A method and device for predicting fracture aperture coefficient of buried hill reservoir based on XRD whole rock logging

Through XRD whole rock recording technology and matrix rock mineral elastic micronuclear model, the problem of difficult to judge the fracture properties of complex latent mountain reservoirs is solved, and the accurate prediction and evaluation of the crack opening of the reservoir is achieved, which improves the accuracy of oil and gas exploration. Sex and efficiency.

CN114720494BActive Publication Date: 2024-11-08CNOOC ENERGY TECHNOLOGY & SERVICES LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202210199743.0
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2022-03-01
Publication Date
2024-11-08
Estimated Expiration
2042-03-01

AI Technical Summary

Technical Problem

In oil and gas exploration, it is difficult to directly judge the fracture properties of complex latent mountain reservoirs. The existing technology has not fully utilized the formation information obtained by XRD diffraction whole rock analysis, especially in the case of fine fragmentation of rocks, and it is difficult to predict the reservoir in real time. Fracture opening and developmental characteristics.

Method used

Through XRD whole rock recording technology, the bottom rock cuttings were collected for X-ray diffraction analysis, and the elastic micronumeral model of matrix rock was constructed. Combined with rheology model theory, mineral elastic micronumerals were established to form series and parallel models of mineral elastic micronumerals, and the crack opening coefficient was calculated. Real-time forecast of the crack development characteristics of the reservoir.

Benefits of technology

Accurate prediction and evaluation of the crack opening of the latent mountain reservoir is achieved, which has the advantages of low cost, high real-time data acquisition, and continuous profile prediction, and improves the accuracy of reservoir exploration.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN114720494B_ABST
    Figure CN114720494B_ABST
Patent Text Reader

Abstract

The present invention discloses a method and device for predicting the fracture aperture coefficient of buried hill reservoir based on XRD whole rock logging. The device includes: a rock cuttings collection, cleaning, drying and grinding device, a portable XRD diffractometer, a matrix rock mineral elastic microelement simulator, a matrix rock elastic parameter calculator, a fracture aperture coefficient calculator, an interpretation mapping device and a long map printing device. The workflow is to sample, clean, dry and grind the returned rock cuttings to prepare XRD diffraction standard rock cuttings powder; test its X-ray diffraction spectrum to determine the mineral type and content; perform mineral elastic microelement series and parallel combination of the matrix rock mineral elastic microelement simulator to calculate the elastic parameters; perform logging and experimental calibration to calculate the matrix rock elastic parameters; calculate the fracture aperture coefficient; interpret the calculation results in real-time while drilling and print the long map. The problem of lack of means for predicting fractures in buried hill reservoirs and real-time evaluation while drilling is solved, and the problems of poor continuity and low accuracy are effectively dealt with.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the field of oil and gas logging, and in particular to a method and device for predicting fracture aperture coefficient of buried hill reservoir based on XRD whole rock logging. Background Art

[0002] With the deepening of oil and gas exploration, there have been certain breakthroughs in buried hill oil and gas reservoirs. The understanding of complex buried hill fractured reservoirs has become more and more urgent. The prediction and evaluation of reservoir fractures is a core task of buried hill reservoir exploration.

[0003] The physical information of rock cuttings obtained by rock cutting logging is the most direct reflection of the properties of the formation. However, with the use of new drilling technologies, the rock cuttings returned from the bottom of the well are usually very fine, even in powder form, making it difficult to directly judge the properties of the reservoir. XRD diffraction whole-rock logging technology is a mainstream logging technology developed in recent years. By performing X-ray diffraction whole-rock analysis on rock cutting samples, the mineral composition and content are obtained. It is currently mainly used in the naming of formation lithology. The actual mineral composition contains rich stratigraphic information and is the main controlling factor of the mechanical properties of the formation and the difficulty of fracture development. At present, this information has not been fully explored. It is particularly urgent and important to deepen the application of this information in rock mechanical characteristics and reservoir fracture development characteristics. Summary of the invention

[0004] The purpose of the present invention is to provide a method and device for predicting the fracture aperture coefficient of buried hill reservoirs based on XRD whole-rock logging. The method and device can perform XRD diffraction whole-rock testing through returned rock cuttings information, calculate the formation fracture aperture coefficient in real time while drilling, and predict the difficulty of fracture development.

[0005] In a first aspect, the present invention provides a method for predicting fracture aperture coefficient of buried hill reservoir based on XRD whole rock logging, which is performed according to the following steps:

[0006] Step 1: Design the sampling interval according to the principle of sparse non-reservoir intervals and dense reservoir intervals, and then continuously pick fresh cuttings from the bottom of the well in front of the vibrating screen in strict accordance with the late arrival time and sampling intervals.

[0007] Step 2: Process the rock cuttings into XRD diffraction analysis standard samples, test their X-ray diffraction spectra, and determine the mineral content of the rock matrix in strata at different depths.

[0008] Step 3: Construct an elastic microelement model of matrix rock minerals, idealize various minerals into an elastic microelement, and make the elastic microelement consistent with the mechanical properties of each mineral itself, characterize and determine the constitutive equation and elastic parameters of each elastic microelement.

[0009] Step 4: Construct a physical model of mineral elastic micro-element combination. Based on the rheological model theory, various mineral elastic micro-elements are connected in series and in parallel to construct a physical model of mineral elastic micro-element combination.

[0010] Step 5: Based on the principle that the total stress of the mineral elastic micro-element series model is equal to the stress of each mineral elastic micro-element, and the total strain of the mineral elastic micro-element series model is equal to the sum of the strains of each mineral elastic micro-element, the constitutive equation and elastic parameters of the mineral elastic micro-element series model are established.

[0011] Step 6: Based on the principle that the total stress of the mineral elastic micro-element parallel model is equal to the sum of the stresses of each mineral elastic micro-element, and the total strain of the mineral elastic micro-element parallel model is equal to the strain of each mineral elastic micro-element, the constitutive equation and elastic parameter model of the mineral elastic micro-element parallel model are established.

[0012] Step 7: The elastic modulus and Poisson's ratio calculated by the mineral elastic micro-element series model and the mineral elastic micro-element parallel model are calibrated by logging and indoor experiments to establish the mathematical and physical equations of the matrix rock elastic modulus and Poisson's ratio suitable for regional characteristics.

[0013] Step 8: Based on the classical equation of the crack opening increment of a uniformly distributed load straight crack under two-dimensional plane strain, define the crack opening coefficient, and establish the elastic modulus and Poisson's ratio expressions of the crack opening coefficient.

[0014] Step 9: Based on the mineral content results of the rock matrix at different depths measured in steps 1 and 2, use the methods of steps 3 and 4 to construct a matrix rock mineral elastic microelement model and a mineral elastic microelement combination physical model. Combined with the principles of steps 5 and 6, deduce the constitutive equations and elastic parameters of the mineral elastic microelement series model and the mineral elastic microelement parallel model. Then, use the method of step 7 to perform logging and indoor experimental calibration, establish the elastic modulus and Poisson's ratio mathematical and physical equations of the matrix rock in the characteristic area, substitute them into step 8 to obtain the fracture aperture coefficient of the matrix rock, and predict the fracture development characteristics of the reservoir.

[0015] A further technical solution is that in step 4, the mineral elastic micro-element combination physical model includes a mineral elastic micro-element series model and a mineral elastic micro-element parallel model, wherein the relationship between the load and deformation of the mineral elastic micro-element series model is as follows:

[0016] F z =F 1z =F 2z =…F nz

[0017] ΔL z =ΔL1+ΔL2+…ΔL n

[0018] Where: F zis the total load on the mineral elastic microelement series model, KN; ΔL z is the total load and deformation of the mineral elastic microelement series model; F iz (i=1,2,…,n) is the load on a mineral elastic microelement; ΔL i (i=1,2,…,n) is the elastic microelement deformation of a certain mineral.

[0019] The load and deformation relationship of the mineral elastic microelement parallel model is as follows:

[0020] F r =F 1r +F 2r +…F nr

[0021] ΔL=ΔL1=ΔL2=…ΔL n

[0022] Where: F r is the total load on the mineral elastic microelement parallel model, KN; ΔL r F is the total load and deformation of the mineral elastic microelement parallel model; ir (i=1,2,…,n) is the load borne by a certain mineral elastic element.

[0023] A further technical solution is that the constitutive equation and elastic parameter characterization of the mineral elastic microelement series model established in step 5 are as follows:

[0024] The constitutive equation of the mineral elastic microelement series model is:

[0025]

[0026] The elastic modulus of the mineral elastic microelement series model is:

[0027]

[0028] The Poisson's ratio of the mineral elastic microelement series model is:

[0029]

[0030] Where: z is the total stress of the mineral elastic microelement series model; E z is the elastic modulus of the mineral elastic microelement series model; μ z E is the Poisson's ratio of the mineral elastic microelement series model; i (i=1,2,…,n) is the elastic modulus of the ith mineral; μ i (i=1,2,…,n) is the elastic microelement Poisson’s ratio of the i-th mineral; is the content of the ith mineral.

[0031] A further technical solution is that the constitutive equation and elastic parameter characterization of the mineral elastic microelement parallel model established in step 6 are as follows:

[0032] Constitutive equation of parallel model of mineral elastic microelement

[0033]

[0034] The elastic modulus of the mineral elastic microelement parallel model is:

[0035]

[0036] The Poisson's ratio of the mineral elastic microelement parallel model is:

[0037]

[0038] Where: r E is the stress of the mineral elastic microelement parallel model; r is the elastic modulus of the mineral elastic microelement parallel model; μ r is the Poisson's ratio of the mineral elastic microelement series model.

[0039] A further technical solution is to calibrate the elastic modulus and Poisson's ratio calculated by the series model and the parallel model in step 7 through logging and indoor experiments, and construct the mathematical and physical equations of matrix elastic parameters suitable for regional characteristics as follows:

[0040]

[0041]

[0042] Where: E A is the equivalent elastic modulus of rock matrix; α is the correction coefficient of the equivalent elastic modulus of rock matrix; μ A is the equivalent Poisson's ratio of rock matrix, and β is the correction coefficient of the equivalent Poisson's ratio of rock matrix.

[0043] A further technical solution is that the elastic modulus and Poisson's ratio of the crack opening coefficient in step 8 are expressed as follows

[0044]

[0045] Where: F w is the crack opening coefficient.

[0046] In the second aspect, the present invention provides a device for predicting the fracture aperture coefficient of a buried hill reservoir based on XRD whole-rock logging, comprising: a rock cuttings collection device, a rock cuttings cleaning device, a rock cuttings drying device, a rock cuttings grinding device, a portable XRD diffractometer, a matrix rock mineral elastic microelement simulator, a matrix rock elastic parameter calculation device, a fracture aperture coefficient calculation device, an interpretation mapping device and a long map printing device.

[0047] The working process of the device is as follows: the rock cuttings collection device is placed below the sand outlet of the vibrating screen, and the rock cuttings fall into the sampler along the inclined surface of the screen cloth; fresh rock cuttings are selected and placed in the rock cuttings cleaning device, and the rock cuttings are cleaned while being fully stirred until the rock cuttings reveal their original color; the cleaned rock cuttings are placed in the rock cuttings drying device and dried under an environment where the temperature is controlled to be less than 85°C; the dried rock cuttings are placed in the rock cuttings grinding device for grinding to make the rock cuttings into powder with a particle size of less than 20um; the ground rock cuttings powder is placed in a portable XRD diffractometer to test its X-ray diffraction spectrum and interpret the mineral type and content data of the rock matrix of different depth formations; the mineral type and content data of the rock matrix are transmitted to the matrix rock mineral elastic microelement simulator, and the matrix rock mineral elastic microelement simulator constructs mineral elastic microelement according to the mineral type and content, and performs series and parallel combination of mineral elastic microelement, and calculates the elastic parameter E under the series and parallel combination z ,μ z ,E r ,μ r ; The calculated elastic parameter E z ,μ z ,E r ,μ r Transmitted to the matrix rock elastic parameter calculation device to calculate the matrix rock elastic parameter E A and μ A ; The matrix rock elastic parameter E A and μ A Transmitted to the crack opening coefficient calculation device to calculate the crack opening coefficient F w ; The matrix rock elastic parameter E calculated by the matrix rock elastic parameter calculation device and the fracture opening coefficient calculation device A and μ A and crack opening coefficient F w The data are transmitted and stored in the interpretation and mapping device for mapping and real-time prediction of reservoir fracture development; finally, the long-map printing device is used to print and archive the data.

[0048] Compared with the prior art, the advantages of the present invention are:

[0049] The present invention uses rock cuttings collected by logging while drilling to perform XRD diffraction whole-rock mineral analysis to obtain the mineral content of rock matrix in strata at different depths. Combined with the mineral composition physical model, the constitutive equation and mechanical parameters of the rock matrix are deduced to predict the fracture aperture coefficient, thereby realizing the prediction and evaluation of reservoir fractures. The method has the advantages of low cost, high real-time data collection and continuity of profile prediction, etc. BRIEF DESCRIPTION OF THE DRAWINGS

[0050] Figure 1 : Flow chart of the method for predicting formation fracture aperture coefficient based on XRD whole-rock logging.

[0051] Figure 2 : Microelement model of mineral elasticity.

[0052] Figure 3 : Microelement series model of mineral elasticity.

[0053] Figure 4 : Parallel model of mineral elasticity.

[0054] Figure 5 : Application example of crack aperture coefficient.

[0055] Figure 6 : Schematic diagram of the formation fracture aperture coefficient prediction device based on XRD whole-rock logging.

[0056] For ordinary technicians in this field, other relevant drawings can be obtained based on the above drawings without any creative work. DETAILED DESCRIPTION

[0057] The present invention is described below based on examples, but it is worth noting that the present invention is not limited to these embodiments. In the detailed description of the present invention below, some specific details are described in detail. However, for the part that is not described in detail, those skilled in the art can also understand the present invention completely.

[0058] In addition, those skilled in the art should understand that the drawings are only provided to illustrate the purpose, features and advantages of the present invention, and the drawings are not actually drawn to scale.

[0059] Example

[0060] Figure 1 This is a flowchart of the formation fracture aperture coefficient prediction method based on XRD full rock logging of the present invention, Figure 1 , describing the specific implementation modes of the present invention.

[0061] Step 1 (101): Design the sampling interval according to the principle that the non-reservoir section is sparse and the reservoir section is dense. Then, pick the cuttings in front of the vibrating screen in strict accordance with the late arrival time and sampling interval, remove all kinds of false cuttings and residual cuttings, collapsed materials and fallen blocks, and select the fresh cuttings that are small in size, fresh in color and with obvious edges and corners and are truly from the bottom of the well.

[0062] Step 2 (102): Grind the fresh rock cuttings into powder, load them into the sample pool of the X-ray diffractometer, conduct an XRD diffraction experiment, test the X-ray diffraction spectrum of the sample, and determine the mineral type and content of the rock matrix in different depths of the strata based on the characteristic peak value of each mineral.

[0063] Step 3 (103): Construct a matrix rock mineral elastic microelement model, idealizing the various minerals that make up the rock into an elastic microelement, as shown in the attached figure. Figure 2 As shown in Table 1, the elastic microelement is consistent with the mechanical properties of each mineral itself. The constitutive equation and elastic parameters of each mineral itself are also the constitutive equation and elastic parameters of the elastic modulus of the elastic microelement. The elastic modulus and Poisson's ratio of common rock-forming mineral elastic microelements are shown in Table 1.

[0064] Table 1 Elastic modulus and Poisson's ratio of elastic microelement of common rock-forming minerals

[0065] mineral Elastic modulus(GPa) Poisson's ratio quartz 96.4 0.09 Calcite 81.0 0.28 Plagioclase 74.9 0.28 Sodium feldspar 78.5 0.29 dolomite 121 0.28 magnetite 230.8 0.26 Pyrite 299.9 0.16 Epidote 154.2 0.26 Spinel 293.3 0.26 muscovite 78.9 0.25 Biotite 69.66 0.25 Hornblende 128.8 0.28 Pyroxene 143.7 0.24 Clay Minerals 14.2 0.30

[0066] Step 4 (104): Construction of a mineral elastic microelement combination physical model based on the rheological model theory method

[0067] Based on the rheological model theory, various mineral elastic micro-elements are connected in series and in parallel to construct a mineral elastic micro-element combination physical model, including a mineral elastic micro-element series model and a mineral elastic micro-element parallel model. Figure 3 , mineral elastic microelement parallel model see Figure 4 .

[0068] Among them, the load and deformation relationship of the mineral elastic microelement series model follows the following principles:

[0069] F z =F 1z =F 2z =…F nz

[0070] ΔL z =ΔL1+ΔL2+…ΔL n

[0071] Among them, the load and deformation relationship of the mineral elastic microelement parallel model follows the following principles:

[0072] F r =F 1r +F 2r +…F nr

[0073] ΔL=ΔL1=ΔL2=…ΔL n

[0074] Step 5 (105): Based on the principle that the total stress of the mineral elastic microelement series model is equal to the stress of each mineral elastic microelement, and the total strain of the mineral elastic microelement series model is equal to the sum of the strains of each mineral elastic microelement, the constitutive equation and elastic parameters of the mineral elastic microelement series model are established.

[0075] The constitutive equation of the mineral elastic microelement series model is:

[0076]

[0077] The elastic modulus of the mineral elastic microelement series model is:

[0078]

[0079] The Poisson's ratio of the mineral elastic microelement series model is:

[0080]

[0081] Step 6 (106): Based on the principle that the total stress of the mineral elastic microelement parallel model is equal to the sum of the stresses of each mineral elastic microelement and the total strain of the mineral elastic microelement parallel model is equal to the strain of each mineral elastic microelement, the constitutive equation and elastic parameter model of the mineral elastic microelement parallel model are established.

[0082] Constitutive equation of parallel model of mineral elastic microelement

[0083]

[0084] The elastic modulus of the mineral elastic microelement parallel model is:

[0085]

[0086] The Poisson's ratio of the mineral elastic microelement parallel model is:

[0087]

[0088] Step 7 (107): The elastic modulus and Poisson's ratio calculated by the mineral elastic micro-element series model and the mineral elastic micro-element parallel model are calibrated by logging and indoor experiments to establish a mathematical physical equation for the elastic modulus and Poisson's ratio of the matrix rock suitable for the corresponding area. The equation is in the following form:

[0089]

[0090]

[0091] Step 8 (108): Prediction of formation fracture aperture coefficient based on XRD whole rock logging

[0092] Based on the classical model of uniformly distributed load straight crack opening increment under two-dimensional plane strain in linear elastic fracture mechanics, the crack opening coefficient is defined as:

[0093]

[0094] For a given driving stress change, the higher the crack opening coefficient, the easier it is for the crack to open.

[0095] Step 9 (109): Based on the mineral content results of the rock matrix at different depths measured in steps 1 and 2, use the methods of steps 3 and 4 to construct a matrix rock mineral elastic microelement model and a mineral elastic microelement combination physical model. Combined with the principles of steps 5 and 6, deduce the constitutive equation and elastic parameters of the response mineral elastic microelement combination physical model. After logging and indoor experimental calibration and back calculation using the method of step 7, establish the rock matrix elastic modulus and Poisson's ratio mathematical and physical equations suitable for regional characteristics, and substitute them into step 8 to obtain the fracture aperture coefficient of the matrix rock.

[0096] Step 10 (110) converts the matrix rock elastic parameter E A and μ A and crack opening coefficient F w Interpret and map the data and print out long pictures to predict reservoir fracture development in real time.

[0097] In the second aspect, the present invention provides a device for predicting the fracture aperture coefficient of a buried hill reservoir based on XRD whole-rock logging, comprising: a rock cuttings collection device 601, a rock cuttings cleaning device 602, a rock cuttings drying device 603, a rock cuttings grinding device 604, a portable XRD diffractometer 605, a matrix rock mineral elastic microelement simulator 606, a matrix rock elastic parameter calculation device 607, a fracture aperture coefficient calculation device 608, an interpretation mapping device 609 and a long map printing device 610.

[0098] The working process of the device is as follows: the rock chip collection device 601 is placed below the sand outlet of the vibrating screen, and the rock chips fall into the sampler along the inclined surface of the screen cloth; fresh rock chips are selected and placed in the rock chip cleaning device 602, and the rock chips are cleaned while being fully stirred until the rock chips reveal their original color; the cleaned rock chips are placed in the rock chip drying device 603, and dried in an environment where the temperature is controlled to be less than 85°C; the dried rock chips are placed in the rock chip grinding device 604 for grinding to make the rock chips into powder with a particle size of less than 20um; the ground rock chip powder is placed in the portable XRD diffractometer 605, and its X-ray diffraction spectrum is tested to interpret the mineral type and content data of the rock matrix of different depth formations; the mineral type and content data of the rock matrix are transmitted to the matrix rock mineral elastic microelement simulator 606, and the matrix rock mineral elastic microelement simulator constructs mineral elastic microelement according to the mineral type and content, and performs series and parallel combination of mineral elastic microelement, and calculates the elastic parameter E under the series and parallel combination z ,μ z ,E r ,μ r ; The calculated elastic parameter E z ,μ z ,E r ,μ r The matrix rock elastic parameter E is transmitted to the matrix rock elastic parameter calculation device 607 to calculate the matrix rock elastic parameter EA and μ A ; The matrix rock elastic parameter E A and μ A The data is transmitted to the crack opening coefficient calculation device 608 to calculate the crack opening coefficient F w ; The matrix rock elastic parameter E calculated by the matrix rock elastic parameter calculation device and the fracture opening coefficient calculation device A and μ A and crack opening coefficient F w Transmitted and stored in the interpretation and mapping device 609, mapped, and predicted the development of reservoir fractures in real time; finally printed and archived through the long map printing device 610

[0099] The above description is only an illustrative embodiment of the present invention and is not intended to limit the scope of the present invention. Any equivalent changes and modifications made by any person skilled in the art without departing from the concept and principle of the present invention shall fall within the scope of protection of the present invention.

Claims

1. A method for predicting fracture aperture coefficient of buried hill reservoir based on XRD whole rock logging, characterized in that: Step 1: Design the sampling interval according to the principle of sparse non-reservoir sections and dense reservoir sections, and then continuously pick fresh rock cuttings from the bottom of the well in front of the vibrating screen in strict accordance with the late arrival time and sampling interval, and wash, dry and grind them to process them into standard rock cuttings powder for XRD diffraction analysis; Step 2: Put the standard rock powder into the sample cell of the portable XRD diffractometer, test its X-ray diffraction spectrum, and determine the mineral types and contents of the rock matrix in the strata at different depths; Step 3: Construct a matrix rock mineral elastic microelement model, idealize various minerals into an elastic microelement, and make the elastic microelement consistent with the mechanical properties of each mineral itself, characterize and determine the constitutive equation and elastic parameters of each mineral elastic microelement; Step 4: Construct a mineral combination physical model. Based on the rheological model theory, various mineral elastic micro-elements are connected in series and in parallel to construct a mineral elastic micro-element combination physical model, including a mineral elastic micro-element series model and a mineral elastic micro-element parallel model. Step 5: Based on the principle that the total stress of the mineral elastic micro-element series model is equal to the stress of each mineral elastic micro-element, and the total strain of the mineral elastic micro-element series model is equal to the sum of the strains of each mineral elastic micro-element, the constitutive equation and elastic parameter model of the mineral elastic micro-element series model are established; Step 6: Based on the principle that the total stress of the mineral elastic micro-element parallel model is equal to the sum of the stresses of each mineral elastic micro-element, and the total strain of the mineral elastic micro-element parallel model is equal to the strain of each mineral elastic micro-element, the constitutive equation and elastic parameter model of the mineral elastic micro-element parallel model are established; Step 7: Conduct well logging and indoor experimental calibration on the elastic modulus and Poisson's ratio calculated by the mineral elastic micro-element series model and the mineral elastic micro-element parallel model, and establish mathematical and physical equations of matrix rock elastic modulus and Poisson's ratio suitable for the characteristic area; Step 8: Based on the classical equation of the crack opening increment under uniform load under plane strain, define the crack opening coefficient, and establish the elastic modulus and Poisson's ratio expression of the crack opening coefficient; Step 9: Based on the mineral content results of the rock matrix at different depths measured in steps 1 and 2, use the methods of steps 3 and 4 to construct a matrix rock mineral elastic microelement model and a mineral elastic microelement combination physical model. Combined with the principles of steps 5 and 6, deduce the constitutive equations and elastic parameters of the mineral elastic microelement series model and the mineral elastic microelement parallel model. Then, use the method of step 7 to perform logging and indoor experimental calibration, establish the elastic modulus and Poisson's ratio mathematical and physical equations of the matrix rock in the characteristic area, substitute them into step 8 to obtain the fracture aperture coefficient of the matrix rock, and predict the fracture development characteristics of the reservoir.

2. The method for predicting fracture aperture coefficient of buried hill reservoir based on XRD whole rock logging according to claim 1, characterized in that: The mineral elastic micro-element combination physical model includes a mineral elastic micro-element series model and a mineral elastic micro-element parallel model; The load and deformation relationship of the mineral elastic microelement series model is: F z =F 1z =F 2z =…=F nz ΔL z =ΔL1+ΔL2+…+ΔL n The load and deformation relationship of the mineral elastic microelement parallel model is: F r =F 1r +F 2r +…+F nr ΔL=ΔL1=ΔL2=…=ΔL n 。 3. The method for predicting fracture aperture coefficient of buried hill reservoir based on XRD whole rock logging according to claim 1, characterized in that: The constitutive equation and elastic parameters of the mineral elastic microelement series model are characterized as follows: Constitutive equation of mineral elastic microelement series model Elastic modulus of mineral elastic microelement series model Poisson's ratio of mineral elastic microelement series model 4. The method for predicting fracture aperture coefficient of buried hill reservoir based on XRD whole rock logging according to claim 1, characterized in that: The constitutive equation and elastic parameters of the mineral elastic microelement parallel model are characterized as follows: Constitutive equation of mineral elastic microelement parallel model Elastic modulus of mineral elastic microelement parallel model Poisson's ratio of mineral elastic microelement parallel model 5. The method for predicting fracture aperture coefficient of buried hill reservoir based on XRD whole rock logging according to claim 1, characterized in that: The mathematical and physical equations of the matrix rock elastic modulus and Poisson's ratio are as follows:

6. The method for predicting fracture aperture coefficient of buried hill reservoir based on XRD whole rock logging according to claim 1, characterized in that: The elastic modulus and Poisson's ratio of the crack opening coefficient are expressed as follows: Where: F w is the crack opening coefficient.

7. A device based on the method for predicting fracture aperture coefficient of buried hill reservoir based on XRD whole rock logging according to claim 1, characterized in that: It includes a rock cuttings collection device, a rock cuttings cleaning device, a rock cuttings drying device, a rock cuttings grinding device, a portable XRD diffractometer, a matrix rock mineral elastic microelement simulator, a matrix rock elastic parameter calculation device, a fracture opening coefficient calculation device, an interpretation mapping device and a long map printing device.

8. The device for predicting fracture aperture coefficient of buried hill reservoir based on XRD whole rock logging according to claim 7, characterized in that: The workflow is as follows: The rock cuttings collection device is placed below the sand outlet of the vibrating screen, and the rock cuttings fall into the sampler along the inclined surface of the screen cloth; fresh rock cuttings are selected and placed in the rock cuttings cleaning device, and the rock cuttings are cleaned while being fully stirred until the rock cuttings reveal their original color; the cleaned rock cuttings are placed in the rock cuttings drying device, and dried under an environment where the temperature is controlled to be less than 85°C, and the dried rock cuttings are placed in the rock cuttings grinding device for grinding to make the rock cuttings into powder with a particle size of less than 20μm; the ground rock cuttings powder is placed in a portable XRD diffractometer, and its X-ray diffraction spectrum is tested to interpret the mineral type and content data of the rock matrix of different depth formations; the mineral type and content data of the rock matrix are transmitted to the matrix rock mineral elastic microelement simulator, and the matrix rock mineral elastic microelement simulator constructs mineral elastic microelement according to the mineral type and content, and performs series and parallel combination of mineral elastic microelement, and calculates the elastic parameter E under the series and parallel combination. z ,μ z ,E r ,μ r ; The calculated elastic parameter E z ,μ z ,E r ,μ r Transmitted to the matrix rock elastic parameter calculation device to calculate the matrix rock elastic parameter E A and μ A ; The matrix rock elastic parameter E A and μ A Transmitted to the crack opening coefficient calculation device to calculate the crack opening coefficient F w ; The matrix rock elastic parameter E calculated by the matrix rock elastic parameter calculation device and the fracture opening coefficient calculation device A and μ A and crack opening coefficient F w The data are transmitted and stored in the interpretation and mapping device for mapping and real-time prediction of reservoir fracture development; finally, the long-map printing device is used to print and archive the data.