A thin strip tail coiling control process
By distinguishing the hysteresis rate according to the thickness and material code of the strip steel and adjusting the roller speed during the coiling process, the problem of thin-spec strip steel and silicon steel tail-mounted sleeves is solved, the coil pass rate and production efficiency are improved, and the product quality is ensured .
Patent Information
- Application Number
- CN202111081973.9
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2021-09-15
- Publication Date
- 2024-11-05
- Estimated Expiration
- 2041-09-15
AI Technical Summary
During the thinning process of hot continuous rolling products, thin strip steel and silicon steel tails with a thickness of ≤2.3mm are often sleeved, resulting in a decrease in the roll pass rate and affecting production quality and efficiency.
By distinguishing different steel types according to the thickness and material code of the strip steel during the winding process, the G roller lag rate is controlled in segments, and the roller speed when the tail of the strip steel reaches different frames is adjusted to ensure a smooth transition of tail tension and avoid a smooth start. set.
It effectively solves the problem of tail sleeves of thin-spec strip steel and silicon steel, improves the roll pass rate, avoids roll unloading abnormalities and stand-alone production, and improves production efficiency and product quality.
Abstract
Description
Technical Field
[0001] The invention belongs to the technical field of hot-rolled strip steel coiling equipment, and in particular relates to a tail coiling control process for thin-gauge strip steel. Background Art
[0002] As hot-rolled products continue to thin, the tail of thin strip steel and silicon steel with a thickness of ≤2.3mm often gets unwound during coiling, which seriously affects the quality of the steel coil, reduces the coil shape qualification rate, and affects the production quality of the next process. Because the coiler coils the abnormal tail coil, it cannot be unloaded normally, and is forced to produce on a single machine, reducing production efficiency. Summary of the invention
[0003] In order to overcome the deficiencies of the prior art and solve the technical problems such as abnormal unloading and decreased coil shape qualification rate caused by the tail coiling of existing thin-gauge strip steel and silicon steel, the present invention provides a thin-gauge strip tail coiling control process.
[0004] The present invention is achieved through the following technical solutions.
[0005] A thin-gauge strip tail coiling control process, wherein:
[0006] When the coiling thickness is less than or equal to 2.3 mm or the material code of the coiled strip is equal to the material code of silicon steel, when the tail of the strip reaches the finishing rolling F2 stand, the G roller speed V1=K1×D×ω×π / 60; when the tail of the strip continues to move forward and reaches the finishing rolling F6 stand, the G roller speed V2=K2×D×ω×π / 60;
[0007] Where: K1 is the first stage hysteresis rate; K2 is the second stage hysteresis rate; D is the roller diameter of the lower pinch roller; ω is the actual angular velocity of the lower pinch roller;
[0008] When the coiling thickness is greater than 2.3 mm and the material code of the coiled strip is not equal to the material code of silicon steel, the lag rate of the G roller table lag speed ranges from 90% to 70%.
[0009] Furthermore, the value range of the first-stage hysteresis rate K1 is 70%~60%; the value range of the second-stage hysteresis rate K2 is 50%~40%.
[0010] The present invention adopts a method of stepwise input of the hysteresis rate of the coiling G roller for different steel thicknesses, solves the problem of tail unwinding of hot-rolled thin-gauge strip steel and silicon steel, coordinates the tail tension of the coiling, allows the tail of the strip to enter the reel flatly, and smoothly completes the coiling process, avoiding problems such as abnormal unloading of the coil and unqualified coil quality at the factory caused by tail unwinding.
[0011] Compared with the prior art, the present invention has the advantages of reasonable design, high working efficiency, good product quality, and the ability to effectively avoid product defects. DETAILED DESCRIPTION
[0012] The present invention is further described in detail below in conjunction with embodiments.
[0013] A thin-gauge strip tail coiling control process, wherein:
[0014] When the coiling thickness is less than or equal to 2.3 mm or the material code of the coiled strip is equal to the material code of silicon steel, when the tail of the strip reaches the finishing rolling F2 stand, the G roller speed V1=K1×D×ω×π / 60; when the tail of the strip or silicon steel continues to move forward and reaches the finishing rolling F6 stand, the G roller speed V2=K2×D×ω×π / 60;
[0015] Among them: K1 is the first-stage hysteresis rate, ranging from 70% to 60%; K2 is the second-stage hysteresis rate, ranging from 50% to 40%; D is the roller diameter of the lower pinch roller; ω is the actual angular velocity of the lower pinch roller;
[0016] When the coiling thickness is greater than 2.3 mm and the material code of the coiled strip is not equal to the material code of silicon steel, the lag rate of the G roller table lag speed ranges from 90% to 70%.
[0017] The working process of the present invention is as follows:
[0018] According to the steel grade material code and thickness parameters received by the computer from the secondary delivery, if the thickness of the currently coiled strip is less than or equal to 2.3mm, or the material code is equal to the material code of silicon steel, then according to the tracking position of the strip tail, it is calculated to determine that the G roller section takes different hysteresis values when the strip tail reaches the finishing F2 stand and the finishing F6 stand respectively. That is, when the strip or silicon steel tail reaches the finishing F2 stand, the G roller speed V1=K1×D×ω×π / 60; when the strip or silicon steel tail continues to move forward and reaches the finishing F6 stand, the G roller speed V2=K2×D×ω×π / 60;
[0019] Among them: K1 is the first-stage hysteresis rate, ranging from 70% to 60%; K2 is the second-stage hysteresis rate, ranging from 50% to 40%; D is the roller diameter of the lower pinch roller; ω is the actual angular velocity of the lower pinch roller;
[0020] If the coiling thickness is greater than 2.3mm, and the material code of the current coiled strip is not equal to the material code of silicon steel, the program executes the original control logic to coil the steel. When the coiling G roller table is at a lag speed, the lag rate ranges from 90% to 70%.
[0021] The present invention makes full use of the characteristics of the coiler, distinguishes the steel types according to the target thickness of the rolled strip and the material code, and selects different G roller hysteresis rates. A segmented control method is adopted in the coiling process to complete the smooth transition of the tail tension, and effectively solves the problem of tail sheathing of thin-gauge strip steel and silicon steel, avoids the abnormal coil shape caused by tail sheathing, affects the normal unloading of the coil, causes the single coiling machine production, and reduces the production efficiency; and reduces the product coil shape quality, improves the qualified rate of steel coils, reduces the amount of downgraded or whole coil scrapped, and achieves good benefits.
[0022] The above is only a specific embodiment of the present invention, but the protection scope of the present invention is not limited thereto. Any changes or substitutions that can be easily thought of by a person skilled in the art within the technical scope disclosed by the present invention should be included in the protection scope of the present invention. Therefore, the protection scope of the present invention shall be based on the protection scope of the claims.
Claims
1. A thin-gauge strip tail coiling control process, characterized in that: When the coiling thickness is less than or equal to 2.3 mm or the material code of the coiled strip is equal to the material code of silicon steel, when the tail of the strip reaches the finishing rolling F2 stand, the G roller speed V1=K1×D×ω×π / 60; when the tail of the strip continues to move forward and reaches the finishing rolling F6 stand, the G roller speed V2=K2×D×ω×π / 60; Wherein: K1 is the first-stage hysteresis rate, and the value range of the first-stage hysteresis rate K1 is 70%~60%; K2 is the second-stage hysteresis rate, and the value range of the second-stage hysteresis rate K2 is 50%~40%; D is the roller diameter of the lower pinch roller; ω is the actual angular velocity of the lower pinch roller; When the coiling thickness is greater than 2.3 mm and the material code of the coiled strip is not equal to the material code of silicon steel, the lag rate of the G roller table lag speed ranges from 90% to 70%.