A method for manufacturing a circuit board by laser processing electroplating hole anti-plating and conductive pattern

Through the use of laser processing technology and non-photosensitive materials, the problems of uneven thickness of the conductive layer in the hole wall in the circuit board manufacturing and the complexity of traditional etching methods are solved, and efficient and fine conductive and solder resistance pattern manufacturing is achieved, which improves the circuit board's Electrical performance and production efficiency.

CN113692131BActive Publication Date: 2024-11-12德中(天津)技术发展股份有限公司
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202111001593.X
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2021-08-30
Publication Date
2024-11-12
Estimated Expiration
2041-08-30

AI Technical Summary

Technical Problem

In the existing circuit board manufacturing technology, the thickness of the hole wall conductive layer is inconsistent with the thickness of the board surface conductive layer, resulting in uneven electrical performance. The traditional etching method is complex and has low efficiency, making it difficult to achieve high-precision conductive patterns and solder resist patterns.

Method used

Using laser processing technology, non-photosensitive materials are used as the electroplating masking film, the masking film is directly removed and copper is only electroplated on the hole wall. Combined with laser, the copper foil in the non-line area is removed, so as to realize the manufacturing of conductive patterns and solder resist patterns, simplifying the process. , improve efficiency.

Benefits of technology

It realizes fine control of the thickness of the conductive layer on the hole wall, improves the electrical performance and manufacturing efficiency of the circuit board, reduces costs, and is suitable for large-scale and small-scale production.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN113692131B_ABST
    Figure CN113692131B_ABST
Patent Text Reader

Abstract

The present invention relates to a method for manufacturing a circuit board by laser processing electroplating hole anti-plating and conductive pattern, drilling holes and depositing a thin metal layer on the hole and the board surface, pasting a non-photosensitive masking film, laser removing the masking layer covering the hole wall to expose the hole wall, only electroplating and thickening the conductive layer in the hole, electroplating solderable metal on the hole wall, using laser to make a conductive pattern, applying non-photosensitive solder resist on the non-circuit area, using laser to make solder resist pattern at the assembly site, and cleaning and solderability treatment of the welding area surface; the present invention can optimize and shorten the circuit board manufacturing process as a whole, improve quality and efficiency, reduce costs, and be environmentally friendly. Using non-photosensitive materials as anti-plating materials, only electroplating and thickening the conductive layer in the hole, only electroplating solderable metal on the hole wall, using laser to make electroplated hole patterns, conductive patterns, and solder resist patterns, with fewer steps and low cost, can manufacture more sophisticated circuit boards. It is suitable for mass production of various circuit boards, and is also suitable for circuit board samples and small batch and multi-variety production.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to a method for manufacturing a circuit board by laser processing electroplating hole anti-plating and conductive pattern, which directly and selectively removes materials and only electroplates holes, and belongs to the technical field of circuit board manufacturing. Background Art

[0002] The present invention uses laser direct material removal technology to manufacture circuit boards, can only electroplate hole walls, and can directly manufacture solder resist and conductive patterns without a pattern transfer process.

[0003] The manufacturing process is as follows: depositing an initial conductive layer on the semi-finished product of a double-sided, multi-layer circuit board with completed drilling, chemically plating or electroplating thin copper → attaching an anti-plating masking film → laser removing the anti-plating masking film layer on the hole area, opening a window for the liquid to enter the hole, and making a pattern of the plated hole wall → electroplating, depositing copper on the hole wall to thicken the hole wall → electroplating and depositing a solderable metal layer on the hole wall → laser removing the anti-plating masking film layer on the non-circuit area → laser removing the copper foil in the non-circuit area to make a conductive pattern → applying and curing solder resist material on the non-circuit area → using a laser to remove organic materials on the conductor in the welding area at the assembly site to make a solder resist pattern, and cleaning and solderability treatment of the welding area surface → adding solder to the connection pad, mounting and inserting components, and performing remelting soldering and / or wave soldering.

[0004] The present invention can be used to replace various subtractive hole-making metal printed circuit board technologies. The starting raw material is a conductive metal foil material, including various rigid copper-clad boards, flexible copper-clad boards, or rigid-flex boards. The present invention uses laser processing technology and the same non-photosensitive material mask as the pattern of the electroplated hole wall and the solder mask pattern, respectively, to control the copper thickness of the hole wall, better meet the electrical requirements of electronic products for circuit boards, and is suitable for small-batch and multi-variety production of circuit boards, and is also suitable for batch manufacturing of circuit boards.

[0005] From concept to finished product, electronic products generally go through three stages: design, material preparation, and assembly.

[0006] After the physical design is completed, material preparation is required, including the selection and customization of various components, connectors, display modules, and other functional modules. Among them, one of the most important materials is the bare circuit board, because the bare circuit board is used to support components and play the role of electrical interconnection between the pins of components. It is a key factor affecting the quality and reliability of electronic products and the difficulty, cost, and speed of the entire manufacturing process. It must be customized according to the design requirements and product properties. Bare circuit board, referred to as bare board, refers to a circuit board that has not yet been installed with components. It is also called printed circuit board, printed circuit board, printed circuit board, printed board, circuit board, circuit board, printed board. Bare boards are generally customized on demand by manufacturers specializing in the manufacture of printed circuit boards. Taking a multi-layer circuit board as an example, the process flow of bare board manufacturing is roughly as follows: making inner conductive patterns - blackening / browning and lamination - drilling holes on a multi-layer copper-clad insulating substrate - performing hole metallization - making outer conductive patterns and removing metal anti-corrosion film or organic anti-corrosion film - applying solder resist - making solder resist patterns and generating welding areas - applying solderability coating to the surface of the welding area - making marking symbols - shipping to manufacturers in the assembly stage.

[0007] The assembly of electronic products is to assemble, match and combine various materials together, and to achieve the fixation of the positions of the materials and the corresponding electrical connections and functional coordination through connection means such as soldering, fastening and bonding. In a narrow sense, the assembly process of installing and soldering components to the circuit board is often called assembly. The product after the components are assembled is generally called an assembled board. In situations where no distinction is needed, bare circuit boards and assembled boards are generally called circuit boards.

[0008] In the past, the assembly technology was mainly based on the through-hole method, that is, the pins of various components, connectors, functional modules, etc. were inserted into the mounting holes of the bare board, and then the pins were brazed with the hole wall and the pads with solder, so that the components were fixed on the circuit board, and the electrical interconnection between the pins of the components was achieved through the pads, interconnection wires, and relay holes on the circuit board. At present, electronic products are more often assembled using surface mounting technology, that is, firstly, solder paste is applied on the connection pad of the circuit board, that is, the pad, and then the pins of various components, connectors, functional modules, etc. are placed on the solder paste layer of the connection pad, and finally the circuit board is heated to melt the powdered or granular solid metal tin / tin alloy in the solder paste, and the molten solder infiltrates the terminal electrodes / pins of the components and the circuit board pads. When cooled into solid metal, the terminal electrodes of the components are brazed with the connection pads, so that the components are mounted and fixed on the surface of the circuit board, and the electrical interconnection between the components is achieved through the conductive channel formed by the pads, wires, and holes on the circuit board. The assembly of circuit boards is either done by professional assembly factories or by electronic product development organizations. Taking SMT technology as an example, the assembly process of circuit boards is roughly as follows: circuit boards from bare board manufacturers - solder paste is printed on the soldering pads - components are picked up and attached to the surface of the circuit board - heating is performed to reflow the solder paste to achieve soldering of pins and pads.

[0009] Considering the bare board manufacturing and component assembly process of the circuit board as a whole, it can be seen that the key to bare circuit board manufacturing is the process of conductive pattern production, lamination, drilling and hole metallization, solder mask pattern production and solderability coating, while solder paste coating, component insertion and welding are the key processes in the assembly production stage. Further analysis shows that these processes are essentially for the purpose of achieving the installation and fixation of components and the electrical interconnection between components. Among them, the manufacturing of conductive patterns is related to the fineness and electrical performance of the circuit board circuit; the manufacturing of solder mask patterns and solderability coating are completed at the bare board stage, but they are the basis of production at the assembly stage; and drilling and hole metallization affect the connection density, mechanical properties, application environment, and matching degree of the installation and fixation of the plug-in on the one hand, and determine the electrical performance and reliability of the Z-direction interconnection between the horizontal conductive layers of the circuit board on the other hand, and directly affect the difficulty of the manufacturing process of the conductive pattern of the horizontal electrical connection of the circuit board.

[0010] With the progress of social economy, the requirements for electronic products are getting higher and higher, the components are getting smaller, the functions are getting stronger, the number of pins is increasing, the requirements for conductive patterns and solder mask patterns are becoming more and more precise, and the requirements for holes are getting smaller and deeper. Whether in the bare board manufacturing stage or the component assembly stage, various process problems affect each other, making the technical difficulty of circuit board manufacturing increasingly greater.

[0011] For example, in the current hole metallization process, in order to meet the minimum reliability and electrical requirements of the physical carrier of Z-direction electrical interconnection, that is, the minimum thickness of the hole wall conductive layer, metal copper must be deposited on the hole wall by electroplating technology, and the electroplating process requires a conductive channel. The existing technology, whether it is graphic electroplating, full-board electroplating etching to make conductive graphics, or laser selective removal of copper foil to make conductive patterns, has to use the original copper foil on the substrate as the power line for copper plating on the hole wall. While electroplating copper to thicken the hole wall conductive layer, the thickness of the conductive layer will inevitably increase synchronously with the hole wall on the basis of the inherent copper foil on the board surface. Moreover, due to the step-by-step factors of the power line, and also due to the depth capacity and the plating capacity of the electroplating process, the thickness of the final board surface deposition layer will be greater than the hole wall deposition layer. The IPC-6012 standard has clear requirements for the thickness of the metallized hole wall, which is at least 20μm. The current PCB manufacturing process has limited deep plating capability. When the hole wall copper thickness reaches 20μm, the increased copper thickness on the board exceeds the hole wall copper thickness. When added to the original copper foil thickness of the material of 18um, the total copper thickness exceeds 40μm, or even reaches 50um. However, this electroplating thickened hole must simultaneously thicken the original copper foil on the board. It does not enhance the performance of the PCB due to the consumption of copper resources, nor does it reduce the difficulty of subsequent processes. On the contrary, such a process has a negative impact on the performance and process of the PCB in the following aspects:

[0012] First, the thickness of the hole wall conductive layer is smaller than that of the board surface conductive layer, resulting in inconsistent electrical properties between the Z-direction conductive link and the X and Y plane conductive link. Second, the conductive layer produced by the hole wall electroplating process of the circuit board becomes the top layer of the conductive pattern conductive layer in the future. Under the action of the skin effect, it is the main medium for the transmission of high-frequency electrical signals. The quality of the copper layer deposited by electroplating technology in the production of circuit boards is slightly lower than the purity of the copper foil produced by electroforming or rolling technology. The crystal is slightly rougher, and the electrical and mechanical properties are slightly worse. Therefore, the increase in the thickness of the conductive layer is not conducive to high-speed and high-frequency signal transmission. Third, the increase in the thickness of the copper foil and the lateral etching caused by it are factors that restrict the fineness of the conductive pattern. In the process of manufacturing the conductive pattern by chemical etching technology, the etching liquid contacts the copper foil for etching. In addition to the vertical etching to the depth of the copper foil, the etching liquid contacts the two sides of the wire, so that the etching is also carried out on the two sides of the wire at the same time. The thicker the etched copper layer and the longer the time, the more serious the lateral etching phenomenon. The lateral etching not only reduces the width of the wire, but also causes wire breakage in severe cases. Fourth, the uneven thickness of the copper foil is a bottleneck for the widespread application of laser conductive patterning technology. Obviously, the thicker the copper foil, the greater the laser energy required, the more times the processing is required, and the slower the processing process will be; the more uneven the thickness of the copper foil, the more difficult the photo-etching process is, either the laser power applied to the area with thicker copper foil is too small, the copper is not completely removed, and the residual copper affects the insulation performance, or the laser power applied to the area with thinner copper foil is too large, the insulating material under the copper foil is ablated, affecting the quality of the circuit board.

[0013] The problem with the existing technology in the conductive pattern manufacturing process is that the traditional etching method is complicated and requires the use of a pattern transfer process to manufacture an anti-etching mask. The pattern transfer process requires the use of photosensitive materials, and a mask plate for selective exposure needs to be manufactured first. After the conductive pattern is etched, the anti-etching mask needs to be removed. The under-etching, over-etching, side-etching, and uneven etching that occur with etching often cause the quality control factors to lose sight of each other, and there are many problems. Although the laser directly removes organic materials to make anti-etching masks, anti-plating masks, and solder masks, and directly removes conductive copper foil to make conductive patterns, the process is simple, but because the laser spot diameter is small, it needs to be processed point by point and line by line, which is slow and inefficient. In addition, in the process of directly removing conductive copper foil from the conductive pattern by laser, because the copper foil layer on the substrate becomes thicker and more uneven after the hole metallization, it is difficult for the laser energy to change accordingly in real time, and it is difficult to ensure the removal quality.

[0014] The problem with solder mask pattern making and solderability coating is that, like the manufacturing of conductive patterns, the traditional technology of solder mask pattern making is a pattern transfer process that requires the use of photosensitive materials and the manufacture of masks for selective exposure. The baking and exposure effects interfere with each other, making quality control difficult, and defects such as pads on solder mask frequently appear. Whether it is hot air leveling or chemical nickel-gold technology for solderability coating, the ingredients are complex and the process is cumbersome, which will bring confusion about unclear welding mechanism and affect reliability.

[0015] The inventor of application number CN201410190917.2 has disclosed a method for selectively electroplating conductive holes in a circuit board, which is suitable for the direct electroplating hole metallization process of a polymer conductive film method. The technical solution is to use a material that is resistant to electroplating, resistant to polymer conductive film deposition, and can be peeled off, that is, a polyester film that is peelable and coated with a silicone rubber adhesive, to mask all areas of the board surface, and expose the surface of the hole wall after drilling. Because these materials have the properties of resisting the pretreatment required for the deposition of polymer conductive films and resisting the deposition of polymer conductive films, in the subsequent direct electroplating process of polymer conductive films, polymer conductive films will only be added to the hole walls. During electroplating, the electroplating power supply uses the copper foil on the board surface as a conductive link channel to provide current to the hole walls, thereby realizing electroplating processing that only deposits copper on the hole walls. The problem is that the hole metallization process of direct electroplating of polymer conductive film method needs to be treated with a solution of 100g / L or more permanganate concentration at a temperature of 90 degrees Celsius for 70 seconds, which will produce destructive oxidation effects on both the peelable glue and the adhesive of the polyester film, causing the masking material, which has a weak adhesion to the substrate, to have a lower bonding strength with the copper foil, resulting in bone separation, delamination, seams, and openings, which will inevitably lead to poor masking board surface effects. After the hole wall is thickened by electroplating copper, the problem of uneven thickness of the copper foil on the copper foil board surface will be aggravated due to the infiltration, overflow, and immersion of the solution. In addition, the direct electroplating hole metallization process of polymer conductive film method has a limited scope of application and is not suitable for multi-layer circuit boards. Considering factors such as quality and cost, it is even more necessary to solve the problems of only metallization and electroplating hole wall faced by traditional chemical copper deposition hole metallization technology, black hole direct electroplating hole metallization technology, and palladium film method direct electroplating hole metallization technology. Because these technologies require acid, alkali or organic solvent treatment before hole metallization, it is obvious that the technical solution of using strippable colloidal materials is not strong enough and cannot be applied to mainstream hole metallization technology. It is necessary to find more suitable materials and methods.

[0016] In summary, it is not difficult to see that the current circuit board manufacturing technology includes a series of indirect processing, chemical treatment, and wet manufacturing processes. These single-function processes have their own inherent technical limitations, and they are mutually restrained and mutually dependent, which is the fundamental reason for limiting higher quality, higher efficiency, and more environmentally friendly. It is necessary to improve and update each single-function process, and also to optimize and upgrade it as a whole. Summary of the invention

[0017] In view of the deficiency of the prior art that only thickening holes can be electroplated, the present invention has developed a new manufacturing method, and the technical solution of the present invention is as follows:

[0018] A method for manufacturing a circuit board by laser processing electroplating hole anti-plating and conductive pattern, drilling holes and depositing a thin metal layer on the hole and the board surface, pasting a non-photosensitive masking film, laser removing the masking layer covering the hole wall to expose the hole wall, only electroplating to thicken the conductive layer in the hole, electroplating a solderable metal on the hole wall, using laser to make a conductive pattern, applying a non-photosensitive solder resist on the non-circuit area, using laser to make a solder resist pattern at the assembly site, and cleaning and soldering the surface of the welding area; the steps are:

[0019] (1) Depositing an initial conductive layer on a double-sided, multi-layer circuit board in production after drilling, and electroplating copper to a thickness that can withstand subsequent processes;

[0020] (2) Affixing a non-photosensitive organic film to the board surface as an anti-plating masking film;

[0021] (3) using a laser to remove the masking material covering the hole wall area to produce an anti-plating pattern, and using a laser to remove the anti-plating masking film layer on the surface of the clamping point of the electroplating fixture to expose the copper surface in the contact area with the electroplating fixture;

[0022] (4) Electroplating, depositing copper on the hole wall to thicken the conductive layer to the thickness required for final inspection;

[0023] (5) Electroplating, depositing solderable metal on the hole wall;

[0024] (6) Use laser to remove the anti-plating masking film on the non-circuit area;

[0025] (7) Use laser to remove the copper foil in the non-circuit area to produce a conductive pattern;

[0026] (8) Applying and curing non-photosensitive solder resist on non-circuit areas at one time;

[0027] (9) Use laser to remove organic materials on the conductors in the welding area at the assembly site, create solder resist patterns, and clean and treat the surface of the welding area for solderability;

[0028] (10) Add solder to the connection pad, mount and insert components, and perform reflow soldering and / or wave soldering.

[0029] The non-photosensitive organic film in step (2) is composed of several layers of different shapes and components, among which the layer in contact with the circuit board has viscosity and fluidity.

[0030] The non-photosensitive organic film in step (2) has anti-plating / anti-welding properties, and the anti-plating masking film covering the circuit area does not need to be removed and serves as a solder resist film for the circuit area.

[0031] The step (2) includes depositing non-photosensitive organic film-forming substances on the plate surface and hole walls by electrophoresis, vacuum coating, and vapor deposition technology; and includes coating liquid photosensitive materials and dry photosensitive films by using existing technology.

[0032] The coating method of step (8) includes spray printing and screen printing; the coating thickness is achieved so that it is flush with the masking film on the circuit after solidification or according to design requirements.

[0033] The steps (7) and (8) include removing all remaining anti-plating masking films on the board surface by laser after the conductive pattern is formed.

[0034] The steps (7) and (8) also include using laser to remove all remaining anti-plating masking films on the board surface, and then applying existing technology and materials to coat the entire board surface and cure it in one go with photosensitive and non-photosensitive solder resist.

[0035] The step (8) also includes applying existing technology and materials to completely coat and cure the photosensitive and non-photosensitive solder resist at the bare board manufacturing site, removing the organic material on the conductor of the welding area with a laser, manufacturing a solder resist pattern, and cleaning the surface of the welding area.

[0036] The specific instructions are as follows:

[0037] The present invention provides a method for manufacturing a circuit board by laser processing electroplating hole anti-plating and conductive pattern, including using a non-photosensitive material as a masking film and laser photoetching to remove the masking film to expose the hole; including only electroplating to thicken the conductive layer in the hole; including using a laser to manufacture a conductive pattern; including only coating a non-photosensitive solder resist on a non-circuit area; including using a laser to manufacture a solder resist pattern at the assembly site, and cleaning and solderability treatment of the surface of the welding area, which can achieve the overall goal of shortening the manufacturing process, improving quality and efficiency, reducing costs, and being environmentally friendly.

[0038] Step (1) depositing an initial conductive layer on a double-sided, multi-layer circuit board in process after drilling, and electroplating copper to a thickness that can withstand subsequent processes;

[0039] The purpose of making thin copper on the initial conductive layer is to increase the reliability of the process. The thickness can reach the lower limit of ensuring the reliability of the process. For example, after traditional chemical copper deposition or black hole formation by carbon film method, 1μm-5μm thin copper is electroplated.

[0040] Step (2) affixing a non-photosensitive organic film onto the board surface as an anti-plating masking film;

[0041] The prior art generally uses photosensitive dry film as an anti-plating mask. The photosensitive dry film is a three-layer structure. The photosensitive adhesive coating is between the carrier film and the protective film. It is composed of adhesives and photopolymer monomers. The pattern forming process is relatively complicated and requires the steps of photo-drawing, film pasting, exposure, and development. Moreover, it is expensive, has low strength, and is relatively thick, generally above 20μm. The resolution is limited and the masking effect is poor. The masking film of the present invention does not need to have photosensitive properties. General pre-coated pressure-sensitive coating films and heat-sensitive coating films can meet the requirements. It is hot-pressed and coated, and the laser is directly removed to form a pattern. The process is simple. Moreover, it has high resolution, low price, high strength, good masking ability, can be removed in steps, and can withstand multiple electroplating processes. For example, a 20μm thick heat-sensitive PI, PVC, PC, PET, and PP film can be hot-pressed as an anti-plating mask, and parylene can also be used as a mask.

[0042] The non-photosensitive organic film in step (2) is composed of several layers of different shapes and compositions, wherein the layer in contact with the circuit board has viscosity and fluidity. The non-photosensitive organic film has anti-plating / anti-welding properties, and the anti-plating masking film covering the circuit area does not need to be removed and serves as the solder resist film of the circuit area.

[0043] The step (2) includes depositing non-photosensitive organic film-forming substances on the plate surface and hole walls by electrophoresis, vacuum coating, and vapor deposition technology; and includes coating liquid photosensitive materials and dry photosensitive films by using existing technology.

[0044] Step (3) using a laser to remove the masking material covering the hole wall area to produce an anti-plating pattern, and using a laser to remove the anti-plating masking film layer on the surface of the clamping point of the electroplating fixture to expose the copper surface in the contact area with the electroplating fixture;

[0045] Laser removes the anti-plating masking film layer on the hole area to open a window for the liquid to enter the hole. For example, a pulsed IR laser with a wavelength of 1064nm is used, with the inner diameter of the hole as the outer contour, to remove the masking film covering the hole wall in blocks by ring cutting or photoetching point by point to expose the hole wall. In order to solve the problems of too small total area, uneven distribution of electric lines, and difficult control of current density when electroplating the hole wall, when making the hole wall electroplating pattern, a laser can be used to remove the dead copper area with no electrical function in the non-circuit part, or the area where its conductive layer needs to be removed and does not have a negative impact on the subsequent removal process, or the area where the copper thickness does not affect its function, or the area where increasing the copper thickness has a positive impact on the function. The anti-plating masking film increases the conductive area, disperses the electric lines, and forms a pattern that is conducive to the balanced electroplating process of the plated hole wall.

[0046] The pattern of the electroplated hole wall made by laser also includes removing dead copper areas with no electrical function that are not circuits and are spaced more than 30μm from the circuits, preferably more than 50μm apart, or areas where the conductive layer needs to be removed and does not have a negative impact on the subsequent removal process, or areas where the copper thickness does not affect its function, or areas where increasing the copper thickness has a positive effect on the function. The anti-plating mask film forms a balanced electroplating pattern that is beneficial to the plated hole wall.

[0047] Step (4) electroplating, depositing copper on the hole wall to thicken the conductive layer to the thickness required for final inspection;

[0048] The control point of this step is the electroplating time. At this time, except for the hole wall and the electroplating balance block, all areas on the board are covered with a mask. The mask is an insulating material. Although it is in contact with the electroplating solution, copper cannot be deposited on the surface. Therefore, only the hole wall and the balance block can deposit copper during the electroplating process. If the electroplating time is sufficient, a copper deposition layer of sufficient thickness can be obtained on the hole wall, achieving the purpose of selectively controlling the copper thickness of the hole wall.

[0049] Step (5) electroplating to deposit a corrosion-resistant and weldable metal on the hole wall;

[0050] The electroplated metal needs to have the corrosion resistance required in step (7). At the same time, it should also protect the corresponding area during transportation and storage of the circuit board and increase the solderability of the welding area during assembly of the circuit board.

[0051] The present invention uses non-photosensitive anti-plating materials with good masking ability, which can withstand longer electroplating time and more stringent plating solutions and operating conditions. In addition, because the other areas of the board surface are masked by a polymer film, the technology of the present invention can only deposit metal on the hole wall and the surface of the electroplating balance block, and the plating area is relatively small, saving materials. Therefore, more types of metals that are both corrosion-resistant, protective, and weldable can be selected, such as nickel and gold.

[0052] Step (6) using a laser to remove the organic film material on the non-circuit area to expose the non-circuit copper and obtain an anti-etching masking pattern;

[0053] When using a laser to remove the anti-electroplating masking film on a non-circuit area, when the ratio of the perimeter of the area to be removed to the diameter of the focused laser beam is small, preferably less than 10, the masking film on the surface of the substrate and the conductive metal copper underneath are removed by point-by-point and line-by-line photolithography using a focused laser beam; when the ratio of the perimeter of the area to be removed to the diameter of the focused laser beam is large, preferably greater than 15, the masking film on the surface of the substrate and the conductive metal copper underneath are first removed by point-by-point photolithography using a focused laser beam along the inner side of the envelope of the area to be removed and with the envelope as the boundary, until a closed insulating channel is formed around the unremoved portion of the area, and then a laser beam with a diameter lower than the minimum optical power density required to remove the metal copper but larger is used to heat the unremoved area, so that the anti-electroplating masking film on it and the conductive metal copper underneath are simultaneously separated from the substrate surface and removed.

[0054] When using laser to remove the anti-plating masking film on the non-circuit area, the focused laser light power density used is kept greater than the minimum power density required to remove the organic material, preferably greater than 1.2 times the minimum light power density required to remove the organic material and lower than or close to the minimum light power density required to remove the metal layer covered thereunder, and the focused laser beam diameter is changed according to the shape and size of the removed area to reduce or remove the overlap of the laser processing area and improve the processing efficiency. When laser removing the anti-plating masking film on the non-circuit area, lasers of the same wavelength and pulse width, as well as lasers of different wavelengths and pulse widths, can be used to complete the process under different parameters such as spot diameter, focal depth, and light power density.

[0055] Step (7) uses laser to remove the copper foil in the non-circuit area to produce a conductive pattern.

[0056] Step (7) includes using a laser to remove all remaining anti-plating masking films on the board surface after the conductive pattern is formed.

[0057] Because the present invention can selectively plate holes, the technology of removing the conductive material in the non-circuit area with a laser is easier to implement. In the current common circuit board manufacturing technology, after the hole metallization electroplating process, due to the limitation of the hole plating capacity of the hole system, the deposition rate of copper is different in different areas on the same substrate material, resulting in a large difference in the thickness of the total conductive layer. In this way, when using laser photo-etching to remove the conductive layer of the non-circuit part, if the laser parameters do not change with the copper thickness, either the copper is not completely removed from the area with a large total copper thickness, and the residual copper affects the insulation performance, or too much energy is applied to the area with a small total copper thickness, resulting in a problem of ablation of the insulating material.

[0058] The technical solution of selectively electroplating holes and conductive patterns of the present invention can avoid copper deposition in non-circuit areas, especially in the laser photoetching removal path, so that the conductive layer under the laser photoetching path is kept as the original copper foil with uniform thickness, thereby reducing the difficulty of laser processing. The present invention adopts the striping and stripping method / Striping & Stripping of German-Chinese technology, firstly using laser photoetching to vaporize the conductive material point by point and layer by layer to form a closed dividing line, and subdividing the conductive layer area to be removed into small pieces with mutually insulated areas within a certain range, which is called striping; then, using laser to heat the small pieces to reduce the bonding force between the small pieces and the substrate, so that the small pieces are separated from the substrate in pieces, which is called stripping.

[0059] When implementing laser striping and stripping technology, it is not necessary to remove the anti-plating masking film in the non-circuit area first. For example, when using ultraviolet laser processing or picosecond laser striping, the masking film and the copper foil layer underneath it can be vaporized by laser photo-erosion until the insulating substrate layer is stopped, forming an insulating channel; when stripping, the masking film and the copper foil layer underneath it are heated together, and the pieces are stripped off through thermal deformation and reduced bonding strength with the insulating substrate. In order to be suitable for laser processing, the anti-plating masking film can be selected from colored materials to produce better absorption effects.

[0060] When laser removal of copper foil on non-circuit areas, the focused laser light power density used is kept greater than the minimum light power density required to remove the conductive metal copper layer, and less than 3 times the minimum light power density required to remove the conductive metal copper layer. The focused laser beam diameter is changed according to the shape and size of the removed area to reduce or remove the overlap of the laser processing area and improve the processing efficiency. When laser removal of copper foil on non-circuit areas, lasers with the same wavelength and pulse width, as well as lasers with different wavelengths and pulse widths, can be used under different parameters such as spot diameter, focal depth, and light power density.

[0061] Step (8) coating the non-circuit area with a non-photosensitive solder resist and curing it once;

[0062] Step (8) also includes using laser to remove all remaining anti-plating masking films on the board surface, and then applying existing technology and materials to coat the entire board surface and cure it in one go with photosensitive and non-photosensitive solder resist.

[0063] The prior art generally uses liquid photosensitive ink as solder resist, which contains adhesives and photopolymerizable monomers. The pattern forming process is very complicated and requires multiple processes such as coating, pre-baking, exposure, development, and curing. Moreover, it is expensive, has low resolution, and is difficult to ensure the coating quality between fine pitch connection pads. The solder resist of the present invention does not need to have photosensitive properties. General pre-coated pressure-sensitive coating films and heat-sensitive coating films can meet the requirements. It is cheap and has high resolution, and can produce fine pattern structures. In addition, the present invention uses hot pressing coating, which does not require an additional curing process. The solder resist pattern is left to be produced on-site by laser before component assembly, and the process is simple. For example, a heat-pressed paste with a thickness of 20μm-200μm of thermal-sensitive PI, PVC, PC, PET, and PP films is used as a solder resist, and parylene can also be used as a solder resist.

[0064] The coating method of step (8) includes spray printing and screen printing; the coating thickness is achieved so that it is flush with the masking film on the circuit after solidification or according to design requirements.

[0065] Step (9) using a laser to remove organic materials on the conductors in the welding area at the assembly site, to produce a solder resist pattern, and to clean and treat the surface of the welding area for solderability;

[0066] This step can be completed in one step on the same equipment, or it can be carried out in two steps on different equipment, namely, the first step: making a solder resist pattern and generating a welding area: using a laser to selectively photoetch to remove the solder resist coating on the welding area, making a solder resist pattern and generating a welding area; the second step, cleaning and solderability treatment of the welding area surface, using another laser to remove the solder resist residue on the surface of the welding area, and slightly photoetching the metal surface layer of the welding area to remove metal oxides, exposing a fresh metal surface, and creating solderability that is easily wetted by molten solder.

[0067] Step (10) adds solder to the connection pad, mounts and inserts components, and performs reflow soldering and / or wave soldering.

[0068] The present invention can optimize and shorten the circuit board manufacturing process as a whole, improve quality and efficiency, reduce costs, and be environmentally friendly. Non-photosensitive materials are used as anti-plating materials, only the conductive layer in the hole is plated to thicken, and only the solderable metal is plated on the hole wall. Lasers are used to manufacture electroplated hole patterns, conductive patterns, and solder resist patterns. There are fewer steps and lower costs, and more sophisticated circuit boards can be manufactured. The present invention is suitable for mass production of various circuit boards, and is also suitable for circuit board samples and small batch, multi-variety production.

[0069] The advantages and effects of the present invention are:

[0070] 1. The present invention can selectively electroplate holes, and the plating thickness can be easily controlled. In particular, only the thickened holes can be electroplated, which can solve the problem of thin hole wall plating thickness and the problem of inconsistency between the hole wall plating thickness and the circuit copper plating thickness.

[0071] 2. The present invention uses a laser direct removal method to manufacture electroplated hole wall patterns, and can use non-photosensitive materials as anti-electroplating materials to reduce costs. It also has good electroplating resistance and can manufacture thicker hole wall conductive layers.

[0072] 3. The present invention realizes electroplating of holes only, and the thickness of the conductive layer of the non-circuit part does not increase. It is suitable for using laser to directly remove the copper foil of the non-circuit part to manufacture conductive patterns. There is no need to remove the anti-plating material, and the steps are few, so that more sophisticated conductive patterns can be manufactured.

[0073] 4. The present invention can remove the anti-plating mask at the same time when laser manufacturing the conductive pattern, and no special film removal process is required, which reduces the number of steps.

[0074] 5. The present invention uses a film pre-coated with a heat-sensitive or pressure-sensitive solder resist material as a solder resist, and uses lasers with different wavelengths, pulse widths, and power densities to manufacture solder resist patterns, which is more efficient and has a better processing effect. BRIEF DESCRIPTION OF THE DRAWINGS

[0075] Figure 1 : Process flow chart of embodiment 1;

[0076] Figure 2 : Process flow chart of embodiment 2;

[0077] Among them: 1. Insulating substrate 2. Copper layer of copper clad laminate 3. Initial conductive layer 4. Electroplated thin copper 5. Anti-plating masking film 6. Hole electroplating layer 7. Solderable metal 8. Solder resist material layer 9. Cleaned and solderable surface 10. Solder 11. Components

[0078] In the attached drawings, each letter A\B\C\D\E\F\G\H corresponds to a partial enlarged schematic diagram of each step. DETAILED DESCRIPTION

[0079] The present invention will be further described below in conjunction with the following embodiments. The following embodiments are illustrative, not restrictive, and the protection scope of the present invention cannot be limited by the following embodiments.

[0080] Example 1

[0081] In the electronics industry, copper clad laminate is often used as a basic material to make circuit boards. The copper clad laminate includes an insulating substrate 1 and a copper layer 2 of the copper clad laminate.

[0082] This embodiment takes a double-sided printed circuit board as an example, and the specific processing steps are as follows:

[0083] (1) The copper-clad laminate of the circuit board substrate includes an insulating substrate 1 and a copper layer 2 of the copper-clad laminate. The copper-clad laminate is drilled, and a starting conductive layer 3 is deposited on the semi-finished product of the double-sided circuit board after the drilling is completed. The copper is electroplated to a thickness that can withstand subsequent processes to form an electroplated thin copper 4. ;

[0084] The purpose of making a thin copper layer on the initial conductive layer is to increase the reliability of the process, and the thickness of the thin copper layer only needs to reach the lower limit of ensuring the reliability of the process.

[0085] The double-sided board with holes drilled is electroplated. Specifically, the double-sided board with holes drilled is brushed to remove the burrs at the hole mouth and clean the board surface. Then the holes are normally blackened and copper is electroplated. The electroplating parameters are: 10ASF*30min, and the thickness of the coating in the hole is about 5um.

[0086] (2) A non-photosensitive polymer film is attached to the board surface as an anti-plating masking film 5.

[0087] The prior art generally uses photosensitive dry film as an anti-plating mask. The photosensitive dry film is a three-layer structure. The photosensitive adhesive coating is between the carrier film and the protective film. It is composed of adhesives and photopolymer monomers. The pattern forming process is relatively complicated and requires the steps of photo-drawing, film pasting, exposure, and development. Moreover, it is expensive, has low strength, and is relatively thick, generally above 20μm. The resolution is limited and the masking effect is poor. The masking film of the present invention does not need to have photosensitive properties. General pre-coated pressure-sensitive coating films and heat-sensitive coating films can meet the requirements. It is hot-pressed and coated, and the laser is directly removed to form a pattern. The process is simple. Moreover, it has high resolution, low price, high strength, good masking ability, can be removed in steps, and can withstand multiple electroplating processes. For example, a 20μm thick heat-sensitive PI, PVC, PC, PET, and PP film can be hot-pressed as an anti-plating mask, and parylene can also be used as a mask.

[0088] The double-sided copper-plated board is brushed to roughen and clean the surface of the double-sided board to enhance the bonding strength between the copper surface and the polymer film to be bonded. Then the high polymer film RPET with anti-electroplating performance is hot-pressed on the double-sided copper-clad board by a film laminating machine. The film thickness is about 10um, and the laminating parameters are: pressure 15kg / cm 2 , temperature 95℃, speed 100mm / min.

[0089] (3) Use laser to remove the masking material covering the hole wall area to produce an anti-plating pattern, and use laser to remove the anti-plating masking film layer on the surface of the clamping point of the electroplating fixture to expose the copper surface in the contact area with the electroplating fixture. Use laser to remove the anti-plating masking film layer on the hole area to open a window for the liquid to enter the hole.

[0090] Specifically, this embodiment uses a 20W ultraviolet nanosecond laser machine to remove the RPET film on the hole wall area, the clamping point of the electroplating fixture, and the electroplating balance block. The circuit board is placed on the laser equipment adsorption table, the engineering data of the laser processing is imported, the circuit board is accurately aligned with the processing data, and the RPET film is removed by laser photoetching. After the top surface processing is completed, the circuit board is turned over, and the film on the bottom surface of the copper clad board is removed in the same way. The processing parameters are as follows:

[0091]

[0092]

[0093] (4) Electroplating: depositing copper on the hole wall to thicken the conductive layer to the thickness required for final inspection, forming the hole electroplating layer 6.

[0094] The control point of this step is the electroplating time. At this time, except for the hole wall and the electroplating balance block, all areas on the board are covered with a mask. The mask is an insulating material. Although it is in contact with the electroplating solution, copper cannot be deposited on the surface. Therefore, only the hole wall and the balance block can deposit copper during the electroplating process. If the electroplating time is sufficient, a copper deposition layer of sufficient thickness can be obtained on the hole wall, achieving the purpose of selectively controlling the copper thickness of the hole wall.

[0095] Since the electroplating area is small, a small current density is used for electroplating in this step. The electroplating parameters are: 10ASF*120min, and the thickness of the coating in the hole is about 25um.

[0096] (5) Electroplating a metal having corrosion resistance and solderability on the hole wall to form solderability metal 7.

[0097] The electroplated metal needs to have the corrosion resistance required in step (7). At the same time, it should also protect the corresponding area during transportation and storage of the circuit board and increase the solderability of the welding area during assembly of the circuit board.

[0098] The present invention uses non-photosensitive anti-plating materials with good masking ability, which can withstand longer electroplating time and more stringent plating solutions and operating conditions. In addition, because the other areas of the board surface are masked by a polymer film, the technology of the present invention can only deposit metal on the hole wall and the surface of the electroplating balance block, and the plating area is relatively small, saving materials. Therefore, more types of metals that are both corrosion-resistant, protective, and weldable can be selected, such as nickel and gold.

[0099] According to the requirements of electroplating area and coating thickness, soft gold is electroplated on the hole wall and pad as a solderable metal protective layer. Electroplating soft gold parameters: 0.3ASD*10min, the coating thickness in the hole is about 2um.

[0100] (6) Use laser to remove the organic film material on the non-circuit area to expose the non-circuit copper and obtain an anti-etching mask pattern.

[0101] Specifically, this embodiment uses a 20W ultraviolet nanosecond laser machine to remove the RPET film on the non-circuit area, places the circuit board on the laser equipment adsorption table, imports the engineering data of laser processing, accurately aligns the circuit board with the processing data, and removes the RPET film by laser photoetching. After the top surface processing is completed, turn the circuit board over, and use the same method to remove the film on the bottom surface of the copper clad board. The processing parameters are as follows:

[0102] Power / W Frequency / kHz Pulse width / ns Processing speed / mm / s Processing times 5.5 150 20 800 1

[0103] (7) Laser removes the copper foil on the non-circuit area to produce a conductive pattern.

[0104] Specifically, this embodiment uses a 20W infrared nanosecond laser to remove the copper foil on the non-circuit area to produce a conductive pattern. In this embodiment, the conductive layer in the laser-removed area is the original copper foil with uniform thickness, which greatly reduces the difficulty of laser processing. The processing parameters are as follows:

[0105] stage Power / W Frequency / kHz Pulse width / ns Processing speed / mm / s Processing times Remark Envelope insulation 15 200 100 800 1 Focus Striping and Sharding 15 200 100 800 1 Focus Heating stripping 30 200 100 900 1 Defocus

[0106] (8) coating and curing a non-photosensitive solder resist on the non-circuit area at one time to form a solder resist material layer 8;

[0107] The prior art generally uses liquid photosensitive ink as solder resist, which contains adhesives and photopolymerizable monomers. The pattern forming process is very complicated and requires multiple processes such as coating, pre-baking, exposure, development, and curing. Moreover, it is expensive, has low resolution, and is difficult to ensure the coating quality between fine pitch connection pads. The solder resist of the present invention does not need to have photosensitive properties. General pre-coated pressure-sensitive coating films and heat-sensitive coating films can meet the requirements. It is cheap and has high resolution, and can produce fine pattern structures. In addition, the present invention uses hot pressing coating, which does not require an additional curing process. The solder resist pattern is left to be produced on-site by laser before component assembly, and the process is simple. For example, a heat-pressed paste with a thickness of 20μm-200μm of thermal-sensitive PI, PVC, PC, PET, and PP films is used as a solder resist, and parylene can also be used as a solder resist.

[0108] Use electrostatic spraying process to spray KSM-386 thermosetting ink produced by Suzhou Guangxin Photosensitive New Materials Co., Ltd. on the non-circuit area of ​​the double-sided board, and fully cure it at one time. The curing conditions are: 150℃*30min, and the thickness of the solder mask ink is about 20um.

[0109] (9) using laser to remove organic materials on the conductor of the welding area at the assembly site to produce a solder resist pattern, and cleaning and solderability treatment of the welding area surface to form a cleaned and solderability treated surface 9;

[0110] This step can be completed in one step on the same equipment, or it can be carried out in two steps on different equipment, namely, the first step: making a solder resist pattern and generating a welding area: using a laser to selectively photoetch to remove the solder resist coating on the welding area, making a solder resist pattern and generating a welding area; the second step, cleaning and solderability treatment of the welding area surface, using another laser to remove the solder resist residue on the surface of the welding area, and slightly photoetching the metal surface layer of the welding area to remove metal oxides, exposing a fresh metal surface, and creating solderability that is easily wetted by molten solder.

[0111] Specifically, the RPET film on the conductor in the welding area is first removed by laser, and the removal parameters are the same as step (6). Then, a UV picosecond laser with a smaller single pulse energy is used to clean and treat the welding area for weldability. The processing parameters are as follows:

[0112] Power / W Frequency / kHz Pulse width / ps Processing speed / mm / s Processing times 10 1000 12 2000 1

[0113] (10) Solder 10 is added to the connection pad, and components 11 are mounted and inserted, followed by reflow soldering and selective wave soldering.

[0114] Example 2

[0115] In the electronics industry, copper clad laminate is often used as a basic material to make circuit boards. The copper clad laminate includes an insulating substrate 1 and a copper layer 2 of the copper clad laminate.

[0116] This embodiment takes a four-layer circuit board with inner layer circuits fabricated as an example, and the specific processing steps are as follows:

[0117] (1) The copper-clad laminate substrate of the circuit board includes an insulating substrate 1 and a copper layer 2 of the copper-clad laminate. The copper-clad laminate is drilled, and an initial conductive layer 3 is deposited on the semi-finished product of the four-layer circuit board after the drilling. Copper is electroplated to a thickness that can withstand subsequent processes to form an electroplated thin copper 4.

[0118] The purpose of making thin copper on the initial conductive layer is to increase the reliability of the process. Its thickness can reach the lower limit of ensuring the reliability of the process. Specifically, the circuit board with holes drilled is brushed to remove the burrs at the hole mouth and clean the board surface. Then, copper electroplating is carried out after removing the glue residue. The electroplating parameters are: 10ASF*35min, and the thickness of the coating in the hole is about 5um.

[0119] (2) A non-photosensitive polymer film is attached to the board surface as an anti-plating masking film 5.

[0120] The four-layer circuit board after thin copper electroplating is brushed and dried, and then hot-pressed to bond the anti-electroplating polymer film RPP. Bonding parameters: pressure 15kg / cm 2 , film thickness is about 10um, temperature is 95℃, speed is 100mm / min.

[0121] (3) Use laser to remove the masking material covering the hole wall area to produce an anti-plating pattern, and use laser to remove the anti-plating masking film layer on the surface of the clamping point of the electroplating fixture to expose the copper surface in the contact area with the electroplating fixture.

[0122] Specifically, this embodiment uses a 20W ultraviolet nanosecond laser machine to remove the RPP film on the hole wall area, the clamping point of the electroplating fixture, and the electroplating balance block. The circuit board is placed on the laser equipment adsorption table, the engineering data of the laser processing is imported, the circuit board is accurately aligned with the processing data, and the RPP film is removed by laser photoetching. After the top surface processing is completed, the circuit board is turned over and the bottom surface film is removed in the same way. The processing parameters are as follows:

[0123] Power / W Frequency / kHz Pulse width / ns Processing speed / mm / s Processing times 6.5 200 20 600 1

[0124] (4) Electroplating: depositing copper on the hole wall to thicken the conductive layer to the thickness required for final inspection, forming the hole electroplating layer 6.

[0125] The control point of this step is the electroplating time. At this time, except for the hole wall and the electroplating balance block, all areas on the board are covered with a mask. The mask is an insulating material. Although it is in contact with the electroplating solution, copper cannot be deposited on the surface. Therefore, only the hole wall and the balance block can deposit copper during the electroplating process. If the electroplating time is sufficient, a copper deposition layer of sufficient thickness can be obtained on the hole wall, achieving the purpose of selectively controlling the copper thickness of the hole wall.

[0126] Since the electroplating area is small, a small current density is used for electroplating in this step. The electroplating parameters are: 10ASF*120min, and the thickness of the coating in the hole is about 25um.

[0127] (5) Electroplating a metal having corrosion resistance and solderability on the hole wall to form solderability metal 7.

[0128] The electroplated metal needs to have the corrosion resistance required in step (7). At the same time, it should also protect the corresponding area during transportation and storage of the circuit board and increase the solderability of the welding area during assembly of the circuit board.

[0129] The present invention uses non-photosensitive anti-plating materials with good masking ability, which can withstand longer electroplating time and more stringent plating solutions and operating conditions. In addition, because the other areas of the board surface are masked by a polymer film, the technology of the present invention can only deposit metal on the hole wall and the surface of the electroplating balance block, and the plating area is relatively small, saving materials. Therefore, more types of metals that are both corrosion-resistant, protective, and weldable can be selected, such as nickel and gold.

[0130] According to the requirements of electroplating area and coating thickness, soft gold is electroplated on the hole wall and pad as a solderable metal protective layer. Electroplating soft gold parameters: 0.3ASD*15min, the coating thickness in the hole is about 2um.

[0131] (6) Use laser to remove the organic film material on the non-circuit area to expose the non-circuit copper and obtain an anti-etching mask pattern.

[0132] Use laser to remove the RPP anti-plating masking film on the non-circuit area of ​​the four-layer circuit board. The removal method and parameters are the same as step (3).

[0133] (7) Laser removes the copper foil on the non-circuit area to produce a conductive pattern.

[0134] Specifically, this embodiment uses a 20W infrared nanosecond laser to remove the copper foil on the non-circuit area to produce a conductive pattern. In this embodiment, the conductive layer in the laser-removed area is the original copper foil with uniform thickness, which greatly reduces the difficulty of laser processing. The processing parameters are as follows:

[0135]

[0136]

[0137] (8) The entire board is coated with a non-photosensitive solder resist and cured at one time to form a solder resist material layer 8.

[0138] In this embodiment, a PI film is laminated on the entire four-layer circuit board as a solder resist. Specifically, before laminating the PI film, a laser is used to remove all remaining anti-plating masking films on the board surface. The removal method and parameters are the same as step (3). Then a laminator is used to laminate the completed circuit board and PI film. The PI film is Kapton HN film produced by DuPont with a thickness of 25um. Silicone rubber pads are used as hot pressing pads during lamination. Before lamination, the RPP masking film needs to be completely removed by laser. According to the material properties, the hot pressing stages and parameters are as follows:

[0139] Serial number Pressing pressure (N / cm2) Pressing temperature(℃) Pressing time (minutes) Phase 1 24 80 15 Phase 2 94 140 25 Phase 3 188 180 25 Phase 4 188 220 60 Phase 5 188→0 220 → Room temperature 45

[0140] (9) using laser to remove organic materials on the conductor of the welding area at the assembly site to produce a solder resist pattern, and cleaning and solderability treatment of the welding area surface to form a cleaned and solderability treated surface 9;

[0141] This step can be completed in one step on the same equipment, or it can be carried out in two steps on different equipment, namely, the first step: making a solder resist pattern and generating a welding area: using a laser to selectively photoetch to remove the solder resist coating on the welding area, making a solder resist pattern and generating a welding area; the second step, cleaning and solderability treatment of the welding area surface, using another laser to remove the solder resist residue on the surface of the welding area, and slightly photoetching the metal surface layer of the welding area to remove metal oxides, exposing a fresh metal surface, and creating solderability that is easily wetted by molten solder.

[0142] Specifically, this embodiment uses a 20W ultraviolet nanosecond laser machine to make the solder mask pattern. The circuit board is placed on the laser equipment adsorption table, the engineering data of the laser processing is imported, the circuit board is accurately aligned with the processing data, and the laser photoetching PI forms the solder mask pattern. After the top surface processing is completed, the circuit board is turned over, and the bottom surface solder mask pattern is completed in the same way. The processing parameters are as follows:

[0143] Power / W Frequency / kHz Pulse width / ns Processing speed / mm / s Processing times 6 200 20 600 1

[0144] The welding area was cleaned and welded using a UV picosecond laser. The processing parameters were as follows:

[0145] Power / W Frequency / kHz Pulse width / ps Processing speed / mm / s Processing times 10 1000 12 2000 1

[0146] (10) Solder 10 is added to the connection pad, and the component 11 is mounted and inserted, and then reflow soldering and selective wave soldering are performed.

[0147] The technical solutions disclosed and proposed by the present invention can be realized by those skilled in the art by referring to the contents of this article and appropriately changing the conditions, routes and other links. Although the methods and preparation techniques of the present invention have been described through preferred embodiments, relevant technicians can obviously modify or re-combine the methods and technical routes described herein without departing from the content, spirit and scope of the present invention to realize the final preparation technology. It should be particularly noted that all similar substitutions and modifications are obvious to those skilled in the art, and they are all considered to be included in the spirit, scope and content of the present invention.

Claims

1. A method for manufacturing a circuit board by laser processing of electroplating hole anti-plating and conductive pattern, Features: Drill holes and deposit a thin metal layer on the hole and board surface, apply a non-photosensitive masking film, remove the masking layer covering the hole wall with a laser to expose the hole wall, then only electroplate and thicken the conductive layer inside the hole, electroplate a solderable metal on the hole wall, use a laser to make a conductive pattern, apply a non-photosensitive solder resist on the non-circuit area, use a laser to make a solder resist pattern at the assembly site, and clean and treat the surface of the welding area for solderability; The steps are: (1) Depositing the initial conductive layer on the finished product of the double-sided, multi-layer circuit board with completed drilling, and electroplating copper to a thickness that can withstand subsequent processes; (2) A non-photosensitive organic film is attached to the board surface as an anti-plating masking film; (3) Using a laser to remove the masking material covering the hole wall area to produce an anti-plating pattern, and using a laser to remove the anti-plating masking film layer on the surface of the clamping point of the electroplating fixture to expose the copper surface in the contact area with the electroplating fixture; (4) Electroplating: depositing copper on the hole wall to thicken the conductive layer to the thickness required for final inspection; (5) Electroplating, depositing solderable metal on the hole wall; (6) Using laser to remove the anti-plating masking film on the non-circuit area; when using laser to remove the anti-plating masking film on the non-circuit area, when the ratio of the perimeter of the area to be removed to the diameter of the focused laser beam is less than 10, the masking film on the surface of the substrate and the conductive metal copper thereunder are removed by point-by-point and line-by-line photolithography using a focused laser beam; when the ratio of the perimeter of the area to be removed to the diameter of the focused laser beam is greater than 15, first use a focused laser beam along the inner side of the envelope of the area to be removed and use the envelope as the boundary to remove the masking film on the surface of the substrate and the conductive metal copper thereunder point-by-point photolithography until a closed adiabatic channel is formed around the unremoved portion of the area, and then use a laser beam with a lower optical power density than the minimum optical power density required to remove the metal copper but with a larger diameter to heat the unremoved area, so that the anti-plating masking film on it and the conductive metal copper thereunder are simultaneously separated from the surface of the substrate and removed; (7) Use laser to remove the copper foil in the non-circuit area to produce a conductive pattern; (8) Apply non-photosensitive solder resist to the non-circuit area and cure it once; (9) Use laser to remove organic materials on the conductors in the welding area at the assembly site, create solder mask patterns, and clean and treat the surface of the welding area for solderability; (10) Add solder to the connection pads, mount and insert components, and perform reflow soldering and / or wave soldering.

2. The method according to claim 1, Its characteristics are: The non-photosensitive organic film in step (2) is composed of several layers of different shapes and compositions, among which the layer in contact with the circuit board has viscosity and fluidity.

3. The method according to claim 1, Its characteristics are: The non-photosensitive organic film in step (2) has anti-plating / anti-welding properties, and the anti-plating masking film covering the circuit area does not need to be removed and can serve as a solder resist film in the circuit area.

4. The method according to claim 1, Its characteristics are: Step (2) includes depositing non-photosensitive organic film-forming substances on the plate surface and hole walls using electrophoresis, vacuum coating, and vapor deposition technology; including using existing technology to coat liquid photosensitive materials and dry photosensitive films.

5. The method according to claim 1, Its characteristics are: The coating method in step (8) includes spray printing and screen printing; the coating thickness is such that after solidification, it is flush with the masking film on the circuit or according to the design requirements.

6. The method according to claim 1, Its characteristics are: Steps (7) and (8) include using a laser to remove all remaining anti-plating masking films on the board surface after the conductive pattern is formed.

7. The method according to claim 1, 5 or 6, Its characteristics are: Steps (7) and (8) include using laser to remove all remaining anti-plating masking films on the board surface, and then applying existing technology and materials to coat the entire board surface and cure the photosensitive and non-photosensitive solder resist in one go.

8. The method according to claim 1, Its characteristics are Step (8) includes applying existing technology and materials to fully coat and cure the photosensitive and non-photosensitive solder resist at one time at the bare board manufacturing site, removing the organic material on the conductor of the welding area with a laser, manufacturing the solder resist pattern, and cleaning the surface of the welding area.