Method for manufacturing TiN floating gate on the sidewall of ultra-fast flash memory
By switching between wafer transfer boxes with different contamination risk levels, controlling the deposition and removal of the TiN layer, combined with photolithography definition and shielding layer processing, the contamination problem in the production of ultra-flash memory TiN floating gates is solved and the device quality is improved. Performance and uniformity.
Patent Information
- Application Number
- CN202111399600.6
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2021-11-24
- Publication Date
- 2024-10-29
- Estimated Expiration
- 2041-11-24
AI Technical Summary
In the manufacturing process of TiN floating gate of ultra-flash memory, pollution problems are prone to occur, which affects the uniformity and stability of the device.
The TiN layer is deposited and removed by pre-processing in a high contamination risk level front-opening wafer transfer box (HK FOUP), and cleaning and cleaning are performed in a low contamination risk level front-opening wafer transfer box (HL FOUP). The wrapping layer is processed to avoid metal contamination. Photolithography is used to define protected areas and non-protected areas to form a shielding layer. The TiN layers in the non-protected areas and protected areas are gradually removed to form the side walls of the wrapping layer and the TiN on the side walls of the trench is retained.
This effectively avoids contamination during the TiN floating gate production process and improves device performance and uniformity.
Smart Images

Figure CN114121674B_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the field of integrated circuit manufacturing, and in particular to a method for manufacturing a TiN floating gate on the side wall of an ultra-fast flash memory. Background Art
[0002] Compared with the third generation Nor flash in the industry, 38SF (ultra-fast flash memory at 38nm technology node) has higher erase efficiency, higher erase and write durability, higher write efficiency, faster write speed, lower erase and write voltage, lower power consumption, no read and write interference, the storage unit size is only half of SF1.0, the process is simple, the test time is short, and the cost is greatly reduced. High speed, low power consumption and low voltage are the highlights of 38SF technology. The growth and etching of each auxiliary layer in the ALD TiN floating gate process has extremely high requirements for uniformity and stability, and pollution problems are prone to occur during the process. Summary of the invention
[0003] A series of simplified concepts are introduced in the Summary of the Invention, which are all simplifications of the prior art in the field, and will be further described in detail in the Detailed Description of the Invention. The Summary of the Invention of the present invention does not mean to attempt to define the key features and essential technical features of the claimed technical solution, nor does it mean to attempt to determine the scope of protection of the claimed technical solution.
[0004] The technical problem to be solved by the present invention is to provide a method for manufacturing a TiN floating gate on the side wall of an ultra-fast flash memory device which can avoid contamination during the TiN floating gate manufacturing process.
[0005] In order to solve the above technical problems, the present invention provides a method for manufacturing a sidewall TiN floating gate of an ultra-fast flash memory, comprising the following steps:
[0006] S1, completing the previous process according to the prior art until the trench etching is completed;
[0007] S2, transfer to HK FOUP and deposit TiN;
[0008] S3, depositing a wrapping layer, wrapping TiN;
[0009] S4, wafer back cleaning and transfer to HL FOUP;
[0010] S5, photolithography defines the protection area and the non-protection area, and forms a shielding layer to protect the protection area and expose the non-protection area;
[0011] S6, transfer to HK FOUP, etch and remove the package layer in the non-protected area to expose the TiN in the non-protected area;
[0012] S7, remove the shielding layer of the protected area;
[0013] S8, etching to remove TiN in non-protected areas;
[0014] S9, depositing a wrapping layer to wrap the TiN in the protection area;
[0015] S10, etching and removing the oxide layer on the top of the active area and the bottom of the trench to form a wrapping layer sidewall;
[0016] S11, etching and removing the TiN on the top of the protection zone and the bottom of the trench and the side wall of the wrapping layer, and retaining the TiN on the side wall of the trench;
[0017] HK FOUP is a front-opening wafer transfer box with a high contamination risk level, and HL FOUP is a front-opening wafer transfer box with a low contamination risk level.
[0018] Optionally, the method for manufacturing the ultra-fast flash memory sidewall TiN floating gate is further improved, and the encapsulating layer is an oxide layer.
[0019] Optionally, the method for manufacturing the ultra-fast flash memory sidewall TiN floating gate is further improved, and the encapsulation layer is formed by a low-temperature atomic layer deposition process.
[0020] Optionally, the method for manufacturing the ultra-fast flash memory sidewall TiN floating gate is further improved, wherein the protection area is an active area, and the non-protection area is an isolation area.
[0021] Optionally, the method for manufacturing the ultra-fast flash memory sidewall TiN floating gate is further improved, and the shielding layer is a photoresist.
[0022] Optionally, the method for manufacturing the ultra-fast flash memory sidewall TiN floating gate is further improved, and step S6 is performed to remove the oxide layer by dry isotropic etching.
[0023] Optionally, the method for manufacturing the ultra-fast flash memory sidewall TiN floating gate is further improved, and step S8 is performed to remove the TiN in the non-protected area by using dry and wet etching.
[0024] Optionally, the method for manufacturing the ultra-fast flash memory sidewall TiN floating gate is further improved, and step S10 is performed to remove the oxide layer at the top of the active area and the bottom of the trench by dry anisotropic etching.
[0025] Optionally, the method for manufacturing the ultra-fast flash memory sidewall TiN floating gate is further improved by performing step S11 to remove the TiN on the top of the protection zone and the bottom of the trench as well as the sidewall of the encapsulation layer by dry and wet etching.
[0026] After the present invention completes the previous process and the groove according to the prior art, it is transferred to HK FOUP to avoid metal contamination. The deposited encapsulation layer encapsulates TiN to avoid exposure of TiN on the wafer surface to produce contamination, and then the wafer back is cleaned and transferred to HL FOUP to avoid residual contamination. The protected area and the non-protected area are defined by photolithography, and a shielding layer is formed to protect the protected area and expose the non-protected area; the process is transferred to HK FOUP to avoid metal contamination, and the encapsulation layer of the non-protected area is etched to remove the TiN in the non-protected area; the shielding layer of the protected area is removed; the TiN in the non-protected area is etched to remove the encapsulation layer; the encapsulation layer is deposited to encapsulate the TiN in the protected area to avoid exposure of TiN on the wafer surface to produce contamination; the encapsulation layer at the top of the protected area and the bottom of the groove is etched to form the side wall of the encapsulation layer; the TiN at the top of the protected area and the bottom of the groove and the side wall of the encapsulation layer are etched to remove the TiN and the side wall of the encapsulation layer, and the TiN on the side wall of the groove is retained. The present invention can prevent the TiN floating gate on the side wall of the ultra-fast flash memory from being contaminated during the production process, and improve the device performance and uniformity. BRIEF DESCRIPTION OF THE DRAWINGS
[0027] The drawings of the present invention are intended to illustrate the general characteristics of the methods, structures and / or materials used in specific exemplary embodiments of the present invention, and to supplement the description in the specification. However, the drawings of the present invention are schematic diagrams not drawn to scale, and thus may not accurately reflect the precise structure or performance characteristics of any given embodiment, and the drawings of the present invention should not be interpreted as limiting or restricting the range of values or properties covered by the exemplary embodiments of the present invention. The present invention is further described in detail below in conjunction with the drawings and specific embodiments:
[0028] Figure 1 It is a schematic diagram of the process of the present invention.
[0029] Figure 2 The intermediate structure of the present invention is shown in FIG. Figure 1 .
[0030] Figure 3 The intermediate structure of the present invention is shown in FIG. Figure 2 .
[0031] Figure 4 The intermediate structure of the present invention is shown in FIG. Figure 3 .
[0032] Figure 5 The intermediate structure of the present invention is shown in FIG. Figure 4 .
[0033] Figure 6 The intermediate structure of the present invention is shown in FIG. Figure 5 .
[0034] Figure 7 The intermediate structure of the present invention is shown in FIG. Figure 6 . DETAILED DESCRIPTION
[0035] The following describes the implementation methods of the present invention through specific specific embodiments, and those skilled in the art can fully understand other advantages and technical effects of the present invention from the contents disclosed in this specification. The present invention can also be implemented or applied through different specific implementation methods, and the details in this specification can also be applied based on different viewpoints, and various modifications or changes can be made without deviating from the overall design concept of the invention. It should be noted that the following embodiments and the features in the embodiments can be combined with each other in the absence of conflict. The following exemplary embodiments of the present invention can be implemented in a variety of different forms and should not be interpreted as being limited to the specific embodiments described herein. It should be understood that these embodiments are provided to make the disclosure of the present invention thorough and complete, and to fully convey the technical solutions of these exemplary specific embodiments to those skilled in the art.
[0036] First embodiment;
[0037] refer to Figure 1 As shown, the present invention provides a method for manufacturing a sidewall TiN floating gate of an ultra-fast flash memory, comprising the following steps:
[0038] S1, completing the previous process according to the prior art until the trench etching is completed;
[0039] S2, transfer to HK FOUP and deposit TiN;
[0040] S3, depositing a wrapping layer, wrapping TiN;
[0041] S4, wafer back cleaning and transfer to HL FOUP;
[0042] S5, photolithography defines the protection area and the non-protection area, and forms a shielding layer to protect the protection area and expose the non-protection area;
[0043] S6, transfer to HK FOUP, etch and remove the package layer in the non-protected area to expose the TiN in the non-protected area;
[0044] S7, remove the shielding layer of the protected area;
[0045] S8, etching to remove TiN in non-protected areas;
[0046] S9, depositing a wrapping layer to wrap the TiN in the protection area;
[0047] S10, etching and removing the oxide layer on the top of the active area and the bottom of the trench to form a wrapping layer sidewall;
[0048] S11, etching and removing the TiN on the top of the protection zone and the bottom of the trench and the side wall of the wrapping layer, and retaining the TiN on the side wall of the trench;
[0049] HK FOUP is a front-opening wafer transfer box with a high contamination risk level, and HL FOUP is a front-opening wafer transfer box with a low contamination risk level.
[0050] Second embodiment;
[0051] The present invention provides a method for manufacturing a sidewall TiN floating gate of an ultra-fast flash memory, comprising the following steps:
[0052] S1, completing the previous process according to the prior art until the trench etching is completed;
[0053] S2, transfer to HK FOUP and deposit TiN;
[0054] S3, using low-temperature atomic layer deposition process to deposit an oxide layer to encapsulate TiN;
[0055] S4, wafer back cleaning and transfer to HL FOUP;
[0056] S5, photolithography defines the active area and the isolation area, and the photoresist shields and protects the active area, exposing the isolation area;
[0057] S6, transfer to HK FOUP, etch and remove the oxide layer of the isolation area to expose the TiN in the isolation area;
[0058] S7, removing the photoresist in the active area;
[0059] S8, etching and removing TiN in the isolation area;
[0060] S9, using low temperature atomic layer deposition process to deposit an oxide layer to cover the TiN in the active area;
[0061] S10, etching and removing the oxide layer at the top of the active area and the bottom of the trench to form an oxide layer sidewall;
[0062] S11, etching and removing the TiN on the top of the protection zone and the bottom of the trench and the side wall of the wrapping layer, and retaining the TiN on the side wall of the trench;
[0063] HK FOUP is a front-opening wafer transfer box with a high contamination risk level, and HL FOUP is a front-opening wafer transfer box with a low contamination risk level.
[0064] In all the accompanying drawings, the same reference numerals represent the same elements all the time. In addition, it should also be understood that, although the terms "first", "second" etc. can be used here to describe different elements, parameters, components, regions, layers and / or parts, these elements, parameters, components, regions, layers and / or parts should not be limited by these terms. These terms are only used to distinguish an element, parameter, component, region, layer or part from another element, parameter, component, region, layer or part. Therefore, without departing from the teaching according to exemplary embodiments of the present invention, the first element, parameter, component, region, layer or part discussed below may also be referred to as the second element, parameter, component, region, layer or part.
[0065] Third embodiment;
[0066] The present invention provides a method for manufacturing a sidewall TiN floating gate of an ultra-fast flash memory, comprising the following steps:
[0067] S1, completing the previous process according to the prior art until the trench etching is completed;
[0068] S2, transfer to HK FOUP and deposit TiN;
[0069] S3, using low temperature atomic layer deposition process to deposit an oxide layer, wrapping TiN, such as Figure 2 As shown;
[0070] S4, wafer back cleaning and transfer to HL FOUP;
[0071] S5, photolithography defines the active area and isolation area, photoresist shields and protects the active area, exposing the isolation area, such as Figure 3 As shown;
[0072] S6, transfer to HK FOUP, use dry isotropic etching to remove the oxide layer of the isolation area to expose the TiN in the isolation area;
[0073] S7, removing the photoresist in the active area, such as Figure 4 As shown;
[0074] S8, etching to remove the TiN in the isolation region, such as Figure 5 As shown;
[0075] S9, using low temperature atomic layer deposition process to deposit an oxide layer to cover the TiN in the active area;
[0076] S10, using dry anisotropic etching to remove the oxide layer at the top of the active area and the bottom of the trench to form an oxide layer sidewall, such as Figure 6 As shown;
[0077] S11, using dry and wet etching to remove the TiN at the top of the protection zone and the bottom of the trench and the sidewall of the oxide layer, and retaining the TiN on the sidewall of the trench, such as Figure 7 As shown;
[0078] HK FOUP is a front-opening wafer transfer box with a high contamination risk level, and HL FOUP is a front-opening wafer transfer box with a low contamination risk level.
[0079] Unless otherwise defined, all terms (including technical and scientific terms) used herein have the same meaning as those commonly understood by those skilled in the art to which the present invention belongs. It will also be understood that, unless expressly defined herein, terms such as those defined in general dictionaries should be interpreted as having a meaning consistent with their meaning in the context of the relevant art, and not interpreted in an ideal or overly formal sense.
[0080] The present invention has been described in detail above through specific implementation modes and embodiments, but these do not constitute limitations of the present invention. Without departing from the principles of the present invention, those skilled in the art may also make many variations and improvements, which should also be regarded as the protection scope of the present invention.
Claims
1. A method for manufacturing a TiN floating gate on the sidewall of an ultra-fast flash memory, characterized in that: The following steps are involved: S1, completing the previous process according to the prior art until the trench etching is completed; S2, transfer to HK FOUP and deposit TiN; S3, depositing a wrapping layer, wrapping TiN; S4, wafer back cleaning and transfer to HL FOUP; S5, photolithography defines the protection area and the non-protection area, and forms a shielding layer to protect the protection area and expose the non-protection area; S6, transfer to HK FOUP, etch and remove the package layer in the non-protected area to expose the TiN in the non-protected area; S7, remove the shielding layer of the protected area; S8, etching to remove TiN in non-protected areas; S9, depositing a wrapping layer to wrap the TiN in the protection area; S10, etching and removing the wrapping layer at the top of the protection zone and the bottom of the trench to form a wrapping layer sidewall; S11, etching and removing the TiN on the top of the protection zone and the bottom of the trench and the side wall of the wrapping layer, and retaining the TiN on the side wall of the trench; HK FOUP is a front-opening wafer transfer box with a high contamination risk level, and HL FOUP is a front-opening wafer transfer box with a low contamination risk level.
2. The method for manufacturing a sidewall TiN floating gate of an ultra-fast flash memory according to claim 1, wherein: The encapsulating layer is an oxide layer.
3. The method for manufacturing a sidewall TiN floating gate of an ultra-fast flash memory as claimed in claim 2, characterized in that: The encapsulation layer is formed by a low-temperature atomic layer deposition process.
4. The method for manufacturing a sidewall TiN floating gate of an ultra-fast flash memory according to claim 1, wherein: The protection area is an active area, and the non-protection area is an isolation area.
5. The method for manufacturing a sidewall TiN floating gate of an ultra-fast flash memory according to claim 1, wherein: The shielding layer is photoresist.
6. The method for manufacturing a sidewall TiN floating gate of an ultra-fast flash memory as claimed in claim 2, characterized in that: In step S6, dry isotropic etching is used to remove the oxide layer.
7. The method for manufacturing a sidewall TiN floating gate of an ultra-fast flash memory according to claim 1, wherein: In step S8, dry and wet etching are used to remove TiN in the non-protected area.
8. The method for manufacturing a sidewall TiN floating gate of an ultra-fast flash memory as claimed in claim 2, characterized in that: Step S10 is implemented to remove the oxide layer on the top of the active area and the bottom of the trench by dry anisotropic etching.
9. The method for manufacturing a sidewall TiN floating gate of an ultra-fast flash memory as claimed in claim 1, characterized in that: Step S11 is implemented to remove the TiN on the top of the protection area and the bottom of the trench as well as the side wall of the encapsulation layer by dry and wet etching.
Citation Information
Patent Citations
Method for manufacturing floating gate TiN film of ultra-flash memory
CN114121633A