A method for preparing fracture-pore cores and saturated oil experiments in ultra-low permeability tight reservoirs

Through interspersed saturated oil method and seam-making technology, the cracks and oil saturation problems of ultra-low permeability dense reservoir cores are solved, and the stability and saturation of the core are achieved, providing a more realistic simulation for oil field development. Experimental conditions.

CN114778245BActive Publication Date: 2024-11-15SOUTHWEST PETROLEUM UNIV

Patent Information

Application Number
CN202210406150.7
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2022-04-18
Publication Date
2024-11-15
Estimated Expiration
2042-04-18

AI Technical Summary

Technical Problem

The prior art is difficult to achieve sufficient crack-making and oil saturation in the core of ultra-low permeability dense reservoirs, especially in the problems of easy damage to the core and poor saturation of the matrix, which makes it difficult to accurately carry out experiments in simulated oil field development.

Method used

The method of interspersed saturated oil is used to clean, dry, vacuum saturate, seam and re-saturation of the core through the intermediate container and core holder, combined with high-temperature drying gun and seam-making equipment, to ensure the liquid phase permeability of the core. and crude oil saturation, using tetrafluoroethylene wrapping and extrusion technology to control crack formation and oil filling.

Benefits of technology

The core of the ultra-low permeability compact reservoir was fully saturated, ensuring the core stability and saturation accuracy in the experiment, providing a simulated experimental environment that is more in line with the real formation conditions, and avoiding core falloff and partial matrix unsaturation. The problem.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN114778245B_ABST
    Figure CN114778245B_ABST
Patent Text Reader

Abstract

The present invention relates to a method for preparing a fracture-pore type core of an ultra-low permeability tight reservoir and an experimental method for saturating the core with oil, which comprises the following steps: (1) selecting a suitable ultra-low permeability tight reservoir core and performing axial and circumferential treatment; (2) cleaning and drying the core; (3) placing the core in an intermediate clamp for vacuuming and saturation; (4) wrapping the saturated core with tetrafluoroethylene heated by a high-temperature drying gun, and performing slit making by a slit making device; (5) re-saturating the core obtained by passing it through a core clamp again, and obtaining its liquid phase permeability; (6) obtaining matrix saturation and oil saturation according to a provided calculation formula. The present invention solves the difficulty that the matrix part of a fracture-type ultra-low permeability tight reservoir core cannot be fully saturated with oil after slit making, and provides a more accurate oil saturation method and an oil saturation calculation formula of the method for the development of fracture-type conglomerate oil fields.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the field of oil and gas field development, and in particular relates to a method for preparing a fracture-pore type core of an ultra-low permeability tight reservoir and a saturated oil experiment. Background Art

[0002] Core fracture creation and oil saturation are one of the important links in the current simulation of reservoir displacement experiments in petroleum development research laboratories. Conventional oil fields are all dual media with fractures and pores. At the same time, during the process of taking core samples on site, the cores obtained basically only contain one medium characteristic. Therefore, it is necessary to perform certain fracture creation treatment on the matrix core to achieve the dual medium characteristics of fractures and pores, so that the treated cores have the formation characteristics of simulated oil field development. Conventional fracture core preparation is divided into mixture preparation and fracture creation of matrix core using fracture creation tools. The core can reach the target permeability through fracture creation; conventional saturated oil is saturated in the core holder by displacement pump to obtain the required saturation. In order to better simulate the actual environment of the reservoir, it is necessary to use fracture creation tools to create fractures on the matrix core, and at the same time, it is necessary to fully saturate the core matrix with oil during the saturation stage. Due to the fragile texture of the core of the ultra-low permeability tight reservoir, it is difficult to control the fracture creation of the core of the ultra-low permeability tight reservoir and it is difficult to achieve full oil saturation after fracture creation. It is necessary to find a method that can control the fracture creation of the core of the ultra-low permeability tight reservoir and fully saturate it with oil.

[0003] The invention patent "A method and device for saturating cores with oil" (CN202010702028.5) mainly provides a method for saturating cores with oil, but does not take into account the influence of fractures on saturation during the core saturation process; the invention patent "A device and method for saturating dense cores with oil in sandstone" (CN201910906032.0) provides an oil saturation method that only takes into account the saturation of ultra-low permeability cores, but does not consider whether this oil saturation method can continue to be used after the matrix core is formed. The saturation methods selected in the above inventions are displacement saturation and intermediate container saturation, but none of them consider whether the saturation method is applicable after the formation of the formation, whether it can still effectively saturate the matrix part of the ultra-low permeability core under the influence of the fracture, and after investigation, no effective saturation method after the formation of ultra-low permeability cores was found, which cannot solve the problem of saturation of the matrix part of the ultra-low permeability core containing fractures. Therefore, a new saturation method and formation method are needed to solve the problem of saturation preparation of ultra-low permeability cores containing fractures. Summary of the invention

[0004] The purpose of the present invention is to provide a method for preparing fracture-pore type cores of ultra-low permeability tight reservoirs and conducting saturated oil experiments. The method has reliable principles and is easy to operate. It can fully saturate the ultra-low permeability tight reservoir cores after fracture creation, and provide cores that are more in line with real formation saturation conditions for indoor simulation experiments on the development of ultra-low permeability oil fields containing fractured conglomerate.

[0005] In order to achieve the above technical objectives, the present invention adopts the following technical solutions.

[0006] The present invention utilizes relevant equipment in the oil development industry, combines actual core fracture creation needs and conventional methods of saturated oil, introduces the concept of interspersing saturated oil during the saturation process, and achieves the need for fully saturating fractured extra-low permeability tight reservoir cores by utilizing intermediate containers and core clamps, thereby solving the problem that the core matrix portion of fractured extra-low permeability tight reservoir cores is not fully saturated with oil after fracture creation, thereby providing a more accurate method of saturating oil for the development of oil fields containing fractured extra-low permeability tight reservoirs.

[0007] A method for preparing fracture-pore cores of ultra-low permeability tight reservoirs and conducting oil saturation experiments comprises the following steps in sequence:

[0008] (1) Select appropriate ultra-low permeability tight reservoir cores;

[0009] (2) cleaning and drying the core obtained in step (1);

[0010] (3) vacuumizing the cleaned and dried core and then saturating it with crude oil;

[0011] (4) heating the surface of the core wrapped with tetrafluoroethylene by a high-temperature drying gun, and then creating seams in the core by a seam-making device;

[0012] (5) The core after fracture creation is saturated with crude oil again to obtain its liquid permeability and crude oil saturation.

[0013] The process of step (1) is as follows: the selected ultra-low permeability tight reservoir core is axially and circumferentially processed to obtain a cylindrical core with a length of L and a diameter of D.

[0014] The process of step (2) is as follows: placing the core in an intermediate container containing petroleum ether, pressurizing it to 10 MPa higher than the formation pressure, and replacing the petroleum ether in the intermediate container after standing for several hours until the petroleum ether no longer changes color; then placing the core in a high-temperature oven, drying out all the petroleum ether and bound water in the core at 100°C, weighing the core every 2 hours until the core mass no longer changes, and recording the core mass at this time as M1.

[0015] The process of step (3) is as follows: the core is placed in a saturated intermediate container, the saturated intermediate container is connected to the crude oil intermediate container, the saturated intermediate container and the crude oil intermediate container are both connected to a constant pressure displacement pump through a valve, firstly, the saturated intermediate container is evacuated to a negative pressure of 0.1 MPa for several hours by a vacuum pump, and then the crude oil intermediate container is provided with a pressure of 10 MPa by the constant pressure displacement pump, and then the valve between the crude oil intermediate container and the saturated intermediate container is opened, and when the pressure displayed by the constant pressure displacement pump is 0, the constant pressure displacement pump is started again to make the pressure in the saturated intermediate container reach 10 MPa higher than the formation pressure, and finally, the valves between the constant pressure displacement pump and the crude oil intermediate container, and between the crude oil intermediate container and the saturated intermediate container are closed, and the connecting valve between the constant pressure displacement pump and the saturated intermediate container is opened, and pressure is provided to the saturated intermediate container at a constant pressure under this pressure. After continuous saturation for 48 hours, the core is taken out and weighed, and the mass of the core at this time is recorded as M2.

[0016] The process of step (4) is as follows: tetrafluoroethylene is wrapped on the surface of the core by a high-temperature drying gun, and the core is weighed, and the core mass at this time is recorded as M3; the core is subjected to axial force to achieve tensile fracture by a seam-making device, the core is taken out, and the crude oil produced by squeezing around the core is cleaned, and the core is weighed, and the core mass at this time is recorded as M4.

[0017] The process of step (5) is as follows: placing the fractured core in a holder, the inlet end of the holder is connected to an intermediate container and a constant speed displacement pump, there is crude oil in the intermediate container, the outlet end is connected to a test tube, the middle section is connected to a confining pressure pump, the speed of the constant speed displacement pump is set to 0.05 ml / min, and the core is slowly saturated with crude oil. After the core fractures are fully saturated with crude oil, the oil flow rate is read at the test tube, and after the oil flow rate in the test tube is stable, the flow rate is recorded as Q, and the pressure gauges at both ends of the holder are read to obtain the inlet pressure and outlet pressure, respectively, which are P1 and P2. The liquid permeability of the fractured core is calculated, the core is taken out, and the core mass at this time is recorded as M5, and the crude oil saturation is calculated.

[0018] In the present invention, the liquid permeability K of the fractured core is calculated by the following formula:

[0019] k=QLμ / ΔPA×100

[0020] Where Q is the flow rate of fluid passing through the core per unit time, cm 3 / s;

[0021] L—core length, cm;

[0022] ΔP—pressure difference before and after the liquid passes through the core (P2-P1), MPa;

[0023] A—Cross-sectional area of ​​liquid passing through the core, cm 2 ;

[0024] μ—viscosity of the liquid, mPa·s;

[0025] k—liquid permeability, mD.

[0026] In the present invention, the process of calculating the crude oil saturation S is as follows:

[0027] M2-M1 is the mass of crude oil saturated with the matrix, M3-M2 is the mass of tetrafluoroethylene (rubber sleeve), M3-M4 is the mass of crude oil squeezed out during the fracture creation process, and M5-M4 is the mass of lost crude oil supplemented in the fracture. The crude oil saturation amount M is obtained as:

[0028] M=M5-M4+(M2-M1)-(M3-M4).

[0029] In the process of core matrix saturation, all saturated oil is considered to be matrix saturated oil. After the joint formation process, the oil produced by extrusion can be considered to be the oil expelled from the cracks formed by the core deformation. This part of oil is formed when the matrix core becomes a fractured core and part of the matrix oil is expelled from the core volume. Therefore, the matrix oil content is M2-M1-(M3-M4). At the same time, in the fracture saturated oil, because the fracture channel is large and easy for fluid to flow, it is easy to fill the core fracture space, and the fracture space accounts for a small proportion of the total matrix space, so the fracture saturation can be considered to be 100%. At this time, all the saturated oil is fracture oil, so the fracture oil content is M5-M4.

[0030] The saturation of each part can be obtained by the following calculation formula:

[0031] Matrix oil saturation S1:

[0032]

[0033] Crude oil saturation S:

[0034]

[0035] Where ρ is crude oil density, g / cm 3 ;

[0036] φ—core porosity, %;

[0037] D—core diameter, cm;

[0038] M—crude oil saturation, g;

[0039] S, S1—crude oil saturation, matrix oil saturation, %.

[0040] Compared with the prior art, the present invention has the following beneficial effects:

[0041] The present invention solves the problem that when cores of ultra-low permeability tight reservoirs are made, cores are easily damaged, resulting in partial detachment of the cores and making it impossible to conduct experiments, and provides a reliable method for making seams for such fragile ultra-low permeability cores. At the same time, a novel saturation method is proposed to solve the problem that the matrix part is not easy to saturate when the ultra-low permeability cores are saturated.

[0042] The invention solves the problems of difficulty in making cores of such cores and difficulty in fully saturating them with oil, prevents the cores of ultra-low permeability reservoirs from falling off during the making process, and ensures the accuracy of calculating the oil saturation of fractured ultra-low permeability tight reservoir cores. BRIEF DESCRIPTION OF THE DRAWINGS

[0043] Figure 1 This is a schematic diagram of core fractures saturated with crude oil.

[0044] Figure 2 Schematic diagram of core matrix saturated with crude oil.

[0045] In the figure: 1. constant speed displacement pump; 2. intermediate container; 3. three-way valve; 4. inlet pressure gauge; 5. outlet pressure gauge; 6. constant pressure pump; 7. core holder; 8. test tube; 9. crude oil intermediate container; 10. saturated intermediate container; 11. core; 12. vacuum pump; 13. constant pressure displacement pump; 901 / 902 / 903 / 904, switch. DETAILED DESCRIPTION

[0046] The present invention is further described below with reference to the accompanying drawings and examples, so that those skilled in the art can understand the present invention. However, it should be clear that the present invention is not limited to the scope of the specific embodiments, and for those skilled in the art, as long as various changes are within the spirit and scope of the present invention defined and determined by the attached claims, they are all protected.

[0047] A method for preparing fracture-pore cores of ultra-low permeability tight reservoirs and conducting oil saturation experiments, comprising the following steps in sequence;

[0048] (1) The core is processed to remove the edge material to obtain a cylindrical core with a length of L = 4.757 cm and a diameter of D = 2.564 cm;

[0049] (2) Place the core in an intermediate container containing petroleum ether and pressurize it to 10 MPa higher than the formation pressure. After standing for 12 hours, replace the petroleum ether in the intermediate container. When the petroleum ether no longer changes color, the core cleaning is complete. Place the cleaned core in a high-temperature oven to dry out all the petroleum ether and bound water in the core. After drying at 100°C for 12 hours, weigh the core and then take it out and weigh it every 2 hours. When the core mass no longer changes, record the core mass as M1 = 60.6709 g;

[0050] (3) Saturate the core matrix with crude oil (see Figure 2 ): Place the core 11 in the saturated intermediate container 10, turn on switch 903, and use the vacuum pump 12 to pump the intermediate container 10 to a negative pressure of 0.1 MPa for 5 hours, then turn off the vacuum pump 12 and switch 903; after the crude oil intermediate container 9 is filled with crude oil, turn on switch 902, and use the displacement pump 13 to provide a certain pressure of 10 MPa to the intermediate container, then turn on switches 901 and 903, and when the displacement pump 13 displays a pressure of 0 MPa, start the displacement pump 13 again to make the pressure in the intermediate container 10 higher than the formation pressure by 10 MPa, then turn off switches 901, 903, and 902, turn on switch 904 and provide pressure to the intermediate container 10 at a constant pressure at this numerical pressure, and continue saturation for 48 hours, take out the core and weigh it, and record the core mass as M2=61.8624g;

[0051] (4) The core is tightly wrapped with tetrafluoroethylene, a specific material, at high temperature, and the weight of the completely wrapped core is recorded as M3 = 63.7739 g; the axial force of the core is controlled by the seam-making equipment to reach tensile fracture, the core is taken out and the crude oil produced by squeezing around the core is cleaned, and the core is weighed and recorded as M4 = 63.7702 g;

[0052] (5) Saturate the core fractures with crude oil (see Figure 1 ): Place the core in the core holder 7, and connect the displacement pump 1, the intermediate container 2, the core holder 7, and the test tube 8 in sequence through the pipeline. The intermediate container 2 is filled with crude oil. Set the speed of the displacement pump 1 to 0.05 ml / min, slowly saturate the core with crude oil, and read the oil flow rate at the test tube 8 after the core fractures are fully saturated with oil. After the oil flow rate in the test tube is stable, read the pressures P1=0.14827 MPa and P2=0.1 MPa at the core inlet pressure gauge 4 and outlet pressure gauge 5 respectively. According to the Darcy formula k=QLμ / ΔPA×100 (the viscosity of crude oil is μ=0.848 mPa·s), the permeability of the fractured core is calculated to be 1.4853 mD. Take out the core and record the core mass M5=63.9201 g; M2-M1 is the matrix saturated oil mass. It is known that the crude oil density ρ=0.69 g / cm 3 , core porosity φ = 8.91, M3-M2 is the weight of the rubber sleeve, M4-M3 is the mass of crude oil squeezed out during the fracture creation process, M5-M4 is the mass of lost crude oil supplemented in the large fractures, and the crude oil saturation is M = M5-M4 + (M2-M1) - (M3-M4) = 1.3451g, which can be obtained according to the following calculation formula:

[0053] Matrix oil saturation S1:

[0054]

[0055] Crude oil saturation S:

[0056]

[0057] Through practical verification, the crude oil saturation of the core, the oil saturation of the matrix and the permeability after fracture creation all meet the experimental requirements.

Claims

1. A method for preparing a fracture-pore core of an ultra-low permeability tight reservoir and conducting an oil saturation experiment, comprising the following steps in sequence: (1) Selecting a suitable ultra-low permeability tight reservoir core; (2) Cleaning and drying the core obtained in step (1); (3) Vacuuming the cleaned and dried core and then saturating it with crude oil; (4) Heating the surface of the core wrapped in tetrafluoroethylene by a high-temperature drying gun, and then slit the core by a slit-making device; (5) Saturating the slit-made core with crude oil again to obtain its liquid permeability and crude oil saturation; The process of step (1) is as follows: axially and circumferentially process the selected ultra-low permeability tight reservoir core to obtain a cylindrical core with a length of L and a diameter of D; The process of step (2) is as follows: placing the core in an intermediate container containing petroleum ether, pressurizing it to 10 MPa higher than the formation pressure, and replacing the petroleum ether in the intermediate container after standing for several hours until the petroleum ether no longer changes color; then placing the core in a high-temperature oven, drying out all the petroleum ether and bound water in the core at 100°C, weighing the core every 2 hours until the core mass no longer changes, and recording the core mass at this time as M1; The process of step (3) is as follows: placing the core in a saturated intermediate container, the saturated intermediate container is connected to the crude oil intermediate container, the saturated intermediate container and the crude oil intermediate container are both connected to a constant pressure displacement pump through a valve, firstly, the saturated intermediate container is evacuated to a negative pressure of 0.1 MPa for several hours by a vacuum pump, and then the constant pressure displacement pump is used to provide a pressure of 10 MPa to the crude oil intermediate container, and then the valve between the crude oil intermediate container and the saturated intermediate container is opened, and when the pressure displayed by the constant pressure displacement pump is 0, the constant pressure displacement pump is started again to make the pressure in the saturated intermediate container reach 10 MPa higher than the formation pressure, and finally, the valves between the constant pressure displacement pump and the crude oil intermediate container, and between the crude oil intermediate container and the saturated intermediate container are closed, and the connecting valve between the constant pressure displacement pump and the saturated intermediate container is opened, and pressure is provided to the saturated intermediate container at a constant pressure under this pressure, and after saturation for 48 hours, the core is taken out and weighed, and the mass of the core at this time is recorded as M2; The process of step (4) is as follows: wrapping tetrafluoroethylene on the surface of the core by a high-temperature drying gun, weighing it, and recording the mass of the core at this time as M3; subjecting the core to axial force to tensile fracture by a seam-making device, taking out the core, and cleaning the crude oil produced by squeezing around the core, and weighing the core, and recording the mass of the core at this time as M4; The process of step (5) is as follows: placing the fractured core in a holder, the inlet end of the holder is connected to an intermediate container and a constant speed displacement pump, there is crude oil in the intermediate container, the outlet end is connected to a test tube, the middle section is connected to a confining pressure pump, the speed of the constant speed displacement pump is set to 0.05 ml / min, and the core is slowly saturated with crude oil. After the core fractures are fully saturated with crude oil, the oil flow rate is read at the test tube, and after the oil flow rate in the test tube is stable, the flow rate is recorded as Q, and the pressure gauges at both ends of the holder are read to obtain the inlet pressure and outlet pressure, respectively, P1 and P2, and the liquid permeability of the fractured core is calculated, the core is taken out, and the core mass at this time is recorded as M5, and the crude oil saturation is calculated; The liquid permeability k of the fractured core is calculated by the following formula: k=QLμ / ΔPA×100 Where, Q is the flow rate of fluid passing through the core per unit time, cm3 / s; L—core length, cm; ΔP—pressure difference before and after the liquid passes through the core (P2-P1), MPa; A—cross-sectional area of ​​liquid passing through the core, cm2; μ—viscosity of the liquid, mPa·s; k—liquid permeability, mD; The process of calculating crude oil saturation S is as follows: M2-M1 is the mass of crude oil saturated with the matrix, M3-M2 is the mass of the tetrafluoroethylene rubber sleeve, M3-M4 is the mass of crude oil squeezed out during the fracture creation process, and M5-M4 is the mass of lost crude oil supplemented in the fracture. The crude oil saturation amount M is obtained as: M=M5-M4+(M2-M1)-(M3-M4) Based on the fact that in the process of core matrix saturation, all saturated oil is considered to be matrix saturated oil. After the formation process, the oil produced by extrusion is considered to be the oil expelled from the cracks formed by the core deformation. This part of oil is formed by the matrix core becoming a fracture core and part of the matrix oil is expelled from the core volume. Therefore, the matrix oil content is M2-M1-(M3-M4); at the same time, in the fracture saturated oil, because the fracture channel is large and easy for fluid flow, it is easy to fill the core fracture space, and the fracture space accounts for a small proportion of the total matrix space, so the fracture saturation is considered to be 100%. At this time, all the saturated oil is fracture oil, so the fracture oil content is M5-M4; The saturation of each part, matrix oil saturation S1, is obtained by the following calculation formula: Crude oil saturation S: Where, ρ—density of crude oil, g / cm3; φ—core porosity, %; D—core diameter, cm; M—crude oil saturation, g; S, S1—crude oil saturation, matrix oil saturation, %.

Citation Information

Patent Citations

  • Device and method for measuring gasometry permeability of rock under high pressure

    CN102455277A

  • Method for processing double-media core and application of double-media core

    CN102809522A

  • Experimental method for evaluating adaptability of plugging agent in low permeability crack rock core

    CN104196487A

  • Hypotonic fractured reservoir imbibition oil-extraction experimental method

    CN104655808A

  • Physical simulation method for enabling water injection induced micro-fracture extension law to reappear under formation conditions

    CN107741390A

Cited By

  • Shale core nano-pore gas-phase saturated oil experimental device and experimental method thereof