A mold for preparing cladding coating

By designing a mold that includes slider, substrate frame and coating thickness measurement device, the problems of traditional coating thickness inaccurate and uneven surface are solved, and precise thickness control of the cladding coating thickness and surface flattening are achieved, reducing the thickness of the coating. defects and experimental errors.

CN114262892BActive Publication Date: 2024-11-22ZHEJIANG UNIV OF TECH
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202111654537.6
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2021-12-31
Publication Date
2024-11-22
Estimated Expiration
2041-12-31

AI Technical Summary

Technical Problem

The traditional adhesive bonding powder coating method results in inaccurate coating thickness and uneven surface, resulting in defects such as cracks, shedding, spheroidization and pores after cladding, and the experimental results are relatively errors.

Method used

A mold including a base, base frame, slider, coating thickness measuring device and cutting device is designed. The slider and the base frame are moved as a whole and the external telescopic baffle and the internal telescopic baffle are combined with the vernier caliper and LED displays the screen, precisely controlling the coating thickness and cutting the excess to ensure a flat surface.

Benefits of technology

It realizes precise control of coating thickness and surface flatness, adapts to substrates of different sizes, reduces coating defects and improves the accuracy of experimental results.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN114262892B_ABST
    Figure CN114262892B_ABST
Patent Text Reader

Abstract

The present invention belongs to the technical field of substrate coating construction, and specifically relates to a mold for preparing cladding coating, including a base, a substrate frame, a slider, a coating thickness measuring device and a cutting device; the base is provided with a first slideway, and the slider is movably matched with the first slideway; the slider is connected to the substrate frame, and the substrate frame is sleeved outside the substrate; the bottom of the base is a platform, the substrate is placed on the platform, the slider and the substrate frame move along the first slideway as a whole, and the space of the substrate frame above the top of the substrate can be filled with coating; the coating thickness measuring device is used to control the coating thickness; the cutting device is used to cut the excess coating beyond the required coating thickness of the substrate. The present invention can control the coating thickness and obtain a coating with a smooth surface and accurate thickness.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the technical field of substrate coating construction, and in particular relates to a mold used for preparing a cladding coating. Background Art

[0002] Compared with plasma spraying, electron beam-physical vapor deposition and other processes, the use of laser cladding or electron beam cladding to prepare coatings has the advantages of low dilution rate, high metallurgical bonding with the substrate, fine structure, no pores and excellent high temperature oxidation resistance. Therefore, pre-coating and then cladding has great prospects in industry. However, a major disadvantage of the traditional method of coating with adhesive-bonded powder is that the coating thickness is inaccurate and the coating surface is not flat. The uneven coating leads to defects such as cracks, shedding, spheroidization and pores in the cladding layer after cladding, and the inability to accurately measure the coating thickness will also cause large errors in the experimental results. Summary of the invention

[0003] The purpose of the present invention is to solve the above technical problems and propose a mold for preparing a cladding coating.

[0004] In order to achieve the above technical objectives, the present invention adopts the following technical solutions:

[0005] A mold for preparing a cladding coating comprises a base, a substrate frame, a slider, a coating thickness measuring device and a cutting device; the base is provided with a first slideway, and the slider is movably matched with the first slideway; the slider is connected to the substrate frame, and the substrate frame is sleeved outside the substrate; the bottom of the base is a platform, the substrate is placed on the platform, the slider and the substrate frame move along the first slideway as a whole, and the space of the substrate frame above the top of the substrate can be filled with coating; the coating thickness measuring device is used to control the coating thickness; the cutting device is used to cut the excess coating beyond the coating thickness required by the substrate.

[0006] Furthermore, the substrate frame includes a fixed baffle, a pulling baffle, an outer telescopic baffle and an inner telescopic baffle, the fixed baffle is parallel to the pulling baffle, one end of the outer telescopic baffle and one end of the inner telescopic baffle are both connected to the fixed baffle; the other end of the outer telescopic baffle and the other end of the inner telescopic baffle are both connected to the pulling baffle; the substrate is located in the space surrounded by the fixed baffle, the pulling baffle, the outer telescopic baffle and the inner telescopic baffle, and the stretching lengths of the outer telescopic baffle and the inner telescopic baffle are adapted to the size of the substrate.

[0007] Furthermore, the substrate frame also includes a mounting platform, the mounting platform is provided with a second slideway, and the baffle is pulled to movably cooperate with the second slideway;

[0008] Furthermore, the pulling baffle is provided with a mounting groove, the other end of the outer telescopic baffle is located in one mounting groove and connected to the pulling baffle, and the other end of the inner telescopic baffle is located in another mounting groove and connected to the pulling baffle.

[0009] Furthermore, the mounting platform is provided with a first screw hole, and the sliding block is provided with a second screw hole matched with the first screw hole.

[0010] Furthermore, the slide block is provided with a channel, the first slideway is cylindrical, and the channel is sleeved outside the first slideway.

[0011] Furthermore, the channel wall is provided with a third screw hole, and the first slideway is provided with a fourth screw hole matched with the third screw hole.

[0012] Furthermore, the coating thickness measuring device is a vernier caliper, the lower jaw of the vernier caliper is set on the mounting table; the upper jaw of the vernier caliper is set on the slider; the length direction of the upper jaw and the length direction of the lower jaw are the same as the length direction of the pulling baffle; the upper jaw is in contact with the top of the inner telescopic baffle and the top of the outer telescopic baffle; the reading of the vernier caliper is the change in the distance between the upper jaw and the lower jaw; the switch, count reset button, and knob of the vernier caliper are all set on the slider.

[0013] Furthermore, the slider is also provided with an LED display screen for displaying the reading of the vernier caliper.

[0014] Furthermore, the cutting device is a blade, the length of which is greater than the distance between the inner telescopic baffle and the outer telescopic baffle; the blade fits the top surface of the telescopic baffle and the top surface of the outer telescopic baffle, and can move toward the upper claw for cutting.

[0015] Compared with the prior art, the beneficial technical effects of the present invention are:

[0016] (1) The present invention can control the coating thickness and obtain a coating with a smooth surface and precise thickness;

[0017] (2) The present invention can adapt to substrates of different sizes through the telescopic performance of the outer telescopic baffle and the inner telescopic baffle;

[0018] (3) The present invention enables the slider and the substrate frame to move as a whole along the first slideway of the base, so that the portion of the substrate frame that is higher than the top surface of the substrate is filled with the coating;

[0019] (4) The present invention can accurately control the coating thickness through a vernier caliper. BRIEF DESCRIPTION OF THE DRAWINGS

[0020] Figure 1 This is the overall structure diagram of this embodiment;

[0021] Figure 2 This is a schematic diagram of the structure when used in this embodiment;

[0022] Figure 3 This is a structural diagram of the base of this embodiment;

[0023] Figure 4 This is a structural diagram of the substrate frame of this embodiment;

[0024] Figure 5 This is a diagram of the shrinkage structure of the substrate frame of this embodiment;

[0025] Figure 6 This is a structural diagram of the slider in this embodiment;

[0026] Figure 7 FIG. 4 is a structural diagram of a substrate having a smooth coating according to this embodiment.

[0027] In the figure, 1 is a base, 11 is a support plate, 12 is a first slide, 13 is a platform, 14 is a fourth screw hole, 2 is a substrate frame, 21 is an outer telescopic baffle, 22 is a pulling baffle, 23 is an inner telescopic baffle, 24 is a fixed baffle, 25 is a mounting platform, 26 is a second slide, 27 is a first screw hole, 28 is a mounting groove, 3 is a slider, 31 is a second screw hole, 32 is a third screw hole, 33 is a channel, 4 is a vernier caliper, 41 is an upper claw, 42 is a lower claw, 43 is a battery replacement cover, 44 is a switch, 45 is a count reset button, 46 is an LED display screen, 47 is a knob, 5 is a substrate, and 6 is a coating. DETAILED DESCRIPTION

[0028] The present invention is further described below in conjunction with specific embodiments, but the protection scope of the present invention is not limited thereto.

[0029] like Figure 1-7 As shown, the present embodiment is a mold for preparing a cladding coating, comprising a base 1, a substrate frame 2, a slider 3, a coating thickness measuring device and a cutting device. The base 1 is provided with a first slide 12, and the slider 3 is movably matched with the first slide 12. The slider 3 is connected to the substrate frame 2, and the substrate frame 2 is sleeved outside the substrate. The bottom of the base 1 is a platform 13, and the substrate is placed on the platform 13. The slider 3 and the substrate frame 2 move along the first slide 12 as a whole, and the space where the substrate frame 2 is higher than the top of the substrate can be filled with the coating. The coating thickness measuring device is used to control the coating thickness. The cutting device is used to cut the excess coating beyond the required coating thickness of the substrate. In order to facilitate the layout of the coating of the required thickness, after the material frame is sleeved outside the substrate, the substrate is stationary on the platform 13, and the distance value of the slider 3 and the substrate frame 2 moving along the first slide 12 as a whole is controlled by the reading of the coating thickness measuring device. After the slider 3 and the substrate frame 2 are moved to the desired position as a whole, the coating is filled to the space where the substrate frame 2 is higher than the substrate surface, and the cutting device horizontally cuts the coating along the top surface of the desired coating thickness, and after removing the excess coating, a coating with a flat surface and accurate thickness is obtained. Therefore, this embodiment can control the coating thickness, so that the substrate surface is flat and the coating with accurate thickness is obtained.

[0030] The substrate frame 2 of this embodiment includes a fixed baffle 24, a pulling baffle 22, an outer telescopic baffle 21 and an inner telescopic baffle 23. The fixed baffle 24 is parallel to the pulling baffle 22. One end of the outer telescopic baffle 21 and one end of the inner telescopic baffle 23 are both connected to the fixed baffle 24; the other end of the outer telescopic baffle 21 and the other end of the inner telescopic baffle 23 are both connected to the pulling baffle 22. The substrate is located in the space surrounded by the fixed baffle 24, the pulling baffle 22, the outer telescopic baffle 21 and the inner telescopic baffle 23. The stretching length of the outer telescopic baffle 21 and the inner telescopic baffle 23 is adapted to the size of the substrate. When the substrate frame 2 is raised, the substrate remains stationary, and the top of the inner telescopic baffle 23 and the outer telescopic baffle 21 are higher than the top surface of the substrate for holding the coating. Therefore, the thickness of the applied coating cannot exceed the height of the outer telescopic baffle 21 and the inner telescopic baffle 23.

[0031] The stretching distance of the outer telescopic baffle 21 and the inner telescopic baffle 23 is 10 cm. The distance between the outer telescopic baffle 21 and the inner telescopic baffle 23 is a fixed value of 10 cm. The size of the substrate frame 2 is first adjusted according to the size of the substrate, and then the substrate frame 2 and the slider 3 are fixed. In order to facilitate the cutting of the coating, the top surface of the outer telescopic baffle 21 and the top surface of the inner telescopic baffle 23 in this embodiment are located in the same horizontal plane, which is the horizontal position of the upper surface of the desired coating. The cutting device can fit the top surface of the inner telescopic baffle 23 and the top surface of the inner telescopic baffle 23 to cut the coating.

[0032] In order to facilitate the connection between the substrate frame 2 and the slider 3, the substrate frame 2 also includes a mounting platform 25. In order to facilitate the extension and retraction of the outer telescopic baffle 21 and the inner telescopic baffle 23, the mounting platform 25 is provided with a second slideway, and the pull baffle 22 is movably matched with the second slideway. When the pull baffle 22 moves linearly along the second slideway, the outer telescopic baffle 21 and the inner telescopic baffle 23 are pulled to extend and retract at the same time. In order to facilitate the connection between the outer telescopic baffle 21 and the inner telescopic baffle 23 and the pull baffle 22, the pull baffle 22 is provided with a mounting groove 28. The other end of the outer telescopic baffle 21 is located in a mounting groove 28 and connected to the pull baffle 22, and the other end of the inner telescopic baffle 23 is located in another mounting groove 28 and connected to the pull baffle 22. The mounting platform 25 is provided with a first screw hole 27, and the slider 3 is provided with a second screw hole 31 adapted to the first screw hole 27. The mounting platform 25 and the slider 3 can be connected after the bolt passes through the first screw hole 27 and the second screw hole 31.

[0033] In order to facilitate the connection between the slider 3 and the first slideway 12, the slider 3 is provided with a channel 33, the first slideway 12 is cylindrical, and the channel 33 is sleeved outside the first slideway 12. The wall of the channel 33 is provided with a third screw hole 32, and the first slideway 12 is provided with a fourth screw hole 14 that matches the third screw hole. The bolt passes through the third screw hole 32 and the fourth screw hole 14 to connect the mounting platform 25 and the slider 3.

[0034] The coating thickness measuring device is a vernier caliper 4, and the lower jaw 42 of the vernier caliper 4 is arranged on the mounting table 25; the upper jaw 41 of the vernier caliper 4 is arranged on the slider 3. The upper jaw 41 and the lower jaw 42 are both in the shape of long strips, and the length direction of the upper jaw 41 and the length direction of the lower jaw 42 are the same as the length direction of the pulling baffle 22. After the slider 3 and the substrate frame 2 are fixed, the upper jaw 41 fits the top of the inner telescopic baffle 23 and the top of the outer telescopic baffle 21. The reading of the vernier caliper 4 is the change value of the distance between the upper jaw 41 and the lower jaw 42; the body, switch 44, count reset button 45 and knob 47 of the vernier caliper 4 are all arranged on the slider 3. The slider 3 is also provided with an LED display screen 46 to display the reading of the vernier caliper 4. The reading of the vernier caliper 4 is accurate to 0.01mm, and the count reset button 45 of the vernier caliper 4 must be pressed after the slider 3 is stable to ensure the high accuracy of the reading. For the material to be measured, the width of the material should be wider than the width of the upper jaw 41 of the vernier caliper 4 by 1 cm.

[0035] When the slider 3 and the substrate frame 2 move down a certain distance along the first slideway 12 as a whole, the upper claw 41 can fit with the upper surface of the substrate, and the distance value between the upper claw 41 and the lower claw 42 is reading 1. When laying the coating, after the slider 3 and the substrate frame 2 move up a certain distance along the first slideway 12 as a whole, the distance value between the upper claw 41 and the lower claw 42 is reading 2, and the difference between reading 2 and reading 1 is the required coating thickness value. The upper surface of the required coating thickness is located in the same plane as the top of the telescopic baffle and the top of the outer telescopic baffle 21. The upper claw 41 fits with the upper surface of the required coating thickness.

[0036] The cutting device of this embodiment is a blade, the length of which is greater than the distance between the inner telescopic baffle 23 and the outer telescopic baffle 21; after the blade is in contact with the top surface of the inner telescopic baffle 23 and the top surface of the outer telescopic baffle 21, it moves toward the upper claw 41 to cut, remove the excess part after the coating thickness, and ensure that the required coating surface is flat.

[0037] The specific operation steps of precisely coating the mold with adhesive powder as a coating in this embodiment are as follows:

[0038] First, after removing all dirt on the surface of the substrate to be coated, the pulling baffle 22 in the substrate frame 2 is pulled according to the size of the substrate, so that the outer telescopic baffle 21 and the inner telescopic baffle 23 begin to extend until the substrate frame 2 just surrounds the substrate;

[0039] Secondly, the substrate frame 2 with adjusted size is lifted to a certain height and then fixed to the slider 3;

[0040] Afterwards, the substrate frame 2 and the slider 3 are slowly lowered from the first slideway 12 until the upper claw 41 of the vernier caliper 4 just touches the upper surface of the substrate;

[0041] Afterwards, tighten the knob 47 of the vernier caliper 4 so that the upper claw 41 is in close contact with the inner and outer telescopic baffles 21;

[0042] Afterwards, the slider 3 is pulled upward so that the slider 3 and the substrate frame 2 move upward along the first slideway 12 as a whole. At this time, the reading of the vernier caliper 4 changes with the change of the straight-line distance between the upper claw 41 and the lower claw 42.

[0043] Afterwards, when the coating thickness reaches a preset value, the slider 3 is fixed on the first slideway 12, and the powder coating mixed with the adhesive is poured onto the upper surface of the substrate in the substrate frame 2; Figure 2 As shown, at this time, the coating is uneven when added to the substrate;

[0044] Finally, a slender blade slightly longer than the linear distance between the two telescopic baffles is used to cut along the telescopic baffles toward the direction of the claw 41 on the vernier caliper 4 to obtain the following: Figure 7 The surface shown is smooth and the coating is of precise thickness.

[0045] The embodiments of the present invention are described in detail above. For those skilled in the art, according to the ideas provided by the present invention, there may be changes in the specific implementation methods, and these changes should also be regarded as the protection scope of the present invention.

Claims

1. A mold for preparing a cladding coating, Features: It includes a base, a substrate frame, a slider, a coating thickness measuring device, and a cutting device; The base is provided with a first slideway, and the slider is movably matched with the first slideway; the slider is connected to the substrate frame, and the substrate frame is sleeved outside the substrate; the bottom of the base is a platform, and the substrate is placed on the platform. The slider and the substrate frame move along the first slideway as a whole, and the space of the substrate frame above the top of the substrate can be filled with coating; the coating thickness measuring device is used to control the coating thickness; the cutting device is used to cut the excess coating beyond the required coating thickness of the substrate; The substrate frame includes a fixed baffle, a pulling baffle, an outer telescopic baffle and an inner telescopic baffle. The fixed baffle is parallel to the pulling baffle. One end of the outer telescopic baffle and one end of the inner telescopic baffle are both connected to the fixed baffle. The other end of the outer telescopic baffle and the other end of the inner telescopic baffle are both connected to the pulling baffle. The substrate is located in a space surrounded by the fixed baffle, the pulling baffle, the outer telescopic baffle and the inner telescopic baffle. The stretching lengths of the outer telescopic baffle and the inner telescopic baffle are adapted to the size of the substrate.

2. The mold for preparing the cladding coating according to claim 1, Features: The substrate frame also includes a mounting platform, which is provided with a second slideway, and the baffle is pulled to movably match the second slideway.

3. The mold for preparing the cladding coating according to claim 1, Features: The pulling baffle is provided with a mounting groove, the other end of the outer telescopic baffle is located in one mounting groove and connected with the pulling baffle, and the other end of the inner telescopic baffle is located in another mounting groove and connected with the pulling baffle.

4. The mold for preparing the cladding coating according to claim 2, Features: The mounting platform is provided with a first screw hole, and the sliding block is provided with a second screw hole matched with the first screw hole.

5. The mold for preparing the cladding coating according to claim 1, Features: The slide block is provided with a channel, the first slideway is cylindrical, and the channel is sleeved outside the first slideway.

6. The mold for preparing the cladding coating according to claim 5, Features: The channel wall is provided with a third screw hole, and the first slideway is provided with a fourth screw hole matched with the third screw hole.

7. The mold for preparing the cladding coating according to claim 2, Features: The coating thickness measuring device is a vernier caliper, the lower jaw of the vernier caliper is set on the mounting table; the upper jaw of the vernier caliper is set on the slider; the length direction of the upper jaw and the length direction of the lower jaw are the same as the length direction of the pulling baffle; the upper jaw is in contact with the top of the inner telescopic baffle and the top of the outer telescopic baffle; the reading of the vernier caliper is the change value of the distance between the upper jaw and the lower jaw; the switch, count reset button and knob of the vernier caliper are all set on the slider.

8. The mold for preparing the cladding coating according to claim 7, Features: The slider is also provided with an LED display screen to display the reading of the vernier caliper.

9. The mold for preparing the cladding coating according to claim 7, Features: The cutting device is a blade, the length of which is greater than the distance between the inner telescopic baffle and the outer telescopic baffle; the blade fits the top surface of the telescopic baffle and the top surface of the outer telescopic baffle, and can move toward the upper claw to cut.