A kind of assembled building roof structure and construction method thereof
Through the prefabricated building roof structure, hot-dip galvanized steel pipe frames, copper plates and stainless steel materials are used to realize the rapid connection and stability improvement of Baoding, ridge and other components, solving the problems of long construction period and insufficient stability of the existing roof structure. , suitable for the rapid construction needs of modern projects and reducing maintenance costs.
Patent Information
- Application Number
- CN202111010302.3
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2021-08-31
- Publication Date
- 2024-09-24
- Estimated Expiration
- 2041-08-31
Smart Images

Figure CN113684959B
Abstract
Description
Technical Field
[0001] The present invention relates to the field of building roof construction, and in particular to an assembled building roof structure and a construction method thereof. Background Art
[0002] my country's building roof construction technology has a long history of thousands of years, and the styles of different dynasties are very different, and the standards in different periods are different. The same thing is that the roofs are mostly made of clay fired ridge decorations, tiles, and main wooden structures. After a long time, they are often deformed and broken. The traditional clay firing of tiles takes a long time, generally two to three months as a cycle, and goes through processes such as raw material excavation and mining, raw material preparation and screening, molding and molding, adobe mold drying, calcination, and quality control. It is not suitable for tight construction schedules. Compared with the firing and molding of traditional clay tiles, the processing and production of metal roof components only takes about 1 month. From this point alone, for most of the current projects that are rushing to meet deadlines and rushing to meet node deadlines, there will be more options for similar construction schedules;
[0003] In addition, some existing buildings have roofs, naves, tiles and other components built on the top to improve the aesthetic performance of the building. However, the connection of these components in the current building structure is not tight, and the stability of the overall structure will be affected by wind and sun over the years. Therefore, there is an urgent need for an assembled building roof structure with a short construction period and strong stability and a construction method thereof. Summary of the invention
[0004] The present invention aims to provide an assembled building roof structure and a construction method thereof, which is convenient for assembly and disassembly through the assembled structural connection of various components, and at the same time, the connection stability of various components is good, and the construction is convenient, which can shorten the construction period.
[0005] The embodiment of the present invention is achieved as follows:
[0006] An assembled building roof structure includes a roof and a ridge. The number of the ridges is multiple and they are arranged around the roof. The end of the ridge away from the roof is provided with a ridge. The roof includes an internal support assembly and an external copper plate. The external copper plate is welded to the periphery of the support assembly. The support assembly includes a main support rod and a first hot-dip galvanized steel pipe frame arranged around the main support rod. The first hot-dip galvanized steel pipe frame is also provided with a modeling skeleton. The periphery of the modeling skeleton is used for welding the external copper plate. The main support rod is vertically fixed on the roof. The side of the main support rod close to the roof is provided with a plurality of steel plate connectors. The steel plate connectors are used to fix with the ridge. The assembled structure of each component is connected, which is convenient for disassembly and assembly. At the same time, the connection stability of each component is good, and the construction is convenient, which can shorten the construction period.
[0007] Preferably, the external copper plate is attached to the periphery of the modeling frame, and encloses and forms the lower part of the top, the lotus seat of the top, the middle part of the top and the upper part of the top from bottom to top, and the main ridge is fixed at the lower part of the top.
[0008] Preferably, the number of the main ridges is 4, and the array is distributed around the main support rod. The main ridge includes a second hot-dip galvanized steel pipe frame and an inner lining aluminum honeycomb panel arranged on both sides of the second hot-dip galvanized steel pipe frame, and a plurality of mutually parallel bending strips are also arranged on the outer side of the inner lining aluminum honeycomb panel.
[0009] Preferably, vertical ridges are arranged on both sides of the front ridges, and the two vertical ridges between two adjacent front ridges are connected to each other and fixed on the keels. The roof is provided with two types of keels, longitudinal and transverse and diagonal, and the keels are conductively connected to the lightning strips on the roof.
[0010] Preferably, the roof is provided with bottom tiles and cover tiles, the bottom tiles are fixed on the keel of the roof, the cover tiles are evenly laid on the roof and cover the bottom tiles, and the vertical ridge and the main ridge are both arranged on the surface of the cover tiles.
[0011] Preferably, the first hot-dip galvanized steel pipe rack includes a plurality of transverse steel pipes and a plurality of vertical steel pipes, which are spliced into a plurality of rectangular frame structures, and the length and width of the rectangular frames decrease in a step-like manner from bottom to top.
[0012] A method for constructing a prefabricated building roof structure is also provided. The method comprises the following steps:
[0013] S1: Prefabricate the lower part of the pagoda, the lotus seat of the pagoda, the middle part of the pagoda and the upper part of the pagoda respectively;
[0014] S2: Install two types of keels, vertical and horizontal, and diagonal, on the roof, and the two types of keels meet at the center of the roof;
[0015] S3: Weld the prefabricated roof at the intersection of the two keels;
[0016] S4: Weld and install multiple ridges around the top of the building;
[0017] S5: Install the ridge on the side of the ridge away from the top of the building;
[0018] S6: Install the vertical ridges on both sides of the front ridge, and reserve the installation positions for the bottom tiles and cover tiles at the bottom;
[0019] S7: Lay bottom tiles and cover tiles on the roof in sequence;
[0020] S8: Install the remaining fixings and trims.
[0021] Preferably, in step S1, the following steps are also included:
[0022] S11: Make the first hot-dip galvanized steel pipe frame and modeling framework. When welding, at least three sides should be fully welded without false welds or leaking welds. After welding, apply three layers of anti-rust paint;
[0023] S12: Make a 1:1 clay mold according to the lotus seat on the top of the treasure, and manually forge the single lotus according to the model to form it, and then weld and assemble it. The other flat parts are formed by laser cutting and mechanical shearing and folding. The spherical part and the decoration on the spherical surface are manually forged according to the lofting size, and the decoration on the spherical surface is spot welded on the spherical shape. The spherical shape and the flat part are fully welded and polished.
[0024] S13: Weld the external copper plate to the modeling frame. The welding is required to be fully welded and welded inside and outside. Weld the single-piece lotus petal assembly to the stainless steel frame. The welding is required to be fully welded inside and outside without voids.
[0025] S14: Conduct preliminary inspection on the shape, size, internal steel frame welding, rust prevention, external decorative copper plate welding and flatness of each roof component; polish, repair weld and trim the products that pass the preliminary inspection;
[0026] S15: The surface of each component is subjected to mechanical and manual roughening treatment, spot removal, deflocculation, pickling and neutralization, and water washing, and then the water is flushed away with a high-pressure air pump;
[0027] S16: The outer copper plate surface of each component of the top is repeatedly washed with chemicals to make it black. After the copper surface is completely black, it is manually drawn. The wire drawing and washing are repeated along a fixed drawing direction. After the specified effect is achieved, the water is flushed away with a high-pressure air pump;
[0028] S17: Spray matte fluorocarbon paint on each component of the roof as a protective layer. No paint flow or leakage is required during painting.
[0029] S18: Send the components of the top of the treasure to a high-temperature oven for drying. The maximum temperature during baking is 160° C. and the time is 30 minutes.
[0030] Preferably, before step S5, the method further includes forging the front nose, and performing surface treatment and anti-oxidation treatment on the front nose; specifically, the following steps are included:
[0031] S51: Make a mud mold model according to the orthogonal drawing, and after confirmation, split and make the fiberglass reinforced plastic model;
[0032] S52: trim the block model, turn the zinc mold, polish the zinc mold, and trim the pattern;
[0033] S53: copper plate cutting and annealing, thermal oxidation, softening and cooling;
[0034] S54: The zinc mold is put on the machine and the annealed copper plate is used for stamping;
[0035] S55: After stamping, secondary annealing is performed, followed by glue filling and manual secondary forging;
[0036] S56: After forging, each component is welded and assembled by argon arc welding, the weld is polished and the whole is polished;
[0037] S57: The treated copper is sent to the antique copper workshop, where the copper surface is repeatedly washed with chemicals to make it black. After the copper surface is completely black, it is manually drawn. It is repeatedly drawn and washed along a fixed drawing direction. When the specified effect is achieved, the water is flushed away with a high-pressure air pump.
[0038] S58: Send the finished front kiss to the dust-free spray paint room and spray the matte fluorocarbon anti-oxidation protective paint. The spraying should be uniform without paint flow and leakage. Check the color difference and surface paint condition one by one.
[0039] S59: The qualified products are sent to a high temperature oven for drying. The maximum temperature is 160℃ and the baking time is 30 minutes.
[0040] Preferably, before step S7, the process further includes making a bottom tile, where the bottom tile is made of 304 stainless steel material and is integrally seamlessly stamped; specifically, the following steps are included:
[0041] S71: Making stamping steel mold;
[0042] S72: Conduct a mold test to check the size, flatness, and stretching of the stamped product, and fine-tune the mold according to the inspection results until it meets the product requirements; fix the mold that has been fine-tuned multiple times, and make a product stamping support frame;
[0043] S73: Punch, and pay attention to prevent the product from shifting during punching. Dust and adhesives should be removed from the mold and the board surface after each punching to ensure the flatness of the product surface. One bottom tile is randomly inspected for every 20 molded bottom tiles;
[0044] S74: Fold the stamped bottom tile to form an upward side-turned water retaining edge. According to the different sacs of each layer of the roof, make a rolling machine, and use the rolling machine to roll the bottom tile to the required arc on the drawing; cut the material according to the size of the drawing and affix the "layer position number" to each bottom tile. The bottom tile at the wing corner needs to be cut at an angle; fully weld the dripping water at the end of the bottom tile, and open a flat opening at the side-turned water retaining edge at the front end of the bottom tile, reserved for installing the hook tile;
[0045] S75: Finely grind the drip welding part, and check the size, cysticity and drip welding strength of the bottom tile. One bottom tile is randomly inspected for every 50 formed bottom tiles;
[0046] S76: polishing the bottom tile surface, removing spots, spraying fine sand on the surface to remove floating and sinking, pickling and neutralization, and washing with clean water;
[0047] S77: After cleaning and drying the bottom tile, spray epoxy primer, dry at room temperature, and spray the confirmation paint after drying;
[0048] S78: Send the finished base tiles to the dust-free spray paint room and spray matte fluorocarbon anti-oxidation protective paint. The spraying should be uniform without paint flow or leakage, and the color difference and surface paint condition should be checked one by one;
[0049] S79: The bottom tiles that have passed the inspection are sent to a high-temperature oven for drying. The maximum temperature during baking is 160°C and the time is about 30 minutes.
[0050] Due to the adoption of the above technical scheme, the beneficial effects of the present invention include: the prefabricated building roof structure of the present invention and its construction method include a roof and a ridge, the number of the ridges is multiple and they are arranged around the roof, and a ridge is arranged at one end of the ridge away from the roof; the roof includes an internal support assembly and an external copper plate, the external copper plate is welded to the periphery of the support assembly, the support assembly includes a main support rod and a first hot-dip galvanized steel pipe frame arranged around the main support rod, the first hot-dip galvanized steel pipe frame is also provided with a modeling skeleton, and the periphery of the modeling skeleton is used for welding the external copper plate; the main support rod is vertically fixed on the roof, and a plurality of steel plate connectors are provided on the side of the main support rod close to the roof, and the steel plate connectors are used to fix with the ridge. Through the prefabricated structural connection of each component, it is convenient to disassemble and assemble, and at the same time, the connection stability of each component is good, and the construction is convenient, which can improve the construction period. BRIEF DESCRIPTION OF THE DRAWINGS
[0051] In order to more clearly illustrate the technical solutions of the embodiments of the present invention, the drawings in the embodiments will be briefly introduced below. It should be understood that the following drawings only show certain embodiments of the present invention and therefore should not be regarded as limiting the scope. For ordinary technicians in this field, other related drawings can be obtained based on these drawings without creative work.
[0052] Figure 1 It is a schematic diagram of the roof structure of the present invention;
[0053] Figure 2 It is a schematic diagram of the structure of the top, the front ridge and the back ridge of the present invention;
[0054] Figure 3 It is a schematic diagram of the cross-sectional structure of the main spine of the present invention.
[0055] Specific element symbol description: 1-top, 2-main ridge, 3-main ridge, 11-main support rod, 12-first hot-dip galvanized steel pipe frame, 13-external copper plate, 14-modeling frame, 15-upper part of the top, 16-middle part of the top, 17-lotus seat of the top, 18-lower part of the top, 19-steel plate connector, 21-second hot-dip galvanized steel pipe frame, 22-lined aluminum honeycomb panel, 23-bending strip. DETAILED DESCRIPTION
[0056] In order to make the purpose, technical solutions and advantages of the embodiments of the present invention clearer, the technical solutions in the embodiments of the present invention will be clearly and completely described below in conjunction with the drawings in the embodiments of the present invention. Obviously, the described embodiments are part of the embodiments of the present invention, not all of the embodiments. The components of the embodiments of the present invention generally described and shown in the drawings here can be arranged and designed in various different configurations. The following detailed description of the embodiments of the present invention provided in the drawings is not intended to limit the scope of the claimed invention, but merely represents selected embodiments of the present invention. Based on the embodiments in the present invention, all other embodiments obtained by ordinary technicians in this field without making creative work are within the scope of protection of the present invention.
[0057] Example 1: Please refer to Figures 1 to 3 The present embodiment is an assembled building roof structure, comprising a roof 1 and a ridge 2, wherein the number of ridges 2 is multiple and arranged around the roof 1, and a ridge 3 is arranged at one end of the ridge 2 away from the roof 1; the roof 1 comprises an internal support assembly and an external copper plate 13, the external copper plate 13 is welded to the periphery of the support assembly, the support assembly comprises a main support rod 11 and a first hot-dip galvanized steel pipe frame 12 arranged around the main support rod 11, and a modeling skeleton 14 is also arranged outside the first hot-dip galvanized steel pipe frame 12, and the periphery of the modeling skeleton 14 is used for welding the external copper plate 13; the main support rod 11 is vertically fixed on the roof, and a plurality of steel plate connectors 19 are arranged on the side of the main support rod 11 close to the roof, and the steel plate connectors 19 are used to be fixed to the ridge 2. The assembled structure of each component is connected, which is convenient for disassembly and assembly, and the connection stability of each component is good, and the construction is convenient, which can improve the construction period.
[0058] Embodiment 2: The external copper plate 13 of this embodiment is attached to the periphery of the modeling skeleton 14, and encloses the lower part of the top 1, the lotus seat of the top 1, the middle part of the top 1 and the upper part of the top 1 from bottom to top, and the main ridge 2 is fixed at the lower part of the top 1. The number of the main ridges 2 of this embodiment is 4, and the array is distributed around the main support rod 11. The main ridge 2 includes a second hot-dip galvanized steel pipe frame 21 and an inner lining aluminum honeycomb panel 22 arranged on both sides of the second hot-dip galvanized steel pipe frame 21. The outer side of the inner lining aluminum honeycomb panel 22 is also provided with a plurality of mutually parallel bending strips 23. Both sides of the front kiss 3 of this embodiment are inclined downwardly provided with vertical ridges, and the two vertical ridges between two adjacent front kisses 3 are interconnected and fixed on the keel. The roof is provided with two types of keels, longitudinal and transverse and diagonal, and the keels are conductively connected to the lightning strips of the roof. The roof of this embodiment is provided with bottom tiles and cover tiles, the bottom tiles are fixed on the keel of the roof, the cover tiles are evenly laid on the roof and cover the bottom tiles, and the vertical ridge and the main ridge 2 are both arranged on the surface of the cover tiles. The first hot-dip galvanized steel pipe frame 12 of this embodiment includes a plurality of transverse steel pipes and a plurality of vertical steel pipes, which are spliced into a plurality of rectangular frame structures, and the length and width of the rectangular frame decrease in a step-like manner from bottom to top.
[0059] Embodiment 3: This embodiment also provides a method for constructing a prefabricated building roof structure, and the construction of the above-mentioned prefabricated building roof structure includes the following steps: S1: prefabricating the lower part of the top 1, the lotus seat of the top 1, the middle part of the top 1 and the upper part of the top 1 respectively; S2: installing two kinds of longitudinal and transverse and diagonal keels on the roof, and the two kinds of keels intersect at the center point of the roof; S3: welding the prefabricated top 1 at the intersection of the two kinds of keels; S4: welding and installing multiple main ridges 2 around the top 1; S5: installing the main ridge 3 on the side of the main ridge 2 away from the top 1; S6: installing the vertical ridges on both sides of the main ridge 3, and reserving the installation position of the bottom tile and the cover tile at the bottom; S7: laying the bottom tile and the cover tile on the roof in sequence; S8: installing the remaining fixings and decorative parts.
[0060] Embodiment 4: In step S1 of this embodiment, the following steps are also included: S11: make a first hot-dip galvanized steel pipe frame 12 and a modeling skeleton 14, and at least three sides are fully welded during welding, without false welding or leaking welding, and three layers of anti-rust paint are applied after welding; S12: make a 1:1 mud mold according to the lotus seat of the top 1, manually forge a single lotus according to the model and then weld and assemble it, and other flat parts are formed by laser cutting and mechanical processing of shearing and folding; the spherical part and the decoration on the spherical surface are manually forged according to the lofting size, the decoration on the spherical surface is spot welded on the spherical shape, and the spherical shape is fully welded and connected with the plane part and polished; S13: weld the external copper plate 13 to the modeling skeleton 14, and full welding is required during welding, and both inside and outside are welded; weld the single-piece formed lotus petals to the stainless steel skeleton, and internal and external welding and full welding without false welding are required during welding; S14: Carry out preliminary inspection on the shape, size, internal steel frame welding, rust prevention, welding and flatness of external decorative copper plates of each component of the top 1; polish, repair weld and trim the products that pass the preliminary inspection; S15: perform mechanical and manual roughening, spot removal, de-floating, pickling and neutralization, and clean water washing on the surface of each component as a whole, and then flush the water with a high-pressure air pump; S16: Repeatedly rinse the surface of the external copper plate 13 of each component of the top 1 with chemicals to blacken it. After the copper surface is completely blackened, manually draw it, repeatedly draw and rinse it along the fixed drawing direction, and flush it repeatedly. After achieving the specified effect, flush the water with a high-pressure air pump; S17: Spray matte fluorocarbon paint on each component of the top 1 as a protective layer. There must be no paint flow and spray leakage during painting; S18: Send each component of the top 1 to a high-temperature oven for drying. The maximum temperature during baking is 160℃ and the time is 30min.
[0061] Embodiment 5: Before step S5, the present embodiment also includes forging and shaping the front kiss 3, and performing surface treatment and anti-oxidation treatment on the front kiss 3; specifically includes the following steps: S51: making a mud mold model according to the front kiss 3 drawing, and dividing and making the glass fiber reinforced plastic model after confirmation; S52: trimming the block model, turning the zinc mold, grinding the zinc mold, and trimming the pattern; S53: unloading the copper plate and annealing it, thermally oxidizing the copper plate, softening it, and cooling it; S54: putting the zinc mold on the machine, and stamping it with the annealed copper plate; S55: performing secondary annealing after stamping, and then filling with glue and manually forging it for the second time; S56: after forging is completed, each component Argon arc welding is used for combined forming, the welds are ground flat, and the whole is polished; S57: The processed front kiss 3 is sent to the bronze workshop, and the surface of the front kiss 3 is repeatedly washed with medicine to turn black. After the copper surface is completely black, it is manually drawn, and the wire drawing and washing are repeated along the fixed drawing direction. After achieving the specified effect, the water is flushed with a high-pressure air pump; S58: The completed front kiss 3 is sent to the dust-free paint spraying room, and matt fluorocarbon anti-oxidation protective paint is sprayed. The spraying is required to be uniform without paint flow and leakage, and the color difference and surface paint condition are checked one by one; S59: The qualified front kiss 3 is sent to the high-temperature oven for drying. The maximum temperature during baking is 160℃, and the time is 30min.
[0062] Embodiment 6: Before step S7, the present embodiment also includes making bottom tiles, which are made of 304 stainless steel material and are seamlessly stamped and formed as a whole; specifically, the following steps are included: S71: making a stamping steel mold; S72: performing a mold test to check the size, flatness, and stretching of the stamped and formed product, and fine-tuning the mold according to the inspection results until it meets the product requirements; fixing the mold that has been fine-tuned for multiple times to make a product stamping support frame; S73: performing stamping, and paying attention to preventing the product from shifting during stamping. After each stamping, the mold and the board surface must be dusted and treated to remove adhesives to ensure the flatness of the product surface, and one bottom tile is randomly inspected for every 20 formed bottom tiles; S74: folding the stamped bottom tile to form an upward side-turning water retaining edge, and making a rolling machine according to the different sacs of each roof layer, and using the rolling machine to roll the bottom tile out of the arc required on the drawing; cutting and blanking according to the size of the drawing and folding each The strip bottom tile is labeled with the "layer position number", and the bottom tile at the wing corner needs to be cut at an angle; the end of the bottom tile is fully welded with a drip, and a flat opening is opened at the water retaining edge at the front end of the bottom tile, reserved for the installation of hook tiles; S75: The drip welding position is finely polished, and the size, sac shape and drip welding strength of the bottom tile are checked. One bottom tile is randomly inspected for every 50 formed bottom tiles; S76: The surface of the bottom tile is polished, the spots are removed, the surface is sprayed with fine sand to remove floating and sinking, pickled and neutralized, and rinsed with clean water; S77: After the bottom tile is cleaned and dried, it is sprayed with epoxy primer, dried at room temperature, and then sprayed with confirmation paint after drying; S78: The completed bottom tile is sent to the dust-free spray paint room and sprayed with matte fluorocarbon anti-oxidation protective paint. The spraying is required to be uniform without paint flow and missing spraying, and the color difference and surface paint condition are checked one by one; S79: The bottom tile that passes the inspection is sent to a high-temperature oven for drying. The maximum temperature during baking is 160℃, and the time is about 30 minutes.
[0063] Embodiment 7: It also includes the production of cover tiles, and the production steps are as follows: (1) Strictly produce stamping steel molds, corner cutting molds, and tail shoulder stamping molds according to the dimensions of the drawings. (2) Calculate the blanking dimensions of the cover tiles according to the drawings and mold dimensions, and test the corner cutting, stamping, and other molds. According to the requirements of the drawings, inspect the test products and trim the molds until the products meet the requirements. (3) Cut a single cover tile by cutting the plate, first trim the tail and front ends of the cover tiles, and then use the cover tile preliminary rounding machine to round them. The cover tiles after preliminary rounding are then formed and stamped. (4) The formed products are then put into the rounding machine for rebound size trimming. The size measurement is required for every 20 tiles trimmed. The quality inspector organizes the inspection of flatness, shape, and size, and randomly inspects one for every 100 cover tiles. (5) Polish the surface of the cover tiles, remove the spots, spray fine sand on the surface (to increase the paint adhesion surface and adhesion), remove the floating and sinking, pickle and neutralize, and rinse with clean water. (6) After cleaning and drying the tiles, spray epoxy primer, dry at room temperature, and then spray the national standard color card N3.25 color paint. (7) Send the completed tiles to the dust-free paint spray room and spray matte fluorocarbon anti-oxidation protective paint. The spraying must be uniform without paint flow or spray leakage. The quality inspection department organizes personnel to check the color difference and surface paint condition one by one. (8) The qualified tiles are sent to a professional high-temperature oven for drying (to increase the hardness and adhesion of the paint layer). The maximum temperature during baking is 160 degrees and the time is about 30 minutes. (9) The final quality inspection of the product is carried out. The inspection quantity is 10% of each batch, but not less than 10 pieces, and each batch should not be less than 3 pieces. After passing the inspection, the finished product is registered and packaged for storage.
[0064] The advantages of the present invention are: the whole body is basically made of brass and 304 stainless steel. 304 stainless steel is the most widely used chromium-nickel stainless steel. As a widely used steel, it has good corrosion resistance, heat resistance, low temperature strength and mechanical properties; stamping, bending and other hot processing properties are good, and there is no heat treatment hardening phenomenon (using temperature -196℃~800℃). It has the characteristics of good processing performance and high toughness, and is widely used in curtain walls, side walls, roofs and other building purposes; brass has high strength, high hardness, strong chemical corrosion resistance, and strong wear resistance. And the processing and production of these two materials can be mechanized, saving labor and time costs, and the service life is longer. In certain circumstances, such as pavilions and towers with a height of more than 40 meters to 50 meters, metal components are used to make roofs, which can also reduce the number of maintenance times. For the maintenance of the roof of ancient buildings, if traditional fired tiles are used, scaffolding will be set up from the bottom for maintenance, and the construction difficulty is relatively large; while for metal component tile roofs, it is difficult for roof tiles and ridge decoration components to deform and need maintenance, which is cost-saving for users.
[0065] The above description is only a preferred embodiment of the present invention and is not intended to limit the present invention. For those skilled in the art, the present invention may have various modifications and variations. Any modification, equivalent replacement, improvement, etc. made within the spirit and principle of the present invention shall be included in the protection scope of the present invention.
Claims
1. An assembled building roof structure, It is characterized in that It comprises a roof (1) and a ridge (2), wherein the number of the ridges (2) is plural and they are arranged around the roof (1), and a ridge (3) is arranged at one end of the ridge (2) away from the roof (1); the roof (1) comprises an internal support assembly and an external copper plate (13), wherein the external copper plate (13) is welded to the periphery of the support assembly, and the support assembly comprises a main support rod (11) and a first hot-dip galvanized steel pipe frame (12) arranged around the main support rod (11), and a modeling frame (14) is also arranged outside the first hot-dip galvanized steel pipe frame (12), and the periphery of the modeling frame (14) is used for welding the external copper plate (13); the main support rod (11) is vertically fixed on the roof, and a plurality of steel plate connectors (19) are arranged on the side of the main support rod (11) close to the roof, and the steel plate connectors (19) are used for fixing to the ridge (2); The outer copper plate (13) is attached to the outer periphery of the modeling frame (14), and encloses and forms the lower part of the top (1), the lotus seat of the top (1), the middle part of the top (1) and the upper part of the top (1) from bottom to top, and the main ridge (2) is fixed at the lower part of the top (1); The number of the main ridges (2) is 4, and the array is distributed around the main support rod (11), the main ridge (2) comprises a second hot-dip galvanized steel pipe frame (21) and an inner lining aluminum honeycomb panel (22) arranged on both sides of the second hot-dip galvanized steel pipe frame (21), and the outer side of the inner lining aluminum honeycomb panel (22) is also provided with a plurality of mutually parallel bending strips (23); Both sides of the front ridge (3) are provided with vertical ridges inclined downward, and the two vertical ridges between two adjacent front ridges (3) are connected to each other and fixed on the keel; The roof is provided with bottom tiles and cover tiles, the bottom tiles are fixed on the keel of the roof, the cover tiles are evenly laid on the roof and cover the bottom tiles, and the vertical ridge and the main ridge (2) are both arranged on the surface of the cover tiles; The first hot-dip galvanized steel pipe rack (12) comprises a plurality of transverse steel pipes and a plurality of vertical steel pipes, which are spliced into a plurality of rectangular frame structures, and the length and width of the rectangular frames decrease in a step-like manner from bottom to top.
2. A method for constructing a prefabricated building roof structure, It is characterized in that The construction of the assembled building roof structure according to claim 1 comprises the following steps: S1: Prefabricate the lower part of the pagoda top (1), the lotus seat of the pagoda top (1), the middle part of the pagoda top (1) and the upper part of the pagoda top (1); S2: Install two types of keels, vertical and horizontal, and diagonal, on the roof, and the two types of keels meet at the center of the roof; S3: welding the prefabricated roof (1) at the intersection of the two keels; S4: welding and installing a plurality of ridges (2) around the top of the building (1); S5: Install the main ridge (3) on the side of the main ridge (2) away from the top of the building (1); S6: Install the vertical ridges on both sides of the front ridge (3), and reserve installation positions for the bottom tiles and cover tiles at the bottom; S7: Lay bottom tiles and cover tiles on the roof in sequence; S8: Install the remaining fixings and trims.
3. A method for constructing an assembled building roof structure according to claim 2, It is characterized in that In step S1, the following steps are also included: S11: manufacturing a first hot-dip galvanized steel pipe frame (12) and a modeling frame (14), wherein at least three sides are fully welded during welding, and there are no false welds or leaking welds, and three layers of anti-rust paint are applied after welding; S12: Make a 1:1 clay mold according to the lotus seat of the pagoda (1), manually forge the single lotus according to the model, and then weld and assemble it. The other flat parts are laser cut and machined to form the plate shearing and folding. The spherical part and the decoration on the spherical surface are manually forged according to the lofting size. The decoration on the spherical surface is spot welded on the spherical shape. The spherical shape and the flat part are fully welded and polished. S13: Weld the outer copper plate (13) to the modeling frame (14), and the welding is required to be fully welded and welded inside and outside; weld the single-piece lotus petals to the stainless steel frame, and the welding is required to be fully welded inside and outside without voids; S14: Conduct preliminary inspection on the shape, size, internal steel frame welding, rust prevention, external decorative copper plate welding, and flatness of each component of the top (1); perform grinding, repair welding, and finishing on products that pass the preliminary inspection; S15: The surface of each component is subjected to mechanical and manual roughening treatment, spot removal, deflocculation, pickling and neutralization, and water washing, and then the water is flushed away with an air pump; S16: The outer copper plates (13) of each component of the top (1) are repeatedly washed with chemicals to make them black. After the copper surface is completely blackened, it is manually drawn, and the drawing and washing are repeated along a fixed drawing direction. After the specified effect is achieved, the water is flushed away with an air pump; S17: Spray matte fluorocarbon paint on each component of the top (1) as a protective layer, and there should be no paint flow or spray leakage during the painting process; S18: Send the components of the top (1) to an oven for drying, with the highest temperature being 160° C. and the time being 30 minutes.
4. A method for constructing an assembled building roof structure according to claim 2, It is characterized in that Before step S5, the method further includes forging the front nose (3), and performing surface treatment and anti-oxidation treatment on the front nose (3); specifically, the method includes the following steps: S51: Making a mud mold model according to the drawing of the front kiss (3), and after confirmation, dividing and making the fiberglass reinforced plastic model; S52: trim the block model, turn the zinc mold, polish the zinc mold, and trim the pattern; S53: copper plate cutting and annealing, thermal oxidation, softening and cooling; S54: The zinc mold is put on the machine and the annealed copper plate is used for stamping; S55: After stamping, secondary annealing is performed, followed by glue filling and manual secondary forging; S56: After forging, each component is welded and assembled by argon arc welding, the weld is polished and the whole is polished; S57: The treated front kiss (3) is sent to the antique bronze workshop. The surface of the front kiss (3) is repeatedly washed with chemicals to make it black. After the copper surface is completely black, it is manually drawn. The wire drawing and washing are repeated along a fixed drawing direction. After the specified effect is achieved, the water is flushed away with a high-pressure air pump. S58: Send the finished front kiss (3) to the dust-free spray paint room and spray matte fluorocarbon anti-oxidation protective paint. The spraying is required to be uniform without paint flow and spray leakage. Check the color difference and surface paint condition one by one; S59: The qualified front kiss (3) is sent to the oven for drying. The maximum temperature during baking is 160° C. and the time is 30 minutes.
5. A method for constructing an assembled building roof structure according to claim 2, It is characterized in that Before step S7, the process also includes making a bottom tile, which is made of 304 stainless steel and is integrally seamlessly stamped; the process specifically includes the following steps: S71: Making stamping steel mold; S72: Conduct a mold test to check the size, flatness, and stretching of the stamped product, and fine-tune the mold according to the inspection results until it meets the product requirements; fix the mold that has been fine-tuned multiple times, and make a product stamping support frame; S73: Punch, and pay attention to prevent the product from shifting during punching. Dust and adhesives should be removed from the mold and the board surface after each punching to ensure the flatness of the product surface. One bottom tile is randomly inspected for every 20 molded bottom tiles; S74: Fold the stamped bottom tile to form an upward side-turned water retaining edge. According to the different sacs of each layer of the roof, make a rolling machine, and use the rolling machine to roll the bottom tile to the required arc on the drawing; cut the material according to the size of the drawing and affix the "layer position number" to each bottom tile. The bottom tile at the wing corner needs to be cut at an angle; fully weld the dripping water at the end of the bottom tile, and open a flat opening at the side-turned water retaining edge at the front end of the bottom tile, reserved for the installation of hook tiles; S75: Finely grind the drip welding part, and check the size, cysticity and drip welding strength of the bottom tile. One bottom tile is randomly inspected for every 50 formed bottom tiles; S76: polishing the bottom tile surface, removing spots, spraying fine sand on the surface to remove floating and sinking, pickling and neutralization, and washing with clean water; S77: After cleaning and drying the bottom tile, spray epoxy primer, dry at room temperature, and spray the confirmation paint after drying; S78: Send the finished base tiles to the dust-free spray paint room and spray matte fluorocarbon anti-oxidation protective paint. The spraying should be uniform without paint flow or leakage. Check the color difference and surface paint condition one by one. S79: The bottom tiles that have passed the inspection are sent to the oven for drying. The maximum temperature during baking needs to be 160℃ and the time is 30 minutes.