A graphene superconducting far-infrared electric heating film and a manufacturing method thereof

By using graphene superconducting far-infrared electric heating film structure in graphene electrothermal film, the stability of the graphene layer is ensured by using mold and extruder technology, and combining aluminum foil reflective layer and rubber warm-insulating layer, the graphene electrothermal film is solved. The problem of position change during the preparation process improves the electric heating performance and warming effect, and improves the energy-saving effect.

CN115038200BActive Publication Date: 2024-11-22HEBEI YUANFEI NEW ENERGY TECH CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202210752057.1
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2022-06-29
Publication Date
2024-11-22
Estimated Expiration
2042-06-29

AI Technical Summary

Technical Problem

During the preparation process, the existing graphene electric heating film changes the graphene position due to vibration, which affects the electric heating performance, and has poor warming performance, affecting the energy-saving effect.

Method used

The graphene superconducting far infrared electric heating film structure is adopted, including graphene heating layer, adhesive layer, intercept layer, aluminum foil reflective layer, rubber warmth layer and environmentally friendly polyester layer. The graphene placement groove and intercept metal groove are formed through the mold. Combining scraper and extruder technology ensures the stability of the graphene layer, and using aluminum foil reflective layer and rubber warm-keeping layer to improve warm-keeping performance.

Benefits of technology

The stable positioning of the graphene layer is achieved, the electric heating performance and warming effect are improved, and the energy-saving performance of the electric heating film is improved.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN115038200B_ABST
    Figure CN115038200B_ABST
Patent Text Reader

Abstract

The present invention discloses a graphene superconducting far-infrared electric heating film and a manufacturing method, which relates to the technical field of electric heating film, including a graphene heating layer, wherein the graphene heating layer is arranged at the upper end of an adhesive layer, and an interception layer is arranged at the lower end of the adhesive layer. The present invention extrude an appropriate amount of the upper end of the graphene superconducting glue by setting a mold, thereby forming a graphene placement groove at the upper end of the graphene superconducting glue, and at the same time, the lower end of the graphene superconducting glue is extruded through a mold to form an interception metal placement groove, and finally dried to a semi-solidified state, and the graphene is placed in the graphene placement groove for relative positioning and storage, and a scraper is used to push out the excess graphene to achieve the effect of stabilizing the thickness of the single-layer graphene heating layer, thereby solving the problem that the graphene electric heating film is mostly vibrated during the preparation process, causing the graphene position to change, thereby affecting the electric heating performance of the subsequent graphene electric heating film to a certain extent.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to a far-infrared electric heating film, in particular to a graphene superconducting far-infrared electric heating film and a manufacturing method thereof. Background Art

[0002] The principle of electric film heating is that under the action of the electric field, the carbon molecules in the heating element produce "Brownian motion", and violent friction and collision occur between the carbon molecules. The heat energy generated is transmitted to the outside in the form of far-infrared radiation and convection. The conversion rate of electric energy to thermal energy is as high as over 98%, and the action of carbon molecules enables the surface of the system to heat up rapidly. When the electric film heating system is installed on the wall (ground), the heat energy will be continuously and evenly transmitted to every corner of the room. The reason why the electric film can quickly heat up the space is that 100% of its electrical energy input is effectively converted into more than 66% of far-infrared heat. Infrared radiation energy and 33% convection heat energy. As the use of electric heating films becomes more and more frequent, the performance requirements for electric heating films are also getting higher and higher. At the same time, with the advancement of science and technology, graphene is added to the electric heating films in the existing technology to ensure the stability of the conductive performance of the electric heating films. However, the electric heating films with added graphene will mostly cause the position of graphene to change due to vibration during the preparation process, which in turn affects the electric heating performance of the subsequent graphene electric heating films to a certain extent. At the same time, the thermal insulation performance of most electric heating films is poor, which in turn affects the energy-saving effect of the electric heating film to a certain extent. Therefore, a graphene superconducting far-infrared electric heating film and a preparation method are proposed. Summary of the invention

[0003] The purpose of the present invention is to provide a graphene superconducting far-infrared electric heating film and a preparation method thereof, so as to solve the problem that the graphene electric heating film proposed in the above background technology will mostly change its position due to vibration during the preparation process, thereby affecting the electric heating performance of the subsequent graphene electric heating film to a certain extent.

[0004] To achieve the above-mentioned purpose, the present invention provides the following technical solutions: a graphene superconducting far-infrared electric heating film and a manufacturing method thereof, comprising a graphene heating layer, wherein the graphene heating layer is arranged at the upper end of an adhesive layer, an interception layer is arranged at the lower end of the adhesive layer, an aluminum foil reflective layer is arranged at the lower end of the interception layer, a rubber thermal insulation layer is arranged at the lower end of the aluminum foil radiation layer, an environmentally friendly polyester layer is arranged at the upper end of the graphene heating layer, an adhesive layer is arranged at the upper end of the environmentally friendly polyester layer, and a flexible anti-scratch layer is arranged at the upper end of the adhesive layer.

[0005] As a preferred technical solution of the present invention, the adhesive layer is specifically a fusion of phenolic resin and silicone resin, the intercepting layer is composed of intercepting metal strips, the adhesive layer is graphene superconducting glue, and a distribution groove in the shape of a graphene heating layer is opened at the upper end of the graphene superconducting glue, and the distribution groove in the shape of the graphene heating layer is the thickness of a single layer of graphene.

[0006] As a preferred technical solution of the present invention, the flexible anti-scratch layer is a flexible ABS plastic layer, and the lower side of the rubber thermal insulation layer is provided with multiple protrusions.

[0007] As a preferred technical solution of the present invention, the thickness of the graphene heating layer is 25-30 um, the thickness of the environmentally friendly polyester layer is 100-110 um, and the thickness of the flexible anti-scratch layer is 120-130 um.

[0008] A method for producing a graphene superconducting far-infrared electric heating film:

[0009] a1. Select flexible ABS plastic to make a flexible anti-scratch layer: cut the flexible anti-scratch layer to a suitable thickness, then clean and remove static electricity from it, and then place it aside for use;

[0010] a2. Select an environmentally friendly polyester layer: eliminate static electricity on the environmentally friendly polyester layer, then use high voltage electricity to perform corona on the environmentally friendly polyester layer, and then dry it for standby use;

[0011] a3. Select a proper amount of graphene superconducting glue to make an adhesive layer: squeeze the upper end of a proper amount of graphene superconducting glue through a mold, so that the upper end of the graphene superconducting glue forms a distribution groove in the shape of a graphene heating layer, and at the same time, squeeze the lower end of the graphene superconducting glue through a mold to form a groove for placing the intercepting metal, and finally dry it to a semi-solidified state;

[0012] a4. Selecting a suitable amount of rubber to form a rubber thermal insulation layer: Extruding the selected suitable amount of rubber through a mold having a concave point at the lower end, and then cooling it for standby use;

[0013] a5. Select an appropriate amount of adhesive layer: obtain the polyester film by mechanical method, clean and remove static electricity at the same time, and then place the polyester film for standby use;

[0014] a6. Spray the selected single-layer graphene powder evenly onto the upper end of the graphene superconducting glue, then scrape off the excess graphene with a scraper, then cover the upper end of the graphene with an environmentally friendly polyester layer, and place the intercepting metal constituting the intercepting layer into the groove at the lower end of the graphene superconducting glue, and finally pass it through a first extruder for bonding and extrusion molding;

[0015] a7. Place the selected adhesive layer on the upper end of the environmentally friendly polyester layer, and simultaneously place the selected flexible anti-scratch layer on the upper end of the adhesive layer, and place the aluminum foil reflective layer on the lower side of the interception layer, and then bond and extrude them through a second extruder;

[0016] a8, inverting the semi-finished product obtained in a7 and placing a rubber thermal insulation layer on the aluminum foil reflective layer, then preheating the third extruder, and then passing the semi-finished product with the rubber thermal insulation layer through the third extruder to achieve a hot melt bonding effect;

[0017] a9. Finally, cut it into respective sizes according to the demand, and test whether its resistance value meets the requirements. Products that do not meet the requirements will be recycled and decomposed, and qualified ones can be stamped and marked, and then the graphene-based far-infrared electric heating film will be obtained.

[0018] As a preferred technical solution of the present invention, the preheating temperature of the third extruder included in a8 is 270-330°C, and the first extruder and the second extruder included in a6 and a7 are both two-roller extrusion mechanisms.

[0019] As a preferred technical solution of the present invention, the distribution groove in the shape of a graphene heating layer formed on the upper end of the graphene superconducting glue included in a3 has a thickness of a single layer of graphene, and the third extruder included in a8 is a two-roller heating extrusion mechanism.

[0020] Compared with the prior art, the present invention has the following beneficial effects:

[0021] The present invention extrude an appropriate amount of graphene superconducting glue on the upper end by setting a mold, thereby forming a graphene placement groove on the upper end of the graphene superconducting glue, and at the same time, extrude the lower end of the graphene superconducting glue through the mold to form a cutoff metal placement groove, and finally dry it to a semi-solidified state, and put the graphene into the graphene placement groove for relative positioning and storage, and use a scraper to push out excess graphene to achieve the effect of stabilizing the thickness of the single-layer graphene heating layer, thereby achieving stable energy saving and heating functionality during later use, thereby solving the problem that the graphene electric heating film is mostly subject to change of graphene position due to vibration during the preparation process, thereby affecting the electric heating performance of the subsequent graphene electric heating film to a certain extent.

[0022] 2. The present invention radiates far infrared rays by providing an aluminum foil reflective layer and a rubber thermal insulation layer, and at the same time uses the rubber thermal insulation layer to isolate the influence of the ground temperature. In addition, a plurality of protrusions are provided on the lower side of the rubber thermal insulation layer, thereby preventing the ground temperature from affecting the warmth after the single-layer graphene is heated, and achieving the effect of convenient positioning and placement, thereby solving the problem that the thermal insulation performance of most electric heating films is poor, which in turn affects the energy-saving effect of the electric heating film to a certain extent. BRIEF DESCRIPTION OF THE DRAWINGS

[0023] Figure 1 It is a schematic diagram of the local cross-sectional structure of the present invention.

[0024] In the picture: 1 flexible anti-scratch layer, 2 adhesive layer, 3 environmentally friendly polyester layer, 4 graphene heating layer, 5 adhesive layer, 6 interception layer, 7 aluminum foil reflective layer, 8 rubber thermal insulation layer. DETAILED DESCRIPTION

[0025] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.

[0026] See also Figure 1 The present invention provides a technical solution of a graphene superconducting far-infrared electric heating film and a manufacturing method thereof:

[0027] The graphene heating layer 4 is arranged on the upper end of the adhesive layer 5. The adhesive layer 5 not only has the effect of conducting electricity, but also has the effect of bonding. What is more important is that a placement groove is formed through the mold and its own plasticity to place the single-layer graphene, thereby avoiding the shape change or self-loss of the graphene due to vibration in the later stage, thereby ensuring the yield rate in the manufacturing process. An interception layer 6 is arranged at the lower end of the adhesive layer 5, and an aluminum foil reflective layer 7 is arranged at the lower end of the interception layer 6. A rubber thermal insulation layer 8 is arranged at the lower end of the aluminum foil radiation layer. The aluminum foil radiation layer is arranged to radiate the infrared rays generated by the graphene to ensure the thermal insulation functionality, and also to protect the interception metal strip included in the interception layer 6. An environmentally friendly polyester layer 3 is arranged on the upper end of the graphene heating layer 4, and an adhesive layer 2 is arranged on the upper end of the environmentally friendly polyester layer 3. A flexible anti-scratch layer 1 is arranged on the upper end of the adhesive layer 2, thereby Protection, but also to form an insulating layer to achieve the effect of insulation protection, and also to ensure the aesthetics of the finished product during transportation, the adhesive layer 2 is specifically a fusion of phenolic resin and silicone resin, the interception layer 6 is composed of interception metal strips, and the adhesive layer 5 is graphene superconducting glue, and the upper end of the graphene superconducting glue is provided with a distribution groove in the shape of a graphene heating layer 4, and the distribution groove in the shape of the graphene heating layer 4 is the thickness of a single layer of graphene, thereby achieving the purpose of positioning the single layer of graphene, the flexible anti-scratch layer 1 is a flexible ABS plastic layer, and the lower side of the rubber thermal insulation layer 8 is provided with multiple protrusions, thereby achieving the effect of convenient positioning and placement while avoiding the ground temperature affecting the heating of the single layer of graphene. The thickness of the graphene heating layer 4 is 25-30um, the thickness of the environmentally friendly polyester layer 3 is 100-110um, and the thickness of the flexible anti-scratch layer 1 is 120-130um.

[0028] A method for producing a graphene superconducting far-infrared electric heating film:

[0029] a1. Select flexible ABS plastic to make a flexible anti-scratch layer 1: cut the flexible anti-scratch layer 1 to a suitable thickness, then clean and remove static electricity from it, and then place it aside for use;

[0030] a2. Select an environmentally friendly polyester layer 3: eliminate static electricity on the environmentally friendly polyester layer 3, then use high voltage electricity to perform corona on the environmentally friendly polyester layer 3, and then dry it for standby use;

[0031] a3. Select a proper amount of graphene superconducting glue to make an adhesive layer 5: squeeze the upper end of a proper amount of graphene superconducting glue through a mold, so that the upper end of the graphene superconducting glue forms a distribution groove in the shape of the graphene heating layer 4, and at the same time, squeeze the lower end of the graphene superconducting glue through a mold to form a cutoff metal placement groove, and finally dry it to a semi-solidified state;

[0032] a4. Selecting a suitable amount of rubber to form a rubber thermal insulation layer 8: Extruding the selected suitable amount of rubber through a mold having a concave point at the lower end, and then cooling it for standby use;

[0033] a5. Select an appropriate amount of adhesive layer 2: obtain a polyester film by a mechanical method, clean and remove static electricity at the same time, and then place the polyester film aside for use;

[0034] a6, spraying the selected single-layer graphene powder evenly onto the upper end of the graphene superconducting glue, then scraping off the excess graphene with a scraper, then covering the upper end of the graphene with an environmentally friendly polyester layer 3, and placing the intercepting metal constituting the intercepting layer 6 into the groove at the lower end of the graphene superconducting glue, and finally passing it through a first extruder for bonding and extrusion molding;

[0035] a7. Place the selected adhesive layer 2 on the upper end of the environmentally friendly polyester layer 3, and simultaneously place the selected flexible anti-scratch layer 1 on the upper end of the adhesive layer 2, and place the aluminum foil reflective layer 7 on the lower side of the interception layer 6, and then bond and extrude them through a second extruder;

[0036] a8, inverting the semi-finished product obtained in a7 and placing a rubber thermal insulation layer 8 on the aluminum foil reflective layer 7, then preheating the third extruder, and then passing the semi-finished product with the rubber thermal insulation layer 8 through the third extruder to achieve a hot melt bonding effect;

[0037] a9. Finally, cut it into respective sizes according to the demand, and test whether its resistance value meets the requirements. Products that do not meet the requirements will be recycled and decomposed, and qualified ones can be stamped and marked, and then the graphene-based far-infrared electric heating film will be obtained.

[0038] The preheating temperature of the third extruder is 270-330° C., and the first extruder and the second extruder are both two-roller extrusion mechanisms.

[0039] The distribution groove in the shape of the graphene heating layer 4 formed on the upper end of the graphene superconducting glue is of a single-layer graphene thickness, and the third extruder is a two-roller heating extrusion mechanism.

[0040] The specific operation mode of the present invention is:

[0041] First, material selection is performed, that is, flexible ABS plastic is selected to make a flexible anti-scratch layer 1: the flexible anti-scratch layer 1 is cut to a suitable thickness, then cleaned and destaticized, and then placed aside for use; an environmentally friendly polyester layer 3 is selected: the environmentally friendly polyester layer 3 is destaticized, and then corona is performed on the environmentally friendly polyester layer 3 using high voltage electricity, and then it is dried and placed aside for use; an appropriate amount of graphene superconducting glue is selected to make an adhesive layer 5: an appropriate amount of graphene superconducting glue is squeezed through a mold to form a graphene placement groove at the upper end of the graphene superconducting glue, and at the same time, the lower end of the graphene superconducting glue is squeezed through a mold to form a cutoff metal placement groove, and finally dried to a semi-solidified state; an appropriate amount of rubber is selected to make a rubber thermal insulation layer 8: the selected appropriate amount of rubber is extruded and formed through a mold with a concave point at the lower end, and then cooled and placed aside; an appropriate amount of adhesive layer 2 is selected: a polyester film is obtained by a mechanical method, and at the same time, it is cleaned and destaticized, and then the polyester film is placed aside for use; the selected single-layer graphene powder is evenly sprayed To the upper end of the graphene superconducting glue, then scrape off the excess graphene with a scraper, then cover the upper end of the graphene with an environmentally friendly polyester layer 3, and place the interception metal that constitutes the interception layer 6 in the groove at the lower end of the graphene superconducting glue, finally pass it through the first extruder for bonding and extrusion molding, place the selected bonding layer 2 on the upper end of the environmentally friendly polyester layer 3, and simultaneously place the selected flexible anti-scratch layer 1 on the upper end of the bonding layer 2, and place the aluminum foil reflective layer 7 on the lower side of the interception layer 6, then pass it through the second extruder for bonding and extrusion molding, reverse the semi-finished product obtained by a7 and place a rubber thermal insulation layer 8 on the aluminum foil reflective layer 7, then preheat the third extruder, and then pass the semi-finished product with the rubber thermal insulation layer 8 through the third extruder to achieve the effect of hot melt bonding, finally cut it into their respective sizes according to needs, test whether its resistance meets the requirements, recycle and decompose the products that do not meet the requirements, and mark the qualified ones with stamps, and then the graphene-based far-infrared electric heating film is obtained and shipped out for assembly of the electric heating film system.

[0042] In the description of the present invention, it is necessary to understand that the indicated orientation or positional relationship is based on the orientation or positional relationship shown in the accompanying drawings, and is only for the convenience of describing the present invention and simplifying the description, rather than indicating or implying that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore cannot be understood as a limitation on the present invention.

[0043] In the present invention, unless otherwise clearly stipulated and limited, for example, it can be a fixed connection, a detachable connection, or an integrated one; it can be a mechanical connection or an electrical connection; it can be directly connected or indirectly connected through an intermediate medium, it can be the internal connection of two elements or the interaction relationship between two elements. Unless otherwise clearly defined, for ordinary technicians in this field, the specific meanings of the above terms in the present invention can be understood according to the specific circumstances.

[0044] Although embodiments of the present invention have been shown and described, it will be appreciated by those skilled in the art that various changes, modifications, substitutions and variations may be made to the embodiments without departing from the principles and spirit of the present invention, and that the scope of the present invention is defined by the appended claims and their equivalents.

Claims

1. A graphene superconducting far-infrared electric heating film, comprising a graphene heating layer (4), characterized in that: The graphene heating layer (4) is arranged on the upper end of the adhesive layer (5), the lower end of the adhesive layer (5) is provided with an interception layer (6), the lower end of the interception layer (6) is provided with an aluminum foil reflection layer (7), the lower end of the aluminum foil radiation layer is provided with a rubber thermal insulation layer (8), the upper end of the graphene heating layer (4) is provided with an environmentally friendly polyester layer (3), the upper end of the environmentally friendly polyester layer (3) is provided with an adhesive layer (2), and the upper end of the adhesive layer (2) is provided with a flexible anti-scratch layer (1); The adhesive layer (2) is specifically a fusion of phenolic resin and silicone resin, the interception layer (6) is composed of an interception metal strip, the adhesive layer (5) is a graphene superconducting glue, and a distribution groove in the shape of a graphene heating layer (4) is provided at the upper end of the graphene superconducting glue, and the distribution groove in the shape of the graphene heating layer (4) is a single layer of graphene thickness, the flexible anti-scratch layer (1) is a flexible ABS plastic layer, and the lower side of the rubber thermal insulation layer (8) is provided with multiple protrusions, the thickness of the graphene heating layer (4) is 25 to 30 um, the thickness of the environmentally friendly polyester layer (3) is 100 to 110 um, and the thickness of the flexible anti-scratch layer (1) is 120 to 130 um; A method for manufacturing a graphene superconducting far-infrared electric heating film, comprising: a1, selecting flexible ABS plastic to manufacture a flexible anti-scratch layer (1); cutting the flexible anti-scratch layer (1) to a suitable thickness, then cleaning and removing static electricity from the flexible anti-scratch layer (1), and then placing the flexible anti-scratch layer (1) for later use; a2. Selecting an environmentally friendly polyester layer (3), eliminating static electricity on the environmentally friendly polyester layer (3), and then using high voltage electricity to perform corona on the environmentally friendly polyester layer (3), and then drying it for later use; a3. Select an appropriate amount of graphene superconducting glue to make an adhesive layer (5): squeeze the upper end of an appropriate amount of graphene superconducting glue through a mold, so that the upper end of the graphene superconducting glue forms a distribution groove in the shape of a graphene heating layer (4), and at the same time squeeze the lower end of the graphene superconducting glue through a mold to form a groove for placing the intercepting metal, and finally dry it to a semi-solidified state; a4. Selecting a suitable amount of rubber to form a rubber thermal insulation layer (8): Extruding the selected suitable amount of rubber through a mold having a concave point at the lower end, and then cooling it for later use; a5. Selecting an appropriate amount of adhesive layer (2): obtaining a polyester film by a mechanical method, and cleaning and removing static electricity at the same time, and then placing the polyester film aside for later use; a6, spraying the selected single-layer graphene powder evenly onto the upper end of the graphene superconducting glue, then scraping off the excess graphene with a scraper, then covering the upper end of the graphene with an environmentally friendly polyester layer (3), and placing the intercepting metal constituting the intercepting layer (6) into the groove at the lower end of the graphene superconducting glue, and finally passing it through a first extruder for bonding and extrusion molding; a7. placing the selected adhesive layer (2) on the upper end of the environmentally friendly polyester layer (3), and simultaneously placing the selected flexible anti-scratch layer (1) on the upper end of the adhesive layer (2), and placing the aluminum foil reflective layer (7) on the lower side of the interception layer (6), and then bonding and extruding them through a second extruder; a8, inverting the semi-finished product obtained in a7 and placing a rubber thermal insulation layer (8) on the aluminum foil reflective layer (7), then preheating the third extruder, and then passing the semi-finished product with the rubber thermal insulation layer (8) through the third extruder to achieve a hot melt bonding effect; a9. Finally, cut it into respective sizes according to the requirements, test whether its resistance value meets the requirements, recycle and decompose the products that do not meet the requirements, and stamp and mark the qualified ones, and then obtain the graphene-based far-infrared electric heating film; The preheating temperature of the third extruder included in a8 is 270-330°C, and the first extruder and the second extruder included in a6 and a7 are both two-roller extrusion mechanisms; The distribution groove in the shape of the graphene heating layer (4) formed on the upper end of the graphene superconducting glue included in a3 has a thickness of a single layer of graphene, and the third extruder included in a8 is a two-roller heating extrusion mechanism.