 25-1 to the column processing unit 25-1. In addition, the system control unit 27 supplies a control signal for controlling the column processing unit 25-2 to the column processing unit 25-2 via the bump 13, and supplies a control signal for controlling the horizontal driving unit 26 to the horizontal driving unit 26 via the bump 13.

[0076] The memory and signal processing unit 28 performs various signal processing on the pixel signal output from the horizontal driving unit 26. At this time, the memory and signal processing unit 28 stores the intermediate result of the signal processing in, for example, an internal memory when necessary, or refers to the intermediate result at a necessary timing. For example, the memory is configured with a dynamic random access memory (DRAM) and a static random access memory (SRAM), etc. The memory and signal processing unit 28 outputs the pixel signal after the signal processing.

[0077] (First Example Structure of CMOS Image Sensor)

[0078] Figure 2 A is shown Figure 1 FIG. 1 is a cross-sectional view of a first example structure of a CMOS image sensor 10 . Figure 2 B is a diagram of a first example structure of the CMOS image sensor 10 as seen from the light irradiation side.

[0079] like Figure 2 A and Figure 2 As shown in FIG. 1B , a pixel region 21 and the like are formed on the semiconductor chip 11. In addition, a peripheral circuit unit 51 including a column processing unit 25-1 and a system control unit 27 is formed in a region of the semiconductor chip 11 corresponding to the semiconductor chip 12. In addition, an electrode pad 52 for wire bonding is also formed on the semiconductor chip 11.

[0080] Bump connection electrode pads 53A are formed in the peripheral circuit unit 51. On the light irradiation side of the semiconductor chip 11, a passivation layer 54A of SiN or the like is formed to have openings in partial regions corresponding to the bump connection electrode pads 53A and the wire bonding electrode pads 52. The bumps (microbumps) 13 are connected to the bump connection electrode pads 53A via the openings of the passivation layer 54A.

[0081] On the other hand, a bump connection electrode pad 53B is formed on the semiconductor chip 12 (column processing unit 25-2). In addition, on the side opposite to the light irradiation side of the semiconductor chip 12, a passivation layer 54B of SiN or the like is formed to have an opening in a partial area corresponding to the bump connection electrode pad 53B. The bump 13 is connected to the bump connection electrode pad 53B via the opening of the passivation layer 54B. Therefore, the semiconductor chip 12 is bonded to the light irradiation side of the semiconductor chip 11 via the bump 13 on the semiconductor chip 12 and the bump 13 on the semiconductor chip 11. That is, the semiconductor chip 12 is flip-chip bonded to the light irradiation side of the semiconductor chip 11.

[0082] In order to maintain mechanical strength, the space between the semiconductor chip 11 and the semiconductor chip 12 is filled with an underfill resin 55. A dam 56 is formed around the region on the semiconductor chip 11 that is bonded to the semiconductor chip 12, and when the space is filled with the underfill resin 55, the dam prevents the underfill resin 55 from leaking into a region outside the bonding region. Therefore, the underfill resin 55 spreads only inside the dam 56.

[0083] In addition, on the light irradiation side of the semiconductor chip 11, a lens material 57 of an organic substance or the like is formed in the pixel region 21, wherein the pixel region is an area outside the bump 13. The lens material 57 may include one organic substance, or may include two or more stacked organic substances. A thin inorganic film of SiO2 and SiN or the like may be stacked as an antireflection film on the organic substance forming the lens material 57.

[0084] The lens material 57 functions as an on-chip lens in the pixel region 21 and collects irradiated light on the pixel region 21. The lens material 57 is not formed in a region 58 outside the pixel region 21 on the semiconductor chip 11. That is, the lens material 57 has an opening in a region outside the pixel region 21.

[0085] It should be noted that, although not shown, a color filter or the like is actually formed between the lens material 57 and the pixel region 21 .

[0086] (Description of a method for manufacturing a CMOS image sensor)

[0087] Figure 3 Is a description Figure 2 An overview diagram of the manufacturing method of a CMOS image sensor.

[0088] First, if Figure 3 As shown in FIG. 1A , a passivation layer 54A and a lens material 57 are stacked on the entire surface of the light irradiation side of the semiconductor chip 11 in which the pixel region 21 , the peripheral circuit unit 51 , and the electrode pad 52 for wire bonding are formed.

[0089] Then, if Figure 3 As shown in B, the region 58 outside the pixel region 21 of the lens material 57 is etched to form an opening. Figure 3 As shown in FIG. C, in order to connect the bump 13 and the bump connection electrode pad 53A, the partial area of ​​the passivation layer 54A corresponding to the bump connection electrode pad 53A is etched to form a bump opening 71. In addition, in order to connect the wire bonding member to the wire bonding electrode pad 52, the partial area corresponding to the wire bonding electrode pad 52 is etched to form a wire bonding opening 72. Then, as shown in FIG. Figure 3 As shown in FIG. 2D , the bumps 13 are formed on the bump connection electrode pads 53A in the peripheral circuit unit 51 , and the dams 56 are formed around the bonding region of the semiconductor chip 12 on the peripheral circuit 51 .

[0090] Then, if Figure 3As shown in FIG. E, the semiconductor chip 12 having the bump connection electrode pad 53B connected to the bump 13 is bonded to the peripheral circuit unit 51 of the semiconductor chip 11 so that the bump 13 of the semiconductor chip 11 is connected to the semiconductor chip 12. Then, the space between the semiconductor chip 11 and the semiconductor chip 12 is filled with the bottom filling resin 55.

[0091] Figure 4 It is an enlarged view of the vicinity of the peripheral circuit unit 51 for describing the details of the method of forming the bumps 13 of the semiconductor chip 11 .

[0092] First, if Figure 4 As shown in A, a seed metal 73 is deposited. Then, as Figure 4 As shown in B, photolithography is performed, and a resist 74 is formed in a region other than a region where the bump 13 is formed.

[0093] Then, if Figure 4 As shown in FIG. C, solder 75 is formed by electroplating growth of solder using resist 74 as a mask. Then, as shown in FIG. Figure 4 As shown in D, the resist 74 is removed. Then, as Figure 4 As shown in E, the seed metal 73 in the area outside the solder 75 is etched. Figure 4 As shown in F, reflow is performed to form bumps 13.

[0094] In contrast, in the case where the lens material 57 is stacked on the entire surface of the light irradiation side of the semiconductor chip 11, the lens material 57 exists in addition to the passivation layer 54A on the light irradiation side of the bump connection electrode pad 53A, as shown in FIG. Figure 5 As shown. Therefore, it is necessary to make openings in the passivation layer 54A and the lens material 57 to form the opening portion 81. As such, the aspect ratio between the depth and the opening width of the opening portion 81 is large.

[0095] Therefore, when forming the bump 13, the embedding property of the solder and the seed metal 73 is reduced, and resist residue due to insufficient exposure and insufficient development during photolithography is likely to occur. As a result, the bump 13 may be deformed or the like.

[0096] In addition, since the lens material 57 includes an organic substance, gas is generated from the lens material 57 around the opening portion 81 of the passivation layer 54A, and the gas generates a reaction product by reacting with the etching gas when etching for forming the opening portion 81 of the passivation layer 54A is performed. In addition, in the case where the lens material 57 is a material that is more brittle than the passivation layer 54A, when etching for forming the opening portion 81 of the passivation layer 54A is performed, the lens material 57 is physically etched to be scattered, and the scattered lens material 57 inhibits the progress of etching for forming the opening portion 81 of the passivation layer 54A. Therefore, an abnormality of the opening portion 81 of the passivation layer 54A occurs, and the bump 13 is deformed and the connection resistance is degraded, etc.

[0097] As the bumps 13 are miniaturized and the pitch of the bumps 13 is narrowed, the aspect ratio of the opening portion 81 is further increased and the above-mentioned problems in forming the bumps 13 are also more significant. However, in the CMOS image sensor 10 in which the column processing unit 25-2 is formed on a semiconductor chip 12 different from the semiconductor chip 11 and flip-chip bonding is performed, the increase in the number of bumps 13 enables high-speed operation. Therefore, it is desirable to configure as many bumps 13 as possible in the semiconductor chip 12 of a limited size, and miniaturization of the bumps 13 and narrowing of the pitch of the bumps 13 are necessary. In addition, in the case in which the lens material 57 is thick, the aspect ratio of the opening portion 81 is also increased, and the above-mentioned problems in forming the bumps 13 are also more significant.

[0098] Since the electrode pad 52 for wire bonding is large enough, the influence of the lens material 57 around the opening portion 72 for wire bonding is small in the etching for forming the opening portion 72 for wire bonding formed on the electrode pad 52 for wire bonding. In addition, the wire ball is not formed by photolithography, but is formed by mechanically forming an alloy using ultrasonic waves and pressure and crimping; therefore, the same problem as when forming the bump 13 does not occur.

[0099] On the other hand, in the CMOS image sensor 10, an opening is made in at least a part of the region in which the bump 13 and the electrode pad 52 for wire bonding are formed; therefore, as shown in FIG. Figure 4 As shown in E, the aspect ratio of the bump opening 71 is smaller than Figure 5 The aspect ratio of the opening portion 81 shown in FIG. 1 is 0.17. Therefore, the embedding property of the solder and the seed metal 73 when the bump 13 is formed can be improved. In addition, the flow of the liquid is not blocked during wet processing (such as development). Therefore, the occurrence of the resist 74 residue caused by insufficient exposure and insufficient development during photolithography can be prevented. In addition, when etching the bump opening portion 71 for forming the passivation layer 54A, the lens material 57 around the bump opening portion 71 can be prevented from inhibiting the etching.

[0100] (Second Example Structure of Pixel Region and Peripheral Circuits)

[0101] Figure 6 It shows Figure 1 FIG. 1 is a cross-sectional view of a second example structure of the CMOS image sensor 10 .

[0102] Figure 6 The structure of the CMOS image sensor 10 is Figure 2 The structure is basically the same, except that Figure 6 In the embodiment, the lens material 57 is formed in a region 91 and a region other than a partial region of the wire bonding electrode pad 52 . The region 91 corresponds to the semiconductor chip 12 and is the entire region inside the dam 56 on the semiconductor chip 11 (including the dam 56 ).

[0103] That is to say, Figure 6 In the example, the lens material 57 is formed to have an opening in a region 91 on the semiconductor chip 11 and a partial region of the electrode pad 52 for wire bonding, wherein the region 91 corresponds to and is larger than the semiconductor chip 12 .

[0104] For example, when the dam 56 is formed at a position approximately 200 μm from the edge of the semiconductor chip 12 , an opening is formed in the lens material 57 approximately 200 μm from the edge of the region where the semiconductor chip 12 is bonded to the semiconductor chip 11 .

[0105] (Third Example Structure of Pixel Region and Peripheral Circuits)

[0106] Figure 7 It is schematically shown Figure 1 FIG. 1 is a cross-sectional view of a third example structure of the CMOS image sensor 10 .

[0107] Figure 7 The structure of the CMOS image sensor 10 is Figure 2 The structure is basically the same, except that Figure 7 In the embodiment, the lens material 57 is formed to have an opening only in a region 92 which is a portion of the inner side of the dam 56 on the semiconductor chip 11 (including the dam 56 ) and larger than the size of the semiconductor chip 12 , and in a partial region of the wire bonding electrode pad 52 .

[0108] That is to say, Figure 7 In the example, the lens material 57 is formed to have an opening in an area on the semiconductor chip 11 corresponding to the semiconductor chip 12, larger than the size of the semiconductor chip 12 and smaller than the area inside the dam 56 (including the dam 56), and in a partial area of ​​the electrode pad 52 for lead bonding.

[0109] As mentioned above, in Figure 6 and Figure 7 In the example of , the lens material 57 is also formed in the area outside the pixel area 21; therefore, the lens material 57 can also protect the area outside the pixel area 21. In addition, when the lens material 57 includes a color filter that prevents reflection of light, reflection of light in the area outside the pixel area 21 can be prevented.

[0110] Although the lens material 57 is not formed in a partial area on the peripheral circuit unit 51, the portion can also be protected because it is filled with the bottom filling resin 55. In addition, by selecting a suitable resin as the bottom filling resin 55, reflection of light inside the dam 56 (excluding the dam 56) can be prevented.

[0111] (Fourth Example Structure of Pixel Region and Peripheral Circuits)

[0112] Figure 8 It is schematically shown Figure 1 FIG. 1 is a cross-sectional view of a fourth example structure of the CMOS image sensor 10 .

[0113] Figure 8 The structure of the CMOS image sensor 10 is Figure 2 The structure is basically the same as in Figure 8 In the embodiment, the lens material 57 is formed to have an opening only in a region 93 inside the dam 56 on the semiconductor chip 11 and in a partial region of the wire bonding electrode pad 52 , and the size of the region 93 is the same as that of the semiconductor chip 12 .

[0114] That is to say, Figure 8 In the example of FIG. 5 , the lens material 57 is formed to have openings in a region 93 on the semiconductor chip 11 that corresponds to the semiconductor chip 12 and has the same size as the semiconductor chip 12 and in a partial region of the electrode pad 52 for wire bonding.

[0115] Considering the misalignment of the semiconductor chip 12, the lens material 57 may have an opening in a region which is closer to the inner misalignment amount than the region 93 and smaller than the size of the semiconductor chip 12. It should be noted that when the opening region of the lens material 57 is too small, the same problem as in the case where the lens material 57 is formed on the entire surface of the semiconductor chip 11 occurs when the bump 13 is formed.

[0116] So, for example, Fig. 9As shown, the opening area 94 outside the electrode pad 52 for wire bonding of the lens material 57 is formed so that the distance 101 from the side of the bump 13 closest to the lens material 57 closest to the lens material 57 to the side of the lens material 57 closest to the bump 13 is greater than the larger of twice the opening size during lithography (i.e., the diameter 102 of the bump 13) and the minimum value 103 of the pitch of the bumps 13.

[0117] Alternatively, if Fig. 9 and Fig.10 As shown, the opening area 94 is formed so that the ratio of the distance 124 from the side of the opening portion 72 for wire bonding closest to the lens material 57 to the side of the lens material 57 closest to the opening portion 72 for wire bonding to the dimension 123 of the opening portion 72 for wire bonding in the direction in which the lens material 57 and the wire bonding member 120 are aligned (hereinafter referred to as the wire bonding ratio) is smaller than the ratio of the distance 105 from the side of the opening portion 71 for bump closest to the lens material 57 to the side of the lens material 57 closest to the opening portion 71 for bump to the dimension 104 of the opening portion 71 for bump in the direction in which the lens material 57 and the bump 13 are aligned (hereinafter referred to as the bump ratio).

[0118] That is, the opening region 94 is formed so that the bump ratio is equal to or greater than the wire bonding ratio that does not cause a problem when forming the wire bonding member 120 .

[0119] As mentioned above, in Figures 8 to 10 In the example, Figure 6 and Figure 7 As in the case of FIG. 5 , the lens material 57 is also formed in the region outside the pixel region 21. Therefore, the region outside the pixel region 21 can also be protected, and reflection of light in the region outside the pixel region 21 can be prevented.

[0120] The size of the opening region (region 93 or opening region 94) of the lens material 57 outside the wire bonding electrode pad 52 is equal to or smaller than the size of the semiconductor chip 12. Therefore, the semiconductor chip 12 and the bottom filling resin 55 can protect the opening region of the lens material 57 on the peripheral circuit unit 51 and prevent reflection of light in the opening region.

[0121] (Example of the shape of region 92)

[0122] Figures 11 to 13 is a diagram of a portion of the semiconductor chip 11 as seen from the light irradiation side, showing Figure 7 An example of the shape of region 92 .

[0123] like Fig.11As shown, for example, region 92 includes an area surrounding all bumps 13 formed on semiconductor chip 11. In this case, the height difference formed by lens material 57 on the surface of the light irradiation side of semiconductor chip 11 is reduced, and the flow of liquid is less likely to be blocked during wet processing such as development.

[0124] It should be pointed out that if Fig.12 As shown, the region 92 may include more than two regions, which divide the bumps 13 into more than two groups and respectively surround the bumps 13 in each group. In addition, the shape of the region 92 is not limited to a rectangular shape, and may be, for example, Fig.13 The circular shape shown.

[0125] Despite using Figure 11 to Figure 13 Region 92 is described, but the same applies to region 93 and opening region 94 .

[0126] In the first embodiment, the case where the embodiment of the present disclosure is applied to a CMOS image sensor is described; however, the embodiment of the present disclosure can also be applied to solid-state imaging devices other than CMOS image sensors, such as charge coupled device (CCD) image sensors, etc. In addition, the embodiment of the present disclosure can be applied to components in which a resin such as polyimide is used as a protective film instead of the lens material 57 and a bump is formed. In addition, the method of allocating the components of the CMOS image sensor 10 to the semiconductor chip 11 and the semiconductor chip 12 is not limited to the above method. In addition, the units connected by the bumps are not limited to the column processing units 25-1 and 25-2, the horizontal drive unit 26, and the system control unit 27. In addition, the semiconductor chip 12 can be formed by a plurality of semiconductor chips. The units formed on the plurality of semiconductor chips may be the same or different.

[0127] <Second Implementation Method>

[0128] (Overview of Example Configuration of Second Embodiment of CMOS Image Sensor)

[0129] Fig.14 is an overview diagram showing an example configuration of a second embodiment of a CMOS image sensor to which the present disclosure is applied.

[0130] exist Fig.14 In the CMOS image sensor 140, the lower chip 141 is the semiconductor chip on the lower side in the figure, and the upper chip 142 is the semiconductor chip on the upper side in the figure, and the two are flip-chip bonded to each other.

[0131] The lower chip 141 includes a semiconductor substrate and a metal wiring layer such as Cu and Al, and a pixel region 141A and a peripheral circuit 141B are formed on the lower chip 141. The configuration of the pixel region 141A is similar to that of the Figure 1 The peripheral circuit 141B having a configuration similar to that of the vertical drive unit 24, the column processing units 25-1 and 25-2, the horizontal drive unit 26, and the system control unit 27 is formed on the same lower chip 141 on which the pixel region 141A is formed, and includes bumps not shown for bonding to the upper chip 142.

[0132] The unillustrated lens material formed on the lower chip 141 is formed to have an opening in a region corresponding to the bonding region of the upper chip 142. Therefore, as in the first embodiment, problems occurring when forming unillustrated bumps included in the peripheral circuit 141B can be prevented.

[0133] The upper chip 142 includes a semiconductor substrate and a metal wiring layer of Cu, Al, etc., and a signal processing circuit 142A is formed on the upper chip 142. The configuration of the signal processing circuit 142A is similar to Figure 1 The configuration of the memory and signal processing unit 28 is similar.

[0134] (Sample configuration of a CMOS image sensor before dicing)

[0135] Fig.15 It shows the Fig.14 A perspective view of an example configuration of the CMOS image sensor 140, Fig.16 It is along Fig.15 Cross-sectional view along the AA direction.

[0136] like Fig.15 As shown, the CMOS image sensor 140 before dicing includes a semiconductor wafer 150 in which lower chips 141 are arranged in an array and an upper chip 142 straddling and bonded to two lower chips 141. It should be noted that Fig.15 Only a portion of the semiconductor wafer 150 in which 2 (laterally)×3 (vertically) lower chips 141 are formed is shown.

[0137] The outer shape of each of the lower chip 141 (first semiconductor chip) and the upper chip 142 is a rectangular shape with a predetermined thickness. A scribe area 151 is provided between the lower chips 141. A test element group (TEG) pattern 161 and a mark 162 are formed in the scribe area 151 between the two lower chips 141, where the upper chip 142 spans and exists on the two lower chips.

[0138] The TEG pattern 161 is a pattern for evaluating a bump (not shown) for bonding the lower chip 141 and the upper chip 142 to each other. The mark 162 is a mark for alignment when bonding the lower chip 141 and the upper chip 142. The lower chip 141 and the upper chip 142 are bonded to each other so that the mark 162 coincides with a mark (not shown) formed on the upper chip 142.

[0139] In addition, an electrode 163 for evaluating a bump not shown for bonding the lower chip 141 and the upper chip 142 is formed in the scribe area 151 to be connected to the TEG pattern 161. A dam 164 is formed around the area on the lower chip 141 to be bonded to the upper chip 142, wherein the dam prevents leakage of the bottom filling resin filling the space between the lower chip 141 and the upper chip 142 when bonding the lower chip 141 and the upper chip 142 to each other.

[0140] The upper chip 142 is formed by a north chip 171 formed on the upper side (north side) of the figure and a south chip 172 formed on the lower side (south side) of the figure, wherein a scribe area 173 is sandwiched between the north chip 171 and the south chip 172. The outer shape of each of the north chip 171 (second semiconductor chip) and the south chip 172 (third semiconductor chip) is a rectangular shape with a predetermined thickness. A mark not shown for alignment when the lower chip 141 and the upper chip 142 are bonded to each other is formed in the scribe area 173.

[0141] On the upper chip 142 , the signal processing circuit 142A is divided into five circuits 181 to 185 , and of these circuits, two circuits 181 and 182 are formed on the north chip 171 , and three circuits 183 to 185 are formed on the south chip 172 .

[0142] The CMOS image sensor 140 before dicing is separated by dicing (cutting) the scribe line area 151 around the lower chip 141, as shown in FIG. Fig.16 shown.

[0143] Therefore, in the separated CMOS image sensor 140, the scribe line region 151 is formed outside the scribe line of the outline of the lower chip 141 added thereto. Fig.15 The entire area of ​​the side surface (first side surface) 191 in the left-right direction (horizontal direction) and the area outside the scribe line of the outline of the north chip 171 to which the scribe line area 173 is added are Fig.15 The entire areas of the side surfaces (second side surfaces) 192 in the left-right direction are flush with each other.

[0144] Furthermore, the entire area of ​​the side (third side) 193 facing the side 191 outside the scribe line of the outline of the lower chip 141 to which the scribe line area 151 is added is aligned with the entire area outside the scribe line of the outline of the south chip 172 to which the scribe line area 173 is added. Fig.15 The entire areas of the side surfaces (fourth side surfaces) 194 in the left-right direction are flush with each other.

[0145] It should be noted that although in the second embodiment, the entire areas of side 191 and side 192 are flush with each other, and the entire areas of side 193 and side 194 are flush with each other, as long as at least part of the area is flush with each other, the entire area does not have to be flush with each other.

[0146] As described above, in the CMOS image sensor 140, the north chip 171 and the south chip 172 are formed on one upper chip 142. Therefore, the north chip 171 and the south chip 172 can be simultaneously bonded to the lower chip 141. In addition, the lower chip 141 can be formed on the semiconductor wafer 150 in the same orientation, and the lower chip 141 does not require a symmetry axis. In addition, the north chip 171 and the south chip 172 do not require a symmetry axis.

[0147] In addition, the TEG pattern 161, the mark 162, and the electrode 163 used only in manufacturing are arranged in the scribe line area 151, and are removed when the CMOS image sensor 140 is separated. Therefore, compared with the case where the TEG pattern 161, the mark 162, and the electrode 163 are arranged in the CMOS image sensor 140, the effective area of ​​the lower chip 141 can be increased.

[0148] In contrast, Fig.17 As shown, in the case where the north chip 203 and the south chip 204 are respectively formed on the lower chip 202 formed on the semiconductor wafer 201, the north chip 203 and the south chip 204 are bonded to the lower chip 202 one by one.

[0149] Therefore, it is necessary to form the mark 205 and the mark 206 for alignment when the north chip 203 and the south chip 204 are bonded. Fig.17 As shown, when the mark 205 and the mark 206 are formed on the lower chip 202 on the semiconductor wafer 201, the size of the lower chip 202 is increased and the manufacturing cost is also increased.

[0150] Furthermore, it is necessary to form dams 207 and 208 to prevent leakage of an underfill resin that fills a space between the lower chip 202 and each of the north chip 203 and the south chip 204 near the bonding region of the north chip 203 and the south chip 204 on the lower chip 202 .

[0151] (Description of a method for manufacturing a CMOS image sensor)

[0152] Fig.18 is a perspective view for describing a method of manufacturing the CMOS image sensor 140 .

[0153] First, if Fig.18 As shown in FIG. 1A , a lower chip 141 is formed on a semiconductor wafer 150. A TEG pattern 161 and a mark 162 are formed in a scribe line region 151 between the lower chips 141, and an electrode 163 is formed in a region other than the region between the lower chips 141 in the scribe line region 151. A dam 164 is formed near a region on the lower chip 141 to which the upper chip 142 is bonded.

[0154] In the peripheral circuit 141B inside the dam 164 on the lower chip 141, a bump 221 such as a ball or a column is formed by a method such as electroplating, electroless plating, transfer or pressing to connect to an electrode for a bump not shown formed in the lower chip 141. For example, the bump 221 is configured to have a narrow pitch of several tens of microns. In order to ensure the electrical characteristics and reliability of the bump 221, the bump includes a barrier layer, a seed layer, a bonding metal layer, etc., which generally use a metal material such as Ni, Pd, Au, Sn, Ag, Pb, Bi, Cu and In.

[0155] Then, if Fig.18 As shown in FIG. 1B , the north chip 171 in which the circuits 181 and 182 are formed and the south chip 172 in which the circuits 183 to 185 are formed are arranged with the scribe area 173 sandwiched therebetween, thereby forming the upper chip 142. Bumps 222 are formed on the north chip 171 and the south chip 172. A mark 231 and a TEG pattern 232 are formed in the scribe area 173.

[0156] Then, if Fig.18 C, the upper chips 142 are sequentially arranged on the semiconductor wafer 150 to be bonded so that the mark 162 overlaps with the mark 231. Thus, the bump 222 on the north chip 171 is bonded to the bump 221 on the south side of one lower chip 141, and the bump 222 on the south chip 172 is bonded to the bump 221 on the north side of another lower chip 141 different from the lower chip 141.

[0157] In this manner, the lower chip 141 and the upper chip 142 are bonded to each other based on the mark 162 and the mark 231 ; therefore, even in the case where the bumps 221 and the bumps 222 are arranged at a high density, the bumps 221 and the bumps 222 can be accurately connected.

[0158] It should be noted that, on the north side of the lower chip 141 in which the north chip 171 is arranged on the south side thereof, a south chip 172 having an upper chip 142 different from the upper chip 142 having the north chip 171 is arranged. In addition, on the south side of the lower chip 141 in which the south chip 172 is arranged on the north side thereof, a north chip 171 having an upper chip 142 different from the upper chip 142 having the south chip 172 is arranged.

[0159] Next, the bottom filling resin is injected between the lower chip 141 and the upper chip 142 from one direction or both directions of the south and the north. In the case where the bottom filling resin is injected from both directions of the south and the north, the bottom filling resin is injected from the left and right opposite directions between the south and the north by line application. In this way, the lower chip 141 and the upper chip 142 are fixed.

[0160] Finally, if Fig.18 As shown in FIG. 2D , the scribe line region 151 around the lower chip 141 is diced and the CMOS image sensor 140 is separated.

[0161] As described above, the north chip 171 and the south chip 172 are bonded together to the lower chip 141, so that Fig.17 Compared with the case where the north chip 203 and the south chip 204 are respectively bonded to the lower chip 202, the bonding times can be greatly reduced. That is, the north chip 171 and the south chip 172 can be easily bonded to the lower chip 141.

[0162] Therefore, the bonding turn-around time (TAT) is shortened and the manufacturing cost can be reduced. In addition, the heat treatment time required for the bump connection is shortened, thereby reducing the heat load on the semiconductor wafer 150 and minimizing the influence of the heat treatment on the characteristics of the CMOS image sensor 140.

[0163] Furthermore, since the north chip 171 and the south chip 172 are bonded to the lower chip 141 in common, the mark for alignment and the TEG pattern for evaluating the bumps can be shared when the north chip 171 and the south chip 172 are bonded.

[0164] Furthermore, the CMOS image sensor 140 does not have layout restrictions such as mirror inversion and symmetry axis; therefore, there is no need to change the physical configuration of the CMOS image sensor 140 .

[0165] Although in the second embodiment, the number of lower chips 141 bonded to one upper chip 142 is two, the number may be greater than two. For example, the upper chip 142 may span and bond to 2 (lateral) × 2 (vertical) lower chips 141 (i.e., 4 lower chips 141), or may span and bond to 3 (lateral) × 2 (vertical) lower chips 141 (i.e., 6 lower chips 141). It should be noted that there is a trade-off relationship between the number of lower chips 141 bonded to one upper chip 142 and the yield.

[0166] Although the number of circuits forming the signal processing circuit 142A is five in the second embodiment, it may be any number greater than one.

[0167] In addition, although the lens material is not formed in the region corresponding to the bonding region of the upper chip 142 on the lower chip 141 in the second embodiment like in the first embodiment, the lens material may be formed in the region.

[0168] Although in the second embodiment, the pixel region 141A and the peripheral circuit 141B are formed on the same lower chip 141, they may be formed on different semiconductor chips. In this case, the bonding between semiconductor chips is also performed in a similar manner to the lower chip 141 and the upper chip 142.

[0169] In addition, the CMOS image sensor 10 and the CMOS image sensor 140 can be a back-side illuminated CMOS image sensor or a front-side illuminated CMOS image sensor. It should be noted that in the case where the CMOS image sensor 10 and the CMOS image sensor 140 are front-side illuminated CMOS image sensors, the electrode pad for bump connection can be formed above the metal wiring layer. Therefore, the formation step of the electrode pad for bump connection can be similar to the formation step of the ordinary electrode pad for wire bonding connection. In addition, unlike the case of the back-side illuminated CMOS image sensor, there is no need to perform a back-side rewiring step of bringing the wiring of the metal wiring layer on the back side to the front side. Therefore, the manufacturing cost can be reduced.

[0170] <Third Implementation Method>

[0171] (Example Configuration of Embodiment of Imaging Device)

[0172] Fig.19 : is a block diagram showing an example configuration of an embodiment of an imaging device as an electronic device to which the present disclosure is applied.

[0173] Fig.19The imaging device 1000 is a camera or a digital camera, etc. The imaging device 1000 includes a lens group 1001, a solid-state image sensor 1002, a DSP circuit 1003, a frame memory 1004, a display unit 1005, a recording unit 1006, an operation unit 1007, and a power supply unit 1008. The DSP circuit 1003, the frame memory 1004, the display unit 1005, the recording unit 1006, the operation unit 1007, and the power supply unit 1008 are interconnected via a bus 1009.

[0174] The lens group 1001 receives incident light (image light) from a subject and forms an image on the imaging surface of the solid-state image sensor 1002. The solid-state image sensor 1002 includes the above-mentioned CMOS image sensor 10(140). The solid-state image sensor 1002 converts the amount of incident light formed by the lens group 1001 on the imaging surface into an electrical signal in units of pixels, and provides the electrical signal as a pixel signal to the DSP circuit 1003.

[0175] The DSP circuit 1003 performs predetermined image processing on the pixel signals provided from the solid-state image sensor 1002, and provides the pixel signals after the image processing to the frame memory 1004 in units of frames for temporarily storing the pixel signals.

[0176] For example, the display unit 1005 is configured with a panel display device such as a liquid crystal panel or an organic electroluminescence (EL) panel, and displays an image based on the pixel signals in units of frames temporarily stored in the frame memory 1004.

[0177] The recording unit 1006 is configured with a digital versatile disc (DVD), a flash memory, etc., and reads and records the pixel signals in units of frames temporarily stored in the frame memory 1004.

[0178] The operation unit 1007 issues operation commands regarding various functions of the imaging device 1000 under the control of a user. The power supply unit 1008 appropriately supplies power to the DSP circuit 1003, the frame memory 1004, the display unit 1005, the recording unit 1006, and the operation unit 1007.

[0179] The electronic device to which this technical embodiment is applicable can be any device that uses a CMOS image sensor in an image capture unit (photoelectric conversion unit). Examples of these devices include portable terminal devices having an imaging function and copying machines that use a CMOS image sensor in an image reading unit, in addition to the imaging device 1000.

[0180] <Application Examples of CMOS Image Sensors>

[0181] Fig. 201 is a diagram showing an application example of the above-mentioned CMOS image sensor 10 ( 140 ).

[0182] For example, the above-described CMOS image sensor 10 ( 140 ) may be used in various situations of sensing light such as visible light, infrared light, ultraviolet light, and X-rays as described below.

[0183] - Devices for capturing images for viewing, such as digital cameras and portable devices with camera functions.

[0184] -Devices for vehicles, such as on-board sensors that capture images of the front and rear, surroundings, and interior of a car, surveillance cameras that monitor moving vehicles and roads, and distance sensors that measure the distance between vehicles, etc. for safe driving (e.g., automatic stopping) and identifying the driver's condition, etc.

[0185] - A device for home appliances (such as televisions, refrigerators, and air conditioners) that captures images of user gestures and performs operations of the appliance based on the gestures.

[0186] - Devices used in medical and health care, such as endoscopes and equipment for angiography by receiving infrared light.

[0187] -Devices for security, such as surveillance cameras for crime prevention and cameras for personal authentication.

[0188] - Devices used for beauty treatments, such as skin measurement devices that take images of the skin and microscopes that take images of the scalp.

[0189] -Devices for sports, such as action cameras and wearable cameras for sports, etc.

[0190] -Devices for use in agriculture, such as cameras for monitoring field and crop conditions.

[0191] It should be noted that the effects described in this specification are merely exemplary and not restrictive; other effects may also be exhibited.

[0192] Furthermore, the embodiments of the present disclosure are not limited to the above-described embodiments, and various changes may occur within the scope of the present disclosure.

[0193] For example, the embodiments of the present technology can also be applied to semiconductor devices other than CMOS image sensors in which a plurality of semiconductor chips are flip-chip-bonded to each other.

[0194] In addition, the present technology may also have the following configurations.

[0195] (1) A semiconductor device comprising:

[0196] a plurality of bumps on the first semiconductor substrate; and

[0197] Lens material in an area outside the multiple bumps on the first semiconductor substrate, wherein the distance between the side of the bump closest to the lens material closest to the lens material and the side of the lens material closest to the bump is greater than twice the diameter of the bump closest to the lens material, and wherein the distance between the side of the bump closest to the lens material closest to the lens material and the side of the lens material closest to the bump is greater than the minimum spacing between the bumps.

[0198] (2) The semiconductor device according to (1),

[0199] The lens material is formed only in the pixel region on the first semiconductor substrate.

[0200] (3) The semiconductor device according to (1),

[0201] The lens material is formed only in a region on the first semiconductor substrate other than a region corresponding to the second semiconductor substrate, and the second semiconductor substrate is configured to be bonded to the first semiconductor substrate via the bump.

[0202] (4) The semiconductor device according to (3),

[0203] The lens material is formed to have an opening in a region on the first semiconductor substrate, and the opening is larger than the second semiconductor substrate.

[0204] (5) The semiconductor device according to (4), further comprising:

[0205] an underfill resin formed between the second semiconductor substrate and the first semiconductor substrate; and

[0206] a dam formed on the first semiconductor substrate and preventing the underfill resin from leaking to a region on the first semiconductor substrate other than a region bonded to the second semiconductor substrate,

[0207] The lens material is formed to have an opening in the entire region inside the dam on the first semiconductor substrate.

[0208] (6) The semiconductor device according to (3), further comprising:

[0209] an underfill resin formed between the second semiconductor substrate and the first semiconductor substrate; and

[0210] a dam formed on the first semiconductor substrate and preventing the underfill resin from leaking to an area on the first semiconductor substrate other than an area bonded to the second semiconductor substrate;

[0211] The lens material is formed to have an opening only in a partial region inside the dam on the first semiconductor substrate.

[0212] (7) The semiconductor device according to (3),

[0213] The lens material is formed to have an opening in a region on the first semiconductor substrate, and the opening is smaller than the second semiconductor substrate.

[0214] (8) The semiconductor device according to (1),

[0215] The side of the lens material closest to the bump is a side of the on-chip lens.

[0216] (9) The semiconductor device according to (1), further comprising:

[0217] a bump-connecting electrode pad formed on the first semiconductor substrate and configured to be connected to the bump; and

[0218] an electrode pad for wire bonding formed on the first semiconductor substrate and arranged to be connected to the wire bonding member,

[0219] Among them, the ratio of the distance between the side of the opening part for lead bonding closest to the lens material and the side of the lens material closest to the opening part for lead bonding and the size of the opening part for lead bonding is smaller than the ratio of the distance between the side of the opening part for bump closest to the lens material and the side of the lens material closest to the opening part for bump and the size of the opening part for bump.

[0220] (10) A method for manufacturing a semiconductor device, the method comprising:

[0221] forming a plurality of bumps on the first semiconductor substrate, and

[0222] A lens material is formed in an area outside the multiple bumps on the first semiconductor substrate, wherein a distance between a side of a bump closest to the lens material closest to the lens material and a side of the lens material closest to the bump is greater than twice a diameter of the bump closest to the lens material, and wherein a distance between a side of a bump closest to the lens material closest to the lens material and a side of the lens material closest to the bump is greater than a minimum pitch between the bumps.

[0223] (11) An electronic device comprising:

[0224] a plurality of bumps on the first semiconductor substrate; and

[0225] Lens material in an area outside the multiple bumps on the first semiconductor substrate, wherein the distance between the side of the bump closest to the lens material closest to the lens material and the side of the lens material closest to the bump is greater than twice the diameter of the bump closest to the lens material, and wherein the distance between the side of the bump closest to the lens material closest to the lens material and the side of the lens material closest to the bump is greater than the minimum spacing between the bumps.

[0226] (12) A semiconductor device comprising:

[0227] a first semiconductor substrate having a rectangular shape;

[0228] a second semiconductor substrate having a rectangular shape, wherein an area of ​​the second semiconductor substrate is smaller than an area of ​​the first semiconductor substrate, and at least a portion of a first edge of the second semiconductor substrate is flush with at least a portion of a first edge of the first semiconductor substrate; and

[0229] A third semiconductor substrate having a rectangular shape, wherein an area of ​​the third semiconductor substrate is smaller than an area of ​​the first semiconductor substrate, and at least a portion of a first edge of the third semiconductor substrate is flush with at least a portion of a second edge of the first semiconductor substrate.

[0230] (13) The semiconductor device according to (12),

[0231] Wherein, the first semiconductor substrate includes a pixel array,

[0232] The second semiconductor substrate and the third semiconductor substrate each include at least one logic circuit.

[0233] wherein each of the first edge of the first semiconductor substrate and the first edge of the second semiconductor substrate corresponds to a scribe line forming a first edge of the stacked semiconductor device, and

[0234] The second edge of the first semiconductor substrate and the first edge of the third semiconductor substrate each correspond to a scribe line forming a second edge of the stacked semiconductor device.

[0235] (14) A method for manufacturing a semiconductor device, the method comprising:

[0236] bonding a first semiconductor substrate including a plurality of logic circuits to a second semiconductor substrate and a third semiconductor substrate configured in an array in a semiconductor wafer, wherein each of the second semiconductor substrate and the third semiconductor substrate includes a pixel array, and wherein the first semiconductor substrate spans the second semiconductor substrate and the third semiconductor substrate; and

[0237] The first edge of the first semiconductor substrate and the first edge of the second semiconductor substrate are cut so that the first edge of the first semiconductor substrate and the first edge of the second semiconductor substrate are flush with each other.

[0238] (15) The method for manufacturing a semiconductor device according to (14), further comprising:

[0239] bonding a fourth semiconductor substrate including a plurality of logic circuits to the second semiconductor substrate and the fifth semiconductor substrate, wherein the fourth semiconductor substrate spans the second semiconductor substrate and the fifth semiconductor substrate; and,

[0240] The second edge of the second semiconductor substrate and the first edge of the fourth semiconductor substrate are cut so that the second edge of the second semiconductor substrate and the first edge of the fourth semiconductor substrate are flush with each other.

[0241] (16) An electronic device comprising:

[0242] a first semiconductor substrate having a rectangular shape;

[0243] a second semiconductor substrate having a rectangular shape, wherein an area of ​​the second semiconductor substrate is smaller than an area of ​​the first semiconductor substrate, and at least a portion of a first edge of the second semiconductor substrate is flush with at least a portion of a first edge of the first semiconductor substrate; and

[0244] A third semiconductor substrate having a rectangular shape, wherein an area of ​​the third semiconductor substrate is smaller than an area of ​​the first semiconductor substrate, and at least a portion of a first edge of the third semiconductor substrate is flush with at least a portion of a second edge of the first semiconductor substrate.

[0245] (17) A semiconductor device comprising:

[0246] a first semiconductor substrate including a plurality of on-chip lenses corresponding to a plurality of pixels; and

[0247] A second semiconductor substrate mounted to a light incident side of a first semiconductor substrate via one or more solder bumps, wherein a size of the first semiconductor substrate is larger than a size of the second semiconductor substrate, and wherein the second semiconductor substrate is configured to receive one or more pixel signals from the first semiconductor substrate, process the one or more pixel signals, and output the processed one or more pixel signals.

[0248] [reference numerals list]

[0249] 10 CMOS Image Sensor

[0250] 11,12 Semiconductor chips

[0251] 13 Bump

[0252] 21 pixel area

[0253] 52 Electrode pad for wire bonding

[0254] 53 Electrode pad for bump connection

[0255] 55 Bottom filling resin

[0256] 56 Dam

[0257] 57 Lens Material

[0258] 71 Bump opening

[0259] 72 Opening portion for wire bonding

[0260] Area 91-93

[0261] 94 Opening area

[0262] 101 Distance

[0263] 102 Diameter

[0264] 103 Minimum

[0265] 104 Size

[0266] 105 Distance

[0267] 120 Wire Bonding Parts

[0268] 123 Size

[0269] 124 Distance

[0270] 140 CMOS Image Sensor

[0271] 141 Lower chip

[0272] 171 North Chip

[0273] 172 South Chip

[0274] 191~194 Side

Claims

1. A semiconductor device, include: a first semiconductor substrate having a rectangular shape; a second semiconductor substrate having a rectangular shape, wherein an area of ​​the second semiconductor substrate is smaller than an area of ​​the first semiconductor substrate, the second semiconductor substrate is stacked with the first semiconductor substrate in a thickness direction of the first semiconductor substrate, and a region of at least a first edge of the second semiconductor substrate is flush with a region of at least a first edge of the first semiconductor substrate; and a third semiconductor substrate having a rectangular shape, wherein an area of ​​the third semiconductor substrate is smaller than an area of ​​the first semiconductor substrate, the third semiconductor substrate is stacked with the first semiconductor substrate in a thickness direction of the first semiconductor substrate, and at least a first edge region of the third semiconductor substrate is flush with at least a second edge region of the first semiconductor substrate, The first semiconductor substrate includes a plurality of pixel arrays, wherein a first pixel array among the plurality of pixel arrays is adjacent to at least a portion of the second semiconductor substrate, and wherein a second pixel array among the plurality of pixel arrays is adjacent to at least a portion of the third semiconductor substrate.

2. The semiconductor device according to claim 1, in, The second semiconductor substrate includes processing circuitry.

3. The semiconductor device according to claim 2, in, The first semiconductor substrate also includes a peripheral circuit.

4. The semiconductor device according to claim 1, in, The first semiconductor substrate is connected to the second semiconductor substrate and the third semiconductor substrate through bumps.

5. The semiconductor device according to claim 4, in, The first semiconductor substrate further includes a plurality of electrodes.

6. The semiconductor device according to claim 5, The second semiconductor substrate includes a first test element group pattern connected to at least a first bump among the bumps, and the third semiconductor substrate includes a second test element group pattern connected to at least a second bump among the bumps.

7. The semiconductor device according to claim 5, in, The plurality of electrodes are formed in a region outside a region of the second semiconductor substrate and a region outside a region of the third semiconductor substrate.

8. The semiconductor device according to claim 1, in, The second semiconductor substrate and the third semiconductor substrate each include at least one logic circuit, wherein each of the first edge of the first semiconductor substrate and the first edge of the second semiconductor substrate corresponds to a scribe line of a first edge of the semiconductor device forming the stack, and Each of the second edge of the first semiconductor substrate and the first edge of the third semiconductor substrate corresponds to a scribe line of a second edge of the semiconductor device forming the stack.

9. The semiconductor device according to claim 8, further comprising: include: a fourth semiconductor substrate having a rectangular shape, wherein an area of ​​the fourth semiconductor substrate is smaller than an area of ​​the first semiconductor substrate, and a region of at least a first edge of the fourth semiconductor substrate is flush with a region of at least a first edge of the first semiconductor substrate; and A fifth semiconductor substrate having a rectangular shape, wherein an area of ​​the fifth semiconductor substrate is smaller than an area of ​​the first semiconductor substrate, and at least a first edge region of the fifth semiconductor substrate is flush with at least a second edge region of the first semiconductor substrate.

10. The semiconductor device according to claim 9, further comprising: include: a sixth semiconductor substrate having a rectangular shape, wherein an area of ​​the sixth semiconductor substrate is smaller than an area of ​​the first semiconductor substrate, and a region of at least a first edge of the sixth semiconductor substrate is flush with a region of at least a first edge of the first semiconductor substrate; and A seventh semiconductor substrate having a rectangular shape, wherein an area of ​​the seventh semiconductor substrate is smaller than an area of ​​the first semiconductor substrate, and at least a first edge region of the seventh semiconductor substrate is flush with at least a second edge region of the first semiconductor substrate.

11. The semiconductor device according to claim 8, An alignment mark is formed on the first semiconductor substrate.

12. A method for manufacturing a semiconductor device, the method include: bonding a first semiconductor substrate including a plurality of logic circuits to a second semiconductor substrate and a third semiconductor substrate arranged in an array in a semiconductor wafer, wherein each of the second semiconductor substrate and the third semiconductor substrate includes a pixel array, and wherein the first semiconductor substrate spans the second semiconductor substrate and the third semiconductor substrate; and The first edge of the first semiconductor substrate and the first edge of the second semiconductor substrate are cut so that the first edge of the first semiconductor substrate and the first edge of the second semiconductor substrate are flush with each other.

13. The method for manufacturing a semiconductor device according to claim 12, further comprising: include: bonding a fourth semiconductor substrate including a plurality of logic circuits to the second semiconductor substrate and the fifth semiconductor substrate, wherein the fourth semiconductor substrate spans the second semiconductor substrate and the fifth semiconductor substrate; and, The second edge of the second semiconductor substrate and the first edge of the fourth semiconductor substrate are cut so that the second edge of the second semiconductor substrate and the first edge of the fourth semiconductor substrate are flush with each other.