Preparation method of carbon tetrahydride by inhibiting isomerization of n-butene

By using sulfonated copolymer resin catalyst and MTBE to inhibit the reaction in the carbon tetra-substant reaction, combined with low temperature conditions and uniform polymerization of methyl methacrylate, the problems of low isobutene conversion and high isomerization of n-butene are solved, and the problem of low-temperature conditions and high isomerization of n-butene is achieved. Efficient n-butene production.

CN113683476BActive Publication Date: 2024-11-12DAN DONG MING ZHU TE ZHONG SHU ZHI YOU XIAN GONG SI +1
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202110705640.2
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2021-06-24
Publication Date
2024-11-12
Estimated Expiration
2041-06-24

AI Technical Summary

Technical Problem

The existing technology is difficult to effectively catalyze the high conversion rate of isobutene and the low isomerization rate of n-butene, which leads to the problems of insufficient raw materials and poor economic benefits in the industrialized production of n-butene.

Method used

Using a method of carbon tetra-superposition that inhibits n-butene isomerization, a cation exchange resin catalyst sulfonated after extraction, drying and sieving of copolymer resin is used to perform a low-temperature reaction in a fixed bed reactor, and MTBE is used. Inhibit n-butene polymerization and uniform polymerization by methyl methacrylate to control the sulfonate distribution and reaction depth to avoid side reactions.

Benefits of technology

The isomerization rate of isomerene exceeds 99% and the isomerization rate of n-butene isomerization rate of 2-butene is less than 5%, ensuring the supply of raw materials and economic benefits of n-butene production.

✦ Generated by Eureka AI based on patent content.
Patent Text Reader

Abstract

The present patent application provides a method for preparing carbon tetrahydrofuran with inhibition of n-butene isomerization and a catalyst for its application. The method for preparing carbon tetrahydrofuran with inhibition of n-butene isomerization uses mixed carbon tetrahydrofuran as industrial raw material, and in a fixed bed reactor filled with a catalyst for its application, the reaction temperature is 40°C-50°C, the reaction pressure is 1.0-1.5Mpa, and the reaction temperature is 0.5-4.0h. ‑1 The reaction is carried out at a space velocity of 1.5 wt % and 2.5 wt % of the mixed carbon four. MTBE is added to the mixed carbon four in an amount of 0.5%-1% of the mass of the mixed carbon four. The superposition application catalyst is a cation exchange resin catalyst, which is prepared by suspension polymerization and sulfonation of styrene, methyl methacrylate, p-ethylstyrene and m-ethylstyrene. The technical scheme has the technical advantages of high isobutylene superposition conversion rate and low isomerization rate of n-butene to 2-butene.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present patent application relates to a polymer copolymer resin catalyst, a preparation method thereof and its catalytic synthesis application in the field of petrochemical industry, and in particular to a catalyst for the synthesis of mixed carbon four isobutylene and a preparation method thereof. Background Art

[0002] Ethanol and MTBE are both oxygen-containing gasoline cleaning additives. However, according to the "Implementation Plan on Expanding the Production of Biofuel Ethanol and Promoting the Use of Ethanol Gasoline for Vehicles" jointly issued by the National Development and Reform Commission and other 15 ministries and commissions, it is required that oxygen-containing compounds shall not be artificially added to ethanol gasoline, that is, etherified components such as MTBE and etherified light gasoline shall not be used as gasoline blending components. Therefore, industry insiders are deeply worried that after the nationwide promotion of ethanol gasoline, the etherification application market of MTBE and light gasoline will inevitably suffer a heavy blow, including the industrial preparation process of first etherifying isobutylene to synthesize MTBE and then using etherified C4 distillation separation to produce n-butene due to the close boiling points of isobutylene and n-butene. Therefore, it is urgent to find another process for the industrial production of n-butene using mixed C4 as industrial raw materials. The process should have a high isobutylene conversion rate and a low n-butene isomerization rate, so as to obtain sufficient raw material content for the subsequent production of n-butene and have reasonable economic benefits for the industrial production of n-butene. Summary of the invention

[0003] The invention purpose of this patent application is to use mixed C4 as industrial polymerization raw material, implement low isomerization rate of n-butene and high conversion rate of isobutene, so as to obtain sufficient raw materials for subsequent n-butene production, make n-butene production have industrial economic benefits, and provide a C4 polymerization preparation method that inhibits n-butene isomerization.

[0004] The present patent application provides a technical solution for the preparation of carbon four superpositions for inhibiting the isomerization of n-butene. The main technical content is: a preparation method for carbon four superpositions for inhibiting the isomerization of n-butene. The method uses mixed carbon four as industrial raw materials, and in a fixed bed reactor filled with a superposition application catalyst, the reaction temperature is 40°C-50°C, the reaction pressure is 1.0-1.5Mpa, and the reaction temperature is 0.5-4.0h -1The reaction is carried out at an air velocity of , wherein MTBE is added to the mixed carbon four, and the addition amount is 0.5%-1% of the mass of the mixed carbon four; the superimposed application catalyst is a cation exchange resin catalyst obtained by extracting, drying, screening, sulfonating and washing the copolymer resin, wherein the copolymer resin ball is formed by suspension copolymerization of the following polymerization monomers, including: 60-80 parts by weight of the main monomer styrene, 20-40 parts by weight of methyl methacrylate, 6-12 parts by weight of p-ethylstyrene, 4-8 parts by weight of m-ethylstyrene, and the cross-linking agent includes 10-15 parts by weight of p-divinylbenzene and 8-12 parts by weight of m-divinylbenzene, and is obtained by heating suspension polymerization in a copolymerization system in which the porogen is propylene glycol diacetate, the initiator is benzoyl peroxide and the dispersant is alum.

[0005] One of the preferred embodiments of the above overall technical solution is that in order to avoid low conversion rate due to too low content and side reactions due to high content, the isobutylene content in the mixed C4 is 3%-6% and the n-butene content is 10%-20%.

[0006] One of the preferred embodiments of the above overall technical solution is that the amount of the porogen is 20-30% of the total mass of the monomer phase.

[0007] One of the preferred top aspects of the overall technical solution is that the sulfonation is as follows: the copolymer resin balls are immersed in a sulfonating agent in a saturated solution of dichloroethane or dichloropropylene in sulfur trioxide, wherein the mass ratio of the copolymer resin balls to sulfur trioxide is 1:2-5, and the copolymer resin balls and the sulfonating agent are fully mixed by stirring for 0.5-2h, and then reacted at a temperature of 100°C-120°C for 8-20h, cooled, and washed with water until neutral.

[0008] One of the preferred embodiments of the above overall technical solution is that the water content of the composite catalyst is 50%±2%.

[0009] The present patent application discloses a technical solution for a C4 superposition preparation method for inhibiting the isomerization of n-butene. In the superposition preparation method, MTBE and mixed C4 industrial raw materials participate in the reaction to cause cracking, and the cracked methanol is used to cover the high active sites of the superposition catalyst to inhibit the polymerization of n-butene, inhibit the isomerization of n-butene to 2-butene, and inhibit the trimerization of isobutylene after dimerization. The superposition catalyst is made of mixed monomer copolymerization and sulfonation. In addition to conventional styrene, the polymerized monomer is also mixed with a corresponding weight portion of methyl methacrylate. One of the functions of the addition of methyl methacrylate is to make the polymerization more uniform, avoid the technical problem that there is still unpolymerized styrene after the cross-linking agent divinylbenzene is fully polymerized, and avoid the different polymerization rates of styrene and divinylbenzene, resulting in the subsequent polymerization mainly of styrene, which further causes the main sulfonation. To make the sulfonic acid group distribution and catalytic activity uneven on styrene, and cause the undesirable n-butene isomerization, this technical means makes the sulfonic acid group of the polymer resin evenly distributed, which is beneficial to avoid the formation of local hot spots in the isobutylene superposition, leading to the occurrence of side reactions; its other key role is that methyl methacrylate, as a component of the polymerization monomer, interacts with the porogen in the copolymerization, so that the ester groups are concentrated in the pores of the resin balls, and its steric hindrance is used to suppress the intensity of the isobutylene superposition reaction, and it is not easy to produce reaction hot spots. At the same time, the reaction depth is controlled, the selectivity is improved, the production of trimers is suppressed, and the production of high polymer products is avoided to block the catalyst pores, and the technical problem of catalyst deactivation is avoided; the above technical means are combined with low temperature reaction temperature, which is beneficial to control the progress of superposition synthesis and further suppress the isomerization of n-butene. The implementation of the patented technical solution of the present invention achieves the technical effect of isobutylene superposition conversion rate>99% and the isomerization rate of n-butene isomerization to 2-butene less than 5% in the preparation of superposition synthesis. DETAILED DESCRIPTION

[0010] Example 1

[0011] The first embodiment of the preparation method of C4 superposition for inhibiting n-butene isomerization is a fixed bed reactor. The fixed bed reactor with an inner diameter of 50 mm and a length of 1000 mm is filled with 400 ml of superposition application catalyst, and mixed C4 is used as an industrial raw material. The reaction is carried out at a temperature of 40°C, a pressure of 1.0 MPa, and a space velocity of 0.5 h-1. Among them, the n-butene content in the mixed C4 is 10%, and the isobutylene content is 3%. 0.6% of MTBE of the added mass of the mixed C4 is also added to the mixed C4, and mixed into the fixed bed reactor for reaction. The superposition application catalyst A used is obtained through the following preparation steps:

[0012] polymerization

[0013] 60 parts by weight of styrene, 20 parts by weight of methyl methacrylate, 6 parts by weight of p-ethylstyrene, 4 parts by weight of m-ethylstyrene, 10 parts by weight of p-divinylbenzene, 8 parts by weight of m-divinylbenzene, porogen propylene glycol diacetate, and 0.4 parts by weight of initiator benzoyl peroxide were weighed and placed in a mixing tank, stirred for 0.5 hours to make the feed liquid evenly mixed to form the oil phase; wherein, the porogen accounts for 20% of the weight of the oil phase. 300 parts by weight of water and 1.0 parts by weight of alum as a dispersant were added to the polymerization kettle, stirred and heated to 40°C, and added to the mixed monomers after they were completely dissolved. The stirring speed was adjusted to 90 rpm according to the dispersion of the monomers, and the temperature was slowly raised to 80°C. After the polymerization reaction lasted for 8 hours, the mixture was cooled and discharged, and the polymer was washed three times with hot water and cold water respectively to separate the copolymer resin balls;

[0014] Extraction, drying and sieving

[0015] Add copolymer resin balls into the extraction kettle, add excess solvent into the distillation kettle and heat it to evaporate the solvent in the kettle and flow into the extraction kettle after condensation. The solvent partially dissolves the porogen in the kettle and the formed mixed solution remains in the extraction kettle. When the liquid level reaches a certain height, it is put into the distillation kettle and heated and evaporated again. This is repeated 6 times and the porogen remaining on the copolymer resin balls is extracted cleanly. Place the extracted copolymer resin balls in a ventilated place and dry them to a water content of 5%. Sieve the copolymer resin balls with a particle size of 0.3~0.9mm as the sulfonated matrix.

[0016] Sulfonation

[0017] The extracted copolymer resin balls were immersed in a saturated sulfur trioxide solution sulfonating agent, wherein the mass ratio of the copolymer resin balls to sulfur trioxide was 1:2, and stirred for 0.5 hours to fully mix the white balls and the sulfonating agent, and then the temperature was controlled to be 100°C for reaction for 8 hours, and the reaction was terminated, cooled, and placed in a water washing column to be rinsed to neutrality, and the resin with a water content of 50%±2% was separated, which was used as a catalyst for the superposition synthesis application of the carbon four superposition preparation method for inhibiting the isomerization of n-butene. The superposition reaction results: the isomerization rate of n-butene to 2-butene was only 3.2%, and the isobutylene superposition conversion rate was as high as 99.1%.

[0018] Example 2

[0019] The first embodiment of the preparation method of carbon four superposition for inhibiting n-butene isomerization is a fixed bed reactor. The fixed bed reactor with an inner diameter of 50 mm and a length of 1000 mm is filled with 400 ml of superposition catalyst. The mixed carbon four is used as the industrial raw material. The temperature is 50°C, the pressure is 1.5 MPa, and the space velocity is 4.0 h. -1The reaction was run. The n-butene content in the mixed C4 was 20%, the isobutylene content was 6%, and 1.0% of the mass of MTBE added to the mixed C4 was added simultaneously to the mixed C4, and the mixture was mixed into a fixed bed reactor for reaction. The composite application catalyst B used was obtained through the following preparation steps:

[0020] polymerization

[0021] 80 parts by weight of styrene, 40 parts by weight of methyl methacrylate, 12 parts by weight of p-ethylstyrene, 8 parts by weight of m-ethylstyrene, 15 parts by weight of p-divinylbenzene, 12 parts by weight of m-divinylbenzene, porogen propylene glycol diacetate, and 1.0 part by weight of initiator benzoyl peroxide were weighed and placed in a mixing tank, stirred for 0.5 hours to make the feed liquid evenly mixed to form the oil phase; wherein, the porogen accounts for 30% of the weight of the oil phase. 400 parts by weight of water and 2.0 parts by weight of alum as a dispersant were added to the polymerization kettle, stirred and heated to 50°C, and added to the mixed monomers after they were completely dissolved, and the stirring speed was adjusted to 100 rpm according to the dispersion of the monomers, and the temperature was slowly raised to 80°C. After the polymerization reaction lasted for 18 hours, the material was cooled and discharged, and the polymer was washed three times with hot water and cold water respectively to separate the copolymer resin balls;

[0022] Extraction, drying and sieving

[0023] Add copolymer resin balls into the extraction kettle, add excess solvent into the distillation kettle and heat it to evaporate the solvent in the kettle, and then flow into the extraction kettle after condensation. The solvent partially dissolves the porogen in the kettle, and the formed mixed solution remains in the extraction kettle. When the liquid level reaches a certain height, it is put into the distillation kettle and heated and evaporated again. This is repeated 20 times, and the porogen remaining on the copolymer resin balls is extracted cleanly; the extracted copolymer resin balls are placed in a ventilated place, dried to a water content of 10%, and the copolymer resin balls with a particle size of 0.3~0.9mm are sieved as sulfonated matrix.

[0024] Sulfonation

[0025] The extracted copolymer resin balls were immersed in a saturated sulfur trioxide solution sulfonating agent, wherein the mass ratio of the copolymer resin balls to sulfur trioxide was 1:5, and stirred for 2.0 hours to fully mix the white balls and the sulfonating agent, and then the temperature was controlled to be 120°C for reaction for 20 hours, the reaction was terminated, cooled, placed in a water washing column and rinsed to neutrality, and the resin with a water content of 50%±2% was separated, which was used as the catalyst for the superposition synthesis application of the carbon four superposition preparation method for inhibiting the isomerization of n-butene. The superposition reaction results: the isomerization rate of n-butene to 2-butene was only 4.7%, and the isobutylene superposition conversion rate was as high as 99.3%.

[0026] Example 3

[0027] The first embodiment of the method for preparing C4 superposition with inhibition of n-butene isomerization is a fixed bed reactor. The fixed bed reactor with an inner diameter of 50 mm and a length of 1000 mm is filled with 400 ml of superposition catalyst. The mixed C4 is used as the industrial raw material. The reactor is heated at a temperature of 45°C, a pressure of 1.2 MPa, and a space velocity of 2.0 h. -1 The reaction is run. The n-butene content in the mixed C4 is 15%, the isobutene content is 5%, and 0.8% of the mass of MTBE added to the mixed C4 is added simultaneously to the mixed C4, and the mixture is mixed into a fixed bed reactor for reaction. The composite application catalyst C used is obtained through the following preparation steps:

[0028] polymerization

[0029] 70 parts by weight of styrene, 30 parts by weight of methyl methacrylate, 8 parts by weight of p-ethylstyrene, 6 parts by weight of m-ethylstyrene, 12 parts by weight of p-divinylbenzene, 10 parts by weight of m-divinylbenzene, porogen propylene glycol diacetate, and 0.6 parts by weight of initiator benzoyl peroxide were weighed and placed in a mixing tank, stirred for 0.5 hours to make the feed liquid evenly mixed to form the oil phase; wherein, the porogen accounts for 25% of the weight of the oil phase. 350 parts by weight of water and 1.5 parts by weight of alum as a dispersant were added to the polymerization kettle, stirred and heated to 45°C, and added to the mixed monomers after they were completely dissolved. The stirring speed was adjusted to 95 rpm according to the dispersion of the monomers, and the temperature was slowly raised to 80°C. After the polymerization reaction lasted for 12 hours, the material was cooled and discharged, and the polymer was washed three times with hot water and cold water respectively to separate the copolymer resin balls;

[0030] Extraction, drying and sieving

[0031] Add copolymer resin balls into the extraction kettle, add excess solvent into the distillation kettle and heat it to evaporate the solvent in the kettle and flow into the extraction kettle after condensation. The solvent partially dissolves the porogen in the kettle and the formed mixed solution remains in the extraction kettle. When the liquid level reaches a certain height, it is put into the distillation kettle and heated and evaporated again. This is repeated 15 times and the porogen remaining on the copolymer resin balls is extracted cleanly. Place the extracted copolymer resin balls in a ventilated place and dry them to a water content of 8%. Sieve the copolymer resin balls with a particle size of 0.3~0.9mm as the sulfonated matrix.

[0032] Sulfonation

[0033] The extracted copolymer resin balls were immersed in a saturated sulfur trioxide solution sulfonating agent, wherein the mass ratio of the copolymer resin balls to sulfur trioxide was 1:3, and stirred for 1.0h to fully mix the copolymer resin balls and the sulfonating agent, and then the temperature was controlled to be 110°C for reaction for 15h, the reaction was terminated, cooled, placed in a water washing column and rinsed to neutrality, and the resin with a water content of 50%±2% was separated, which was used as the catalyst for the superposition synthesis application of the carbon four superposition preparation method for inhibiting the isomerization of n-butene. The superposition reaction results: the isomerization rate of n-butene to 2-butene was only 3.9%, and the isobutylene superposition conversion rate was as high as 99.2%.

Claims

1. A method for preparing C4 by superposition with suppressed n-butene isomerization, wherein the method uses mixed C4 as industrial raw material, and operates the reaction in a fixed bed reactor filled with a superposition catalyst at a reaction temperature of 40°C-50°C, a reaction pressure of 1.0-1.5 MPa, and a space velocity of 0.5-4.0 h-1, characterized in that: The isobutylene content of the mixed C4 is 3%-6%, and the n-butene content is 10%-20%. MTBE is added to the mixed C4 in an amount of 0.5%-1% of the mass of the mixed C4. The superimposed application catalyst is a cation exchange resin catalyst obtained by extracting, drying, screening, sulfonating and washing copolymer resin balls. The copolymer resin balls are formed by suspension copolymerization of the following monomers, including: 60-80 parts by weight of main monomer styrene, 20-40 parts by weight of methyl methacrylate, 6-12 parts by weight of p-ethylstyrene, 4-8 parts by weight of m-ethylstyrene, and the cross-linking agent includes 10-15 parts by weight of p-divinylbenzene and 8-12 parts by weight of m-divinylbenzene, and are obtained by heating suspension polymerization in a copolymerization system in which the porogen is propylene glycol diacetate, the initiator is benzoyl peroxide and the dispersant is alum. The porogen is used in an amount of 20-30% of the total mass of the monomer phase.

2. The method for preparing C4 superposition by suppressing isomerization of n-butene according to claim 1, characterized in that: The water content of the composite catalyst is 50%±2%.

3. The method for preparing C4 superposition by suppressing isomerization of n-butene according to claim 1, characterized in that: The amount of MTBE added is 0.6%-0.8% of the mass of the mixed C4.

4. The method for preparing C4-polymerization by suppressing isomerization of n-butene according to claim 1, 2 or 3, characterized in that: The sulfonation method is as follows: the copolymer resin balls are immersed in a sulfonating agent of a saturated solution of ethylene dichloride or propylene dichloride in sulfur trioxide, wherein the mass ratio of the copolymer resin balls to sulfur trioxide is 1:2-5, and the copolymer resin balls and the sulfonating agent are fully mixed by stirring for 0.5-2 hours, and then reacted at a temperature of 100°C-120°C for 8-20 hours, cooled, and washed with water until neutral.