A demetallized dynamically thermally tunable triple narrow-band terahertz perfect absorber
By designing a demetallized dynamically thermally adjustable three-narrowband terahertz perfect absorber, using vanadium dioxide and silica materials, it achieves dual-functional performance of low-temperature transparency and high-temperature complete absorption, solving the problem of wave absorption in the existing technology. It solves the problem of insufficient sensor performance and is suitable for the fields of thermal sensors and photoelectric detection.
Patent Information
- Application Number
- CN202111387698.3
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2021-11-22
- Publication Date
- 2024-10-15
- Estimated Expiration
- 2041-11-22
AI Technical Summary
Existing perfect terahertz absorbers usually require metal materials, have complex structures and are difficult to achieve dual-functional performance of transparency at low temperatures and high absorption at high temperatures. They also lack flexible temperature response and multi-peak modulation capabilities, making it difficult to be widely used in thermal sensing devices. and photoelectric detection fields.
A demetallized dynamic thermally adjustable three-narrow-band terahertz perfect absorber is designed, which adopts a three-layer micron-scale thin film structure. The top and bottom layers are vanadium dioxide, and the middle layer is silicon dioxide. The structural unit consists of an inner and outer square ring. It is constructed and equipped with asymmetric air cutting grooves to achieve narrow bandwidth and multi-peak modulation through temperature adjustment. The material is simple and easy to process.
It achieves transparency of terahertz waves at low temperatures and complete absorption at high temperatures. It has strong temperature-controlled absorption intensity and high refractive index sensitivity. It is suitable for thermal sensing devices, thermal modulators and photoelectric detection fields, and has a simple structure and is easy to produce.
Smart Images

Figure CN113948876B_ABST
Abstract
Description
Technical Field
[0001] The invention belongs to the field of terahertz perfect absorbers, and in particular relates to a demetallized dynamically heat-adjustable three-narrow-band terahertz perfect absorber. Background Art
[0002] Vanadium dioxide is a thermotropic phase change material. When the phase transition temperature is higher than 68°C, VO2 will undergo a reversible phase transition from dielectric phase to metallic phase, and the change in resistivity before and after the phase transition can reach up to 5 orders of magnitude. Terahertz waves are electromagnetic waves with a frequency between 0.1 and 10 THz. It has the characteristics of high signal-to-noise ratio and strong penetration, and is widely used in the fields of communications and non-destructive testing. Terahertz absorbers have the ability to manipulate the amplitude, phase and propagation direction of terahertz waves. They are usually micron-scale arrays composed of metal and dielectric materials. Perfect absorption, polarization conversion and phase delay in the terahertz band can be achieved through the reasonable design of unit resonators, dimensions or media.
[0003] The perfect absorber generally adopts a three-layer structure. The top layer is a periodic metal resonant structure, the middle layer is a dielectric or insulator material with a certain thickness, and the bottom layer is a continuous metal film with a thickness much greater than the skin depth of electromagnetic waves in metal, which can play a role in blocking the transmission of electromagnetic waves. By rationally optimizing the structural parameters, the operating wavelength of the device can be changed and the absorption can be adjusted. The feasibility of achieving perfect absorption of electromagnetic waves using a three-layer composite structure (metal-dielectric-metal) was first proposed in 2008, and a single narrow-band perfect absorption peak was obtained at 11.5GHz.
[0004] The dynamic thermally adjustable three-narrowband perfect absorber proposed in the present invention has the advantages of flexible design, adjustable response, small thickness, strong absorption, etc. Through the reasonable design of the structure, it can achieve extremely narrow bandwidth and multi-peak modulation, and can be widely used in thermal sensing devices, thermal modulators, photoelectric detection and other fields. Summary of the invention
[0005] The purpose of the present invention is to provide a demetallized dynamically heat-adjustable three-narrowband terahertz perfect absorber, which has the dual functions of high terahertz wave transmission at low temperature and high absorption at high temperature. The absorber can be effectively used in thermal sensor devices, thermal modulators, and photoelectric detection fields.
[0006] To achieve the above object, the technical solution adopted by the present invention is:
[0007] A demetallized dynamic thermally adjustable three-narrowband terahertz perfect absorber is composed of three layers of micron-level thin films, the top layer is a vanadium dioxide pattern layer, the middle layer is a silicon dioxide dielectric layer, and the bottom layer is a vanadium dioxide substrate layer. The vanadium dioxide pattern layer is formed by periodic arrangement of structural units, each of which is composed of an inner square ring and an outer square ring, the inner square ring is arranged inside the outer square ring, and the edges on both sides of the outer square ring are provided with asymmetric air grooves; the absorber can generate three absorption peaks, the positions of the peaks are constant, and when the temperature is equal to 73°C, the intensity of the three absorption peaks is 100%.
[0008] Preferably, the thickness of the vanadium dioxide pattern layer is 0.5 μm-2 μm, the thickness of the silicon dioxide dielectric layer is 8 μm-20 μm, the thickness of the vanadium dioxide base layer is 3 μm-8 μm, and the dielectric constant of the silicon dioxide dielectric layer is 3.09-3.73.
[0009] Preferably, the period P of the structural unit along the x and y axes is x =P y =49μm-51μm.
[0010] Preferably, the inner ring side length of the inner square ring is l1=15μm-16μm, the outer ring side length of the inner square ring is l2=20μm-29μm, the inner ring side length of the outer square ring is l3=33μm-41μm, the outer ring side length of the outer square ring is l4=46μm-48μm, the width of the air groove opened on the edge of the outer square ring is 3.5μm-4.5μm, the air groove is opened in the center of one side of the outer square ring, and the corresponding other side is offset upward by 2.5μm-3.5μm.
[0011] A demetallized dynamically thermally tunable triple narrowband terahertz perfect absorber for applications in thermal sensing devices, thermal modulators, and photoelectric detection.
[0012] Beneficial Effects
[0013] The absorber provided by the present invention is a perfect absorber, which is composed of three layers of micron-sized thin films and uses only two materials, vanadium dioxide and silicon dioxide. Vanadium dioxide is arranged on the top and bottom layers, and the middle medium layer is silicon dioxide. The materials used are simple, and metal is not required. The use of metal and complex structure are abandoned, and demetallization is achieved. Perfect absorption can be achieved without the use of metal. In addition, due to demetallization and simple structure, the thickness is in the micron level, which is easy to process and more conducive to production.
[0014] The perfect absorber provided by the present invention has dual functions: at low temperatures, the entire device is transparent in the terahertz band; at high temperatures, the absorber can produce three narrow-band perfect absorption peaks, which can completely absorb electromagnetic waves, making the reflection R 0 and the absorption A close to 100%, thereby achieving complete absorption; the absorber can produce a large-area temperature response through dynamic temperature regulation, thereby controlling the intensity of the absorption peak.
[0015] The structural unit of the present invention is composed of double rings of different sizes. Asymmetric air grooves are opened on the ring edges of the outer square ring on both sides. The air grooves and their asymmetric structure can effectively improve the electromagnetic wave absorption intensity. The structures of the inner and outer square rings interact and influence each other, which can generate LC resonance and electric dipole resonance, and resonance extremes appear at certain frequencies, thereby generating three narrow-band absorption peaks.
[0016] The absorber of the present invention can generate three absorption peaks, and the positions of the peaks are constant. When the temperature is equal to 73°C, the intensity of the three absorption peaks is 100%. The position of the resonance absorption peak can be adjusted by setting the thickness of the intermediate medium layer. Therefore, the absorber of the present invention can effectively adjust the intensity and position of the absorption peak by adjusting different temperatures or geometric parameters. At room temperature, that is, below the phase transition point of 68°C, the absorption is very weak, and the device presents high transmittance, that is, terahertz transparency. When the temperature rises, the absorption intensity gradually increases, and when the phase transition point is 68°C, three narrow-band perfect absorption is formed.
[0017] The absorber of the present invention has strong temperature-controlled absorption intensity and high refractive index sensitivity, and can be applied in the fields of dynamic thermal sensor devices, thermal modulators, and photoelectric detection. BRIEF DESCRIPTION OF THE DRAWINGS
[0018] Figure 1 It is a schematic diagram of the overall structure of the present invention;
[0019] Figure 2 A top view of the structural unit of the present invention
[0020] Figure 3 It is a three-dimensional diagram of the structural unit of the present invention;
[0021] Figure 4 is a response diagram of the absorption spectrum of the absorber of the present invention to different temperatures;
[0022] Figure 5 This is the impedance matching diagram corresponding to the absorber of the present invention at 73°C;
[0023] Figure 6 A comparison diagram of the electric field distribution on the surface of the intermediate medium of the absorber of the present invention at the absorption peak and the current distribution formed on the upper and lower surfaces of the medium;
[0024] Figure 7is a response diagram of the absorption spectrum of the absorber of the present invention to the geometric parameter l2 of the top pattern;
[0025] Figure 8 is a response diagram of the absorption spectrum of the absorber of the present invention to the geometric parameter l3 of the top pattern;
[0026] Fig. 9 is a response diagram of the absorption spectrum of the absorber of the present invention to the geometric parameter l4 of the top pattern;
[0027] Fig.10 The absorption spectrum of the absorber of the present invention responds to the thickness t2 of the intermediate dielectric layer.
[0028] Fig.11 is a response diagram of the absorption spectrum of the absorber of the present invention to the change of the dielectric constant;
[0029] Fig.12 is a response diagram of the absorption spectrum of the absorber of the present invention to the change of the incident angle;
[0030] Fig.13 The diagram is a response diagram of the absorption spectrum of the absorber of the present invention to the changes in different environments in which the device is located. DETAILED DESCRIPTION
[0031] The technical solution of the present invention is further described below in conjunction with the embodiments, but is not limited thereto. Any modification or equivalent replacement of the technical solution of the present invention without departing from the spirit and scope of the technical solution of the present invention should be included in the protection scope of the present invention.
[0032] Example 1
[0033] The absorber is Figure 1-3 As shown, the bottom layer of vanadium dioxide is 4 μm thick. The middle dielectric layer is silicon dioxide, which has a dielectric constant of 3.73 and a thickness of 16 μm. The top layer of vanadium dioxide is 2 μm thick. The period P along the x and y axes is x =P y =50μm, among which l1=16μm, l2=26μm, l3=33μm, l4=48μm, the width of the outer ring air groove is 4μm, centered on the left side and offset upward by 3μm on the right side.
[0034] The dielectric constant of vanadium dioxide is obtained using effective dielectric theory in the form of:
[0035] The dielectric constant of the dielectric phase vanadium dioxide is ε i =9, the dielectric constant of the metallic phase of vanadium dioxide is obtained from the Drude model, that is, Where τ is the relaxation time, f is the volume fraction of the vanadium dioxide metal phase in the entire lattice,
[0036] f=f max {1-1 / [1+Exp[(TT c ) / ΔT]]}, where T c is the phase transition temperature and ΔT is the thermal hysteresis temperature.
[0037] Example 2
[0038] The absorber is Figure 1-3 As shown, the bottom layer of vanadium dioxide is 3um thick. The middle dielectric layer is silicon dioxide, with a dielectric constant of 3.09 and a thickness of 8μm. The top layer of vanadium dioxide is 0.5μm thick. The period P along the x and y axes is x =P y =49μm, among which l1=15μm, l2=20μm, l3=33μm, l4=46μm, the width of the outer ring air groove is 3.5μm, centered on the left side and offset upward by 2.5μm on the right side.
[0039] The dielectric constant of vanadium dioxide is obtained using effective dielectric theory in the form of:
[0040] The dielectric constant of the dielectric phase vanadium dioxide is ε i =9, the dielectric constant of the metallic phase of vanadium dioxide is obtained from the Drude model, that is, Where τ is the relaxation time, f is the volume fraction of the vanadium dioxide metal phase in the entire lattice,
[0041] f=f max {1-1 / [1+Exp[(TT c ) / ΔT]]}, where T c is the phase transition temperature and ΔT is the thermal hysteresis temperature.
[0042] Example 3
[0043] The absorber is Figure 1-3 As shown, the bottom layer of vanadium dioxide is 8 μm thick. The middle dielectric layer is silicon dioxide, which has a dielectric constant of 3.73 and a thickness of 20 μm. The top layer of vanadium dioxide is 2 μm thick. The period P along the x and y axes is x =P y =51μm, among which l1=17μm, l2=29μm, l3=41μm, l4=48μm, the width of the outer ring air groove is 4.5μm, centered on the left side and offset upward by 3.5μm on the right side.
[0044] The dielectric constant of vanadium dioxide is obtained using effective dielectric theory in the form of:
[0045] The dielectric constant of the dielectric phase vanadium dioxide is ε i =9, the dielectric constant of the metallic phase of vanadium dioxide is obtained from the Drude model, that is, Where τ is the relaxation time, f is the volume fraction of the vanadium dioxide metal phase in the entire lattice, and f = f max {1-1 / [1+Exp[(TT c ) / ΔT]]}, where T c is the phase transition temperature and ΔT is the thermal hysteresis temperature.
[0046] Test example:
[0047] 1. The influence of temperature on the absorption spectrum of the absorber
[0048] Figure 4 The three narrow-band absorption spectra of the absorber at different temperatures. As the temperature increases, the intensity of the three absorption peaks increases from 0 to 100%, and the position of the peaks remains unchanged. Therefore, the intensity of the three narrow-band absorption peaks can be flexibly modulated by setting the temperature.
[0049] When the temperature is much lower than 68°C, the intensity of the three absorption peaks is 0. As the temperature rises, the intensity of the absorption gradually increases. At 63°C, the absorption peak intensities are 0, 0, and 9.10%, respectively. When the temperature rises to 68°C, the corresponding absorption intensities suddenly change to 98.12%, 82.26%, and 93.23%. When the temperature is 73°C, it reaches the optimum and achieves perfect absorption, with corresponding absorption intensities of 95.86%, 100%, and 100%. As the temperature continues to rise, the absorption intensity will decrease. At 78°C, the corresponding absorption intensity drops to 84.71%, 94.92%, and 95.09%. As the temperature continues to increase, the intensity of the absorption peak will decrease, and the three absorption peaks will still maintain a high absorption of more than 80%.
[0050] 2. Impedance matching diagram of absorber in terahertz band
[0051] According to the impedance matching theory, the reflectivity of the absorber can be expressed as
[0052] R=|[Z eff -Z0] / [Z eff +Z0]| 2 , where Z eff is the effective impedance of the absorber, Z o is the air impedance. At the resonant position, the reflectivity R is approximately equal to 0. According to the formula A=1-R, the corresponding absorption A is 1.0. Figure 5The impedance matching diagram of the device at 73°C. At the three resonant frequency positions, the real part of the impedance is equal to 1.0, and the imaginary part is approximately 0, which is equal to the impedance value of air, achieving perfect matching. Therefore, the incident electromagnetic wave completely enters the absorber and is perfectly absorbed.
[0053] 3. Electric field and surface current distribution on the upper and lower surfaces of the middle layer of the absorber
[0054] Figure 6 The electric field and surface current distribution diagram of the upper and lower surfaces of the intermediate dielectric layer. Figure 6 (a) is the electric field distribution at f1 = 0.67 THz. The electric field is mainly distributed on both sides of the outer ring. The perfect absorption peak is generated due to the strong electric field coupling with the adjacent outer ring in the x direction. Figure 6 (d) is the corresponding surface current distribution in the upper layer of the medium, the current direction points to the left, and Figure 6 (g) is the direction of current on the lower surface of the dielectric, which is antiparallel to the direction of current on the upper surface.
[0055] Figure 6 (b) is the electric field distribution at f2 = 2.39 THz, which is due to Figure 6 (b) is caused by the strong dipole resonance between the inner and outer rings. Figure 6 (e) and Figure 6 On both sides of the middle layer of (h), the directions of the induced currents are also antiparallel.
[0056] exist Figure 6 In (c), the electric field is located around the inner and outer rings at f3 = 3.62 THz. Figure 6 The induced currents in (g, i) are in opposite directions, forming a closed loop. The magnetic dipole resonance caused by the closed loop structure confines the electromagnetic waves to the middle dielectric layer.
[0057] 4. The influence of the top layer's geometric parameters l2, l3, and l4 on the absorption spectrum
[0058] Figure 7-9 is the effect of geometric parameters on absorber performance. When l2 increases from 20μm to 29μm, the absorption peak of f2 is Figure 7 There is an obvious red shift in the absorption peak f2. As l2 increases, the inner ring gets closer and closer to the outer ring. They form a structure similar to a parallel plate capacitor. According to the LC resonance theory, the capacitance is inversely proportional to the distance d, so the corresponding absorption peak f2 is red shifted. Figure 8 In the figure, as l3 increases, the outer ring width decreases and the air slot width increases, resulting in redistribution of the coupling energy and a redshift of f2. Fig. 9 In the figure, when l4 increases, the absorption peaks of f1 and f3 move to the low-frequency region, but the absorption of f2 hardly changes.
[0059] 5. Effect of the thickness and dielectric constant of the intermediate dielectric layer on the absorption spectrum
[0060] Figure 10-11 is the effect of the intermediate dielectric layer on absorption. Fig.10 , when the thickness t2 increases from 8μm to 20μm, the resonance absorption peak moves to the low-frequency region. Fig.11 The absorption spectra of different media as the intermediate layer. When the dielectric constant increases from 2.0 to 3.5, the three narrow-band absorption peaks red-shift. The increase in the thickness and dielectric constant of the intermediate medium corresponds to an increase in the optical path of the propagating light. According to the principle of interference cancellation Increasing the optical path length by 6 will lead to an increase in the absorption wavelength, so the absorption spectrum will be red-shifted.
[0061] 6. Effect of incident angle on absorption spectrum
[0062] Fig.12 The influence of different incident angles on the absorber performance. The incident angle is the angle between the incident electromagnetic wave and the z-axis. When the incident angle increases from 0° to 90°, the absorption peak position remains almost unchanged, and f1 and f2 still maintain high absorption. The intensity of f3 decreases at large angles. The reason for the decrease is that when the incident angle is large, the resonance mode changes from symmetric to asymmetric.
[0063] 7. The influence of refractive index on absorption spectrum under different environments
[0064] Fig.13 The effect of refractive index on absorption spectrum under different environments. The refractive index increases from 1.0 to 1.4 with an interval of 0.1. As the refractive index n increases, the three narrow-band perfect absorption peaks show obvious red shifts, and the resonance intensity remains at a high value.
Claims
1. A demetallized dynamically thermally tunable triple narrowband terahertz perfect absorber, characterized in that: It is composed of three layers of micron-scale thin films, the top layer is a vanadium dioxide pattern layer, the middle layer is a silicon dioxide dielectric layer, and the bottom layer is a vanadium dioxide substrate layer. The vanadium dioxide pattern layer is formed by a periodic arrangement of structural units, and each of the structural units is composed of an inner square ring and an outer square ring. The inner square ring is arranged inside the outer square ring, and the edges of the outer square ring on both sides are provided with asymmetric air cuts; at low temperatures, the entire device is transparent in the terahertz band; at high temperatures, the absorber can produce three narrow-band perfect absorption peaks, which can completely absorb electromagnetic waves; the thickness of the vanadium dioxide pattern layer is 0.5μm-2μm, the thickness of the silicon dioxide dielectric layer is 8μm-20μm, the thickness of the vanadium dioxide substrate layer is 3μm-8μm, and the dielectric constant of the silicon dioxide dielectric layer is 3.09-3.73; the inner ring side length of the inner square ring is l 1 =15μm-17μm, the outer ring side length of the inner square ring l 2 =20μm-29μm, the inner ring side length of the outer square ring l 3 =33μm-41μm, the outer ring side length of the outer square ring l 4 =46μm-48μm, the width of the air groove opened on the edge of the outer square ring is 3.5μm-4.5μm, the air groove is opened in the center of one side of the outer square ring, and the corresponding other side is offset upward by 2.5μm-3.5μm.
2. According to claim 1, a demetallized dynamically thermally tunable triple narrow-band terahertz perfect absorber is characterized in that: The structural unit is along x , y Axis period Px = Py =49μm-51μm.
3. Application of the absorber according to any one of claims 1 to 2 in thermal sensors, thermal modulators, and photoelectric detection.
Citation Information
Patent Citations
Light modulation device with dynamic color display based on phase change material and preparation method thereof
CN107942540A
Broadband transfer wave absorber based on mercury thermal expansion and cold contraction regulation and control
CN110635249A
Broadband adjustable wave absorber with vanadium dioxide metamaterial loaded on dielectric layer
CN111525277A
Double-tuned polarization-insensitive electromagnetic induction transparent unit structure
CN111934100A
Switching type broadband terahertz wave absorber based on VO2 and absorption device
CN112490686A