FFU rectifier plate for airflow zoning control and glue coating process for adjusting glue shape
Through the FFU rectifier plate controlled by air flow zones, the adjustable baffle combination is used to adjust the air flow environment of the glue coating chamber, which solves the complex problems of glue coating uniformity and thickness control in the photolithography process, and achieves precise control of film thickness and Consistency and stability.
Patent Information
- Application Number
- CN201911052499.X
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2019-10-31
- Publication Date
- 2024-09-17
- Estimated Expiration
- 2039-10-31
AI Technical Summary
In the photolithography process, the uniformity and thickness control of the glue coating process are complex, making it difficult to meet high standards.
Design an FFU rectifier plate with airflow zone control. Through the combination of the upper and lower adjustable baffles, the airflow environment in the glue coating chamber is adjusted to ensure the uniformity and thickness requirements of the photoresist on the silicon wafer. The rectifying plate includes an upper guide plate and a lower adjustable guide plate. The rotation of the circular and annular baffles is used to adjust the position of the guide holes, control the size of the airflow, and thereby regulate the gel shape.
It achieves precise control of photoresist film thickness, easily improves multi-cavity consistency issues, ensures film thickness stability, and meets process requirements.
Smart Images

Figure CN112748639B
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of photoresist coating technology, and in particular to an FFU rectifying plate with airflow zoning regulation and a coating technology for adjusting the shape of the glue. Background Art
[0002] With the rapid development of the information age, photolithography is a key technology in the manufacturing process of large-scale integrated circuits. The technology is constantly innovating and developing, and the requirements for photolithography are also increasing. The photolithography process includes the coating process, the photolithography process, and the development process. The coating process is the basis of the photolithography process, and the coating process technical requirements include coating uniformity and thickness.
[0003] Under the high standards of the glue coating process, adjusting the glue coating process becomes a complicated task. This invention aims to optimize the uniformity of the glue coating process by adjusting the air flow. Summary of the invention
[0004] The purpose of the present invention is to provide an FFU rectifier plate for airflow zoning regulation and a glue-spreading process for adjusting glue shape, by adjusting the upper and lower guide plates of the FFU rectifier plate to change the airflow in the glue coating cavity, thereby improving the glue coating effect. The process can be precisely regulated according to the uniformity and thickness requirements of the photoresist coating on the silicon wafer.
[0005] In order to achieve the above object, the technical solution adopted by the present invention is as follows:
[0006] A FFU rectifier for airflow zoning regulation, comprising an upper guide plate and a lower adjustable guide plate; wherein: the upper guide plate is installed below the FFU (the FFU is a fan filter unit, comprising a fan above and a filter below, and the bottom surface of the FFU refers to the bottom air outlet surface of the filter), the upper guide plate is installed parallel to the bottom surface of the FFU and in close contact with the bottom surface of the FFU; the lower adjustable guide plate is installed below the upper guide plate; the lower adjustable guide plate comprises a circular baffle and at least one annular baffle, the circular baffle and the annular baffle are concentric, and the annular baffle is arranged on the outer periphery of the circular baffle (the inner diameter of the annular baffle is greater than or equal to the diameter of the circular baffle).
[0007] A plurality of guide holes with the same diameter are evenly distributed on the upper guide plate, the circular baffle and the annular baffle, and the diameter of the guide holes is 0.3-2 mm.
[0008] The wafer to be spin-coated is placed below the lower adjustable guide plate, and the downward vertical projection of the center of the circular baffle of the lower guide plate coincides with the center of the wafer.
[0009] The circular baffle can rotate around the center of the circle, and the size of the airflow output to the center of the wafer can be controlled by rotating at different angles, thereby adjusting the glue shape at the center of the wafer; the annular baffle can rotate around the center of the annular baffle, and the airflow environment output to the position around the center of the wafer can be controlled by rotating at different angles, thereby achieving control of the glue shape at the edge of the wafer.
[0010] A bolt hole is arranged at the center of the circular baffle, and the circular baffle is fixed to the upper guide plate by bolts. After manually adjusting the overlap degree between the hole on the circular baffle and the hole at the corresponding position on the upper guide plate, the bolts are tightened to fix it.
[0011] The annular baffle comprises an annular sheet and an annular fixing groove, a plurality of guide holes are arranged on the annular sheet, the notch of the annular fixing groove faces downward, and the lower edge of the notch is bent inward by 90° to form an inward convex edge; the annular sheet is placed on the convex edge in the annular fixing groove, and the position of the annular sheet can be manually adjusted to make the degree of overlap between the guide holes on the annular sheet and the holes at corresponding positions on the upper guide plate different; the upper edge of the notch of the annular fixing groove is fixed to the upper guide plate.
[0012] The upper guide plate and the lower adjustable guide plate are made of carbon steel.
[0013] The process of adjusting the glue shape by using the FFU rectifier plate includes the following steps:
[0014] (1) Set the environment inside the glue coating chamber to meet the glue coating conditions, including temperature, humidity and wind speed, and the FFU controls the wind speed;
[0015] (2) Install the upper guide plate on the air outlet surface of the filter bottom of the FFU, so that the upper guide plate is parallel to the bottom surface of the FFU and fits tightly to the bottom surface of the FFU to prevent air leakage from the side wall;
[0016] (3) installing the lower adjustable guide plate to the upper guide plate, the downward vertical projection of the center of the circular baffle coincides with the center of the wafer, and the circular baffle and the annular baffle are concentric;
[0017] (4) By adjusting the overlap position of the guide holes on the central wafer and the guide holes on the upper guide plate, the airflow size at the center of the wafer is changed, thereby changing the film thickness at the center of the wafer; by adjusting the overlap position of the guide holes on the annular baffle and the guide holes on the upper guide plate, the airflow size at the edge of the wafer is changed, thereby changing the film thickness at the edge of the wafer.
[0018] The advantages and beneficial effects of the present invention are as follows:
[0019] 1. The present invention changes the airflow environment of the glue coating cavity by designing an FFU rectifier plate with a specific structure, thereby realizing zoning control of the airflow, which is used to control the glue coating film thickness at the center and edge of the wafer.
[0020] 2. By changing the airflow environment of the cavity, the consistency problem of multiple cavities can be improved more easily, so that the consistency of each cavity meets the process requirements and has strong stability. In a steady-state environment, the film thickness is not easy to change. BRIEF DESCRIPTION OF THE DRAWINGS
[0021] Figure 1 Schematic diagram of the placement of the circular baffle and the upper rectifier plate.
[0022] Figure 2 Schematic diagram of the placement of the annular baffle and the upper rectifier plate.
[0023] Figure 3 Schematic diagram of the annular baffle structure.
[0024] Figure 4 Schematic diagram of the annular fixing groove structure of the annular baffle (longitudinal section view).
[0025] In the figure: 1-upper guide plate; 2-circular baffle; 3-annular baffle; 301-annular fixing groove; 302-convex edge. DETAILED DESCRIPTION
[0026] The present invention is described in detail below with reference to the accompanying drawings and embodiments.
[0027] The present invention provides an FFU rectifier plate for airflow zoning control and a glue coating process for adjusting the glue shape, such as Figure 1-4 As shown, the FFU rectifier plate for airflow partition regulation includes an upper guide plate 1 and a lower adjustable guide plate; the upper guide plate is installed on the bottom surface of the FFU, and the FFU is a fan filter unit, including a fan above and a filter below, and the bottom surface of the FFU refers to the air outlet surface at the bottom of the filter. The upper guide plate is installed parallel to the bottom surface of the FFU and is in close contact with the bottom surface of the FFU. The lower adjustable guide plate is installed below the upper guide plate; the lower adjustable guide plate includes a circular baffle 2 and at least one annular baffle 3, the circular baffle and the annular baffle are concentric, the annular baffle is arranged on the outer periphery of the circular baffle, and the inner diameter of the annular baffle is greater than the diameter of the circular baffle. A plurality of guide holes of the same diameter are evenly distributed on the upper guide plate, the circular baffle and the annular baffle, and the diameter of the guide hole is 0.3-2mm.
[0028] The wafer to be spin-coated is placed below the lower adjustable guide plate, and the downward vertical projections of the centers of the circular baffle and the annular baffle coincide with the center of the wafer.
[0029] The circular baffle can rotate around the center of the circle (manually adjusted), and by rotating at different angles, the holes on the circular baffle can completely overlap or partially overlap with the holes at the corresponding positions on the upper guide plate, thereby controlling the size of the airflow output to the center of the wafer, and then adjusting the glue shape at the center of the wafer; the annular baffle can rotate around the center of the annular baffle (manually adjusted), and by rotating at different angles, the holes on the annular baffle can completely overlap or partially overlap with the holes at the corresponding positions on the upper guide plate, thereby controlling the airflow environment output to the edge of the wafer, and then achieving control of the glue shape at the edge of the wafer.
[0030] The circular baffle can be fixed on the upper guide plate by bolts. For example, a bolt hole is set at the center of the circular baffle, and the bolt is fixed on the upper guide plate through the bolt hole. After manually adjusting the circular baffle to a suitable position, the bolt is tightened to fix it.
[0031] The annular baffle comprises an annular sheet and an annular fixing groove 301, a plurality of guide holes are arranged on the annular sheet, the notch of the annular fixing groove faces downward, and the lower edge of the notch is bent inward 90° to form an inward convex edge 302; the annular sheet is placed on the convex edge in the annular fixing groove, and the position of the annular sheet can be manually adjusted to make the degree of overlap between the guide holes on the annular sheet and the holes at the corresponding positions on the upper guide plate different; the upper edge of the notch of the annular fixing groove is fixed to the upper guide plate (it can also be fixed by bolts, etc.). The material of the upper guide plate and the lower adjustable guide plate is required to be wear-resistant and not chipped to prevent the generation of particles during the adjustment process, such as 20# carbon steel.
[0032] The process of adjusting the glue shape by using the FFU rectifier plate includes the following steps:
[0033] (1) Set the environment inside the glue coating chamber to meet the glue coating conditions, including temperature, humidity and wind speed, and the FFU controls the wind speed;
[0034] (2) Install the upper guide plate on the air outlet surface of the filter bottom of the FFU, so that the upper guide plate is parallel to the bottom surface of the FFU and fits tightly to the bottom surface of the FFU to prevent air leakage from the side wall;
[0035] (3) installing the lower adjustable guide plate to the upper guide plate, the downward vertical projection of the center of the circular baffle coincides with the center of the wafer, and the circular baffle and the annular baffle are concentric;
[0036] (4) By adjusting the overlap position of the guide holes on the central wafer and the guide holes on the upper guide plate, the airflow size at the center of the wafer is changed, thereby changing the film thickness at the center of the wafer; by adjusting the overlap position of the guide holes on the annular baffle and the guide holes on the upper guide plate, the airflow size at the edge of the wafer is changed, thereby changing the film thickness at the edge of the wafer.
[0037] Embodiment 1:
[0038] This embodiment is a glue-splitting process for adjusting the glue shape by using the FFU rectifier plate, and the specific process is as follows:
[0039] 1. Set the internal environment of the gluing chamber to meet the gluing conditions, including temperature, humidity and wind speed;
[0040] 2. Collect the wafer film thickness data in the three glue coating units when the FFU rectifier board is not installed;
[0041] 3. Install the upper guide plate under the FFU, and then install the lower adjustable guide plate to the upper guide plate. The circular baffle and the annular baffle must be completely concentric with the wafer below during installation.
[0042] 4. By adjusting the degree of overlap between the central circular baffle and the upper hole on the upper guide plate, the airflow size at the center of the wafer is changed, thereby changing the film thickness at the center; after the change is completed, the cavity environment is restored so that the temperature and humidity in the cavity meet the process requirements, and the film thickness data after changing a single condition is collected.
[0043] 5. By adjusting the overlap between the annular baffle and the upper hole of the upper guide plate, the airflow size at the edge of the wafer is changed, thereby changing the film thickness at the edge of the wafer; after the change is completed, the cavity environment is restored so that the cavity environment (temperature and humidity) meets the process requirements, and the film thickness data after changing a single condition is collected.
[0044] 6. After adjusting the first single-cavity film thickness process to meet the requirements, adjust the other cavities (second and third cavities) to the same environment as the adjusted first cavity, and then collect the film thickness data of the three coating units for comparison.
[0045] Fine-tune the adjustable guide plates above the second and third cavities so that their process data are the same as those of the first cavity.
[0046] The present invention can improve the consistency problem of multiple cavities more simply by changing the airflow environment of the cavity, so that the consistency of each cavity meets the process requirements and has strong stability. In a steady-state environment, the film thickness is not easy to change.
Claims
1. An FFU rectifier plate for airflow zoning control, characterized in that: The FFU rectifier plate includes an upper guide plate and a lower adjustable guide plate; wherein: the upper guide plate is installed below the FFU, the upper guide plate is installed parallel to the bottom surface of the FFU and is in close contact with the bottom surface of the FFU; the lower adjustable guide plate is installed below the upper guide plate; the lower adjustable guide plate includes a circular baffle and at least one annular baffle, the circular baffle and the annular baffle are concentric, and the annular baffle is arranged on the outer periphery of the circular baffle; The upper guide plate, the circular baffle and the annular baffle are evenly distributed with a plurality of guide holes with the same diameter, and the diameter of the guide holes is 0.3-2 mm; The circular baffle can rotate around the center of the circle, and the size of the airflow output to the center of the wafer can be controlled by rotating at different angles, thereby adjusting the glue shape at the center of the wafer; the annular baffle can rotate around the center of the annular baffle, and the airflow environment output to the position around the center of the wafer can be controlled by rotating at different angles, thereby achieving control of the glue shape at the edge of the wafer.
2. The FFU rectifier plate for airflow zoning control according to claim 1 is characterized in that: The wafer to be spin-coated is placed below the lower adjustable guide plate, and the downward vertical projection of the center of the circular baffle of the lower adjustable guide plate coincides with the center of the wafer.
3. The FFU rectifier plate for airflow zoning control according to claim 1 is characterized in that: A bolt hole is arranged at the center of the circular baffle, and the circular baffle is fixed to the upper guide plate by bolts. After manually adjusting the overlap degree between the hole on the circular baffle and the hole at the corresponding position on the upper guide plate, the bolts are tightened to fix it.
4. The FFU rectifier plate for airflow zoning control according to claim 1 is characterized in that: The annular baffle comprises an annular sheet and an annular fixing groove, a plurality of guide holes are arranged on the annular sheet, the notch of the annular fixing groove faces downward, and the lower edge of the notch is bent inward 90° to form an inward convex edge; the annular sheet is placed on the convex edge in the annular fixing groove, and the position of the annular sheet can be manually adjusted to make the degree of overlap between the guide holes on the annular sheet and the holes at corresponding positions on the upper guide plate different; the upper edge of the notch of the annular fixing groove is fixed to the upper guide plate.
5. The FFU rectifier plate for airflow zoning control according to claim 1 is characterized in that: The upper guide plate and the lower adjustable guide plate are made of carbon steel.
6. A glue-splitting process for adjusting glue shape by using the FFU rectifier plate according to any one of claims 1 to 5, characterized in that: The process includes the following steps: (1) Set the environment inside the glue coating chamber to meet the glue coating conditions, including temperature, humidity and wind speed, and the FFU controls the wind speed; (2) Install the upper guide plate on the air outlet surface of the filter bottom of the FFU, so that the upper guide plate is parallel to the bottom surface of the FFU and fits tightly to the bottom surface of the FFU to prevent air leakage from the side wall; (3) Install the lower adjustable guide plate to the upper guide plate, so that the downward vertical projection of the center of the circular baffle coincides with the center of the wafer, and the circular baffle and the annular baffle are concentric; (4) By adjusting the overlap position of the guide holes on the central wafer and the guide holes on the upper guide plate, the airflow size at the center of the wafer is changed, thereby changing the film thickness at the center of the wafer; by adjusting the overlap position of the guide holes on the annular baffle and the guide holes on the upper guide plate, the airflow size at the edge of the wafer is changed, thereby changing the film thickness at the edge of the wafer.
Citation Information
Patent Citations
Single-air-outlet spin-coating development cavity
CN104977818A
Microenvironment control system
CN105652790A
Device for changing gas flow mode, and wafer processing method and equipment
CN105742203A
Glue coating development process module and control method for module internal environment parameters
CN106610568A
Gumming machine system capable of controlling photoresist sputtering
CN107783374A
Cited By
Gluing method for leveling surface of photoresist by utilizing airflow and liquid medicine steam
CN122018235A