Mold and sample making method for making tensile specimen of composite sheet

By designing a mold with adjustment grooves and limiting blocks, the problems of operating error and inaccurate positioning in the production of composite sheet tensile samples are solved, and uniform stress and precise bonding of the sample reinforcement sheet are achieved, thereby improving the The accuracy and efficiency of sample testing are achieved.

CN114428012BActive Publication Date: 2024-11-26CHINA PETROLEUM & CHEMICAL CORP +1
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202011084130.X
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2020-10-12
Publication Date
2024-11-26
Estimated Expiration
2040-10-12

AI Technical Summary

Technical Problem

The molds made of existing composite sheet tensile samples have problems such as operating error, inaccurate positioning and difficult to control the bonding effect, which affect the test quality of the tensile performance of the samples.

Method used

A mold including an upper base plate, a lower base plate, a width adjustment positioning block, a thickness adjustment positioning plate, a positioning pin and a bolt are designed. Pressure is applied by adjusting the elasticity of the bolts to ensure that the uniform force of the sample reinforcement sheet is applied, and through adjustment, The grooves and limit blocks prevent displacement, achieving accurate bonding between the sample reinforcement sheet and the sample.

Benefits of technology

Improve the efficiency and accuracy of composite sample production, ensure the uniform stress and bonding quality between the sample reinforcement sheet and the sample, thereby improving the accuracy of tensile strength data, and is suitable for tests of different sizes and specifications. Sample preparation.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN114428012B_ABST
    Figure CN114428012B_ABST
Patent Text Reader

Abstract

The present invention discloses a mold for preparing tensile specimens of composite sheet materials and a method for preparing the specimens. The mold comprises an upper base plate, a lower base plate, a width adjustment positioning block, a thickness adjustment positioning plate, a positioning pin and a bolt. A plurality of adjustment slots are provided on the base plate, and the thickness is adjusted by the thickness adjustment positioning plate. The mold has a simple structure, and one-time positioning of multiple specimens is achieved by the width adjustment positioning block and the thickness adjustment positioning plate. At the same time, uniform stress is applied to all specimen reinforcement sheets by the pressure between the base plates, and the bonding quality between the specimen reinforcement sheet and the specimen is ensured, thereby improving the accuracy of tensile strength data when testing composite specimens of the same batch. In addition, the mold can also be applied to the preparation of tensile specimens of composite sheet materials of different sizes and specifications.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of molds, and in particular to a mold for preparing a tensile specimen of a composite material sheet and a method for preparing the specimen. Background Art

[0002] At present, the molds for making tensile specimens are mainly made of resin and metal materials, while there are very few molds for making tensile specimens of composite sheets. The few existing molds still have certain defects when making specimens, as follows.

[0003] (1) Each sample is prepared separately, which is time-consuming and labor-intensive. In addition, the clamping force and precise positioning cannot be guaranteed during manual operation, which inevitably leads to operational errors.

[0004] (2) The bonding pressure between the specimen reinforcement sheet and the specimen only acts on the local bonding surface. If the positioning is inaccurate, displacement is likely to occur, and the bonding effect is difficult to control, which ultimately affects the tensile performance test quality of the specimen.

[0005] Therefore, there is an urgent need for a mold for making composite sheet tensile specimens to ensure high efficiency and accuracy in the preparation process of composite sheet tensile specimens while meeting the accuracy of composite sheet tensile strength test data. Summary of the invention

[0006] In order to overcome the deficiencies of the prior art, the object of the present invention is to provide a mold and a sample preparation method for preparing a composite material sheet tensile specimen, which can solve the above-mentioned problems.

[0007] The present invention is implemented by adopting the following technical solutions.

[0008] A mold for making composite sheet tensile specimens, comprising an upper base plate, a lower base plate, a width adjustment positioning block, a thickness adjustment positioning sheet, positioning pins and bolts. The difference between the upper base plate and the lower base plate is that the upper base plate has two left-right symmetrical demoulding holes perpendicular to the upper base plate on both sides parallel to the specimen.

[0009] There is no difference between the upper base plate and the lower base plate when preparing the sample, which is the orientation when removing the mold.

[0010] The thickness adjustment limit plate is fixed and connected to the upper base plate and the lower base plate by positioning pins and hexagonal bolts, and pressure is applied on the surface of the composite material sheet tensile specimen reinforcement plate by adjusting the tightness of the bolts.

[0011] The upper bottom plate has equal and bilaterally symmetrical adjustment grooves, i.e., recesses, on both vertical sides of the sample.

[0012] The adjustment groove of the upper base plate is the placement position of the sample reinforcement piece and the width adjustment limit block.

[0013] The length of the adjusting groove of the upper bottom plate is equal to the length of the sample reinforcement sheet.

[0014] The width of the adjustment slot of the upper base plate is equal to the sum of the width of the sample reinforcement sheet and the thickness of the twice width adjustment limit block.

[0015] The distance between the adjusting grooves of the upper bottom plate is equal to the length of the sample minus twice the length of the groove.

[0016] The length of the width adjustment limit block is equal to the length of the adjustment slot.

[0017] The height of the width adjustment limit block is greater than the sum of the depth of the adjustment groove and the thickness of the sample, and less than twice the sum of the depth of the adjustment groove and the thickness of the sample.

[0018] The thickness of the width adjustment limit block is adjusted according to the width of the sample, which is equal to half of the difference between the width of the adjustment slot and the width of the sample.

[0019] The width adjustment limit blocks are placed on both sides of the adjustment slot of the bottom plate, parallel to the sample, to prevent the sample and the sample reinforcement sheet from being displaced left and right when the film is closed.

[0020] The thickness of the thickness adjustment limit piece is equal to the thickness of the sample.

[0021] The length of the thickness adjustment limiting piece is equal to the side length of the corresponding bottom plate.

[0022] The width of the thickness adjustment limit piece is equal to the length of the bottom plate frame from the side width of the bottom plate groove.

[0023] The thickness adjustment limit pieces are placed at both ends of the sample, perpendicular to the sample, to prevent the sample from moving forward and backward during film closing, and to ensure the parallelism of the sample reinforcement piece and the sample during preparation and testing, as well as the accuracy of the bonding thickness.

[0024] Preferably, the number of the grooves is greater than or equal to 3.

[0025] Preferably, the height of the width adjustment limit block is greater than or equal to twice the height of the groove.

[0026] Preferably, the thickness of the width adjustment limit block is greater than or equal to 1 mm.

[0027] The process of preparing the composite sheet tensile specimen is as follows:

[0028] S1. Before preparing the sample, spray a liquid release agent on the sample preparation surface of the upper base plate 1 and the lower base plate 2, the surface of the width adjustment limit block 3, and the surface of the thickness adjustment limit plate 4 to facilitate the cleaning of the adhesive residue after preparing the sample;

[0029] S2. When preparing the sample, first grind and clean the two sides of the sample reinforcement sheet 9 to be pasted at both ends of the test sample 8, and then evenly apply adhesive, then clean the surface of the pasting part of the sample reinforcement sheet 9 and evenly apply adhesive;

[0030] S3, place the sample reinforcement sheet 9 into the groove of the lower bottom plate 2 (with the bonding surface facing upward), and then place the width adjustment limit blocks 3 into the groove of the bottom plate 2 (one block is placed on each side of the sample reinforcement sheet 9);

[0031] S4. Place the sample 8 between the four width adjustment limit blocks 3, and install the thickness adjustment limit plates 4 on both sides of the lower base plate 2 through the positioning pins 5, ensuring that the adhesive surfaces at both ends of the lower surface of the sample 8 match the adhesive surfaces of the sample reinforcement plates 9 in the groove of the lower base plate 2;

[0032] S5. Place the sample reinforcement sheet 9 on the adhesive surfaces at both ends of the upper surface of the sample 8 and between the two width adjustment limit blocks 3;

[0033] S6. Put the upper base plate 1 and the lower base plate 2 together, first fix the upper and lower base plates by the positioning pins 11, and finally tighten and fix them with hexagonal bolts so that the specimen reinforcement sheet is evenly stressed, ensuring the bonding quality between the specimen reinforcement sheet and the specimen.

[0034] Compared with the prior art, the present invention has the following beneficial effects:

[0035] 1) The mold has a simple structure. It can realize one-time positioning of multiple specimens through width adjustment positioning blocks and thickness adjustment positioning sheets. At the same time, the pressure between the bottom plates can realize uniform force on all specimen reinforcement sheets, ensuring the bonding quality between the specimen reinforcement sheets and the specimens, thereby improving the accuracy of the tensile strength data when testing the same batch of composite material specimens.

[0036] 2) The mold can be used for the preparation of tensile specimens of composite sheets of different sizes.

[0037] 3) The mold can achieve high efficiency and accuracy in the preparation of composite sheet tensile specimens. BRIEF DESCRIPTION OF THE DRAWINGS

[0038] Figure 1 is a top view schematic diagram of the upper base plate;

[0039] Figure 2 is a schematic diagram of a side cross section of the upper base plate;

[0040] Figure 3 is a schematic diagram of the end section of the upper base plate;

[0041] Figure 4 is a top view schematic diagram of the lower base plate;

[0042] Figure 5is a schematic diagram of a side cross section of the lower base plate;

[0043] Figure 6 is a schematic diagram of the end section of the lower base plate;

[0044] Figure 7 It is a schematic diagram of a thickness adjustment limit piece;

[0045] Figure 8 A schematic diagram of the mold assembly for making tensile specimens of composite sheets;

[0046] Fig. 9 for Figure 8 Schematic diagram of the cross section at A in the middle;

[0047] Fig.10 for Figure 8 Schematic diagram of the cross section at point B.

[0048] In the figure: 1. upper base plate; 2. lower base plate; 3. width adjustment limit block; 4. thickness adjustment limit plate; 5. positioning pin hole; 6. demoulding hole; 7. bolt hole; 8. specimen; 9. specimen reinforcement plate; 11. positioning pin; 12. bolt. DETAILED DESCRIPTION

[0049] In order to make the purpose, technical solution and advantages of the embodiments of the present invention clearer, the technical solution in the embodiments of the present invention will be clearly and completely described below in conjunction with the drawings in the embodiments of the present invention. Obviously, the described embodiments are part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.

[0050] The present invention is used for the mold for making the composite sheet tensile test specimen, please refer to Figures 1 to 10 The mold includes an upper mold 1, a lower mold 2, a width adjustment limit block 3, a thickness adjustment limit plate 4, a positioning pin 11 and a bolt 12.

[0051] See also Figure 1-Figure 6 Bolt holes 7 are provided on the upper base plate 1 and the lower base plate 2 near the four sides, and positioning pin holes 5 are provided on the upper base plate 1 and the lower base plate 2 at both ends for installing the sample 8; the positioning pin holes 5 and the bolt holes 7 are used for passing the positioning pins 11 and the bolts 12 through when closing the mold to fix and connect the upper base plate 1, the lower base plate 2, and the thickness adjustment limit plate 4.

[0052] Demolding holes 6 are provided on the upper base plate 1 and penetrate through both side ends parallel to the installation direction of the sample 8 .

[0053] On at least one of the butt joint surfaces of the upper base plate 1 and the lower base plate 2 , equal numbers of left-right symmetrical adjustment grooves 10 are provided on both sides perpendicular to the sample 8 , and the adjustment grooves 10 are used to accommodate the width adjustment positioning blocks 3 and the sample reinforcement sheets 9 .

[0054] The thickness adjustment positioning piece 4 is between the two ends of the upper base plate 1 and the lower base plate 2, and the corresponding pressure is applied to the surface of the sample 8, the width adjustment positioning block 3, and the sample reinforcement piece 9 by adjusting the tightness of the bolts.

[0055] Adjustment slot parameters: The depth of the adjustment slot 10 is equal to an integral multiple of the thickness of the sample reinforcement sheet 9 , the length of the adjustment slot 10 is equal to the length of the sample reinforcement sheet 9 , and the width of the adjustment slot 10 is equal to the sum of the width of the sample reinforcement sheet 9 and the thickness of the twice-width adjustment positioning block 3 .

[0056] The distance between two adjacent adjustment grooves 10 is equal to the length of the sample 8 minus twice the length of the adjustment groove 10 .

[0057] The number of the adjustment slots 10 is greater than or equal to 3, and preferably is 5.

[0058] Width adjustment limit block parameters: The length of the width adjustment limit block 3 is equal to the length of the adjustment slot 10. The height of the width adjustment limit block 3 is greater than the sum of the depth of the adjustment slot 10 and the thickness of the sample 8, and less than twice the sum of the depth of the adjustment slot 10 and the thickness of the sample 8; the thickness of the width adjustment limit block 3 is adjusted according to the width of the sample 8, and is equal to half of the difference between the width of the adjustment slot 10 and the width of the sample 8. The width adjustment limit blocks 3 are arranged on both sides of the adjustment slot 10, parallel to the sample 8, to prevent the sample 8 and the sample reinforcement sheet 9 from being displaced left and right when the film is closed.

[0059] Thickness adjustment limit plate parameters: the thickness of the thickness adjustment limit plate 4 is equal to the thickness of the sample 8, the length of the thickness adjustment limit plate 4 is equal to the side length of the corresponding bottom plate, and the width of the thickness adjustment limit plate 4 is equal to the length of the side width of the adjustment slot 10 of the bottom plate to the bottom plate frame.

[0060] The thickness adjustment limit pieces 4 are placed at both ends of the sample 8, perpendicular to the sample 8, to prevent the sample 8 from moving forward and backward during film closing, and to ensure the parallelism of the sample reinforcement piece 9 and the sample 8 during preparation and testing, as well as the accuracy of the bonding thickness.

[0061] Assembly and preparation method: A method for preparing a composite material sheet tensile test specimen using the above-mentioned mold includes the following steps.

[0062] S1. Spraying a mold release agent: first spray a liquid mold release agent on the sample preparation surface of the upper base plate 1 and the lower base plate 2, the surface of the width adjustment limit block 3, and the surface of the thickness adjustment limit plate 4 to facilitate the cleaning of the adhesive residue after sample preparation.

[0063] S2. Sample processing: grind the two sides of the sample 8 to be tested to be pasted with the sample reinforcement sheet 9, clean them and evenly apply adhesive, then clean the surface of the pasting part of the sample reinforcement sheet 9 and evenly apply adhesive.

[0064] S3. Fill the lower groove, place the sample reinforcement sheet 9 into the adjustment groove 10 of the lower bottom plate 2, and make the bonding surface of the sample reinforcement sheet 9 face up, then place the width adjustment limit block 3 into the adjustment groove 10 of the lower bottom plate 2, and place one width adjustment limit block 3 on each side of the sample reinforcement sheet 9.

[0065] S4. Place the sample, insert the sample 8 between the four width adjustment limit blocks 3, and install the thickness adjustment limit plates 4 on both sides of the lower base plate 2 through the positioning pins 11, ensuring that the adhesive surfaces at both ends of the lower surface of the sample 8 are in contact with the adhesive surfaces of the sample reinforcement plate 9 in the adjustment groove 10 of the lower base plate 2.

[0066] S5. Place the sample reinforcement sheet on the upper part, and then take the sample reinforcement sheet 9 and place it on the adhesive surfaces at both ends of the upper surface of the sample 8, and between the two width adjustment limit blocks 3.

[0067] S6. Close the mold and fix it. Press the upper base plate 1 onto the lower base plate 2 to close the mold. First, fix the upper and lower base plates with the positioning pins 11, and finally tighten and fix them with bolts 12, so that the sample reinforcement sheet 9 is evenly stressed, ensuring the bonding quality of the sample reinforcement sheet 9 and the sample 8.

[0068] The composite sheet tensile test specimen preparation of this embodiment can realize one-time positioning of multiple test specimens, and at the same time, the pressure between the bottom plates can realize uniform stress on all the test specimen reinforcement sheets, ensuring the bonding quality between the test specimen reinforcement sheets and the test specimens, thereby improving the accuracy of the tensile strength data when testing the same batch of composite sheet tensile test specimens. In addition, the mold can be applied to the preparation of composite sheet tensile test specimens of different sizes and specifications, and can achieve high efficiency and accuracy in the preparation process of composite sheet tensile test specimens.

[0069] In summary, the mold realizes one-time positioning of multiple specimens 8 through the width adjustment positioning block 3 and the thickness adjustment positioning piece 4, and realizes uniform force on all specimen reinforcement sheets 9 through the pressure between the bottom plates, ensuring the bonding quality of the specimen reinforcement sheets 9 and the specimens 8, thereby improving the accuracy of the tensile strength data when testing the same batch of composite material specimens. In addition, the mold can also be used for the preparation of tensile specimens of composite sheet materials of different sizes, which is convenient for promotion and application.

[0070] Finally, it should be noted that the above embodiments are only used to illustrate the technical solutions of the present invention, rather than to limit it. Although the present invention has been described in detail with reference to the aforementioned embodiments, those skilled in the art should understand that they can still modify the technical solutions described in the aforementioned embodiments, or make equivalent replacements for some of the technical features therein. However, these modifications or replacements do not deviate the essence of the corresponding technical solutions from the spirit and scope of the technical solutions of the embodiments of the present invention.

Claims

1. A mold for making tensile specimens of composite sheets, Features: The mold comprises an upper base plate (1), a lower base plate (2), a width adjustment positioning block (3), a thickness adjustment positioning sheet (4), a positioning pin (11) and a bolt (12), and is characterized in that: Bolt holes (7) are provided on the upper base plate (1) and the lower base plate (2) so as to penetrate through the four sides thereof, and positioning pin holes (5) are provided on the upper base plate (1) and the lower base plate (2) so as to penetrate through the two ends of the test specimen (8) for mounting; the positioning pin holes (5) and the bolt holes (7) are used to pass positioning pins (11) and bolts (12) through them when the mold is closed, so as to fix and connect the upper base plate (1), the lower base plate (2), and the thickness adjustment limit plate (4); Demolding holes (6) are provided on the upper base plate (1) and are through-going at both side ends parallel to the installation direction of the sample (8); An equal number of left-right symmetrical adjustment grooves (10) are provided on the butt joint surface of at least one of the upper base plate (1) and the lower base plate (2) on both sides of the sample (8) in a vertical direction, and the adjustment grooves (10) are used to accommodate the width adjustment positioning block (3) and the sample reinforcement sheet (9); The thickness adjustment positioning piece (4) is located between the ends of the upper base plate (1) and the lower base plate (2), and corresponding pressure is applied to the surface of the sample (8), the width adjustment positioning block (3), and the sample reinforcement piece (9) by adjusting the tightness of the bolts; The depth of the adjustment groove (10) is equal to an integral multiple of the thickness of the sample reinforcement sheet (9), the length of the adjustment groove (10) is equal to the length of the sample reinforcement sheet (9), and the width of the adjustment groove (10) is equal to the sum of the width of the sample reinforcement sheet (9) and the thickness of the twice width adjustment positioning block (3); The length of the width adjustment positioning block (3) is equal to the length of the adjustment slot (10).

2. The mold according to claim 1, Features: The distance between two adjacent adjustment grooves (10) is equal to the length of the sample (8) minus twice the length of the adjustment groove (10).

3. The mold according to claim 1, Features: The height of the width adjustment positioning block (3) is greater than the sum of the depth of the adjustment groove (10) and the thickness of the sample (8), and less than twice the sum of the depth of the adjustment groove (10) and the thickness of the sample (8); the thickness of the width adjustment positioning block (3) is adjusted according to the width of the sample (8), and is equal to half of the difference between the width of the adjustment groove (10) and the width of the sample (8).

4. The mold according to claim 1, Features: The width adjustment positioning blocks (3) are arranged on both sides of the adjustment groove (10) and are parallel to the sample (8) to prevent the sample (8) and the sample reinforcement sheet (9) from being displaced left and right when the film is closed.

5. The mold according to claim 1, Features: The thickness of the thickness adjustment limit piece (4) is equal to the thickness of the sample (8), the length of the thickness adjustment limit piece (4) is equal to the side length of the corresponding bottom plate, and the width of the thickness adjustment limit piece (4) is equal to the length of the side width of the adjustment slot (10) of the bottom plate to the bottom plate frame.

6. The mold according to claim 5, Features: The thickness adjustment limit plates (4) are placed at both ends of the sample (8) and are perpendicular to the sample (8) to prevent the sample (8) from moving forward and backward when the film is closed, thereby ensuring the parallelism of the sample reinforcement plate (9) and the sample (8) during preparation and testing, as well as the accuracy of the bonding thickness.

7. A method for preparing a tensile test specimen of a composite material sheet by using the mold according to any one of claims 1 to 6, It is characterized in that The method comprises the following steps: S1, spraying a mold release agent, first spraying a liquid mold release agent on the sample preparation surface of the upper base plate (1) and the lower base plate (2), the surface of the width adjustment positioning block (3), and the surface of the thickness adjustment limit plate (4) to facilitate the cleaning of the adhesive residue after sample preparation; S2, sample processing, grinding the two sides of the sample (8) to be tested to be attached to the sample reinforcement sheet (9), cleaning and evenly applying adhesive, and then cleaning the surface of the attachment part of the sample reinforcement sheet (9) and evenly applying adhesive; S3, fill the lower groove, place the sample reinforcement sheet (9) into the adjustment groove (10) of the lower bottom plate (2), and make the bonding surface of the sample reinforcement sheet (9) face upwards, then place the width adjustment positioning block (3) into the adjustment groove (10) of the lower bottom plate (2), and place one width adjustment positioning block (3) on each side of the sample reinforcement sheet (9); S4. Place the sample, insert the sample (8) between the four width adjustment positioning blocks (3), and install the thickness adjustment limit plates (4) on both sides of the lower base plate (2) through the positioning pins (11), ensuring that the adhesive surfaces at both ends of the lower surface of the sample (8) are in contact with the adhesive surfaces of the sample reinforcement plate (9) in the adjustment groove (10) of the lower base plate (2); S5. Place the sample reinforcement sheet on the top, then take the sample reinforcement sheet (9) and place it on the adhesive surfaces at both ends of the upper surface of the sample (8), and between the two width adjustment positioning blocks (3); S6. The mold is closed and fixed. The upper base plate (1) is pressed onto the lower base plate (2) to close the mold. The upper and lower base plates are first fixed by positioning pins (11), and finally tightened and fixed by bolts (12) so that the specimen reinforcement sheet (9) is evenly stressed, thereby ensuring the bonding quality of the specimen reinforcement sheet (9) and the specimen (8).