High voltage device test structure and defect detection method

By designing the test structure and defect detection method of high-voltage device, using current sensing resistors to judge the surface defects of the device, the problems of slow detection speed and limitations are solved, and comprehensive detection is achieved. Efficiency and yield.

CN114023723BActive Publication Date: 2024-11-01SHANGHAI HUALI INTEGRATED CIRCUIT CORP
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202111226509.4
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2021-10-21
Publication Date
2024-11-01
Estimated Expiration
2041-10-21

AI Technical Summary

Technical Problem

In high-voltage devices, the metal gate process stability detection sampling speed is low, and the detection is limited, so it cannot be fully detected, resulting in device failure.

Method used

A high-voltage device testing structure is designed, including a low-voltage core area and a medium-voltage IO area. By setting up a test unit and a pad, applying voltage to detect current, and calculating resistance, it is used to determine whether there are defects on the surface, covering all possible residual areas.

Benefits of technology

A large and comprehensive inspection of the stability of metal gate process of high-voltage devices is achieved, which improves detection speed and efficiency, avoids device failure, and improves yield.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN114023723B_ABST
    Figure CN114023723B_ABST
Patent Text Reader

Abstract

The present invention provides a high-voltage device test structure, including: a substrate and a test unit, wherein the substrate includes: a medium-voltage IO area and two low-voltage core areas located on both sides of the medium-voltage IO area; the test unit includes: a first pad, a first test component, a second test component, a second first test component and a second pad connected in sequence, each of the first test components is respectively arranged on each of the low-voltage core areas, and the second test component is arranged on the medium-voltage IO area. The present invention also provides a defect detection method. The present application uses the first test component to detect whether there are Dummy Poly residues on the low-voltage core area and uses the second test component to detect whether there are Dummy Poly residues on the medium-voltage IO area, which can realize a large number of comprehensive tests on the stability of the metal gate process of the high-voltage device, thereby improving the speed and efficiency of the detection.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present application relates to the technical field of semiconductor devices, and in particular to a high-voltage device test structure and a defect detection method. Background Art

[0002] As the size of transistors continues to shrink, HKMG (high-K insulating layer + metal gate) has gradually replaced the original silicon dioxide insulating layer + polysilicon gate configuration, becoming an indispensable part of the process below 28nm.

[0003] The metal gate process usually first uses Dummy Poly to make an amorphous silicon gate (pseudo polysilicon gate), and then removes the Dummy Poly through a dry etching process and a wet etching process in the subsequent process to form a groove, and finally fills the groove with metal material to form a metal gate. However, in high-voltage devices, the thickness difference between the gate oxide layer in the low-voltage core area and the gate oxide layer in the medium-voltage IO area is relatively large, resulting in a relatively large step difference in STI / AA (shallow trench isolation structure / active area). The difference in STI / AA steps will directly affect the process window for Dummy Poly removal. Experimental data show that if the step difference is too large, Dummy Poly will not be completely removed globally, affecting the subsequent filling of metal materials and causing device failure.

[0004] In order to detect the stability of the metal gate process, the only method currently available is defect scanning, but this method has a low sampling speed and cannot perform large-scale and comprehensive detection. Summary of the invention

[0005] The present application provides a high-voltage device test structure and defect detection method, which can solve the problems of low sampling speed of defect scanning and too limited detection when detecting the stability of metal gate process in high-voltage devices.

[0006] On the one hand, an embodiment of the present application provides a high voltage device test structure, including:

[0007] A substrate, the substrate comprising: two low-voltage core regions and one medium-voltage IO region, the low-voltage core regions being located at two opposite sides of the medium-voltage IO region;

[0008] A test unit, the test unit comprising: a first solder pad, a second solder pad, two first test components and one second test component, wherein the first solder pad, the first first test component, the second test component, the second first test component and the second solder pad are connected in sequence, the first test components are respectively arranged on the low-voltage core areas, and the second test components are arranged on the medium-voltage IO area.

[0009] Optionally, in the high-voltage device test structure, the low-voltage core area includes a plurality of first shallow trench isolation structures and a plurality of first active areas, the first shallow trench isolation structures and the first active areas are arranged alternately from left to right, and the first test component is at least arranged on all of the first active areas; the medium-voltage IO area includes a plurality of second shallow trench isolation structures and a plurality of second active areas, the second shallow trench isolation structures and the second active areas are arranged alternately from left to right, and the second test structure covers at least all interfaces between the second shallow trench isolation structures and the second active areas.

[0010] Optionally, in the high-voltage device test structure, the first test component includes: a plurality of first rods arranged side by side and connected in series in sequence.

[0011] Optionally, in the high-voltage device test structure, a width of the first rod portion is 28 nm to 55 nm, and a distance between adjacent first rod portions is 80 nm to 150 nm.

[0012] Optionally, in the high-voltage device test structure, the first rod portion is evenly laid on a surface of the first active area and a surface of the first shallow trench isolation structure.

[0013] Optionally, in the high-voltage device test structure, the second test component includes: a plurality of second rods arranged side by side and connected in series in sequence.

[0014] Optionally, in the high-voltage device test structure, the width of the second rod portion is 80 nm to 900 nm, and the spacing between adjacent second rod portions is 100 nm to 500 nm.

[0015] Optionally, in the high-voltage device test structure, the second rod portion is evenly laid on the surface of the second active area and the surface of the second shallow trench isolation structure, and a second rod portion is correspondingly arranged on all interfaces between the second shallow trench isolation structure and the second active area.

[0016] Optionally, in the high-voltage device test structure, the test unit further includes: a third pad and a fourth pad, the third pad being arranged between the first test component and the second test component, and the fourth pad being arranged between the second test component and the second test component.

[0017] Optionally, in the high-voltage device test structure, both the first test component and the second test component are serpentine structures.

[0018] On the other hand, an embodiment of the present application provides a defect detection method, including:

[0019] Providing the high voltage device test structure;

[0020] Applying a voltage between a first pad of a test unit of the high voltage device test structure and a second pad of a test unit of the test structure;

[0021] detecting currents of a first test component of the test unit and a second test component of the test unit;

[0022] calculating the resistance of the first test component and the second test component according to the current;

[0023] Whether there is a defect on the surface of the high-voltage device is determined according to the value of the resistance.

[0024] The technical solution of this application has at least the following advantages:

[0025] The present application utilizes the first test component to detect whether there are any Dummy Poly residues on the low-voltage core area and utilizes the second test component to detect whether there are any Dummy Poly residues on the medium-voltage IO area. This can achieve large-scale and comprehensive detection of the stability of the metal gate process of high-voltage devices, thereby improving the speed and efficiency of detection, avoiding the situation where high voltage cannot be detected in large quantities and comprehensively, improving the comprehensiveness of device detection, and avoiding the failure of high-voltage devices, thereby ensuring the yield of the device. BRIEF DESCRIPTION OF THE DRAWINGS

[0026] In order to more clearly illustrate the specific implementation methods of the present application or the technical solutions in the prior art, the drawings required for use in the specific implementation methods or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are some implementation methods of the present application. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying any creative work.

[0027] Figure 1 is a schematic top view of a substrate according to an embodiment of the present invention;

[0028] Figure 2 is a schematic cross-sectional view of a substrate according to an embodiment of the present invention;

[0029] Figure 3 is a schematic diagram of a test unit according to an embodiment of the present invention;

[0030] Figure 4 is a schematic top view of a high voltage device test structure according to an embodiment of the present invention;

[0031] Figure 5 is a schematic cross-sectional view of a high voltage device test structure according to an embodiment of the present invention;

[0032] The reference numerals are described as follows:

[0033] 100 - substrate, 10 - low voltage core region, 11 - first active region, 12 - first shallow trench isolation structure, 20 - medium voltage IO region, 21 - second active region, 22 - second shallow trench isolation structure, 23 - interface between the second active region and the second shallow trench isolation structure;

[0034] 200 - test unit, 31 - first pad, 32 - second pad, 33 - third pad, 34 - fourth pad, 40 - first test component, 41 - first rod, 50 - second test rod, 51 - second rod. DETAILED DESCRIPTION

[0035] The following will be combined with the accompanying drawings to clearly and completely describe the technical solutions in this application. Obviously, the described embodiments are part of the embodiments of this application, not all of them. Based on the embodiments in this application, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of this application.

[0036] In the description of the present application, it should be noted that the terms "center", "upper", "lower", "left", "right", "vertical", "horizontal", "inner", "outer", etc., indicating the orientation or positional relationship, are based on the orientation or positional relationship shown in the drawings, and are only for the convenience of describing the present application and simplifying the description, rather than indicating or implying that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore cannot be understood as limiting the present application. In addition, the terms "first", "second", and "third" are used for descriptive purposes only, and cannot be understood as indicating or implying relative importance.

[0037] In the description of this application, it should be noted that, unless otherwise clearly specified and limited, the terms "installed", "connected", and "connected" should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection or an electrical connection; it can be a direct connection, or it can be indirectly connected through an intermediate medium, it can also be the internal connection of two components, it can be a wireless connection, or it can be a wired connection. For ordinary technicians in this field, the specific meanings of the above terms in this application can be understood according to specific circumstances.

[0038] In addition, the technical features involved in the different embodiments of the present application described below can be combined with each other as long as they do not conflict with each other.

[0039] The present application embodiment provides a high voltage device test structure, referring to Figure 4 and Figure 5 , Figure 4is a schematic top view of a high voltage device test structure according to an embodiment of the present invention, Figure 5 1 is a schematic cross-sectional view of a high-voltage device test structure according to an embodiment of the present invention. The high-voltage device test structure includes a substrate 100 and a test unit 200 .

[0040] For details, please refer to Figure 1 and Figure 2 , Figure 1 is a schematic top view of a substrate according to an embodiment of the present invention, Figure 2 is a schematic cross-sectional view of a substrate of an embodiment of the present invention, wherein the substrate 100 comprises: two low-voltage core regions 10 and one medium-voltage IO region 20, wherein the low-voltage core regions 10 are respectively located on two opposite sides of the medium-voltage IO region 20. Furthermore, the low-voltage core region 10 comprises a plurality of first shallow trench isolation structures 12 and a plurality of first active regions 11, wherein the first shallow trench isolation structures 12 and the first active regions 11 are alternately arranged from left to right. Since the first shallow trench isolation structures 12 and the first active regions 11 have different stresses in the substrate, the upper surface of the first shallow trench isolation structure 12 will be slightly higher than the upper surface of the first active region 11. In this embodiment, there may be multiple groups of the first shallow trench isolation structures 12 and the first active regions 11 in the medium-voltage IO region 20, from Figure 1 It can be seen that each group of the first shallow trench isolation structures 12 and the first active areas 11 are arranged front to back. The medium voltage IO area 20 may include a plurality of second shallow trench isolation structures 22 and a plurality of second active areas 21, and the second shallow trench isolation structures 22 and the second active areas 21 are also arranged alternately from left to right.

[0041] For further information, please refer to Figure 3 , Figure 3 It is a schematic diagram of a test unit of an embodiment of the present invention. The test unit 200 includes: a first pad 31, a second pad 32, two first test components 40 and a second test component 50, wherein the first pad 31, the first first test component 40, the second test component 50, the second first test component 40 and the second pad 32 are connected in sequence, and each of the first test components 40 is respectively arranged on each of the low-voltage core areas 10, and the second test component 50 is arranged on the medium-voltage IO area 20. In the present application, the first test component 40 is arranged on the low-voltage core area 10, and the second test component 50 is arranged on the medium-voltage IO area 20, so as to detect whether there is Dummy Poly residue on the low-voltage core area 10 and / or the medium-voltage IO area 20, thereby realizing a large number of and comprehensive tests on the stability of the metal gate process of the high-voltage device, thereby improving the speed and efficiency of the test.

[0042] In the manufacturing process of high-voltage devices, when the dummy poly formed on the first active area 11 and the first shallow trench isolation structure 12 is removed from the low-voltage core area 10 in the back-end process, since the upper surface of the first shallow trench isolation structure 12 is slightly higher than the upper surface of the first active area 11, dummy poly is likely to remain on the upper surface of the first active area 11. In addition, in the medium-voltage IO area 20, after performing the LDD IMP (lightly doped drain ion implantation) process, a small gap will be formed in the second shallow trench isolation structure 22 at the edge of the second active area 21 due to the LDD IMP process, resulting in the second shallow trench isolation structure 22 at the edge of the second active area 21 being lower than the second active area 21, and the thickness of the thicker medium-voltage gate oxide layer will also increase the height difference, making the dummy poly at the edge of the second active area 21 too thick, resulting in the dummy poly at the interface 23 between the second shallow trench isolation structure 22 and the second active area 21 being difficult to remove cleanly. Therefore, in the present invention, reference is made to Figure 4 , the first test component 40 is at least arranged on all the first active regions 11, and the second test structure 50 at least covers all the interfaces 23 between the second shallow trench isolation structures 22 and the second active regions 21. In this way, it can be ensured that the high-voltage device test structure provided by the present invention can cover all surfaces where dummy poly may remain, so that when the high-voltage device test structure is used for detection, all defects on the surface of the high-voltage device can be found quickly and accurately, thereby improving the stability of the metal gate process of the high-voltage device and improving the yield of the high-voltage device.

[0043] Preferably, the first test component 40 and the second test component 50 are both serpentine structures. The first test component 40 and the second test component 50 can both be metal grids.

[0044] Specifically, refer to Figure 3-Figure 5, the first test component 40 includes: a plurality of first rods 41 arranged side by side and connected in series in sequence. The first rods 41 are evenly laid on the surface of the first active area 11 and the surface of the first shallow trench isolation structure 12. The width of the first rod 41 itself and the spacing between adjacent first rods 41 can be adjusted according to the size of the area of ​​the upper surface of the entire substrate of the low-voltage core area 10 and the size of the area of ​​the upper surface of the first active area 11 and the size of the area of ​​the upper surface of the first shallow trench isolation structure 12. The present invention needs to ensure that the first rods 41 are at least evenly laid on the surface of the first active area 11 to facilitate the detection of whether there is dummy poly residue on the surface of the first active area 11. In this embodiment, the width of the first rod 41 can be set to 28nm~55nm, and the spacing between adjacent first rods 41 can be 80nm~150nm.

[0045] For further reference, Figure 3-Figure 5 The second test component 50 includes: a plurality of second rods 51 arranged side by side and connected in series. The second rods 51 are evenly laid on the surface of the second active area 21 and the surface of the second shallow trench isolation structure 22, and one second rod 51 is correspondingly arranged on all the interfaces 23 between the second shallow trench isolation structure 22 and the second active area 21. The width of the second rod 51 itself and the spacing between adjacent second rods 51 can be adjusted according to the size of the area of ​​the upper surface of the entire substrate of the medium voltage IO area 20, the size of the area of ​​the upper surface of the second active area 21 therein, and the size of the area of ​​the upper surface of the second shallow trench isolation structure 22. The present invention needs to ensure that the second rod 51 is at least all the interfaces 23 between the second shallow trench isolation structure 22 and the second active area 21 to facilitate the detection of whether there is dummy poly residue at the interface 23 between the second shallow trench isolation structure 22 and the second active area 21. In this embodiment, the width of the second rod portion 51 is 80 nm to 900 nm, and the distance between adjacent second rod portions 51 is 100 nm to 500 nm.

[0046] On the other hand, an embodiment of the present application provides a defect detection method, including:

[0047] Providing the high voltage device test structure;

[0048] Applying a voltage between a first pad 31 of a test unit 200 of the high voltage device test structure and a second pad 32 of the test unit 200 of the test structure;

[0049] Detecting the current of the first test component 40 of the test unit 200 and the second test component 50 of the test unit 200;

[0050] Calculating the resistance of the first test component 40 and the second test component 50 according to the current;

[0051] Whether there are defects on the surface of the low-voltage core area 10 and the surface of the medium-voltage IO area 20 is determined based on the numerical value of the resistance, that is, whether there are dummypoly residues at the interface 23 of the first active area 11 of the low-voltage core area 10 and / or all the second shallow trench isolation structures 22 and the second active area 21 of the medium-voltage IO area is determined based on the numerical value of the resistance.

[0052] Preferably, the test unit 200 further includes: a third pad 33 and a fourth pad 34, wherein the third pad 33 is disposed between the first first test component 40 and the second test component 50, and the fourth pad 34 is disposed between the second test component 50 and the second first test component 40. The defect detection method provided in the embodiment of the present application may also apply a voltage between the first pad 31 and the third pad 33, detect the current of the first first test component 40, calculate the resistance of the first first test component 40 according to the current, and judge whether there is a defect on the surface of the low-voltage core area 10 (judge whether there is dummy poly residue on the surface of the low-voltage core area 10) according to the value of the resistance. Similarly, the defect detection method provided in the embodiment of the present application may also apply a voltage between the third pad 33 and the fourth pad 34, detect the current of the second test component 50, calculate the resistance of the second test component 50 according to the current, and judge whether there is a defect on the surface of the medium-voltage IO area 20 (judge whether there is dummy poly residue on the surface of the medium-voltage IO area 20) according to the value of the resistance. Similarly, the defect detection method provided in the embodiment of the present application can also apply a voltage between the fourth pad 34 and the second pad 32, detect the current of the second first test component 40, calculate the resistance of the second first test component 40 based on the current, and determine whether there is a defect on the surface of the corresponding low-voltage core area 10 (determine whether there is any dummypoly residue on the surface of the low-voltage core area 10) based on the value of the resistance.

[0053] Obviously, the above embodiments are merely examples for the purpose of clear explanation, and are not intended to limit the implementation methods. For those skilled in the art, other different forms of changes or modifications can be made based on the above description. It is not necessary and impossible to list all the implementation methods here. The obvious changes or modifications derived therefrom are still within the scope of protection created by this application.

Claims

1. A high voltage device test structure, characterized in that: include: A substrate, the substrate comprising: two low-voltage core regions and one medium-voltage IO region, the low-voltage core regions being located at two opposite sides of the medium-voltage IO region; A test unit, the test unit comprising: a first pad, a second pad, two first test components and a second test component, wherein the first pad, the first first test component, the second second test component, the second first test component and the second pad are connected in sequence, each of the first test components is respectively arranged on each of the low-voltage core areas, and the second test component is arranged on the medium-voltage IO area, wherein, The low-voltage core area includes a plurality of first shallow trench isolation structures and a plurality of first active areas, the first shallow trench isolation structures and the first active areas are arranged alternately from left to right, and the first test component is at least arranged on all the first active areas; the medium-voltage IO area includes a plurality of second shallow trench isolation structures and a plurality of second active areas, the second shallow trench isolation structures and the second active areas are arranged alternately from left to right, and the second test structure at least covers all interfaces between the second shallow trench isolation structures and the second active areas; The first test component comprises: a plurality of first rods arranged side by side and connected in series in sequence, the first rods being evenly laid on the surface of the first active region and the surface of the first shallow trench isolation structure; The second test component includes: a plurality of second rod portions arranged side by side and connected in series in sequence, the second rod portions are evenly laid on the surface of the second active area and the surface of the second shallow trench isolation structure, and a second rod portion is correspondingly arranged on all interfaces between the second shallow trench isolation structure and the second active area.

2. The high voltage device test structure according to claim 1, characterized in that: The width of the first rod portion is 28 nm to 55 nm, and the distance between adjacent first rod portions is 80 nm to 150 nm.

3. The high voltage device test structure according to claim 1, characterized in that: The width of the second rod portion is 80 nm to 900 nm, and the distance between adjacent second rod portions is 100 nm to 500 nm.

4. The high voltage device test structure according to claim 1, characterized in that: The test unit further includes: a third pad and a fourth pad, the third pad being arranged between a first one of the first test components and the second one of the second test components, and the fourth pad being arranged between the second one of the first test components and the second one of the first test components.

5. The high voltage device test structure according to claim 1, characterized in that: The first test component and the second test component are both serpentine structures.

6. A defect detection method, characterized in that: include: Providing a high voltage device test structure as claimed in any one of claims 1 to 5; Applying a voltage between a first pad of a test unit of the high voltage device test structure and a second pad of a test unit of the test structure; detecting currents of a first test component of the test unit and a second test component of the test unit; calculating the resistance of the first test component and the second test component according to the current; Whether there is a defect on the surface of the high-voltage device is determined according to the value of the resistance.