Conductive particle arrangement film, manufacturing method thereof, inspection probe unit, and conduction inspection method

By using conductive particles to configure the film in the conduction inspection probe unit, the problem of high-precision conduction inspection on non-smooth semiconductor devices is solved, low-resistance and high-precision conduction inspection are achieved, and appearance damage is avoided.

CN114221146BActive Publication Date: 2024-11-22DEXERIALS CORP
View PDF 17 Cites 0 Cited by

Patent Information

Application Number
CN202111522759.2
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Priority Date
2016-11-30
Filing Date
2017-11-20
Publication Date
2024-11-22
Estimated Expiration
2037-11-20

AI Technical Summary

Technical Problem

The existing conduction inspection probe unit is difficult to achieve high-precision conduction inspection on non-smooth semiconductor devices, and it is easy to lead to poor appearance.

Method used

The conductive particle configuration film is adopted. The depth of the conductive particles buried in the elastomer film is approximately the same as its average particle diameter, and is arranged in the surface direction. It is used as a inspection probe material, connector or adapter to form a conductive particle configuration film through a transfer mold. , and applied on the electronic circuit board for conduction inspection.

Benefits of technology

High-precision conduction inspection in non-smooth areas is realized, the on-resistance value is reduced, and the appearance is avoided, and it is suitable for conduction inspection of micro-pitch and non-micro-pitch.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN114221146B_ABST
    Figure CN114221146B_ABST
Patent Text Reader

Abstract

The conductive particle configuration film of the present invention is useful for an inspection probe unit for conducting a conduction inspection of a micro-pitch conduction inspection object such as a semiconductor device, and conductive particles are configured in the surface direction of an elastomer film. The thickness of the elastomer film is roughly consistent with the average particle size of the conductive particles. The ends of the conductive particles are located near the outermost surfaces of each of the two sides of the elastomer film. The same or different conductive particle configuration films may also be stacked. An adhesive layer may also be formed on at least one side of the conductive particle configuration film.
Need to check novelty before this filing date? Find Prior Art

Description

[0001] This application is a divisional application; the application number of the parent application is "2017800707014", and the name of the invention is "Conductive particle configuration film, its manufacturing method, inspection probe unit, and conductivity inspection method". Technical Field

[0002] The present invention relates to a conductive particle arrangement film useful as an inspection probe material of an inspection probe unit used in a continuity inspection of a semiconductor device or the like, an anisotropic conductive connector, or an anisotropic conductive adapter. Background Art

[0003] In the case of conducting a semiconductor device, a test probe unit is generally used, which is formed by connecting a probe material to a circuit substrate for inspection. The probe material has a plurality of fine rod-shaped electrodes arranged in the surface direction. However, the inspection target area is not necessarily smooth but has concavities and convexities, so the existing simple test probe unit cannot follow the concavities and convexities of the inspection target area, and there is a concern that a high-precision conduction test result cannot be obtained. In addition, since the probe material is directly crimped to the terminal of the semiconductor device, there is also a concern that the appearance of the inspection area may be poor. Therefore, in order to prevent the reduction of the inspection accuracy caused by the concavities and convexities of the inspection target area during the conduction inspection and to prevent the appearance of the semiconductor device from being poor, it is considered to configure an anisotropic conductive elastomer sheet (Patent Document 1) as an anisotropic conductive connector between the probe material in the inspection probe unit and the circuit substrate for inspection. The anisotropic conductive elastomer sheet is isolated in the surface direction and has a conductive particle group that is continuous in the thickness direction due to a parallel magnetic field (Patent Document 2).

[0004] Prior art literature

[0005] Patent Literature

[0006] Patent Document 1: Japanese Patent Application Laid-Open No. 10-188672

[0007] Patent Document 2: Japanese Patent Application Publication No. 2009-98065 Summary of the invention

[0008] Problems to be solved by the invention

[0009] However, in the anisotropic conductive elastomer sheet of Patent Document 1, the conductive particle group that is continuous in the thickness direction may be bent due to the influence of the magnetic field, and in order to stably ensure the insulation between the conductive particle groups that are isolated in the plane direction, there is a problem that the fine pitch of the anisotropic conductive elastomer sheet in the plane direction must be sacrificed. In addition, since there are many specifications for inspection in such a sheet, a component with better operability is required.

[0010] The subject of the present invention is to obtain high-precision continuity test results and avoid appearance defects when using an inspection probe unit to perform a continuity inspection of a micro-pitch continuity inspection object such as a semiconductor device, even if the inspection object area is not smooth but has unevenness. In addition, the present invention provides a continuity inspection component that is easy to use and has excellent operability even if the inspection object area is smooth and the continuity inspection object is not micro-pitch.

[0011] Solutions to Solve Problems

[0012] The inventors have discovered that, instead of the anisotropic conductive elastomer sheet of Patent Document 1, a conductive particle configuration film in which conductive particles are embedded at half the depth direction of an elastomer film having a thickness approximately equal to its average particle size and configured in the surface direction can be used as an inspection probe material, an anisotropic conductive connector, or an anisotropic conductive adapter, thereby solving the above-mentioned problems and completing the present invention.

[0013] That is, the present invention provides a conductive particle arrangement film, in which conductive particles are arranged in the surface direction of an elastomer film, wherein:

[0014] The thickness of the elastomer film is roughly consistent with the average particle size of the conductive particles.

[0015] The ends of the conductive particles are located near the outermost surfaces of both surfaces of the elastomer film.

[0016] Furthermore, the present invention provides a manufacturing method, which is a manufacturing method of the above-mentioned conductive particle arrangement film, wherein:

[0017] Conductive particles are arranged in the concave portions of a transfer mold having multiple concave portions formed along a planar direction, and the conductive particles are transferred by pressing an elastomer film against the concave forming surface of the transfer mold. The elastomer film with the transferred conductive particles is clamped between a pair of flat plates, and the conductive particles are pressed into the elastomer film by heating and pressurizing.

[0018] Furthermore, the present invention provides an inspection probe unit, wherein the above-mentioned conductive particle arrangement film is provided on an electronic circuit substrate for conduction inspection as an inspection probe material.

[0019] In addition, the present invention provides an inspection probe unit, comprising an electronic circuit substrate for conducting inspection, and a probe material having an electrode structure that is in electrical conduction with the electronic circuit substrate for conducting inspection, wherein:

[0020] The above-mentioned conductive particle arrangement film is arranged as an anisotropic conductive connector between the electronic circuit board for conduction inspection and the probe material.

[0021] In addition, the present invention provides an inspection probe unit, comprising an electronic circuit substrate for conducting inspection, and a probe material having an electrode structure that is in electrical conduction with the electronic circuit substrate for conducting inspection, wherein:

[0022] The above-mentioned conductive particle arrangement film is arranged as an anisotropic conductive adapter at the tip of the probe material on the side opposite to the electronic circuit board for continuity inspection.

[0023] Furthermore, the present invention provides an inspection probe unit, comprising an electronic circuit substrate for conducting inspection, and a probe material having an electrode structure that is in electrical conduction with the electronic circuit substrate for conducting inspection, wherein:

[0024] The conductive particle arrangement films as anisotropic conductive adapters are arranged at the tip of the probe material on the side opposite to the continuity test electronic circuit board and at the tip of the probe material on the side opposite to the continuity test electronic circuit board.

[0025] In addition, the present invention also provides a continuity inspection method, wherein the inspection probe unit described above is applied to a continuity inspection object.

[0026] The effects of the invention are as follows.

[0027] In the conductive particle configuration film of the present invention, the conductive particles are embedded in the half position in the depth direction of the elastic film having a thickness substantially equal to its average particle size and are configured in the surface direction. Therefore, it is not necessary to connect the conductive particles in the film thickness direction, so that the continuity inspection of the micro-pitch continuity inspection object (e.g., rectangular terminals with a width of 2 to 15 μm, terminals with a distance between terminals of 3 to 25 μm, etc.) of the semiconductor device can be performed. In addition, in order to improve the accuracy of the continuity inspection, for example, in the case of a continuity inspection with a lower resistance value of less than 1000 mΩ, a plurality of conductive particles can be brought into contact with the terminal, so that even if the distance between the terminals of the continuity inspection object is larger than the above range, the continuity inspection can be performed with low resistance and high precision. In addition, since it is pressed roughly in a plane with the continuity inspection object, the appearance of the continuity inspection object can be avoided. In addition, it is also possible to perform high-precision continuity inspection on the continuity inspection object with a smooth inspection object area and the non-micro-pitch continuity inspection object. In other words, it is possible to easily and non-destructively determine whether the continuity is on or not for the continuity inspection object.

[0028] Furthermore, the inspection probe unit having the conductive particle arrangement film of the present invention can achieve the inventive effect produced by the conductive particle arrangement film of the present invention. Furthermore, if the conductive particle arrangement film corresponds to a fine pitch, it can be applied to a conduction inspection object with a wider pitch without changing the design of the conductive particle arrangement film. BRIEF DESCRIPTION OF THE DRAWINGS

[0029] Figure 1It is a cross-sectional view of the conductive particle arrangement film of the present invention.

[0030] Figure 2 It is a cross-sectional view of the conductive particle arrangement film of the present invention.

[0031] Figure 3A This is a diagram for explaining the positional relationship between the outermost surface of the elastic film and the conductive particles.

[0032] Figure 3B This is a diagram for explaining the positional relationship between the outermost surface of the elastic film and the conductive particles.

[0033] Figure 3C This is a diagram for explaining the positional relationship between the outermost surface of the elastic film and the conductive particles.

[0034] Figure 4A It is a cross-sectional view of the laminated conductive particle arrangement film of the present invention.

[0035] Figure 4B It is a cross-sectional view of the laminated conductive particle arrangement film of the present invention.

[0036] Figure 5A This is a cross-sectional view of the laminated conductive particle arrangement film of the present invention using a flexible connector sheet.

[0037] Figure 5B This is a cross-sectional view of the laminated conductive particle arrangement film of the present invention using a flexible connector sheet.

[0038] Figure 5C yes Figure 5B Top view of the conductive particle configuration film.

[0039] Figure 5D This is a cross-sectional view of the laminated conductive particle arrangement film of the present invention using a flexible connector sheet.

[0040] Fig. 6A This is a schematic cross-sectional view of an inspection probe unit using the conductive particle arrangement film of the present invention as an inspection probe.

[0041] Figure 6B This is a schematic cross-sectional view of an inspection probe unit using the conductive particle arrangement film of the present invention as an anisotropic conductive connector.

[0042] Figure 6C This is a schematic cross-sectional view of an inspection probe unit using the conductive particle arrangement film of the present invention as an anisotropic conductive adapter. DETAILED DESCRIPTION

[0043] Hereinafter, an example of the conductive particle arrangement film of the present invention will be described in detail with reference to the drawings. In the drawings, the same reference numerals represent the same or equivalent components.

[0044] <Overall structure of conductive particle arrangement film>

[0045] Figure 1 2 is a cross-sectional view of a conductive particle arrangement film 10 of the present invention. The conductive particle arrangement film 10 has conductive particles 1 arranged in the surface direction of the elastomer film 2. Here, "arranged in the surface direction" means that when the conductive particle arrangement film 10 is viewed from above, the conductive particles 1 are arranged in a state of being separated from each other (preferably in a state of being arranged regularly (for example, in a square lattice, a rectangular lattice, a rhombus lattice, or a hexagonal lattice)). In this case, it is also possible to Figure 2 As shown, a plurality of conductive particles 1 are assembled or connected on a plane to form a unit and isolated from each other. As for the minimum distance of isolation (the shortest distance between conductive particles), as an example, in order to avoid unnecessary contact between conductive particles, it is preferably 0.5 times or more of the conductive particle diameter, and more preferably 0.7 times or more. The upper limit is not particularly limited and can be appropriately set according to the object, but as an example for micro-pitch, it is preferably less than 10 times the conductive particle diameter, more preferably less than 5 times, and further preferably less than 2 times. In addition, the conductive particles 1 are configured to be isolated from each other, which means that, for example, in an area of ​​a rectangle or square with a conductive particle number of more than 1000, preferably more than 2000, the total number of conductive particles is preferably more than 95%, more preferably more than 98%, and further preferably more than 99.5% are independent. In the case of intentional connection, the connected conductive particles are counted as one number of conductive particles (the conductive particle diameter refers to the size of each conductive particle).

[0046] Furthermore, the distance between the conductive particles and the distance between the terminals of the continuity inspection object do not have to be the same, and the distance between the conductive particles is preferably smaller than the distance between the terminals of the continuity inspection object. The reason is that by making a plurality of conductive particles contact the terminals of the continuity inspection object, the conduction resistance value can be reduced. Therefore, the number of conductive particles in contact with the terminals can be one, but preferably three or more, and more preferably eleven or more.

[0047] In the conductive particle arrangement film 10 of the present invention, Figure 1 As shown, the thickness t of the elastic film 2 is roughly consistent with the average particle size d of the conductive particles 1. The reason for "roughly consistent" is that the conductive particles can be connected to both sides of the film and can be pressed to the object of the continuity inspection in a roughly flat manner. Generally, there is a relationship of 0.70d≤t≤1.10d.

[0048] In addition, regarding the positional relationship between the elastic film 2 and the conductive particles 1, in the present invention, the ends of the conductive particles 1 need to be located near the outermost surfaces of both sides of the elastic film 2. Figure 3A to Figure 3C The state of "nearby" is shown. Figure 3AThe state in which the end portion of the conductive particle 1 is in contact with the surface of the elastomer film 2 is shown. Figure 3B The end of the conductive particle 1 is shown embedded in the elastomer film 2 from the surface of the film. The embedding depth (elastomer coating thickness) a is usually within 10% of the thickness from one side of the surface of the elastomer film 2, and preferably within 5%. Figure 3C The state where the end of the conductive particle 1 is exposed from the surface of the elastomer film 2 is shown. The exposed height b is preferably within 30% of the thickness from one side of the surface of the elastomer film 2. Therefore, regarding the pattern "near" both sides of the elastomer film 2, it is assumed that both sides are Figure 3A , Figure 3B or Figure 3C The shape of Figure 3A The other side is Figure 3B The shape of Figure 3A The other side is Figure 3C The shape and one side is Figure 3B The other side is Figure 3C Furthermore, the degree of the conductive particles exposed from the elastomer film and the degree of coverage by the elastomer may be the same or different on one side of the conductive particle arrangement film and the other side.

[0049] (Elastomer film 2)

[0050] The thickness t of the elastomer film 2 is mainly determined by the surface unevenness of the conduction inspection object, the handleability of the conductive particle configuration film, etc., but can be appropriately adjusted according to the stacking form of the conductive particle configuration film as described below. In the case of application to semiconductor devices, if the bump height and its deviation are considered, it is preferably 3 μm or more, more preferably 10 μm or more, and particularly preferably 30 μm or more. The upper limit of the thickness is not particularly limited, but considering the handleability of the conductive particle configuration film, micro-pitch correspondence, etc., it is usually 200 μm or less, preferably 100 μm or less, and more preferably 50 μm or less. In addition, the thickness t of the elastomer film 2 can be measured using a known film thickness meter (for example, FUJIWORK Co., Ltd., film testing machine thickness measuring instrument, HKT Handy series).

[0051] As the elastomer film 2 described above, conjugated diene rubbers such as polybutadiene, natural rubber, polyisoprene, SBR, NBR and their hydrides, block copolymers such as styrene-butadiene-diene block copolymers, styrene-isoprene block copolymers and their hydrides, chloroprene, polyurethane rubber, polyester rubber, epichlorohydrin rubber, silicone rubber, ethylene-propylene copolymers, ethylene-propylene-diene copolymers, silicone rubber and other elastomer films can be cited. When the elastomer film 2 needs to have weather resistance, it is preferably an elastomer film other than conjugated diene rubber, especially from the viewpoint of forming processability and electrical properties, preferably silicone rubber film. In addition, anisotropic conductive connecting materials such as thermosetting anisotropic conductive films, thermosetting electronic device connecting materials not containing conductive particles, adhesive compositions for electronic devices, adhesive compositions, and resin compositions for bottom filling purposes can also be included. In addition, a plurality of identical or different films can also be stacked to make a laminated elastomer film 2. From the viewpoint of convenience, it is desirable that the elastic film 2 has the property of being attachable to and detachable from the continuity inspection object during inspection. This point can be one of the major differences compared with known curable adhesive films for electronic components (eg, thermosetting anisotropic conductive films).

[0052] In addition, when a heat-cured elastic film is used as the elastic film 2, the laminated elastic film has the effect of providing more options for manufacturing conditions. In addition, it is possible to fine-tune the inspection conditions by laminating various films before the inspection process, or to black-box the inspection process itself. Furthermore, when the elastic film 2 does not include a heat-cured elastic film and is composed of a composition substantially the same as that of a slightly adhesive adhesive film, there are more options for handling the inspection process, such as replacing each continuity inspection object. In the case of the laminated type, it is sufficient to adjust to the desired characteristics by combining in this way.

[0053] (Conductive particles 1)

[0054] On the other hand, the average particle size of the conductive particles 1 is a size roughly consistent with the elastomer film, usually less than 200 μm, preferably more than 2 μm and less than 50 μm, more preferably more than 2.5 μm and less than 30 μm, and particularly preferably more than 2.8 μm and less than 20 μm. In addition, in order to improve the accuracy of the conduction inspection, it is desired that the conductive particle size is uniform. Specifically, the CV value (conductive particle size standard deviation / average particle size of the conductive particles) is preferably less than 20%, more preferably less than 10%, and further preferably less than 5%. In addition, the smaller the lower limit of the CV value, the more uniform the particle size is, and thus there is no particular restriction.

[0055] Furthermore, as the conductive particles 1, metal particles showing magnetic properties such as nickel, iron, and cobalt or their alloy particles, non-magnetic solder particles, etc. can be cited. The above-mentioned particles may also contain precious metals such as gold, silver, palladium, and rhodium, preferably containing gold or silver. Furthermore, the above-mentioned metal particles or alloy particles may be used as cores, and the surface of the cores may be coated with precious metals by electroplating, electroless plating, sputtering, vacuum evaporation, etc. Alternatively, inorganic particles such as non-magnetic metal particles or glass beads or organic polymer particles may be used as cores, and the cores may be coated with conductive magnetic bodies such as nickel and cobalt, and coated with precious metals, and the particles thus obtained may be used as conductive particles 1. In the case of using metal-coated resin particles obtained by coating with metals or the like using organic polymer particles as cores, it is easy to adjust the conductive state from the deformation of the conductive particles during pressurization and the reaction of the organic polymer particles, which is preferred in this regard. Furthermore, metal-coated resin particles containing conductive microparticles obtained by coating with metals or the like may also be used. The effect of further reducing the on-resistance value can be expected. In the present invention, two or more types of the above-mentioned conductive particles 1 may be used simultaneously.

[0056] (Lamination of Conductive Particle Arrangement Films)

[0057] The conductive particle arrangement film 10 of the present invention is intended to increase its overall thickness, and a plurality of the same conductive particle arrangement films 10 ( Figure 4A Furthermore, when stacking, a plurality of different conductive particle configuration films 10 and 11 can also be stacked ( Figure 4B In the latter case, since conductive particles having relatively different particle sizes are used in the conductive particle arrangement film 10 and the conductive particle arrangement film 11, it is easy to maintain the connection state of the conductive particles in the thickness direction of the conductive particle arrangement film, which is preferred.

[0058] Furthermore, when the conductive particle arrangement film 10 is stacked, the conductive particle arrangement film 10 and a flexible connector sheet may be stacked and made into a unit. The flexible connector sheet may have through-electrodes formed on an insulating flexible sheet. Figure 5A As shown in FIG. 1 , a flexible connector sheet 32 ​​having through electrodes 31 is sandwiched between two conductive particle configuration films 10 (see Japanese Patent No. 3951333). In this case, Figure 5B As shown, in the conductive particle configuration film 10, corresponding to the through electrode 31, there may be one or two conductive particles, but preferably more (preferably three or more, more preferably ten or more) conductive particles 1 are configured. The plurality of conductive particles 1 configured corresponding to one through electrode 31 may be connected to each other, or may be connected as shown in FIG. Figure 5CAs shown, when viewed from above, the plurality of conductive particles 1 (upper) corresponding to one through electrode 31 are not connected to each other but are independently isolated and arranged. At this time, it is preferred that the conductive particles 1 (lower) of the conductive particle arrangement film arranged below the flexible connector sheet do not overlap with the conductive particles 1 (upper) of the conductive particle arrangement film arranged above the flexible connector sheet. Figure 5C Such a configuration state of conductive particles can be formed, for example, by changing the distance or number between conductive particles, or by making the configuration pattern itself different, or by changing the angle relative to the reference line in the case of the same configuration pattern. As the reference line, for example, one side of the conductive particle configuration film, one side of the terminal, etc. can be used. This can prevent the deviation of the pressing force during the conduction test. In addition, it is also possible to Figure 5D As shown, the conductive particles 1 exist in the region S of the conductive particle arrangement film 10 that does not face the through-electrode 31 .

[0059] The insulating flexible sheet may be, for example, an FPC using a known polyimide, or a sheet having through holes and electrodes provided in a material used as a buffer material such as a silicone rubber sheet. Moreover, their thickness can be appropriately set in the same manner as the conductive particle configuration film 10 according to the purpose of inspection. The number of stacked sheets is not particularly limited and can be appropriately set according to the purpose of stacking. The overall thickness including the insulating flexible sheet is the same as the overall thickness of the stacked conductive particle configuration film 10 described later.

[0060] In addition, the film thickness t of the conductive particle configuration film disposed on the inner side of the stacked conductive particle configuration film and the average particle size d of the conductive particles may not satisfy the relationship of 0.70d≤t≤1.10d. The reason is that, as described above, when a through electrode is provided on the insulating flexible sheet, if the through electrode protrudes from the surface of the insulating flexible sheet, the conductive particles present in the conductive particle configuration film located on the inner side of the stack are pressed by the protruding through electrode. In addition, it is also assumed that an elastomer film 2 (a component after the conductive particles are removed from the conductive particle configuration film) is stacked on at least one side of the conductive particle configuration film. The reason is that if the through electrode protrudes from the surface of the insulating flexible sheet, a resin is required to fill the space around the protruding through electrode. In addition, with respect to stacking, a conductive particle configuration film in which conductive particles with smaller particle sizes are closely laid and a conductive particle configuration film composed of conductive particles with larger particle sizes (as an example, 10 to 50 μm, preferably 10 to 30 μm) can be stacked. The conductive particle configuration film with conductive particles having a smaller particle size (2 to 9 μm as an example) tightly laid can set the conductive particles of 2 to 9 μm to a hexagonal lattice or a configuration based thereon (a lattice slightly deformed or stretched from a hexagonal lattice, a square lattice, a lattice with conductive particles at the center of a square lattice, etc.). In order to become the required conduction path, the conductive particles with a larger particle size can be sandwiched with conductive particles with a small particle size. If it is only a large particle size, the contact between the particles may be insufficient, so it can be considered that the small particle size plays an auxiliary role. The large particle size is more than 2 times the small particle size, preferably more than 2.5 times, and more preferably more than 3 times. In order to easily design the conductive path, the arrangement of the small particle size and the large particle size is similar, so that the arrangement is preferably the same. In addition, it is preferred to arrange differently in order to avoid forming irregular conductive paths in the direction of the film surface.

[0061] Furthermore, when a plurality of conductive particles are arranged corresponding to the through-electrode 31, the conductive particle diameter becomes relatively smaller than when one conductive particle is arranged, and the thickness of the stacked conductive particle arrangement film 10 becomes thinner accordingly. Therefore, by stacking two or more groups, preferably four or more groups, of the unit composed of the conductive particle arrangement film 10 and the flexible connector sheet 32, the overall thickness can be easily increased to a thickness of, for example, 30 μm or more, so that it can be easily adapted to the inspection of various conduction inspection objects represented by semiconductor devices. In general semiconductor packages, the height of the solder electrode is about 100 μm. Considering this aspect, it is desirable to set the thickness to about 400 μm (in this case, the stacking type is preferred from the relationship between the thickness and the size of the conductive particles). Moreover, in recent years, when the terminal of the semiconductor device contains Au, in order to reduce the material cost, the demand for low profile has become higher. For example, it is 8 μm or less, preferably 6 μm or less, and more preferably 3 μm or less. In this case, or when the inspection is performed before the terminal is set (an example of a state where the conduction inspection object is roughly smooth), the conductive particle arrangement film 10 can also be 30 μm or less.

[0062] In addition, in consideration of the actual application to the conduction inspection, the overall thickness of the laminated conductive particle configuration film 10 (in the case of an insulating flexible sheet as described above, the total thickness including the insulating flexible sheet) is set according to the bump height of the conduction inspection object such as a semiconductor device or semiconductor package, a wiring substrate with electrodes, etc., and the lower limit direction is preferably 20 μm or more, more preferably 30 μm or more, and further preferably 50 μm or more, and the upper limit direction is preferably 400 μm or less, more preferably 200 μm or less, and further preferably 150 μm or less. In addition, when the electrodes having a circuit formed on the substrate of the conduction inspection object are protected by a passivation film of about several μm thickness, there are cases where it can be applied even if it is thinner than the above-mentioned overall thickness range.

[0063] In addition, in the case of a laminated conductive particle configuration film, the conductive particles in the outermost elastomer film can also be configured on one side in a hexagonal lattice pattern or a lattice pattern after deforming it. The reason is that the number density of the conductive particles can be increased. In order to easily identify the pattern shape, it can also be configured on one side in a square lattice, a rectangular lattice or a lattice pattern after deforming it. In addition, a regular configuration can also be set corresponding to the terminal arrangement. For example, since the terminals are generally rectangular or circular, by setting a configuration similar to the outer shape of the above-mentioned terminals, it is possible to determine whether the conduction is being checked.

[0064] In addition, whether or not it is a stacked type, two or more conductive particle configuration films having different conduction paths relative to the terminals of the conduction inspection object are prepared, and they are respectively applied to the conduction inspection of the same semiconductor device or other conduction inspection object, so that the conduction failure of the terminals of the conduction inspection object can be accurately determined. Here, different conduction paths refer to the path from the conductive particles in contact with the terminals of the conduction inspection object to the receiving part (the conduction part of the inspection probe unit described later) for detecting conduction, and the conductive parts such as conductive particles and through electrodes are different in the film cross-section. By designing the configuration of conductive particles for each conductive particle configuration film according to the terminal shape and terminal arrangement state of the conduction inspection object such as the semiconductor device, two or more conductive particle configuration films with different conduction paths can be obtained. Alternatively, by changing the angle of the plane direction so that a conductive particle configuration film is in contact with the conduction inspection object such as the semiconductor device (for example, by changing the conductive particle configuration film at a changed angle), the conduction inspection can be realized using a conductive particle configuration film that actually has two different conduction paths. The reason for this is that by comparing the inspection results obtained in this way, it is possible to cope with fine pitches and to expand the inspectable range with one or a minimum number of sheets.

[0065] In addition, the conductive particle configuration film 10 of the present invention may also be formed with an adhesive layer on at least one side. By providing an adhesive layer, the conductive particle configuration film 10 can be loaded and unloaded relative to the conduction inspection object, etc. In addition, since such an adhesive layer is a component different from the elastomer film, the adhesive layer covers the ends of the conductive particles and functions as a protective material for the conductive particles. Therefore, by providing such an adhesive layer, the conduction inspection using the conductive particle configuration film 10 can be stably performed multiple times. In addition, when an adhesive layer is provided, it can be provided not only on one side of the conductive particle configuration film 10, but also on two sides. For example, if the conductive particles are metal-coated resin particles described later, there is a situation where they cannot withstand multiple uses depending on the inspection conditions. Even so, it is also desirable to be able to load and unload, and sometimes it is also preferred to provide a micro-adhesive layer. Regarding the thickness, since a micro-adhesive layer can also be provided to protect the conductive particles, the height of the conductive particles exposed from the elastomer film can be thicker. Specifically, it can be set to less than 25 μm by further adding a difference of 10% of the conductive particle diameter of 200 μm. In order to obtain sufficient adhesion, a thickness of 1 μm or more is preferred, and a thickness of 2 μm or more is more preferred.

[0066] Furthermore, the area of ​​the conductive particle configuration film 10 can be determined according to the purpose of the inspection, and can be selected from the following combinations. As an example, the lower limit of one side is preferably 0.5 mm or more, more preferably 0.8 mm or more, and further preferably 2 mm or more. It assumes the film width in the connector of a general anisotropic conductive film (i.e., the length of the short side of the driver IC, the width of the tool for actually pressing the electrode of the FPC). The larger the upper limit of one side, the more preferred it is. If practical operability is further considered, as an example, it is preferably 600 mm or less, more preferably 450 mm or less, and further preferably 300 mm or less. In addition, as the product form of the conductive particle configuration film 10, especially if transportability is considered, a roll is preferably used. And, especially if operability is considered, a single-sheet processing body is preferably used.

[0067] <Method for producing conductive particle arrangement film>

[0068] The conductive particle arrangement film of the present invention described above can be manufactured in the same manner as the conventional method for manufacturing an anisotropic conductive film in which conductive particles are regularly arranged. For example, it can be manufactured by arranging conductive particles in the concave portions of a transfer mold having a plurality of concave portions formed along a planar direction, pressing an elastomer film against the concave portion forming surface of the transfer mold to transfer the conductive particles, sandwiching the elastomer film to which the conductive particles are transferred between a pair of flat plates, and pressing the conductive particles into the elastomer film by heating and pressurizing (for example, refer to Japanese Patent No. 6187665).

[0069] <Inspecting the probe unit>

[0070] The conductive particle arrangement film of the present invention can be preferably used as an inspection probe material of an inspection probe unit, an anisotropic conductive connector, or an anisotropic conductive adapter.

[0071] As an example of the inspection probe unit of the present invention, the following can be cited: Fig. 6A As shown in FIG. 1 , the conductive particle arrangement film 10 of the present invention is provided on the electronic circuit board 50 for conducting inspection (see FIG. 1 ). Figure 1 ) as the inspection probe unit 100 of the inspection probe material. In this case, it is possible to use Figure 2 , Figure 4A , Figure 4B , Figures 5A to 5D The conductive particle arrangement film is replaced with a conductive particle arrangement film 10. In addition, as the continuity test electronic circuit board 50, a conventionally known continuity test electronic circuit board can be used.

[0072] As other examples of the inspection probe unit of the present invention, the following can be cited: Figure 6BAs shown, the conductive particle arrangement film 10 of the present invention is arranged between the continuity inspection electronic circuit substrate 50 and the probe material 60 of the inspection probe unit 200 as an inspection probe unit of an anisotropic conductive connector, wherein the inspection probe unit 200 includes the continuity inspection electronic circuit substrate 50 and the probe material 60 having an electrode structure 61 that is in electrical contact with the continuity inspection electronic circuit substrate 50. In this case, the electrode structure 61 and the probe material 60 may be conventionally known components.

[0073] Furthermore, as another example of the inspection probe unit of the present invention, there can be cited the following Figure 6C As shown, the conductive particle arrangement film 10 of the present invention is arranged at the front end of the probe material 60 of the inspection probe unit 300 on the side opposite to the electronic circuit substrate 50 for the continuity inspection as an inspection probe unit of an anisotropic conductive adapter, wherein the inspection probe unit 300 includes the electronic circuit substrate 50 for the continuity inspection and the probe material 60 having an electrode structure 61 that is conductive to the electronic circuit substrate 50 for the continuity inspection. In this case, the conductive particle arrangement film 10 of the present invention may be additionally arranged between the electronic circuit substrate 50 for the continuity inspection and the probe material 60.

[0074] Furthermore, the above-mentioned inspection probe unit sometimes needs to change specifications each time due to the bump layout, but if the conductive particle configuration film used as the probe material corresponds to the micro pitch, it can be applied to the inspection probe unit with a wider pitch without changing the design of the conductive particle configuration film, thereby having excellent economic efficiency.

[0075] <Conductivity test method>

[0076] The inspection probe unit of the present invention can be preferably applied to the continuity inspection of various electronic devices such as semiconductor devices. Specifically, the probe material of the inspection probe unit is pressed against the electrode of the electronic device as the continuity inspection object, and the resistance value between the electrode of the electronic device and the electronic circuit substrate for continuity inspection constituting the inspection probe unit is measured by a known method through a conductive particle configuration film, thereby realizing the continuity inspection.

[0077] In addition, in such a continuity test, in order to achieve a high-precision test, the lower the resistance value of each terminal to be measured, the better. As an example, if it is less than 1000mΩ, there is no problem in practical use, preferably less than 200mΩ, more preferably less than 100mΩ, and further preferably less than 50mΩ. It can be appropriately selected according to the object of inspection and the conditions of inspection. The conduction resistance value in this case is expected to be a state in which a stable resistance value is shown by applying sufficient pressure to the conduction inspection object.

[0078] The temperature conditions for the continuity test include room temperature (20°C ± 15°C), low temperature (eg -40°C), or high temperature (eg 100°C). Thermal cycle temperature conditions (-40°C / 100°C / 1000 cycles) are also included.

[0079] The terminal pitch (minimum terminal length + space between terminals) of the conduction inspection object such as semiconductor devices is generally about 200μm, and the inspection probe unit of the present invention can correspond to a narrower terminal pitch. The reason is that conductive particles with a particle size of about 2.5μm to 30μm can be arranged on the outermost surface of the inspection probe unit. Specifically, in the case where only one conductive particle is required to function as a probe, if conductive particles with a particle size of 3μm are arranged in a hexagonal lattice with a center distance of 6μm between particles, it can be set to an inspection terminal of about 10×10μm. Therefore, the terminal pitch of the conduction inspection object depends on the size of the electrode in contact with the conductive particles. If the minimum length of the electrode is set to about 10μm and the minimum distance between the electrodes is set to about 10μm, the terminal pitch can be set to about 20μm.

[0080] In addition, it is believed that the conduction resistance value measured in the conduction test depends on the material and size of the conductive particles, and the number of conductive particles in contact with the electrode, so that depending on the conduction resistance value to be measured, there are also cases where a larger terminal spacing is required. Therefore, with respect to the terminal spacing that can be applied to the conduction test, the lower limit direction is preferably 20 μm or more, more preferably 30 μm or more, and further preferably 50 μm or more, and the upper limit direction is preferably 400 μm or less, more preferably 200 μm or less, and further preferably 150 μm or less.

[0081] Industrial Applicability

[0082] In the conductive particle arrangement film of the present invention, the conductive particles are embedded in the half position in the depth direction of the elastic film having a thickness substantially equal to the average particle diameter thereof and arranged in the surface direction. Therefore, the conductive particle arrangement film of the present invention is useful for high-precision continuity inspection of a continuity inspection object with a micro pitch such as a semiconductor device. In addition, it is also useful for high-precision continuity inspection of a continuity inspection object with a smooth inspection object area and a continuity inspection object with a non-micro pitch.

[0083] Explanation of symbols

[0084] 1—conductive particles, 2—elastomeric film, 10, 11—conductive particle configuration film, 30—insulating flexible sheet, 31—through electrode, 32—flexible connector sheet, 50—electronic circuit substrate for conductivity inspection, 60—probe material, 61—electrode structure, 100, 200, 300—inspection probe unit, t—elastomeric film thickness, d—average particle size of conductive particles.

Claims

1. A laminated connector unit comprising a flexible connector sheet having a through electrode provided on an insulating elastic film and a pair of conductive particle arrangement films as a test probe material sandwiching the flexible connector sheet, wherein: The conductive particle configuration film is a conductive particle configuration film in which conductive particles are configured in the surface direction of the elastomer film, the thickness of the elastomer film is substantially consistent with the average particle size of the conductive particles, and the ends of the conductive particles are located near the outermost surfaces of both sides of the elastomer film. On each conductive particle arrangement film, a plurality of conductive particles are arranged locally corresponding to the through-electrodes in a manner that they are not connected to each other but are independently isolated. The average particle size d of the conductive particles and the thickness t of the elastomer film satisfy the following equation: 0.70d≤t≤1.10d, The conductive particles are embedded in a manner such that the ends of the conductive particles are located within 10% of the thickness from one surface of the elastomer film, or the conductive particles are exposed in a manner such that the ends of the conductive particles are located within 30% of the thickness from one surface of the elastomer film, The inter-particle distance between conductive particles locally arranged on one of the pair of conductive particle arrangement films and the inter-particle distance between conductive particles locally arranged on the other of the pair of conductive particle arrangement films are different from each other so that the conductive particles do not overlap in a plan view.

2. The connector unit according to claim 1, characterized in that The elastic film has the property of being attachable and detachable.

3. The connector unit according to claim 1, characterized in that At least 95% of all the conductive particles within the area of ​​a rectangle or square in which the number of conductive particles is 2000 or more are independently and regularly arranged in a plan view.

4. The connector unit according to claim 1, characterized in that The elastomer film is composed of cured resin.

5. The connector unit according to claim 1, characterized in that The elastic film is formed by laminating a plurality of films.

6. The connector unit according to claim 1, characterized in that The number of conductive particles locally arranged on one of the pair of conductive particle arrangement films and the number of conductive particles locally arranged on the other are different from each other so that the conductive particles do not overlap in a plan view.

7. The connector unit according to claim 1, characterized in that The arrangement pattern of the conductive particles locally arranged on one of the pair of conductive particle arrangement films and the arrangement pattern of the conductive particles locally arranged on the other are different from each other so that the conductive particles do not overlap in a plan view.

8. The connector unit according to claim 1, characterized in that The conductive particles have uniform particle sizes.

9. The connector unit according to claim 1, characterized in that The CV value of the average particle size of the conductive particles is 20% or less.

10. The connector unit according to claim 1, characterized in that More than 95% of the fully conductive particles are independent.

11. The connector unit according to claim 1, characterized in that The conductive particles are one or more selected from metal particles, alloy particles, solder particles, metal-coated resin particles, and metal-coated resin particles containing conductive fine particles.

12. A continuity inspection method, characterized in that: The connector unit according to any one of claims 1 to 11 is applied to a conduction inspection object.

Citation Information

Patent Citations

  • Conductive elastomer composition

    JP1998188672A

  • Probe member and manufacturing method thereof, and application of probe member

    JP2009098065A

  • Anisotropic conductive film and manufacturing method therefor

    CN104541411A

  • Anisotropic conductive film

    CN107112067A

  • Microparticle arrangement film, electrical connection film, electrical connection stracture and microparticle arrangement method

    CN1434980A