A band-stop filter and a method for manufacturing the same
By embedding the coplanar waveguide and MEMS bridge with resonant structure in the metamaterial filter, the problems of slow tuning speed and high loss in the prior art are solved, and the rapid tuning and low loss of the metamaterial filter are achieved, which is suitable for Ka Tunable band-stop filter design in bands.
Patent Information
- Application Number
- CN202110246236.3
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2021-03-05
- Publication Date
- 2024-12-03
- Estimated Expiration
- 2041-03-05
AI Technical Summary
The tuning speed of existing metamaterial filters is slow and have high losses, making it difficult to dynamically adjust the response characteristics of metamaterial structures, affecting their practicality.
A band-stop filter is designed, and the expansion of the tuning range and the reduction of loss is achieved by embedding the coplanar waveguide and MEMS bridge of the resonant structure in the metamaterial structure. It is suitable for Compatibility of integrated circuits.
It achieves the improvement of tuning speed and the reduction of loss, expands the tuning range, is suitable for the Ka band, and has good compatibility and stability.
Smart Images

Figure CN112864551B_ABST
Abstract
Description
Technical Field
[0001] The embodiments of the present invention relate to the technical field of filters, and in particular to a band-stop filter and a manufacturing method thereof. Background Art
[0002] Artificial materials have unique electromagnetic properties that are not easily observed in nature and are therefore theoretically postulated as metamaterials by Viselager. Currently, metamaterial filters can be realized by two different approaches, one is the CL loading approach and the other is the resonant transmission line approach. The former depicts a transmission line loaded with series interdigital capacitors and shunt inductors, while the latter involves the use of resonant metamaterial structures. In both approaches, composite right-left-handed (CRLH) transmission lines are realized, in which the negative refractive index leads to backward wave propagation around the resonant frequency. The resonant approach is preferred over the CL loading approach because of the inherent resonant properties present in such metamaterial structures, resulting in a sharp cutoff around the resonant frequency of the filter.
[0003] Based on the above-mentioned problems that may arise in metamaterial filters, in order to dynamically adjust the response characteristics of the metamaterial structure and increase the practicality of the metamaterial filter, tunability is added to the metamaterial filter. Generally speaking, different physical effects and materials are used through tunable microwave components to achieve the desired tuning range. However, at present, tunable microwave components using magnetic components usually require large control power and are bulky. Although liquid crystals have low losses, the tuning speed is slow. Therefore, the problems faced by the tunability of the resonant frequency of metamaterial filters have not been truly solved. Summary of the invention
[0004] The embodiment of the present invention provides a band-stop filter and a manufacturing method thereof, so as to improve the tuning speed and reduce the loss, have a wide application range, and achieve the compatibility of integrated circuits.
[0005] In a first aspect, an embodiment of the present invention provides a band-stop filter, the band-stop filter comprising:
[0006] a first substrate and a second substrate;
[0007] The first substrate comprises a first base substrate, a first metal layer located on one side of the first base substrate, and a first bonding pin and a second bonding pin arranged on a side of the first metal layer away from the first base substrate; a metamaterial structure is formed on a side of the first metal layer away from the first base substrate; a height of the metamaterial structure is g1, a height of the first metal layer is g2, and g1<g2;
[0008] The second substrate comprises a second base substrate, a third bonding pin and a fourth bonding pin located on one side of the second base substrate, and a second metal layer and a third metal layer connecting the third bonding pin and the fourth bonding pin;
[0009] The first bonding pin is bonded to the third bonding pin, and the second bonding pin is bonded to the fourth bonding pin, so as to bond the first substrate and the second substrate.
[0010] Further, the first substrate includes a first dielectric layer and a first oxide layer located on one side of the first dielectric layer;
[0011] The second substrate includes a second dielectric layer and a second oxide layer located on one side of the second dielectric layer.
[0012] Further, the first oxide layer includes a first oxide isolation layer and a second oxide isolation layer;
[0013] The first oxidized isolation layer is disposed on a side of the first dielectric layer close to the first metal layer, and the second oxidized isolation layer is disposed on a side of the first oxidized isolation layer away from the first dielectric layer.
[0014] Furthermore, the metamaterial structure includes a ground layer located on one side of the first substrate and a signal layer arranged on a side of the ground layer away from the first substrate.
[0015] Furthermore, the band-stop filter further includes an isolation layer;
[0016] The isolation layer is arranged on a side of the metamaterial structure away from the first substrate, and a vertical projection of the isolation layer on a plane where the metamaterial structure is located overlaps with vertical projections of the second metal layer and the third metal layer on the plane where the metamaterial structure is located.
[0017] Furthermore, the metamaterial structure forms a coplanar waveguide embedded in a resonant structure on a side away from the first substrate;
[0018] The resonant structure includes a first inductor, a first capacitor and a first resistor connected in parallel.
[0019] Furthermore, the second metal layer forms a first bridge on a side facing away from the second substrate;
[0020] The third metal layer forms a second bridge on a side facing away from the second substrate.
[0021] Further, the first bridge connector includes a first bridge inductor, a first bridge capacitor and a first bridge resistor connected in series;
[0022] The second bridge connector includes a second bridge inductor, a second bridge capacitor, and a second bridge resistor connected in series.
[0023] In a second aspect, an embodiment of the present invention further provides a method for manufacturing a band-stop filter, the method for manufacturing the band-stop filter comprising:
[0024] Providing a first substrate, and forming a first metal layer on one side of the first substrate;
[0025] A first bonding pin and a second bonding pin on a side of the first metal layer facing away from the first substrate;
[0026] Wherein, a metamaterial structure is formed on the side of the first metal layer away from the first substrate; the height of the metamaterial structure is g1, the height of the first metal layer is g2, and g1<g2;
[0027] The first substrate comprises the first base substrate, the first metal layer, the first bonding pin and the second bonding pin;
[0028] Providing a second substrate substrate, a third bonding pin and a fourth bonding pin on one side of the second substrate substrate;
[0029] forming a second metal layer and a third metal layer connecting the third bonding pin and the fourth bonding pin;
[0030] The second substrate comprises the second base substrate, the third bonding pin, the fourth bonding pin, the second metal layer and the third metal layer;
[0031] The first bonding pin is bonded to the third bonding pin, and the second bonding pin is bonded to the fourth bonding pin, so as to bond the first substrate and the second substrate.
[0032] Furthermore, after bonding the first substrate and the second substrate, the method further includes:
[0033] A first groove is formed on a side of the first substrate facing away from the second substrate, and a second groove is formed on a side of the second substrate facing away from the first substrate.
[0034] The technical solution of the embodiment of the present invention, the band-stop filter includes a first substrate and a second substrate; the first substrate includes a first base substrate, a first metal layer located on one side of the first base substrate, and a first bonding pin and a second bonding pin arranged on the side of the first metal layer away from the first base substrate; the first metal layer forms a metamaterial structure on the side away from the first base substrate; the height of the metamaterial structure is g1, the height of the first metal layer is g2, g1<g2; the second substrate includes a second base substrate, a third bonding pin and a fourth bonding pin located on one side of the second base substrate, and a second metal layer and a third metal layer connecting the third bonding pin and the fourth bonding pin; the first bonding pin is bonded to the third bonding pin, and the second bonding pin is bonded to the fourth bonding pin to bond the first substrate and the second substrate. The problem of unstable tuning range and slow tuning speed in the prior art is solved, so as to improve the tuning speed and reduce the loss, have a wide range of applications, and achieve compatibility of integrated circuits. BRIEF DESCRIPTION OF THE DRAWINGS
[0035] Figure 1 is a schematic diagram of a cross-sectional structure of a band-stop filter provided by an embodiment of the present invention;
[0036] Figure 2 is a schematic diagram of a three-dimensional structure of a band-stop filter before bonding provided by an embodiment of the present invention;
[0037] Figure 3 is a schematic diagram of a cross-sectional structure of a band-stop filter provided by an embodiment of the present invention;
[0038] Figure 4 A schematic diagram of an equivalent circuit structure of a band-stop filter provided by an embodiment of the present invention;
[0039] Figure 5 A schematic diagram of a top view structure of a band-stop filter provided by an embodiment of the present invention;
[0040] Figure 6 It is a flow chart of a method for manufacturing a band-stop filter provided by an embodiment of the present invention. DETAILED DESCRIPTION
[0041] In order to make the purpose, technical solution and advantages of the present invention clearer, the specific embodiments of the present invention are further described in detail below in conjunction with the accompanying drawings. It should be understood that the specific embodiments described here are only used to explain the present invention, rather than to limit the present invention.
[0042] It should also be noted that, for ease of description, only the part relevant to the present invention but not all content is shown in the accompanying drawings. It should be mentioned before discussing exemplary embodiments in more detail that some exemplary embodiments are described as processing or methods depicted as flow charts. Although the flow chart describes each operation (or step) as sequential processing, many operations therein can be implemented in parallel, concurrently or simultaneously. In addition, the order of each operation can be rearranged. When its operation is completed, the processing can be terminated, but it can also have additional steps not included in the accompanying drawings. The processing can correspond to methods, functions, procedures, subroutines, subprograms, etc.
[0043] The embodiment of the present invention provides a band-stop filter, which can be applied to the filter to achieve a desired tunable range. Figure 1 A schematic cross-sectional structure diagram of a band-stop filter provided by an embodiment of the present invention, Figure 2 A schematic diagram of a three-dimensional structure of a band-stop filter before bonding provided by an embodiment of the present invention, see Figure 1 and Figure 2 , the specific structure of the band-stop filter includes the following:
[0044] A first substrate 100 and a second substrate 200;
[0045] The first substrate 100 includes a first base substrate 110, a first metal layer 120 located on one side of the first base substrate 110, and a first bonding pin 130 and a second bonding pin 140 arranged on the side of the first metal layer 120 away from the first base substrate 110; a metamaterial structure 150 is formed on the side of the first metal layer 120 away from the first base substrate 110; the height of the metamaterial structure 150 is g1, the height of the first metal layer is g2, and g1<g2;
[0046] The second substrate 200 includes a second base substrate 210, a third bonding pin 220 and a fourth bonding pin 230 located on one side of the second base substrate 210, and a second metal layer 240 and a third metal layer 250 connecting the third bonding pin 220 and the fourth bonding pin 230;
[0047] The first bonding pin 130 is bonded to the third bonding pin 220 , and the second bonding pin 140 is bonded to the fourth bonding pin 230 , so as to bond the first substrate 100 and the second substrate 200 .
[0048] The first substrate 110 is a low dielectric constant, high resistivity silicon substrate, and is used to provide support and protection for the first metal layer 120, while providing mechanical stability for the band-stop filter provided in this embodiment.
[0049] A hollow pattern is formed on the side of the first metal layer 120 away from the first base substrate 110, that is, Figure 1 The metamaterial structure 150 shown, in this embodiment, forms a coplanar waveguide embedded with a resonant structure in the metamaterial structure 150 .
[0050] The second base substrate 210 is a low dielectric constant, high resistivity silicon substrate, and is used to provide support and protection for the third bonding pin 220 , the fourth bonding pin, the second metal layer 240 and the third metal layer 250 .
[0051] Continue to see Figure 2 The first bonding pin 130 is bonded to the third bonding pin 220, and the second bonding pin 140 is bonded to the fourth bonding pin 230. The specific bonding processing method is not limited in this embodiment. Optionally, the first bonding pin 130 is bonded to the third bonding pin 220, and the second bonding pin 140 is bonded to the fourth bonding pin 230, so as to bond the first substrate 100 and the second substrate 200 by a micromachining method to obtain the band-stop filter provided in this embodiment.
[0052] Continue to see Figure 1 After the first substrate 100 and the second substrate 200 are bonded, the silicon in the first substrate 110 and the second substrate 210 below and above the center line of the coplanar waveguide in the metamaterial structure 150 is removed. The coplanar waveguide is an edge-coupled device. After the silicon is removed from the above volume, a virtual air base can be formed. In this embodiment, a tunable band-stop filter with a tuning range of 13% from 28 GHz to 32 GHz and suitable for Ka band is realized through the resonant structure embedded in the coplanar waveguide, the second metal layer 240 and the third metal layer 250, and the virtual air base. The design and production of the band-stop filter are further explained below.
[0053] Figure 3 A schematic diagram of a cross-sectional structure of a band-stop filter provided by an embodiment of the present invention, see Figure 3 , based on the above embodiment, the first substrate 110 includes a first dielectric layer 111 and a first oxide layer 112 located on one side of the first dielectric layer 111;
[0054] The second substrate 210 includes a second dielectric layer 211 and a second oxide layer 212 located on one side of the second dielectric layer 211 .
[0055] The material of the first dielectric layer 111 can be a micro-mechanical silicon substrate, and an oxidation isolation layer 113 can be formed on the side of the first dielectric layer 111 away from the first oxide layer 112, and the oxidation isolation layer 113 is used to protect the micro-mechanical silicon substrate. Optionally, the thickness of the first dielectric layer 111 can be 275 μm, and the oxidation isolation layer 113 can be made by oxidizing silicon dioxide using an existing manufacturing process, and the thickness of the oxidation isolation layer 113 can be 1 μm. This embodiment does not impose any restrictions on the specific manufacturing process of the oxidation isolation layer 113.
[0056] In order to adapt to the trend of thinning electronic products, the thickness of the first base substrate 110 may be 276 μm, so as to achieve the slimming of the first base substrate 110 while having good mechanical stability and protection performance.
[0057] The material of the second dielectric layer 211 can be a micro-mechanical silicon substrate, and an oxidation isolation layer 213 can be formed on the side of the second dielectric layer 211 away from the second oxide layer 212, and the oxidation isolation layer 213 is used to protect the micro-mechanical silicon substrate. Optionally, the thickness of the second dielectric layer 211 can be 275 μm, and the oxidation isolation layer 213 can be made by oxidizing silicon dioxide using an existing manufacturing process, and the thickness of the oxidation isolation layer 213 can be 1 μm. This embodiment does not impose any restrictions on the specific manufacturing process of the oxidation isolation layer 213.
[0058] In order to adapt to the trend of thinning electronic products, the thickness of the second base substrate 210 can be 276 μm, and the second base substrate 210 can be made thinner while having good mechanical stability and protection performance.
[0059] Continue to see Figure 3 On the basis of the above embodiment, the first oxide layer 112 includes a first oxide isolation layer 1121 and a second oxide isolation layer 1122;
[0060] The first oxidized isolation layer 1121 is disposed on a side of the first dielectric layer 111 close to the first metal layer 120 , and the second oxidized isolation layer 1122 is disposed on a side of the first oxidized isolation layer 1121 away from the first dielectric layer 111 .
[0061] The first oxidized isolation layer 1121 is formed on the first dielectric layer 111 by oxidizing through thermal decomposition. The first oxidized isolation layer 1121 may also be formed by other processes. In this embodiment, no specific limitation is imposed on the preparation process of the first oxidized isolation layer 1121.
[0062] The first oxide isolation layer 1121 is used to prevent the resonant structure from short-circuiting with the third metal layer 240 and the fourth metal layer 250. In the present invention, the material of the first oxide isolation layer 1121 is silicon dioxide, and the thickness of the first oxide isolation layer 1121 is 1 μm.
[0063] A second oxidation isolation layer 1122 is formed by hot wire chemical vapor deposition coating on the side of the first oxidation isolation layer 1121 away from the first dielectric layer 111. The second oxidation isolation layer 1122 can also be formed by other processes. In this embodiment, no specific limitation is imposed on the preparation process of the first oxidation isolation layer 1121.
[0064] The second oxide isolation layer 1122 is used to provide mechanical strength for the resonant structure. In the present invention, the material of the second oxide isolation layer 1122 is silicon nitride, and the thickness of the second oxide isolation layer 1122 is 0.8 μm.
[0065] Continue to see Figure 1 On the basis of the above embodiment, the metamaterial structure 150 includes a ground layer located on one side of the first substrate 110 and a signal layer arranged on a side of the ground layer away from the first substrate 110 .
[0066] Continue to see Figure 1 and Figure 2 , based on the above embodiment, the band-stop filter further includes an isolation layer 160;
[0067] The isolation layer 160 is disposed on a side of the metamaterial structure 150 away from the first substrate 110 , and a vertical projection of the isolation layer 160 on the plane where the metamaterial structure 150 is located overlaps with a vertical projection of the second metal layer 240 and the third metal layer 250 on the plane where the metamaterial structure 150 is located.
[0068] The isolation layer 160 may be sputtered on the side of the metamaterial structure 150 away from the first substrate 110 , that is, the center of the coplanar waveguide, through a silicon dioxide isolator by a sputtering process to prevent the two electrodes from being short-circuited during startup.
[0069] The isolation layer 160 may be made of silicon dioxide, and the thickness of the isolation layer 160 is 0.1 μm.
[0070] Figure 4 A schematic diagram of an equivalent circuit structure of a band-stop filter provided by an embodiment of the present invention, see Figure 4 and Figure 1 , based on the above embodiment, the metamaterial structure 150 forms a coplanar waveguide embedded in a resonant structure on the side away from the first substrate 110;
[0071] The resonant structure includes a first inductor L, a first capacitor C and a first resistor R connected in parallel.
[0072] Among them, the coplanar waveguide of the band-stop filter uses a metamaterial structure as a frequency-selective geometry, see Figure 1 The silicon removed from the first substrate 110 is removed from below / above the coplanar waveguide centerline and a portion of the coplanar waveguide ground layer, thereby forming a virtual air base.
[0073] In this embodiment, the resonant structure is composed of a CLR resonant loop, and the resonant structure is used to provide a shunt load on the transmission line corresponding to the band-stop filter.
[0074] Since the metamaterial structure is etched on the signal line of the coplanar waveguide, the CLR energy reservoir appears to be connected in parallel with the transmission line of the coplanar waveguide. t Series connection.
[0075] Continue to see Figure 2 , based on the above embodiment, the second metal layer 240 forms a first bridge on the side away from the second substrate 210;
[0076] The third metal layer 250 forms a second bridge on a side away from the second substrate 210 .
[0077] In this embodiment, the coplanar waveguide of the band-stop filter adopts a metamaterial structure as a frequency selective geometric body, and the coplanar waveguide achieves tunability by means of the second metal layer 240 and the third metal layer 250 .
[0078] The first bridge and the second bridge are two MEMS bridges for improving the quality factor of the band stop filter.
[0079] Continue to see Figure 4 Based on the above embodiment, the first bridge connector includes a first bridge inductor L connected in series. h 、First bridge capacitor C c and the first bridge resistor R b ;
[0080] The second bridge connector includes a second bridge inductor L connected in series. b , the second bridge capacitor C c and the second bridge resistor R b .
[0081] Specifically, the shunt resistor R in the first bridge and the second bridge b The shunt load for any given transmission line is changed depending on the execution state of the first bridge and the second bridge. Therefore, when the MEMS bridge resistor is shunted and placed on the transmission line embedded in the metamaterial structure, the effective shunt load of the device will change, which will cause the resonant frequency under different action states to change.
[0082] Continue to see Figure 4, it can be seen that the contribution of the metamaterial structure to the shunt impedance is fixed. The bridge capacitance varies according to its height above the transmission line and changes the total shunt loading of the transmission line.
[0083] pass Figure 4 After basic circuit analysis, the parallel impedance Z in the shunt path is obtained according to the following formula: sh ,
[0084]
[0085] Among them, C sh =C t +C c and C bu / bd is the bridge capacitance in the upper and lower states.
[0086] Since the bridge is placed in different working states according to different capacitance values, if the capacitance value is set to the capacitance value of the upper state, the bridge is placed in the upper state, otherwise it is placed in the lower state. Generally speaking, the capacitance value is controlled by the MEMS bridge switch.
[0087] Furthermore, the tunability of the band-stop coordinator provided in this embodiment is determined by the bridge capacitance C b To obtain a higher tuning range, C b Should be better than the line capacitance C t and the resonator capacitance C c Therefore, tunability is achieved with the help of varactors in the first bridge and the second bridge.
[0088] It should be noted that the sizes of the first bridge and the second bridge are mainly determined by the static (eg, driving voltage) and dynamic (eg, switching time) switching requirements of the final device.
[0089] The standard aspect ratio of the first bridge and the second bridge is in the range of 2 to 3, providing a stand-off capacitance in the range of 30–140 fF for a bridge height of 2-3 μm above the coplanar waveguide. sh The resonant frequency (f unloaded / f loaded_up ), varies with the fraction of the capacitive loading on the bridge.
[0090] In this embodiment, the resonant frequency f unloaded is determined by the resonant frequency of the metamaterial structure of the varactor diode without the first bridge and the second bridge, and the resonant frequency f loaded_up Determined by the resonant frequency of the varactor diode under loading (maximum g0 = 3μm), the following formula can be obtained:
[0091]
[0092]
[0093] From the above formula for resonant frequency, it can be clearly seen that for higher capacitance values C sh , the capacitive load of the bridge has almost no effect on the metamaterial-loaded transmission line.
[0094] Therefore, in order to reduce C t and C c The first substrate 110 is selected from a substrate with a lower dielectric constant value (ideally, air). Finite element simulation shows that the resonant frequency drops by 15-20 GHz. When a coplanar waveguide embedded with a metamaterial on a low dielectric constant substrate is subjected to a capacitive load of 30-140 fF, the above result will occur. Therefore, in order to obtain the Ka-band tunable band-stop filter with two memory characteristics provided in this embodiment, the bridgeless metal structure filter on the low dielectric constant substrate should resonate at 50-52 GHz.
[0095] It should also be noted that for the selection of the impedance of the unloaded coplanar waveguide, since the 50Ω characteristic impedance will be achieved after loading the resonant structure and the two MEMS bridges, Figure 4 It is obvious from the equivalent circuit that the resonant structure load will increase the line impedance, while the MEMS bridge load will reduce the line impedance. Since the resonant structure is located on a low dielectric constant substrate (approximately air in this case), the combined capacitance effect of the series capacitors is much smaller than the bridge capacitors. Therefore, W / S / W corresponds to 10 / 200 / 10μm on the first substrate substrate 110 resulting in an impedance of 64Ω, and the unloaded coplanar waveguide impedance needs to be maintained at a higher 50Ω.
[0096] Figure 5 A schematic diagram of a top view of a band-stop filter provided by an embodiment of the present invention, see Figure 5 , it can be seen that the resonant structure is composed of two U-shaped concentric structures. Since the metamaterial structure 150 is configured corresponding to W / S / W on the first substrate 110 and is metallized when formed, the resonant structure is etched out from the metallization.
[0097] Continue to see Figure 5 The resonant structure is patterned with the center line of the coplanar waveguide, and the length of the resonant structure, the width of the resonant structure, the width of the ring, and the spacing between the rings are L, T, c, and d, respectively.
[0098] Continue to see Figure 5 and Figure 3, based on the above embodiment, the first bridge and the second bridge are suspended at the air gap g0, and their length, width and thickness are l, b and t respectively (thickness is not shown in the figure). Removing silicon from the first base substrate 110 and the second base substrate 210 In order to manufacture the virtual air substrate 300, the removal of silicon occurs at a width of W win and length L win On two substrates
[0099] For further information, see Figure 5 A window S is opened on the second substrate 210 for detecting the characteristics of the device.
[0100] In this embodiment, bulk micromachining of silicon is proposed to obtain a virtual air substrate. Since the manufacturing method of the band-stop filter in this embodiment involves two bonded silicon wafers, the two silicon wafers must be micromachined. At the same time, conformal mapping is performed to calculate the size of the window used for micromachining.
[0101] For the transmission line of the coplanar waveguide, the total capacitance per unit length is the sum of the capacitance provided by the second substrate 210 and the first substrate 110. Since the conductivity of silicon is much greater than that of air, it can be assumed that the electric field through the air dielectric terminates at the silicon wall, and the capacitance caused by the air dielectric can be evaluated by a series of suitable configurations.
[0102] The capacitance provided by the virtual air substrate is for micro-machined windows of different widths (the width of the virtual air substrate is W win ) calculated, for a virtual air substrate width corresponding to 600 μm, the capacitance provided by the virtual air substrate is equal to the capacitance provided by the total air substrate.
[0103] After selecting a suitable coplanar waveguide configuration, the center frequency (with load) of the metamaterial structure composed of the resonant structure is selected to be 51 GHz, which will result in an upward float corresponding to the Ka-band frequency. The length L of the resonant structure depends on the unit cell length and is less than 1459 microns. Since the width of the CUSR is mainly determined by the width of the center line of the coplanar waveguide or the ground layer, the width is not analyzed parametrically. Table 1 below lists the optimal dimensions of the coplanar waveguide embedded in the resonant structure.
[0104] Table 1 Optimal dimensions of a coplanar waveguide embedded in a resonant structure
[0105]
[0106] Considering two MEMS bridges 400 μm apart in order to have a high quality factor and a small filter bandwidth, the optimal size of the corresponding MEMS bridge is shown in Table 2 below. The MEMS bridge will achieve a balance between the required excitation voltage and switching time at the current size.
[0107] Table 2 Optimal size of MEMS bridge
[0108]
[0109] The embodiment of the present invention provides a tunable band-stop filter with a tuning range of 13% in the range of 28 GHz to 32 GHz based on a metamaterial structure. It uses two silicon wafers to make a resonant structure embedded coplanar waveguide and a MEMS bridge. At the same time, in order to enhance the capacitive effect of the MEMS bridge on the coplanar waveguide embedded in the resonant structure, the silicon below the center line of the coplanar waveguide and a part of the coplanar waveguide ground layer are removed to create a virtual air substrate. The technical solution of the embodiment of the present invention also provides the details of the design and manufacturing steps of the tunable band-stop filter, which has a certain degree of repeatability. For details, refer to the following method for making the band-stop filter.
[0110] In order to realize the band-stop filter design of the embodiment of the present invention, a virtual air substrate is created for the coplanar waveguide based on the metamaterial embedded resonant structure. In order to produce the virtual air substrate, silicon needs to be removed from the bulk substrate, so bulk micromachining is the most suitable choice. For the single-wafer process, the MEMS bridge can be manufactured on a silicon substrate that has been micromachined, and the silicon substrate accommodates the coplanar waveguide embedded in the resonant structure. However, since the coplanar waveguide embedded in the resonant structure has been micromachined, any subsequent processing (such as lithography, etching, etc.) requires a virtual wafer. In addition, in order to realize the virtual air substrate through bulk micromachining, the metallization of the gold layer may be damaged due to long-term etching. In order to overcome the limitations of the single-wafer process, an embodiment of the present invention provides a method for manufacturing a band-stop filter, and the specific steps are as follows.
[0111] Figure 6 1 is a flow chart of a method for manufacturing a band-stop filter provided by an embodiment of the present invention. This embodiment is applicable to the case where the filter realizes a desired tunable range. The method for manufacturing the band-stop filter specifically includes the following steps:
[0112] S610: Provide a first substrate, and form a first metal layer on one side of the first substrate.
[0113] Among them, the first substrate includes a first dielectric layer and a first oxide layer located on one side of the first dielectric layer, the first oxide layer includes a first oxide isolation layer and a second oxide isolation layer; the first oxide isolation layer is arranged on the side of the first dielectric layer close to the first metal layer, and the second oxide isolation layer is arranged on the side of the first oxide isolation layer away from the first dielectric layer.
[0114] The first substrate is oxidized by pyrolysis to form a first oxide isolation layer, and then a second oxide isolation layer is formed by hot wire chemical vapor deposition coating. The first oxide isolation layer and the second oxide isolation layer provide mechanical stability for the subsequently formed resonant structure.
[0115] S620, forming a first bonding pin and a second bonding pin on a side of the first metal layer away from the first substrate;
[0116] The first metal layer forms a metamaterial structure on a side facing away from the first substrate; the height of the metamaterial structure is g1, the height of the first metal layer is g2, and g1<g2.
[0117] Specifically, a thin layer of Cr–Au is used as a seed layer, and 1 μm of gold is plated in KAu(CN)2 to obtain the metallization of the buried coplanar waveguide of the resonant structure, that is, to obtain the first metal layer forming the metamaterial structure.
[0118] After the resonant structure geometry is patterned, selective gold plating of the ground layer of the coplanar waveguide is completed to a height of 3.6 microns. In addition, without breaking the vacuum, a stack of Au-AuGe-Au (corresponding thicknesses of 100nm-200nm-100nm, respectively) layers is sequentially deposited by electron beam evaporation and patterned on the resonant structure ground layer by lift-off technology. Among them, the purpose of the first layer of evaporated gold is to reduce the roughness of the electroplated gold, while the last layer of evaporated gold is used to prevent oxidation of the AuGe eutectic layer. The stack has a melting temperature of about 360°C as two layers with AuGe eutectic (88% gold; 12% germanium).
[0119] It can be noted that the height difference between the resonant structure signal layer and the ground layer corresponds to a bridge height of 3 μm.
[0120] Furthermore, the band-stop filter also includes an isolation layer; the isolation layer is arranged on the side of the metamaterial structure away from the first substrate, and the vertical projection of the isolation layer on the plane where the metamaterial structure is located overlaps with the vertical projections of the second metal layer and the third metal layer on the plane where the metamaterial structure is located.
[0121] Specifically, the isolation layer is sputtered at the center of the coplanar waveguide to prevent the two electrodes from short-circuiting when starting. Figure 5 It can be seen that the vertical projection of the isolation layer on the plane where the metamaterial structure is located overlaps with the vertical projections of the second metal layer and the third metal layer on the plane where the metamaterial structure is located, but they are not completely overlapped, but only partially symmetrically overlapped.
[0122] The first substrate includes the first base substrate, the first metal layer, the first bonding pin and the second bonding pin.
[0123] S630, providing a second substrate, and providing a third bonding pin and a fourth bonding pin on one side of the second substrate.
[0124] The second substrate includes a second dielectric layer and a second oxide layer located on one side of the second dielectric layer.
[0125] Specifically, the second oxide layer is formed by oxidation, chromium-gold is sputtered, and then gold is electroplated to form a second dielectric layer to obtain the third bonding pin and the fourth bonding pin, which are then patterned.
[0126] S640, forming a second metal layer and a third metal layer connecting the third bonding pin and the fourth bonding pin.
[0127] Specifically, the second metal layer forms a first bridge on a side away from the second substrate, and the third metal layer forms a second bridge on a side away from the second substrate.
[0128] The second substrate includes the second base substrate, the third bonding pin, the fourth bonding pin, the second metal layer and the third metal layer.
[0129] S650, bond the first bonding pin to the third bonding pin, bond the second bonding pin to the fourth bonding pin, so as to bond the first substrate to the second substrate.
[0130] Continue to see Figure 5 , a hole with a size similar to L is opened on the back of the first substrate and the second substrate win and W win The corresponding windows are used for subsequent micromachining. The first substrate and the second substrate are then properly aligned in a wafer bonding machine so that they can be bonded at 400°C with a contact force of 1.5 kN at 20 cm 2 Bonding was performed in the area for 2 hours.
[0131] Furthermore, after bonding the first substrate and the second substrate, the method further includes:
[0132] A first groove is formed on a side of the first substrate facing away from the second substrate, and a second groove is formed on a side of the second substrate facing away from the first substrate.
[0133] Specifically, the silicon of the first substrate and the second substrate is removed from the center line of the coplanar waveguide and a portion of the ground layer of the coplanar waveguide to form a first groove and a second groove. The specific structures of the first groove and the second groove can be seen in Figure 1, to form a virtual air substrate, to improve the capacitance effect of the band-stop filter of the embodiment of the present invention, and further to obtain a tunable band-stop filter using a metamaterial structure and a MEMS bridge on a silicon substrate.
[0134] Note that the above are only preferred embodiments of the present invention and the technical principles used. Those skilled in the art will understand that the present invention is not limited to the specific embodiments described herein, and that various obvious changes, readjustments and substitutions can be made by those skilled in the art without departing from the scope of protection of the present invention. Therefore, although the present invention has been described in more detail through the above embodiments, the present invention is not limited to the above embodiments, and may include more other equivalent embodiments without departing from the concept of the present invention, and the scope of the present invention is determined by the scope of the appended claims.
Claims
1. A band-stop filter, characterized in that: include: a first substrate and a second substrate; The first substrate comprises a first base substrate, a first metal layer located on one side of the first base substrate, and a first bonding pin and a second bonding pin arranged on the side of the first metal layer away from the first base substrate; a metamaterial structure is formed on the side of the first metal layer away from the first base substrate; the height of the metamaterial structure is g1, the height of the first metal layer is g2, and g1<g2; wherein the first base substrate is a low dielectric constant, high resistivity silicon substrate; The second substrate comprises a second base substrate, a third bonding pin and a fourth bonding pin located on one side of the second base substrate, and a second metal layer and a third metal layer connecting the third bonding pin and the fourth bonding pin; The first bonding pin is bonded to the third bonding pin, and the second bonding pin is bonded to the fourth bonding pin, so as to bond the first substrate and the second substrate; The second metal layer forms a first bridge on a side facing away from the second substrate; The third metal layer forms a second bridge on a side away from the second substrate; The first bridge connector includes a first bridge inductor, a first bridge capacitor and a first bridge resistor connected in series; The second bridge connector includes a second bridge inductor, a second bridge capacitor, and a second bridge resistor connected in series.
2. The band-stop filter according to claim 1, characterized in that: The first substrate includes a first dielectric layer and a first oxide layer located on one side of the first dielectric layer; The second substrate includes a second dielectric layer and a second oxide layer located on one side of the second dielectric layer.
3. The band-stop filter according to claim 2, characterized in that: The first oxide layer includes a first oxide isolation layer and a second oxide isolation layer; The first oxidized isolation layer is disposed on a side of the first dielectric layer close to the first metal layer, and the second oxidized isolation layer is disposed on a side of the first oxidized isolation layer away from the first dielectric layer.
4. The band-stop filter according to claim 1, characterized in that: The metamaterial structure includes a ground layer located on one side of the first substrate and a signal layer arranged on a side of the ground layer away from the first substrate.
5. The band-stop filter according to claim 1, characterized in that: The band-stop filter further comprises an isolation layer; The isolation layer is arranged on a side of the metamaterial structure away from the first substrate, and a vertical projection of the isolation layer on a plane where the metamaterial structure is located overlaps with vertical projections of the second metal layer and the third metal layer on the plane where the metamaterial structure is located.
6. The band-stop filter according to claim 1, characterized in that: The metamaterial structure forms a coplanar waveguide embedded in a resonant structure on a side away from the first substrate; The resonant structure includes a first inductor, a first capacitor and a first resistor connected in parallel.
7. A method for manufacturing a band-stop filter, characterized in that: include: Providing a first substrate, and forming a first metal layer on one side of the first substrate; A first bonding pin and a second bonding pin on a side of the first metal layer facing away from the first substrate; Wherein, a metamaterial structure is formed on the side of the first metal layer away from the first substrate; the height of the metamaterial structure is g1, the height of the first metal layer is g2, and g1<g2; The first substrate comprises the first base substrate, the first metal layer, the first bonding pin and the second bonding pin; Providing a second substrate substrate, a third bonding pin and a fourth bonding pin on one side of the second substrate substrate; A second metal layer and a third metal layer are formed to connect the third bonding pin and the fourth bonding pin; wherein the second metal layer forms a first bridge on a side away from the second substrate; the third metal layer forms a second bridge on a side away from the second substrate; the first bridge comprises a first bridge inductor, a first bridge capacitor and a first bridge resistor connected in series; the second bridge comprises a second bridge inductor, a second bridge capacitor and a second bridge resistor connected in series; The second substrate comprises the second base substrate, the third bonding pin, the fourth bonding pin, the second metal layer and the third metal layer; The first bonding pin is bonded to the third bonding pin, and the second bonding pin is bonded to the fourth bonding pin, so as to bond the first substrate and the second substrate.
8. The method for manufacturing a band-stop filter according to claim 7, characterized in that: After bonding the first substrate and the second substrate, the method further includes: A first groove is formed on a side of the first substrate facing away from the second substrate, and a second groove is formed on a side of the second substrate facing away from the first substrate.