A method for preparing a multi-dimensional nano high-performance flexible humidity sensor

By combining nanocellulose suspension with carbon fiber and nanotitanium dioxide, a multi-dimensional nano high-performance flexible humidity sensor was prepared, which solved the problem of development of flexible functional materials and realized a humidity sensor based on nanotitanium dioxide materials, with excellent sensitivity and Responsive recovery performance.

CN114660122BInactive Publication Date: 2024-11-05ZHEJIANG UNIV OF SCI & TECH
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202210443235.2
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2022-04-25
Publication Date
2024-11-05
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

In the context of modern industrial technology development, it is difficult to effectively solve the problem of how to obtain flexible functional materials for humidity sensors on the basis of ensuring the characteristics of nano titanium dioxide materials, especially in environmental pollution detection and treatment.

Method used

The nanocellulose suspension was mixed with carbon fiber and nanotitanium dioxide, and filtered through ultrasonic dispersion and polyvinylidene fluoride membrane to prepare a titanium dioxide-carbon fiber-nanocellulose gel. After pressing and drying, the golden cross finger electrode was processed on the composite membrane. Form a multi-dimensional nano high-performance flexible humidity sensor.

Benefits of technology

The prepared humidity sensor is not only flexible, excellent in performance and sensitive in response, but also has excellent sensitivity values ​​in the relative humidity range of 33%-97%, and has high humidity sensitivity response values ​​and good response recovery performance.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN114660122B_ABST
    Figure CN114660122B_ABST
Patent Text Reader

Abstract

The invention discloses a method for preparing a multidimensional nano high-performance flexible humidity sensor, wherein a nanocellulose suspension, carbon fiber and nano titanium dioxide are mixed, and after ultrasonic dispersion, vacuum-assisted filtration is performed with a polyvinylidene fluoride membrane filter to obtain a titanium dioxide-carbon fiber-nanocellulose gel, and then the titanium dioxide-carbon fiber-nanocellulose gel is pressed and dried to obtain a composite film, and finally a gold interdigital electrode is processed on the composite film by ion sputtering to form a flexible humidity sensor. The manufacturing process of the invention is convenient, and the obtained humidity sensor has good flexibility and excellent performance.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of humidity sensors, and in particular to a method for preparing a multi-dimensional nano high-performance flexible humidity sensor. Background Art

[0002] Humidity sensor is an important tool for detecting humidity changes and is widely used in our daily life. It is also suitable for real-time monitoring of human breathing, because it can quickly convert human breathing signals into visual electrical signals, which greatly facilitates people's lives.

[0003] With the development of modern industrial technology, global environmental problems have become increasingly prominent, and people are paying more attention to the detection and treatment technology of pollutants in the environment. Nano titanium dioxide (TiO2) has become one of the popular semiconductor materials due to its excellent photocatalytic performance, gas sensitivity, and no secondary pollution. In addition, due to the large specific surface area and special surface morphology of porous irregular morphology TiO2 nanotubes, it is bound to bring more possibilities for improving gas-sensitive performance. Especially at the moment when flexible devices are developing rapidly, how to obtain flexible functional materials while ensuring the characteristics of nano TiO2 materials is an urgent problem to be solved. Summary of the invention

[0004] The purpose of the present invention is to provide a method for preparing a multi-dimensional nano high-performance flexible humidity sensor. The manufacturing process of the present invention is convenient, and the humidity sensor prepared has good flexibility and excellent performance.

[0005] The technical solution of the present invention is a method for preparing a multi-dimensional nano high-performance flexible humidity sensor, which comprises mixing a nanocellulose suspension, carbon fiber and nano-titanium dioxide, and performing vacuum assisted filtration with a polyvinylidene fluoride membrane filter after ultrasonic dispersion to obtain a titanium dioxide-carbon fiber-nanocellulose gel, and then pressing and drying the titanium dioxide-carbon fiber-nanocellulose gel to obtain a composite film, and finally processing gold interdigital electrodes on the composite film by ion sputtering to form a flexible humidity sensor.

[0006] The above-mentioned method for preparing a multidimensional nano high-performance flexible humidity sensor, the preparation of the nano titanium dioxide is to place a titanium metal foil in an ethylene glycol solution containing 0.50-0.60wt% ammonium fluoride and 20-30wt% deionized water, and grow it at 30V-50V for 6-12 hours, so that white nano titanium dioxide grows on the surface of the titanium foil.

[0007] The aforementioned method for preparing a multidimensional nano high-performance flexible humidity sensor, the preparation of the nano titanium dioxide is to place a titanium metal foil in an ethylene glycol solution containing 0.55wt% ammonium fluoride and 25wt% deionized water, and grow it at 40V for 10 hours, so that white nano titanium dioxide grows on the surface of the titanium foil.

[0008] The above-mentioned method for preparing a multidimensional nano high-performance flexible humidity sensor, the preparation of the nanocellulose suspension is based on fiber material as raw material, after swelling in a propylene glycol aqueous solution with a mass concentration of 40-60% for 1-3 hours, pre-treated by enzymatic hydrolysis, and then continuously washed and centrifuged to obtain pretreated pulp, and then the pretreated pulp is ultrasonically treated at 25000psi for 15 minutes in a high-pressure micro-spray homogenizer to obtain the final nanocellulose suspension.

[0009] In the aforementioned method for preparing a multi-dimensional nano high-performance flexible humidity sensor, the concentration of the enzyme in the enzymatic hydrolysis is 10 U / mL, and the enzyme is a mixture of cellulase and xylanase at a concentration ratio of 9:1.

[0010] In the aforementioned method for preparing a multi-dimensional nano high-performance flexible humidity sensor, the temperature of the enzymatic hydrolysis is 50° C. and the hydrolysis time is 12 hours.

[0011] In the aforementioned method for preparing a multi-dimensional nano high-performance flexible humidity sensor, the ultrasonic dispersion is performed using an ultrasonic processor at an amplitude of 50%-80% for 5 minutes to 10 minutes.

[0012] In the aforementioned method for preparing a multi-dimensional nano high-performance flexible humidity sensor, the concentration of the nanocellulose suspension is 0.1 wt %.

[0013] In the aforementioned method for preparing a multi-dimensional nano high-performance flexible humidity sensor, the content of titanium dioxide in the titanium dioxide-carbon fiber-nanocellulose gel is 6%.

[0014] In the aforementioned method for preparing a multi-dimensional nano high-performance flexible humidity sensor, the content of carbon fiber in the titanium dioxide-carbon fiber-nanocellulose gel is 0.1-2%.

[0015] Compared with the prior art, the present invention combines nanocellulose suspension, carbon fiber and nano titanium dioxide, and utilizes the good biocompatibility, renewability, biodegradability and mechanical properties of nanocellulose itself, and the fibers are interlaced and connected with each other, which is easy to form a porous structure that is convenient for ion and electron transmission. In addition, carbon fiber has good conductivity, and the charges formed by water molecules can be efficiently migrated in the composite membrane, thereby improving the sensitivity of the sensor. Thus, the humidity sensor prepared by the present invention has both flexibility and good gas-sensitive performance. The manufacturing process of the present invention is convenient, and the humidity sensor prepared has good flexibility, excellent performance, and sensitive response, and shows excellent sensitivity values ​​in the relative humidity range of 33%-97%. In addition, because the sensor has a unique multidimensional structure, it can have a high humidity-sensitive response value while maintaining good response recovery performance. BRIEF DESCRIPTION OF THE DRAWINGS

[0016] Figure 1 is a schematic diagram of a humidity sensor of the present invention;

[0017] Figure 2 is the SEM image of titanium dioxide;

[0018] Figure 3 yes Figure 2 A magnified image of titanium dioxide in the medium;

[0019] Figure 4 This is a schematic diagram of the process of titanium dioxide nanotubes adsorbing water molecules;

[0020] Figure 5 is a response curve diagram of the humidity sensor prepared by the present invention to different humidity;

[0021] Figure 6 It is a graph showing the change in response value of humidity sensors with different titanium dioxide contents prepared by the present invention to humidity. DETAILED DESCRIPTION

[0022] The present invention is further described below in conjunction with the accompanying drawings and embodiments, but they are not intended to limit the present invention.

[0023] Example 1: A method for preparing a multidimensional nano high-performance flexible humidity sensor, wherein a nanocellulose suspension (containing 0.1wt% CNC, 50mL), carbon fiber (1%) and nano-titanium dioxide are mixed, and after ultrasonic dispersion, vacuum filtration is performed using a polyvinylidene fluoride membrane filter with a pore size of 0.22 microns to obtain a titanium dioxide-carbon fiber-nanocellulose gel, and then the titanium dioxide-carbon fiber-nanocellulose gel is pressed and dried to obtain a composite membrane, and finally gold interdigital electrodes are processed on the composite membrane by ion sputtering, such as Figure 1 As shown, a flexible humidity sensor is formed. Figure 1 In the figure, 1 represents the fibers in the composite membrane (including nanocellulose fibers and carbon fibers), 2 represents titanium dioxide nanotubes and nanospheres, and 3 represents electrodes.

[0024] Example 2: A method for preparing a multi-dimensional nano high-performance flexible humidity sensor, according to the following steps:

[0025] Step 1: Place a titanium metal foil (0.1 mm-0.5 mm) in an ethylene glycol solution containing 0.55 wt% ammonium fluoride and 25 wt% deionized water, and grow it at 40 V for 10 hours to grow white nano-titanium dioxide on the surface of the titanium foil. Use a scraper to gently peel off the titanium dioxide layer to obtain nano-titanium dioxide.

[0026] Step 2: Using wood pulp, cotton pulp, bamboo pulp and other fiber materials as raw materials, after swelling in a 50% glycerol aqueous solution for 2 hours, pre-treated by enzymatic hydrolysis. The concentration of the enzyme in the enzymatic hydrolysis is 10U / mL, the enzyme is a mixture of cellulase and xylanase at a concentration ratio of 9:1, the temperature of the enzymatic hydrolysis is 50°C, the hydrolysis time is 12 hours, and then continuous washing and centrifugation cycles are performed to obtain pre-treated pulp. After that, it is ultrasonically treated at 25,000 psi for 15 minutes in a high-pressure micro-spray homogenizer to obtain the final nanocellulose suspension.

[0027] Step 3: dilute the obtained nanocellulose suspension with ultrapure water to a concentration of 0.1 wt %. Thereafter, mix the nanocellulose suspension (containing 0.1 wt % CNC, 50 mL), carbon fiber (1%) and nano-titanium dioxide in step 1, and disperse them using an ultrasonic processor at an amplitude of 50%-80% for 5 minutes to 1 minute.

[0028] Step 4: Using a polyvinylidene fluoride membrane filter with a pore size of 0.22 microns, a titanium dioxide-carbon fiber-nanocellulose gel with a titanium dioxide content of 6% is prepared by vacuum assisted filtration. In other embodiments, the titanium dioxide content is 1% / 3%9% and 12% respectively. After filtration, the titanium dioxide-nanocellulose gel is pressed and dried under a laboratory environment and then peeled off from the filter membrane. Gold interdigitated electrodes are processed on the composite membrane by ion sputtering to form a humidity sensor.

[0029] The applicant used a scanning electron microscope to observe the titanium dioxide on the composite film and obtained the following Figure 2 and Figure 3 The SEM images shown. Figure 2 and Figure 3 It can be seen that the titanium dioxide on the composite film in the present application is in the form of hollow nanotubes with a tube mouth diameter of about 100 nm, and each nanotube is formed by stacking small balls with an average diameter of 80 nm. Therefore, the nanomaterial is composed of 0-dimensional nanoballs and 1-dimensional nanotubes, and has a multi-dimensional nanostructure. Figure 4 The figure shows the process of titanium dioxide nanotubes adsorbing water molecules (the hollow structure and spherical surface of the nanotubes provide a large number of adsorption sites for water molecules). The chemical adsorption process of water molecules causes the oxygen vacancy defects of titanium dioxide to migrate from the subsurface to the surface and causes the dissociation of water molecules, resulting in OH on the titanium dioxide surface. - As the humidity increases, the interaction between water molecules and OH groups increases. - The combination of groups forms a physical adsorption layer, through which the carriers can be easily transferred, and the response value of the humidity sensor is further improved. Figure 4 It is explained that the titanium dioxide formed by the present invention has good sensing ability to water molecules, making humidity sensing sensitive.

[0030] Furthermore, the present application uses the humidity sensor prepared in Example 2 to perform response analysis at different humidity levels, and obtains the following Figure 5 The humidity sensor shown in the figure shows the response curve to different humidity. Figure 5 It can be seen that the dynamic response curve of the humidity sensor prepared by the present invention to different humidity levels. Figure 5 It shows that high sensitivity of the humidity sensor is observed when exposed to conditions below 50% RH. When exposed to high humidity, the sensitivity of the sensor increases rapidly. When the relative humidity increases to 67%, the sensitivity of the sensor increases 55 times compared to when it increases to 33%. When the relative humidity is 97%, the sensor still shows a good response, with a sensitivity value close to 2000, which shows that the sensor has excellent sensitivity to both low and high humidity. At the same time, from Figure 5 The response recovery time of the sensor to different humidity can be calculated from the dynamic response curve. The response and recovery time of the sensor to 43% humidity are 34s and 18s respectively, which is sensitive. Furthermore, the present application uses the humidity sensors prepared with different titanium dioxide contents to perform response analysis at different humidity levels, and obtains the following Figure 6 The fitting curves between humidity sensors with different titanium dioxide contents and relative humidity are shown. Figure 6 It can be seen that the humidity sensors with different titanium dioxide contents of the present invention all have good responsiveness to humidity, and the humidity sensor with a titanium dioxide content of 6% preferably has the best response effect.

[0031] In summary, the present invention combines nanocellulose suspension, carbon fiber and nano titanium dioxide, and utilizes the good biocompatibility, renewability, biodegradability and mechanical properties of nanocellulose itself, and the fibers are interlaced and connected with each other, which is easy to form a porous structure that is convenient for ion and electron transmission. In addition, carbon fiber has good electrical conductivity, and the charges formed by water molecules can be efficiently migrated in the composite film, thereby improving the sensitivity of the sensor. Thus, the humidity sensor prepared by the present invention has both flexibility and good gas-sensitive performance. The manufacturing process of the present invention is convenient, and the prepared humidity sensor has good flexibility, excellent performance and sensitive response.

Claims

1. A method for preparing a multidimensional nano high-performance flexible humidity sensor, characterized in that: The nanocellulose suspension, carbon fiber and nano-titanium dioxide are mixed, and after ultrasonic dispersion, vacuum filtration is performed using a polyvinylidene fluoride membrane filter to obtain a titanium dioxide-carbon fiber-nanocellulose gel, and then the titanium dioxide-carbon fiber-nanocellulose gel is pressed and dried to obtain a composite membrane, and finally gold interdigital electrodes are processed on the composite membrane by ion sputtering to form a flexible humidity sensor; The preparation of the nano titanium dioxide is to place a titanium metal foil in an ethylene glycol solution containing 0.50-0.60wt% ammonium fluoride and 20-30wt% deionized water, and grow it at 30V-50V for 6-12 hours, so that white nano titanium dioxide grows on the surface of the titanium foil; The preparation of the nanocellulose suspension is to use fiber material as raw material, swell it in a glycerol aqueous solution with a mass concentration of 40-60% for 1-3 hours, pre-treat it by enzymatic hydrolysis, and then continuously wash and centrifuge to obtain pre-treated pulp, and then ultrasonically treat the pre-treated pulp in a high-pressure micro-spray homogenizer at 25000 psi for 15 minutes to obtain the final nanocellulose suspension; The content of titanium dioxide in the titanium dioxide-carbon fiber-nanocellulose gel is 6%; The content of carbon fiber in the titanium dioxide-carbon fiber-nanocellulose gel is 0.1-2%.

2. The method for preparing a multidimensional nano high-performance flexible humidity sensor according to claim 1, characterized in that: The nano titanium dioxide is prepared by placing a titanium metal foil in an ethylene glycol solution containing 0.55 wt % ammonium fluoride and 25 wt % deionized water, and growing it at 40 V for 10 hours, so that white nano titanium dioxide grows on the surface of the titanium foil.

3. The method for preparing a multidimensional nano high-performance flexible humidity sensor according to claim 1, characterized in that: The enzyme concentration in the enzymatic hydrolysis was 10 U / mL, and the enzyme was a mixture of cellulase and xylanase at a concentration ratio of 9:

1.

4. The method for preparing a multi-dimensional nano high-performance flexible humidity sensor according to claim 1, characterized in that: The temperature of the enzymatic hydrolysis is 50° C., and the hydrolysis time is 12 hours.

5. The method for preparing a multi-dimensional nano high-performance flexible humidity sensor according to claim 1, characterized in that: The ultrasonic dispersion is performed using an ultrasonic processor at an amplitude of 50% to 80% for 5 minutes to 10 minutes.

6. The method for preparing a multi-dimensional nano high-performance flexible humidity sensor according to claim 1, characterized in that: The concentration of the nanocellulose suspension is 0.1 wt %.