A method for optimizing the division of hot-dip galvanized finished coils

By introducing the coil setting calculation process in the hot-dip galvanized production line, combining welding and shear information, the strip coil length is optimized, and the problem of uneven coil separation is solved, and the coil separation accuracy and compliance rate of finished coil weight is improved. .

CN114955691BActive Publication Date: 2024-12-03GANSU JIU STEEL GRP HONGXING IRON & STEEL CO LTD
View PDF 3 Cites 0 Cited by

Patent Information

Application Number
CN202210362312.1
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2022-04-08
Publication Date
2024-12-03
Estimated Expiration
2042-04-08

AI Technical Summary

Technical Problem

During the process of decoding the finished coil of hot-dip galvanized steel strip, the scrap cutting and elongation of the strip steel during the production process was not considered, resulting in uneven coil division, resulting in the weight of the finished coil not meeting the requirements, reducing the roll weight compliance rate, and increasing the Difficulty of outbound and inventory.

Method used

By triggering the calculation process of the coil setting in the basic automation system, combining welding and shear information, the formula is used to calculate the shear length of the strip coil, considering the cutting loss and elongation of the galvanized line, and selecting the appropriate coil mode ( length shear or weld shear) to optimize the rolling settings and improve the rolling accuracy.

Benefits of technology

The accuracy of the coil division is improved, especially for thick strip steel, which eliminates the situation where the weight deviation reaches 200Kg or even more than 300Kg, and achieves more accurate coil division control, which improves the coil weight compliance rate of the finished coil.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure BDA0003585758620000021
    Figure BDA0003585758620000021
  • Figure BDA0003585758620000041
    Figure BDA0003585758620000041
  • Figure BDA0003585758620000051
    Figure BDA0003585758620000051
Patent Text Reader

Abstract

The present invention discloses a method for optimizing the splitting of hot-dip galvanized finished coils, including triggering of a splitting setting calculation process, determination of a splitting mode, determination of a splitting mode optimization scheme for length shearing, calculation of the strip splitting shearing length, generation of weld shearing information to perform weld shearing operations or splitting length shearing operations. The present invention adds a splitting shearing optimization setting calculation process to the strip splitting setting. When performing the splitting shearing setting of the finished coils, by determining the actual welding performance and shearing performance of the strip in the production line, the calculation of the head and tail strip sampling, scrap cutting, skin pass machine elongation, and straightening machine elongation is comprehensively considered, thereby obtaining the strip length used for the splitting optimization setting.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the technical field of hot-dip galvanizing production control, and in particular relates to a hot-dip galvanizing finished product coil division optimization method. Background Art

[0002] Hot-dip galvanizing production is to immerse the cleaned and annealed strip steel into molten zinc liquid so that the strip steel surface adheres to a zinc layer, thereby achieving the purpose of corrosion protection. The head of the hot-dip galvanizing production line opens the strip steel of the raw material coil through the unwinder, and welds the strip steel of the raw material coil into one piece through the welding machine for production. After the strip steel at the exit of the production line has completed a series of production processes such as hot-dip galvanizing, skin-passing, straightening, and passivation film coating, it needs to be divided into coils at the exit shear according to the requirements of the contract and loading, and finally the finished coil is coiled by the coiler, thus completing the production of galvanized finished steel coils.

[0003] Usually, when finished coils are divided into fixed lengths, the process conditions such as waste cutting and elongation of the strip during the production process are not taken into consideration. The requirements for the division of the finished coils are simply met. This may cause unreasonable settings for the division of the strip, and the weight of the finished coils divided may not meet the requirements, thereby reducing the weight compliance rate of the finished coils. Summary of the invention

[0004] The purpose of the present invention is to provide a method for optimizing the splitting of hot-dip galvanized finished coils, so as to solve the problem of uneven splitting in the existing galvanized steel strip continuous production line, improve the rate of product coil weight compliance, and reduce the difficulty of vehicle allocation and product inventory requirements when the products are shipped out.

[0005] In order to achieve the above object, the technical solution adopted by the present invention is:

[0006] A method for optimizing the division of hot-dip galvanized finished coils, comprising the following steps:

[0007] S1. Triggering of the volume setting calculation process:

[0008] The setting calculation process is triggered by the basic automation system. When the basic automation system sends the strip exit shearing information or the entrance welding information to the process control system, the roll setting process is triggered.

[0009] S2. Determination of volume splitting mode:

[0010] Before the splitting operation, the process control system determines whether to execute the weld shearing splitting mode:

[0011] If the remaining steel coil length is less than the set minimum product length, the weld shearing and splitting mode is executed and S4-1 is entered;

[0012] If the roll division information of the previous finished roll received from the basic automation system is in manual roll division mode, the weld shearing roll division mode is executed and S4-1 is entered;

[0013] If the final volume weight is less than the finished product order weight, the weld shearing volume mode is executed and the process goes to S4-1; otherwise, the length shearing volume mode is executed and the process goes to S3;

[0014] S3, used for determining the optimization scheme of length shearing and coiling mode and calculating the shearing length of strip coiling:

[0015] If the process control system receives a signal from the basic automation system that the tail welding is completed, the formula (1) is used to calculate the shear length of the strip:

[0016]

[0017] Where: Length—the calculated length of the strip sheared;

[0018] Weight—weight of raw steel coil;

[0019] Width—Width of raw material strip;

[0020] Thickness—thickness of raw strip steel;

[0021] Density—density of raw strip steel;

[0022] Length crop —Length of the head and tail plate of the raw strip;

[0023] α—Proportional coefficient between actual strip length and coiling length;

[0024] ε—the sum of the elongation of the skin pass machine and the tension leveler;

[0025] Count—the planned number of rolls of the raw material roll;

[0026] If the strip tail welding completion signal is not received, the strip steel coil shear length is calculated using formula (2);

[0027] If the process control system searches the shear information table at the same time, when the shear information table contains the shear information of the coil, the formula (2) is also used to calculate the shear length of the strip coil:

[0028] Length = {L4 × (α + ε) - Length crop}÷Count (2)

[0029] Where: Length—the calculated length of the strip sheared;

[0030] Length crop —Length of the head and tail plate of the raw strip;

[0031] Count—the planned number of rolls of the raw material roll;

[0032] L4—unwinding length of raw material roll;

[0033] S4-1, generating weld shearing information and executing weld shearing operation;

[0034] S4-2, perform the roll length cutting operation:

[0035] The process control system sends the cut length value calculated by S3 optimization to the basic automation system, and controls the exit shear to perform the cut operation.

[0036] Compared with the prior art, the present invention has the following beneficial effects:

[0037] The present invention adds a calculation process for optimizing the setting of coil shearing in the setting of coiling of strip steel. When setting the coil shearing of finished coils, the strip steel welding performance and shearing performance in the production line are determined, and the calculation of the sampling of the head and tail strip steel, the scrap cutting, the elongation of the skin pass mill, and the elongation of the straightening machine are comprehensively considered, so as to obtain the strip steel length for optimizing the setting of coiling.

[0038] The calculation formula (1) of the present invention for the optimization scheme of the length shearing and coiling mode takes into account the cutting loss and elongation of the galvanizing line, thereby improving the accuracy of coiling, especially for thick strip steel that is sensitive to cutting loss. The coiling accuracy is high, eliminating the situation where the early deviation reaches 200 kg or even 300 kg or more; the calculation formula (2) for the optimization scheme of the length shearing and coiling mode is aimed at the characteristics that the thick specification strip steel is short in length and the tail of the strip is welded before coiling, that is, the uncoiling length measured by the entrance of the galvanizing line, that is, the length of the mother coil of the raw material on the line (the cutting loss at the entrance has been removed) is used for coiling control. DETAILED DESCRIPTION

[0039] The present invention will be further described below in conjunction with specific implementation modes.

[0040] A method for optimizing the division of hot-dip galvanized finished coils, comprising the following steps:

[0041] S1. Triggering of the calculation process of volume setting:

[0042] The setting calculation process is triggered by the basic automation system. When the basic automation system sends the strip exit shearing information or the entrance welding information to the process control system, the roll setting process is triggered.

[0043] S2. Determination of volume splitting mode:

[0044] Before the splitting operation, the process control system determines whether to execute the weld shearing splitting mode:

[0045] If the remaining steel coil length is less than the set minimum product length, the weld shearing and splitting mode is executed and S4-1 is entered;

[0046] If the roll division information of the previous finished roll received from the basic automation system is in manual roll division mode, the weld shearing roll division mode is executed and S4-1 is entered;

[0047] If the final volume weight is less than the finished product order weight, the weld shearing volume mode is executed and the process goes to S4-1; otherwise, the length shearing volume mode is executed and the process goes to S3;

[0048] S3, used for determining the optimization scheme of length shearing and coiling mode and calculating the shearing length of strip coiling:

[0049] The galvanizing line relies on the length calculated by the online tracking system to control the steel coils. In order to achieve the control target and maximize the control accuracy, accurate raw material coil length information is necessary. At present, there are five sources of direct and indirect raw material coil length information:

[0050] The length of the raw material coil in the PDI data is L1; the length L2 calculated by converting the diameter of the steel coil measured at the entrance of the galvanizing line; the length L3 calculated by the weight, length and width specifications of the raw material coil in the PDI data; the unwinding length of the strip steel is L4; the coiling length of the strip steel is L5;

[0051] Through production practice, the raw material roll length L1 brought by PDI data is not as accurate as L3 calculated according to weight specifications;

[0052] The length L2 calculated by converting the steel coil diameter measured at the entrance of the galvanizing line depends on the inner and outer diameters and thickness of the raw material;

[0053] The unwinding length L4 measured by the 1# tensioning roller encoder at the entrance of the galvanizing line;

[0054] L5 is the curling length of the product after it comes off the production line, including the extension of the strip during the production process (including annealing furnace, skin pass, and tension leveling) (L b ), cannot be obtained when planning the volume division, and can only be used for data analysis to determine parameters;

[0055] In addition, the following factors that change the strip length on the production line should also be considered when splitting in order to obtain more accurate splitting results:

[0056] Cutting head and tail of imported raw material rolls (L a ); Cutting and sampling when exporting rolls (L c );

[0057] If the process control system receives a signal from the basic automation system that the tail welding is completed, the formula (1) is used to calculate the shear length of the strip:

[0058]

[0059] Where: Length—the calculated length of the strip sheared;

[0060] Weight—weight of raw steel coil;

[0061] Width—Width of raw material strip;

[0062] Thickness—thickness of raw strip steel;

[0063] Density—density of raw strip steel;

[0064] Length crop —Length of the head and tail plate of the raw strip;

[0065] α—Proportional coefficient between actual strip length and coiling length;

[0066] ε—the sum of the elongation of the skin pass machine and the tension leveler;

[0067] Count—the planned number of rolls of the raw material roll;

[0068] The ratio coefficient between the actual strip length L3 and the strip coiling length L5:

[0069]

[0070] Galvanized wire cutting length:

[0071] Length crop =L a +L c

[0072] This solution takes into account the cutting loss and elongation of the galvanizing line, and improves the accuracy of coiling, especially for thick strip steel that is sensitive to cutting loss. The coiling accuracy is greatly improved, eliminating the situation where the early deviation reaches 200 kg or even 300 kg.

[0073] In view of the fact that the thick strip is short and the tail of the strip has been welded before coiling, a supplementary solution for coiling control is proposed, that is, the uncoiling length L4 measured by the 1# tensioning roller encoder at the entrance of the galvanizing line, that is, the length of the parent coil on the raw material line (the length of the cut loss at the entrance has been removed) is used for coiling control;

[0074] If the strip tail welding completion signal is not received, the strip steel coil shear length is calculated using formula (2);

[0075] If the process control system searches the shear information table at the same time, when the shear information table contains the shear information of the coil, the formula (2) is also used to calculate the shear length of the strip coil:

[0076] Length = {L4 × (α + ε) - Length crop}÷Count (2)

[0077] Where: Length—the calculated length of the strip sheared;

[0078] Length crop —Length of the head and tail plate of the raw strip;

[0079] Count—the planned number of rolls of the raw material roll;

[0080] L4—unwinding length of raw material roll;

[0081] The unwinding length L4 measured by the 1# tensioning roller encoder at the entrance of the galvanizing line is the accurate data after removing the entrance cutting loss. There is no need to calculate the entrance cutting loss, and thus there is no corresponding error. The unwinding length L4 does not need to be calculated by weight and strip steel specification data, eliminating the impact of inaccurate strip steel specification data on coiling. It is particularly effective for thick strip steel coiling.

[0082] S4-1, generating weld shearing information and executing weld shearing operation;

[0083] S4-2, perform the roll length cutting operation:

[0084] The process control system sends the cut length value calculated by S3 optimization to the basic automation system, and controls the exit shear to perform the cut operation.

[0085] Taking a domestic hot-dip galvanizing production line as an example, the following describes in detail the coil parameter setting and calculation process.

[0086] The galvanizing line relies on the length calculated by the online tracking system to control the steel coils. In order to achieve the control target and maximize the control accuracy, accurate information on the length of the raw material coil is necessary.

[0087] Galvanizing line coil control optimization plan:

[0088] When the MES system (hereinafter referred to as Level 3) issues a production plan, it will bring out the requirements for sub-rolls in the PDI data. The weight of sub-rolls in the PDI is for the raw material rolls, not the weight of the finished product rolls. For example, if the raw material mother roll weighs 21001 kg and is divided into three rolls, then the roll weight issued by Level 3 is 7000 kg for sub-roll A, 7000 kg for sub-roll B, and 7001 kg for roll C (21001-21001 / 3-21001 / 3). In other words, the sub-roll weight requirements given by Level 3 do not take into account the zinc layer thickness and the galvanizing line cutting loss.

[0089] Since the PDI data issued by the third level gives the weight requirements, the weight cannot be directly controlled when the galvanizing line is split. In order to achieve the goal of split weight control, the weight data of the raw material roll must be converted into strip length data, and the weight control purpose can be achieved by controlling the strip length of the split roll. The calculation formula for converting weight to length is as follows:

[0090]

[0091] Where: Length—the calculated length of the strip sheared;

[0092] Weight—target weight of strip coil;

[0093] Width—strip width;

[0094] Thickness—strip thickness;

[0095] Density—strip density;

[0096] If the target volume weight is Weight, the second level will send the Length calculated by the above formula to the first level for volume control.

[0097] Disadvantages and shortcomings of the original design:

[0098] The weight of the strip is measured by the previous process weighing and is an accurate value. The density of steel is a constant. In order to obtain the accurate length value of the strip, it is necessary to ensure that the specifications (width and thickness) of the strip are accurate. Through actual data analysis, under the assumption that the weight (Weight), width (Width), thickness (Thickness), and length (Length) given in the previous process PDI are accurate, the density of the steel is calculated using the PDI data. The resulting density values ​​range from a minimum of 7.826 to a maximum of 7.925t / m3, as shown in the following table:

[0099]

[0100] From the above analysis data, we can see that the data given by the previous process is not accurate. In the case of the actual measured weight, the most likely reason is that the raw material strip steel specification information is inaccurate. From the exact raw material coil specification data, we also know that the nominal width is narrower than the actual value, and the thickness may be thick or thin. Each batch is different, which has a great impact on the weight control of the galvanized line. In addition, since the annealing and skin straightening processes of the galvanized line have a certain elongation, it will affect the length of the finished strip steel. Under the control strategy of controlling the weight by length, it will also have a certain impact on the weight of the strip steel. Thirdly, the head and tail cutting at the entrance of the galvanized line, the sampling and cutting loss at the exit also have a great impact on the weight of the finished coil, especially the thick specification strip steel. Finally, when the weight deviation of the steel coil is large, the only parameter that can be adjusted is the density value of the steel coil. As can be seen from the above table, the adjustment of this parameter is not universal.

[0101] Volume control optimization solution:

[0102] Used to determine the optimal solution for length shearing and coiling mode and calculate the shearing length of strip coils:

[0103] The galvanizing line relies on the length calculated by the online tracking system to control the steel coils. In order to achieve the control target and maximize the control accuracy, accurate raw material coil length information is necessary. At present, there are five sources of direct and indirect raw material coil length information:

[0104] The length of the raw material coil in the PDI data is L1; the length L2 calculated by converting the diameter of the steel coil measured at the entrance of the galvanizing line; the length L3 calculated by the weight, length and width specifications of the raw material coil in the PDI data; the unwinding length of the strip steel is L4; the coiling length of the strip steel is L5;

[0105] Through production practice, the raw material roll length L1 brought by PDI data is not as accurate as L3 calculated according to weight specifications;

[0106] The length L2 calculated by converting the steel coil diameter measured at the entrance of the galvanizing line depends on the inner and outer diameters and thickness of the raw material;

[0107] The unwinding length L4 measured by the 1# tensioning roller encoder at the entrance of the galvanizing line;

[0108] L5 is the curling length of the product after it comes off the production line, including the extension of the strip during the production process (including annealing furnace, skin-passing, and tensioning) (L b ), cannot be obtained when planning the volume division, and can only be used for data analysis to determine parameters;

[0109] In addition, the following factors that change the strip length on the production line should also be considered when splitting in order to obtain more accurate splitting results:

[0110] Cutting head and tail of imported raw material rolls (La ); Cutting and sampling when exporting rolls (L c );

[0111] If the process control system receives a signal from the basic automation system that the tail welding is completed, the formula (1) is used to calculate the shear length of the strip:

[0112]

[0113] Where: Length—the calculated length of the strip sheared;

[0114] Weight—weight of raw steel coil;

[0115] Width—Width of raw material strip;

[0116] Thickness—thickness of raw strip steel;

[0117] Density—density of raw strip steel;

[0118] Length crop —Length of the head and tail plate of the raw strip;

[0119] α—Proportional coefficient between actual strip length and coiling length;

[0120] ε—the sum of the elongation of the skin pass machine and the tension leveler;

[0121] Count—the planned number of rolls of the raw material roll;

[0122] The ratio coefficient between the actual strip length L3 and the strip coiling length L5:

[0123]

[0124] Galvanized wire cutting length:

[0125] Length crop =L a +L c

[0126] This solution takes into account the cutting loss and elongation of the galvanizing line, and improves the accuracy of coiling, especially for thick strip steel that is sensitive to cutting loss. The coiling accuracy is greatly improved, eliminating the situation where the early deviation reaches 200 kg or even 300 kg.

[0127] In view of the fact that the thick strip is short and the tail of the strip has been welded before coiling, a supplementary solution for coiling control is proposed, that is, the uncoiling length L4 measured by the 1# tensioning roller encoder at the entrance of the galvanizing line, that is, the length of the parent coil on the raw material line (the length of the cut loss at the entrance has been removed) is used for coiling control;

[0128] If the strip tail welding completion signal is not received, the strip steel coil shear length is calculated using formula (2);

[0129] If the process control system searches the shear information table at the same time, when the shear information table contains the shear information of the coil, the formula (2) is also used to calculate the shear length of the strip coil:

[0130] Length = {L4 × (α + ε) - Length crop}÷Count (2)

[0131] Where: Length—the calculated length of the strip sheared;

[0132] Length crop —Length of the head and tail plate of the raw strip;

[0133] Count—the planned number of rolls of the raw material roll;

[0134] L4—unwinding length of raw material roll;

[0135] The unwinding length L4 measured by the 1# tensioning roller encoder at the entrance of the galvanizing line is the accurate data after removing the entrance cutting loss. There is no need to calculate the entrance cutting loss, and thus there is no corresponding error. The unwinding length L4 does not need to be calculated by weight and strip steel specification data, eliminating the impact of inaccurate strip steel specification data on coiling. It is particularly effective for thick strip steel coiling.

[0136] S4-1, generating weld shearing information and executing weld shearing operation;

[0137] S4-2, perform the roll length cutting operation:

[0138] The process control system sends the cut length value calculated by S3 optimization to the basic automation system, and controls the exit shear to perform the cut operation.

[0139] Example:

[0140]

[0141] Note: 1) The actual length of the unwinding in Example 1 is obtained after the actual splitting. The splitting length is calculated using the first calculation length of 731.4 meters, and the second calculation length of 734.3 meters is calculated after the analysis.

[0142] 2) In Example 2, the actual length of unwinding is obtained before the actual splitting of the rolls. The secondary calculated length is used to correct the primary calculated length. The actual secondary calculated length used is 335.2 meters.

[0143] After optimizing the coiling process according to this method, the weight deviation of the finished steel coils of the galvanizing line is greatly reduced, achieving the goal of precise weight control of the coils of the galvanizing line.

Claims

1. A method for optimizing the splitting of hot-dip galvanized finished coils, characterized in that The steps include: S1. Triggering of the calculation process of volume setting: The setting calculation process is triggered by the basic automation system. When the basic automation system sends the strip exit shearing information or the entrance welding information to the process control system, the roll setting process is triggered. S2. Determination of volume splitting mode: Before the splitting operation, the process control system determines whether to execute the weld shearing splitting mode: If the remaining steel coil length is less than the set minimum product length, the weld shearing and splitting mode is executed and S4-1 is entered; If the roll division information of the previous finished roll received from the basic automation system is in manual roll division mode, the weld shearing roll division mode is executed and S4-1 is entered; If the final volume weight is less than the finished product order weight, the weld shearing volume mode is executed and the process goes to S4-1; otherwise, the length shearing volume mode is executed and the process goes to S3; S3, used for determining the optimization scheme of length shearing and coiling mode and calculating the shearing length of strip coiling: If the process control system receives a signal from the basic automation system that the tail welding is completed, the formula (1) is used to calculate the shear length of the strip: Where: Length—the calculated length of the strip sheared; Weight—weight of raw steel coil; Width—Width of raw material strip; Thickness—thickness of raw strip steel; Density—density of raw strip steel; Length crop —Length of the head and tail plate of the raw strip; α—Proportional coefficient between actual strip length and coiling length; ε—the sum of the elongation of the skin pass machine and the tension leveler; Count—the planned number of rolls of the raw material roll; If the strip tail welding completion signal is not received, the strip steel coil shear length is calculated using formula (2); If the process control system searches the shear information table at the same time, when the shear information table contains the shear information of the coil, the formula (2) is also used to calculate the shear length of the strip coil: Length={L4×(α+ε)-Length crop }÷Count (2) Where: Length—the calculated length of the strip sheared; Length crop —Length of the head and tail plate of the raw strip; Count—the planned number of rolls of the raw material roll; L4—unwinding length of raw material roll; S4-1, generating weld shearing information and executing weld shearing operation; S4-2, perform the roll length cutting operation: The process control system sends the cut length value calculated by S3 optimization to the basic automation system, and controls the exit shear to perform the cut operation.

Citation Information

Patent Citations

  • Method for bundling surface quality information of band steel

    CN103512887A

  • Coiled material winding tension real-time detection and regulation system

    CN108975041A

  • Optical film layered roll and method and device for manufacturing the same

    WO2009128115A1