A method for evaluating the aging state of silicone rubber insulators by combining macroscopic and microscopic hydrophobic properties
By combining macro and micro hydrophobic performance evaluation methods, using online detection and micro simulation databases, the aging state of silicone rubber insulators in the railway system is evaluated, which solves the problems of traditional detection being time-consuming and ineffective, and achieves efficient and effective inspection of insulators. Accurate aging performance assessment meets the needs for efficient maintenance in high-speed railway environments.
Patent Information
- Application Number
- CN202210930853.X
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2022-08-04
- Publication Date
- 2024-10-29
- Estimated Expiration
- 2042-08-04
AI Technical Summary
The aging performance testing of silicone rubber insulators in railway systems has the problems of long time consumption, high cost and average online monitoring effect, making it difficult to meet the needs of efficient maintenance in high-speed railway environments.
Combining macro and micro hydrophobic performance evaluation methods, through online detection and micro simulation database, the static contact angle and Si-CH3 quantity changes of the insulator are evaluated, the degree of hardness deterioration is calculated, and the aging state of the insulator is accurately evaluated.
It achieves efficient and accurate aging performance evaluation of silicone rubber insulators, reduces maintenance costs, improves maintenance efficiency, and can more accurately judge the aging degree and service life of insulators.
Smart Images

Figure CN115326644B_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the field of aging assessment of silicone rubber insulators, and in particular to a method for assessing the aging state of silicone rubber insulators by combining macroscopic and microscopic hydrophobic properties. Background Art
[0002] According to the actual working conditions of my country's railway transportation system, the working environment of the insulators in the traction power supply system is relatively harsh. The high-voltage insulators on the roof work under the "pantograph-contact network" system (pantograph-network system). The metal dust generated by the high-speed sliding friction of the pantograph-network will scatter and adsorb on the surface of the high-voltage insulators on the roof, causing the electrical strength of the insulators to be significantly reduced. The amount of coal ash and dust along the lines in heavily polluted areas is greater, and the problem of pollution accumulation on insulators is more prominent. With the opening and operation of my country's medium and long-distance high-speed railways (such as the Lanzhou-Xinjiang Line and the Harbin-Dalian Line), the high-voltage insulators on the roofs of high-speed trains must withstand changes in various climatic environments along the lines, which puts higher requirements on their environmental adaptability. Due to the particularity of some structures in the railway system, the structural size of the insulators is limited, and the trains are also faced with the impact of high-speed airflow during operation. Therefore, compared with insulators in other power systems, the insulators used in the railway system have higher performance requirements.
[0003] Compared with power system lines, arm insulators in railway systems also face the important problem of high maintenance difficulty. Trains frequently pass through electrified railway lines, and the maintenance and cleaning of insulators can only be carried out within a limited time, and the maintenance time is short; on the other hand, my country's high-speed railways mostly use viaduct structures, the lines are erected high, and are limited by on-site conditions, making insulator maintenance difficult.
[0004] Therefore, the study of the aging performance of synthetic insulators in railway systems is of great significance. The existing different aging performance detection methods have achieved results, but they all have limitations. The traditional offline detection method requires the railway power supply system to be shut down for sampling, which is time-consuming, high in manpower and material costs, and affects production efficiency and economic benefits. At present, online monitoring methods (including 6C and its inspection vehicles) can only measure some basic indicators and can only briefly analyze the performance of insulators. They can find obvious faults but cannot evaluate them, and the evaluation effect on aging is average.
[0005] In view of the particularity of the railway system, it is urgent to design an online monitoring system for insulator aging performance detection, and at the same time find a synthetic insulator aging performance evaluation technology that can more efficiently and accurately evaluate the insulator aging performance and aging degree, reduce maintenance costs, and improve maintenance efficiency.
[0006] All changes in the macroscopic properties of materials are based on changes in microscopic parameters. Studies have shown that the static contact angle of silicone rubber used in wrist insulators is positively correlated with the amount of Si-CH3, and the elongation at break is negatively correlated with the ratio of the amount of Si-O-Si to Si-C. With the development of computer technology, simulation can be used to explore the microscopic mechanism of materials, greatly reducing experimental costs and cycles. Summary of the invention
[0007] The purpose of the present invention is to propose a method for evaluating the aging state of silicone rubber insulators by combining macroscopic and microscopic hydrophobic properties, and to evaluate the insulators more accurately by combining online monitoring and a microscopic simulation database.
[0008] The technical solution to achieve the purpose of this program is as follows:
[0009] A method for evaluating the aging state of silicone rubber insulators by combining macroscopic and microscopic hydrophobic properties, comprising:
[0010] Step 1: Based on online detection, the degradation of hydrophobicity is evaluated. The sub-steps are as follows:
[0011] 1) According to the type of the arm insulator being tested, measure the static contact angle A0 of the new insulator;
[0012] 2) Online detection of the current static contact angle A of the insulator;
[0013] 3) The degree of hydrophobicity degradation of the insulator is:
[0014]
[0015] Step 2: Record the actual temperature T2, electric field strength E2, and humidity H2 during the test;
[0016] Step 3: Find the best matching case in the micro-simulation database based on the recorded temperature, electric field strength, and humidity, and obtain the change in hardness. The sub-steps are as follows:
[0017] 1) Establish a micro-simulation database, the steps are as follows:
[0018] (1) Build a silicone rubber model on the Materials Studio platform and determine the initial amount of Si-CH3 and the ratio of Si-C to Si-O-Si, denoted as N 0 Si-CH3 、N 0Si-C / Si-O-Si , and import the model into Lammps software;
[0019] (2) Set the temperature T1 in the interval [273K, 1000K], with a minimum interval of 10K; set the electric field strength E1 in the interval [0, 30kV / cm], with a minimum interval of 0.1kV / cm; set the humidity H1 in the interval [1%, 90%], with a minimum interval of 1%;
[0020] (3) The above condition parameters are randomly combined with different values according to the minimum interval within the interval, and each combination is simulated 100 times, with a simulation time of 30 ps. The change of the amount of Si-CH3 over time is counted, where the amount of Si-CH3 is the result of taking the average value of 100 sets of simulation data;
[0021] 2) Find the case that best matches the conditions at the time of detection in the microscopic database, the method is as follows:
[0022] Calculated according to the following formula, the closer K is to 0, the higher the matching degree:
[0023]
[0024] (2) In the formula, x 1i 、x 2i are the i-th element in vectors X1 and X2 respectively; X1 is the conditional vector in the database,
[0025] X2 is the conditional vector during detection; define X1 = [T1, E1, H1] T ; X2 = [T2, E2, H2] T ;
[0026] 3) Obtain the degree of hardness degradation, set as I B , calculated according to the following formula:
[0027]
[0028]
[0029] In formulas (3) and (4), N Si-C / Si-O-Si It represents the ratio of Si-C to Si-O-Si in the simulation model at time t. Similarly, N Si-O-Si / Si-C It represents the ratio of the number of Si-O-Si to Si-C in the simulation model at time t; (3) where α, β, and γ are the weights of temperature, electric field strength, and humidity, respectively, α = 0.632, β = 0.214, and γ = 0.154; T, E, and H represent the normalized temperature, electric field strength, and humidity:
[0030]
[0031]
[0032]
[0033] In formulas (5), (6), and (7), T0 is 298K, E0 is 0.2kV / cm, and H0 is 20%. In formula (3), t is the simulation time, which is obtained as follows:
[0034] According to the hydrophobicity degradation degree obtained in step 1 (3), the amount of Si-CH3 in the insulator microscopic model at time t can be obtained by the following formula:
[0035]
[0036]
[0037] In formulas (8) and (9), N 0 Si-CH3 is the initial amount of Si-CH3, N Si-CH3 is the amount of Si-CH3 at time t; Based on the amount of Si-CH3 and the variation of Si-CH3 with time counted in sub-step 1) of step 3 (3), t can be obtained;
[0038] Step 4: Comprehensively evaluate the aging of the insulators based on the degradation of their hydrophobicity and hardness as follows:
[0039] When I A ,I B When both are greater than or equal to 50%, the insulator is in a benign usable stage; when only one value is less than 50%, the insulator is seriously aged and should be replaced or repaired in time; when both are less than 35%, the insulator should be replaced immediately.
[0040] Compared with the prior art, the advantages of the present invention are as follows:
[0041] On the basis of traditional online detection, the aging degree of the insulator hardness performance can be obtained through the micro-simulation database, which more comprehensively reflects the overall aging of the insulator and realizes the evaluation of the insulator aging performance. Compared with traditional macro experiments, the use of micro-simulation to build a database not only saves cost and time, but also achieves higher accuracy through a large number of simulations. BRIEF DESCRIPTION OF THE DRAWINGS
[0042] Figure 1 Simulation model diagram of silicone rubber
[0043] Figure 2 The normalized Si-CH3 quantity changes with time DETAILED DESCRIPTION
[0044] The specific implementation of the present invention is further described below in conjunction with the accompanying drawings and examples. The following examples are only used to more clearly illustrate the technical solution of the present invention, and cannot be used to limit the protection scope of the invention.
[0045] A method for evaluating the aging state of a silicone rubber insulator by combining macroscopic and microscopic hydrophobic properties comprises the following steps:
[0046] Step 1: Based on online detection, the degradation of hydrophobicity is evaluated. The sub-steps are as follows:
[0047] 1) According to the type of the arm insulator being tested, measure the static contact angle A0 of the new insulator, A0 = 110°;
[0048] 2) Online detection of the current static contact angle A of the insulator, A = 90°;
[0049] 3) The degree of hydrophobicity degradation of the insulator is:
[0050]
[0051] Step 2: Record the actual temperature T1, electric field strength E1, and humidity H1 during the test; T1 = 500K, E1 = 0.5KV / cm, H1 = 30%;
[0052] Step 3: Find the best matching case in the micro-simulation database based on the recorded temperature, electric field strength, and humidity, and obtain the change in hardness. The sub-steps are as follows:
[0053] 1) Establish a micro-simulation database, the steps are as follows:
[0054] (1) Build a silicone rubber model on the Materials Studio platform, such as Figure 1 Determine the initial amount of Si-CH3 and the ratio of Si-C to Si-O-Si, denoted as N 0 Si-CH3 、N 0Si-C\Si-O-Si In this case, N 0 Si-CH3 =90, N 0Si-C\Si-O-Si =0.46. The model was imported into Lammps software;
[0055] (2) Set the temperature T1 in the interval [273K, 1000K], with a minimum interval of 10K; set the electric field strength E1 in the interval [0, 30kV / cm], with a minimum interval of 0.1kV / cm; set the humidity H1 in the interval [1%, 90%], with a minimum interval of 1%;
[0056] (3) The above condition parameters are randomly combined with different values according to the minimum interval within the interval, and each combination is simulated 100 times, with a simulation time of 30 ps. The change of the amount of Si-CH3 over time is counted, where the amount of Si-CH3 is the result of taking the average value of 100 sets of simulation data;
[0057] 2) Find the case that best matches the conditions at the time of detection in the microscopic database, the method is as follows:
[0058] Calculated according to the following formula, the closer K is to 0, the higher the matching degree:
[0059]
[0060] In the formula, x 1i 、x 2i are the i-th element in vectors X1 and X2 respectively; X1 is the conditional vector in the database, and X2 is the conditional vector during detection; define X1 = [T1, E1, H1] T ; X2 = [T2, E2, H2] T In this case, the conditional vector for testing is X2 = [500K, 0.5KV / cm, 30%] T ;
[0061] 3) Obtain the degree of hardness degradation, set as I B , calculated according to the following formula:
[0062]
[0063]
[0064] In formulas (3) and (4), N Si-C / Si-O-Si It represents the ratio of Si-C to Si-O-Si in the simulation model at time t. Similarly, N Si-O-Si / Si-C It represents the ratio of the number of Si-O-Si to Si-C in the simulation model at time t; (3) where α, β, and γ are the weights of temperature, electric field strength, and humidity, respectively, α = 0.632, β = 0.214, and γ = 0.154; T, E, and H represent the normalized temperature, electric field strength, and humidity. T is in Kelvin, T = 273.15 + T(t), and the unit of T(t) is Celsius.
[0065]
[0066]
[0067]
[0068] In formulas (5), (6), and (7), T0 is 298K, E0 is (0.2kV / cm), and H0 is (20%), then T≈1.68,
[0069] E = 2.5, H = 1.5;
[0070] (3) Where t is the simulation time, which can be obtained as follows:
[0071] According to the hydrophobicity degradation degree obtained in step 1 (3), the amount of Si-CH3 in the insulator microscopic model at time t can be obtained by the following formula:
[0072]
[0073]
[0074] In formulas (8) and (9), N 0 Si-CH3 is the initial amount of Si-CH3, N Si-CH3 is the amount of Si-CH3 at time t, N Si-CH3 ≈73; Based on the amount of Si-CH3 and the change of Si-CH3 with time counted in sub-step 1) of step 3 (3), t can be obtained, Figure 2 This is the relationship between the amount of Si-CH3 and time after normalization. It can be obtained that t = 11.98ps, so the degree of hardness degradation in this case is 0.67;
[0075] Step 4: Comprehensively evaluate the aging of the insulators based on the degradation of their hydrophobicity and hardness as follows:
[0076] When I A ,I B When both are greater than or equal to 50%, the insulator is in a benign usable stage; when only one value is less than 50%, the insulator is seriously aged and should be replaced or repaired in time; when both are less than 35%, the insulator should be replaced immediately. Therefore, the insulator in this case is in a benign usable stage and does not need to be replaced.
Claims
1. A method for evaluating the aging state of silicone rubber insulators by combining macroscopic and microscopic hydrophobic properties, characterized in that: Include: Step 1: Based on online detection, the degradation of hydrophobicity is evaluated. The sub-steps are as follows: 1) According to the type of the arm insulator being tested, measure the static contact angle A0 of the new insulator; 2) Online detection of the current static contact angle A of the insulator; 3) The degree of hydrophobicity degradation of the insulator is: Step 2: Record the actual temperature T2, electric field strength E2, and humidity H2 during the test; Step 3: Find the best matching case in the micro-simulation database based on the recorded temperature, electric field strength, and humidity, and obtain the change in hardness. The sub-steps are as follows: 1) Establish a micro-simulation database, the steps are as follows: (1) Build a silicone rubber model on the Materials Studio platform and determine the initial amount of Si-CH3 and the ratio of Si-C to Si-O-Si, denoted as N 0Si-CH3 、N 0Si-C / Si-O-Si , and import the model into Lammps software; (2) Set the temperature T1 in the interval [273K, 1000K], with a minimum interval of 10K; set the electric field strength E1 in the interval [0, 30kV / cm], with a minimum interval of 0.1kV / cm; set the humidity H1 in the interval [1%, 90%], with a minimum interval of 1%; (3) The above condition parameters are randomly combined with different values according to the minimum interval within the interval, and each combination is simulated 100 times, with a simulation time of 30 ps. The change of the amount of Si-CH3 over time is counted, where the amount of Si-CH3 is the result of taking the average value of 100 sets of simulation data; 2) Find the case that best matches the conditions at the time of detection in the microscopic database, the method is as follows: Calculated according to the following formula, the closer K is to 0, the higher the matching degree: (2) In the formula, x 1i 、x 2i are the i-th element in vectors X1 and X2 respectively; X1 is the conditional vector in the database, and X2 is the conditional vector during detection; define X1 = [T1, E1, H1] T , X2=[T2,E2,H2] T ; 3) Obtain the degree of hardness degradation, set as I B , calculated according to the following formula: In formulas (3) and (4), N Si-C / Si-O-Si It represents the ratio of Si-C to Si-O-Si in the simulation model at time t. Similarly, N Si-O-Si / Si-C It represents the ratio of the number of Si-O-Si to Si-C in the simulation model at time t; (3) where α, β, and γ are the weights of temperature, electric field strength, and humidity, respectively, α = 0.632, β = 0.214, and γ = 0.154; T, E, and H represent the normalized temperature, electric field strength, and humidity: In formulas (5), (6), and (7), T0 is 298K, E0 is 0.2kV / cm, and H0 is 20%. In formula (3), t is the simulation time, which is obtained as follows: According to the hydrophobicity degradation degree obtained in sub-step 3) of step 1, the amount of Si-CH3 in the insulator microscopic model at time t can be obtained by the following formula: In formulas (8) and (9), N 0Si-CH3 is the initial amount of Si-CH3, N Si-CH3 is the amount of Si-CH3 at time t; t can be obtained based on the amount of Si-CH3 and the change of Si-CH3 with time counted in (3) of sub-step 1) of step 3; Step 4: Comprehensively evaluate the aging of the insulators based on the degradation of their hydrophobicity and hardness as follows: When I A ,I B When both are greater than or equal to 50%, the insulator is in a benign usable stage; when only one value is less than 50%, the insulator is seriously aged and should be replaced or repaired in time; when both are less than 35%, the insulator should be replaced immediately.
Citation Information
Patent Citations
Multi-dimensional parameter assessment method of aging degree of running composite insulator
CN106771765A
Evaluation method for aging state of composite insulator and terminal equipment
CN108872059A
Cited By
GIS basin-type insulator operation state evaluation method and system