Test structure, test structure forming method and working method
By designing test units arranged in an M row × N column array on the semiconductor chip and using electron beams and piezoelectric connections, the time-consuming problem of locating the failure location in the existing technology is solved, and the analysis efficiency and accuracy are improved.
Patent Information
- Application Number
- CN202011157504.6
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2020-10-26
- Publication Date
- 2024-10-22
- Estimated Expiration
- 2040-10-26
AI Technical Summary
In the existing technology, during the failure analysis process of semiconductor chips, multiple nanoprobe tests are needed to locate the failure location, which results in long time consumption and low efficiency.
Design a test structure, including forming test units arranged in an M row × N column array on a substrate. The test unit includes a gate structure and a metal layer arranged in parallel along a first direction, and is connected through electron beam irradiation and piezoelectricity. , simplify the testing process to locate the failure location.
By simplifying the test process, the efficiency of failure analysis is improved, manpower and equipment resources are saved, and the failure location is accurately located.
Smart Images

Figure CN114496989B_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the field of semiconductor testing technology, and in particular to a testing structure, a forming method of the testing structure and a working method. Background Art
[0002] In the process of manufacturing semiconductor integrated circuits (ICs), after the back-end of line (BEOL) process is completed, the interconnection layer for back-end interconnection has been prepared on the chip. At this time, the chip needs to be subjected to failure analysis (Failure Analysis), including EBAC (Electron Beam Absorbed Current) test.
[0003] EBAC testing is an effective back-end defect detection method. When performing EBAC testing, the chip to be tested needs to be placed in a scanning electron microscope (SEM), and the electron beam is irradiated to the surface of the chip. The nanoprobe contacts the test point (node) of the chip to be tested. The nanoprobe can detect the strength of the current, thereby determining the defects in the back-end interconnect layer, including open circuit, short circuit (bridge) and high resistance short circuit (high resistance short).
[0004] In the prior art, a chip to be tested has test units arranged in an array, and it is necessary to use a nanoprobe to test several times before locating the failure position, which takes a lot of time and wastes manpower and equipment utilization.
[0005] Therefore, how to improve the efficiency of failure analysis is an urgent problem to be solved. Summary of the invention
[0006] The technical problem solved by the present invention is to provide a test structure, a test structure forming method and a working method to improve the efficiency of failure analysis.
[0007] To solve the above technical problems, the technical solution of the present invention provides a test structure, including: a substrate; test units arranged in an array of M rows × N columns on the substrate, wherein M is a natural number greater than 1, and N is a natural number greater than 1, and the test units include: a plurality of gate structures arranged in parallel along a first direction, and a plurality of first metal layers located between adjacent gate structures, wherein the first direction is parallel to the substrate surface; a plurality of second metal layers located on the first metal layers, wherein any of the second metal layers is electrically connected to a first metal layer, and an extension direction of the second metal layer is parallel to an extension direction of the first metal layer; M third metal layers, wherein any of the third metal layers is electrically connected to a row of gate structures arranged in parallel along the first direction, and the third metal layer is parallel to the first direction; a fourth metal layer electrically connected to the M third metal layers, and the fourth metal layer, the third metal layer and the second metal layer are located on the same layer.
[0008] Optionally, the number of gate structures in the test unit is 3, and the number of first metal layers in the test unit is 2.
[0009] Optionally, an extension direction of the fourth metal layer is perpendicular to an extension direction of the third metal layer.
[0010] Optionally, it further includes: a plurality of fifth metal layers located on the second metal layer, any of the fifth metal layers is electrically connected to a row of second metal layers arranged in parallel along the first direction, and the fifth metal layer is parallel to the first direction.
[0011] Optionally, it also includes: a sixth metal layer electrically connected to the plurality of fifth metal layers, the extension direction of the sixth metal layer is perpendicular to the extension direction of the fifth metal layer, and the sixth metal layer and the fifth metal layer are located in the same layer.
[0012] Optionally, the number of the fifth metal layers is 2×M, and the number of the fifth metal layers electrically connected to any row of the second metal layers is 2.
[0013] Optionally, the gate structure includes a gate dielectric layer and a gate layer located on the gate dielectric layer.
[0014] Optionally, the material of the gate dielectric layer includes hafnium oxide or aluminum oxide; and the material of the gate layer includes tungsten.
[0015] Optionally, it also includes: a dielectric structure located on the substrate; the test unit, the second metal layer, the third metal layer, the fourth metal layer, the fifth metal layer and the sixth metal layer are located in the dielectric structure.
[0016] Optionally, it also includes: an isolation layer located on the substrate; and the test unit is located on the isolation layer.
[0017] Correspondingly, the technical solution of the present invention also provides a method for forming a test structure, comprising: providing a substrate; forming test units arranged in an array of M rows × N columns on the substrate, wherein M is a natural number greater than 1, and N is a natural number greater than 1, and the test units include: a plurality of gate structures arranged in parallel along a first direction, and a plurality of first metal layers located between adjacent gate structures, wherein the first direction is parallel to the surface of the substrate; forming a plurality of second metal layers located on the first metal layers, wherein any of the second metal layers is electrically connected to a first metal layer, and an extension direction of the second metal layer is parallel to an extension direction of the first metal layer; forming M third metal layers, wherein any of the third metal layers is electrically connected to a row of gate structures arranged in parallel along the first direction, and the third metal layer is parallel to the first direction; forming a fourth metal layer electrically connected to the M third metal layers, and the fourth metal layer, the third metal layer and the second metal layer are located on the same layer.
[0018] Optionally, the number of gate structures in the test unit is 3, and the number of first metal layers in the test unit is 2.
[0019] Optionally, an extension direction of the fourth metal layer is perpendicular to an extension direction of the third metal layer.
[0020] Optionally, the method further includes: forming a plurality of fifth metal layers on the second metal layers, any of the fifth metal layers being electrically connected to a row of second metal layers arranged in parallel along a first direction, and the fifth metal layers being parallel to the first direction.
[0021] Optionally, the method further includes: forming a sixth metal layer electrically connected to the plurality of fifth metal layers, wherein an extension direction of the sixth metal layer is perpendicular to an extension direction of the fifth metal layer, and the sixth metal layer and the fifth metal layer are located in the same layer.
[0022] Optionally, the number of the fifth metal layers is 2×M, and the number of the fifth metal layers electrically connected to any row of the second metal layers is 2.
[0023] Optionally, the method further includes: forming a dielectric structure on the substrate; the test unit, the second metal layer, the third metal layer, the fourth metal layer, the fifth metal layer and the sixth metal layer are located in the dielectric structure.
[0024] Correspondingly, the technical solution of the present invention also provides a testing method for a test structure, comprising: providing a test structure, the test structure comprising: a substrate; test units arranged in an array of M rows × N columns on the substrate, wherein M is a natural number greater than 1, and N is a natural number greater than 1, the test units comprising: a plurality of gate structures arranged in parallel along a first direction, and a plurality of first metal layers located between adjacent gate structures, wherein the first direction is parallel to the substrate surface; a plurality of second metal layers located on the first metal layer, any of the second metal layers being electrically connected to a first metal layer, and an extension direction of the second metal layer being parallel to an extension direction of the first metal layer; M third metal layers, any of the third metal layers being electrically connected to a row of gate structures arranged in parallel along the first direction, and the third metal layer being parallel to the first direction; a fourth metal layer electrically connected to the M third metal layers, the fourth metal layer, the third metal layer and the second metal layer being located on the same layer; grounding the gate structure and pressurizing the fourth metal layer; and detecting using a scanning electron microscope to obtain a failure position.
[0025] Optionally, the test structure also includes: a plurality of fifth metal layers located on the second metal layer, any of the fifth metal layers being electrically connected to a row of second metal layers arranged parallel to a first direction, and the fifth metal layer being parallel to the first direction; a sixth metal layer electrically connected to the plurality of fifth metal layers, the extension direction of the sixth metal layer being perpendicular to the extension direction of the fifth metal layer, and the sixth metal layer and the fifth metal layer being located on the same layer.
[0026] Optionally, the testing method of the test structure also includes: before grounding the gate structure and pressurizing the fourth metal layer, pressurizing the sixth metal layer to obtain the current of the test structure, and if the current is greater than a preset value, removing the fifth metal layer and the sixth metal layer to expose the fourth metal layer, the third metal layer and the second metal layer.
[0027] Optionally, the process of removing the fifth metal layer and the sixth metal layer includes a chemical mechanical polishing process.
[0028] Compared with the prior art, the technical solution of the present invention has the following beneficial effects:
[0029] The technical solution of the present invention provides a test structure, the test structure includes several second metal layers, any of the second metal layers is electrically connected to a first metal layer, the extension direction of the second metal layer is parallel to the extension direction of the first metal layer, the test structure also includes M third metal layers, any of the third metal layers is electrically connected to a row of gate structures arranged in parallel along the first direction, the third metal layer is parallel to the first direction, and the M third metal layers are electrically connected to the fourth metal layer. Therefore, during failure analysis, if the first metal layer and the gate structure are short-circuited, when the fourth metal layer is pressurized and several gate structures are grounded at the same time, the second metal layer electrically connected to the first metal layer will generate dark current under the irradiation of the electron beam, so that the short-circuit structure can be easily detected under a scanning electron microscope, so that the failure position can be accurately located. The test structure simplifies the test process, saves manpower and material resources, and improves test efficiency. BRIEF DESCRIPTION OF THE DRAWINGS
[0030] Figure 1 is a schematic structural diagram of a test structure in one embodiment;
[0031] Figures 2 to 5 is a structural schematic diagram of a test structure forming process in an embodiment of the present invention;
[0032] Figure 6 It is a flow chart of a testing method for a testing structure in an embodiment of the present invention. DETAILED DESCRIPTION
[0033] As described in the background art, how to improve the efficiency of failure analysis in the existing test structure is an urgent problem to be solved. Now, an analysis and explanation will be given in conjunction with a specific embodiment.
[0034] Figure 1 It is a schematic diagram of the structure of a test structure in one embodiment.
[0035] Please refer to Figure 1 , Figure 1 The top view of the dielectric structure is omitted for the test structure, which includes: a substrate 100; a plurality of test units located on the substrate 100, wherein the plurality of test units are arranged in an M×N array, and the test units include: three gate structures 101 arranged along a first direction parallel to the surface of the substrate 100; a first metal layer 102 located between adjacent gate structures 101; a second metal layer 103 connected to any row of the first metal layer 102; a third metal layer 104 connected to any row of the gate structures 101; and other metal layers (not shown) connected to the second metal layer 103 or connected to the third metal layer 104.
[0036] The test structure is formed simultaneously with the effective semiconductor structure. In the test structure, the first metal layer 102 is located between adjacent gate structures 101. Due to the shrinking of semiconductor technology nodes and the influence of the formation process, the first metal layer 102 is easily in contact with the adjacent gate structure 101 and causes a short circuit, thereby rendering the effective semiconductor structure formed simultaneously with the test structure inoperative.
[0037] Usually, the EBAC test is used to perform failure analysis on the test structure. First, the test structure is stripped layer by layer to expose the second metal layer 103 and the third metal layer 104, and then the M second metal layers 103 are contact-detected by a nanoprobe until the row m where the failed test unit is located is located. Then, the second metal layer 103 and the third metal layer 104 are removed to expose the first metal layer 102, and then the three gate structures 101 and the two first metal layers 102 in the test unit are detected by a nanoprobe to obtain the location of the failure. However, the test structure includes M×N test units, so the process takes a long time, and the test machine has limited machine time and cannot implement such a complicated test process.
[0038] In order to solve the above problems, the technical solution of the present invention provides a test structure, a test structure forming method and a working method, by electrically connecting any of the second metal layers to a first metal layer, the extension direction of the second metal layer is parallel to the extension direction of the first metal layer, the test structure also includes M third metal layers, any of the third metal layers is electrically connected to a row of gate structures arranged in parallel along the first direction, the third metal layer is parallel to the first direction, and the M third metal layers are electrically connected to the fourth metal layer. Therefore, during failure analysis, if the first metal layer and the gate structure are short-circuited, when the fourth metal layer is pressurized and several gate structures are grounded at the same time, the second metal layer electrically connected to the first metal layer will generate dark current under the irradiation of the electron beam, so that the short-circuit structure can be easily detected under a scanning electron microscope, so that the failure position can be accurately located. The test structure simplifies the test process, saves manpower and material resources, and improves test efficiency.
[0039] In order to make the above-mentioned objects, features and beneficial effects of the present invention more obvious and easy to understand, specific embodiments of the present invention are described in detail below with reference to the accompanying drawings.
[0040] Figures 2 to 5 Schematic diagram of the test structure forming process in an embodiment of the present invention.
[0041] Please refer to Figure 2 , providing a substrate 200.
[0042] In this embodiment, the material of the substrate 200 is silicon.
[0043] In other embodiments, the substrate material includes silicon carbide, silicon germanium, a multinary semiconductor material composed of group III-V elements, silicon on insulator (SOI) or germanium on insulator (GOI). Among them, the multinary semiconductor material composed of group III-V elements includes InP, GaAs, GaP, InAs, InSb, InGaAs or InGaAsP.
[0044] Please continue to refer to Figure 2 , a test unit arranged in an M-row×N-column array is formed on a substrate 200, where M is a natural number greater than 1, and N is a natural number greater than 1. The test unit includes: a plurality of gate structures 201 arranged in parallel along a first direction X, and a plurality of first metal layers 202 located between adjacent gate structures 201, and the first direction X is parallel to the surface of the substrate 200.
[0045] The number of gate structures 201 in the test unit is three, and the number of first metal layers 202 in the test unit is two.
[0046] In other embodiments, the number of gate structures in the test unit may be other numbers, and the number of first metal layers in the test unit may be other numbers.
[0047] The method for forming the test unit includes: forming a plurality of dummy gate structures on a substrate 200; forming a first dielectric layer (not shown) on the sidewalls of the dummy gate structures and the substrate 200; removing the dummy gate structures and forming a gate opening (not shown) in the first dielectric layer; forming a gate structure 201 in the gate opening; forming a second dielectric layer (not shown) on the gate structure 201 and the first dielectric layer; forming a plurality of first metal layers 202 in the second dielectric layer and the first dielectric layer, wherein the first metal layer 202 is located on the substrate 200 between adjacent gate structures 201.
[0048] In this embodiment, the gate structure 201 includes a gate dielectric layer (not shown) and a gate layer (not shown) located on the gate dielectric layer.
[0049] In this embodiment, the material of the gate dielectric layer includes a high dielectric constant material, the dielectric constant of the high dielectric constant material is greater than 3.9, and the high dielectric constant material includes aluminum oxide or hafnium oxide; the material of the gate layer includes a metal, and the metal includes tungsten.
[0050] The material of the first dielectric layer and the second dielectric layer includes a dielectric material, and the dielectric material includes a combination of one or more of silicon oxide, silicon nitride, silicon carbide, silicon oxycarbide, silicon oxynitride, aluminum oxide, aluminum nitride, silicon carbide nitride, and silicon oxycarbon nitride. In this embodiment, the material of the first dielectric layer and the second dielectric layer includes silicon oxide.
[0051] The material of the first metal layer 202 includes one or more of copper, titanium, aluminum, tungsten, cobalt, nickel and tantalum. In this embodiment, the material of the first metal layer 202 includes copper.
[0052] In this embodiment, before forming the test units arranged in an array of M rows×N columns on the substrate 200 , the method further includes: forming an isolation layer (not shown) on the substrate 200 ; and the test units are located on the isolation layer.
[0053] The material of the isolation layer includes a dielectric material, and the dielectric material includes a combination of one or more of silicon oxide, silicon nitride, silicon carbide, silicon oxycarbide, silicon oxynitride, aluminum oxide, aluminum nitride, silicon carbide nitride, and silicon oxycarbon nitride. In this embodiment, the material of the isolation layer includes silicon oxide.
[0054] Please refer to Figure 3 , forming a plurality of second metal layers 203 located on the first metal layer 202 , any second metal layer 203 is electrically connected to a first metal layer 202 , and an extension direction of the second metal layer 203 is parallel to an extension direction of the first metal layer 202 .
[0055] The method for forming the second metal layer 203 includes: forming a third dielectric layer (not shown) on the first metal layer 202 and the second dielectric layer; forming a first plug (not shown) in the third dielectric layer, the first plug is located on the first metal layer 202, and the first plug is electrically connected to the first metal layer 202; forming a fourth dielectric layer on the first plug and the third dielectric layer; forming the second metal layer 203 in the fourth dielectric layer, the second metal layer 203 is located on the first metal layer 202.
[0056] The material of the third dielectric layer and the fourth dielectric layer comprises a dielectric material, and the dielectric material comprises a combination of one or more of silicon oxide, silicon nitride, silicon carbide, silicon oxycarbide, silicon oxynitride, aluminum oxide, aluminum nitride, silicon carbide nitride, and silicon oxycarbon nitride. In this embodiment, the material of the third dielectric layer and the fourth dielectric layer comprises silicon oxide.
[0057] The material of the second metal layer 203 includes one or more of copper, titanium, aluminum, tungsten, cobalt, nickel and tantalum. In this embodiment, the material of the second metal layer 203 includes copper.
[0058] Please refer to Figure 4, forming M third metal layers 204, any of the third metal layers 204 is electrically connected to a row of gate structures 201 arranged in parallel along a first direction X, and the third metal layer 204 is parallel to the first direction X; forming a fourth metal layer 205 electrically connected to the M third metal layers 204, and the fourth metal layer 205, the third metal layer 204 and the second metal layer 203 are located in the same layer.
[0059] The fourth metal layer 205, the third metal layer 204 and the second metal layer 203 are formed simultaneously, and the fourth metal layer 205, the third metal layer 204 and the second metal layer 203 are located in the fourth dielectric layer. The third metal layer 204 is electrically connected to the gate structure 201 through a second plug (not shown) located on the gate structure 201, and the second plug is located in the third dielectric layer, and the second plug is formed simultaneously with the first plug.
[0060] In this embodiment, the extension direction of the fourth metal layer 205 is perpendicular to the extension direction of the third metal layer 204 .
[0061] Please refer to Figure 5 After forming the fourth metal layer 205, the third metal layer 204 and the second metal layer 203, a plurality of fifth metal layers 206 are formed on the second metal layer 203, and any of the fifth metal layers 206 is electrically connected to a row of second metal layers 203 arranged parallel to the first direction X, and the fifth metal layer 206 is parallel to the first direction X.
[0062] The method for forming the fifth metal layer 206 includes: forming a fifth dielectric layer (not shown) on the fourth dielectric layer, the fourth metal layer 205, the third metal layer 204 and the second metal layer 203; forming a third plug (not shown) in the fifth dielectric layer, the third plug is located on the second metal layer 203 and is electrically connected to the second metal layer 203; forming a sixth dielectric layer (not shown) on the third plug and the fifth dielectric layer; forming a fifth metal layer 206 in the sixth dielectric layer, the fifth metal layer 206 is located on the third plug.
[0063] The material of the fifth dielectric layer and the sixth dielectric layer includes a dielectric material, and the dielectric material includes a combination of one or more of silicon oxide, silicon nitride, silicon carbide, silicon oxycarbide, silicon oxynitride, aluminum oxide, aluminum nitride, silicon carbide nitride, and silicon oxycarbon nitride. In this embodiment, the material of the fifth dielectric layer and the sixth dielectric layer includes silicon oxide.
[0064] The material of the fifth metal layer 206 includes one or more of copper, titanium, aluminum, tungsten, cobalt, nickel and tantalum. In this embodiment, the material of the fifth metal layer 206 includes copper.
[0065] In this embodiment, the number of the fifth metal layers 206 is 2×M, and the number of the fifth metal layers 206 electrically connected to any row of the second metal layers 203 is 2. The two fifth metal layers 206 are electrically connected to a row of the second metal layers 203, so that the current density can be shared and the current carrying capacity of the third plug and the fifth metal layer 206 can be enhanced.
[0066] In other embodiments, the number of the fifth metal layers electrically connected to any row of the second metal layers may be other numbers.
[0067] Please continue to refer to Figure 5 , while forming the fifth metal layer 206, it also includes: forming a sixth metal layer 207 electrically connected to the plurality of fifth metal layers 206, wherein the extension direction of the sixth metal layer 207 is perpendicular to the extension direction of the fifth metal layer 206, and the sixth metal layer 207 and the fifth metal layer 206 are located in the same layer.
[0068] The sixth metal layer 207 is located in the sixth dielectric layer.
[0069] After the sixth metal layer 207 is formed, the process further includes: forming other metal layers and dielectric layers on the sixth dielectric layer and the sixth metal layer 207 , which are not shown in the figure.
[0070] The first dielectric layer, the second dielectric layer, the third dielectric layer, the fourth dielectric layer, the fifth dielectric layer, the sixth dielectric layer and other dielectric layers together constitute a dielectric structure located on the substrate 200, and the test unit, the second metal layer 203, the third metal layer 204, the fourth metal layer 205, the fifth metal layer 206, the sixth metal layer 207 and other metal layers are located in the dielectric structure, and the dielectric structure provides structural support for the test unit, the second metal layer 203, the third metal layer 204, the fourth metal layer 205, the fifth metal layer 206, the sixth metal layer 207 and other metal layers.
[0071] At this point, the test structure is formed, the test structure includes a plurality of second metal layers 203, any of the second metal layers 203 is electrically connected to a first metal layer 202, the extension direction of the second metal layer 203 is parallel to the extension direction of the first metal layer 202, the test structure also includes M third metal layers 204, any of the third metal layers 204 is electrically connected to a row of gate structures 201 arranged in parallel along the first direction X, the third metal layer 204 is parallel to the first direction X, and the M third metal layers 204 are electrically connected to the fourth metal layer 205. Therefore, during failure analysis, if the first metal layer 202 and the gate structure 201 are short-circuited, when the fourth metal layer 205 is pressurized and the plurality of gate structures 201 are grounded at the same time, the second metal layer 203 electrically connected to the first metal layer 202 will generate dark current under the irradiation of the electron beam, so that the short-circuit structure can be easily detected under a scanning electron microscope, so that the failure position can be accurately located. The test structure simplifies the test process, saves manpower and material resources, and improves test efficiency.
[0072] Accordingly, the embodiment of the present invention also provides a test structure, please continue to refer to Figure 5 ,include:
[0073] Substrate 200;
[0074] A test unit arranged in an M-row×N-column array on a substrate 200, where M is a natural number greater than 1, and N is a natural number greater than 1, and the test unit includes: a plurality of gate structures 201 arranged in parallel along a first direction X, and a plurality of first metal layers 202 located between adjacent gate structures 201, where the first direction X is parallel to the surface of the substrate 200;
[0075] A plurality of second metal layers 203 located on the first metal layer 202, any of the second metal layers 203 is electrically connected to one first metal layer 202, and an extension direction of the second metal layer 203 is parallel to an extension direction of the first metal layer 202;
[0076] M third metal layers 204, any of the third metal layers 204 being electrically connected to a row of gate structures 201 arranged in parallel along a first direction X, and the third metal layers 204 being parallel to the first direction X;
[0077] The fourth metal layer 205 is electrically connected to the M third metal layers 204 , and the fourth metal layer 205 , the third metal layer 204 and the second metal layer 202 are located in the same layer.
[0078] In this embodiment, the number of gate structures 201 in the test unit is three, and the number of first metal layers 202 in the test unit is two.
[0079] In this embodiment, the extension direction of the fourth metal layer 205 is perpendicular to the extension direction of the third metal layer 204 .
[0080] In this embodiment, it further includes: a plurality of fifth metal layers 206 located on the second metal layer 203 , any of the fifth metal layers 206 is electrically connected to a row of second metal layers 203 arranged in parallel along the first direction X, and the fifth metal layer 206 is parallel to the first direction X.
[0081] In this embodiment, it also includes: a sixth metal layer 207 electrically connected to the plurality of fifth metal layers 206 , the extension direction of the sixth metal layer 207 is perpendicular to the extension direction of the fifth metal layer 206 , and the sixth metal layer 207 and the fifth metal layer 206 are located in the same layer.
[0082] In this embodiment, the number of the fifth metal layers 206 is 2×M, and the number of the fifth metal layers 206 electrically connected to any row of the second metal layers 203 is 2.
[0083] In this embodiment, the gate structure 201 includes a gate dielectric layer (not shown) and a gate layer (not shown) located on the gate dielectric layer.
[0084] In this embodiment, the material of the gate dielectric layer includes hafnium oxide or aluminum oxide; the material of the gate layer includes tungsten.
[0085] In this embodiment, it also includes: a dielectric structure (not shown) located on the substrate 200; the test unit, the second metal layer 203, the third metal layer 204, the fourth metal layer 205, the fifth metal layer 206 and the sixth metal layer 207 are located in the dielectric structure.
[0086] In this embodiment, it further includes: an isolation layer (not shown) located on the substrate 200; and the test unit is located on the isolation layer.
[0087] The test structure includes a plurality of second metal layers 203, any of the second metal layers 203 is electrically connected to a first metal layer 202, the extension direction of the second metal layer 203 is parallel to the extension direction of the first metal layer 202, and the test structure also includes M third metal layers 204, any of the third metal layers 204 is electrically connected to a row of gate structures 201 arranged in parallel along a first direction X, the third metal layer 204 is parallel to the first direction X, and the M third metal layers 204 are electrically connected to the fourth metal layer 205. Therefore, during failure analysis, if the first metal layer 202 and the gate structure 201 are short-circuited, when the fourth metal layer 205 is pressurized and the plurality of gate structures 201 are grounded at the same time, the second metal layer 203 electrically connected to the first metal layer 202 will generate dark current under the irradiation of the electron beam, so that the short-circuit structure can be easily detected under a scanning electron microscope, so that the failure position can be accurately located. The test structure simplifies the test process, saves manpower and material resources, and improves the test efficiency.
[0088] Figure 6 4 is a flow chart of a testing method for a testing structure in an embodiment of the present invention.
[0089] Please refer to Figure 6 , the testing method of the test structure includes:
[0090] S100: Provide a test structure. For the formation process of the test structure, please refer to Figures 2 to 5 The test structure comprises: a substrate 200; test units arranged in an array of M rows×N columns on the substrate 200, wherein M is a natural number greater than 1, and N is a natural number greater than 1, and the test units comprise: a plurality of gate structures 201 arranged in parallel along a first direction X, and a plurality of first metal layers 202 located between adjacent gate structures 201, wherein the first direction X is parallel to the surface of the substrate 200; a plurality of second metal layers 203 located on the first metal layers 202, wherein any of the second metal layers 203 is electrically connected to a first metal layer 202, and an extension direction of the second metal layer 203 is parallel to an extension direction of the first metal layer 202; M third metal layers 204, wherein any of the third metal layers 204 is electrically connected to a row of gate structures 201 arranged in parallel along the first direction X, and the third metal layer 204 is parallel to the first direction X; and a fourth metal layer 205 electrically connected to the M third metal layers 204, wherein the fourth metal layer 205, the third metal layer 204, and the second metal layer 203 are located on the same layer.
[0091] In this embodiment, the test structure also includes: a plurality of fifth metal layers 206 located on the second metal layer 202, any of the fifth metal layers 206 being electrically connected to a row of second metal layers 203 arranged in parallel along a first direction X, and the fifth metal layer 206 being parallel to the first direction X; a sixth metal layer 207 electrically connected to the plurality of fifth metal layers 206, an extension direction of the sixth metal layer 207 being perpendicular to an extension direction of the fifth metal layer 206, and the sixth metal layer 207 and the fifth metal layer 206 being located on the same layer.
[0092] S200 : grounding the gate structure 201 and applying pressure to the fourth metal layer 205 .
[0093] In this embodiment, before the gate structure 201 is grounded and the fourth metal layer 205 is pressurized, the sixth metal layer 207 is pressurized to obtain the current of the test structure. If the current is greater than a preset value, the fifth metal layer 206 and the sixth metal layer 207 are removed to expose the fourth metal layer 205, the third metal layer 204 and the second metal layer 203.
[0094] In the test structure, if the first metal layer 202 and the gate structure 201 are in contact and short circuit, the current of the test structure will be larger than the preset current value, so it can be determined that the first metal layer 202 and the gate structure 201 are in contact and short circuit, and failure analysis is required.
[0095] In this embodiment, the process of removing the fifth metal layer 206 and the sixth metal layer 207 includes a chemical mechanical polishing process.
[0096] S300: Use scanning electron microscope to detect and obtain the failure location.
[0097] When the gate structure 201 is grounded and the fourth metal layer 205 is pressurized, the second metal layer 203 electrically connected to the first metal layer 202 generates dark current under the irradiation of the electron beam, and the first metal layer 202 and the gate structure 201 are short-circuited. The second metal layer 203 at the short-circuit position is easily detected under a scanning electron microscope, so that the failure position can be accurately located. The test structure simplifies the test process, saves manpower and material resources, and improves test efficiency.
[0098] Although the present invention is disclosed as above, the present invention is not limited thereto. Any person skilled in the art can make various changes and modifications without departing from the spirit and scope of the present invention. Therefore, the protection scope of the present invention shall be subject to the scope defined by the claims.
Claims
1. A test structure, characterized in that: include: substrate; A test unit arranged in an M-row×N-column array on a substrate, wherein M is a natural number greater than 1, and N is a natural number greater than 1, wherein the test unit comprises: a plurality of gate structures arranged in parallel along a first direction, and a plurality of first metal layers between adjacent gate structures, wherein the first direction is parallel to a surface of the substrate; A plurality of second metal layers located on the first metal layer, any of the second metal layers is electrically connected to a first metal layer, and an extension direction of the second metal layer is parallel to an extension direction of the first metal layer; M third metal layers, any of the third metal layers being electrically connected to a row of gate structures arranged in parallel along a first direction, and the third metal layers being parallel to the first direction; A fourth metal layer electrically connected to the M third metal layers, wherein the fourth metal layer, the third metal layer and the second metal layer are located in the same layer.
2. The test structure according to claim 1, characterized in that The number of gate structures in the test unit is 3, and the number of first metal layers in the test unit is 2.
3. The test structure according to claim 1, characterized in that: An extending direction of the fourth metal layer is perpendicular to an extending direction of the third metal layer.
4. The test structure according to claim 1, characterized in that: Also includes: A plurality of fifth metal layers are located on the second metal layers, any of the fifth metal layers is electrically connected to a row of second metal layers arranged in parallel along a first direction, and the fifth metal layers are parallel to the first direction.
5. The test structure according to claim 4, characterized in that: Also includes: A sixth metal layer is electrically connected to the plurality of fifth metal layers, wherein an extension direction of the sixth metal layer is perpendicular to an extension direction of the fifth metal layer, and the sixth metal layer and the fifth metal layer are located in the same layer.
6. The test structure according to claim 4, characterized in that: The number of the fifth metal layers is 2×M, and the number of the fifth metal layers electrically connected to any row of the second metal layers is 2.
7. The test structure according to claim 1, characterized in that: The gate structure includes a gate dielectric layer and a gate layer located on the gate dielectric layer.
8. The test structure according to claim 7, characterized in that: The material of the gate dielectric layer includes hafnium oxide or aluminum oxide; the material of the gate layer includes tungsten.
9. The test structure according to claim 5, characterized in that: Also includes: a dielectric structure disposed on a substrate; The test unit, the second metal layer, the third metal layer, the fourth metal layer, the fifth metal layer and the sixth metal layer are located in the dielectric structure.
10. The test structure according to claim 1, characterized in that: Also includes: An isolation layer is located on the substrate; and the test unit is located on the isolation layer.
11. A method for forming a test structure, characterized in that: include: providing a substrate; Forming a test unit arranged in an M-row×N-column array on a substrate, wherein M is a natural number greater than 1, and N is a natural number greater than 1, wherein the test unit comprises: a plurality of gate structures arranged in parallel along a first direction, and a plurality of first metal layers located between adjacent gate structures, wherein the first direction is parallel to a surface of the substrate; forming a plurality of second metal layers on the first metal layer, wherein any second metal layer is electrically connected to a first metal layer, and an extension direction of the second metal layer is parallel to an extension direction of the first metal layer; Forming M third metal layers, any of the third metal layers being electrically connected to a row of gate structures arranged in parallel along a first direction, and the third metal layers being parallel to the first direction; A fourth metal layer electrically connected to the M third metal layers is formed, and the fourth metal layer, the third metal layer and the second metal layer are located in the same layer.
12. The method for forming a test structure according to claim 11, wherein: The number of gate structures in the test unit is 3, and the number of first metal layers in the test unit is 2.
13. The method for forming a test structure according to claim 11, wherein: An extending direction of the fourth metal layer is perpendicular to an extending direction of the third metal layer.
14. The method for forming a test structure according to claim 11, wherein: Also includes: A plurality of fifth metal layers are formed on the second metal layers, any of the fifth metal layers is electrically connected to a row of second metal layers arranged in parallel along a first direction, and the fifth metal layers are parallel to the first direction.
15. The method for forming a test structure according to claim 14, wherein: Also includes: A sixth metal layer electrically connected to the plurality of fifth metal layers is formed, wherein an extension direction of the sixth metal layer is perpendicular to an extension direction of the fifth metal layer, and the sixth metal layer and the fifth metal layer are located in the same layer.
16. The method for forming a test structure according to claim 14, wherein: The number of the fifth metal layers is 2×M, and the number of the fifth metal layers electrically connected to any row of the second metal layers is 2.
17. The method for forming a test structure according to claim 15, wherein: Also includes: forming a dielectric structure on a substrate; The test unit, the second metal layer, the third metal layer, the fourth metal layer, the fifth metal layer and the sixth metal layer are located in the dielectric structure.
18. A method for testing a test structure, characterized in that: include: A test structure is provided, the test structure comprising: a substrate; test units arranged in an array of M rows×N columns on the substrate, wherein M is a natural number greater than 1, and N is a natural number greater than 1, the test units comprising: a plurality of gate structures arranged in parallel along a first direction, and a plurality of first metal layers located between adjacent gate structures, wherein the first direction is parallel to a surface of the substrate; a plurality of second metal layers located on the first metal layers, wherein any of the second metal layers is electrically connected to a first metal layer, and an extension direction of the second metal layer is parallel to an extension direction of the first metal layer; M third metal layers, wherein any of the third metal layers is electrically connected to a row of gate structures arranged in parallel along the first direction, and the third metal layer is parallel to the first direction; a fourth metal layer electrically connected to the M third metal layers, wherein the fourth metal layer, the third metal layer, and the second metal layer are located on the same layer; Grounding the gate structure and pressurizing the fourth metal layer; Scanning electron microscopy was used to detect the failure location.
19. The method for testing a test structure according to claim 18, wherein: The test structure also includes: a plurality of fifth metal layers located on the second metal layer, any of the fifth metal layers being electrically connected to a row of second metal layers arranged in parallel along a first direction, and the fifth metal layer being parallel to the first direction; a sixth metal layer being electrically connected to the plurality of fifth metal layers, an extension direction of the sixth metal layer being perpendicular to an extension direction of the fifth metal layer, and the sixth metal layer and the fifth metal layer being located on the same layer.
20. The method for testing a test structure according to claim 19, wherein: The testing method of the test structure also includes: before grounding the gate structure and pressurizing the fourth metal layer, pressurizing the sixth metal layer to obtain the current of the test structure, and if the current is greater than a preset value, removing the fifth metal layer and the sixth metal layer to expose the fourth metal layer, the third metal layer and the second metal layer.
21. The method for testing a test structure according to claim 20, wherein: The process of removing the fifth metal layer and the sixth metal layer includes a chemical mechanical polishing process.