A method for processing a pole piece, a pole piece processing device and a negative pole piece
By pre-treating the electrode and depositing a passivation layer on the lithium layer surface, the problems of lithium replenishment difficulties in the negative electrode and impurities in the passivation layer are solved, thereby improving the performance of lithium-ion batteries.
Patent Information
- Application Number
- CN202210907470.0
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2022-07-29
- Publication Date
- 2024-11-05
- Estimated Expiration
- 2042-07-29
AI Technical Summary
In existing technologies, it is difficult to replenish lithium on the negative electrode sheet, and passivation layer impurities are easily generated on the surface of the lithium metal layer, which affects the performance of the lithium battery cell.
Impurities are removed by pre-treating the electrode sheets, forming a lithium layer, and a passivation layer is deposited on the surface of the lithium layer. Materials such as graphite or silicon that do not affect the performance of the battery cell are used.
It improves lithium replenishment, stabilizes the lithium layer, and enhances the initial efficiency and cycle life of lithium-ion batteries.
Smart Images

Figure CN115275087B_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the field of battery technology, and in particular to a pole piece processing method, pole piece processing equipment and a negative pole piece. Background Art
[0002] Lithium-ion batteries have low initial efficiency and low cycle life, which are usually solved by evaporating lithium or rolling lithium on the negative electrode. Because the negative electrode material on the surface of the negative electrode is porous graphite, a large amount of impurity gas and some other substances will be adsorbed in the porous graphite. During the lithium replenishment process, these impurities will be released, forming a strong resistance to the deposited lithium atoms, making the lithium evaporation process very difficult;
[0003] In addition, because lithium metal is too active and easily reacts with various substances in the air, a layer of passivation layer impurities is easily produced on the surface of the lithium metal layer after the negative electrode is replenished with lithium, which ultimately affects the performance of the lithium battery cell. Summary of the invention
[0004] One object of the present invention is to provide a pole piece processing method, which can solve the problem that it is very difficult to replenish lithium to the negative pole piece and the surface of the formed lithium metal layer is prone to generate passivation layer impurities and affect the performance of the lithium battery cell.
[0005] To achieve this object, the present invention adopts the following technical solutions:
[0006] A method for processing a pole piece, the pole piece comprising a base layer and a graphite active layer arranged on the base layer, the method for processing the pole piece comprising:
[0007] Pre-treating the pole piece to discharge impurities adsorbed in the graphite active layer;
[0008] Adding lithium to the pole piece to form a lithium layer on the surface of the graphite active layer;
[0009] A passivation layer is plated on the surface of the lithium layer.
[0010] As an optional solution of the above-mentioned pole piece processing method, the pretreatment includes at least one of heating the pole piece and bombarding the pole piece.
[0011] As an optional solution of the above-mentioned electrode piece processing method, during the pretreatment process, the environment where the electrode piece is located is continuously vacuumed.
[0012] As an optional solution of the above-mentioned pole piece processing method, when bombarding the pole piece, the front side and the back side of the pole piece are bombarded respectively.
[0013] As an optional solution of the above-mentioned pole piece processing method, in the pre-treatment process, the pole piece is first heated and then bombarded.
[0014] As an optional solution of the above-mentioned electrode processing method, the passivation layer is a graphite layer or a silicon layer.
[0015] Another object of the present invention is to provide a pole piece processing device that can solve the problem that it is very difficult to replenish lithium to the negative pole piece and the surface of the formed lithium metal layer is prone to produce passivation layer impurities and affect the performance of the lithium battery cell.
[0016] To achieve this object, the present invention adopts the following technical solutions:
[0017] A pole piece processing device comprises a pretreatment mechanism, a lithium replenishing chamber and a coating chamber which are connected in sequence; the pretreatment mechanism is used for pretreatment of the pole piece to discharge impurities adsorbed in the pole piece; the lithium replenishing chamber is used for replenishing lithium to the pole piece to form a lithium layer; the coating chamber is used for coating a passivation layer on the surface of the lithium layer.
[0018] As an optional solution of the above-mentioned electrode processing equipment, the pretreatment mechanism includes a connected heating chamber and an ion source chamber, and the heating chamber and the ion source chamber are both connected to a pump group, and the pump group is used to vacuum the heating chamber and the ion source chamber.
[0019] As an optional solution of the above-mentioned electrode processing equipment, a heating assembly is arranged in the heating chamber, and the heating assembly includes two heating plates arranged opposite to each other, and the electrode can pass between the two heating plates.
[0020] As an optional solution of the above-mentioned electrode piece processing equipment, an ion source assembly is arranged in the ion source chamber, and the ion source assembly includes two ion sources arranged opposite to each other, and the electrode piece can pass between the two ion sources.
[0021] Another object of the present invention is to provide a negative electrode plate, which can solve the problem in the technology that impurities in the passivation layer are easily generated on the surface of the lithium metal layer of the negative electrode plate, thereby affecting the performance of the lithium battery cell.
[0022] To achieve this object, the present invention adopts the following technical solutions:
[0023] A negative electrode plate comprises a base layer, a graphite active layer arranged on the surface of the base layer, a lithium layer arranged on the surface of the graphite active layer, and a passivation layer arranged on the surface of the lithium layer. The negative electrode plate is manufactured by the above-mentioned plate processing method.
[0024] Beneficial effects of the present invention:
[0025] In the electrode processing method provided by the present invention, gas impurities adsorbed in the electrode are discharged through pretreatment, so as to avoid the difficulty of lithium atom deposition caused by the release of gas impurities during the lithium replenishment process, which is conducive to improving the lithium replenishment effect. By plating a passivation layer on the surface of the lithium layer, it is possible to avoid the lithium layer from contacting the air and generating a passivation impurity layer;
[0026] In the present invention, the passivation layer material is silicon, graphite or other materials that do not affect the performance of the battery cell, so as to avoid affecting the performance of the lithium battery cell due to the addition of the passivation layer.
[0027] The pole piece processing equipment provided by the present invention can adopt the pole piece processing method mentioned above, and can ensure the performance of the lithium battery cell.
[0028] The lithium layer in the negative electrode plate provided by the present invention is stable, and after being used in a lithium-ion battery, it is beneficial to improve the initial efficiency of the battery and extend the cycle life of the battery cell. BRIEF DESCRIPTION OF THE DRAWINGS
[0029] Figure 1 It is a flow chart of the pole piece processing method provided by the present invention;
[0030] Figure 2 It is a partial structural schematic diagram of the electrode processing equipment provided by the present invention;
[0031] Figure 3 It is a schematic diagram of the structure of the negative electrode plate provided by the present invention.
[0032] In the figure:
[0033] 1. Heating chamber; 2. Ion source chamber; 3. Heating plate; 4. Ion source; 5. Guide roller; 6. Pump group; 10. Pole piece; 101. Base layer; 102. Graphite active layer; 20. Lithium layer; 30. Passivation layer. DETAILED DESCRIPTION
[0034] The present invention will be further described in detail below in conjunction with the accompanying drawings and embodiments. It is to be understood that the specific embodiments described herein are only used to explain the present invention, rather than to limit the present invention. It should also be noted that, for ease of description, only parts related to the present invention, rather than all structures, are shown in the accompanying drawings.
[0035] In the description of the present invention, unless otherwise clearly specified and limited, the terms "connected", "connected", and "fixed" should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection or an electrical connection; it can be a direct connection or an indirect connection through an intermediate medium, it can be the internal connection of two elements or the interaction relationship between two elements. For ordinary technicians in this field, the specific meanings of the above terms in the present invention can be understood according to specific circumstances.
[0036] In the present invention, unless otherwise clearly specified and limited, a first feature being "above" or "below" a second feature may include that the first and second features are in direct contact, or may include that the first and second features are not in direct contact but are in contact through another feature between them. Moreover, a first feature being "above", "above" and "above" a second feature includes that the first feature is directly above and obliquely above the second feature, or simply indicates that the first feature is higher in level than the second feature. A first feature being "below", "below" and "below" a second feature includes that the first feature is directly below and obliquely below the second feature, or simply indicates that the first feature is lower in level than the second feature.
[0037] In the description of this embodiment, the terms "upper", "lower", "right", etc., directions or positional relationships are based on the directions or positional relationships shown in the drawings, and are only for the convenience of description and simplification of operation, rather than indicating or implying that the device or element referred to must have a specific direction, be constructed and operated in a specific direction, and therefore cannot be understood as limiting the present invention. In addition, the terms "first" and "second" are only used to distinguish in the description and have no special meaning.
[0038] Embodiment 1
[0039] The pole piece 10 includes a copper foil and a graphite active layer 102 coated on the copper foil. Since graphite is a porous material, it is easy to absorb gas impurities or other substances, which affects the lithium replenishment effect of the pole piece 10.
[0040] In order to improve the lithium replenishment effect of the electrode 10, this embodiment provides a method for processing the electrode, such as Figure 1 As shown, the pole piece 10 is first pretreated to discharge the impurities adsorbed in the pole piece 10; then lithium is added to the pole piece 10 to form a lithium layer 20 on the surface of the pole piece 10. By pre-treating the pole piece 10 to discharge the gas impurities and other substances adsorbed in the pole piece 10, and then performing the lithium addition operation, the difficulty of lithium metal adhering to the surface of the pole piece 10 during lithium addition can be reduced, which is beneficial to improving the lithium addition effect of the pole piece 10, and is beneficial to improving the initial efficiency of the lithium-ion battery and extending the cycle life of the battery cell.
[0041] Since lithium metal is relatively active, lithium is easily reacted with various substances in the air when it comes into direct contact with the air, resulting in the formation of a passivation layer of impurities on the surface of the lithium layer 20, which ultimately affects the performance of the lithium battery cell. In order to avoid the formation of a passivation impurity layer on the surface of the lithium layer 20, after lithium is replenished to the pole piece 10, a passivation layer 30 that does not affect the performance of the battery cell is plated on the surface of the lithium layer 20. The passivation layer 30 can protect the lithium layer 20, prevent the lithium layer 20 from reacting with substances in the air, and avoid the generation of passivation layer impurities. The material of the passivation layer 30 can be a material that does not affect the performance of the battery cell and can avoid the effect of the lithium layer 20 reacting with substances in the air, such as silicon or graphite. In the present embodiment, preferably, the material of the passivation layer 30 is graphite, so that the passivation layer 30 is consistent with the material of the graphite active layer 102 in the pole piece 10, which will not affect the performance of the lithium battery cell.
[0042] In order to discharge the gas impurities in the graphite active layer 102, the pole piece 10 needs to be pretreated, and the pretreatment includes but is not limited to various pretreatment methods of bombarding the pole piece 10 such as heat treatment, electron beam treatment, etc., for example, at least one of heat treatment and / or electron beam bombardment treatment.
[0043] In this embodiment, the pretreatment includes heating the pole piece 10. By heating the pole piece 10, the gas impurities adsorbed in the graphite can be automatically detached by the heat, thereby preparing for the subsequent lithium replenishment process.
[0044] In order to prevent the gas impurities that are automatically detached by heat from being adsorbed by the graphite material again, when the pole piece 10 is heated, the environment where the pole piece 10 is located is continuously evacuated so that the detached gas impurities can be discharged in time to prevent the gas impurities from being adsorbed by the graphite material again.
[0045] In order to further improve the removal effect of gas impurities in the pole piece 10, in this embodiment, the pretreatment also includes bombarding the pole piece 10. Specifically, after heating the pole piece 10, the ion beam generated by the ion source 4 bombards the pole piece 10, which can further discharge the impurities in the pole piece 10 and create a good surface condition of the pole piece 10 for subsequent lithium replenishment.
[0046] In this embodiment, preferably, the electrode 10 is heated first so that the gas impurities in the graphite that are easier to be discharged are separated by heat. This method can perform rough processing on the graphite layer 102 to discharge the impurity gas in the graphite layer 102. Thereafter, the electrode 10 is bombarded with an ion beam. This method can perform fine processing on the graphite layer 102 to further discharge other impurities such as gas and solids remaining on the surface of the electrode 10, thereby improving the impurity removal effect and thus improving the lithium replenishment effect.
[0047] Furthermore, in order to prevent the discharged gas impurities from being adsorbed by graphite again when the ion beam bombards the pole piece 10, the environment of the pole piece 10 is continuously evacuated during the ion beam bombardment to remove the discharged gas impurities and prevent the gas impurities from contacting the pole piece 10 again.
[0048] Furthermore, when the pole piece 10 is bombarded by the ion beam, the ion beam bombards the front side and the back side of the pole piece 10 respectively, so as to further improve the gas impurity discharge effect.
[0049] In some embodiments, the pretreatment of the pole piece 10 may only include heating or bombarding the pole piece. When bombarding the pole piece 10, an electron beam or a laser beam may be used to bombard the pole piece 10 for pretreatment.
[0050] In this embodiment, lithium replenishment for the electrode 10 can be performed by evaporation or rolling. The passivation layer 30 can be plated on the surface of the lithium layer 20 by magnetron sputtering or evaporation coating. The evaporation coating methods include electron beam evaporation, resistance evaporation and high-frequency induction thermal evaporation.
[0051] Embodiment 2
[0052] The present embodiment provides a pole piece processing device, which can adopt the pole piece processing method in the first embodiment. Among them, the pole piece processing device includes a pretreatment mechanism, a lithium replenishing chamber and a coating chamber which are connected in sequence. When the pole piece 10 is processed, it first enters the pretreatment mechanism for pretreatment to discharge gas impurities or other substances adsorbed in the pole piece 10. Afterwards, the pole piece 10 enters the lithium replenishing chamber and the coating chamber in sequence, and the lithium replenishing operation is performed in the lithium replenishing chamber, so as to form a lithium layer 20 on the surface of the pole piece 10, and the passivation layer 30 is plated in the coating chamber. The passivation layer 30 protects the lithium layer 20 to prevent the lithium layer 20 from contacting with the air and generating a passivation impurity layer.
[0053] Specifically, Figure 2 As shown, the pretreatment mechanism includes a connected heating chamber 1 and an ion source chamber 2, and the heating chamber 1 and the ion source chamber 2 are both connected to a pump group 6. The pump group 6 is used to evacuate the heating chamber 1 and the ion source chamber 2 to prevent the gas impurities discharged from the electrode 10 from being adsorbed by the electrode 10 again, thereby improving the pretreatment effect on the electrode 10.
[0054] In this embodiment, both the lithium replenishment chamber and the coating chamber use vacuum coating to replenish lithium and coat the passivation layer 30, so that the pole piece 10 will no longer come into contact with the air after pretreatment, which can prevent the graphite active layer 102 from absorbing impurities again during the lithium replenishment process.
[0055] In order to improve the heating effect of the electrode 10 and make the gas impurities discharged more thoroughly, a heating assembly is provided in the heating chamber 1, and the heating assembly includes two heating plates 3 arranged opposite to each other, and the electrode 10 can pass between the two heating plates 3. By controlling the heating power of the heating plates 3 and the movement speed of the electrode 10 relative to the heating plates 3, the electrode 10 can be evenly heated at all places, which is conducive to making the gas impurities discharged more thoroughly.
[0056] Optionally, a plurality of heating components are arranged in the heating chamber 1, and the pole piece 10 passes through the plurality of heating components in sequence, which can further promote the discharge of gas impurities.
[0057] In order to enable the electrode 10 to be flattened when passing between the two heating plates 3, a guide roller 5 is provided in the heating chamber 1. The electrode 10 passes around the guide roller 5 and moves and is tensioned along a preset trajectory under the action of the guide roller 5 to ensure that the electrode 10 remains flattened and heated, which is beneficial to improving the discharge effect of gas impurities.
[0058] In this embodiment, an ion source assembly is arranged in the ion source chamber 2, and the ion source assembly includes two ion sources 4 arranged opposite to each other. The electrode 10 can pass between the two ion sources 4, so that the front and back sides of the electrode 10 can be bombarded by the ion beam emitted by the ion source 4, so that the gas impurities or other substances adsorbed in the electrode 10 can be better discharged, thereby avoiding the electrode 10 from overflowing due to gas impurities when replenishing lithium and affecting the lithium replenishment effect.
[0059] Optionally, multiple groups of ion source components can be provided as needed to ensure that the surface condition of the pole piece 10 before coating reaches an excellent state.
[0060] Optionally, a plurality of guide rollers 5 are provided in the ion source chamber 2 , and the plurality of guide rollers 5 are used to tension and guide the pole piece 10 to move, so as to improve the discharge effect of gas impurities.
[0061] Embodiment 3
[0062] This embodiment provides a negative electrode plate, which can be prepared using the plate processing method in the first embodiment and the plate processing equipment in the second embodiment.
[0063] Specifically, Figure 3As shown, the negative electrode plate includes a base layer 101, a graphite active layer 102 disposed on both sides of the base layer 101, a lithium layer 20 disposed on the surface of the graphite active layer 102, and a passivation layer 30 disposed on the surface of the lithium layer 20, wherein the base layer 101 may be a copper foil. The graphite active layer 102 may be coated on the surface of the base layer 101, the lithium layer 20 may be formed by evaporation or rolling, and the passivation layer 30 may be formed by magnetron sputtering or evaporation coating. Compared with the graphite active layer 102, the passivation layer 30 formed by vacuum coating has a dense film structure and can provide good protection for the lithium layer 20.
[0064] Obviously, the above embodiments of the present invention are merely examples for clearly illustrating the present invention, and are not intended to limit the embodiments of the present invention. For those skilled in the art, various obvious changes, readjustments and substitutions can be made without departing from the protection scope of the present invention. It is not necessary and impossible to list all the embodiments here. Any modifications, equivalent substitutions and improvements made within the spirit and principles of the present invention should be included in the protection scope of the claims of the present invention.
Claims
1. A method for processing a pole piece, wherein the pole piece (10) comprises a base layer (101) and a graphite active layer (102) arranged on both sides of the base layer (101). It is characterized in that The pole piece processing method comprises: Pre-treating the pole piece (10) to discharge impurities adsorbed in the graphite active layer (102); Wherein, the pretreatment is performed in a pretreatment mechanism, and the pretreatment mechanism is used to pretreatment the pole piece (10) to discharge impurities adsorbed in the pole piece (10); The pretreatment mechanism comprises a heating chamber (1) and an ion source chamber (2) which are connected to each other, wherein the heating chamber (1) and the ion source chamber (2) are both connected to a pump group (6), and the pump group (6) is used to evacuate the heating chamber (1) and the ion source chamber (2); A heating assembly is arranged in the heating chamber (1), the heating assembly comprising at least one set of two heating plates (3) arranged opposite to each other, and the electrode (10) can pass between the two heating plates (3); An ion source assembly is arranged in the ion source chamber (2), the ion source assembly comprising at least one group of two ion sources (4) arranged opposite to each other, and the pole piece (10) can pass between the two ion sources (4); During the pretreatment process, the environment in which the pole piece (10) is located is continuously evacuated; In the pretreatment process, the pole piece (10) is first heated, and then the pole piece (10) is bombarded; and when bombarding the pole piece (10), the front side and the back side of the pole piece (10) are bombarded respectively; Adding lithium to the pole piece (10) to form a lithium layer (20) on the surface of the graphite active layer (102); A passivation layer (30) is plated on the surface of the lithium layer (20).
2. The electrode processing method according to claim 1, It is characterized in that The passivation layer (30) is a graphite layer or a silicon layer.
3. A pole piece processing device, used to implement the pole piece processing method according to any one of claims 1 to 2, It is characterized in that The invention comprises a pretreatment mechanism, a lithium replenishing chamber and a coating chamber which are connected in sequence; the pretreatment mechanism is used for pretreatment of a pole piece (10) to discharge impurities adsorbed in the pole piece (10); the lithium replenishing chamber is used for replenishing lithium to the pole piece (10) to form a lithium layer (20); and the coating chamber is used for coating a passivation layer (30) on the surface of the lithium layer (20).
4. A negative electrode sheet, It is characterized in that The negative electrode comprises a base layer (101), a graphite active layer (102) arranged on both sides of the base layer (101), a lithium layer (20) arranged on the surface of the graphite active layer (102), and a passivation layer (30) arranged on the surface of the lithium layer (20), wherein the negative electrode plate is manufactured by the plate processing method described in claim 1.