Method for achieving single exciton gain in semiconductor nanocrystals using circularly polarized laser

By using circularly polarized lasers for pumping and detection in semiconductor nanocrystals, measuring the ground state bleaching signal intensity, and determining the gain threshold of single excitons, the problem of low efficiency caused by multi-exciton energy loss was solved and a lower laser threshold was achieved. and efficient optical gain.

CN114268019BActive Publication Date: 2024-10-01UNIV OF SCI & TECH OF CHINA
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202111593962.9
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2021-12-22
Publication Date
2024-10-01
Estimated Expiration
2041-12-22

AI Technical Summary

Technical Problem

In semiconductor nanocrystals, the energy loss of multi-excitons results in low stimulated radiation efficiency, making it difficult to lower the threshold. It is difficult to achieve low-threshold laser gain with existing technology.

Method used

Circularly polarized laser is used for pumping and detection. By changing the polarization of the excitation light, the ground state bleaching signal intensity of the film sample is measured, and the critical light intensity of the pump light is judged to determine the gain threshold of single exciton. Perovskite nanocrystal materials such as Prepare thin film samples from CsPbBr3, CsPbI3, MAPbI3 or MAPbBr3.

Benefits of technology

The optical gain threshold when excited by circularly polarized light is lower, indicating that the gain is dominated by single excitons, which significantly reduces the threshold of laser generation and improves the stimulated emission efficiency.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN114268019B_ABST
    Figure CN114268019B_ABST
Patent Text Reader

Abstract

The present invention provides a method for realizing single exciton gain in semiconductor nanocrystals by using circularly polarized lasers, and relates to the field of laser technology. The method comprises the following steps: preparing a thin film sample by using semiconductor nanocrystals, so that the sample molecules are densely packed and fixed in position; measuring the absorbance of the thin film sample by using an ultraviolet-visible absorption spectrometer; using a femtosecond laser and a circular polarizer to generate a beam of circularly polarized light, which is focused on the thin film sample as pump light; changing the light intensity of the pump light, using another beam of circularly polarized light as a detection light, and detecting the ground state bleaching signal intensity of the thin film sample; judging whether the ground state bleaching signal intensity is equal to the absorbance, and if so, determining the critical light intensity of the pump light, which is the gain threshold of the single exciton.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the field of laser technology, and in particular to a method for realizing single exciton gain in semiconductor nanocrystals by utilizing circularly polarized laser. Background Art

[0002] Laser technology has a wide range of applications in communications, medical treatment, scientific research and other fields, and has a huge market demand. Laser threshold is one of the core issues in laser research. How to reduce the laser threshold and find new materials with low threshold are the key topics of laser technology.

[0003] At present, the research on the principle of laser has become mature, and the understanding of laser threshold has gradually deepened. The basis of laser generation is the occurrence of amplified spontaneous radiation. The electrons in the excited state transition back to the valence band and generate photons through spontaneous radiation. These photons further induce the excited state electrons to generate stimulated radiation, thereby achieving the purpose of light amplification. When the photons generated by stimulated radiation are greater than the stimulated absorption, the remaining photons will be emitted in the form of laser. The incident light intensity that just meets the laser emission conditions is the threshold.

[0004] In recent years, semiconductor nanocrystals have become a research hotspot for optical gain materials due to their excellent luminescence properties such as continuously tunable wavelength, narrowband emission, and high photoluminescence quantum yield. However, in semiconductor nanocrystals, excited electrons will combine with valence band holes to form excitons, and the interaction between excitons will cause them to combine to form multi-excitons. Due to the existence of Auger recombination, the energy of multi-excitons will be lost in the form of heat energy, resulting in low efficiency of stimulated radiation and difficulty in lowering the threshold. Summary of the invention

[0005] In view of the above-mentioned deficiencies in the prior art, the present invention provides a method for realizing single exciton gain in semiconductor nanocrystals by using circularly polarized laser.

[0006] The present invention provides a method for realizing single exciton gain in semiconductor nanocrystals by using circularly polarized lasers, comprising the following steps: preparing a thin film sample by using semiconductor nanocrystals, so that the sample molecules are densely packed and fixed in position; measuring the absorbance of the thin film sample by using an ultraviolet-visible absorption spectrometer; generating a beam of circularly polarized light by using a femtosecond laser and a circular polarizer, and focusing the beam of circularly polarized light on the thin film sample as pump light; changing the light intensity of the pump light, using another beam of circularly polarized light as detection light, and detecting the ground state bleaching signal intensity of the thin film sample; judging whether the ground state bleaching signal intensity is equal to the absorbance, and if so, determining the critical light intensity of the pump light as the gain threshold of the single exciton.

[0007] Furthermore, the semiconductor nanocrystal is a perovskite nanocrystal material, and the perovskite nanocrystal material includes CsPbBr3, CsPbI3, MAPbI3 or MAPbBr3.

[0008] Furthermore, the step of preparing the thin film sample includes: using a spin coater to spin coat the solution sample onto a glass sheet, and after the solvent evaporates, the sample molecules are densely filled and the positions are fixed.

[0009] Further, the absorbance of the film sample is measured, including:

[0010] The absorbance of the film sample was measured in the wavelength range of 400nm to 600nm. The absorbance was measured according to the following formula:

[0011]

[0012] In the formula, α0 represents the absorbance of the thin film sample in the wavelength range of 400nm to 600nm; I0 represents the original intensity of white light; I represents the intensity of white light after passing through the thin film sample without pump light excitation.

[0013] Furthermore, the wavelength range of the pump light is 450 nm to 515 nm.

[0014] Furthermore, the wavelength range of the detection light is 450nm to 550nm.

[0015] Furthermore, the ground state bleaching signal intensity is the change in the absorption of the detection light by the thin film sample under the conditions of pump light and without pump light excitation; the ground state bleaching signal intensity is measured according to the following formula:

[0016]

[0017] Where Δα represents the ground state bleaching signal intensity of the thin film sample; I represents the intensity of the probe light after passing through the thin film sample without pump light excitation; I1 represents the intensity of the probe light after passing through the thin film sample with pump light excitation.

[0018] Further, determining whether the ground state bleaching signal intensity is greater than or equal to the absorbance includes:

[0019] When α0+Δα≤0, stimulated radiation compensates for absorption and generates optical gain. The critical intensity of the pump light is determined as the gain threshold of the single exciton, where the critical intensity of the pump light is the intensity of the pump light when I1=I.

[0020] Compared with the prior art, the method provided by the present invention uses circularly polarized laser to achieve single exciton gain in semiconductor nanocrystals. By changing the polarization of the excitation light, the absorption and stimulated emission of the thin film sample after excitation are detected as a function of the incident power. After comparing with the absorbance, it is concluded that the threshold of optical gain is lower when excited by circularly polarized light, indicating that the gain is dominated by single excitons. BRIEF DESCRIPTION OF THE DRAWINGS

[0021] The above and other objects, features and advantages of the present invention will become more apparent through the following description of the embodiments of the present invention with reference to the accompanying drawings, in which:

[0022] Figure 1 A flow chart schematically shows a method for achieving single exciton gain in semiconductor nanocrystals using circularly polarized lasers;

[0023] Figure 2 A simplified apparatus diagram schematically illustrates a method for achieving single exciton gain in semiconductor nanocrystals;

[0024] Figure 3 The schematic diagram shows the principle of generating single exciton gain by circularly polarized light;

[0025] Figure 4 Schematically showing the test result diagram when the pump light and the probe light have circular polarizations of the same / opposite handedness;

[0026] Figure 5 The gain threshold diagram under circularly polarized light / non-circularly polarized light excitation is schematically shown. DETAILED DESCRIPTION

[0027] In order to make the purpose, technical scheme and advantages of the present invention more clearly understood, the present invention is further described in detail below in combination with specific embodiments and with reference to the accompanying drawings. Obviously, the described embodiments are part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.

[0028] The terms used herein are only for describing specific embodiments and are not intended to limit the present invention. The terms "comprise", "include", etc. used herein indicate the existence of the features, steps, operations and / or components, but do not exclude the existence or addition of one or more other features, steps, operations or components.

[0029] In the present invention, unless otherwise clearly specified and limited, the terms "installed", "connected", "connected", "fixed" and the like should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection, an electrical connection, or can communicate with each other; it can be a direct connection, or an indirect connection through an intermediate medium, it can be the internal connection of two elements or the interaction relationship between two elements. For ordinary technicians in this field, the specific meanings of the above terms in the present invention can be understood according to specific circumstances.

[0030] All terms (including technical and scientific terms) used herein have the meanings commonly understood by those skilled in the art, unless otherwise defined. It should be noted that the terms used herein should be interpreted as having a meaning consistent with the context of this specification, and should not be interpreted in an idealized or overly rigid manner.

[0031] Figure 1 The flowchart of the method for realizing single exciton gain in semiconductor nanocrystals using circularly polarized laser is schematically shown. Figure 1 As shown, the method for realizing single exciton gain in semiconductor nanocrystals by using circularly polarized laser provided in an embodiment of the present invention comprises the following steps:

[0032] Step S1, using semiconductor nanocrystals to prepare a thin film sample so that the sample molecules are densely packed and fixed in position;

[0033] Step S2, using an ultraviolet-visible absorption spectrometer to measure the absorbance of the film sample;

[0034] Step S3, using a femtosecond laser and a circular polarizer to generate a beam of circularly polarized light, which is focused onto the thin film sample as pump light;

[0035] Step S4, changing the intensity of the pump light, using another circularly polarized light beam as a detection light, and detecting the intensity of the ground state bleaching signal of the thin film sample;

[0036] Step S5, determining whether the ground state bleaching signal intensity is equal to the absorbance, if so, determining the critical light intensity of the pump light as the gain threshold of the single exciton.

[0037] Experiments have shown that the threshold under circularly polarized light excitation is significantly lower than the threshold dominated by biexcitons under non-circularly polarized light excitation, indicating that its gain is dominated by single excitons.

[0038] In an embodiment of the present invention, the semiconductor nanocrystal is a perovskite nanocrystal material, and the perovskite nanocrystal material includes CsPbBr3, CsPbI3, MAPbI3 or MAPbBr3.

[0039] In an embodiment of the present invention, the step of preparing a thin film sample includes: using a spin coater to spin coat the solution sample onto a glass sheet, and after the solvent evaporates, the sample molecules are densely packed and the positions are fixed, so as to generate laser light emitted in a specific direction.

[0040] In the embodiment of the present invention, measuring the absorbance of the film sample includes: measuring the absorbance of the film sample in the wavelength range of 400nm to 600nm, and the absorbance is measured according to the following formula:

[0041]

[0042] In the formula, α0 represents the absorbance of the thin film sample in the wavelength range of 400nm to 600nm; I0 represents the original intensity of white light; I represents the intensity of white light after passing through the thin film sample without pump light excitation.

[0043] In the embodiment of the present invention, the wavelength range of the pump light is 450 nm to 515 nm.

[0044] In the embodiment of the present invention, the wavelength range of the detection light is 450nm to 550nm.

[0045] In the embodiment of the present invention, the ground state bleaching signal intensity is the change in the absorption of the detection light by the thin film sample under the conditions of pump light and without pump light excitation; the ground state bleaching signal intensity is measured according to the following formula:

[0046]

[0047] Where Δα represents the ground state bleaching signal intensity of the thin film sample; I represents the intensity of the probe light after passing through the thin film sample without pump light excitation; I1 represents the intensity of the probe light after passing through the thin film sample with pump light excitation.

[0048] In an embodiment of the present invention, judging whether the ground state bleaching signal intensity is greater than or equal to the absorbance includes: when α0+Δα≤0, the stimulated radiation compensates for the absorption and generates optical gain, and determining the critical light intensity of the pump light is the gain threshold of the single exciton, wherein the critical light intensity of the pump light is the light intensity of the pump light when I1=I.

[0049] Through the embodiments of the present invention, the gain generated by the sample is measured by using absorption spectrum and transient absorption spectrum. First, the absorbance of the sample in the range of 400nm to 600nm is measured using an ultraviolet-visible absorption spectrometer to obtain the ratio of the original intensity of white light to the intensity after passing through the sample. Then, the intensity of the probe light passing through the sample when there is pump light is obtained through the experimental device of transient absorption spectrum. Compared with the case where the non-circular polarization excitation is dominated by biexcitons, the gain threshold during circular polarized light excitation is significantly reduced, indicating that its gain is dominated by single excitons.

[0050] The present invention uses absorption spectrum and transient absorption spectrum to measure the gain generated by the sample. The specific device is as follows: the 1030nm femtosecond pulse generated by the femtosecond laser is divided into two beams after passing through a beam splitter, one of which has a continuously adjustable wavelength after passing through an optical parametric amplifier and serves as pump light. The other beam is extended to a wavelength range of 450nm to 550nm after passing through a BBO crystal (β-phase barium borate crystal, β-BaB2O4) and a sapphire crystal, and serves as a probe light. By changing the time difference between the pump light and the probe light reaching the sample, the changes that occur in the sample within a period of time after the pump light excites the sample can be obtained. After the pump light excites some electrons to the conduction band, the sample's absorption of the probe light will be reduced. At the same time, due to the presence of stimulated radiation, the intensity of the probe light passing through the sample will be greater than the intensity of the probe light passing through the sample when there is no pump light excitation, which is called the ground state bleaching signal.

[0051] Figure 2 A simplified apparatus diagram schematically illustrates a method for achieving single exciton gain in semiconductor nanocrystals.

[0052] In order to measure the gain threshold under different polarization excitations, the following Figure 2 The simplified experimental setup for single exciton gain measurement is shown. After the pump light passes through the circular polarizer, a beam of left-handed circularly polarized light is generated, which is incident on the sample at a certain angle; then, another beam of left-handed circularly polarized light is generated using a linear polarizer and a quarter-wave plate and focused on the sample. After passing through the sample, the transmitted light is collected to detect the ground state bleaching signal intensity of the sample. The gain threshold can be calculated by combining the ground state bleaching signal intensity with the absorbance.

[0053] It should be noted that Figure 2 Two achromatic prisms and a fiber collector are also arranged behind the sample to be tested. It can be understood that the achromatic prism is mainly used for chromatic aberration correction and light focusing. The fiber collector is mainly used to collect the light required for the test, effectively improving the light collection efficiency.

[0054] Based on the above disclosure, the principle of achieving single exciton gain by circularly polarized light is described in detail below.

[0055] Figure 3 The schematic diagram shows the principle of circularly polarized light generating single exciton gain. Figure 3As shown, considering the doubly degenerate valence band and conduction band, the electron spin can be ±1 / 2. When non-polarized light is used for excitation, the nanocrystal in the ground state will absorb, which reduces the intensity of the transmitted light, while the nanocrystal in the single exciton state will not only absorb some photons, but also generate some photons due to stimulated radiation. Since the number of absorbed and generated photons is equal, the light intensity will not change when the excitation light passes through the nanocrystal, and the nanocrystal is transparent to the excitation light. However, when the nanocrystal is in the biexciton state, the conduction band population has been filled, and the population inversion has been achieved, so the nanocrystal will not absorb the excitation light, but will emit additional photons due to stimulated radiation, thereby generating gain. In the case of non-polarized light excitation, when the number of biexciton nanocrystals generated after excitation is greater than the number of nanocrystals in the ground state, photons can be emitted. In the case of circularly polarized light excitation, only electrons that meet the transition selection rule can be excited to the conduction band. Therefore, only when the nanocrystal is in the ground state will it absorb the excitation light. When the nanocrystal is in a single exciton state, gain can be generated. Therefore, under the condition of specific circularly polarized light excitation, the condition for gain is that the number of nanocrystals in the single exciton state is greater than the number of nanocrystals in the ground state. Compared with the case of non-polarized light excitation, the threshold condition to be met when circularly polarized light is used for excitation is lower, and its gain is mainly dominated by single excitons.

[0056] The following experiments demonstrate that the effect of single exciton gain can be achieved by applying circularly polarized light excitation.

[0057] Figure 4 The diagram schematically shows the test results when the pump light and the probe light have circular polarizations of the same / opposite handedness. Figure 5 The gain threshold diagram under circularly polarized light / non-circularly polarized light excitation is schematically shown.

[0058] Example 1 is a spin lifetime test. Under the condition of left-handed circularly polarized light excitation, left-handed and right-handed circularly polarized light are used to detect the ground state bleaching signal of the sample, and the following can be obtained: Figure 4 The experimental results are shown. When the sample is excited by left-handed circularly polarized light, the signal detected by left-handed circularly polarized light rises rapidly to the maximum value, while the signal detected by right-handed circularly polarized light rises slowly. After 7ps, the two overlap, indicating that the pump light generates electrons with an angular momentum of -1 / 2. Due to the transition selection rule, only left-handed circularly polarized light can detect the corresponding ground state bleaching signal. As the electron spin relaxes to 1 / 2, right-handed circularly polarized light gradually detects the signal. Therefore, through the amplitude difference of the two signals, it can be obtained that the polarization degree generated by the excitation light is 75%. This shows that within 7ps, the use of circularly polarized light excitation can achieve the polarization of electrons, reduce the energy level degeneracy, and only generate single excitons, reflecting the feasibility of single exciton gain.

[0059] Since the incident light polarization can only be maintained for 7ps, the gain data of 1.5ps after excitation is mainly detected. The incident light power is adjusted and the curve of the ground state bleaching signal changing with power is recorded. When α0+Δα≤0, gain is generated. In order to compare with the case of biexciton gain, Figure 5 The graph of the ground state bleaching signal under circularly polarized light / non-circularly polarized light excitation versus power shows that when non-circularly polarized light is used for excitation, that is, when the gain is dominated by biexcitons, the threshold is 140 μJ / cm 2 , while when circularly polarized light is used for excitation, the threshold is 90 μJ / cm 2 , which is significantly smaller than the case of non-circular polarization excitation. Therefore, it is experimentally demonstrated that single exciton gain can be achieved using circularly polarized light.

[0060] In summary, the embodiments of the present invention provide a method for realizing single exciton gain in semiconductor nanocrystals using circularly polarized lasers. By changing the polarization of the excitation light, the absorption and stimulated emission of the thin film sample after excitation are detected as a function of the incident power. After comparing with the absorbance, it is concluded that the threshold of the optical gain is lower when excited by circularly polarized light, indicating that the gain is dominated by single excitons.

[0061] It should also be noted that, unless specifically described or steps must occur in sequence, the order of the above steps is not limited to the above list, and can be changed or rearranged according to the required design. In addition, the above embodiments can be mixed and matched with each other or with other embodiments based on design and reliability considerations, that is, the technical features in different embodiments can be freely combined to form more embodiments.

[0062] In the description of the present invention, it is necessary to understand that the directions or positional relationships indicated by the terms "up", "down", "front", "back", "left", "right", etc. are based on the directions or positional relationships shown in the accompanying drawings, and are only for the convenience of describing the present invention and simplifying the description, rather than indicating or implying that the device or element referred to must have a specific direction, be constructed and operated in a specific direction, and therefore cannot be understood as a limitation on the present invention.

[0063] Throughout the drawings, the same elements are represented by the same or similar reference numerals. Conventional structures or configurations will be omitted when they may cause confusion in the understanding of the present invention. The shapes, sizes, and positional relationships of the components in the drawings do not reflect the actual size, proportion, and actual positional relationship. In addition, in the description of the present invention, the meaning of "multiple" is at least two, such as two, three, etc., unless otherwise clearly and specifically defined.

[0064] The specific embodiments described above further illustrate the objectives, technical solutions and beneficial effects of the present invention in detail. It should be understood that the above description is only a specific embodiment of the present invention and is not intended to limit the present invention. Any modifications, equivalent substitutions, improvements, etc. made within the spirit and principles of the present invention should be included in the protection scope of the present invention.

Claims

1. A method for achieving single exciton gain in semiconductor nanocrystals using circularly polarized laser, characterized in that: The following steps are involved: Semiconductor nanocrystals are used to prepare thin film samples, so that the sample molecules are densely packed and fixed in position; The absorbance of the film sample is measured using an ultraviolet-visible absorption spectrometer; including: measuring the absorbance of the film sample in the wavelength range of 400nm~600nm, and the absorbance is measured according to the following formula: In the formula, Indicates the absorbance of the film sample in the wavelength range of 400nm~600nm; Represents the original intensity of white light; It indicates the intensity of white light after passing through the thin film sample without pump light excitation; A femtosecond laser and a circular polarizer are used to generate a beam of circularly polarized light, which is focused onto the thin film sample as pump light; The light intensity of the pump light is changed, and another circularly polarized light is used as the detection light to detect the ground state bleaching signal intensity of the thin film sample; the ground state bleaching signal intensity is the change in the absorption of the detection light by the thin film sample under the conditions of pump light and without pump light excitation; the ground state bleaching signal intensity is measured according to the following formula: In the formula, represents the ground state bleaching signal intensity of the film sample; It indicates the intensity of white light after passing through the thin film sample without pump light excitation; It indicates the intensity of the probe light after passing through the thin film sample under the condition of pump light excitation; It is determined whether the ground state bleaching signal intensity is equal to the absorbance, and if so, the critical light intensity of the pump light is determined to be the gain threshold of the single exciton.

2. The method for realizing single exciton gain in semiconductor nanocrystals using circularly polarized laser according to claim 1, wherein: The semiconductor nanocrystal is a perovskite nanocrystal material, and the perovskite nanocrystal material includes CsPbBr3, CsPbI3, MAPbI3 or MAPbBr3.

3. The method for realizing single exciton gain in semiconductor nanocrystals using circularly polarized laser according to claim 1, wherein: The steps of preparing the film sample include: Use a spin coater to spin coat the solution sample onto a glass slide. After the solvent evaporates, the sample molecules are densely packed and their positions are fixed.

4. The method for realizing single exciton gain in semiconductor nanocrystals using circularly polarized laser according to claim 1, wherein: The wavelength range of the pump light is 450nm~515nm.

5. The method for realizing single exciton gain in semiconductor nanocrystals using circularly polarized laser according to claim 1, wherein: The wavelength range of the detection light is 450nm~550nm.

6. The method for realizing single exciton gain in semiconductor nanocrystals using circularly polarized laser according to claim 1, wherein: The determining whether the ground state bleaching signal intensity is greater than or equal to the absorbance comprises: when When the stimulated radiation compensates for the absorption and generates optical gain, the critical light intensity of the pump light is determined to be the gain threshold of the single exciton, wherein the critical light intensity of the pump light is The intensity of the pump light.