Semiconductor device and method for manufacturing semiconductor device
By forming a material film and a resist film with a predetermined pattern on the front of the semiconductor substrate, the problem of uneven thickness of the resist film is solved, impurity introduction and cost control with high position accuracy are achieved, and performance and efficiency of the semiconductor device are improved. .
Patent Information
- Application Number
- CN202080018058.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Priority Date
- 2019-09-05
- Filing Date
- 2020-08-11
- Publication Date
- 2024-12-03
- Estimated Expiration
- 2040-08-11
AI Technical Summary
When existing semiconductor wafers are irradiated with helium, the uneven thickness of the resist film causes an increase in leakage current and conduction loss in the IGBT region. In order to thicken the resist film thickness, it is usually necessary to increase the resist material or usage amount, resulting in Increased cost.
By forming a material film of a predetermined pattern on the front surface of the semiconductor substrate and providing a resist film at a predetermined distance away from the opening of the protective film, a resist film covering the entire impurity defect introduction area is formed, ensuring a high position of the impurity defect. Accuracy is introduced, and multiple material films are arranged within a distance less than 1 mm from the protective film to reduce step height and achieve equal thickness of the resist film.
It is possible to introduce impurities with high position accuracy in a predetermined area, prevent cost increase, and ensure equal thickness of the resist film, thereby improving the performance of the semiconductor device and reducing production costs.
Smart Images

Figure CN113544824B_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to a semiconductor device and a method for manufacturing the semiconductor device. Background Art
[0002] In the past, a power element has been developed that achieves improved characteristics and characteristics by introducing impurity defects that act as carrier lifetime inhibitors into the interior of a semiconductor substrate through ion implantation at a high acceleration energy from the surface of the semiconductor substrate to a relatively deep position. The structure of a conventional semiconductor device into which impurity defects that act as carrier lifetime inhibitors are introduced is described. Fig.12 , Fig.13 This is a plan view showing an example of the layout of a conventional semiconductor device as viewed from the front side of a semiconductor substrate. Fig.14 , Fig.15 It is shown Fig.12 A cross-sectional view of an example of a cross-sectional structure taken along the cutting line AA-AA′.
[0003] For example, in a reverse-conducting IGBT (RC-IGBT) having a structure in which an IGBT (Insulated Gate Bipolar Transistor) and a FWD (Free Wheeling Diode) connected in reverse parallel to the IGBT are built into the same semiconductor substrate (semiconductor chip) 110 and integrated, impurity defects 114 that serve as carrier lifetime inhibitors are introduced into the n-type IGBT by helium (He) irradiation. - Type drift region 101 (refer to Fig.14 ).
[0004] Specifically, Fig.12 , Fig.13 The conventional semiconductor device 140 shown in the figure includes an IGBT region 131 serving as an IGBT operation region and a FWD region 132 serving as an FWD operation region in an active region 141 of a semiconductor substrate 110. The IGBT region 131 and the FWD region 132 are disposed along the front surface (n) of the semiconductor substrate 110. + The IGBT region 131 and the FWD region 132 are arranged alternately and repeatedly in contact with each other in a first direction X parallel to the main surface of the semiconductor substrate 110 on the side of the emitter region 103. The IGBT region 131 and the FWD region 132 are arranged in a strip shape extending in a second direction Y parallel to the front surface of the semiconductor substrate 110 and orthogonal to the first direction X. The edge termination region 142 surrounds the periphery of the active region 141.
[0005] The front surface of the semiconductor substrate 110 is covered with a polyimide film (hereinafter referred to as a polyimide protective film) 121 as a passivation protective film. The polyimide protective film 121 is formed with an opening 121a that exposes the entire area of the active region 141. The polyimide protective film 121 is left in the edge termination region 142 ( Fig.12 In the opening 121a of the polyimide protective film 121, polyimide protective films 122 and 123 ( ) serving as passivation protective films may be left in a manner that covers the p-type well region directly below the gate wiring layer (not shown) disposed in the active region 141 and directly below the cathode wiring layer (not shown) of the temperature sensing diode. Fig.13 ). The IGBT region 131 is located directly below the polyimide protection films 122 and 123 .
[0006] In FWD zone 132, in n - The interior of the drift region 101 is n - Impurity defects 114 generated by helium irradiation are introduced near the boundary between the n-type drift region 101 and the n-type carrier storage region 104. - The impurity defects 114 are introduced into the drift region 101, thereby shortening the carrier lifetime of minority carriers in the FWD region 132 and shortening the reverse recovery time of the FWD. If the helium irradiation is performed from the entire surface of the semiconductor substrate 110, the impurity defects 114 are introduced into the entire region of the semiconductor substrate 110, and therefore the impurity defects 114 are also introduced into the IGBT region 131 ( Fig.14 ).
[0007] When the impurity defects 114 are introduced into the IGBT region 131, it is confirmed that the leakage current and / or conduction loss of the IGBT increases. Therefore, a method of shielding the helium irradiation to the IGBT region 131 and introducing the impurity defects 114 only into the FWD region 132 is proposed ( Fig.15 In this case, for example, the impurity defects 114 are introduced into the entire region of the FWD region 132 in a manner extending to a portion (hereinafter referred to as an overlapping region) 133 of the IGBT region 131 on the FWD region 132 side. The impurity defects 114 may be caused by hydrogen ions (H + ) irradiation introduces hydrogen ion defects.
[0008] exist Fig.12 , Fig.13 In the figure, the dotted line is used to indicate that the intermediate region between the active region 141 and the edge termination region 142 is disposed on the surface region of the front side of the semiconductor substrate 110 and surrounds the active region 141. + The profile of the type well region 116 is shown by using the ratio +The thicker dashed line of the outline of the well region 116 indicates the boundary between the short carrier lifetime region 134 where the impurity defects 114 are introduced by helium irradiation to shorten the carrier lifetime and the region where the impurity defects 114 are not introduced. The passivation protective film (polyimide protective films 121 to 123) is indicated by a thick outline and hatching.
[0009] Reference numerals 102, 108, 109, 111, 113, and 115 are respectively a p-type base region, an interlayer insulating film, an emitter, and a p-type electrode of the IGBT region 131. + The symbol 112 is the n type collector region, the n type field stop region and the collector. + The p-type base region 102, the emitter 109 and the collector 115 are also arranged in the FWD region 132, and serve as the p-type anode region, the anode electrode and the cathode electrode of the FWD respectively. The trench gate structure formed by the trench 105, the gate insulating film 106 and the gate electrode 107 is also arranged in the FWD region 132.
[0010] The method of introducing the impurity defects 114 will be described by taking the case of introducing the impurity defects 114 by helium irradiation as an example. Fig.16 , Fig.17 1 is a cross-sectional view showing a state in the middle of manufacturing a conventional semiconductor device. Fig.16 As shown, from the back side (p + When helium irradiation 152 is performed on the main surface of the collector region 111 side, the helium irradiation 152 is performed using high acceleration energy in a manner such that the defect amount of the impurity defects 114 becomes maximum (defect peak) at a position deeper from the back side of the semiconductor wafer 110', and therefore a metal mask 151 with high shielding energy is used as a shielding film.
[0011] Specifically, after the element structures of the IGBT and FWD are formed on the semiconductor wafer 110', the metal mask 151 is fixed to the semiconductor wafer 110' by, for example, a fixing clip or a screw (not shown) so as to face the back side of the semiconductor wafer 110'. By using the metal mask 151 as a mask and performing helium irradiation 152 from the back side of the semiconductor wafer 110', the impurity defects 114 are introduced from the opening 151a of the metal mask 151 to a position shallower than the bottom surface of the trench 105 from the back side of the semiconductor wafer 110' in the overlapping region 133 of the IGBT region 131 and the FWD region 132.
[0012] Since the metal mask 151 is mechanically processed by cutting or wire cutting, the position accuracy and / or processing accuracy of the opening 151a is deteriorated. In addition, since the positioning (alignment) accuracy between the metal mask 151 and the semiconductor wafer 110' is about several tens of μm, it is difficult to achieve sub-micron positioning with the resist film 161 (see FIG. 1 ) formed by photolithography. Fig.17 ) compared to the positioning accuracy. Fig.17 As shown, in the case of performing helium irradiation 162 from the front side of the semiconductor wafer 110 ′, the resist film 161 having more favorable processing accuracy and / or positioning accuracy than the metal mask 151 can be used as a shielding film.
[0013] Specifically, after the element structures of the IGBT and FWD are formed on the semiconductor wafer 110', a resist film 161 having an opening 161a for exposing the overlapping region 133 of the IGBT region 131 and the FWD region 132 is formed on the front surface of the semiconductor wafer 110'. By using the resist film 161 as a mask (blocking film), helium irradiation 162 is performed in a manner that passes over the emitter 109, thereby introducing impurity defects 114 into the overlapping region 133 of the IGBT region 131 and the FWD region 132 at a position deeper than the bottom surface of the trench 105 from the front surface of the semiconductor wafer 110'.
[0014] As a method for selectively injecting impurities using a resist film as a shielding film, a method for forming a resist film having a thickness of 220 μm or more that can be used as a shielding film during helium irradiation by controlling the number of revolutions of a semiconductor wafer when applying the resist using a spin coating method and when removing the end of the dried resist film has been proposed (for example, refer to Patent Document 1 below). In Patent Document 1 below, a high-viscosity resist is used and / or the resist coating is performed twice or more to ensure a predetermined thickness of the resist film. In addition, Patent Document 1 below discloses that both positive resists and negative resists can be applied.
[0015] In addition, as another method for selectively injecting impurities by using a resist film as a shielding film, a method for preventing impurities from being injected into a region where impurities are not required by determining the thickness of the resist film based on the range of the injected impurities in the semiconductor substrate has been proposed (for example, refer to the following patent document 2). The following patent document 2 discloses the use of a negative photosensitive dry film as a thick resist film that can be used as a shielding film. In addition, the following patent document 2 discloses the use of an inkjet method to eject a resist to form a resist film of a predetermined thickness at a predetermined location.
[0016] Prior art literature
[0017] Patent Literature
[0018] Patent Document 1: International Publication No. 2018 / 105299
[0019] Patent Document 2: Japanese Patent Application Publication No. 2017-092256 Summary of the invention
[0020] Technical issues
[0021] When the helium irradiation 162 is performed from the front surface of the semiconductor wafer 110' as described above, the resist film 161 can be used as a shielding film (see Fig.17 ). When the resist film 161 is formed on the front surface of the semiconductor wafer 110', the resist is applied on the step on the front surface of the semiconductor wafer 110' (hereinafter referred to as the step on the front surface of the semiconductor wafer 110') generated by the formed front element structure. At this time, the thickness of the resist film 161 may become uneven due to the step on the front surface of the semiconductor wafer 110'.
[0022] The step on the front surface of the semiconductor wafer 110' is a step caused by the height difference between the surface of the polyimide protection film 121 and the surface of the emitter 109 exposed in the opening 121a of the polyimide protection film 121. Fig.11 2 shows a state in which the thickness of the resist film 161 formed on the front surface of the semiconductor wafer 110 ′ is not made uniform. Fig.11 1 is a cross-sectional view showing a state in the middle of manufacturing a conventional semiconductor device. Fig.11 In the figure, the trench gate structure of the front device structure formed on the front side of the semiconductor wafer 110 ′ and the device structure on the back side of the semiconductor wafer 110 ′ are omitted.
[0023] Specifically, if Fig.11 As shown, the resist film 161 generally has thicker thicknesses t101 and t103 near a portion higher than other portions such as the polyimide protective film 121 on the front surface of the semiconductor wafer 110', and the thickness t102 tends to become thinner at a portion away from the high portion. If the resist film 161 has a portion with a thinner thickness t102, helium (or hydrogen ions in hydrogen ion irradiation) is introduced into the portion of the IGBT region 131 that should be shielded except for the overlapping region 133 during the helium irradiation 162.
[0024] When helium or hydrogen ions are introduced into the portion of the IGBT region 131 other than the overlap region 133, the leakage current increases, the conduction loss increases, and the gate threshold voltage decreases in the IGBT region 131, thereby causing the IGBT characteristics to deteriorate. In order to solve this problem, the thickness of the resist film 161 can be increased as a whole so that the portion where the thickness t102 of the resist film 161 is thinned is thickened to a degree that it can be used as a shielding film during helium irradiation 162.
[0025] However, in order to further increase the thickness of the entire resist film 161, it is necessary to change the resist material or increase the amount of resist used, etc. The increase in the amount of resist used also includes applying the resist in a double-layered manner as a resist film to be the resist film 161. Such measures for increasing the thickness of the resist film 161 generally have the problem of increasing costs.
[0026] In order to eliminate the above-mentioned problems based on the prior art, the present invention aims to provide a semiconductor device and a method for manufacturing a semiconductor device, which can use a resist film as a shielding film to introduce predetermined impurities into a predetermined area with high positional accuracy and prevent cost increases.
[0027] Technical Solution
[0028] In order to solve the above-mentioned problems and achieve the purpose of the present invention, the manufacturing method of the semiconductor device of the present invention has the following characteristics. A first process is performed to form a predetermined element structure on the front side of the semiconductor substrate. A second process is performed to form a protective film for protecting the element structure on the front side of the semiconductor substrate. A third process is performed to form a predetermined pattern of a material film at an opening of the protective film at a predetermined distance from the protective film on the front side of the semiconductor substrate. A fourth process is performed to form a resist film on the front side of the semiconductor substrate that covers the protective film and the material film and has an introduction area for impurity defects. A fifth process is performed to introduce the impurity defects into the interior of the semiconductor substrate using the resist film as a mask. In the third process, at least one material film is formed at least at the predetermined distance less than 1 mm from the protective film.
[0029] In addition, the method for manufacturing a semiconductor device according to the present invention is characterized in that, in the above invention, there are a plurality of the material films, and in the third step, the plurality of the material films are arranged at intervals of less than 1 mm.
[0030] In addition, the method for manufacturing a semiconductor device according to the present invention is characterized in that, in the fourth step, the material film is completely covered with the resist film.
[0031] In addition, the method for manufacturing a semiconductor device of the present invention is characterized in that, in the fourth step, the distance from the material film to the end of the resist film covering the material film is set to be greater than 20 μm and less than 1 mm.
[0032] In addition, the method for manufacturing a semiconductor device of the present invention is characterized in that, in the third step, the material film is formed at a height that is more than half the height of the protective film and less than the same height as the protective film.
[0033] In addition, the method for manufacturing a semiconductor device according to the present invention is characterized in that, in the third step, the material film is formed to extend linearly in a direction parallel to the front surface of the semiconductor substrate.
[0034] In addition, the method for manufacturing a semiconductor device according to the present invention is characterized in that the third step is performed simultaneously with the second step, and the material film is formed using the same material as that of the protective film.
[0035] In addition, in the method for manufacturing a semiconductor device according to the present invention, in the above invention, the protective film is a polyimide film.
[0036] In addition, the method for manufacturing a semiconductor device of the present invention is characterized in that, based on the above invention, in the first step, an insulated gate bipolar transistor is formed as the element structure in the first region of the active region of the semiconductor substrate, and a diode reversely connected in parallel with the insulated gate bipolar transistor is formed in the second region of the active region other than the first region. In the second step, the protective film is formed to expose the active region in the opening. In the third step, a predetermined pattern of the material film is formed in the first region in the opening of the protective film. In the fifth step, the impurity defects are introduced into the entire region of the second region using the resist film as a mask.
[0037] In addition, the method for manufacturing a semiconductor device according to the present invention is characterized in that, in the fifth step, the impurity defects are introduced near a boundary between the first region and the second region using the resist film as a mask.
[0038] In addition, in order to solve the above-mentioned problems and achieve the purpose of the present invention, the semiconductor device of the present invention has the following characteristics. A predetermined element structure is provided on the front surface of the semiconductor substrate. The element structure is an insulated gate bipolar transistor provided in a first region of the active region of the semiconductor substrate, and a diode provided in a second region other than the first region of the active region and connected in reverse parallel to the insulated gate bipolar transistor.
[0039] A protective film for protecting the element structure is provided on the front side of the semiconductor substrate. The protective film has an opening portion exposing the active area. In the opening portion of the protective film, at least one material film is provided in a predetermined pattern at a predetermined distance from the protective film in the first region. A low carrier lifetime region in which the carrier lifetime is shortened by introducing impurity defects is provided in the entire area of the second region. The material film is characterized in that it is at least arranged at the predetermined distance less than 1 mm from the protective film.
[0040] In addition, the semiconductor device of the present invention is characterized in that, in the above invention, there are a plurality of the material films, and in the first region, the plurality of the material films are arranged at intervals of less than 1 mm.
[0041] In addition, the semiconductor device of the present invention is characterized in that, based on the above invention,
[0042] The height of the material film is not less than half the height of the protective film and not more than the same height as the height of the protective film.
[0043] In addition, in the semiconductor device of the present invention, the protective film is a polyimide film, and the material film is the same polyimide film as the protective film.
[0044] According to the above invention, the pattern interval between the protective film and the material film on the front side of the semiconductor wafer (semiconductor substrate) can be narrowed. Thus, the step height of the front side of the semiconductor wafer can be increased, and the resist film can be formed to a substantially uniform thickness that can function as a shielding film regardless of the distance from the protective film within the surface of the semiconductor wafer.
[0045] Technical Effects
[0046] According to the semiconductor device and the method for manufacturing the semiconductor device of the present invention, it is possible to introduce a predetermined impurity into a predetermined region with high positional accuracy using a resist film as a shielding film, and to prevent an increase in cost. BRIEF DESCRIPTION OF THE DRAWINGS
[0047] Figure 11 is a plan view showing a state where the semiconductor device according to the first embodiment is viewed from the front side of the semiconductor substrate.
[0048] Figure 2 It is shown Figure 1 A cross-sectional view of the cross-sectional structure taken along the cutting line AA'.
[0049] Figure 3 This is a cross-sectional view showing a state in the middle of manufacturing the semiconductor device according to the first embodiment.
[0050] Figure 4 This is a cross-sectional view showing a state in the middle of manufacturing the semiconductor device according to the first embodiment.
[0051] Figure 5 This is a cross-sectional view showing another example of a state during the manufacture of the semiconductor device according to the first embodiment.
[0052] Figure 6 This is a plan view showing an example of a state where the semiconductor device according to the second embodiment is viewed from the front side of the semiconductor substrate.
[0053] Figure 7 This is a plan view showing an example of a state where the semiconductor device according to the second embodiment is viewed from the front side of the semiconductor substrate.
[0054] Figure 8 This is a plan view showing an example of a state where the semiconductor device according to the second embodiment is viewed from the front side of the semiconductor substrate.
[0055] Fig. 9 This is a plan view showing an example of a state where the semiconductor device according to the second embodiment is viewed from the front side of the semiconductor substrate.
[0056] Fig.10 1 is a plan view showing an example of a state where the semiconductor device according to the third embodiment is viewed from the front side of the semiconductor substrate.
[0057] Fig.11 This is a cross-sectional view showing a state in the middle of manufacturing a conventional semiconductor device.
[0058] Fig.12 FIG. 1 is a plan view showing an example of a layout of a conventional semiconductor device as viewed from the front side of a semiconductor substrate.
[0059] Fig.13 FIG. 1 is a plan view showing an example of a layout of a conventional semiconductor device as viewed from the front side of a semiconductor substrate.
[0060] Fig.14 It is shown Fig.12 A cross-sectional view of an example of a cross-sectional structure taken along the cutting line AA-AA′.
[0061] Fig.15 It is shown Fig.12 A cross-sectional view of an example of a cross-sectional structure taken along the cutting line AA-AA′.
[0062] Fig.16 This is a cross-sectional view showing a state in the middle of manufacturing a conventional semiconductor device.
[0063] Fig.17 This is a cross-sectional view showing a state in the middle of manufacturing a conventional semiconductor device.
[0064] Explanation of symbols
[0065] 1 n - Drift zone
[0066] 2 p-type base region
[0067] 3 n + Type emission area
[0068] 4 n-type carrier accumulation region
[0069] 5 Grooves
[0070] 6 Gate insulation film
[0071] 7. Gate electrode
[0072] 8a Interlayer insulation film
[0073] 8b Field oxide film
[0074] 9 Front electrode
[0075] 10 Semiconductor substrate
[0076] 10' semiconductor wafer
[0077] 11 p + Type collector area
[0078] 12 n + Cathode region
[0079] 13 n-type FS region
[0080] 14 Impurity defects
[0081] 15 Back electrode
[0082] 16 p + Well
[0083] 18 n-type channel cutoff region
[0084] 20 Channel-interrupting electrode
[0085] 21. Polyimide protective film
[0086] 21a, 21b Opening of polyimide protective film
[0087] 22, 61, 62, 71, 72 Polyimide film for dummy pattern
[0088] 22a, 61a, 62a, 71a, 72a First polyimide film of polyimide film for dummy pattern
[0089] 22b, 61b, 62b, 71b, 72b Second polyimide film of polyimide film for dummy pattern
[0090] 31, 31' IGBT area
[0091] 32, 32' FWD Zone
[0092] 33, 33' Overlap Area
[0093] 34, 34' Low carrier lifetime region
[0094] 40, 40', 60, 60', 70, 70' semiconductor devices
[0095] 41 Active area
[0096] 42 Edge terminal area
[0097] 43 Middle District
[0098] 50 Chip Zone
[0099] 51 Cutting Area
[0100] 52, 52' Resist film
[0101] 52a, 52a' opening of resist film
[0102] h1 Height of polyimide film for dummy pattern
[0103] t1, t2 Thickness of resist film
[0104] w1, w31, w41, w51, w61 The distance between the first polyimide film and the polyimide protective film
[0105] w2, w32, w42, w42', w52, w62 The distance between the polyimide film used for the dummy pattern and the overlap area
[0106] w3, w33, w33', w43, w43', w53, w63 Distance between adjacent dummy pattern polyimide films
[0107] w4 Width of polyimide film for dummy pattern
[0108] w5 Width of cutting area
[0109] w6, w16, w16' Width of resist film
[0110] x1 Width of the IGBT region in the first direction
[0111] x2 The width of the FWD area in the first direction
[0112] x3 Width of the overlap area
[0113] x4, x4': opening width of the opening of the resist film
[0114] X Direction parallel to the front surface of the semiconductor substrate (first direction)
[0115] Y is a direction parallel to the front surface of the semiconductor substrate and perpendicular to the first direction (second direction)
[0116] Z Depth DETAILED DESCRIPTION
[0117] Hereinafter, with reference to the accompanying drawings, preferred embodiments of the semiconductor device and the method for manufacturing the semiconductor device of the present invention are described in detail. In this specification and the accompanying drawings, the layers or regions prefixed with n or p respectively indicate that electrons or holes are majority carriers. In addition, + and - marked on n or p respectively indicate that the impurity concentration is higher and lower than the impurity concentration of the layers or regions not marked with + and -. It should be noted that in the following descriptions of the embodiments and the accompanying drawings, the same symbols are marked for the same structures, and repeated descriptions are omitted.
[0118] (Implementation Method 1)
[0119] The structure of the semiconductor device according to the first embodiment will be described. Figure 1 1 is a plan view showing a state where the semiconductor device according to the first embodiment is viewed from the front side of the semiconductor substrate. Figure 1 The semiconductor device 40 of the first embodiment shown in the figure has an IGBT region (first region) 31 which is an IGBT operation region and a FWD region (second region) 32 which is an FWD operation region in an active region 41 of a semiconductor substrate (semiconductor chip) 10, and an impurity defect 14 which is a carrier lifetime inhibitor is introduced into the FWD region 32 by helium (He) irradiation (in Figure 2 RC-IGBT (indicated by × in the figure).
[0120] The IGBT region 31 and the FWD region 32 are connected to the front surface (n + Main surface of type emission region 3 side: refer to Figure 2) are arranged alternately and repeatedly in contact with each other in a first direction X parallel to the first direction X. The IGBT region 31 and the FWD region 32 are arranged in a strip shape extending in a second direction Y parallel to the front surface of the semiconductor substrate 10 and orthogonal to the first direction X. In the active region 41, the IGBT region 31 is arranged at the outermost side (chip end side) in the first direction X.
[0121] Impurity defects 14 are introduced into the semiconductor substrate 10 in the entire region of the overlapping region 33 described later of the IGBT region 31 and the entire region of the FWD region 32 (see Figure 2 By introducing the impurity defects 14, the carrier lifetime of minority carriers in the FWD region 32 can be shortened, and the reverse recovery time of the FWD can be shortened. The impurity defects 14 can be helium (He) defects introduced by helium irradiation or hydrogen ions (H + ) irradiation introduces hydrogen ion defects.
[0122] The portion (overlapping region) 33 from the boundary with the adjacent FWD region 32 in the IGBT region 31 to the predetermined width x3 in the first direction X is an ineffective region that does not operate as an IGBT. Since the overlapping region 33 reduces the characteristics of the IGBT, when the impurity defects 14 are introduced into the FWD region 32, the impurity defects 14 are also intentionally introduced into the overlapping region 33. The IGBT region 31 is a region that includes the overlapping region 33 and operates as an IGBT. In this embodiment, although the case where there is an overlapping region 33 is described, there may be a case where there is no overlapping region 33, and there may also be a case where there is a region where the impurity defects 14 are not formed on the FWD region 32 side.
[0123] The semiconductor substrate 10 has a rectangular planar shape, for example. One side of the width (chip size) of the semiconductor substrate 10 is, for example, greater than 4 mm and less than 20 mm. The width x1 of the IGBT region 31 in the first direction X is, for example, about 1200 μm. The width x2 of the FWD region 32 in the first direction X is, for example, about 600 μm. The active region 41 has a rectangular planar shape, for example. The active region 41 is a region where current flows when the IGBT is in the on state. The active region 41 is surrounded by an edge termination region 42.
[0124] The edge termination region 42 is a region between the active region 41 and the end (chip end) of the semiconductor substrate 10, and is a region for relaxing the electric field on the front side of the semiconductor substrate 10 to maintain a withstand voltage (voltage resistance). The withstand voltage is a limit voltage that does not cause malfunction and / or damage to the element when the leakage current does not increase excessively. The edge termination region 42 is provided with a withstand voltage structure such as a field limiting ring (FLR: Field Limiting Ring) 17 and / or a field plate (FP: Field Plate) 19.
[0125] The front surface of the semiconductor substrate 10 is covered with a polyimide film (polyimide protective film) 21 as a passivation protective film. The polyimide protective film 21 is formed with an opening 21a that exposes the entire active region 41 and one or more openings 21b that selectively expose the edge termination region 42. The front electrode 9 (see FIG. 1 ) is exposed in the opening 21a that exposes the entire active region 41. Figure 2 The portion of the front electrode 9 exposed in the opening 21 a of the polyimide protective film 21 functions as a front electrode pad for extracting the potential of the front electrode 9 to the outside.
[0126] In the opening 21b (in the Figure 1 The electrode pads other than the front electrode pads are exposed. The electrode pads other than the front electrode pads are, for example, the gate electrodes 7 (see FIG. 1 ) of the IGBT region 31 and the gate electrodes 7 of the IGBT. Figure 2 ) is electrically connected to the gate pad, an electrode pad for current sensing that detects overcurrent (OC: Over Current) such as surge flowing through the IGBT, and an electrode pad for a temperature sensing unit that detects temperature using the temperature characteristics of a diode.
[0127] The polyimide protective film 21 covers the front surface of the semiconductor substrate 10 in the edge terminal area 42, and surrounds the active area 41 into a roughly rectangular shape. That is, the polyimide protective film 21 has openings 21a and 21b in the portion where the electrode pad is formed, and covers and protects the portion where the electrode pad is not formed. The end of the inner side (the center side of the chip) of the polyimide protective film 21 can extend to the middle area 43 between the active area 41 and the edge terminal area 42, and the end position is determined by the design conditions. The middle area 43 can be exposed in the opening 21a of the polyimide protective film 21.
[0128] In the opening 21a of the polyimide protective film 21, a dummy polyimide film (hereinafter referred to as a dummy pattern polyimide film (material film)) 22 that does not function as a passivation protective film is selectively provided in each IGBT region 31 except for the overlap region 33 described later. The dummy pattern polyimide film 22 is provided to prevent the resist film 52 (see FIG. 1 ) used as a shielding film during the helium irradiation described later from being formed. Figure 3 , Figure 4 ) is formed and arranged with approximately uniform thickness and remains in the original state in the product (semiconductor device 40). The helium irradiation is performed to introduce impurity defects 14 into the semiconductor substrate 10.
[0129] The dummy pattern polyimide film 22 is arranged so that the distance w1 between the dummy pattern polyimide film 22 and the polyimide protective film 21, the distance w2 between the dummy pattern polyimide film 22 and the overlap region 33, and the distance w3 between adjacent dummy pattern polyimide films 22 are within the range described below. By arranging the dummy pattern of the dummy pattern polyimide film 22 at these distances w1 to w3, the resist film 52 covering the polyimide protective film 21 and the dummy pattern polyimide film 22 can be formed with a substantially uniform thickness during the manufacture (manufacturing) of the semiconductor device 40. The substantially uniform thickness means that the thickness is substantially the same within the range including the error allowed due to the deviation of the process.
[0130] Specifically, a plurality of dummy pattern polyimide films 22 are provided in parallel with each other in a linear manner extending in the second direction Y. The dummy pattern polyimide film 22 can extend in the second direction Y and be connected to the polyimide protection film 21. At least one dummy pattern polyimide film 22 is arranged in the outermost IGBT region 31 in the first direction X. The one dummy pattern polyimide film 22 arranged in the outermost IGBT region 31 in the first direction X is a first polyimide film 22a arranged in the outermost side in the first direction X among the plurality of dummy pattern polyimide films 22.
[0131] The distance w1 between the first polyimide film 22a and the portion of the polyimide protective film 21 along the side parallel to the second direction Y is, for example, less than 1 mm. In addition, one or more dummy pattern polyimide films 22 are arranged in each IGBT region 31 in a manner that satisfies the conditions of a distance w2 from the overlapping region 33 described later and a distance w3 between adjacent dummy pattern polyimide films 22. The second polyimide film 22b other than the first polyimide film 22a among the plurality of dummy pattern polyimide films 22 is arranged at a position further inside than the first polyimide film 22a.
[0132] The second polyimide film 22b is arranged between the first polyimide film 22a and the overlapping region 33 in the outermost IGBT region 31 in the first direction X, and in the IGBT region 31 other than the outermost IGBT region 31 in the first direction X. When the distance (distance w2 described later) from the first polyimide film 22a to the overlapping region 33 of the outermost IGBT region 31 in the first direction X is less than 1 mm, the second polyimide film 22b may not be arranged in the outermost IGBT region 31 in the first direction X.
[0133] The dummy pattern polyimide film 22 is arranged to be separated from the adjacent overlapping region 33. Specifically, the dummy pattern polyimide film 22 may be separated from the adjacent overlapping region 33 by a distance of, for example, 20 μm or more and less than 1 mm. The lower limit of the distance w2 is the minimum distance ( 100 Å) from the end of the resist film 52 to the dummy pattern polyimide film 22 required to completely cover the dummy pattern polyimide film 22 with the resist film 52 when manufacturing the semiconductor device 40. Figure 4 The upper limit value of the distance w2 is the upper limit value for obtaining the effect of the first embodiment. The distance w3 between adjacent dummy pattern polyimide films 22 is, for example, less than 1 mm. That is, the plurality of dummy pattern polyimide films 22 are arranged at intervals less than 1 mm.
[0134] The height h1 of the dummy pattern polyimide film 22 (see Figure 2 ) is more than half the height of the polyimide protective film 21 and less than the height that is approximately the same as the height of the polyimide protective film 21. The lower the height h1 of the polyimide film 22 for the dummy pattern, the better the diffusion of the resist when the resist film 52 described later is formed. By setting the height h1 of the polyimide film 22 for the dummy pattern to be less than the height of the polyimide protective film 21, it is possible to form the resist film 52 with a substantially uniform thickness, and the resist film 52 is formed in a manner covering the polyimide film 22 for the dummy pattern when the semiconductor device 40 is manufactured. In addition, by configuring the polyimide film 22 for the dummy pattern in a straight line parallel to the front surface of the semiconductor substrate 10, the resist is easily diffused when the resist film 52 is formed.
[0135] The width w4 and height h1 of the dummy pattern polyimide film 22 are equal (width w4: height h1 = 1:1). Although the wider the width w4 of the dummy pattern polyimide film 22, the higher the strength of the dummy pattern polyimide film 22 becomes, the wider the width w4 of the dummy pattern polyimide film 22, the larger the surface area of the front electrode 9 covered by the dummy pattern polyimide film 22 becomes, which reduces the heat dissipation of the semiconductor substrate 10. Therefore, the width w4 of the dummy pattern polyimide film 22 is preferably as narrow as possible within the range of ensuring the strength of the dummy pattern polyimide film 22.
[0136] In addition, the dummy pattern polyimide film 22 is not arranged at the wire bonding portion. The surface of the front electrode 9 between the dummy pattern polyimide films 22 is wire-bonded. When a wire (not shown) with a diameter of, for example, 500 μm is bonded to the front electrode 9 between the dummy pattern polyimide films 22, although the load of the wire bonding tool is applied to the dummy pattern polyimide film 22, it does not adversely affect the electrical characteristics of the semiconductor device 40. The shape of the bonding wire may be linear or strip-shaped.
[0137] The polyimide film 22 for dummy patterns is not arranged in the low carrier lifetime region 34 where the impurity defects 14 are introduced. This is because the polyimide film 22 for dummy patterns functions as a shielding film during helium irradiation for introducing the impurity defects 14 described later. Instead of the dummy pattern of the polyimide film 22 for dummy patterns, a dummy pattern of a material film using another material as described later may be arranged. The dummy pattern of the polyimide film 22 for dummy patterns may be arranged in different layouts in each IGBT region 31.
[0138] exist Figure 1 In FIG. 4 , the outline of the intermediate region 43 between the active region 41 and the edge termination region 42 is indicated by a dotted line. The boundary between the low carrier lifetime region 34 where the impurity defects 14 are introduced to shorten the carrier lifetime and the region where the impurity defects 14 are not introduced is indicated by a dotted line thicker than the dotted line indicating the outline of the intermediate region 43. The region of the IGBT region 31 where the impurity defects 14 are not introduced is the region of the IGBT region 31 excluding the overlapping region 33. The polyimide protection film 21 and the polyimide film 22 for the dummy pattern (in FIG. 4 ) are indicated by a thick outline and hatching. Figure 6 to Figure 10 The same is true in ).
[0139] Next, a cross-sectional structure of the semiconductor device 40 according to the first embodiment will be described. Figure 2 It is shown Figure 1 A cross-sectional view of the cross-sectional structure of the cutting line AA'. Figure 2 As shown in FIG. 1 , the semiconductor device 40 of the first embodiment includes an active region 41 and an edge termination region 42 on a semiconductor substrate (semiconductor chip) 10 as described above, and includes an IGBT region 31 and a FWD region 32 on the active region 41. An n-type region extending from the active region 41 to the edge termination region 42 and reaching the end of the semiconductor substrate 10 is provided inside the semiconductor substrate 10. - Type drift region 1.
[0140] In the active region 41, the front surface of the semiconductor substrate 10 is connected to the n -In the IGBT region 31, an n-type base region 2 is selectively provided between the front surface of the semiconductor substrate 10 and the p-type base region 2 so as to be in contact with the p-type base region 2 and exposed to the front surface of the semiconductor substrate 10. + Type 3 emitter and p + Type contact area (not shown). + Type 3 emitter and p + For example, the type contact regions are in contact with each other and are alternately and repeatedly arranged along the second direction Y.
[0141] exist Figure 2 As shown in n + Type emission region 3, a cross-sectional structure of a cutting line AA' parallel to the first direction X, omitting a cross-sectional structure parallel to the first direction X and passing through p + The cross-sectional structure of the cutting line of the type contact area is shown in FIG. + Type contact area. Without setting p + In the case of type contact area, n + The n-type emission regions 3 are dispersed along the second direction Y. + Between the p-type emitter regions 3 , the p-type base region 2 is exposed on the front surface of the semiconductor substrate 10 .
[0142] In n - Between the p-type drift region 1 and the p-type base region 2, it can be connected to the n-type drift region 1 and the p-type base region 2. - An n-type carrier storage (CS: Carrier Storage) region 4 is provided in contact with the p-type drift region 1 and the p-type base region 2. The n-type carrier storage region 4 has a function of accumulating holes when the IGBT is turned on to reduce the surface resistance of the front side of the semiconductor substrate 10 and reduce the on-resistance of the IGBT. - The p-type drift region 1 and the p-type base region 2 are in contact with each other.
[0143] Groove 5 through n + Type emission region 3, p + type contact region, p-type base region 2 and n-type carrier accumulation region 4 to reach n - The trench 5 extends in a strip shape in the second direction. + The trench 5 is terminated in the well region 16. As described later, the trench 5 is also arranged in the FWD region 32. The outermost trench 5 in the first direction X is arranged in the intermediate region 43. A gate electrode 7 is provided inside the trench 5 via a gate insulating film 6.
[0144] In the FWD region 32, a p-type base region 2, an n-type carrier storage region 4, a trench 5, a gate insulating film 6, and a gate electrode 7 are provided in the same manner as in the IGBT region 31. The p-type base region 2 and the n-type carrier storage region 4 extend from the IGBT region 31 to the FWD region 32. In the FWD region 32, the p-type base region 2 functions as a p-type anode region. The trench 5 is arranged in parallel with the trench 5 of the IGBT region 31 at the same pitch as the trench 5 of the IGBT region 31. No n-type base region 2 is provided in the FWD region 32. + Type emission area 3.
[0145] The back surface of the semiconductor substrate 10 is connected to the n - There is a p + Type collector region 11, n + p-type cathode region 12 and n-type field stop (FS: Field Stop) region 13. + The p-type collector region 11 is arranged in the IGBT region 31 and is exposed on the back surface of the semiconductor substrate 10. The p-type collector region 11 arranged on the outermost side of the IGBT region 31 in the first direction X + The collector region 11 extends from the IGBT region 31 toward the edge termination region 42 and reaches the end of the semiconductor substrate 10 .
[0146] n + The cathode region 12 is arranged in the FWD region 32 and is exposed on the back surface of the semiconductor substrate 10. + The cathode region 12 is connected to the p-type cathode region 12 in the first direction X. + The collector region 11 is in contact with the p + The n-type collector region 11 is arranged in parallel. - The n-type FS region 13 contacts the p-type drift region 1 and extends from the active region 41 to the edge termination region 42 to reach the end of the semiconductor substrate 10. The n-type FS region 13 has a function of suppressing the extension of the depletion layer extending from the pn junction between the p-type base region 2 and the n-type carrier storage region 4 when the IGBT is turned off.
[0147] In the overlapping region 33 of the IGBT region 31 and the FWD region 32, - Inside the drift region 1, toward n - An impurity defect 14 is introduced near the boundary between the n-type drift region 1 and the n-type carrier accumulation region 4. The impurity defect 14 has an impurity concentration peak (maximum value) at a depth of, for example, about 15 μm from the front surface of the semiconductor substrate 10 and at a depth of, for example, about 100 μm from the back surface of the semiconductor substrate 10. The overlapping region 33 of the IGBT region 31 and the FWD region 32 are low carrier lifetime regions 34 where the impurity defects 14 are introduced to shorten the carrier lifetime.
[0148] In the entire area of the intermediate region 43, the front surface of the semiconductor substrate 10 and the n -There is a p + type well region 16. + The inner part of the well region 16 is the active region 41. + The portion between the well region 16 and the end of the semiconductor substrate 10 is an edge termination region 42. + The well region 16 and the n - The p-type drift region 1 is in contact with the p-type base region 2 and is exposed on the front surface of the semiconductor substrate 10. + The type well region 16 reaches a position deeper than the trench 5 from the front surface of the semiconductor substrate 10 and surrounds the entire trench 5 at the outermost side in the first direction. + The end of the well region 16 in the second direction Y of the trench 5 surrounds the bottom surface of the trench 5 .
[0149] In the edge termination region 42, the front surface of the semiconductor substrate 10 is connected to the n - type drift region 1, at a ratio of p + The well region 16 is located further outside and adjacent to the p + A plurality of field limiting rings (FLRs) 17 as floating p-type regions are provided separately from the p-type well region 16. In addition, in the edge termination region 42, the front surface of the semiconductor substrate 10 and the n-type well region 16 are connected to each other. - Between the n-type drift regions 1, an n-type channel stopper region 18 is selectively provided outside the FLR 17 and separated from the FLR 17.
[0150] FLR17 and n-type channel stopper region 18 are connected to n - The FLR 17 is in contact with the p-type drift region 1 and is exposed to the front surface of the semiconductor substrate 10. The FLR 17 is a substantially rectangular planar shape (not shown) and + The n-type well region 16 is surrounded by concentric circles. The n-type channel stopper region 18 is exposed to the end of the semiconductor substrate 10. In the active region 41, the interlayer insulating film 8a is provided on the front surface of the semiconductor substrate 10 and covers the gate electrode 7. In the edge termination region 42, the field oxide film 8b is provided on the front surface of the semiconductor substrate 10.
[0151] In the IGBT region 31, the front electrode 9 is connected to the n through the contact hole of the interlayer insulating film 8a. + Type 3 emitter and p + The IGBT region 31 is not provided with a p-type contact region. + In the case of a type contact region, the front electrode 9 is connected to the n + The p-type emitter region 3 is in contact with and electrically connected to the p-type base region 2. The front electrode 9 is electrically insulated from the gate electrode 7 by an interlayer insulating film 8a.
[0152] In the FWD region 32, the front electrode 9 is connected to the p-type base region 2 (in the case where the p + In the case of a p-type contact region, the p-type base region 2 and the p + The front electrode 9 also serves as an anode electrode. The front electrode 9 extends from the active area 41 to the middle area 43. + In the middle region 43, the front electrode 9 is connected to the p-type well region 16 via the contact hole of the interlayer insulating film 8a. + The well region 16 is in contact with each other and is electrically connected.
[0153] The FP19 is separated from the front electrode 9 and arranged at a position opposite to each FLR17 in the depth direction Z. Each FP19 contacts and is electrically connected to the FLR17 opposite to each other in the depth direction Z via the contact hole of the field oxide film 8b. The channel stopper electrode 20 is separated from the FP19 and arranged at a position opposite to the n-type channel stopper region 18 in the depth direction Z. The channel stopper electrode 20 contacts and is electrically connected to the n-type channel stopper region 18 via the contact hole of the field oxide film 8b.
[0154] The polyimide protective film 21 is provided in substantially the entire area of the edge termination region 42 and covers the FP19 and the channel stopper electrode 20. The polyimide protective film 21 extends from the edge termination region 42 to the middle region 43 and covers the end of the front electrode 9. In the area other than the overlap region 33 of the IGBT region 31, the dummy pattern polyimide film 22 is selectively provided on the front electrode 9. The back electrode 15 is provided on the entire back side of the semiconductor substrate 10 and is in contact with the p + Type collector region 11 and n + The back electrode 15 is electrically connected to the cathode region 12. The back electrode 15 serves as both a collector electrode and a cathode electrode.
[0155] Next, the method for manufacturing the semiconductor device 40 according to the first embodiment will be described by taking the case of manufacturing an RC-IGBT of a withstand voltage class of 1200 V as an example. Figure 3 , Figure 4 This is a cross-sectional view showing a state in the middle of manufacturing the semiconductor device according to the first embodiment. Figure 5 This is a cross-sectional view showing another example of a state during the manufacture of the semiconductor device according to the first embodiment. Figure 3 to Figure 5 FIG. 2 shows a state after the formation of a resist film 52 serving as a shielding film during helium irradiation. Figure 3 4 shows the vicinity of a dicing region 51 of a semiconductor wafer 10 ′.
[0156] exist Figure 4 , Figure 5 FIG. 5 shows a chip region 50, which is provided in plurality on the semiconductor wafer 10' and becomes the semiconductor substrate 10 when cut from the semiconductor wafer 10' (see FIG. 5 ). Figure 1 ).exist Figure 3 to Figure 5 In the figure, n is omitted + Type emission region 3, p + The type contact region, the trench gate structure, the interlayer insulating film 8a, the field oxide film 8b and the parts on the back side of the semiconductor wafer 10'. Figure 4 , Figure 5 In the figure, the voltage-withstand structure of the n-type carrier accumulation region 4 and the edge termination region 42 is omitted. Figure 1 , Figure 2 Yes Figure 3 to Figure 5 The parts not shown in the figure are described below.
[0157] First, prepare to become n - The resistivity of the drift region 1 is high n - A semiconductor wafer 10' of type is prepared. The front side of the semiconductor wafer 10' may be, for example, a (001) side. The thickness of the semiconductor wafer 10' (the thickness before back grinding described later) may also be, for example, 725 μm. Next, a process consisting of photolithography and ion implantation is repeatedly performed under different conditions to form a p-type base region 2 and an n-type carrier storage region 4 in the entire area of the active region 41 of each chip region 50 of the semiconductor wafer 10'.
[0158] Next, the front surface of the semiconductor wafer 10' is thermally oxidized to form a field oxide film 8b covering the front surface of the semiconductor wafer 10' in the edge termination region. Next, photolithography and etching are used to form a field oxide film 8b in the IGBT region 31 that penetrates the p-type base region 2 and the n-type carrier storage region 4 and reaches the n-type carrier storage region 4. - A trench 5 of the type drift region 1 is formed. Next, a gate insulating film 6 is formed along the inner wall of the trench 5 by, for example, thermal oxidation, and a polysilicon (poly-Si) layer is buried in the trench 5 to form a gate electrode 7.
[0159] Next, a set of processes including photolithography and ion implantation is repeatedly performed under different conditions to selectively form n IGBT regions 31 in the active regions 41 of the chip regions 50 of the semiconductor wafer 10 ′. + Type 3 emitter and p + In addition, a p-type contact region is selectively formed in the middle region 43 of each chip region 50 of the semiconductor wafer 10'. + The FLR 17 and the n-type channel stopper region 18 are selectively formed in the FWD region 32 of each chip region 50 of the semiconductor wafer 10'.
[0160] Next, after forming the interlayer insulating film 8a on the front surface of the semiconductor wafer 10', the interlayer insulating film 8a is selectively removed to leave only the portion covering the gate electrode 7, thereby forming a gate electrode in the active region 41. + Type 3 emitter and p+ At this time, when forming the contact hole in the active region 41, the field oxide film 8b and the gate insulating film 6 are selectively removed to form contact holes in the edge termination region 42 to expose the FLR 17 and the n-type channel stopper region 18, respectively.
[0161] Next, on the front side of the semiconductor wafer 10', a metal electrode is formed and patterned in a manner of burying the contact hole, leaving a portion to become the front electrode 9, FP19, and the channel stopper electrode 20. At this time, an electrode layer (for example, a gate pad of an IGBT, an electrode pad for current sensing, and an electrode pad for a temperature sensing portion, etc.) provided at the same level as the front electrode 9 can be formed simultaneously with the formation of the front electrode 9. Next, the semiconductor wafer 10' is ground from the back side (back grinding) until it reaches the position of the product thickness.
[0162] Next, a set of processes consisting of photolithography and ion implantation is repeatedly performed under different conditions to form n electrodes at different depths from the back surface of the semiconductor wafer 10' and from the active region 41 to the entire chip region 50. + Then, by using photolithography and ion implantation of p-type impurities, n-type cathode region 12 and n-type FS region 13 are formed. + The portion of the cathode region 12 corresponding to the IGBT region 31 becomes p + Type thus forming p + Type collector region 11 (first step).
[0163] Then, if Figure 3 , Figure 4 As shown, in the edge termination region 42, a polyimide protective film 21 serving as a passivation protective film and a dummy pattern of a polyimide film 22 (22a, 22b) for a dummy pattern are formed on the front surface of the semiconductor wafer 10' (second process, third process). In the region other than the overlap region 33 of the IGBT region 31, a dummy pattern of a polyimide film 22 for a dummy pattern is formed on the front surface electrode 9 under the condition of the above-mentioned distance w1 to w3. The polyimide protective film 21 and the polyimide film 22 for a dummy pattern may be, for example, a non-photosensitive polyimide film.
[0164] The polyimide protective film 21 and the polyimide film 22 for the dummy pattern may also be formed at the same time. In this case, the polyimide film applied to the entire front surface of the semiconductor wafer 10' is selectively removed by wet etching, leaving the portion that becomes the polyimide protective film 21 and the polyimide film 22 for the dummy pattern. By using wet etching in the process of selectively removing the polyimide film, it is possible to suppress damage to the metal electrode on the front surface of the semiconductor wafer 10'. The cross-sectional shape of the polyimide film 22 for the dummy pattern may be a roughly rectangular shape or a trapezoidal shape (not shown) whose width becomes narrower as it moves away from the front surface of the semiconductor wafer 10'.
[0165] As long as a dummy pattern of a material film of a predetermined height h1 is formed on the front electrode 9 under the conditions of the above-mentioned distances w1 to w3 in the region other than the overlapping region 33 of the IGBT region 31, a dummy pattern may be formed using other compositions or other materials instead of the dummy pattern polyimide film 22. For example, instead of the dummy pattern polyimide film 22, a metal film such as aluminum, a resist film having a composition different from that of the resist film 52 to be a shielding film described later, and a polyimide film having a composition different from that of the polyimide protective film 21 may be formed.
[0166] The polyimide protective film 21 is not formed in a dicing area 51 where, for example, a dicing line is formed. The dicing area 51 is an area between adjacent chip areas 50 of the semiconductor wafer 10' that is not used as the semiconductor substrate 10. The width w5 of the dicing area 51 is, for example, about 100 μm. Figure 3 , Figure 4 In the embodiment, although the n-type channel stopper region 18 is formed in the cut region 51 , since the cut region 51 is a region that is removed by cutting, no impurity diffusion region may be formed in the cut region 51 .
[0167] Next, a resist film 52 is formed on the front surface of the semiconductor wafer 10' so as to open the overlap region 33 of the IGBT region 31 and the portion corresponding to the FWD region 32 (the fourth step). By forming the dummy pattern of the dummy pattern polyimide film 22 (22a, 22b) in the region other than the overlap region 33 of the IGBT region 31 as described above, the pattern interval of the polyimide film (the pattern interval between the polyimide protection film 21 and the dummy pattern polyimide film 22, and the pattern interval between adjacent dummy pattern polyimide films 22) is narrowed.
[0168] The pattern of the passivation protective film is the highest step in the surface of the semiconductor wafer 10'. Fig.11), the polyimide protective film 121 functioning as a passivation protective film is provided only on the periphery of the chip region 150 in a manner surrounding the periphery of the active region 141. Therefore, although the thicknesses t101 and t103 of the resist film 161 near the polyimide protective film 121 hardly change, the thickness t102 becomes thinner as it moves away from the polyimide protective film 121 toward the inner side (the central side of the chip region 50).
[0169] Specifically, the thickness difference t104 between the thickness t102 of the resist film 161 which is only about 1 mm away from the polyimide protective film 121 and the thickness t101 and t103 near the polyimide protective film 121 is about 5 μm. When the distance w101 from the polyimide protective film 121 exceeds 1 mm, the thickness of the resist film 161 is maintained in a state where only the difference t104 between the thickness t101 near the polyimide protective film 121 and the thickness t102 of the portion away from the polyimide protective film 121 is thinned, and the surface becomes substantially flat.
[0170] Therefore, in order to set the thickness t102 of the resist film 161 to a thickness that enables the resist film 161 to function as a shielding film during helium irradiation as described later, i.e., to 42 μm, the thickness t101 of the resist film 161 near the polyimide protective film 121 must be set to 47 μm or more in the portion 1 mm away from the polyimide protective film 121 by a distance w101. Therefore, in order to form the resist film 161 thicker, it is necessary to change the resist material or increase the amount of resist used, etc., which leads to increased costs.
[0171] On the other hand, in the first embodiment, by disposing the dummy pattern of the polyimide film 22 for dummy pattern in the active region 41 under the condition of the above-mentioned distance w1 to w3, the high portion of the step (step on the front surface of the semiconductor substrate 10) generated on the front surface of the semiconductor substrate 10 due to the front element structure can be increased in the active region 41. Thus, in the plane of the semiconductor wafer 10', regardless of the distance from the polyimide protective film 21, the resist film 52 can be set to a substantially uniform thickness that can function as a shielding film.
[0172] The cross-sectional shape of the resist film 52 is, for example, a substantially rectangular shape ( Figure 4). In this case, the cross-sectional shape of the opening 52a of the resist film 52 is, for example, a substantially rectangular shape. The opening width x4 of the opening 52a of the resist film 52 is less than 1 mm. The overlapping region 33 of the IGBT region 31 and the FWD region 32 are exposed in the opening 52a of the resist film 52. In the helium irradiation described later, the impurity amount of the impurity defects 14 introduced into the overlapping region 33 of the IGBT region 31 and the FWD region 32 is equal.
[0173] In addition, if Figure 5 As shown, the cross-sectional shape of the resist film 52' may be a substantially trapezoidal shape in which the thickness becomes thinner in the portion covering the overlap region 33 than in the portion of the IGBT region 31 other than the overlap region 33. In this case, as long as the width w6 ( Figure 4 ) under the same conditions as those in the embodiment of the present invention, the width w16 of the upper surface (upper side) of the resist film 52' is set. Figure 5 ). For example, when the width w16 of the upper surface of the resist film 52' is about 10 μm, the width w16' of the lower surface (bottom side: contact surface with the front electrode 9) of the resist film 52' can be about 30 μm. More preferably, when the width w16 of the upper surface of the resist film 52' is about 10 μm, the width w16' of the lower surface of the resist film 52' can be less than 20 μm.
[0174] The cross-sectional shape of the opening 52a' of the resist film 52' is a substantially trapezoidal shape in which the opening width becomes wider as it moves away from the front surface of the semiconductor wafer 10'. The width x4' on the upper surface side of the opening 52a' of the resist film 52' is less than 1 mm. Only the FWD region 32 is exposed in the opening 52a' of the resist film 52'. As described above, since the thickness of the resist film 52' becomes thinner in the portion covering the overlapping region 33 of the IGBT region 31, in the helium irradiation described later, the impurity defects 14 are also introduced into the overlapping region 33 of the IGBT region 31 with less impurities than the FWD region 32.
[0175] By adjusting the viscosity of the resist material of the resist films 52 and 52', after forming the polyimide film 22 for dummy patterns and before forming the resist films 52 and 52', the entire front surface of the semiconductor wafer 10' is wetted with a solvent such as a diluent to perform a pre-wetting treatment that improves the wetting and diffusion of the resist, thereby improving the wetting and diffusion of the resist between the adjacent polyimide protection films 21 and the polyimide films 22 for dummy patterns, or between the adjacent polyimide films 22 for dummy patterns. The resist may also be applied in a manner that the resist films 52 and 52' are laminated in two layers.
[0176] Next, the semiconductor wafer 10' is irradiated with helium from the front side using the resist film 52 as a mask (blocking film), thereby - Helium impurity defects 14 that serve as lifetime inhibitors are introduced (formed) near the boundary between the n-type drift region 1 and the n-type carrier storage region 4 (fifth step). The range of helium irradiation is, for example, about 15 μm from the front surface of the semiconductor wafer 10'. In order to make the resist film 52 function as a shielding film during the helium irradiation, the thickness t1 and t2 of the resist film 52 must be greater than 42 μm, preferably greater than 45 μm.
[0177] By this helium irradiation, impurity defects 14 are introduced into the overlapping region 33 of the IGBT region 31 and the FWD region 32 exposed in the opening 52a of the resist film 52, and then - The low carrier lifetime region 34 is formed inside the drift region 1. The region other than the overlap region 33 of the IGBT region 31 is covered by the resist film 52 without introducing the impurity defects 14. It is also possible to use hydrogen ions (H + ) irradiation to introduce impurity defects 14 instead of using helium irradiation to introduce impurity defects 14.
[0178] Next, the resist film 52 is removed by ashing. When a dummy pattern is formed by a resist film instead of the dummy pattern polyimide film 22, the resist film forming the dummy pattern is also removed by ashing. The dummy pattern polyimide film 22 or the metal film forming the dummy pattern instead of the dummy pattern polyimide film 22 may be left without being removed.
[0179] Next, a back electrode 15 is formed on the entire back side of the semiconductor wafer 10'. After that, the semiconductor wafer 10' is cut (diced) along the dicing lines to be singulated into individual chips. The dicing lines are formed in the dicing areas 51 between the adjacent chip areas 50 of the semiconductor wafer 10' as described above. Each chip area 50 of the semiconductor wafer 10' is separated according to the dicing area 51 to form a semiconductor substrate 10, thereby completing the semiconductor device 40 of the first embodiment.
[0180] As described above, according to the first embodiment, by configuring a dummy pattern of a polyimide film for a dummy pattern in addition to a polyimide protective film on the front side of a semiconductor wafer, the pattern spacing of the polyimide film on the front side of the semiconductor wafer can be narrowed. Thus, the portion of the step height on the front side of the semiconductor wafer can be increased, and within the surface of the semiconductor wafer, regardless of the distance from the polyimide protective film, the resist film can be formed into a roughly uniform thickness that can act as a shielding film. The dummy pattern of the polyimide film for a dummy pattern is configured in an area where impurity defects are not introduced. Therefore, the resist film can be used as a shielding film and a predetermined impurity can be introduced into a predetermined area with high position accuracy. In addition, since the resist film can be formed with a roughly uniform thickness, there is no need to make the resist film too thick, which can prevent the cost from increasing.
[0181] (Implementation Method 2)
[0182] Next, a semiconductor device according to a second embodiment will be described. Figure 6 to Figure 9 1 is a top view showing an example of a state of the semiconductor device of the second embodiment as viewed from the front side of the semiconductor substrate. The layout of the dummy patterns of the polyimide films 61, 62, 71, 72 for the dummy patterns of the semiconductor devices 60, 60', 70, 70' of the second embodiment is similar to that of the semiconductor device 40 of the first embodiment (see FIG. Figure 1 The dummy pattern polyimide films 61, 62, 71, 72 are arranged in the region other than the overlapping region 33 of the IGBT region 31, and form a predetermined dummy pattern.
[0183] Specifically, Figure 6 The semiconductor device 60 of the second embodiment shown has a configuration in which dummy patterns of a substantially rectangular planar shape are separated from each other and dispersed by polyimide films 61 in the region other than the overlap region 33 of the IGBT region 31. The first polyimide film 61a is dispersed at predetermined intervals on a row of straight lines parallel to the second direction Y in the outermost IGBT region 31 in the first direction X. The second polyimide film 61b is dispersed at predetermined intervals on one or more rows of straight lines parallel to the second direction Y at a position further inside than the first polyimide film 61a.
[0184] The dummy pattern polyimide films 61 (61a, 61b) are adjacent to other dummy pattern polyimide films 61 in the first direction X. The distance w31 between the first polyimide film 61a and the polyimide protective film 21, the distance w32 between the dummy pattern polyimide film 61 and the overlapping region 33, and the distance w33 between adjacent dummy pattern polyimide films 61 are respectively the same as the distances w1 to w3 described above in the first embodiment (see Figure 1The distance w33′ between the adjacent dummy pattern polyimide films 61 in the direction inclined with respect to the second direction Y is, for example, less than 1 mm.
[0185] Figure 7 The semiconductor device 60' of the second embodiment shown in FIG. Figure 6 The semiconductor device 60 of the second embodiment shown is different in that the dummy pattern polyimide films 62 are dispersed so as to be adjacent to each other in the second direction Y. The dummy pattern polyimide films 62 that are closest to each other in the second direction Y are adjacent to each other in a direction inclined with respect to the second direction Y. The outermost IGBT region 31 in the first direction X may be adjacent to the outermost IGBT region 31 in the first direction X. Figure 6 The first polyimide film 61a is similarly provided with the first polyimide film 62a. Reference numeral 62b is a second polyimide film.
[0186] The distance w41 between the first polyimide film 62a and the polyimide protective film 21 is the same as the distance w1 described above in the first embodiment (see Figure 1 The distances w42 and w42' between the dummy pattern polyimide film 62 and the overlap region 33 are the same as the distance w2 described above in the first embodiment (see Figure 1 The distance w43 between adjacent dummy pattern polyimide films 62 is the same as the distance w3 described above in the first embodiment (see Figure 1 The distance w43′ between the dummy pattern polyimide films 62 adjacent to each other in the direction inclined relative to the second direction Y is, for example, less than 1 mm.
[0187] Figure 8 The semiconductor device 70 of the second embodiment shown in the figure adopts a configuration in which a plurality of dummy pattern polyimide films 71 are arranged parallel to each other in a linear manner extending in the first direction X in the region other than the overlap region 33 of the IGBT region 31. The distance w51 between the first polyimide film 71a and the polyimide protection film 21, the distance w52 between the dummy pattern polyimide film 71 and the overlap region 33, and the distance w53 between adjacent dummy pattern polyimide films 71 are respectively the same as the distances w1 to w3 described above in the first embodiment (see FIG. Figure 1 Reference numeral 71b is a second polyimide film.
[0188] Fig. 9 The semiconductor device 70' of the second embodiment shown in FIG. Figure 8The semiconductor device 70 of the second embodiment shown in the figure is different in that the dummy pattern polyimide film 72 having a substantially rectangular planar shape that is long in the first direction X is arranged in parallel with the first direction X. The distance w61 between the first polyimide film 72a and the polyimide protective film 21, the distance w62 between the dummy pattern polyimide film 72 and the overlapping region 33, and the distance w63 between adjacent dummy pattern polyimide films 72 are respectively the same as the distances w1 to w3 described above in the first embodiment (see FIG. Figure 1 Reference numeral 72b is a second polyimide film.
[0189] The method for manufacturing the semiconductor devices 60, 60', 70, 70' of the second embodiment only needs to be repeated in the method for manufacturing the semiconductor device 40 of the first embodiment (see Figure 3 to Figure 5 ) in the embodiment of the present invention, it is sufficient to change the layout of the dummy patterns of the polyimide films 61, 62, 71, 72 used for the dummy patterns.
[0190] As described above, according to the second embodiment, the polyimide film for dummy patterns is configured by setting the distance between the first polyimide film and the polyimide protective film, the distance between the polyimide film for dummy patterns and the overlapping area, and the distance between adjacent polyimide films for dummy patterns to the above conditions, so that even if the dummy pattern of the polyimide film for dummy patterns is changed, the same effect as in the first embodiment can be obtained.
[0191] (Implementation Method 3)
[0192] Next, a semiconductor device according to a third embodiment will be described. Fig.10 1 is a plan view showing an example of a state where the semiconductor device according to the third embodiment is viewed from the front side of the semiconductor substrate.
[0193] The layout of the IGBT region 31' and the FWD region 32' of the semiconductor device 40' of the third embodiment is similar to that of the semiconductor device 40 of the first embodiment (see Figure 1 Specifically, in the third embodiment, a plurality of FWD regions 32' (in the active region 41) having a substantially rectangular shape, for example, which is long in the second direction Y, are provided. Fig.10 The overlapping region 33' of the IGBT region 31' surrounds the FWD region 32' in a substantially rectangular shape.
[0194] In the region other than the overlap region 33' of the IGBT region 31', a dummy pattern of the polyimide film 22 for dummy pattern is arranged in the same manner as in the first embodiment. The short carrier lifetime region 34' is a substantially rectangular region formed by the overlap region 33' of the IGBT region 31' and the FWD region 32' and extending in the second direction Y. The periphery of the short carrier lifetime region 34' is surrounded by the non-introduced impurity defects 14 of the IGBT region 31' (see Figure 2 ) area.
[0195] The third embodiment may be applied to the semiconductor devices 60 , 60 ′, 70 , 70 ′ of the second embodiment to change the layout of the IGBT region 31 ′ and the FWD region 32 ′.
[0196] The method for manufacturing the semiconductor device 40 ′ of the third embodiment only requires changing the arrangement of the IGBT region 31 ′ and the FWD region 32 ′ and the arrangement of the region (the short carrier lifetime region 34 ′) where the impurity defects 14 are introduced in the semiconductor device of the first embodiment.
[0197] As described above, according to the third embodiment, even if the arrangement of the IGBT region and the FWD region is changed, the same effect as that of the first embodiment can be obtained by arranging the dummy pattern of the polyimide film for dummy pattern in the region other than the overlapping region of the IGBT region.
[0198] As mentioned above, the present invention is not limited to the above-mentioned embodiment, and various changes can be made without departing from the scope of the present invention.
[0199] Industrial Applicability
[0200] As described above, the semiconductor device and the method for manufacturing the semiconductor device of the present invention are useful for power semiconductor devices used in power conversion devices and / or power supply devices for various industrial machines and the like.
Claims
1. A method for manufacturing a semiconductor device, It is characterized in that include: In a first step, a predetermined device structure is formed on the front surface of the semiconductor substrate; The second step is to form a protective film on the front surface of the semiconductor substrate to protect the device structure; A third step is to form a predetermined pattern of a plurality of material films at the opening of the protective film on the front surface of the semiconductor substrate away from the protective film; In a fourth step, a resist film is formed on the front surface of the semiconductor substrate, covering the protection film and the material film and having an impurity defect introduction region; as well as In a fifth step, the impurity defects are introduced into the interior of the semiconductor substrate using the resist film as a mask. In the first step, as the element structure, an insulated gate bipolar transistor is formed in a first region of the active region of the semiconductor substrate, and a diode connected in reverse parallel to the insulated gate bipolar transistor is formed in a second region of the active region other than the first region, and a front electrode shared by the insulated gate bipolar transistor and the diode is formed on the front surface of the semiconductor substrate. In the third step, the plurality of material films include a plurality of first material films formed at a predetermined distance less than 1 mm from the protective film, and a plurality of second material films formed at a predetermined distance less than 1 mm from the first material films, adjacent first material films are arranged at intervals less than 1 mm, and adjacent second material films are arranged at intervals less than 1 mm, In the fourth step, the protective film and the first material film are completely and continuously covered with the resist film, and the distance from the first material film to the end of the resist film covering the first material film is set to be greater than 20 μm and less than 1 mm, In the fourth step, the second material film is completely covered with the resist film, and the distance from the second material film to the end of the resist film covering the second material film is set to be greater than 20 μm and less than 1 mm, In each of the first regions, the material film is formed on the front electrode exposed by the opening of the protective film. The protection film and the material film are polyimide films.
2. The method for manufacturing a semiconductor device according to claim 1, It is characterized in that In the third step, the material film is formed to have a height that is not less than half the height of the protective film and not more than the same height as the protective film.
3. The method for manufacturing a semiconductor device according to claim 1, It is characterized in that In the third step, the material film is formed to extend linearly in a direction parallel to the front surface of the semiconductor substrate.
4. The method for manufacturing a semiconductor device according to claim 1, It is characterized in that The third step is performed simultaneously with the second step.
5. The method for manufacturing a semiconductor device according to any one of claims 1 to 4, It is characterized in that In the second step, the protective film is formed so as to expose the active region in the opening. In the third step, a predetermined pattern of the material film is formed in the first region in the opening of the protective film. In the fifth step, the impurity defects are introduced into the entire second region using the resist film as a mask.
6. The method for manufacturing a semiconductor device according to claim 5, It is characterized in that In the fifth step, the impurity defects are introduced into the vicinity of the boundary between the first region and the second region using the resist film as a mask.
7. A semiconductor device, It is characterized in that have: A predetermined element structure is disposed on the front surface of the semiconductor substrate; an insulated gate bipolar transistor, which is disposed as the element structure in a first region of the active area of the semiconductor substrate; a diode, which is provided as the element structure in a second region of the active region other than the first region and is connected in reverse parallel to the insulated gate bipolar transistor; A protective film, which is disposed on the front surface of the semiconductor substrate, has an opening portion exposing the active area, and protects the element structure; A plurality of material films are arranged in a predetermined pattern in the opening of the protective film and away from the protective film in the first region; a short carrier lifetime region, which is disposed throughout the entire second region and shortens the carrier lifetime by introducing impurity defects; and a front electrode, which is disposed on the front surface of the semiconductor substrate and is shared by the insulated gate bipolar transistor and the diode, The plurality of material films include a plurality of first material films formed at a predetermined distance less than 1 mm from the protective film, and a plurality of second material films formed at a predetermined distance less than 1 mm from the first material films, adjacent first material films are arranged at intervals less than 1 mm, and adjacent second material films are arranged at intervals less than 1 mm, The material film is provided on the front electrode exposed by the opening of the protective film in each of the first regions, The protection film and the material film are polyimide films.
8. The semiconductor device according to claim 7, It is characterized in that The height of the material film is not less than half the height of the protective film and not more than the same height as the height of the protective film.
9. The semiconductor device according to claim 7, It is characterized in that The protection film is disposed on the front electrode.
10. The semiconductor device according to claim 9, It is characterized in that The semiconductor device includes an interlayer insulating film provided on the front surface of the semiconductor substrate and covering the gate electrode of the insulated gate bipolar transistor. The front electrode is provided on the surface of the interlayer insulating film and is in contact with the front surface of the semiconductor substrate via a contact hole of the interlayer insulating film.
Citation Information
Patent Citations
Semiconductor device manufacturing method
JP2017092256A
Semiconductor device manufacturing method
WO2018105299A1
Semiconductor device and production method
CN109314134A
Semiconductor device
JP2008112872A