Three-dimensional flash memory based on ferroelectric materials and its fabrication
By using ferroelectric film and CAAC crystal structure materials in three-dimensional flash memory, the problems of horizontal descaling and high operating voltage in the existing technology are solved, the integration level and reliability are improved, and multi-layer data storage is realized. .
Patent Information
- Application Number
- CN201980089104.5
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Priority Date
- 2019-07-26
- Filing Date
- 2019-12-26
- Publication Date
- 2024-10-15
- Estimated Expiration
- 2039-12-26
AI Technical Summary
Existing three-dimensional flash memory is difficult to descale in the horizontal direction and requires high operating voltage, which affects its performance and reliability.
The ferroelectric film formed by a single film is used as the data storage area, and the channel layer is formed by zinc, indium, gallium, Group 4 semiconductor materials with CAAC crystal structure or semiconductor materials containing Group 3-5 compounds to increase unit current and reduce leakage. Current, and multi-layered data storage is achieved by adjusting the thickness and polarization charge of the ferroelectric film.
It improves the integration level in the horizontal direction, reduces the operating voltage, enhances reliability and temperature resistance, and realizes a multi-layered data storage structure based on ferroelectric film.
Smart Images

Figure CN113330566B_ABST
Abstract
Description
Technical Field
[0001] The following embodiments relate to a three-dimensional flash memory, and more particularly, to a three-dimensional flash memory with improved integration in a horizontal direction and a method for manufacturing the same. Background Art
[0002] Flash memory devices are electrically erasable programmable read only memory (EEPRROM), which can be widely used in many aspects, such as computers, digital cameras, MP3 players, game systems, memory sticks, etc. This flash memory device electrically controls the input and output of data through Fowler-Nordheim tunneling or hot electron injection.
[0003] Specifically, referring to the array of the conventional three-dimensional flash memory Figure 1 The array of the three-dimensional flash memory may include a common source line CSL, a bit line BL, and a plurality of cell strings CSTR arranged between the common source line CSL and the bit line BL.
[0004] A plurality of bit lines are arranged in a two-dimensional manner and are respectively connected to a plurality of cell strings CSTR in parallel. A plurality of cell strings CSTR may be connected to a common source line CSL in common. That is, a plurality of cell strings CSTR may be configured between a plurality of bit lines and a common source line CSL. In this case, there may be a plurality of common source lines CSL, and the plurality of common source lines CSL may be arranged in a two-dimensional manner. A voltage having the same voltage value may be applied to the plurality of common source lines CSL, or the plurality of common source lines CSL may be electrically controlled individually.
[0005] The plurality of cell strings CSTR respectively include: a ground selection transistor GST connected to a common source line CSL; a string selection transistor SST connected to a bit line BL; and a plurality of memory cell transistors MCT arranged between the plurality of ground selection transistors GST and the plurality of string selection transistors SST. Moreover, the ground selection transistor GST, the string selection transistor SST and the memory cell transistor MCT may be connected in series.
[0006] The common source line CSL can be commonly connected to the multiple sources of the multiple ground selection transistors GST. In addition, the ground selection line GSL, the multiple word lines WL0-WL3 and the multiple string selection lines SSL arranged between the common source line CSL and the bit line BL can be used as the multiple electrode layers of the ground selection transistor GST, the multiple memory cell transistors MCT and the multiple string selection transistors SST respectively. In addition, the multiple memory cell transistors MCT respectively include memory elements.
[0007] On the other hand, in order to meet the excellent performance and low price required by consumers, the existing three-dimensional flash memory can increase the integration by vertically stacking cells.
[0008] For example, referring to the structure of the conventional three-dimensional flash memory Figure 2 The existing three-dimensional flash memory is manufactured by configuring an electrode structure 215 on a substrate 200, in which a plurality of interlayer insulating layers 211 and a plurality of horizontal structures 250 are alternately and repeatedly formed. The plurality of interlayer insulating layers 211 and the plurality of horizontal structures 250 may extend along a first direction. As an example, the plurality of interlayer insulating layers 211 may be a silicon oxide film, and the bottom interlayer insulating layer 211a among the plurality of interlayer insulating layers 211 may be thinner in thickness than the remaining plurality of interlayer insulating layers 211. The plurality of horizontal structures 250 may respectively include a first adhesion insulating film 242, a second adhesion insulating film 243 and an electrode layer 245. A plurality of electrode structures 215 are provided, and the plurality of electrode structures 215 may be configured in a facing manner along a second direction intersecting the first direction. The first direction and the second direction may respectively correspond to Figure 2 A plurality of grooves 240 for separating the plurality of electrode structures 215 may be formed extending along the first direction between the plurality of electrode structures 215. A plurality of impurity regions doped with a high concentration may be formed in the substrate 200 exposed by the plurality of grooves 240, thereby configuring a common source line CSL. Although not shown, a plurality of separation insulating films for filling the grooves 240 may also be configured.
[0009] A plurality of vertical structures 230 that penetrate the electrode structure 215 may be configured. As an example, from a plane perspective, a plurality of vertical structures 230 may be arranged along the first direction and the second direction to be arranged in a matrix form. In another example, a plurality of vertical structures 230 may be arranged along the second direction but arranged in a zigzag shape along the first direction. The plurality of vertical structures 230 may include a protective film 224, a charge storage film 225, a channel insulating film 226, and a channel layer 227, respectively. As an example, the channel layer 227 may be configured in a hollow tube form, in which case a buried film 228 for filling the channel layer 227 may also be configured. A drain region D may be configured on the upper portion of the channel layer 227, and a conductive pattern 229 may be formed on the drain region D to be connected to the bit line BL. The bit line BL may extend in a direction intersecting with the plurality of horizontal electrodes 250, for example, may extend in the second direction. As an example, a plurality of vertical structures 230 arranged along the second direction may be connected to one bit line BL.
[0010] The first blocking insulating film 242 and the second blocking insulating film 243 included in the plurality of horizontal structures 250 and the charge storage film 225 and the channel insulating film 226 included in the plurality of vertical structures 230 may be defined as an oxide-nitride-oxide (ONO) layer as an information storage element of a three-dimensional flash memory. That is, a portion of the information storage element is included in the vertical structure 230, and the remaining portion may be included in the plurality of horizontal structures 250. As an example, the charge storage film 225 and the channel insulating film 226 in the multiple information storage elements may be included in each vertical structure 230, and the first blocking insulating film 242 and the second blocking insulating film 243 may be included in the plurality of horizontal structures 250. However, this is not limited thereto, and the charge storage film 225 and the channel insulating film 226 defined as an oxide-nitride-oxide layer may be included only in the vertical structure 230.
[0011] A plurality of epitaxial patterns 222 may be arranged between the substrate 200 and the vertical structures 230. The plurality of epitaxial patterns 222 connect the substrate 200 and the plurality of vertical structures 230. The plurality of epitaxial patterns 222 may be in contact with at least one layer of the plurality of horizontal structures 250. That is, the plurality of epitaxial patterns 222 may be arranged in contact with the bottom horizontal structure 250a. According to another embodiment, the plurality of epitaxial patterns 222 may also be arranged in contact with the plurality of layers, for example, may be arranged in contact with the plurality of horizontal structures 250 of two layers. On the other hand, in the case where the plurality of epitaxial patterns 222 are arranged in contact with the bottom horizontal structure 250a, the thickness of the bottom horizontal structure 250a may be greater than the thickness of the remaining plurality of horizontal structures 250. The bottom horizontal structure 250a in contact with the plurality of epitaxial patterns 222 may be equivalent to the reference horizontal structure 250a. Figure 1 The ground selection line GSL of the described three-dimensional flash memory array and the remaining plurality of horizontal structures 250 in contact with the plurality of vertical structures 230 may correspond to the plurality of word lines WL0 - WL3 .
[0012] The plurality of epitaxial patterns 222 each have an embedded sidewall 222a. Thus, the bottom horizontal structure 250a in contact with the plurality of epitaxial patterns 222 can be arranged along the contour of the embedded sidewall 222a. That is, the bottom horizontal structure 250a can be arranged along the embedded sidewall 222a of the plurality of epitaxial patterns 222 in a protruding manner toward the inside.
[0013] In the existing three-dimensional flash memory having the structure as described above, the thickness of the oxide-nitride-oxide layer included in the plurality of vertical structures 230 is 40nm, and therefore has the following disadvantages, namely, it is difficult to achieve horizontal descaling, and in addition, the characteristics of the charge trap flash (CTF) using the oxide-nitride-oxide (ONO) layer require a high operating voltage of 20V due to the FN (Fowler Nordheim) tunneling operation.
[0014] Therefore, there is a need for a technology for solving the above-mentioned disadvantages. Summary of the invention
[0015] Technical issues
[0016] An object of one embodiment of the present invention is to provide a three-dimensional flash memory and a method for manufacturing the same, wherein a ferroelectric film formed by a single film is used as a data storage area, thereby increasing the integration in the horizontal direction to achieve integration and improving reliability through a low operating voltage.
[0017] Furthermore, an object of an embodiment of the present invention is to provide a three-dimensional flash memory and a method for manufacturing the same, wherein a channel layer is formed by zinc (Zn), indium (In), gallium (Ga), a Group 4 semiconductor material, or a semiconductor material containing a Group 3-5 compound having a CAAC (C-axis aligned crystal) structure, thereby increasing a cell current, reducing a leakage current, and improving heat resistance reliability.
[0018] Furthermore, an object of an embodiment of the present invention is to provide a three-dimensional flash memory and an operating method thereof, that is, to realize multi-layering of data storage structural elements based on ferroelectric films.
[0019] Technical Solution
[0020] According to one embodiment, a three-dimensional flash memory includes: at least one channel layer extending along a direction; at least one ferroelectric film extending along the one direction in a manner of surrounding the at least one channel layer, serving as a data storage area; and a plurality of electrode layers stacked in a manner of being vertically connected relative to the at least one ferroelectric film.
[0021] According to one embodiment, the present invention is characterized in that the at least one ferroelectric film can realize multiple memory cells through multiple regions in contact with the multiple electrode layers, and the at least one ferroelectric film can satisfy the following conditions, namely, the turn-on voltage of the at least one channel layer is less than the operating voltage of each of the memory cells and greater than the threshold voltage when programming each of the memory cells.
[0022] According to still another embodiment, the present invention is characterized in that the at least one ferroelectric film can satisfy the above conditions by adjusting its thickness.
[0023] According to another embodiment, the present invention is characterized in that the at least one ferroelectric film may be made of a ferroelectric material of hafnium dioxide (HfO 2 ) having an orthorhombic crystal structure.
[0024] According to another embodiment, the present invention is characterized in that the at least one ferroelectric film can be made of PZT (Pb (Zr, Ti) O3), PTO (PbTiO3), SBT (SrBi2Ti2O3), BLT (Bi (La, Ti) O3), PLZT (Pb (La, Zr) TiO3), BST (Bi (Sr, Ti) O3), barium titanate (BaTiO3), P (VDF-TrFE), PVDF, AlO x 、ZnO x 、TiO x 、TaO x or InO x Made of at least one ferroelectric material.
[0025] According to another embodiment, the present invention is characterized in that the at least one channel layer is made of zinc, indium, gallium, a Group 4 semiconductor material or a semiconductor material containing Group 3-5 compounds having a CAAC (C-axisali gned crystal) structure.
[0026] According to one embodiment, the present invention is characterized in that a ferroelectric film is used for a three-dimensional flash memory, and the three-dimensional flash memory includes: at least one channel layer, which is extended along a direction; and a plurality of electrode layers, which are vertically stacked relative to the at least one channel layer. The ferroelectric film is characterized in that the at least one ferroelectric film is extended along the one direction in a manner of surrounding the at least one channel layer, and is used as a data storage area. A plurality of storage cells are realized by a plurality of regions in contact with the plurality of electrode layers. The at least one ferroelectric film satisfies the following condition, namely, the turn-on voltage of the at least one channel layer is less than the operating voltage of each of the above storage cells and greater than the threshold voltage when programming each of the above storage cells.
[0027] According to one embodiment, a method for manufacturing a three-dimensional flash memory includes the following steps: preparing a mold structure consisting of a plurality of interlayer insulating layers and a plurality of electrode layers alternately stacked on a substrate; forming at least one string hole extending along a direction to expose the substrate by penetrating the mold structure; forming at least one ferroelectric film serving as a data storage area extending along the one direction in the at least one string hole, wherein the at least one ferroelectric film includes an internal vertical hole; and forming at least one channel layer extending along the one direction in the vertical hole of the at least one ferroelectric film.
[0028] According to one embodiment, a method for manufacturing a three-dimensional flash memory includes the following steps: preparing a mold structure consisting of a plurality of interlayer insulating layers and a plurality of sacrificial layers alternately stacked on a substrate; forming at least one string hole extending along a direction to expose the substrate by penetrating the mold structure; forming at least one ferroelectric film used as a data storage area extending along the one direction in the at least one string hole, the at least one ferroelectric film including an internal vertical hole; forming at least one channel layer extending along the one direction in the vertical hole of the at least one ferroelectric film; and removing the multiple sacrificial layers and filling the multiple spaces where the multiple sacrificial layers are removed with multiple electrode layers.
[0029] According to one embodiment, a three-dimensional flash memory is multi-layered based on ferroelectric materials, and is characterized in that it includes: at least one channel layer, which is formed by extending along a direction on a substrate; a plurality of electrode layers, which are stacked along a vertical direction relative to the at least one channel layer; and at least one ferroelectric film, which surrounds the at least one channel layer, and is arranged along the one direction between the at least one channel layer and the plurality of electrode layers to realize a plurality of storage units and serve as data storage areas through a plurality of regions in contact with the plurality of electrode layers, and the multi-layering of the object storage unit is realized by changing the amount of polarization charge of a portion of the at least one ferroelectric film corresponding to the object storage unit that becomes the object of program work among the plurality of storage units.
[0030] According to one embodiment, the present invention is characterized in that the three-dimensional flash memory can change the polarization charge amount of the at least one ferroelectric film by adjusting a program voltage applied to the target memory cell between a negative value and a positive value.
[0031] According to still another embodiment, the present invention is characterized in that the three-dimensional flash memory can change the polarization charge amount of the at least one ferroelectric film by applying a negative program voltage and a positive program voltage different from each other to the target memory cell.
[0032] According to another embodiment, the present invention is characterized in that the above-mentioned three-dimensional flash memory can control the number of polarized atoms or the polarization rotation angle in a part of the above-mentioned at least one ferroelectric film by adjusting the program voltage applied to the above-mentioned object storage unit between negative values and positive values, and change the above-mentioned polarization charge amount based on the controlled above-mentioned number of atoms or polarization rotation angle.
[0033] According to one embodiment, in a multi-layer implementation method of a three-dimensional flash memory, the three-dimensional flash memory includes: at least one channel layer, which is formed by extending along a direction on a substrate; a plurality of electrode layers, which are stacked along a vertical direction relative to the at least one channel layer; and at least one ferroelectric film, which surrounds the at least one channel layer, and is arranged along the one direction between the at least one channel layer and the plurality of electrode layers to implement a plurality of storage cells through a plurality of regions in contact with the plurality of electrode layers and used as data storage areas. The multi-layer implementation method of the three-dimensional flash memory includes: a determination step, determining a range of a program voltage applied to a target storage cell that becomes a program work object among the plurality of storage cells between negative values and positive values; an adjustment step, adjusting the program voltage applied to the target storage cell within a range between negative values and positive values based on the determination result; and a multi-layer step, as the program voltage applied to the target storage cell is adjusted, the multi-layering of the target storage cell is implemented by changing the amount of polarization charge of a portion of the at least one ferroelectric film corresponding to the target storage cell.
[0034] According to one embodiment, the present invention is characterized in that, in the above-mentioned determination step, the range of the program voltage applied to the above-mentioned object storage unit can be determined between negative values and positive values based on the thickness of the above-mentioned at least one ferroelectric film and the breakdown voltage of the above-mentioned at least one ferroelectric film.
[0035] Effects of the Invention
[0036] An embodiment of the present invention can provide a three-dimensional flash memory and a method for manufacturing the same, that is, a ferroelectric film formed of a single film is used as a data storage area, thereby increasing the integration in the horizontal direction to achieve integration and improving reliability through a low operating voltage.
[0037] Furthermore, an embodiment of the present invention may provide a three-dimensional flash memory and a method for manufacturing the same, that is, a channel layer is formed by using zinc, indium, gallium, a Group 4 semiconductor material or a semiconductor material containing a Group 3-5 compound having a CAAC (C-axis aligned crystal) structure, thereby increasing a cell current, reducing a leakage current, and improving heat resistance reliability.
[0038] Furthermore, an embodiment of the present invention can provide a three-dimensional flash memory and an operating method thereof, that is, realizing multi-layering of data storage structural elements based on ferroelectric films. BRIEF DESCRIPTION OF THE DRAWINGS
[0039] Figure 1 A circuit diagram briefly showing an array of conventional three-dimensional flash memories;
[0040] Figure 2 A three-dimensional diagram showing the structure of a conventional three-dimensional flash memory;
[0041] Figure 3 A cross-sectional view showing a three-dimensional flash memory according to an embodiment;
[0042] Figure 4 A diagram showing memory characteristics of a three-dimensional flash memory for explaining an embodiment;
[0043] Figure 5 A flowchart showing a method for manufacturing a three-dimensional flash memory according to an embodiment of the present invention;
[0044] Figure 6 A flowchart showing a method for manufacturing a three-dimensional flash memory according to another embodiment;
[0045] Figure 7 A cross-sectional view showing a three-dimensional flash memory according to an embodiment;
[0046] Figures 8 to 9 A diagram for explaining the multi-layering of a three-dimensional flash memory according to an embodiment;
[0047] Figure 10 to Figure 11 A cross-sectional view for explaining a program operation of a three-dimensional flash memory according to an embodiment;
[0048] Fig.12 A cross-sectional view for illustrating an erasing operation of a three-dimensional flash memory according to an embodiment;
[0049] Fig.13 A cross-sectional view for illustrating a reading operation of a three-dimensional flash memory according to an embodiment;
[0050] Fig.14 FIG. 1 is a flow chart showing a method for implementing multi-layered three-dimensional flash memory according to an embodiment of the present invention. DETAILED DESCRIPTION
[0051] Hereinafter, the embodiments will be described in detail with reference to the accompanying drawings. However, the present invention is not limited to or restricted to the embodiments. Also, the same reference numerals shown in the various drawings represent the same components.
[0052] Furthermore, the terminology used in this specification is used to appropriately express the preferred embodiments of the present invention, and such terminology may vary depending on the intention of the user or operator or the conventions of the technical field to which the present invention belongs. Therefore, these terms should be defined based on the entire content of this specification.
[0053] Figure 3 FIG. 2 is a cross-sectional view showing a three-dimensional flash memory according to an embodiment of the present invention. Figure 4 FIG. 1 is a diagram showing memory characteristics of a three-dimensional flash memory for explaining an embodiment.
[0054] Reference Figure 3 to Figure 4 , a three-dimensional flash memory 300 of an embodiment includes at least one channel layer 310 , at least one ferroelectric film 320 , and a plurality of electrode layers 330 .
[0055] At least one channel layer 310 is formed on a substrate (not shown) along a direction (eg, Figure 2 In this case, at least one channel layer 310 may be formed by a selective epitaxial growth process or a phase change epitaxial process using a substrate as a base material, such as Figure 2 As shown, a buried membrane (not shown) may also be included, which is in the form of a tube with a space formed inside, and is used to fill the inside of the channel layer 310.
[0056] The at least one channel layer 310 is made of zinc, indium, gallium, a group 4 semiconductor material or a semiconductor material containing a group 3-5 compound having a CAAC (C-axis aligned crystal) crystal structure, thereby increasing the cell current, reducing the leakage current, and improving the temperature resistance reliability. For example, the at least one channel layer 310 can be made of ZnO containing at least one of AZO, ZTO, IZO, ITO, IGZO or Ag-ZnO. x However, the at least one channel layer 310 is not limited to or confined thereto, and like the existing channel layer, can be formed of single crystal silicon or polycrystalline silicon.
[0057] Furthermore, although not shown, a drain line (not shown) may be connected to an upper portion of at least one channel layer 310 .
[0058] At least one ferroelectric film 320 is formed to extend in one direction in a manner of surrounding at least one channel layer 310, and is used as a data storage area. For example, at least one ferroelectric film 320 may be made of a ferroelectric material of hafnium dioxide having an orthorhombic crystal structure, and as a more specific example, may be made of a ferroelectric material of hafnium dioxide (HfO2) doped with at least one of aluminum (Al), zirconium (Zr) or silicon (Si). As another example, at least one ferroelectric film 320 may be made of a material including PZT (Pb (Zr, Ti) O3), PTO (PbTiO3), SBT (SrBi2Ti2O3), BLT (Bi (La, Ti) O3), PLZT (Pb (La, Zr) TiO3), BST (Bi (Sr, Ti) O3), barium titanate (BaTiO3), P (VDF-TrFE), PVDF, AlO x 、ZnO x 、TiO x 、TaO x or InO x Made of at least one ferroelectric material.
[0059] Hereinafter, serving as a data storage area refers to representing (storing) a value of binary data due to a voltage change caused by a polarization phenomenon of a ferroelectric material constituting the at least one ferroelectric film 320 .
[0060] In this case, at least one ferroelectric film 320 is a single film of 20 nm or less made of a ferroelectric material. Since its thickness is significantly thinner than that of the existing oxide-nitride-oxide, it can have a lower operating voltage and improve the integration in the horizontal direction compared to the existing three-dimensional flash memory using oxide-nitride-oxide. However, at least one ferroelectric film 320 is not limited to or restricted to this, and can be formed not only as a single film but also as a plurality of films. In this case, the total thickness of the plurality of films can be maintained at a level of less than 20 nm.
[0061] In particular, at least one ferroelectric film 320 may have an appropriate operating voltage to achieve stable turn-on of at least one channel layer 310. More specifically, at least one ferroelectric film 320 is characterized by satisfying the following condition (the condition of the following formula 1), that is, the turn-on voltage of at least one channel layer 310 is less than the operating voltage of each memory cell 340, 350, 360 and greater than the threshold voltage when programming each memory cell 340, 350, 360. For example, Figure 4As shown, the following conditions are satisfied, that is, the turn-on voltage 410 of at least one channel layer 310 is less than the working voltage 420 of each memory cell 340, 350, 360 and is greater than the threshold voltage 430 when programming each memory cell 340, 350, 360. As a more specific example, the following conditions can be satisfied, that is, the turn-on voltage of at least one channel layer 310 is 6V (±6V), which is less than 8V (±8V) and greater than 3V (±3V), 8V (±8V) is the working voltage of each memory cell 340, 350, 360, and 3V (±3V) is the threshold voltage when programming each memory cell 340, 350, 360. Hereinafter, the plurality of memory cells 340, 350, 360 are realized by a plurality of regions where at least one ferroelectric film 320 contacts the plurality of electrode layers 330.
[0062] <Formula 1>
[0063] Cell Operation Voltage>Vpass>Vh
[0064] In Formula 1, Cell Operation Voltage refers to the operating voltage of each memory cell 340 , 350 , 360 , Vpass refers to the turn-on voltage of at least one channel layer 310 , and Vh refers to the threshold voltage when programming each memory cell 340 , 350 , 360 .
[0065] The above conditions can be met by adjusting the thickness of at least one ferroelectric film 320. That is, the thickness of at least one ferroelectric film 320 can be adjusted so that the turn-on voltage of at least one channel layer 310 meets the following conditions: it is less than the working voltage of each memory cell 340, 350, 360 and is greater than the threshold voltage when programming each memory cell 340, 350, 360.
[0066] Furthermore, the above conditions are satisfied not only by the thickness of the at least one ferroelectric film 320, but also by the ferroelectric material of which the at least one ferroelectric film 320 is made. As an example, in order to make the turn-on voltage of the at least one channel layer 310 lower than the operating voltage of each memory cell 340, 350, 360 and higher than the threshold voltage when programming each memory cell, the at least one ferroelectric film 320 may be made of a ferroelectric material of hafnium dioxide doped with at least one of zirconium or silicon so as to have a high polarization voltage.
[0067] Due to the above-mentioned features, the 3D flash memory 300 of one embodiment can be directly applied to the serial operations (programming operation, erasing operation and reading operation) of the existing 3D flash memory.
[0068] Furthermore, at least one ferroelectric film 320 obtains multiple levels based on the degree of polarization phenomenon, and therefore can have a multi-layered characteristic representing multiple bits of data, and can be formed through an atomic layer deposition (ALD) process to achieve step coverage and nanometer-level thickness control.
[0069] The plurality of electrode layers 330 are stacked in a manner of being vertically connected to at least one ferroelectric film 320, and are arranged along other directions (eg, Figure 2 As constituent materials of the plurality of electrode layers 330, conductive materials such as tungsten, titanium, and tantalum can be used.
[0070] When the program threshold voltage is high in the 0 state, the three-dimensional flash memory 300 having the above structure can apply an operating voltage for generating polarization to the gate electrode to operate, so that the voltage of at least one channel layer 310 maintains 0V or an appropriate reference voltage. On the contrary, when the storage threshold voltage is low in the 1 state (that is, when the erase state is stored), the three-dimensional flash memory 300 can apply an operating voltage for inverting polarization to at least one channel layer 310 to operate, so that the gate voltage maintains 0V or an appropriate reference voltage.
[0071] As such, the three-dimensional flash memory 300 of one embodiment uses at least one ferroelectric film 320 formed of a single film as a data storage area, thereby increasing the integration degree in the horizontal direction to achieve integration and improving reliability characteristics through low operating voltage. In addition, the three-dimensional flash memory 300 forms at least one channel layer 310 with zinc, indium, gallium, a group 4 semiconductor material or a semiconductor material containing a group 3-5 compound having a CAAC (C-axis aligned crystal) crystal structure, thereby increasing the cell current, reducing the leakage current, and improving the temperature resistance reliability. Figures 5 and 6 , a method for manufacturing the three-dimensional flash memory 300 is described in detail.
[0072] Figure 5 FIG. 1 is a flow chart showing a method for manufacturing a three-dimensional flash memory according to an embodiment of the present invention.
[0073] The three-dimensional flash memory manufactured by the method for manufacturing the three-dimensional flash memory has the following features: Figure 3 Furthermore, as the main body for executing the manufacturing method of the three-dimensional flash memory, an automated and mechanized manufacturing system can be used.
[0074] Reference Figure 5 In step S510 , the manufacturing system prepares a mold structure having a plurality of interlayer insulating layers and a plurality of sacrificial layers alternately stacked on a substrate.
[0075] Next, in step S520 , the manufacturing system forms at least one string hole for exposing the substrate by extending along a direction through the mold structure.
[0076] Subsequently, in step S530, the manufacturing system extends along a direction to form at least one ferroelectric film used as a data storage area in at least one string hole (at least one ferroelectric film includes an internal vertical hole). For example, the manufacturing system can form at least one ferroelectric film by using a ferroelectric material of hafnium dioxide having an orthorhombic crystal structure. As a more specific example, the manufacturing system can form at least one ferroelectric film by using a ferroelectric material of hafnium dioxide doped with at least one of aluminum, zirconium or silicon.
[0077] In particular, in step S530, in the process of realizing multiple memory cells by means of multiple regions in contact with multiple electrode layers on at least one ferroelectric film, the manufacturing system can form at least one ferroelectric film that satisfies the following conditions, namely, a turn-on voltage of at least one channel layer is less than an operating voltage of each of the above-mentioned memory cells and greater than a threshold voltage when programming each memory cell.
[0078] In more detail, in order to satisfy the above conditions, the manufacturing system may adjust the thickness of at least one ferroelectric film or selectively determine the ferroelectric material constituting the at least one ferroelectric film. As an example, in order to satisfy the above conditions, the manufacturing system may form at least one ferroelectric film by a ferroelectric material of hafnium dioxide doped with at least one of zirconium or silicon having a higher polarization voltage.
[0079] Then, in step S540, the manufacturing system forms at least one channel layer by extending the vertical hole of at least one ferroelectric film along a direction. In this case, the manufacturing system can form at least one channel layer by using zinc, indium, gallium, a Group 4 semiconductor material or a semiconductor material containing a Group 3-5 compound having a CAAC crystal structure.
[0080] In this case, a method for manufacturing a three-dimensional flash memory according to an embodiment is characterized in that the manufacturing system can continuously perform step S530 to step S540 using an atomic layer deposition process.
[0081] The above-described method for manufacturing a three-dimensional flash memory is not limited to or confined to steps S510 to S540, and may include steps for manufacturing Figure 3 As an example, in Figure 3 The three-dimensional flash memory described in the above can be manufactured using a mold structure including a plurality of sacrificial layers, rather than a mold structure including a plurality of electrode layers. Figure 6 , which explains this in detail.
[0082] Figure 6FIG. 4 is a flow chart showing a method for manufacturing a three-dimensional flash memory according to another embodiment.
[0083] The three-dimensional flash memory manufactured by the method for manufacturing the three-dimensional flash memory has the following features: Figure 3 Furthermore, as the main body for executing the manufacturing method of the three-dimensional flash memory, an automated and mechanized manufacturing system can be used.
[0084] Reference Figure 6 In step S610 , the manufacturing system prepares a mold structure having a plurality of interlayer insulating layers and a plurality of sacrificial layers alternately stacked on a substrate.
[0085] Next, in step S620 , the manufacturing system forms at least one string hole for exposing the substrate by extending along a direction through the mold structure.
[0086] Subsequently, in step S630, the manufacturing system extends along a direction to form at least one ferroelectric film used as a data storage area in at least one string hole (at least one ferroelectric film includes an internal vertical hole). For example, the manufacturing system can form at least one ferroelectric film using a ferroelectric material of hafnium dioxide having an orthorhombic crystal structure. As a more specific example, the manufacturing system can form at least one ferroelectric film using a ferroelectric material of hafnium dioxide doped with at least one of aluminum, zirconium, or silicon.
[0087] In particular, in step S630, in the process of realizing multiple memory cells by means of multiple regions in contact with multiple electrode layers on at least one ferroelectric film, the manufacturing system can form at least one ferroelectric film that satisfies the following conditions, namely, a turn-on voltage of at least one channel layer is less than an operating voltage of each of the above-mentioned memory cells and greater than a threshold voltage when programming each memory cell.
[0088] In more detail, in order to satisfy the above conditions, the manufacturing system may adjust the thickness of at least one ferroelectric film or selectively determine the ferroelectric material constituting the at least one ferroelectric film. As an example, in order to satisfy the above conditions, the manufacturing system may form at least one ferroelectric film by a ferroelectric material of hafnium dioxide doped with at least one of zirconium or silicon having a higher polarization voltage.
[0089] Then, in step S640, the manufacturing system forms at least one channel layer by extending the vertical hole of at least one ferroelectric film along a direction. In this case, the manufacturing system can form at least one channel layer by using zinc, indium, gallium, a Group 4 semiconductor material or a semiconductor material containing a Group 3-5 compound having a CAAC crystal structure.
[0090] In this case, a method for manufacturing a three-dimensional flash memory according to another embodiment is characterized in that the manufacturing system can continuously perform step S630 to step S640 using an atomic layer deposition process.
[0091] Next, in step S650 , the manufacturing system removes the plurality of sacrificial layers and fills the plurality of spaces where the plurality of sacrificial layers are removed with a plurality of electrode layers.
[0092] The above-described method for manufacturing a three-dimensional flash memory is not limited to or confined to steps S610 to S650, and may include steps for manufacturing Figure 3 The multiple steps of the three-dimensional flash memory are described in detail.
[0093] Figure 7 FIG. 2 is a cross-sectional view showing a three-dimensional flash memory according to an embodiment of the present invention. Figures 8 to 9 FIG. 1 is a diagram for explaining the multi-layering of a three-dimensional flash memory according to an embodiment. Specifically, Figure 8 FIG. 1 is a diagram for explaining a change in the amount of polarization charge of at least one ferroelectric film in a three-dimensional flash memory according to an embodiment of the present invention. Fig. 9 FIG. 1 is a diagram for explaining various operating voltages when a three-dimensional flash memory is multi-layered according to an embodiment of the present invention.
[0094] Reference Figures 7 to 9 , a three-dimensional flash memory 700 of an embodiment includes at least one channel layer 710 , a plurality of electrode layers 720 , and at least one ferroelectric film 730 .
[0095] At least one channel layer 710 is formed on a substrate (not shown) along a direction (eg, Figure 2 In this case, at least one channel layer 710 may be formed by a selective epitaxial growth process or a phase change epitaxial process using a substrate as a base material, such as Figure 2 As shown, a buried film (not shown) may also be included, which is in the form of a tube with a space formed inside, and is used to fill the inside of the channel layer 710.
[0096] The at least one channel layer 710 is made of zinc, indium, gallium, a group 4 semiconductor material or a semiconductor material containing a group 3-5 compound having a CAAC crystal structure, thereby increasing the unit current, reducing the leakage current, and improving the temperature resistance reliability. For example, the at least one channel layer 710 can be made of ZnO containing at least one of AZO, ZTO, IZO, ITO, IGZO or Ag-ZnO. x However, the at least one channel layer 710 is not limited to or confined thereto, and like the existing channel layer, can be formed of single crystal silicon or polycrystalline silicon.
[0097] Furthermore, although not shown, a drain line (not shown) may be connected to an upper portion of at least one channel layer 710 .
[0098] The plurality of electrode layers 720 are stacked along a vertical direction relative to the at least one channel layer 710, and along other directions (eg, Figure 2 As a constituent material of the plurality of electrode layers 720, a conductive material such as tungsten, titanium, or tantalum can be used.
[0099] At least one ferroelectric film 730 surrounds at least one channel layer 710 and extends along a direction (eg, Figure 2 The plurality of storage cells 731, 732, 733, 734 are implemented through a plurality of regions in contact with the plurality of electrode layers 720 and are used as data storage areas.
[0100] In this case, at least one ferroelectric film 730 may be made of a ferroelectric material of hafnium dioxide having an orthorhombic crystal structure, for example, a ferroelectric material of hafnium dioxide doped with at least one of aluminum, zirconium or silicon. As another example, at least one ferroelectric film 730 may be made of a material including PZT (Pb (Zr, Ti) O3), PTO (PbTiO3), SBT (SrBi2Ti2O3), BLT (Bi (La, Ti) O3), PLZT (Pb (La, Zr) TiO3), BST (Bi (Sr, Ti) O3), barium titanate (BaTiO3), P (VDF-TrFE), PVDF, AlO x 、ZnO x 、TiO x 、TaO x or InO x Made of at least one ferroelectric material.
[0101] Hereinafter, serving as a data storage area means that each region of at least one ferroelectric film 730 constituting a plurality of memory cells 731, 732, 733, 734 respectively represents (stores) a value of binary data through a voltage change caused by a polarization phenomenon.
[0102] Among them, at least one ferroelectric film 730 is a single film of less than 20nm made of ferroelectric material. Since its thickness is significantly thinner than the existing oxide-nitride-oxide, it can have a lower operating voltage and improve the integration in the horizontal direction compared to the existing three-dimensional flash memory using oxide-nitride-oxide. However, at least one ferroelectric film 730 is not limited to or restricted to this, and can be formed not only as a single film, but also as a plurality of films. In this case, the total thickness of the plurality of films can be maintained at a level below 20nm.
[0103] The three-dimensional flash memory 700 having the above-described structure is characterized in that the object storage unit 733 is multilayered by changing the polarization charge amount of a portion of at least one ferroelectric film 730 corresponding to the object storage unit 733 that is the object of program operation among the plurality of storage units 731, 732, 733, and 734. The portion of at least one ferroelectric film 730 corresponding to the object storage unit 733 refers to the object storage unit 733 itself.
[0104] In more detail, Figure 8 As shown, the polarization charge amount when the atoms of the object storage unit 733 are polarized in the case shown in part (a) is different from the polarization charge amount when the atoms of the object storage unit 733 are polarized in the case shown in part (b). Similarly, the polarization charge amount in the case shown in part (c) and the polarization charge amount in the case shown in part (d) are different from the case shown in part (a) and the case shown in part (b), respectively.
[0105] Thus, by controlling the number of atoms polarized or the polarization rotation angle in the object storage unit 733, the three-dimensional flash memory 700 can change the polarization charge amount of the object storage unit 733 based on the controlled number of atoms or the polarization rotation angle. For example, as shown in the case shown in part (a), the case shown in part (b), the case shown in part (c), and the case shown in part (d), the three-dimensional flash memory 700 controls the number of atoms polarized or the polarization rotation angle in the object storage unit 733 in different ways, so that the polarization charge amounts of the object storage units 733 can become different from each other.
[0106] As a more specific example, the three-dimensional flash memory 700 may be changed as follows, that is, as shown in part (a), the object storage unit 733 has a polarized charge amount of a first program state by controlling the number of polarized atoms or the polarization rotation angle in the object storage unit 733; as shown in part (c), the object storage unit 733 has a polarized charge amount of a second program state by controlling the number of polarized atoms or the polarization rotation angle in the object storage unit 733; as shown in part (d), the object storage unit 733 has a polarized charge amount of a third program state by controlling the number of polarized atoms or the polarization rotation angle in the object storage unit 733; as shown in part (b), the object storage unit 733 has an erased state polarized charge amount by controlling the number of polarized atoms or the polarization rotation angle in the object storage unit 733.
[0107] In this case, the number of atoms polarized or the polarization rotation angle in the object storage unit 733 can be controlled by adjusting the voltage applied to the object storage unit 733. That is, the three-dimensional flash memory 700 can control the number of atoms polarized or the polarization rotation angle in the object storage unit 733 by adjusting the voltage applied to the object storage unit 733 between a negative value and a positive value, thereby changing the amount of polarization charge in the object storage unit 733.
[0108] In connection with this, further reference is made to Fig. 9 The three-dimensional flash memory 700 can control the number of atoms polarized or the polarization rotation angle in the object storage unit 733 to be 10V by applying a negative first program voltage (e.g., -10V) to the object storage unit 733. Figure 8 The case shown in part (a) of the embodiment is thus programmed in such a manner that the polarization charge amount of the object storage unit 733 is changed so that the object storage unit 733 has the first program state and thus represents the binary data 00. Similarly, the three-dimensional flash memory 700 can control the number of atoms polarized in the object storage unit 733 or the polarization rotation angle to be 00 by applying a negative second program voltage (e.g., -9 V) to the object storage unit 733. Figure 8 In the case shown in part (c) of the embodiment, the polarization charge amount of the object storage unit 733 is changed to a second program state and thus represents the binary data 01, and the number of atoms polarized in the object storage unit 733 or the polarization rotation angle can be controlled to be 01 by applying a third program voltage of a negative value (e.g., -8 V) to the object storage unit 733. Figure 8 The case shown in part (d) of is thereby programmed in such a manner that the polarization charge amount of the object memory cell 733 has a third program state and thereby represents binary data 10 .
[0109] Furthermore, the three-dimensional flash memory 700 can control the number of atoms polarized or the polarization rotation angle in the object storage unit 733 to be 10V by applying a fourth program voltage of a positive value (eg, 10V) to the object storage unit 733. Figure 8 The situation shown in part (b) of the embodiment is thereby programmed in a manner that the object storage unit 733 has a polarization charge amount of a fourth program state and thereby represents binary data 11. The polarization charge amount of the fourth program state as described above is the polarization charge amount of the erased state described above, and since the three-dimensional flash memory 700 uses the erased state of the object storage unit 733 caused by applying a positive voltage to the object storage unit 733 as the fourth program state, it is advantageous to realize multi-layering of the object storage unit 733.
[0110] That is, as shown in the illustrated example, the three-dimensional flash memory 700 can adjust the polarization charge amount of at least one ferroelectric film 730 by applying a program voltage between -10V as a negative value and 10V as a positive value to the target memory cell 733. Figure 8 The situation shown in part (a) of Figure 8 The situations shown in part (d) change, with the situation shown in part (a) representing binary data 00, the situation shown in part (c) representing binary data 01, the situation shown in part (d) representing binary data 10, and the situation shown in part (b) representing binary data 11, thereby achieving multi-layering.
[0111] The range between the negative value and the positive value for adjusting the program voltage applied to the object storage unit 733 may be determined based on the thickness of at least one ferroelectric film 730 and the breakdown voltage of at least one ferroelectric film 730. In other words, the range between the negative value and the positive value for adjusting the program voltage applied to the object storage unit 733 may be determined based on the breakdown voltage margin generated by the thickness of at least one ferroelectric film 730. For example, when the thickness of at least one ferroelectric film 730 reaches 20nm, the breakdown voltage margin of at least one ferroelectric film 730 reaches the level of 16V, and the range between the negative value and the positive value for adjusting the program voltage applied to the object storage unit 733 may be determined to be in the range of -14V to 10V. As another example, when the thickness of at least one ferroelectric film 730 reaches 15nm, the breakdown voltage margin of at least one ferroelectric film 730 reaches the level of 12V, and the range between the negative value and the positive value for adjusting the program voltage applied to the object storage unit 733 may be determined to be in the range of -12V to 10V.
[0112] Thus, the three-dimensional flash memory 700 can adjust the program voltage applied to the target memory cell 733 in a range between a negative value and a positive value determined based on the thickness of the at least one ferroelectric film 730 and the breakdown voltage of the at least one ferroelectric film 730 .
[0113] In this way, by adjusting the program voltage applied to the object storage unit 733 between negative and positive values (applying different negative program voltages and positive program voltages to the object storage unit 733), the polarization charge amount of at least one ferroelectric film 730 is changed, thereby, the three-dimensional flash memory 700 can achieve multi-layering of the object storage unit 733.
[0114] In this case, the process of applying a negative program voltage (the case of applying the first program voltage, the case of applying the second program voltage, and the case of applying the third program voltage as described above) to the object storage unit 733 can be performed by applying different negative voltages (a negative voltage corresponding to the first program voltage, a negative voltage corresponding to the second program voltage, and a negative voltage corresponding to the third program voltage) to the electrode layer 721 corresponding to the object storage unit 733 among the multiple electrode layers 720 and applying a voltage of 0V to the channel layer 710 of the string where the object storage unit 733 is located or the channel layer 710 in the substrate corresponding to the string.
[0115] However, this is not limited to or restricted to this, and the process of applying a negative program voltage to the object storage unit 733 (the case of applying the first program voltage, the case of applying the second program voltage, and the case of applying the third program voltage as described above) can also be performed by applying a voltage of 0V to the electrode layer 721 corresponding to the object storage unit 733 among the multiple electrode layers 720 and applying different positive voltages (a positive voltage corresponding to the first program voltage, a positive voltage corresponding to the second program voltage, and a positive voltage corresponding to the third program voltage) to the channel layer 710 of the string where the object storage unit 733 is located or the channel layer 710 in the substrate corresponding to the string.
[0116] Below, refer to Figure 10 to Figure 11 , describing in detail the manner in which a negative programming voltage is applied to the object storage cell 733.
[0117] Although the above describes a method of implementing 2-bit multi-layering using the three-dimensional flash memory 700, it is not limited to or restricted to this. Multi-layering of bits above 3 bits can also be implemented through the same principle (the principle of implementing multi-layering by adjusting the program voltage applied to the object storage unit 733 between negative and positive values to change the polarization charge amount of the object storage unit 733).
[0118] Figure 10 to Figure 11 A cross-sectional view for explaining a program operation of a three-dimensional flash memory according to an embodiment.
[0119] Reference Fig.10 , the three-dimensional flash memory 1000 can apply a negative program voltage to the target memory cell 1020 by applying a negative voltage to the electrode layer 1011 corresponding to the target memory cell 1020 among the plurality of electrode layers 1010 and applying a voltage of 0V to the channel layer of the string where the target memory cell 1020 is located or the channel layer in the substrate corresponding to the string. In this case, among the plurality of electrode layers 1010, the pass voltage can be applied to the remaining electrode layers except the electrode layer 1011 corresponding to the target memory cell 1020, respectively.
[0120] For example, in order to make the object storage unit 1020 have Figure 8 The three-dimensional flash memory 1000 needs to apply -10V as the first program voltage to the target memory cell 1020 in order to obtain the same polarization charge as the case shown in part (a) of FIG. 1 . Thus, the three-dimensional flash memory 1000 can apply -10V to the target memory cell 1020 by applying -10V to the electrode layer 1011 corresponding to the target memory cell 1020 among the plurality of electrode layers 1010 and applying a voltage of 0V to the channel layer of the string where the target memory cell 1020 is located or the channel layer in the substrate corresponding to the string.
[0121] Figure 8 The case shown in part (c) and the case shown in part (d) are the same as the case shown in part (a), and a negative program voltage is applied to both. Therefore, only the voltage value applied to the electrode layer 1011 can be changed and executed in the same manner (as an example, the case shown in part (c) indicates that -9V is applied to the electrode layer 1011, and the case shown in part (d) indicates that -8V is applied to the electrode layer 1011). In this case, since the case shown in part (b) indicates that a positive program voltage is applied, the following can be performed. Fig.12 The erasure work in .
[0122] However, in addition to the above-described method, the method of applying a negative program voltage to the target memory cell 1020 may also be implemented in other ways. Fig.11 The three-dimensional flash memory 1100 can apply a negative program voltage to the object memory cell 1120 by applying a voltage of 0V to an electrode layer 1111 corresponding to the object memory cell 1120 among the multiple electrode layers 1110 and applying a positive voltage to a channel layer of the string where the object memory cell 1120 is located or a channel layer in the substrate corresponding to the string.
[0123] In which, the positive voltage applied to the channel layer of the string or the channel layer in the substrate corresponding to the string is used as a value corresponding to the negative programming voltage that should be applied to the object storage unit 1120, which can be obtained by changing the sign of the negative programming voltage applied to the object storage unit 1120.
[0124] For example, in order to make the object storage unit 1120 have Figure 8The three-dimensional flash memory 1100 needs to apply -10V as the first program voltage to the target memory cell 1120 to obtain the same polarization charge as the case shown in part (a). Thus, the three-dimensional flash memory 1100 can apply 10V to the target memory cell 1120 by applying 0V to the electrode layer 1111 corresponding to the target memory cell 1120 among the plurality of electrode layers 1110 and applying a voltage of 10V to the channel layer of the string where the target memory cell 1120 is located or the channel layer in the substrate corresponding to the string.
[0125] Figure 8 The case shown in part (c) and the case shown in part (d) are the same as the case shown in part (a), and a negative program voltage is applied to both. Therefore, only the voltage value applied to the electrode layer 1111 can be changed and executed in the same manner (as an example, the case shown in part (c) indicates that 9V is applied to the channel layer of the string or the channel layer in the substrate corresponding to the string, and the case shown in part (d) indicates that 8V is applied to the channel layer of the string or the channel layer in the substrate corresponding to the string). In this case, since the case shown in part (b) indicates that a positive program voltage is applied, the following can be performed. Fig.12 The erasure work in .
[0126] Fig.12 FIG. 4 is a cross-sectional view for explaining an erasing operation of a three-dimensional flash memory according to an embodiment.
[0127] Reference Fig.12 In one embodiment, the three-dimensional flash memory 1200 can respectively apply an erase voltage (for example, 10V) to the multiple electrode layers 1210 and respectively apply a voltage of 0V to the channel layer of the string or the channel layer in the substrate corresponding to the string to perform an erase operation on the multiple storage cells included in the three-dimensional flash memory 1200.
[0128] The polarization charge amount based on the erasing operation as described above can be used as a state for realizing the multi-layering of the target memory cell 1220. That is, the three-dimensional flash memory 1200 represents any one of the binary data (for example, 11) as the erase state of the target memory cell 1220, and the erase voltage of 10V as a positive value applied to the target memory cell 1220 in the erasing operation (the erase voltage of 10V as a positive value applied to the plurality of electrode layers 1210, respectively) can be named as a program voltage of a positive value for programming the binary data 11.
[0129] Therefore, as reference Figures 7 to 12 As described above, the three-dimensional flash memory can realize multi-layering by applying not only mutually different negative program voltages to target memory cells but also positive program voltages (positive erase voltages) in an erased state.
[0130] Below, refer to Fig.13 , explaining the reading operation of a multi-layered three-dimensional flash memory like this.
[0131] Fig.13 FIG. 4 is a cross-sectional view for explaining a read operation of a three-dimensional flash memory according to an embodiment.
[0132] Reference Fig.13 In the process of applying 0V to the electrode layer 1311 corresponding to the target storage unit 1320 among the plurality of electrode layers 1310 and applying a pass voltage to the remaining electrode layers 1311, the three-dimensional flash memory 1300 of one embodiment can perform a reading operation for the target storage unit 1320 by applying a read voltage (e.g., 1V) to the channel layer of the string where the target storage unit 1320 is located or the channel layer in the substrate corresponding to the string. Thus, the binary data represented by the target storage unit 1320 can be read from the multi-layered binary data.
[0133] Fig.14 FIG. 1 is a flowchart showing a method for implementing a multi-layered three-dimensional flash memory according to an embodiment of the present invention. Figures 7 to 13 Illustrated three-dimensional flash memory.
[0134] Reference Fig.14 In step S1410, the three-dimensional flash memory determines a range of a program voltage applied to a target memory cell that is a program operation target among a plurality of memory cells between a negative value and a positive value.
[0135] In more detail, in step S1410, the three-dimensional flash memory may determine a range of a program voltage applied to a target memory cell between negative and positive values based on a thickness of at least one ferroelectric film and a breakdown voltage of at least one ferroelectric film.
[0136] Next, in step S1420, the three-dimensional flash memory adjusts a program voltage applied to the target memory cell in a range between a negative value and a positive value based on the determination result.
[0137] In this case, in step 1420, adjusting the program voltage applied to the target memory cell in a range between a negative value and a positive value based on the determination result means applying a program voltage of a negative value and a program voltage of a positive value different from each other to the target memory cell.
[0138] As a method of applying mutually different negative program voltages to the object memory cell, a first method or a second method can be used. The first method is to apply a negative program voltage to the object memory cell by applying a negative voltage to an electrode layer among multiple electrode layers corresponding to the object memory cell and applying a 0V voltage to a channel layer of the string where the object memory cell is located or a channel layer in a substrate corresponding to the string. The second method is to apply a negative program voltage to the object memory cell by applying a 0V voltage to an electrode layer among multiple electrode layers corresponding to the object memory cell and applying a positive voltage to the channel layer of the string where the object memory cell is located or a channel layer in a substrate corresponding to the string.
[0139] Next, as the program voltage applied to the target memory cell is adjusted, the three-dimensional flash memory realizes multi-layering of the target memory cell by changing the polarization charge amount of a portion of at least one ferroelectric film corresponding to the target memory cell in step S1430.
[0140] The following describes step S1410 to step S1430. Figure 8 In step S1410, the three-dimensional flash memory may determine the range of the program voltage applied to the target memory cell to be between -10V and 10V. Then, in step S1420, the three-dimensional flash memory may apply a negative first program voltage (e.g., -10V) to the target memory cell to make the target memory cell have the same voltage as that of the first program voltage. Figure 8 Alternatively, a negative second program voltage (e.g., -9 V) may be applied to the target memory cell to make the target memory cell have the same polarization charge as that in the case shown in part (a) of FIG. Figure 8 Alternatively, a third program voltage of a negative value (e.g., -8 V) may be applied to the target memory cell to make the target memory cell have the same polarization charge as that in the case shown in part (c) of FIG. Figure 8 Alternatively, a fourth program voltage (e.g., 10 V) of a positive value may be applied to the target memory cell to make the target memory cell have the same polarization charge as that of the case shown in part (d) of FIG. Figure 8 Thus, in step S1430, the three-dimensional flash memory can realize multi-layering of the target memory cell.
[0141] Although multiple embodiments are described above through limited embodiments and drawings, a person skilled in the art of the present invention may make various modifications and variations according to the above description. For example, the above-described techniques and / or the above-described structural elements such as systems, structures, devices, circuits, etc. may be combined or combined in a different form than the described method, or even if they are replaced or substituted by other structural elements or equivalent technical solutions, appropriate results may be achieved.
[0142] Therefore, other implementation modes, other examples and equivalent technical solutions that are equivalent to the scope of protection claimed by the invention all belong to the scope of protection claimed by the invention of the present invention.
Claims
1. A three-dimensional flash memory, It is characterized in that include: At least one channel layer is formed extending along a direction; At least one ferroelectric film is formed and extended along the one direction in a manner of surrounding the at least one channel layer, and is used as a data storage area; as well as A plurality of electrode layers are stacked in a manner vertically connected to the at least one ferroelectric film; The at least one ferroelectric film realizes a plurality of storage units through a plurality of regions in contact with the plurality of electrode layers. The at least one ferroelectric film satisfies the following conditions, that is, the turn-on voltage of the at least one channel layer is less than the working voltage of each of the memory cells and greater than the threshold voltage when programming each of the memory cells. The at least one ferroelectric film satisfies the above conditions by adjusting its thickness, and Wherein, the at least one ferroelectric film is formed of a ferroelectric material to satisfy the above conditions; When programming the first state to the plurality of memory cells with a high threshold voltage, the three-dimensional flash memory applies an operating voltage for satisfying the condition to the plurality of electrode layers, and applies 0V or an appropriate reference voltage to the at least one channel layer; and When programming the second state to the plurality of memory cells at a low threshold voltage, the three-dimensional flash memory applies a satisfying operating voltage to the at least one channel layer, and applies 0V or the appropriate reference voltage to the plurality of electrode layers.
2. The three-dimensional flash memory according to claim 1, It is characterized in that The at least one ferroelectric film is made of the ferroelectric material of hafnium dioxide having an orthorhombic crystal structure.
3. The three-dimensional flash memory according to claim 1, It is characterized in that The at least one ferroelectric film is composed of PZT (Pb (Zr, Ti) O 3 )、PTO(PbTiO 3 )、SBT(SrBi 2 Ti 2 O 3 )、BLT(Bi(La,Ti)O 3 )、PLZT(Pb(La, Zr)TiO 3 )、BST(Bi(Sr,Ti)O 3 ), barium titanate (BaTiO 3 )、P(VDF-TrFE)、PVDF、AlO x 、ZnO x 、TiO x 、TaO x or InO x is made of at least one of the ferroelectric materials.
4. The three-dimensional flash memory according to claim 1, It is characterized in that The at least one channel layer is made of zinc, indium, gallium, a Group 4 semiconductor material or a semiconductor material containing Group 3-5 compounds having a CAAC crystal structure.
5. A method for manufacturing a three-dimensional flash memory according to claim 1, It is characterized in that The steps include: Preparing a mold structure having a plurality of interlayer insulating layers and a plurality of electrode layers alternately stacked on a substrate; At least one string hole is formed by penetrating the mold structure and extending along a direction to expose the substrate; At least one ferroelectric film extending along the one direction in the at least one string of holes and used as a data storage area is formed, and the at least one ferroelectric film includes an internal vertical hole; as well as The vertical holes in the at least one ferroelectric film extend along the one direction to form at least one channel layer.
6. A method for manufacturing a three-dimensional flash memory according to claim 1, It is characterized in that The steps include: Preparing a mold structure having a plurality of interlayer insulating layers and a plurality of sacrificial layers alternately stacked on a substrate; At least one string hole is formed by penetrating the mold structure and extending along a direction to expose the substrate; At least one ferroelectric film extending along the one direction in the at least one string of holes and used as a data storage area is formed, and the at least one ferroelectric film includes an internal vertical hole; The vertical hole of the at least one ferroelectric film extends along the one direction to form at least one channel layer; as well as The plurality of sacrificial layers are removed and a plurality of electrode layers are filled into the plurality of spaces where the plurality of sacrificial layers are removed.
7. A three-dimensional flash memory, based on ferroelectric materials to achieve multi-layer, It is characterized in that include: At least one channel layer is formed on the substrate and extends along a direction; A plurality of electrode layers are stacked in a vertical direction relative to the at least one channel layer; and at least one ferroelectric film surrounds the at least one channel layer, and is disposed between the at least one channel layer and the plurality of electrode layers along the one direction to realize a plurality of memory cells through a plurality of regions in contact with the plurality of electrode layers and used as a data storage area, The target memory cell is multilayered by changing the polarization charge amount of a part of the at least one ferroelectric film corresponding to the target memory cell to be the program operation target among the plurality of memory cells; The three-dimensional flash memory changes the polarization charge of the at least one ferroelectric film by adjusting the program voltage applied to the target storage unit between a negative value and a positive value; When a negative value of program voltage is applied to the target memory cell, a different negative value of program voltage is applied to multilayer the target memory cell, applying different negative voltages to the electrode layers corresponding to the target memory cells among the plurality of electrode layers, and applying 0V to the channel layer of the string where the target memory cell is located or to the channel layer of the substrate corresponding to the string, so that the target memory cell has a program voltage of different negative values for multilayering, Alternatively, 0V is applied to the electrode layer corresponding to the object memory cell, and a different positive voltage is applied to the channel layer of the string where the object memory cell is located or to the channel layer of the substrate corresponding to the string, so that the object memory cell has a program voltage of different negative values for multi-layering.
8. The three-dimensional flash memory according to claim 7, It is characterized in that The three-dimensional flash memory changes the polarization charge amount of the at least one ferroelectric film by applying mutually different negative and positive program voltages to the target memory cell.
9. The three-dimensional flash memory according to claim 7, It is characterized in that The three-dimensional flash memory controls the number of polarized atoms or the polarization rotation angle in a portion of the at least one ferroelectric film by adjusting the program voltage applied to the object storage unit between negative and positive values, and changes the polarization charge based on the controlled number of atoms or polarization rotation angle.
10. A method for realizing multi-layering of a three-dimensional flash memory, wherein the three-dimensional flash memory include: At least one channel layer is formed on the substrate and extends along a direction; A plurality of electrode layers are stacked in a vertical direction relative to the at least one channel layer; and at least one ferroelectric film, surrounding the at least one channel layer, in a state of being disposed along the one direction between the at least one channel layer and the plurality of electrode layers, so as to realize a plurality of memory cells through a plurality of regions in contact with the plurality of electrode layers and serve as a data storage area, The above-mentioned method for realizing multi-layered three-dimensional flash memory is characterized by comprising: A determining step of determining a range of a program voltage to be applied to a target memory cell of the plurality of memory cells to be a program operation target between a negative value and a positive value; an adjusting step of adjusting a program voltage applied to the target memory cell within a range between a negative value and a positive value based on the determination result; and A multilayering step, in which the target memory cell is multilayered by changing the amount of polarization charge of a portion of the at least one ferroelectric film corresponding to the target memory cell as the program voltage applied to the target memory cell is adjusted; When a negative value of program voltage is applied to the target memory cell, a different negative value of program voltage is applied to multilayer the target memory cell, applying different negative voltages to the electrode layers corresponding to the target memory cells among the plurality of electrode layers, and applying 0V to the channel layer of the string where the target memory cell is located or to the channel layer of the substrate corresponding to the string, so that the target memory cell has a program voltage of different negative values for multilayering, Alternatively, 0V is applied to the electrode layer corresponding to the object memory cell, and a different positive voltage is applied to the channel layer of the string where the object memory cell is located or to the channel layer of the substrate corresponding to the string, so that the object memory cell has a program voltage of different negative values for multi-layering.
11. The method for realizing multi-layered three-dimensional flash memory according to claim 10, It is characterized in that In the determining step, a range of a program voltage applied to the target memory cell is determined between a negative value and a positive value based on a thickness of the at least one ferroelectric film and a breakdown voltage of the at least one ferroelectric film.