A process for controlling the slippage of the main edge line of the side panel
By adding raised shapes and adjusting the draft angle and fillet of the outer side panel during the process design stage, the problem of the main edge line slippage line was solved, achieving efficient part forming and overall vehicle styling effect, and reducing mold development and debugging costs.
Patent Information
- Application Number
- CN202210723699.9
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2022-06-23
- Publication Date
- 2024-11-08
- Estimated Expiration
- 2042-06-23
AI Technical Summary
During the drawing process of the outer side panel of the vehicle body, the main edge line is prone to slippage defects due to its small surface angle and location in the middle of the product. This affects the appearance quality of the part and the aesthetics of the whole vehicle, and existing technologies are difficult to control effectively.
By adjusting the process supplement modeling method on the outside of the product during the process design stage, and adding a raised shape outside the product boundary line when designing the drawing die process, the sliding line of the main edge is optimized. Specifically, this includes adjusting the included angle and radius of the draft surface 1, draft surface 2, and draft surface 3, as well as the height difference between the high point of the process model and the high point of the main edge, in order to control the generation of the sliding line.
Effective control of main edge slip line defects shortens mold development cycle, reduces technical requirements, reduces debugging workload, ensures part forming quality and overall vehicle styling effect, and avoids increased mold design and processing costs.
Smart Images

Figure CN115213276B_ABST
Abstract
Description
Technical Field
[0001] The invention belongs to the technical field of cold stamping and relates to a process method for controlling the sliding of a main ridgeline of a side panel. Background Art
[0002] In order to highlight the styling features, the side outer panel is often designed with multiple ridges. During the drawing process, the slip line defects of each ridge need to be comprehensively considered. The main ridge has a defect of excessive slip line due to its small surface angle, prominent ridge and being located in the middle of the product. During the forming process of the part, the high point of the main ridge first contacts the sheet material, causing hardening. The marks produced after slipping remain on the part, resulting in more serious slip lines. Usually, during the debugging stage, the problem is solved by adjusting the strength of the draw ribs according to the sliding direction of the slip line and increasing the compaction of the colored slip points on both sides of the die ridge line. This method is heavily dependent on the operating skills of the fitter, the optimization cycle is too long, and it cannot guarantee the complete elimination of this surface defect. This defect affects the visual effect of the area and reduces the aesthetics of the entire vehicle.
[0003] At present, the body styling styles of cars are different. In order to make the products have distinctive characteristics, the ridge areas of the body appearance are gradually transitioning to a sharper trend. The waistline of the vehicle body formed by the front fender, door and side panel is prominent and has sharp rounded corners. In the overall waistline area of the vehicle body, the relative angles between surfaces and the rounded corner values have sharper characteristics, which makes the formability of the body sheet metal and the appearance quality of the product more difficult to control.
[0004] The side panel is one of the key components of the vehicle body exterior covering, and its structural size is the largest among the covering parts. This type of part has a complex geometric shape, and requires extremely high surface quality and dimensional accuracy. In order to achieve the design intention of the product shape, it is necessary to study the forming process, realize the styling characteristics of the side panel outer panel, and ensure the forming quality of the product in each process of the stamping die during the forming process; therefore, it is necessary to study the formability of the appearance edges and surface quality of the side panel outer panel, and control it layer by layer to achieve sharp product shape characteristics.
[0005] During the drawing process of the side outer panel, due to the angle between the faces at the main edge, the height difference between the edge and the profile is even worse. Under the premise that the sheet forming performance remains unchanged, the main edge forming limit is a very severe challenge. In terms of the product qualification rate in the manufacturing process, whether it is the smoothness of the fillet, the continuity of the A-level surface, the slip line at the edge and other defects, they are all technical links that cause manufacturing defects. How to avoid the occurrence of related defects through effective process means and forming methods and produce qualified parts is the technical difficulty of this project.
[0006] Patent document 1 (CN206215773U) A drawing die with a sheet material supporting device;
[0007] The utility model discloses a drawing die with a sheet material supporting device, which comprises an upper die base, a lower die base and a pressure ring. A drawing die is arranged on the upper die base, and a drawing punch matched with the drawing die is arranged on the lower die base. The drawing punch is arranged inside the pressure ring and is slidably connected with the pressure ring. A sheet material supporting device is arranged in a working cavity of the drawing punch. The upper end of the sheet material supporting device is arc-shaped and arranged on the inner side of the wheel eyebrow ridge line. The center of the arc of the upper end of the sheet material supporting device is the same as the center of the arc of the wheel eyebrow ridge line. A channel for the upper end of the sheet material supporting device to pass through is arranged on the top of the drawing punch. Moreover, the sheet material supporting device can move up and down in the working cavity under the action of the die push rod. When the sheet material supporting device moves upward, the upper end of the sheet material supporting device can support the sheet material after passing through the channel, thereby delaying the contact time between the wheel eyebrow ridge line and the sheet material, so that the sheet material avoids the appearance of a slip line at the wheel eyebrow position.
[0008] Patent document 2 (CN112620466A) A die and stamping test method for studying the formation law of stamping slip lines;
[0009] A mold and a stamping test method for studying the formation law of stamping slip lines belong to the field of stamping. The mold includes an upper and lower mold plate, a first and a second die, a first and a second pressure ring, and a punch. The punch is arranged on the lower mold plate, and the first and the second spring components connecting the first and the second pressure rings are arranged on both sides of the lower mold plate; the die is arranged on both sides of the upper mold plate, and the space between the pressure ring and the die is used to place the stamping sheet; the first, the second, and the third pressure rings are provided with the first, the second, and the third pressure grooves, and the first, the second, and the third die are provided with the first, the second, and the third grooves; the first, the second, and the third pressure grooves respectively accommodate the first, the second, and the third active draw ribs and their gaskets; the overall height of the first active draw rib is greater than the overall height of the second or the third active draw rib, so that the resistance generated by the sheet flowing through the first active draw rib is equal to the resistance generated by the sheet flowing through the second and the third active draw ribs. The method is implemented using the above mold. The present invention systematically considers the important factors of slip line formation.
[0010] Patent document 3 (CN114192649A) Aluminum hood outer panel stamping forming method;
[0011] The present invention relates to a stamping forming method for an aluminum hood outer panel. The stamping forming method is suitable for the case where the characteristic edge line in the middle of the product is annular and the fillet is less than R10. Through one-time drawing forming, the flow of sheet metal on both sides of the edge line cannot be controlled, and it is easy to produce relative movement with the punch, resulting in slip defects. The stamping forming method includes the following steps: drawing, trimming, trimming + shaping, and flanging. By directly adding a pressing mechanism on both sides of the edge fillet, the flow of sheet metal during the edge forming process is controlled to prevent the generation of slip lines. Through the forming method from bottom to top, the contact marks caused by the punch forming on the exposed surface of the product can be avoided, thereby improving the forming surface quality of the product. The present invention can ensure that the appearance quality of the extremely small fillet forming of the plate edge line meets the quality requirements of clear and smooth edges and no slip defects.
[0012] The above patents have low relevance to this application. Summary of the invention
[0013] The present invention is a process method for controlling the slippage of the main edge of the side panel, and proposes an effective method by studying the product modeling and the principle of the generation of the slip line, such as the angle of the main edge of the side panel, the distance between the peak and the valley, and the size of the edge fillet. The present invention can ensure the forming quality of the product in the production process, reduce the risk of the slip line generated by the drawing forming, and solve the light and shadow surface defects at the edge.
[0014] It should be noted that, in this article, relational terms such as first and second, etc. are only used to distinguish one entity or operation from another entity or operation, and do not necessarily require or imply any such actual relationship or order between these entities or operations. Moreover, the terms "include", "comprise" or any other variants thereof are intended to cover non-exclusive inclusion, so that a process, method, article or device including a series of elements includes not only those elements, but also other elements not explicitly listed, or also includes elements inherent to such process, method, article or device.
[0015] In order to solve the above technical problems, the present invention is implemented by adopting the following technical solutions:
[0016] A process method for controlling the sliding of the main edge line of the side panel, characterized in that: in the process design stage, by adjusting the product outer side process supplementary modeling method, changing the contact point with the sheet material during the drawing process, the sliding line generated by the main edge line is optimized and controlled.
[0017] Furthermore, the method for adjusting the process supplementary modeling of the outer side of the product includes: when designing the process modeling of the drawing die, a convex modeling is designed on the process supplementary surface outside the product boundary line.
[0018] Furthermore, the protrusion design process includes:
[0019] First, extend the boundary line of the side outer panel product outward in a direction tangent to the product, with a length of 5-15 mm, preferably 10 mm;
[0020] Then, based on the completion of the product epitaxial surface in the previous step, the draft surface three is designed, and the draft surface three forms an angle of 15-30 degrees with the stamping direction;
[0021] The draft surface is upward in three directions (i.e., the top of the product's epitaxial surface);
[0022] The height of the draft surface 3 needs to ensure that after the rounding R3 of the draft surface 2, the height difference H2 between the process modeling high point and the main edge line high point is between 8-20mm;
[0023] The draft surface 2 is at an angle of 45-60 degrees to the stamping direction, and at an angle of 120-135 degrees to the draft surface 3. The draft surface 2 and the draft surface 3 are rounded by R3, with a size of 15-30mm;
[0024] Design the draft surface one, and make the angle A of draft surface one to the stamping direction at 15-45 degrees. At the same time, the angle B between draft surface one and draft surface two is controlled at 120-160 degrees.
[0025] Through the three design factors of "draft surface one, draft surface two, and draft surface three", the convex process shape is formed after the original angle is chamfered, and the height of the convexity is controlled by adjusting the three draft surfaces and the fillet sizes between them;
[0026] Furthermore, the drawing process shape that controls the slippage of the main edge line is achieved by adjusting the draft surface one, the draft surface two, the draft surface three, the angle A between the draft surface one and the stamping direction, the angle B between the draft surface one and the draft surface two, the chamfer R3 between the draft surface two and the draft surface three, and the height difference H2 between the high point of the process shape and the high point of the main edge line.
[0027] The process modeling is the design of draft surface one, draft surface two, draft surface three and the chamfers between them. The high point of the process modeling is the chamfer R3 between draft surface three and draft surface two.
[0028] Furthermore, the height difference H1 between the main ridgeline and the fender ridgeline of the product is controlled within 10 mm, balancing the consistency of the slip line generated by the main ridgeline and the fender ridgeline.
[0029] Theoretically, H1 is best at 0, but this is not achievable in actual product design and should be controlled within 10mm.
[0030] There is a height difference between the edge line and the high point of the craft shape, and the slip line is controlled by this height difference.
[0031] Furthermore, the slip line criteria are checked based on the distance the material passes over the mold radius sliding mark. First, run the simulation results to the end of the drawing simulation, and execute AutoForm / Results / Skid to evaluate the slip line: 1) No back and forth sliding; 2) Slip distance ≤ 1 / 2R angle arc.
[0032] Autoform is a simulation analysis software used in stamping process design; Results is the software simulation analysis result view; Skid is the slip line mentioned in the present invention, an evaluation index in formability analysis; the oblique line represents the level, the analysis result in the software, and the slip line evaluation index in the analysis result.
[0033] 1) No back and forth slip; 2) Slip distance ≤ 1 / 2R angle arc, which are the specific requirements, professional terms and specifications in the slip line evaluation indicators.
[0034] The R mentioned in the evaluation indicators refers to the R angle of the product's edge line.
[0035] Furthermore, the contact state between the sheet and the high point of the main edge and the high point of the process shape during the forming process is simulated. The sheet first contacts the high point of the process shape by 8-15 mm to eliminate the slip line generated by the sheet at the main edge.
[0036] When the sheet surface first contacts a certain point on the main edge R of the product, it is a point, and the entire main edge R is equivalent to a line; during the drawing process, if the sheet does not move on the main edge R, no slip line will be generated, and it is just a line. This is an ideal state; in fact, the sheet will move to one side and slip, that is, the distance moved by the line that the sheet first contacts at the end of the drawing is the size of the slip line; use the above-mentioned no back and forth slip, slip distance ≤ 1 / 2R angle arc evaluation indicators to judge whether it is reasonable.
[0037] Simulation refers to Autoform software analysis, which is carried out by importing it into Autoform software after the process modeling design is completed to evaluate whether the process modeling is reasonable, whether there are slip lines, etc.
[0038] Preferably, the draft surface 3 forms an angle of 25 degrees with the stamping direction.
[0039] Preferably, the height difference H2 between the high point of the process shape and the high point of the main edge line is 10 mm.
[0040] Preferably, the rounded angle R3 of the second draft surface and the third draft surface is 25 mm.
[0041] Compared with the prior art, the present invention has the following beneficial effects:
[0042] The present invention studies the product modeling such as the angle of the main edge surface of the side enclosure, the peak-to-valley distance, the size of the edge radius, and the principle of the generation of the slip line. In the process design stage, reasonable process modeling is adopted to change the contact point with the sheet material during the drawing process, solve the main edge slip defect of the part, shorten the mold development cycle, and also reduce the technical requirements for the staff, which can greatly reduce the debugging workload and shorten the rectification cycle.
[0043] According to the traditional side panel forming process, it is proposed to increase the radius of the main edge line of the side panel in the stamping SE (Stamping Simultaneous engineering) stage, which leads to a weakening of the sharpening effect of the shape and changes the shape effect of the whole vehicle. The present invention solves the problem of the sliding line of the main edge line of the side panel through process means to ensure the shape effect of the whole vehicle.
[0044] When the side panel shape cannot be changed and the main edge slip defect is relatively serious in the process design stage, the present invention avoids the method of enlarging the main edge corner by stretching and sharpening the main edge corner in subsequent shaping, which brings about an increase in mold design and processing and manufacturing costs and the risk of uneven edges in subsequent shaping.
[0045] When there are multiple ridges in the side panel shape, the present invention avoids using a drawing die with a sheet support device to delay the contact between a certain ridge and the sheet to eliminate the slip line, which increases the difficulty and cost of die design, processing and manufacturing. BRIEF DESCRIPTION OF THE DRAWINGS
[0046] The present invention will be further described below in conjunction with the accompanying drawings:
[0047] Figure 1 Schematic diagram of the ridges of the side perimeter;
[0048] Figure 2 Schematic diagram of various parameters of the main ridge section of the side panel;
[0049] Figure 3 It is a schematic diagram of the side panel drawing profile;
[0050] Figure 4 It is a schematic diagram of various parameters of the side panel drawing process modeling section;
[0051] Figure 5 yes Figure 4 A partial enlarged view of
[0052] Figure 6 It is a cross-sectional schematic diagram of the side panel drawing simulation forming process;
[0053] Figure 7 It is a schematic diagram of the cross section of the side drawing die.
[0054] Description of reference numerals:
[0055] ①-Rear window ridgeline, ②-Main ridgeline, ③-Fender ridgeline;
[0056] M-technical modeling;
[0057] 1-die, 2-punch, 3-pressing ring, 4-sheet, 5-high point of main edge, 6-high point of process modeling, 7-draft surface one, 8-draft surface two, 9-draft surface three. DETAILED DESCRIPTION
[0058] In order to make the purpose, technical scheme and advantages of the implementation of the present invention clearer, the technical scheme in the embodiment of the present invention will be described in more detail below in conjunction with the drawings in the embodiment of the present invention. In the drawings, the same or similar reference numerals throughout represent the same or similar elements or elements with the same or similar functions. The described embodiments are part of the embodiments of the present invention, not all of the embodiments. The embodiments described below with reference to the drawings are exemplary and are intended to be used to explain the present invention, and should not be construed as limitations on the present invention. Based on the embodiments in the present invention, all other embodiments obtained by ordinary technicians in this field without making creative work are within the scope of protection of the present invention. The embodiments of the present invention are described in detail below in conjunction with the drawings.
[0059] In the description of the present invention, it should be understood that the terms "center", "longitudinal", "lateral", "front", "back", "left", "right", "vertical", "horizontal", "top", "bottom", "inside", "outside" and the like indicate orientations or positional relationships based on the orientations or positional relationships shown in the accompanying drawings, and are only for the convenience of describing the present invention and simplifying the description, rather than indicating or implying that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore should not be understood as limiting the scope of protection of the present invention.
[0060] The present invention is described in detail below in conjunction with the accompanying drawings:
[0061] The present invention is a process method for controlling the slippage of the main edge of the side enclosure, including product modeling research on the angle of the main edge of the side enclosure, the distance between the peak and the valley, and the size of the edge fillet, formulating a reasonable drawing process modeling, and adjusting the high point of the main edge of the side enclosure, the high point of the process modeling and the contact state of the sheet material through simulation verification to solve the problem of main edge slippage. The present invention can not only ensure the forming quality of the parts in the production process, reduce the risk of slip lines generated by drawing forming, solve the light and shadow surface defects at the edge, but also greatly reduce the debugging workload, shorten the rectification cycle, and provide a simple and effective problem-solving method for the later stage of part rectification.
[0062] The technical solution of the present invention is: a process method for controlling the slip of the main edge of the side panel. During the forming process of the main edge, when the sheet metal contacts the punch edge, when the sheet metal edge begins to plastically deform and moves with the uneven feeding, a slip mark will be generated on one side of the edge. This slip mark is the slip line. When the slip line moves to the outside of the R angle of the main edge, even after painting, there will be clearly visible slip marks on the product, affecting the appearance of the part and causing slip defects on the product. When the radius of the main edge is less than R10, the risk of product slip defects generally increases exponentially. Severe slip line phenomenon on the surface of parts cannot be accepted by customers. The smaller the radius of the main edge, the smaller the angle between adjacent planes, the greater the risk of slip, and the more difficult it is to ensure the quality of the parts.
[0063] Through the analysis of the product modeling and drawing modeling simulation verification results through long-term experience, it can be concluded that when the slip line is generated, the flow of the sheet on both sides of the main edge can be controlled by modifying the original product definition (adjusting the size of the main edge fillet, increasing the angle between the two sides of the edge), adjusting the process supplementary modeling of the outer side of the drawing die product, etc., so as to prevent the slip mark from sliding beyond the product edge R. Although these two methods can solve such problems to a certain extent, adjusting the size of the main edge fillet, or increasing the angle between the two sides of the main edge will change the original product design concept, limit the breakthrough of the body design, and be unfavorable to the body modeling. Only by adjusting the process supplementary modeling method on the outer side of the product can the slip line generated by the main edge be optimized and controlled.
[0064] The drawing process modeling for controlling the sliding of the main edge line is characterized by: when designing the drawing die process modeling, first design a raised shape on the process supplementary surface outside the product boundary line. The raised process modeling design process: first extend the boundary line of the side outer panel product outward in the direction tangent to the product, with a length of 5-15mm, preferably 10mm; then, in the direction at an angle of 15-30 degrees to the stamping direction, preferably 25 degrees, which is the draft surface three 9; the height of the draft surface three 9 needs to ensure that after the rounding R3 with the draft surface two 8, the height difference H2 between the high point of the process modeling and the high point of the main edge line is between 8-20mm, preferably 10mm (simulation is required to verify the size of the main edge line sliding line , adjust the height difference H2 value); the draft surface 2 8 is at an angle of 45-60 degrees to the stamping direction, and at the same time at an angle of 120-135 degrees to the draft surface 3 9, the draft surface 2 8 and the draft surface 3 9 are chamfered with a radius R3 of 15-30mm, preferably 25mm. The size of R3 needs to comprehensively consider the angle between the draft surface 2 8 and the draft surface 3 9 and the height difference H2 between the high point of the process modeling and the high point of the main edge line. The three key parameters determine the control effect of the process modeling on the slip of the main edge line. Since the angle of the draft surface 28 is relatively large, if it is directly extended to the pressing surface, it will lead to a large punch contour line and low material utilization. Therefore, it is necessary to design the draft surface 17 after the draft surface is extended to a certain length. The draft surface 17 forms an angle A of 15-45 degrees with the stamping direction, and the angle B with the draft surface 28 is controlled at 120-160 degrees. The key point of the shape design here is the reasonable punch contour line and the required formability. There should be no unnecessary waste of materials and cracking and wrinkling of the draft surface 17 during the drawing process. In short, the drawing process shape that controls the slippage of the main ridge needs to adjust the draft surface 17, the draft surface 28, the draft surface 39, the angle A between the draft surface 17 and the stamping direction, the angle B between the draft surface 17 and the draft surface 28, the rounded angle R3 between the draft surface 28 and the draft surface 39, and the most important height difference H2 between the high point of the process shape and the high point of the main ridge, and design a reasonable process shape to control the slip line problem of the main ridge.
[0065] Before designing the drawing process, it is necessary to plan the stamping direction of the drawing in advance. It is necessary to consider that the drawing depth at the side panel top cover and the door sill is as deep as possible, the height difference H1 between the main edge line of the product and the wheel arch edge line is as small as possible, and the consistency of the slip line generated by the main edge line and the wheel arch edge line is balanced. Check the skid line (Skid & Impact line) criterion, that is, judge based on the distance of the material over the sliding mark of the mold radius. First run the simulation results to the end of the drawing simulation, and execute AutoForm / Results / Skid to evaluate the skid line (Skid line): 1) No back and forth sliding; 2) Slip distance (curve measurement) ≤ 1 / 2R angle arc.
[0066] See also Figure 1Schematic diagram of the ridges of the side wall; the ridges shown in the figure are the distribution of the ridges that are prone to slip lines during the forming process in the present invention.
[0067] See also Figure 2 Schematic diagram of the main ridge section parameters of the side panel; the main ridge section parameters shown in the figure analyze and summarize the main ridge surface angle, peak-to-valley distance and ridge radius size of multiple models.
[0068] See also Figure 3 Schematic diagram of the side panel drawing surface modeling; the overall effect of the process modeling is shown in the figure.
[0069] See also Figure 4 , Figure 5 Schematic diagram of the parameters of the side panel drawing process section; the main edge line parameters and process modeling parameters shown in the figure, with the main edge line of the product marked.
[0070] Figure 4 The middle is the cross section of the overall drawn profile after the drawing process, which includes the product and process shapes. The shaping profile is larger and the internal feature points are smaller.
[0071] Angle A is the angle between the draft surface 1 7 and the stamping direction; Angle B is the angle between the draft surface 1 7 and the draft surface 2 8;
[0072] H1 is the height difference between the main ridgeline and the fender ridgeline, that is, the height difference mentioned above is preferably 0, and is controlled within 10mm; H2 is the height difference between the high point of the main ridgeline and the high point of the process shape;
[0073] R3 is the fillet between the draft surface three 9 and the draft surface two 8;
[0074] R1 and R2 are both product edge fillets, R1 is Figure 1 The fillet of the main edge line, R2 is Figure 1 The rounded corners of the center wheel arch ridgeline;
[0075] See also Figure 6 Schematic diagram of the cross-section of the side panel drawing simulation forming process; the figure shows the contact state between the sheet metal and the high point of the main edge and the high point of the process shape during the simulation forming process. The sheet metal first contacts the high point of the process shape for 8-15mm to eliminate the slip line generated by the sheet metal at the main edge.
[0076] See also Figure 7 Schematic diagram of the cross section of the side drawing die; when the die works, the die 1 moves, and the pressure ring 3 lifts up the stroke until the die 1 contacts the pressure ring 3 to start pressing the material, the die 1 and the pressure ring 3 press the sheet material and start moving downward, and the sheet material contacts the punch 2 and the sheet material forming begins. During the entire drawing process, the die 1 and the pressure ring 3 keep pressing the sheet material and complete the drawing process together with the punch 2 until the die 1 contacts the punch 2 and the drawing is completed.
[0077] Model Angle between surfaces C Peak to valley distance S mm Edge radius R mm Edge sharpening mm A brand model 1 144.7 11.85 6.45 R-1 A brand model 2 148 2.6 2.35 R-1 A brand model 3 132.8 14.35 4.5 3 A brand model 4 135 13.5 3.3 0.7 B brand model 149.9 8.75 2.6 0.7 C brand model 160.1 9.9 5 0.7 D brand model 1 160.3 7.08 5 R D brand model 2 125 18.63 3.5 R-1 E brand model 154.9 3.15 2 0.7
[0078] The present invention discloses a process method for controlling the slippage of the main edge line of the side enclosure. Through the research on product modeling such as the surface angle of the main edge line of the side enclosure, the distance between peaks and valleys, the size of the edge fillet, and the principle of the generation of the slip line, reasonable process modeling is adopted in the process design stage, the contact point with the sheet material is changed during the drawing process, the slippage defect of the main edge line of the product is solved, the development cycle of the mold is shortened, and the technical requirements for the staff are also reduced, so that the debugging workload can be greatly reduced and the rectification cycle can be shortened.
[0079] There is no need to propose increasing the radius of the main edge lines of the side panel during the stamping SE (Stamping Simultaneous engineering) stage. Instead, the problem of the slip line of the main edge lines of the side panel is solved through technological means to ensure the styling effect of the entire vehicle.
[0080] This avoids the method of enlarging the main edge corner by stretching and sharpening the main edge corner by secondary shaping, which increases the cost of mold design and processing and manufacturing and the risk of uneven edges in subsequent shaping.
[0081] Avoid using a drawing die with a sheet support device to delay the contact between a certain edge and the sheet to eliminate the slip line, which will increase the difficulty and cost of die design, processing and manufacturing.
[0082] The drawing process modeling that controls the slip of the main edge line needs to adjust the draft surface 1 7, the draft surface 2 8, the draft surface 3 9, the angle A between the draft surface 1 7 and the stamping direction, the angle B between the draft surface 1 7 and the draft surface 2 8, the chamfer R3 between the draft surface 2 8 and the draft surface 3 9, and the most important height difference H2 between the high point of the process modeling and the high point of the main edge line, so as to design a reasonable process modeling to control the slip line problem of the main edge line.
[0083] The above is only a specific implementation of the present invention, but the protection scope of the present invention is not limited thereto. Any modification, equivalent replacement and improvement made by any person skilled in the art within the technical scope disclosed by the present invention and within the spirit and principle of the present invention shall be covered within the protection scope of the present invention. At the same time, the contents not described in detail in this specification belong to the prior art known to those skilled in the art.
Claims
1. A process for controlling the sliding of the main ridgeline of the side panel, characterized in that: In the process design stage, by adjusting the product outer process to supplement the modeling method, changing the contact point with the sheet during the drawing process, the slip line generated by the main edge line is optimized and controlled; The method for adjusting the process supplementary modeling of the outer side of the product is as follows: when designing the process modeling of the drawing die, a convex modeling is designed on the process supplementary surface outside the product boundary line. The design process of the convex modeling is as follows: First, extend the boundary line of the side outer panel product outward in the direction tangent to the product, with a length of 5-15mm; Then, based on the completion of the product epitaxial surface in the previous step, the draft surface three is designed, and the draft surface three forms an angle of 15-30 degrees with the stamping direction; The draft surface is upward in three directions, that is, above the epitaxial surface of the product; The height of the draft surface three needs to ensure that after the rounding R3 with the draft surface two, the height difference H2 between the process modeling high point and the main edge line high point is between 8-20mm. The process modeling high point is the rounding R3 between the draft surface three and the draft surface two. The draft surface 2 is at an angle of 45-60 degrees to the stamping direction, and at an angle of 120-135 degrees to the draft surface 3. The draft surface 2 and the draft surface 3 are rounded by R3, with a size of 15-30mm; Design the draft surface 1, the draft surface 1 forms an angle A of 15-45 degrees with the stamping direction, and the angle B between the draft surface 1 and the draft surface 2 is controlled at 120-160 degrees; The drawing process modeling for controlling the slippage of the main ridge line is achieved by adjusting the draft surface 1, the draft surface 2, the draft surface 3, the angle A between the draft surface 1 and the stamping direction, the angle B between the draft surface 1 and the draft surface 2, the rounded angle R3 between the draft surface 2 and the draft surface 3, and the height difference H2 between the high point of the process modeling and the high point of the main ridge line; The height difference H1 between the main ridgeline and the fender ridgeline of the product is controlled within 10mm to balance the consistency of the slip line generated by the main ridgeline and the fender ridgeline; Check the slip line criteria, which is determined by the distance of the material sliding over the mold radius. First, run the simulation results to the end of the drawing simulation, and execute AutoForm / Results / Skid to evaluate the slip line: 1) No back and forth sliding; 2) Slip distance ≤ 1 / 2R angle arc; The contact state between the sheet metal and the high point of the main edge and the high point of the process shape during the forming process is simulated. The sheet metal first contacts the high point of the process shape by 8-15mm to eliminate the slip line generated by the sheet metal at the main edge.
2. A process for controlling the sliding of the main edge line of the side panel according to claim 1, characterized in that: The side outer panel product boundary line is extended outward in a direction tangent to the product, with a length of 10 mm.
3. A process for controlling the sliding of the main edge line of the side panel according to claim 1, characterized in that: The draft surface 3 forms an angle of 25 degrees with the stamping direction.
4. A process for controlling the sliding of the main edge line of the side panel according to claim 1, characterized in that: The height difference H2 between the high point of the process shape and the high point of the main edge line is 10mm.
5. The process for controlling the sliding of the main edge line of the side panel according to claim 1, characterized in that: The value of the chamfer R3 of the draft surface 2 and the draft surface 3 is 25mm.
Citation Information
Patent Citations
Die for researching stamping slip line forming rule and stamping test method
CN112620466A
Punch forming method for outer plate of aluminum hood
CN114192649A
Drawing die with sheet material strutting arrangement
CN206215773U
Process additional method for vehicle exterior panel
CN101398680A
Process method for solving deformation of periphery of doorknob of automotive door outer plate
CN102847849A