Semiconductor structure and method for manufacturing the same
By performing wet treatment and dry etching in the semiconductor structure, the Cu metal residue problem is solved, the electrical performance of the device is improved, and the connection between Cu metal inside and outside the insulating layer is avoided.
Patent Information
- Application Number
- CN202010921606.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2020-09-04
- Publication Date
- 2024-11-26
- Estimated Expiration
- 2040-09-04
AI Technical Summary
In the prior art, Cu metal is prone to remain after the planarization process, affecting the electrical performance of high-density and small-pitch semiconductor devices.
Cu metal residue is removed by forming trenches, insulating layers and Cu columns on the Si substrate, and Cu metal residues are removed by dry etching of the Si substrate to create a height difference to avoid Cu metal connections.
Effectively remove Cu metal residue, avoiding the connection between Cu metal inside and outside the insulating layer, and improving the electrical performance of the device.
Smart Images

Figure CN114141699B_ABST
Abstract
Description
Technical Field
[0001] The invention belongs to the field of semiconductor manufacturing and relates to a semiconductor structure and a preparation method thereof. Background Art
[0002] As integrated circuits become more powerful, more performant and more integrated, packaging technology plays an increasingly important role in integrated circuit products, and accounts for an increasing proportion of the value of the entire electronic system. Wafer-level packaging (WLP) technology has become an important packaging method for electronic devices such as high-demand mobile / wireless networks, and is currently one of the most promising packaging technologies, due to its advantages of miniaturization, low cost, high integration, better performance and higher energy efficiency.
[0003] The redistribution layer (RDL) can re-layout the soldering area positions of the chip's solder pads and arrange the new soldering areas in an array. Therefore, RDL is widely used in the WLP process. With the development of packaging technology, high-density, small-pitch RDL metal lines are urgently needed.
[0004] In the prior art, Cu metal is widely used as a conductive material in the WLP process. However, due to the forgeability of Cu metal, Cu metal is easily left after the planarization process, and the residual Cu metal will affect the electrical performance of the prepared high-density, small-pitch devices.
[0005] Therefore, it is necessary to provide a semiconductor structure and a method for manufacturing the same to completely remove the residual Cu metal. Summary of the invention
[0006] In view of the above-mentioned shortcomings of the prior art, an object of the present invention is to provide a semiconductor structure and a method for preparing the same, so as to solve the problem of residual Cu metal after the planarization process in the prior art.
[0007] To achieve the above object and other related objects, the present invention provides a method for preparing a semiconductor structure, comprising the following steps:
[0008] Providing a Si substrate;
[0009] Patterning the Si substrate to form a groove;
[0010] forming an insulating layer in the trench to cover the bottom and sidewalls of the trench;
[0011] forming a Cu column to fill the trench;
[0012] Performing planarization to expose the Si substrate, the insulating layer and the Cu pillar;
[0013] Performing wet processing to remove Cu metal residues and part of the Cu column so that the Cu column and the insulating layer have a first height difference;
[0014] The Si substrate is dry-etched so that a second height difference exists between the Si substrate and the insulating layer, and the second height difference is greater than the first height difference.
[0015] Optionally, the treatment solution used in the wet treatment includes an acidic solution that chemically reacts with Cu metal, and the acidic solution includes one or a mixed solution of H2O2, H3PO4 and H2SO4.
[0016] Optionally, the first height difference ranges from 0.1 μm to 0.5 μm, and the second height difference ranges from 2 μm to 5 μm.
[0017] Optionally, the planarization includes one or a combination of mechanical polishing and chemical mechanical polishing.
[0018] Optionally, after forming the insulating layer and before forming the Cu column, the method further includes forming a metal seed layer.
[0019] The present invention also provides a semiconductor structure, which includes: a Si substrate, an insulating layer and a Cu column, wherein the Cu column is located in the Si substrate, the insulating layer covers the side wall and the bottom of the Cu column and contacts the Si substrate, and the Cu column and the insulating layer have a first height difference, the Si substrate and the insulating layer have a second height difference, and the second height difference is greater than the first height difference.
[0020] Optionally, the first height difference ranges from 0.1 μm to 0.5 μm.
[0021] Optionally, the second height difference ranges from 2 μm to 5 μm.
[0022] Optionally, a metal seed layer is further included between the insulating layer and the Cu column, and the metal seed layer and the Cu column have the same height.
[0023] Optionally, the insulating layer includes one or a combination of a SiO2 layer and a Si3N4 layer.
[0024] As described above, the semiconductor structure and preparation method thereof of the present invention can effectively remove the residual Cu metal near the edge of the Cu column through wet treatment after planarization, and make the Cu column and the insulating layer have a first height difference, and further make the Si substrate have a second height difference with the insulating layer through dry etching, and the second height difference is greater than the first height difference, thereby further avoiding the connection of the Cu metal inside and outside the insulating layer, so as to effectively avoid affecting the electrical performance of the device. BRIEF DESCRIPTION OF THE DRAWINGS
[0025] Figure 1 It is a schematic diagram of the process flow of preparing a semiconductor structure in an embodiment.
[0026] Figure 2 It is a schematic diagram of the structure after flattening in the embodiment.
[0027] Figure 3 It is a schematic diagram of the structure after wet processing in the embodiment.
[0028] Figure 4 It is a schematic diagram of the structure after dry etching in the embodiment.
[0029] Component number description
[0030] 100 Si substrate
[0031] 200 Insulation
[0032] 300 Cu column
[0033] 400 Cu metal residue
[0034] D1 First height difference
[0035] D2 Second height difference DETAILED DESCRIPTION
[0036] The following describes the embodiments of the present invention through specific examples, and those skilled in the art can easily understand other advantages and effects of the present invention from the contents disclosed in this specification. The present invention can also be implemented or applied through other different specific embodiments, and the details in this specification can also be modified or changed in various ways based on different viewpoints and applications without departing from the spirit of the present invention.
[0037] For example, when describing the embodiments of the present invention in detail, for the sake of convenience, the cross-sectional view showing the device structure will not be partially enlarged according to the general scale, and the schematic view is only an example, which should not limit the scope of protection of the present invention. In addition, in actual production, the three-dimensional space dimensions of length, width and depth should be included.
[0038] For ease of description, spatial relational terms such as "under", "below", "below", "below", "above", "on", etc. may be used herein to describe the relationship of one element or feature shown in the drawings to other elements or features. It will be understood that these spatial relational terms are intended to include other directions of the device in use or operation in addition to the directions depicted in the drawings. In addition, when a layer is referred to as being "between" two layers, it can be the only layer between the two layers, or there can be one or more intervening layers. As used herein, "between..." means including the end point values.
[0039] In the context of the present application, a structure in which a first feature is described as being "above" a second feature may include embodiments in which the first and second features are formed in direct contact, and may also include embodiments in which additional features are formed between the first and second features, such that the first and second features may not be in direct contact.
[0040] It should be noted that the illustrations provided in this embodiment are only used to illustrate the basic concept of the present invention in a schematic manner, and therefore the illustrations only show components related to the present invention rather than being drawn according to the number, shape and size of components in actual implementation. In actual implementation, the type, quantity and proportion of each component may be changed arbitrarily, and the component layout may also be more complicated.
[0041] See also Figure 1 to Figure 4 This embodiment provides a method for preparing a semiconductor structure, comprising the following steps:
[0042] Providing a Si substrate 100;
[0043] Patterning the Si substrate 100 to form a groove (not shown);
[0044] forming an insulating layer 200 in the trench to cover the bottom and sidewalls of the trench;
[0045] forming a Cu column 300 to fill the trench;
[0046] Planarization is performed to expose the Si substrate 100, the insulating layer 200 and the Cu pillar 300;
[0047] Performing wet processing to remove the Cu metal residue 400 and a portion of the Cu column 300 so that the Cu column 300 and the insulating layer 200 have a first height difference D1;
[0048] The Si substrate 100 is dry-etched so that a second height difference D2 is formed between the Si substrate 100 and the insulating layer 200 , and the second height difference D2 is greater than the first height difference D1 .
[0049] In the method for preparing the semiconductor structure of this embodiment, after the planarization, the Cu metal residue 400 can be removed by the wet treatment, and the Cu column 300 and the insulating layer 200 have the first height difference D1. Furthermore, a portion of the Si substrate 100 is removed by the dry etching, so that the Si substrate 100 and the insulating layer 200 have the second height difference D2, and the second height difference D2 is greater than the first height difference D1, thereby further avoiding the connection of the Cu metal inside and outside the insulating layer 200, so as to effectively avoid affecting the electrical performance of the device.
[0050] See also Figure 1 First, a Si substrate 100 is provided, and the Si substrate 100 is patterned to form a groove (not shown).
[0051] Specifically, the method for patterning the Si substrate 100 may adopt a conventional photolithography method, such as patterning using a mask, the mask may include photoresist, but is not limited thereto. The depth, width and distribution of the grooves may be selected as required, and are not excessively limited here.
[0052] Next, an insulating layer 200 is formed in the trench to cover the bottom and sidewalls of the trench.
[0053] As an example, the insulating layer 200 includes one or a combination of a SiO2 layer and a Si3N4 layer. By covering the bottom and sidewalls of the groove, the insulating layer 200 can effectively prevent the formation of a conductive channel between the subsequently formed Cu column 300 and the Si substrate 100, thereby achieving a good insulation effect. The specific formation method, thickness, and material of the insulating layer 200 can be selected as needed, and no excessive restrictions are made here. In this embodiment, the insulating layer 200 adopts a SiO2 layer, but it is not limited to this. The insulating layer 200 can also adopt a Si3N4 layer or a stack of a SiO2 layer and a Si3N4 layer.
[0054] As an example, after forming the insulating layer 200 and before forming the Cu pillar 300 , a step of forming a metal seed layer (not shown) is further included.
[0055] Specifically, the metal seed layer can be formed on the surface of the insulating layer 200 by PVD method, and the metal seed layer can include a Ti / Cu metal seed layer or a Cu metal seed layer, but is not limited thereto, and can be selected according to needs. Among them, it is preferred that the metal seed layer adopts a Cu metal seed layer, so that when the first height difference D1 is formed later, the metal seed layer and the Cu column 300 can have the same etching rate, so that the metal seed layer and the Cu column 300 have the same height, and the metal seed layer is prevented from connecting with the Cu metal outside the insulating layer 200.
[0056] Next, the Cu pillar 300 is formed to fill the trench.
[0057] Specifically, when the metal seed layer is present in the groove, the Cu column 300 may be formed by electroplating, but is not limited thereto. For example, the Cu column 300 may also be prepared by a patterned mask and a deposition method, which is not excessively limited herein.
[0058] Next, planarization is performed to expose the Si substrate 100 , the insulating layer 200 and the Cu pillar 300 .
[0059] As an example, the planarization includes one or a combination of mechanical polishing and chemical mechanical polishing.
[0060] Specifically, in this embodiment, mechanical grinding is first performed, and then fine chemical mechanical grinding is performed, so that a relatively flat surface can be obtained, but the planarization process is not limited to this. For example, only mechanical grinding or only chemical mechanical grinding can be used as needed, and no excessive restrictions are made here. However, since Cu metal has good forgeability, during the planarization process, Cu metal residue 400 will be formed near the edge of the Cu column 300, and this part of the residual Cu metal will affect the electrical performance of the high-density, small-pitch devices prepared subsequently, so it is necessary to completely remove the Cu metal residue 400, see Figure 2 .
[0061] Next, see Figure 3 , performing wet processing to remove the Cu metal residue 400 and a portion of the Cu column 300 , so that the Cu column 300 and the insulating layer 200 have a first height difference D1 .
[0062] As an example, the processing solution used in the wet processing includes an acidic solution that chemically reacts with Cu metal, and the acidic solution includes one or a mixed solution of H2O2, H3PO4 and H2SO4.
[0063] Specifically, the Cu metal residue 400 located at the edge of the Cu column 300 can be effectively removed through the wet treatment of the acidic solution, and further, the acidic solution can also remove part of the Cu column 300 so that the Cu column 300 and the insulating layer 200 have the first height difference D1, thereby further avoiding the Cu metal residue 400 that has not been completely removed from contacting the Cu column 300, so as to improve the electrical performance of the subsequently prepared device.
[0064] As an example, the first height difference D1 ranges from 0.1 μm to 0.5 μm.
[0065] Specifically, the larger the value of the first height difference D1 is, the more conducive it is to avoiding contact between the Cu metal residue 400 and the Cu column 300. However, if the first height difference D1 is too large, it will cause defects such as cracks in the insulating layer 200 during the subsequent grinding process, which will in turn cause the hidden danger of electrical conduction between the Cu column 300 and the Si substrate 100. Therefore, in this embodiment, the first height difference D1 is preferably 0.3μm, but is not limited to this, and may also be 0.2μm, 0.4μm, etc.
[0066] Next, see Figure 4 , dry-etching the Si substrate 100 so that the Si substrate 100 and the insulating layer 200 have a second height difference D2, and the second height difference D2 is greater than the first height difference D1.
[0067] Specifically, through the dry etching, the Si substrate 100 and the insulating layer 200 can have the second height difference D2, and the second height difference D2 is greater than the first height difference D1, thereby further avoiding the connection of the Cu metal inside and outside the insulating layer 200, so as to effectively avoid affecting the electrical performance of the device.
[0068] As an example, the second height difference D2 ranges from 2 μm to 5 μm.
[0069] Specifically, the larger the value of the second height difference D2 is, the more conducive it is to avoiding contact between the Cu metal residue 400 and the Cu column 300. However, if the second height difference D2 is too large, it will cause defects such as cracks in the insulating layer 200 during the subsequent grinding process, which will in turn cause the hidden danger of electrical conduction between the Cu column 300 and the Si substrate 100. Therefore, in this embodiment, the second height difference D2 is preferably 3μm, but is not limited to this, and 2μm, 4μm, etc. may also be used.
[0070] See also Figure 4This embodiment also provides a semiconductor structure. The semiconductor structure of this embodiment can be prepared by the above method, but is not limited thereto.
[0071] Specifically, the semiconductor structure includes a Si substrate 100, an insulating layer 200 and a Cu column 300, wherein the Cu column 300 is located in the Si substrate 100, the insulating layer 200 covers the side wall and the bottom of the Cu column 300 and contacts the Si substrate 100, and the Cu column 300 and the insulating layer 200 have a first height difference D1, the Si substrate 100 and the insulating layer 200 have a second height difference D2, and the second height difference D2 is greater than the first height difference D1.
[0072] The semiconductor structure of the present embodiment can effectively avoid affecting the electrical performance of the device because the Cu column 300 and the insulating layer 200 have the first height difference D1; further, because the Si substrate 100 and the insulating layer 200 have the second height difference D2, and the second height difference D2 is greater than the first height difference D1, the connection between the inner and outer Cu metals of the insulating layer 200 can be further avoided, so as to effectively avoid affecting the electrical performance of the device.
[0073] As an example, the first height difference D1 ranges from 0.1 μm to 0.5 μm.
[0074] Specifically, the larger the value of the first height difference D1 is, the more conducive it is to avoiding the contact between the Cu metal residue and the Cu column 300. However, if the first height difference D1 is too large, it will cause defects such as cracks in the insulating layer 200 during the subsequent grinding process, which will in turn cause the hidden danger of electrical conduction between the Cu column 300 and the Si substrate 100. Therefore, in this embodiment, the first height difference D1 is preferably 0.3μm, but is not limited to this, and may also be 0.2μm, 0.4μm, etc.
[0075] As an example, the second height difference D2 ranges from 2 μm to 5 μm.
[0076] Specifically, the larger the value of the second height difference D2 is, the more conducive it is to avoiding contact between Cu metal residues and the Cu column 300. However, if the second height difference D2 is too large, it will cause defects such as cracks in the insulating layer 200 during the subsequent grinding process, which will in turn cause the hidden danger of electrical conduction between the Cu column 300 and the Si substrate 100. Therefore, in this embodiment, the second height difference D2 is preferably 3μm, but is not limited to this, and 2μm, 4μm, etc. may also be used.
[0077] As an example, a metal seed layer (not shown) is further included between the insulating layer 200 and the Cu pillar 300 , and the metal seed layer and the Cu pillar 300 have the same height.
[0078] Specifically, the metal seed layer may include a Ti / Cu metal seed layer or a Cu metal seed layer, but is not limited thereto and may be selected as required. Preferably, the metal seed layer is a Cu metal seed layer and the metal seed layer and the Cu column 300 have the same height to avoid the metal seed layer from being connected to the Cu metal outside the insulating layer 200.
[0079] As an example, the insulating layer 200 includes one or a combination of a SiO 2 layer and a Si 3 N 4 layer.
[0080] Specifically, the insulating layer 200 can effectively prevent the formation of a conductive channel between the Cu column 300 and the Si substrate 100, thereby achieving a good insulating effect. The specific formation method, thickness, and material of the insulating layer 200 can be selected as needed, and no excessive restrictions are made here. In this embodiment, the insulating layer 200 is a SiO2 layer, but it is not limited to this. The insulating layer 200 can also be a Si3N4 layer or a stack of a SiO2 layer and a Si3N4 layer.
[0081] In summary, the semiconductor structure and preparation method thereof of the present invention, after planarization, can effectively remove the residual Cu metal near the edge of the Cu column through wet treatment, and make the Cu column and the insulating layer have a first height difference, and further through dry etching of the Si substrate, make the Si substrate and the insulating layer have a second height difference, and the second height difference is greater than the first height difference, thereby further avoiding the connection of the Cu metal inside and outside the insulating layer, so as to effectively avoid affecting the electrical performance of the device.
[0082] The above embodiments are merely illustrative of the principles and effects of the present invention, and are not intended to limit the present invention. Anyone familiar with the art may modify or alter the above embodiments without departing from the spirit and scope of the present invention. Therefore, all equivalent modifications or alterations made by a person of ordinary skill in the art without departing from the spirit and technical concept disclosed by the present invention shall still be covered by the claims of the present invention.
Claims
1. A method for preparing a semiconductor structure, characterized in that: The following steps are involved: Providing a Si substrate; Patterning the Si substrate to form a groove; forming an insulating layer in the trench to cover the bottom and sidewalls of the trench; forming a Cu column to fill the trench; Performing planarization to expose the Si substrate, the insulating layer and the Cu pillar; Performing wet processing to remove Cu metal residues and part of the Cu column so that the Cu column and the insulating layer have a first height difference; The Si substrate is dry-etched so that there is a second height difference between the Si substrate and the insulating layer, and the second height difference is greater than the first height difference, the first height difference ranges from 0.1 μm to 0.5 μm, and the second height difference ranges from 2 μm to 5 μm.
2. The method for preparing a semiconductor structure according to claim 1, characterized in that: The treatment solution used in the wet treatment includes an acidic solution that chemically reacts with Cu metal, and the acidic solution includes one or a mixed solution of H2O2, H3PO4 and H2SO4.
3. The method for preparing a semiconductor structure according to claim 1, wherein: The planarization includes one or a combination of mechanical polishing and chemical mechanical polishing.
4. The method for preparing a semiconductor structure according to claim 1, wherein: After forming the insulating layer and before forming the Cu column, the method further includes forming a metal seed layer.
5. A semiconductor structure, characterized in that: The semiconductor structure includes: a Si substrate, an insulating layer and a Cu column, wherein the Cu column is located in the Si substrate, the insulating layer covers the side wall and the bottom of the Cu column and contacts the Si substrate, and the Cu column and the insulating layer have a first height difference, the Si substrate and the insulating layer have a second height difference, and the second height difference is greater than the first height difference, the first height difference ranges from 0.1μm to 0.5μm, and the second height difference ranges from 2μm to 5μm.
6. The semiconductor structure according to claim 5, characterized in that: A metal seed layer is further included between the insulating layer and the Cu column, and the metal seed layer and the Cu column have the same height.
7. The semiconductor structure according to claim 5, characterized in that: The insulating layer includes one or a combination of a SiO2 layer and a Si3N4 layer.