A titanium alloy rear base shaping method and shaping tooling
By using a central positioning cylinder, annular calibration block and adjustment components, combined with pickling and stress-removing annealing steps, the problems of inaccurate size and poor coaxiality during the calibration process of the titanium alloy are solved. Accurate calibration and material performance improvements have been achieved.
Patent Information
- Application Number
- CN202211058022.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2022-08-30
- Publication Date
- 2024-11-19
- Estimated Expiration
- 2042-08-30
AI Technical Summary
During the calibration process, the back base of the titanium alloy is prone to inaccurate size and poor coaxiality due to deformation. The existing thermal creep calibration methods cannot accurately adjust the deformation of the casting, which is prone to surface crack defects, affecting the performance of the material.
Using a calibration tool including a central positioning cylinder, annular calibration block and adjustment components, the alpha layer is removed by acid washing to form a reference hole, and the small-end ring is used as a calibration reference to accurately correct the deformation size of the large-end ring and Coaxiality, combined with stress removal annealing step, eliminate internal stress and reduce the limitations of calibrated tooling materials.
Accurate calibration of the rear base of the titanium alloy, ensuring the roundness of the large-end ring and the coaxiality of the small-end ring, avoiding surface crack defects, improving the fatigue and impact performance of the material, and reducing calibration cost of shaped tooling.
Smart Images

Figure CN115464008B_ABST
Abstract
Description
Technical Field
[0001] The invention belongs to the technical field of titanium alloy processing, and in particular relates to a shaping method and shaping tooling for a titanium alloy rear base. Background Art
[0002] Titanium alloys are widely used in the field of aerospace and aero-engine fluid supply due to their high specific strength, good heat resistance, good low temperature resistance and excellent corrosion resistance. The titanium alloy rear base is a structural part of an aerospace engine. It is a simple casting made of titanium alloy casting. The minimum wall thickness of the casting is 3mm, the wall thickness of the large end ring is 6mm, and the outer diameter is more than 500mm. The contour size of the large end ring of the casting is relatively large and the wall thickness difference of the casting is relatively large. Due to the influence of factors such as casting stress, the large end ring of the casting is very easy to deform; the wall thickness of the small end ring of the casting is more than 20mm, the outer diameter of the ring is less than 100mm, the small end ring is relatively small, the wall thickness is large, the deformation resistance is strong, and the ring is not easy to form; the outer circle of the large end ring of the casting and the inner hole of the small end ring are relatively high, and they are all single-sided processing areas. Castings with large deformation cannot guarantee the processing volume and casting wall thickness. The large end ring of the casting has black skin leakage after processing due to local deformation.
[0003] In the prior art, the shaping method for titanium alloy ring parts mainly adopts thermal creep shaping. The thermal creep shaping mold material is made of heat-resistant steel and graphite. It is heated to more than 900 degrees in a vacuum furnace. A heavy object is placed in the upper mold. Under the action of gravity, the casting creeps to achieve the required size and shape of the casting. The shaping equipment and shaping materials have relatively high requirements. The deformation size of the casting cannot be accurately adjusted during the shaping process, and the coaxiality size requirements of the casting cannot be guaranteed. Since the α-layer brittle and hard phase on the surface of the casting is not removed, the internal stress generated by the shaping will cause crack defects on the surface of the casting. Repairing the defects will cause a certain degree of scrapping of the casting. Summary of the invention
[0004] The object of the present invention is to provide a shaping method and shaping tool for a titanium alloy rear base, so as to at least solve part of the above-mentioned technical problems.
[0005] The first aspect of the present invention provides a profiling tool for a titanium alloy rear base casting, comprising:
[0006] A center positioning cylinder, wherein the inner and outer circumferences of the center positioning cylinder are coaxially arranged;
[0007] An annular profiling block, which is sleeved on one end of the center positioning cylinder and is provided with a plurality of radial through holes;
[0008] The adjustment component comprises a profiling bolt and a locking nut. The profiling bolt is inserted into the through hole, and the locking nut is sleeved on the profiling bolt and is suitable for adjusting the depth of the profiling bolt.
[0009] Furthermore, the shaping tooling for the titanium alloy rear base casting provided by the present invention may also have the following additional technical features:
[0010] In a specific embodiment of the present invention, it also includes a plurality of reinforcing ribs, which are evenly distributed along the radial direction of the center positioning tube, and one end of the reinforcing ribs is connected to the outer wall of the center positioning tube, and the other end is connected to the inner wall of the annular correction block.
[0011] In a specific embodiment of the present invention, the center positioning cylinder, the annular shaping block and the reinforcing ribs are all made of No. 45 steel.
[0012] In a specific embodiment of the present invention, 9 through holes are evenly distributed on the annular shaping block, and one shaping bolt is inserted into each of the through holes.
[0013] Another aspect of the present invention provides a method for adjusting the shape of a titanium alloy rear base casting, wherein the titanium alloy rear base casting comprises a large end ring, a small end ring, and a shell connecting the large end ring and the small end ring, and the method comprises the following steps:
[0014] Pickling of castings: pickling the castings with an acid solution to remove the surface α layer of the castings;
[0015] Casting rough reference processing: rough processing is performed on the inner hole of the small end ring to form a reference hole;
[0016] Casting calibration: Take any of the calibration tools described above, and make the center positioning cylinder of the calibration tool and the reference hole of the casting have the same diameter as the base hole, and then adjust the locking nut to drive the calibration bolt to calibrate the large end ring;
[0017] Stress relief annealing of castings: Place the casting and the shaping tool in a heating device and wrap them with titanium chips, heat to 500-550°C, keep warm for 1-2 hours and then cool to room temperature; take out the casting and the shaping tool and remove the shaping tool to obtain the shaped titanium alloy rear base.
[0018] Furthermore, the method for correcting the shape of the titanium alloy rear base casting provided by the present invention may also have the following additional technical features:
[0019] In a specific embodiment of the present invention, in the pickling step of the casting, the thickness of the α layer on the surface of the casting is determined by metallographic method, and the pickling removal amount of the casting is determined according to the thickness of the surface α layer, and the pickling removal amount is 1.2-1.5 times the thickness of the surface α layer.
[0020] In a specific embodiment of the present invention, in the casting pickling step, hydrofluoric acid, nitric acid and deionized water are mixed to form an acidic solution.
[0021] In a specific embodiment of the present invention, in the casting shaping step, adjusting the locking nut to drive the shaping bolt to shape the large end ring includes:
[0022] The deformation direction of the casting in the axial direction of the profiling bolt is obtained by measurement;
[0023] Adjust the correction bolts corresponding to the inward deformation area of the casting through the locking nut to support the large end ring until the large end ring of the casting at the corresponding position is consistent with the theoretical position;
[0024] Adjust the correction bolts at other positions in sequence until the large end ring of the casting is consistent with the theoretical position.
[0025] In a specific embodiment of the present invention, the distance from the inner circumference of the center positioning cylinder to the outer circumference of the large end ring of the casting in the length direction of the profiling bolt is measured, and the measured distance is compared with the theoretical distance. The deformation direction of the casting and whether the large end ring of the casting is consistent with the theoretical position are judged based on the comparison result.
[0026] In one embodiment of the present invention, in the step of stress relief annealing of the casting, placing the casting and the shaper in a heating device and wrapping them with titanium chips comprises:
[0027] Place the casting and the bottom of the profiling tool in a protective barrel with titanium chips of preset thickness, and put titanium chips of preset thickness around and on the top of the casting so that the titanium chips completely cover the casting;
[0028] Place the casting together with the shaping tool and protective barrel in the heating device.
[0029] The shaping tool provided in the present application matches the center positioning cylinder with the reference hole of the small end circular ring of the casting, takes advantage of the fact that the small end circular ring in the rear base casting is not easily deformed and uses it as the shaping reference, and then transfers the reference to the center positioning cylinder, and then uses the end of the center positioning cylinder flush with the large end circular ring as the reference, and adjusts the distance between different areas of the large end circular ring of the casting and the end of the center positioning cylinder through the adjustment component, thereby achieving the shaping of the large end circular ring. In the above-mentioned shaping, not only can the deformation size of the large end circular ring be accurately corrected to ensure its roundness, but also the coaxiality of the large end circular ring and the small end circular ring can be ensured, thereby ensuring the correction accuracy of the base casting after correction.
[0030] The shaping method provided in the present application includes the steps of pickling of castings, rough reference processing of castings, shaping of castings and stress relief annealing of castings. First, the α layer on the surface of the casting is removed by pickling, thereby eliminating crack defects on the surface of the casting caused by the internal stress generated by the shaping; then, a reference hole is formed on the small end ring of the casting, and the shaping is performed using a shaping tool with a specific structure, so as to ensure the coaxiality of the large end ring and the small end ring while ensuring the roundness of the large end ring; then, the casting and the shaping tool are placed in a heating device and heated to relieve stress by covering with titanium chips, which not only eliminates the shaping stress of the casting while protecting the casting, but also avoids the risk of the casting becoming elliptical again. The heating equipment is simple and efficient, and the stress relief annealing temperature is not high. Both the tooling and the casting are carried out under the protection of titanium chips, which can reduce the restrictions on the materials of the shaping tooling and reduce the cost of the shaping tooling. BRIEF DESCRIPTION OF THE DRAWINGS
[0031] In order to more clearly illustrate the specific implementation methods of the present invention or the technical solutions in the prior art, the drawings required for use in the specific implementation methods or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are some implementation methods of the present invention. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative work.
[0032] Figure 1 It is a schematic diagram of the structure of the titanium alloy rear base in one direction of the present invention;
[0033] Figure 2 It is a schematic diagram of the structure of the titanium alloy rear base in another direction of the present invention;
[0034] Figure 3 It is a schematic diagram of the alignment tooling and the alignment coordination of the titanium alloy rear base casting in the present invention.
[0035] Description of reference numerals:
[0036] 10-rear base, 11-small end ring, 12-large end ring, 13-reference hole;
[0037] 21-center positioning cylinder, 22-annular correction block, 23-correction bolt, 24-locking nut, 25-reinforcement rib; 20-vernier caliper. DETAILED DESCRIPTION
[0038] The exemplary embodiments of the present invention will be described in more detail below with reference to the accompanying drawings. Although the exemplary embodiments of the present invention are shown in the accompanying drawings, it should be understood that the present invention can be implemented in various forms and should not be limited by the embodiments described herein. On the contrary, these embodiments are provided in order to enable a more thorough understanding of the present invention and to fully convey the scope of the present invention to those skilled in the art.
[0039] It should be understood that the terms used herein are only for the purpose of describing specific example embodiments and are not intended to be limiting. Unless the context clearly indicates otherwise, the singular forms "one", "an" and "said" as used herein may also be meant to include plural forms. The terms "include", "comprise", "contain", and "have" are inclusive, and therefore specify the existence of stated features, steps, operations, elements and / or parts, but do not exclude the existence or addition of one or more other features, steps, operations, elements, parts, and / or combinations thereof. The method steps, processes, and operations described herein are not interpreted as necessarily requiring them to be performed in the specific order described or illustrated, unless the execution order is clearly indicated. It should also be understood that additional or alternative steps may be used.
[0040] Although the terms first, second, third, etc. can be used in the text to describe multiple elements, components, regions, layers and / or sections, these elements, components, regions, layers and / or sections should not be limited by these terms. These terms can only be used to distinguish an element, component, region, layer or section from another region, layer or section. Unless the context clearly indicates, terms such as "first", "second" and other numerical terms do not imply order or sequence when used in the text. Therefore, the first element, component, region, layer or section discussed below can be referred to as the second element, component, region, layer or section without departing from the teaching of the example embodiments.
[0041] For ease of description, spatial relative terms may be used herein to describe the relationship of one element or feature relative to another element or feature as shown in the figure, such as "inside", "outside", "inner side", "outer side", "below", "below", "above", "above", etc. Such spatial relative terms are intended to include different orientations of the device in use or operation in addition to the orientation depicted in the figure. For example, if the device in the figure is turned over, then the elements described as "below other elements or features" or "below other elements or features" will subsequently be oriented as "above other elements or features" or "above other elements or features". Therefore, the example term "below..." can include both upper and lower orientations. The device can be oriented otherwise (rotated 90 degrees or in other directions) and the spatial relative descriptors used in the text are interpreted accordingly.
[0042] like Figure 1-2As shown, the shaping tooling and shaping method provided by the present invention are both used for shaping of a titanium alloy rear base 10 casting. Specifically, the casting of the titanium alloy rear base 10 includes a large end ring 12, a small end ring 11, and a shell connecting the large end ring 12 and the small end ring 11. During shaping, the large end ring 12 of the casting will be deformed due to its small wall thickness, thereby affecting the coaxiality of the large end ring 12 and the small end ring 11.
[0043] like Figure 3 As shown, the first aspect of the present invention provides a profiling tool for a titanium alloy rear base 10 casting, the profiling tool comprising a center positioning cylinder 21, an annular profiling block 22 and an adjustment assembly, wherein the inner and outer circumferences of the center positioning cylinder 21 are coaxially arranged; the annular profiling block 22 is sleeved on one end of the center positioning cylinder, and a plurality of radial through holes are provided on the annular profiling block 22; the adjustment assembly comprises a profiling bolt 23 and a locking nut 24, the profiling bolt 23 is inserted into the through hole, and the locking nut 24 is sleeved on the profiling bolt 23, and is suitable for adjusting the depth of the profiling bolt 23.
[0044] The center positioning cylinder 21 is a cylindrical structure with a circular cross section, which has a consistent inner diameter and outer diameter, and the outer circle is coaxially arranged with the inner circle. The center positioning cylinder 21 is suitable for being adapted to be connected with the reference hole 13 of the small end circular ring 11 of the titanium alloy rear base 10 casting, so as to transfer the positioning reference on the rear base 10 from the reference hole 13 of the small end circular ring 11 to the inner circle of the center positioning cylinder 21, so as to facilitate the subsequent correction of the large end circular ring 12 of the casting with the inner circle of the center positioning cylinder 21 as the reference. In order to facilitate subsequent correction, the outer diameter of the center positioning cylinder 21 should be the same as the inner diameter of the reference hole 13 of the small end circular ring 11 of the titanium alloy rear base 10, and the length should be the same as the overall height of the titanium alloy rear base 10. When matched with the reference hole 13 of the small end circular ring 11 of the titanium alloy rear base 10, the end face of the center positioning cylinder 21 is flush with the end face of the small end circular ring 11 of the titanium alloy rear base 10.
[0045] The annular shape correction block 22 is connected to one end of the center positioning cylinder 21, and the outer end surface is flush with the center positioning cylinder 21. Preferably, the inner circumference and the outer circumference of the annular shape correction block 22 are coaxially arranged with the center positioning cylinder 21. A plurality of radially arranged through holes are evenly arranged along the circumference of the annular shape correction block 22, that is, the central axis of the through hole is located in the radial direction of the annular shape correction block 22.
[0046] In the adjustment assembly, the shaping bolt 23 is inserted into the through hole of the annular shaping block 22, and the locking nut 24 is screwed on the shaping bolt 23. During the shaping process, one end of the shaping bolt 23 inserted in the through hole abuts against the inner circle of the large end ring 12 of the rear base 10 casting, and the other end abuts against the outer circle of the annular shaping block 22 through the locking nut 24. By adjusting the locking nut 24, the length of the shaping bolt 23 between the inner circle of the large end ring 12 and the outer circle of the annular shaping block 22 can be adjusted, thereby realizing the adjustment of the large end ring 12.
[0047] The shaping tool provided in the present application utilizes the characteristic that the small end circular ring 11 in the rear base 10 casting is not easy to deform, and uses it as a shaping reference, and transmits the reference to the center positioning tube 21 through the cooperation between the small end circular ring 11 and the center positioning tube 21, and then the end of the center positioning tube 21 that is flush with the large end circular ring 12 can be used as a reference, and the different areas of the large end circular ring 12 of the casting can be adjusted by adjusting the adjustment component, so as to achieve the shaping of the large end circular ring 12. In the above shaping, not only can the deformation size of the large end circular ring 12 be accurately corrected to ensure its roundness, but also the coaxiality of the large end circular ring 12 and the small end circular ring 11 can be ensured, thereby ensuring the correction accuracy of the calibrated rear base 10 casting.
[0048] In a specific embodiment of the present invention, a plurality of reinforcing ribs 25 are further included, and the plurality of reinforcing ribs 25 are evenly distributed along the radial direction of the center positioning cylinder 21, and one end of the reinforcing ribs 25 is connected to the outer wall of the center positioning cylinder 21, and the other end is connected to the inner wall of the annular shape correction block 22. The center positioning cylinder 21 and the annular shape correction block 22 are connected by the reinforcing ribs 25, so that the connection strength between the center positioning cylinder 21 and the annular shape correction block 22 is ensured.
[0049] In a specific embodiment of the present invention, 9 through holes are evenly arranged on the annular shaping block 22, and a shaping bolt 23 is inserted into each through hole. In the above arrangement, the large end ring 12 of the casting is divided into 9 areas by arranging 9 shaping bolts 23, so that the area corresponding to each shaping bolt 23 is reduced, and the shaping accuracy of the corresponding area is improved. In addition, arranging 9 shaping bolts 23 allows each shaping bolt 23 to be arranged opposite to two shaping bolts 23, thereby facilitating the adjustment of roundness.
[0050] In a specific embodiment of the present invention, the center positioning cylinder 21, the annular shape correction block 22 and the reinforcing ribs 25 are all made of No. 45 steel.
[0051] Another aspect of the present invention further provides a method for correcting the shape of a titanium alloy rear base 10 casting, wherein the titanium alloy rear base 10 casting comprises a large end ring 12, a small end ring 11, and a shell connecting the large end ring 12 and the small end ring 11, and the correction method comprises the following steps:
[0052] Pickling of castings: pickling the castings with an acid solution to remove the surface α layer of the castings;
[0053] Casting rough reference processing: rough processing is performed on the inner hole of the small end ring 11 to form a reference hole 13;
[0054] Casting calibration: Take any of the calibration tools described above, and make the center positioning cylinder 21 of the calibration tool and the reference hole 13 of the casting have the same diameter as the base hole system, and then adjust the locking nut 24 to drive the calibration bolt 23 to calibrate the large end ring 12;
[0055] Stress relief annealing of castings: place the casting and the shaping tool in a heating device and wrap them with titanium chips, heat to 500-550°C, keep warm for 1-2 hours and then cool to room temperature; take out the casting and the shaping tool and remove the shaping tool to obtain the shaped titanium alloy rear base 10.
[0056] Since titanium alloys are highly chemically active at high temperatures, especially during casting and heat treatment, an α layer will be formed on the surface. The surface α layer has high hardness and low plasticity. In subsequent shaping, repair welding, processing and other processes, the casting generates internal stress. The internal stress acts on the surface α layer of the casting, which will cause cracks on the surface of the casting, thereby reducing the fatigue performance, fracture performance and impact performance of the material. At the same time, this crack defect is difficult to repair, which will cause a certain degree of scrapping of the casting. In order to avoid crack defects on the surface of the casting due to stress concentration during the shaping process, the present application adopts a pickling method to remove the surface α layer of the casting.
[0057] In the pickling step, it is first necessary to determine the thickness of the pickling removal amount of the casting. In order to ensure that the surface α layer of the casting is completely removed, the thickness of the pickling removal amount of the casting is usually set to 1.2 to 1.5 times the thickness of the surface α layer. Specifically, the casting body is sampled, and the thickness of the α layer on the surface of the casting is determined by metallographic method. Then, the pickling removal amount of the casting is calculated based on the thickness of the α layer on the surface of the casting. The acid solution is a solution mixed with hydrofluoric acid, nitric acid and a certain proportion of deionized water. After pickling, the wall thickness of the casting is tested to ensure that the pickling amount meets the set requirements.
[0058] In the casting of the rear base 10, the large end circular ring 12 is large in size and thin in wall thickness, so it is very easy to deform during processing, while the small end circular ring 11 is small in size and thicker in wall thickness, so it has strong deformation resistance and is not easy to deform. Therefore, in order to ensure the coaxial requirements of the outer circle of the large end circular ring 12 and the inner hole of the small end circular ring 11 of the casting during the correction process, the large end circular ring 12 can be corrected with the small end circular ring 11 as a reference. Specifically, a lathe is used to rough-process the inner hole of the small end circular ring 11 of the rear base 10 to form a reference hole 13. During the rough processing process, the single-sided removal amount of the inner hole of the small end circular ring 11 is about 1 mm.
[0059] In the casting correction step, a correction tool is selected in which the outer diameter of the center positioning cylinder 21 is the same as the aperture of the reference hole 13 of the small end ring 11, and the height of the center positioning cylinder 21 is the same as the height of the rear base 10. Then, one end of the center positioning cylinder 21 is matched with the reference hole 13 of the small end ring 11 of the casting using the base hole system, so that the end of the center positioning cylinder 21 with the annular correction block is located inside the casting and flush with the large end ring 12.
[0060] Then, a wrench is used to rotate and adjust the locking nut 24 that is close to the outer cylindrical end face of the annular profiling block 22, and the rotation of the locking nut 24 drives the profiling bolt 23 to move axially until the end face of the profiling bolt 23 is about 2 mm away from the inner wall of the large end ring 12 of the rear base 10.
[0061] Afterwards, a digital display vernier caliper 20 is used to measure and record the distance between the inner wall of the center positioning cylinder 21 and the outer circle of the large end ring 12 of the rear base 10 along the axial direction of the correction bolt 23, and then compare it with the theoretical distance size of the casting. If it is smaller than the theoretical distance size, it means that the area of the casting is deformed toward the center of the casting, and if it is greater than the theoretical distance size, it means that the area of the casting is deformed in the opposite direction to the center of the casting.
[0062] According to the above judgment, the locking nut 24 is adjusted. Specifically, the area with large deformation toward the center of the casting is first calibrated, and the fixed clamping foot of the digital display vernier caliper 30 is pressed against the outer circle of the large end ring 12 of the casting and the movable clamping foot is pressed against the inner wall of the center positioning cylinder 21 along the axial direction of the calibration bolt 23 for pre-locking. The locking nut 24 is rotated to drive the axial movement of the calibration bolt 23 through the rotation of the nut. The calibration bolt 23 first contacts the inner wall of the large end ring 12 of the casting. The locking nut 24 is continued to be rotated to support the deformed area. When the displayed size of the digital display vernier caliper 30 is consistent with the theoretical distance size of the casting, the locking nut 24 is stopped from being rotated. Then, according to this plan, other areas deformed toward the center of the casting are adjusted in turn according to the amount of deformation; the areas deformed in the opposite direction to the center of the casting, because the areas deformed toward the center of the casting are stretched out and the reverse deformation areas are contracted, respectively check whether the axial distance corresponding to the correction bolt 23 is consistent with the theoretical distance size. If they are consistent, rotate the adjustment locking nut 24 to make the correction bolt 23 contact with the inner wall of the large end ring 12 to form support and complete the correction. If there is a deviation from the theoretical distance size, continue to adjust until the size meets the requirements of the drawing.
[0063] After the shaping process, the casting needs to be subjected to stress relief annealing. Internal stress is generated during the shaping process. If the internal stress is not eliminated, the casting after shaping will have a large rebound force. After removing the constraint of the shaping tooling, it will return to an elliptical shape. Conventional stress relief annealing is generally carried out in a vacuum furnace, which requires complex equipment and has low efficiency. In order to improve the efficiency of the casting and avoid the formation of an oxide layer on the surface of the casting during the heating and annealing process of the casting, the casting and the constraint shaping tooling are placed in a drum, and clean titanium chips are placed at the bottom of the drum. Titanium chips are placed around and on the top of the casting. The thickness of the titanium chips is more than 30 mm, and the casting is completely covered by titanium chips to avoid oxidation of the casting. The casting, together with the tooling and the protective barrel, is placed in a box-type resistance furnace, heated to 500-550 degrees for 1-2 hours, and naturally cooled to room temperature. Since the shaping stress is eliminated and the shaping tooling is removed, after testing, the size of the casting meets the requirements of the drawing. After sand blasting, the castings were tested by fluorescence and no cracks were found on the surface. At the same time, since the stress relief annealing temperature is not high and both the tooling and castings are protected by titanium chips, the tooling material can be 45# steel, which has good toughness and certain wear resistance, is cheap, and meets the tooling requirements.
[0064] Finally, it should be noted that the above embodiments are only used to illustrate the technical solutions of the present invention, rather than to limit it. Although the present invention has been described in detail with reference to the aforementioned embodiments, those skilled in the art should understand that they can still modify the technical solutions described in the aforementioned embodiments, or replace some or all of the technical features therein with equivalents. However, these modifications or replacements do not cause the essence of the corresponding technical solutions to deviate from the scope of the technical solutions of the embodiments of the present invention.
Claims
1. A method for correcting the shape of a titanium alloy rear base casting, characterized in that: The casting of the titanium alloy rear base includes a large end ring, a small end ring and a shell connecting the large end ring and the small end ring, and the shaping tooling includes: A center positioning cylinder, wherein the inner and outer circumferences of the center positioning cylinder are coaxially arranged; An annular profiling block, which is sleeved on one end of the central positioning cylinder and is provided with a plurality of radial through holes; An adjustment component, comprising a profile adjustment bolt and a locking nut, wherein the profile adjustment bolt is inserted into the through hole, and the locking nut is sleeved on the profile adjustment bolt and is suitable for adjusting the depth of the profile adjustment bolt; The calibration method comprises the following steps: Pickling of castings: pickling the castings with an acid solution to remove the surface α layer of the castings; Casting rough reference processing: rough processing is performed on the inner hole of the small end ring to form a reference hole; Casting calibration: Take the calibration tool, and make the central positioning cylinder of the calibration tool and the reference hole of the casting have the same diameter as the base hole, and then adjust the locking nut to drive the calibration bolt to calibrate the large end ring; Stress relief annealing of castings: Place the casting and the shaping tool in a heating device and wrap them with titanium chips, heat to 500-550°C, keep warm for 1-2 hours and then cool to room temperature; take out the casting and the shaping tool and remove the shaping tool to obtain the shaped titanium alloy rear base; In the casting shaping step, adjusting the locking nut to drive the shaping bolt to shape the large end ring includes: The deformation direction of the casting in the axial direction of the profiling bolt is obtained by measurement; Adjust the correction bolts corresponding to the inward deformation area of the casting through the locking nut to support the large end ring until the large end ring of the casting at the corresponding position is consistent with the theoretical position; Adjust the correction bolts at other positions in sequence until the large end ring of the casting is consistent with the theoretical position; By measuring the distance from the inner circumference of the center positioning cylinder to the outer circumference of the large end ring of the casting in the length direction of the proofreading bolt, and comparing the measured distance with the theoretical distance, the deformation direction of the casting and whether the large end ring of the casting is consistent with the theoretical position can be judged based on the comparison results.
2. The method for correcting the shape of a titanium alloy rear base casting according to claim 1, characterized in that: It also includes a plurality of reinforcing ribs, which are evenly distributed along the radial direction of the center positioning tube, and one end of the reinforcing ribs is connected to the outer wall of the center positioning tube, and the other end is connected to the inner wall of the annular correction block.
3. The method for correcting the shape of a titanium alloy rear base casting according to claim 2, characterized in that: The center positioning cylinder, the annular shape correction block and the reinforcing ribs are all made of No. 45 steel.
4. The method for correcting the shape of a titanium alloy rear base casting according to claim 1, characterized in that: Nine through holes are evenly arranged on the annular shaping block, and one shaping bolt is inserted into each of the through holes.
5. The method for correcting the shape of a titanium alloy rear base casting according to claim 1, characterized in that: In the casting pickling step, the thickness of the α layer on the surface of the casting is determined by metallographic method, and the pickling removal amount of the casting is determined according to the thickness of the α layer on the surface, and the pickling removal amount is 1.2-1.5 times the thickness of the α layer on the surface.
6. The method for correcting the shape of a titanium alloy rear base casting according to claim 5, characterized in that: In the casting pickling step, an acidic solution is prepared by mixing hydrofluoric acid, nitric acid and deionized water.
7. The method for correcting the shape of a titanium alloy rear base casting according to claim 1, characterized in that: In the step of stress relief annealing of the casting, the casting and the molder are placed in a heating device and wrapped with titanium chips, including: Place the casting and the bottom of the profiling tool in a protective barrel with titanium chips of preset thickness, and put titanium chips of preset thickness around and on the top of the casting so that the titanium chips completely cover the casting; Place the casting together with the shaping tooling and protective barrel in the heating device.
Citation Information
Patent Citations
Thermal shaping clamp of titanium alloy thin-wall tubular part
CN103639247A
Correcting method for roundness of casting and correcting tool adopting same
CN107617654A
Thin-walled cylindrical part calibration tool
CN110814097A
Method for preventing stainless steel heat treatment oxidation
CN110835673A
Local deformation correcting method for titanium alloy component
CN112338002A