Temperature Control Method for Forging of 35CrNi3Mo Die Casting Ingot Precision Forging Machine

Through high-temperature heating and rapid cooling of 35CrNi3Mo die-cast ingots, combined with the high-frequency forging and annealing process of the precision forging machine, the problem of segregation lines when the die-cast ingots are forged on the precision forging machine is solved, and the fracture structure quality and quality of the forgings are improved. Performance index, achieving fibrous optimization of fracture structure and performance improvement.

CN114210894BActive Publication Date: 2024-10-01INNER MONGOLIA NORTH HEAVY INDS GROUP +1
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202111617001.7
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2021-12-27
Publication Date
2024-10-01
Estimated Expiration
2041-12-27

AI Technical Summary

Technical Problem

When the 35CrNi3Mo die-cast ingot is forged on a precision forging machine, the solidified phase and the precipitated phase extend longitudinally to form strip-like segregation lines, resulting in an unqualified fracture. The existing technology cannot effectively control the problem of precipitates forming segregation lines.

Method used

The steel ingot is heated at 1210℃-1230℃, rapidly cooled after 0.6h/100mm heat preservation, and then high-frequency forging is performed on the precision forging machine. The total forging ratio is controlled above 2.8. After forging, it is air-cooled to 480℃-530℃, and then heated at 600 Annealing in the furnace at ℃-650℃ ensures that the fracture structure of the forging is fibrous and avoids the formation of segregation lines.

Benefits of technology

It effectively solves the problem of segregation lines in the fracture structure of 35CrNi3Mo gun steel forgings, improves the qualification rate of forgings, ensures that the fracture structure is 100% fibrous, and various performance indicators meet or exceed standards, reducing scrapping.

✦ Generated by Eureka AI based on patent content.
Patent Text Reader

Abstract

The invention discloses a forging temperature control method for a 35PCrNi3Mo die-cast ingot precision forging machine, and belongs to the field of material forming. The improved heating temperature, cooling and forging technology are used to solve the problem of segregation lines appearing in the fracture structure of 35CrNi3Mo gun steel forgings. The heating temperature of the 35CrNi3Mo die-cast steel ingot is 1210℃-1230℃, and the temperature is kept at 0.6h / 100mm after reaching the temperature. The maximum residence time after keeping warm is ≤2h / 100mm, and the purpose is to dissolve the BN and CrN precipitates solidified and precipitated from the die-cast steel ingot. After the heating and heat preservation of the die-cast steel ingot is completed, it is taken out and cooled in the air. After the air cooling time reaches the requirement, forging on the precision forging machine is started. The use of a new heating, forging and cooling process after forging ensures that the fibrous proportion of the fracture structure of the forging is increased and there is no segregation line.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the technical field of material forming and is a forging temperature control method of a 35CrNi3Mo die casting ingot precision forging machine. Background Art

[0002] Domestic precision forging machines are generally equipped with blanking machines for preforming. After preforming, the billet temperature is 850℃-950℃ for precision forging machines. However, the use of steel ingots directly on precision forging machines is rare. In order to prevent the excessive growth of the ingot grains, 35CrNi3Mo steel ingots are made of 1110 -20 ℃ heating and forging, but because the solidification phase and precipitation phase of the die-cast ingot cannot be fully dissolved, under the high-frequency forging action of the four hammers of the precision forging machine, the solidification phase and precipitation phase extend longitudinally to form strips, and type II segregation lines are shown in the fracture detection. Subsequent fracture electron microscope analysis shows BN, CrN single phase and composite nitride precipitation phases. Similar Cr-Ni-Mo refined die-cast gun steel ingots are forged on the precision forging machine, and the unqualified rate is as high as 22.5%. In the past, there was no heating process method that effectively controls the formation of segregation lines of precipitates in forging on the precision forging machine. Therefore, solving the problem of controlling the segregation line of 35CrNi3Mo die-cast ingots directly forged on the precision forging machine has become our primary problem. Summary of the invention

[0003] The object of the present invention is to provide a forging temperature control method for a 35CrNi3Mo die casting ingot precision forging machine, which solves the problem of segregation lines appearing in the fracture structure of 35CrNi3Mo forgings.

[0004] The technical solution of the present invention:

[0005] A method for controlling the forging temperature of a 5CrNi3Mo die casting ingot precision forging machine, characterized in that the method comprises the following contents:

[0006] 1) Control of ingot heating temperature:

[0007] The heating temperature of 35CrNi3Mo die-cast steel ingot is 1210℃-1230℃, and the temperature is kept at 0.6h / 100mm. The maximum residence time after the temperature is kept is ≤2h / 100mm;

[0008] 2) Control of the initial temperature of die-cast steel ingot forging:

[0009] After the heat preservation is completed, take it out and cool it down quickly in the air. The air cooling time is (3.75-4.25)×D 1 / 2 min control, where D is the average diameter of the heated ingot, in mm, and then forging is performed on the precision forging machine;

[0010] 3) Control of forging ratio and post-forging cooling

[0011] The total forging ratio of the precision forging machine is controlled at above 2.8. After forging, the forgings are air-cooled to a surface temperature of 480℃-530℃, and then loaded into a 600℃-650℃ furnace for waiting and annealing.

[0012] Further: 1) In the control of the heating temperature of the steel ingot: the mold-cast steel ingot is hot-delivered, the average temperature of the steel ingot is above 450°C, and it is placed in a 650°C-850°C furnace for insulation, and the insulation time is 0.5h / 100mm, and then the temperature is raised to 1210°C-1230°C at a heating rate of ≤100°C / h.

[0013] Further: 1) In the control of the heating temperature of the steel ingot: the die-cast ingot with an average diameter of φ657 mm is placed in a 680°C-730°C furnace, kept warm for 3.5 hours, and then heated to 1210°C-1230°C for 6 hours.

[0014] Technical effects of the present invention:

[0015] The problem of segregation lines in the fracture structure of 35CrNi3Mo gun steel forgings was solved by using improved heating temperature, cooling and forging technology.

[0016] The method of using high temperature heating of die-cast steel ingots and air cooling of discharge materials to reduce the forging temperature and terminal temperature to accelerate the cooling rate of forgings ensures that the fibrous proportion of the quenched and tempered fracture structure in the forgings is increased. The problem of scrapping of 35CrNi3Mo die-cast ingots due to fracture segregation lines is reduced.

[0017] Furthermore, the forging quenched and tempered fracture structure is 100% fibrous without any segregation line.

[0018] Furthermore, by using forging temperature control technology, the qualified rate of fracture structure in forgings forged by 35CrNiMo die-cast ingot precision forging machine (technical index: segregation line ≤ Grade I) was increased from 77.5% to 100%, and all performance indexes of forgings were qualified, the actual grain size was ≥ Grade 5.0, and no abnormalities were found during the trial production process. DETAILED DESCRIPTION

[0019] The present invention is described in further detail below.

[0020] The principle of the present invention is:

[0021] The heating temperature of 35CrNi3Mo die-cast steel ingot is 1210℃-1230℃, and the temperature is kept at 0.6h / 100mm. The maximum residence time after keeping is ≤2h / 100mm. The purpose is to dissolve the BN and CrN precipitates that solidify and precipitate from the die-cast steel ingot. After heating and keeping, take it out and cool it down quickly in the air. The air cooling time is controlled by (3.75-4.25)×D1 / 2min, and then it is forged by a precision forging machine to prevent BN and CrN from precipitating again. The total forging ratio of the precision forging machine is controlled at more than 2.8 to break the coarse grains. After forging, the forging is air-cooled to a surface temperature of 480℃-530℃, and then loaded into a 600℃-650℃ furnace for waiting and annealing. Specific implementation method 1

[0023] 1. Control of ingot heating temperature:

[0024] The die-cast steel ingots are delivered hot, with an average temperature of over 450°C. They are placed in a 650°C-850°C furnace for insulation for 0.5h / 100mm. The temperature is then raised to 1210°C-1230°C at a heating rate of ≤100°C / h. When they are heated, they are then kept warm for 0.6h / 100mm. The maximum residence time after insulation is ≤2h / 100mm.

[0025] 2. Control of the starting temperature of die-cast steel ingot forging:

[0026] After the die-cast steel ingot is heated and insulated, it is taken out and cooled in the air. The air cooling time is (3.75-4.25)×D 1 / 2 min, where D is the average diameter of the heated ingot, in mm. After the air cooling time reaches the requirement, forging on the fine forging machine begins.

[0027] 3. Control of forging ratio and post-forging cooling

[0028] After high-temperature heating, the total forging ratio of the precision forging machine is controlled above 2.8. After forging, the forgings are air-cooled to a surface temperature of 480℃-530℃ and loaded into a 600℃-650℃ furnace for stripping and annealing. Specific implementation method 2

[0030] 1. Put 32 3.25t die-cast ingots with an average diameter of φ657mm into a 680℃-730℃ furnace in two batches, 16 in each furnace, keep warm for 3.5 hours, then heat to 1210℃-1230℃ for 6 hours and keep warm for 4 hours.

[0031] 2. After the ingot is heat-insulated, it is taken out and air-cooled for 10 minutes. Then it is forged on a precision forging machine. The forging is divided into three passes to press the large head to φ325mm and four passes to press the small head to 265mm. The forging ratios are 4.08 and 6.12 respectively. The final forging temperature is controlled at 780℃-850℃. After forging, it is cooled in the air to the surface temperature of the forging of 480℃-530℃, and then loaded into a 600℃-650℃ furnace for waiting and annealing. The first furnace forged 15 pieces for a total of 7.5h, and the second furnace for 15 pieces for a total of 9h, within the longest residence time.

[0032] 3. After annealing, the forgings were sliced ​​at both ends for fracture microstructure testing. 12 forgings were sliced ​​at both ends, and the fracture microstructures were tested after the specimens were quenched and tempered. All 24 fracture microstructures were 100% fibrous.

[0033] 4. After rough machining, the forgings are subjected to quenching and tempering heat treatment, and the quenching and tempering forging blanks are sliced ​​at both ends for fracture, performance, and grain size testing. 32 heat-treated pieces are sliced ​​at both ends for fracture and performance testing. The fracture structures are all 100% fibrous, and no other fracture structures are found. The yield strength Rp0.2 is between 970Mpa-1005Mpa, which is higher than the index of 835Mpa. The room temperature impact ku is between 38J-47J, which is higher than the index of 17J. The actual grain size is between 6.0 and 7.5.

Claims

1. A method for controlling the forging temperature of a 35CrNi3Mo die casting ingot precision forging machine. It is characterized in that The method includes the following: 1) Control of ingot heating temperature: The heating temperature of 35CrNi3Mo die-cast steel ingot is 1210℃-1230℃, and the temperature is kept at 0.6h / 100mm. The maximum residence time after the temperature is kept is ≤2h / 100mm; 2) Control of the initial temperature of die-cast ingot forging: After the heat preservation is completed, take it out and cool it down quickly in the air. The air cooling time is (3.75-4.25)×D 1 / 2 min control, where D is the average diameter of the heated ingot, in mm, and then forging is performed on the precision forging machine; 3) Control of forging ratio and post-forging cooling The total forging ratio of the precision forging machine is controlled at above 2.

8. After forging, the forgings are air-cooled to a surface temperature of 480℃-530℃, and then loaded into a 600℃-650℃ furnace for waiting and annealing.

2. A forging temperature control method for a 35CrNi3Mo die casting ingot precision forging machine according to claim 1, It is characterized in that 1) Control of ingot heating temperature: The die-cast ingot is hot-delivered, and the average temperature of the ingot is above 450°C. It is placed in a 650°C-850°C furnace for insulation. The insulation time is 0.5h / 100mm, and then the temperature is raised to 1210°C-1230°C at a heating rate of ≤100°C / h.

3. A forging temperature control method for a 35CrNi3Mo die casting ingot precision forging machine according to claim 1, It is characterized in that 1) Control of the heating temperature of the steel ingot: The die-cast ingot with an average diameter of φ657 mm is placed in a 680℃-730℃ furnace, kept warm for 3.5 hours, and then heated to 1210℃-1230℃ for 6 hours.

4. A forging temperature control method for a 35CrNi3Mo die casting ingot precision forging machine according to claim 3, It is characterized in that 2) Control of the initial temperature of die-cast ingot forging: After the ingot is heated, take it out and air cool it for 10 minutes. 3) Control of forging ratio and post-forging cooling Forging is performed on a precision forging machine in three passes to a large head of φ325mm and in four passes to a small head of 265mm, with forging ratios of 4.08 and 6.12 respectively; the final forging temperature is controlled at 780℃-850℃, and after forging, it is cooled in air to a surface temperature of 480℃-530℃, and then loaded into a 600℃-650℃ furnace for waiting and annealing.