Semiconductor structure and method for preparing semiconductor structure
By forming a barrier layer in the peripheral region of the semiconductor structure and adjusting the etching depth, the substrate leakage problem caused by the shallow junction depth of the source and drain region is solved, and the stability and conductivity of the semiconductor structure are improved.
Patent Information
- Application Number
- CN202110996603.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2021-08-27
- Publication Date
- 2024-12-06
- Estimated Expiration
- 2041-08-27
AI Technical Summary
In the existing semiconductor structure, the junction depth of the source and drain region becomes shallow, resulting in deep contact through holes, causing excessive leakage of the substrate, affecting structural stability.
A barrier layer is formed on the substrate of the peripheral region. The barrier layer is located on the surface of the second doped region, and the etching depth is adjusted through the etching rate of different materials, increasing the PN junction distance between the conductive contact structure and the source and drain region, and reducing the second The depth of the two conductive columns is kept away from the depletion zone, thereby reducing leakage.
The leakage between the conductive contact structure and the substrate of the semiconductor structure is effectively reduced, and the stability and conductivity of the semiconductor structure are improved.
Smart Images

Figure CN115842023B_ABST
Abstract
Description
Technical Field
[0001] The embodiments of the present application relate to the semiconductor field, and in particular, to a semiconductor structure and a method for preparing the semiconductor structure. Background Art
[0002] With the continuous development of integrated circuit technology and process technology, the characteristic size of transistor (MOS) devices has been continuously reduced in order to improve the integration of integrated circuits. At process nodes such as high dielectric metal gate (HKMG) and fin-type transistors (Finfet), a series of problems need to be faced while increasing the operating speed of MOS devices and reducing their power consumption.
[0003] Especially as the source-drain junction depth becomes shallower, how to improve the depth of the contact via, thereby improving the problem of excessive substrate leakage of the semiconductor structure and improving the stability of the semiconductor structure has become an important issue that needs to be urgently solved by those skilled in the art. Summary of the invention
[0004] The embodiments of the present application provide a semiconductor structure and a method for preparing the semiconductor structure, which can solve the problem of shallow junction depth in the existing semiconductor structure and excessive substrate leakage caused by excessively deep contact holes.
[0005] According to some embodiments of the present application, on one hand, an embodiment of the present application provides a method for preparing a semiconductor structure, including: providing a substrate, the substrate including a core region and a peripheral region, and the substrates of the core region and the peripheral region both have gate structures, the substrates on opposite sides of the gate structure of the core region have first doped regions, and the substrates on opposite sides of the gate structure of the peripheral region have second doped regions; forming a barrier layer on the substrate of the peripheral region, the barrier layer being located on the surface of the second doped region; forming a mask layer with an opening on the substrate of the core region and the peripheral region, the mask layer being also located on the surface of the barrier layer, the material of the mask layer being different from the material of the barrier layer; using the mask layer as a mask, etching the dielectric layer and the first doped region of the core region along the opening to form a first groove in the first doped region, and at the same time etching the barrier layer and the second doped region of the peripheral region along the opening to form a second groove in the second doped region, and the depth of the first groove is greater than the depth of the second groove; forming a first conductive column, the first conductive column filling the first groove and protruding from the substrate surface; forming a second conductive column, the second conductive column filling the second groove and protruding from the substrate surface.
[0006] According to some embodiments of the present application, on the other hand, the embodiments of the present application further provide a semiconductor structure, including: a substrate, the substrate including a core region and a peripheral region, and the substrates in the core region and the peripheral region both have gate structures, the gate structure in the core region has first doped regions in the substrate on opposite sides, and the gate structure in the peripheral region has second doped regions in the substrate on opposite sides; a first conductive column, the first conductive column is located in the first doped region and protrudes from the surface of the substrate; the second conductive column is located in the second doped region and protrudes from the surface of the substrate, and the depth of the second conductive column in the second doped region is less than the depth of the first conductive column in the first doped region.
[0007] The technical solutions provided by some embodiments of the present application have at least the following advantages: In some embodiments of the present application, by forming a barrier layer on the substrate in the peripheral region, and the barrier layer is located on the surface of the second doping region, the etching depth is adjusted by the etching rate of different materials, thereby increasing the distance between the bottom of the conductive contact structure and the depletion region of the PN junction directly formed by the source-drain region and the substrate, thereby improving the leakage problem at the contact between the conductive contact structure and the semiconductor substrate. In some embodiments of the present application, the depth of the second conductive column located in the second doping region is reduced, so that the second conductive column is far away from the depletion region of the PN junction formed between the source-drain region and the substrate, which is beneficial to improving the stability of the semiconductor structure; in addition, the first conductive column is located in the first doping region and protrudes from the substrate surface; the second conductive column is located in the second doping region and protrudes from the substrate surface, and the depth of the second conductive column located in the second doping region is less than the depth of the first conductive column located in the first doping region. On the one hand, the depth of the first conductive column located in the first doping region ensures that the core region and the conductive column have good conductivity, and on the other hand, it can avoid the second conductive column being located in the second doping region. The depth is too great, which may cause the second conductive column to touch the depletion region of the PN junction directly formed by the source-drain region and the substrate, which is beneficial to improving the problem of excessive substrate leakage of the semiconductor structure. BRIEF DESCRIPTION OF THE DRAWINGS
[0008] One or more embodiments are exemplarily described by pictures in the corresponding drawings, and these exemplifications do not constitute limitations on the embodiments. Unless otherwise stated, the pictures in the drawings do not constitute proportional limitations.
[0009] Figure 1 is a schematic structural diagram of a semiconductor structure;
[0010] Figure 2 to Figure 10 A schematic diagram of structures corresponding to each step in a method for forming a semiconductor structure provided in an embodiment of the present application;
[0011] Fig.11 Another structural schematic diagram of a semiconductor structure provided by an embodiment of the present application;
[0012] Figures 12 to 20A schematic structural diagram corresponding to each step in a method for forming a semiconductor structure provided in another embodiment of the present application. DETAILED DESCRIPTION
[0013] At present, the junction depth of the source and drain regions of the existing semiconductor structure is becoming shallower, but the depth of the contact through hole is too deep, which will cause leakage between the substrate.
[0014] Analysis found that the main reasons for the above problems include: as the device size continues to shrink, the distance between the conductive contact structure and the depletion region of the source and drain continues to narrow, which will lead to the formation of a leakage channel between the substrate. Figure 1 This is a schematic diagram of a semiconductor structure. Figure 1 An analysis is conducted, wherein the substrate 100 includes a core region 101 and a peripheral region 102, and the core region 101 has a first gate 112, the peripheral region 102 has a second gate 122, the core region 101 on opposite sides of the first gate 112 has a first doping region 111, and the peripheral region 102 on opposite sides of the second gate 122 has a second doping region 121; a dielectric layer 103, located on the top surface of the core region 101; a first conductive column 146, the first conductive column 146 is partially located in the first doping region 111, and partially protrudes from the surface of the substrate 100; a second conductive column 156, the second conductive column 156 is partially located in the second doping region 121, and partially protrudes from the surface of the substrate 100, and due to the uniformity of the production process, the depth of the second conductive column 156 in the second doping region 121 is the same as the depth of the first conductive column 146 in the dielectric layer 103. Among them, for the semiconductor PN junction, due to the difference in the original chemical potential of the semiconductors on both sides of the interface (the contact surface between the P-type semiconductor and the N-type semiconductor), the energy band is bent near the interface, and the interface area where the carrier concentration decreases in the energy band bending area is the depletion area. Since there is a PN interface between the source and drain regions and the substrate, the second conductive column 156 is located at a relatively large depth in the second doped region 121, and the distance between the second conductive column 156 and the depletion region is also small, so the substrate contact leakage of the conductive contact structure and the semiconductor structure increases.
[0015] Among them, the doped region can be used as the source or drain of the semiconductor structure, and the ion concentration of the doped region is a Gaussian doping distribution, wherein the closer the region is to the substrate surface, the lower the doping concentration. When highly doped, the concentration difference of carriers in the semiconductor located on both sides of the depletion region is large, the diffusion movement of the majority carriers is violent, and the space charge region is theoretically widened. However, the internal electric field generated by the space charge region causes the drift movement of the minority carriers to be violent, and the space charge region is theoretically narrowed. Finally, the diffusion movement rate of the majority carriers and the drift movement rate of the minority carriers reach a dynamic equilibrium. When highly doped, the time for the carriers to reach dynamic equilibrium is shorter than that for low doping, the recombination time of electrons and holes is shortened, and the width of the depletion region is narrowed. When the second conductive column 156 is located at a relatively large depth in the second doped region 121, the two ends of the depletion region are in the low-doped region, and the thickness of the formed depletion region is thick, resulting in a narrower distance between the second conductive column 156 and the depletion region, and as the device size shrinks, the distance between the conductive column and the depletion region is smaller, and the conductive contact structure and the substrate contact leakage of the semiconductor structure increase, which seriously affects the stability of the semiconductor structure.
[0016] Some embodiments of the present application provide a semiconductor structure and a method for preparing the semiconductor structure. By forming a barrier layer on the substrate in the peripheral region, and the barrier layer is located on the surface of the second doping region, the etching depth is adjusted, thereby increasing the distance between the bottom of the conductive contact structure and the PN junction formed between the source and drain terminals / substrate, thereby reducing the leakage between the conductive contact structure and the substrate of the semiconductor. The embodiments of the present application reduce the depth of the second conductive column in the second doping region, so that the second conductive column is far away from the depletion region, and at the same time, the second doping region is ion-doped by pretreatment. Therefore, the contact resistance between the conductive contact structure and the semiconductor is small, which is beneficial to improving the conductive performance of the semiconductor structure, and the conductive contact structure and the substrate of the semiconductor structure have small contact leakage, which is beneficial to improving the stability of the semiconductor structure.
[0017] In order to make the purpose, technical scheme and advantages of the embodiments of the present application clearer, the embodiments of the present application will be described in detail below in conjunction with the accompanying drawings. However, it will be appreciated by those skilled in the art that in the embodiments of the present application, many technical details are provided in order to enable the reader to better understand the present application. However, even without these technical details and various changes and modifications based on the following embodiments, the technical scheme claimed in the present application can be implemented.
[0018] Figure 2 to Figure 10 A schematic diagram of structures corresponding to each step in a method for forming a semiconductor structure provided in an embodiment of the present application.
[0019] refer to Figure 2A substrate 200 is provided, the substrate 200 includes a core area 201 and a peripheral area 202, and the substrate 200 of the core area 201 has a first gate 212, and the substrate 200 on opposite sides of the first gate 212 of the core area 201 has a first doped area 211, the substrate 200 exposes the top surface of the first doped area 211, and the top surface of the first doped area 211 has a dielectric layer 203; the substrate 200 of the peripheral area 202 has a second gate 222, and the substrate 200 on opposite sides of the second gate 222 of the peripheral area 202 has a second doped area 221.
[0020] In some embodiments, the core region 201 is used to connect the conductive structure to form a storage unit, and the peripheral region 202 is used to connect the conductive structure to form a logic unit to ensure that the function of the core region is realized.
[0021] The material of the substrate 200 is a semiconductor material. Specifically, in some embodiments, the material of the substrate 200 is silicon. In other embodiments, the material of the substrate may also be germanium, germanium silicon or silicon carbide.
[0022] In some embodiments, the first gate 212 of the core region 201 is a buried gate, and the second gate 222 of the peripheral region 202 is a planar gate.
[0023] The core region 201 further includes a first gate sidewall 232 and a first gate cap layer 242 .
[0024] Specifically, the first gate spacer 232 covers the bottom wall and side wall of the first gate 212, and is used to prevent the mutual diffusion of particles of the first gate 212 and particles of the first doping region 211. The material of the first gate spacer 232 is metal oxide, such as titanium nitride, tantalum nitride, titanium or tantalum.
[0025] The first gate capping layer 242 covers the surface of the first gate 212, and is used to isolate the first gate 212 from the dielectric layer 203, wherein the material of the first gate capping layer 242 is an insulating material, for example, silicon dioxide, silicon carbide or silicon nitride. In some embodiments, the material of the first gate 212 is metal tungsten, and in other embodiments, the material of the first gate may also be other metal materials such as copper or aluminum.
[0026] Specifically, in some embodiments, the first gate 212 includes a first gate first conductive layer. In other embodiments, the first gate includes a first gate first conductive layer, a first gate dielectric layer and a first gate second conductive layer stacked in sequence, and the materials of the first gate first conductive layer and the first gate second conductive layer may be different.
[0027] The peripheral region 202 further includes a second gate oxide layer 252 covering the substrate 200 , and the second gate oxide layer 252 is located between the substrate 200 and the second gate 222 .
[0028] Specifically, the material of the second gate oxide layer 252 is an insulating material, for example, silicon dioxide, silicon carbide or silicon nitride, for isolating the second gate 222 from the substrate 200. In some embodiments, the second gate oxide layer 252 is made of the same material as the first gate cap layer 242. In other embodiments, the second gate oxide layer and the first gate cap layer may also be made of different materials.
[0029] In some embodiments, the material of the second gate 222 is tungsten. In other embodiments, the material of the second gate 222 may also be copper, aluminum or other metal materials. In some embodiments, the first gate 212 and the second gate 222 are made of the same material. In other embodiments, the first gate and the second gate may also be made of different materials.
[0030] Specifically, in some embodiments, the second gate 222 includes a second gate first conductive layer. In other embodiments, the second gate includes a second gate first conductive layer, a second gate dielectric layer and a second gate second conductive layer stacked in sequence, and the materials of the second gate first conductive layer and the second gate second conductive layer may be different.
[0031] The first doping region 211 is an N-type doping region, and the second doping region 221 can be an N-type doping region or a P-type doping region; in some embodiments, the first doping region 211 and the second doping region 221 are N-type doping regions, the substrate 200 is a P-type doping region, the first doping region 211 and the second doping region 221 are doped with N-type ions, and the substrate 200 is doped with P-type ions. In other embodiments, the doping region is a P-type doping region, the substrate is an N-type doping region, the doping region is doped with P-type ions, and the substrate is doped with N-type ions. Specifically, the doping ions of the second doping region 221 are boron ions among P-type ions. In other embodiments, the doping ions can also be phosphorus ions and arsenic ions among N-type ions and aluminum ions and boron fluoride ions among P-type ions.
[0032] For the first gate 212, the first doped region 211 located on one side of the first gate 212 serves as a source, and the first doped region 211 located on the other side of the first gate 212 serves as a drain; similarly, for the second gate 222, the second doped region 221 located on one side of the second gate 222 serves as a source, and the second doped region 221 located on the other side of the second gate 222 serves as a drain.
[0033] The dielectric layer 203 is located on the top surface of the first doped region 211, wherein the material of the dielectric layer 203 can be insulating materials such as silicon, silicon oxide, silicon carbide, silicon nitride, or other high dielectric constant materials. In some embodiments, the dielectric layer 203 covers the top surface of the first doped region 211, and the dielectric layer 203 also covers the upper surface of the first gate cap layer 242.
[0034] refer to Figure 3 , a barrier layer 230 is formed on the substrate 200 in the peripheral region 202 , and the barrier layer 230 is located on the surface of the second doping region 221 .
[0035] Specifically, the barrier layer 230 is also located on the sidewall of the second gate 222 in the peripheral region 202, and the material of the barrier layer 230 is different from that of the dielectric layer 203. In some embodiments, the barrier layer 230 is made of silicon oxide, and in other embodiments, the barrier layer may also be made of SiNx or C.
[0036] More specifically, during the etching process of the same material, the etching rate of the barrier layer 230 is lower than the etching rate of the dielectric layer 203 .
[0037] A barrier layer 230 is formed on the substrate 200 of the peripheral region 202, and the barrier layer 230 is located on the surface of the second doped region 221, wherein in the process of etching by the same material, the etching rate of the barrier layer 230 is lower than the etching rate of the dielectric layer 203, so as to adjust the time of forming the through hole on the barrier layer 230 and the time of forming the through hole on the dielectric layer 203 to have a difference, so that in the process of forming the through hole on the dielectric layer 203, part of the second doped region 221 is etched, thereby increasing the distance between the bottom of the conductive contact structure subsequently formed in the groove of the second doped region 221 and the PN junction subsequently using the second doped region 221 as the source and drain terminals, thereby reducing the leakage current between the conductive contact structure and the substrate of the semiconductor structure.
[0038] In some embodiments of the present application, the process steps for forming a barrier layer include: forming a continuous initial barrier film on the surface of the substrate 200 in the core area 201 and the peripheral area 202, and then removing the initial barrier film located in the core area 201, and the remaining initial barrier film serves as the barrier layer 230.
[0039] Specifically, the surface of the formed barrier layer 230 is flush with the surface of the dielectric layer 203; thus, the surfaces of the dielectric layer 203 and the barrier layer 230 on the substrate 200 are a flat surface, simplifying the morphology of the semiconductor structure. In addition, by ensuring that the surfaces of the dielectric layer 203 and the barrier layer 230 are a flat surface, the depth of the groove formed in the second doping region 221 depends on the etching selectivity of the dielectric layer 203 and the barrier layer 230, thereby achieving precise control of the depth of the groove formed in the second doping region 221, and further achieving precise control of the distance between the subsequently formed conductive contact structure and the PN junction.
[0040] In some embodiments, the initial barrier film is formed by an atomic deposition process. In other embodiments, the initial barrier film may also be formed by a chemical vapor deposition process.
[0041] refer to Figure 4A mask layer 240 is formed on the substrate 200 in the core region 201 and the peripheral region 202 , and the mask layer 240 is also located on the surface of the barrier layer 230 and the dielectric layer 203 . The material of the mask layer 240 is different from that of the barrier layer 230 .
[0042] refer to Figure 5 , using the mask layer 240 as a mask, patterning the mask layer 240 to form an opening, and then etching the dielectric layer 203 of the core area 201 along the opening to form a first trench 261 in the dielectric layer 203, the first trench 261 exposing the top surface of the first doping region 211, and also etching the barrier layer 230 and part of the second doping region 221 of the peripheral area 202 along the opening to form a second trench 262 in the barrier layer 230 and the second doping region 221, and the depth of the first trench 261 in the first doping region 211 is greater than the depth of the second trench 262 in the second doping region 221, so that the distance between the bottom of the second trench 262 (the bottom of the conductive contact structure formed subsequently) and the PN junction is further increased, which is beneficial to reduce the contact leakage between the conductive contact structure formed subsequently and the substrate of the semiconductor structure, and is beneficial to improve the stability of the semiconductor structure.
[0043] In some embodiments, a wet etching process is used to remove part of the mask layer 240 and the dielectric layer 203 to form a first trench 261; in this way, the first trench 261 exposes the top surface of the first doping region 211, and the conductive pillars that are subsequently formed to fill the first trench 261 can contact the region with the highest doping ion concentration in the first doping region 211, which is beneficial to improving the metal / semiconductor contact performance. In other embodiments, a dry etching process can also be used to remove part of the mask layer and the dielectric layer to form the first trench; similarly, in some embodiments, a wet etching process is used to remove part of the mask layer 240, the barrier layer 230, and the second doping region 221 to form a second trench 262; in this way, the second trench 262 exposes the sidewall of the second doping region 221, and the conductive pillars that are subsequently formed to fill the second trench 262 can contact the region with the highest doping ion concentration in the second doping region 221, which is beneficial to improving the metal / semiconductor contact performance. In other embodiments, a dry etching process can also be used to remove part of the mask layer, the barrier layer, and the second doping region to form the second trench.
[0044] refer to Figure 6 , a first mask layer 241 is formed on the substrate 200 in the core area 201, and the second trench 262 is pre-treated to increase the concentration of doping ions in the second doping area 221 exposed by the second trench 262; after the pre-treatment, the first mask layer 241 is removed.
[0045] In some embodiments, the pretreatment includes: a first step of pretreatment to dope fluorine ions on the surface of the second doping region 221 exposed by the second trench 262; and a second step of pretreatment to dope ions of the same type as the doping ions of the second doping region 221 on the surface of the second doping region 221 exposed by the second trench 262. By doping fluorine ions and additionally injecting ions of the same type as the doping ions of the second doping region, the concentration of doping ions in the second doping region exposed by the second trench is increased, and the contact resistance of the metal / semiconductor is reduced.
[0046] Specifically, in some embodiments, the doping ions are boron ions and aluminum ions among P-type ions, and in some other embodiments, the doping ions may also be phosphorus ions, arsenic ions, etc. among N-type ions.
[0047] In other embodiments, both the first trench and the second trench are pre-treated.
[0048] refer to Figure 7 , forming a metal layer 204, the metal layer 204 is located on the surface of the first groove 261, the surface of the second groove 262 and the surface of the mask layer 240. In some embodiments, the material of the metal layer 204 is cobalt, and in other embodiments, the material of the metal layer can also be nickel, titanium and other metals.
[0049] Specifically, in some embodiments, the metal layer 204 is formed by vacuum evaporation technology, and in other embodiments, the metal layer may also be formed by sputtering technology or vapor deposition technology.
[0050] In other embodiments, a metal layer is formed, and the metal layer is only located on the surface of the second trench and the surface of the mask layer directly above the second trench.
[0051] refer to Figure 8 , forming a first metal silicide layer 245 and a second metal silicide layer 255.
[0052] Specifically, the process steps for forming the first metal silicide layer 245 and the second metal silicide layer 255 include: annealing the metal layer 204, reacting the metal layer 204 with the first doping region 211 to form the first metal silicide layer 245, reacting the metal layer 204 with the second doping region 221 to form the second metal silicide layer 255; and removing the unreacted metal layer 204.
[0053] In some embodiments, the material of the first metal silicide layer 245 is cobalt silicide, which is used to reduce the resistance of the diffusion region and the contact resistance of the metal / semiconductor contact hole; in other embodiments, the first metal silicide layer can be a metal silicide such as titanium silicide or nickel silicide; similarly, in some embodiments, the material of the second metal silicide layer 255 is cobalt silicide, which is used to reduce the resistance of the diffusion region and the contact resistance of the metal / semiconductor contact hole, and in other embodiments, the second metal silicide layer can be a metal silicide such as titanium silicide or nickel silicide.
[0054] In some embodiments, the second metal silicide layer 255 and the first metal silicide layer 245 are made of the same material. In other embodiments, the second metal silicide layer and the first metal silicide layer may be made of different materials.
[0055] In other embodiments, only the second metal silicide layer is formed.
[0056] refer to Fig. 9 and Fig.10 , forming a first conductive column 246 and a second conductive column 256 . The first conductive column 246 fills the first groove 261 and protrudes from the surface of the substrate 200 , and the second conductive column 256 fills the second groove 262 and protrudes from the surface of the substrate 200 .
[0057] Specifically, the process steps for forming the first conductive pillar 246 and the second conductive pillar 256 include: forming a conductive film 250 that fills the first groove 261, the second groove 262 and the opening, and the conductive film 250 is also located on the top surface of the mask layer 240; removing the conductive film 250 above the top surface of the mask layer 240, and the remaining conductive film 250 located in the core area 201 is used as the first conductive pillar 246, and the remaining conductive film 250 located in the peripheral area 202 is used as the second conductive pillar 256, and the mask layer 240 is removed.
[0058] Specifically, refer to Fig. 9 , forming a conductive film 250 that fills the first trench 261 , the second trench 262 and the opening, and the conductive film 250 is also located on the top surface of the mask layer 240 .
[0059] In some embodiments, the material of the conductive film 250 is tungsten; in other embodiments, the material of the conductive film may also be metal such as silver.
[0060] refer to Fig.10 , remove the conductive film 250 above the top surface of the mask layer 240, the remaining conductive film 250 located in the core area 201 is used as the first conductive column 246, and the remaining conductive film 250 located in the peripheral area 202 is used as the second conductive column 256, and remove the mask layer.
[0061] It should be noted that, in some embodiments, the first metal silicide layer 245 is located at the bottom of the first trench 261 and between the first conductive column 246 and the first doped region 211 ; the second metal silicide layer 255 is located at the bottom of the second trench 262 and between the second conductive column 256 and the second doped region 221 .
[0062] Specifically, the contact resistance between the first metal silicon silicide 245 and the second metal silicide layer 255 is relatively small, which is beneficial to improving the conductive contact structure and the second doped region 221 to have a better conductive effect.
[0063] In some embodiments, the second metal silicide layer 255 is located at the bottom surface of the second trench and the side wall of the second doped region 221 to form a groove; in this way, the second metal silicide layer 255 and the second doped region 221 have a larger contact area. The larger the contact area, the smaller the contact resistance between the second metal silicide layer 255 and the second doped region 221, which is beneficial to improving the conductive effect of the second metal silicide layer 255 and the second doped region 221, thereby improving the performance of the semiconductor structure.
[0064] In some embodiments, a barrier layer is formed on the substrate of the peripheral region, and the barrier layer is located on the surface of the second doping region, and the etching depth is adjusted by the etching rate of different materials, so as to increase the distance between the bottom of the conductive contact structure and the PN junction formed between the source and drain end / substrate, thereby adjusting the contact leakage between the conductive contact structure and the substrate of the semiconductor structure. Some embodiments of the present application reduce the depth of the second conductive column in the second doping region, so that the second conductive column is far away from the depletion region, which is conducive to improving the problem of excessive substrate leakage of the semiconductor structure, and thus is conducive to improving the stability of the semiconductor structure; in addition, the first conductive column is located in the first doping region and protrudes from the substrate surface; the second conductive column is located in the second doping region and protrudes from the substrate surface, and the depth of the second conductive column in the second doping region is less than the depth of the first conductive column in the first doping region. On the one hand, the depth of the first conductive column in the first doping region ensures that the core region and the conductive column have good conductivity, and on the other hand, it can avoid the problem of excessive substrate leakage of the semiconductor structure caused by the second conductive column being located in the second doping region. Figures 12 to 20 A schematic structural diagram corresponding to each step in a method for forming a semiconductor structure provided in another embodiment of the present application.
[0065] refer to Fig.12A substrate 300 is provided, the substrate 300 includes a core area 301 and a peripheral area 302, and the substrate 300 of the core area 301 has a first gate 312, and the substrate 300 on opposite sides of the first gate 312 of the core area 301 has a first doped area 311, the substrate 300 exposes the top surface of the first doped area 311, and the top surface of the first doped area 311 has a dielectric layer 303; the substrate 300 of the peripheral area 302 has a second gate 322, and the substrate 300 on opposite sides of the second gate 322 of the peripheral area 302 has a second doped area 321.
[0066] refer to Fig.13 , a barrier layer is deposited on the substrate 300 in the peripheral region 302 and the core region 301 , and then a barrier layer 330 with a preset thickness is formed by chemical mechanical polishing or etching. The barrier layer 330 is located on the surface of the second doping region 321 and the surface of the dielectric layer 303 .
[0067] Specifically, in the direction perpendicular to the substrate 300, the thickness of the barrier layer 330 is 5-20 nm. The inventors have found that when the thickness is 5-20 nm, the etching depth of the second conductive column in the second doping region is lower than the etching depth of the first conductive column in the first doping region.
[0068] Figures 14 to 20 The semiconductor structure forming method corresponding to each step in Figures 4 to 10 The method for forming the semiconductor structure corresponding to each step is the same and will not be described in detail here.
[0069] In some embodiments, a barrier layer is formed on the substrate of the peripheral region and the core region, and the barrier layer is located on the surface of the second doped region and the surface of the dielectric layer. On the one hand, by adjusting the thickness of the barrier layer on the surface of the dielectric layer, the depth of the first conductive column in the first doped region is adjusted to ensure that the first conductive column and the first doped region have good conductivity; on the other hand, by adjusting the thickness of the barrier layer on the surface of the second doped region, the different etching rates of different materials are used to ensure that the etching depth in the second doped region is lower than the etching depth in the first doped region, so that the second conductive column is far away from the depletion region, which is conducive to improving the problem of excessive substrate leakage of the semiconductor structure, and thus is conducive to improving the stability of the semiconductor structure.
[0070] Some embodiments of the present application provide a method for preparing a semiconductor structure, and the method for preparing a semiconductor structure can form semiconductor structures provided by some of the following embodiments. The semiconductor structures provided by some embodiments of the present application will be described in detail below with reference to the accompanying drawings.
[0071] Fig.10 A schematic diagram of a semiconductor structure provided in accordance with an embodiment of the present application.
[0072] refer to Fig.10The semiconductor structure includes: a substrate 200, the substrate 200 includes a core region 201 and a peripheral region 202, and the substrate 200 of the core region 201 has a first gate 212, and the substrate 200 on opposite sides of the first gate 212 of the core region 201 has a first doping region 211, the substrate 200 exposes the top surface of the first doping region 211, and the top surface of the first doping region 211 has a dielectric layer 203; the substrate 200 of the peripheral region 202 has a second gate 222, and the substrate 200 on opposite sides of the second gate 222 of the peripheral region 202 has a second doping region 221; the first conductive column 246 is located in the first doping region 211 and protrudes from the surface of the substrate 200; the second conductive column 256 is located in the second doping region 221 and protrudes from the surface of the substrate 200, and the depth of the second conductive column 256 in the second doping region 221 is less than the depth of the first conductive column 246 in the first doping region 211.
[0073] In some embodiments, the core region 201 is used to connect the conductive structure to form a storage unit, and the peripheral region 202 is used to connect the conductive structure to form a logic unit to ensure that the function of the core region is realized.
[0074] The material of the substrate 200 is a semiconductor material. Specifically, in some embodiments, the material of the substrate 200 is silicon. In other embodiments, the material of the substrate may also be germanium, germanium silicon or silicon carbide.
[0075] In some embodiments, the first gate 212 of the core region 201 is a buried gate, and the second gate 222 of the peripheral region 202 is a planar gate.
[0076] The core region 101 further includes a first gate spacer 232 and a first gate cap layer 242 .
[0077] Specifically, the first gate spacer 232 covers the bottom wall and side wall of the first gate 212, and is used to prevent the mutual diffusion of particles of the first gate 212 and particles of the first doping region 211. The material of the first gate spacer 232 is metal oxide, such as titanium nitride, tantalum nitride, titanium or tantalum.
[0078] The first gate capping layer 242 covers the surface of the first gate 212, and is used to isolate the first gate 212 from the dielectric layer 203, wherein the material of the first gate capping layer 242 is an insulating material, for example, silicon dioxide, silicon carbide or silicon nitride. In some embodiments, the material of the first gate 212 is metal tungsten, and in other embodiments, the material of the first gate may also be other metal materials such as copper or aluminum.
[0079] Specifically, in some embodiments, the first gate 212 includes a first gate first conductive layer. In other embodiments, the first gate includes a first gate first conductive layer, a first gate dielectric layer and a first gate second conductive layer stacked in sequence, and the materials of the first gate first conductive layer and the first gate second conductive layer may be different.
[0080] The peripheral region 202 further includes a second gate oxide layer 252 covering the substrate 200 , and the second gate oxide layer 252 is located between the substrate 200 and the second gate 222 .
[0081] Specifically, the material of the second gate oxide layer 252 is an insulating material, for example, silicon dioxide, silicon carbide or silicon nitride, for isolating the second gate 222 from the substrate 200. In some embodiments, the second gate oxide layer 252 is made of the same material as the first gate cap layer 242. In other embodiments, the second gate oxide layer and the first gate cap layer may also be made of different materials.
[0082] In some embodiments, the material of the second gate 222 is tungsten. In other embodiments, the material of the second gate 222 may also be copper, aluminum or other metal materials. In some embodiments, the first gate 212 and the second gate 222 are made of the same material. In other embodiments, the first gate and the second gate may also be made of different materials.
[0083] Specifically, in some embodiments, the second gate 222 includes a second gate first conductive layer. In other embodiments, the second gate includes a second gate first conductive layer, a second gate dielectric layer and a second gate second conductive layer stacked in sequence, and the materials of the second gate first conductive layer and the second gate second conductive layer may be different.
[0084] The first doping region 211 is an N-type doping region, and the second doping region 221 can be an N-type doping region or a P-type doping region; in some embodiments, the first doping region 211 and the second doping region 221 are N-type doping regions, the substrate 200 is a P-type doping region, the first doping region 211 and the second doping region 221 are doped with N-type ions, and the substrate 200 is doped with P-type ions. In other embodiments, the doping region is a P-type doping region, the substrate is an N-type doping region, the doping region is doped with P-type ions, and the substrate is doped with N-type ions. Specifically, the doping ions of the second doping region 221 are boron ions among P-type ions. In other embodiments, the doping ions can also be phosphorus ions and arsenic ions among N-type ions and aluminum ions and boron fluoride ions among P-type ions.
[0085] For the first gate 212, the first doped region 211 located on one side of the first gate 212 serves as a source, and the first doped region 211 located on the other side of the first gate 212 serves as a drain; similarly, for the second gate 222, the second doped region 221 located on one side of the second gate 222 serves as a source, and the second doped region 221 located on the other side of the second gate 222 serves as a drain.
[0086] The dielectric layer 203 is located on the top surface of the first doped region 211, wherein the material of the dielectric layer 203 can be insulating materials such as silicon, silicon oxide, silicon carbide, silicon nitride, or other high dielectric constant materials. In some embodiments, the dielectric layer 203 covers the top surface of the first doped region 211, and the dielectric layer 203 also covers the upper surface of the first gate cap layer 242.
[0087] The first conductive pillar 246 is located in the first doped region 211 and protrudes from the surface of the substrate 200 , which is beneficial for the core region and the conductive pillar to have good conductivity.
[0088] Specifically, in some embodiments, the second conductive pillar 256 and the first conductive pillar 246 are made of the same material, tungsten. In other embodiments, the second conductive pillar and the first conductive pillar may be made of different materials.
[0089] The second conductive pillar 256 is located in the second doping region 221 and protrudes from the surface of the substrate 200 . The depth of the second conductive pillar 256 in the second doping region 221 is less than the depth of the first conductive pillar 246 in the dielectric layer 203 .
[0090] In this way, the distance between the second conductive column 256 and the PN junction depletion region within the second doping 221 increases, and under the influence of the high doping ion concentration, the width of the PN junction depletion region becomes narrower, which is beneficial for the doped ions to prepare excellent ohmic contact at the metal / semiconductor contact through the high doping ion concentration, effectively avoiding the situation where the contact resistance between the conductive contact structure and the semiconductor is too large, and is beneficial to improving the stability of the semiconductor structure.
[0091] The first metal silicide layer 245 is located between the first conductive pillar 246 and the first doped region 211 ; the second metal silicide layer 255 is located between the second conductive pillar 256 and the second doped region 221 , and the second metal silicide layer 255 is located on the bottom surface of the second conductive pillar 256 .
[0092] In some embodiments, the material of the first metal silicide layer 245 is cobalt silicide, which is used to reduce the resistance of the diffusion region and the contact resistance of the metal / semiconductor contact hole; in other embodiments, the first metal silicide layer can also be a metal silicide such as titanium silicide or nickel silicide. Similarly, in some embodiments, the material of the second metal silicide layer 255 and the first metal silicide layer 245 is the same, and in other embodiments, the material of the second metal silicide layer and the first metal silicide layer can also be different. Therefore, the contact resistance of the second metal silicide layer is small, which is beneficial to improving the conductive effect of the second conductive pillar and the second doped region.
[0093] Fig.11 Another structural schematic diagram of a semiconductor structure provided in an embodiment of the present application.
[0094] refer to Fig.11 In other embodiments, the second metal silicide layer is located on the bottom and side surfaces of the second conductive column. Therefore, the second metal silicide layer and the second doped region have a larger contact area. The larger the contact area, the smaller the contact resistance between the second metal silicide layer and the second doped region, which is beneficial to improving the conductive effect of the second metal silicide layer and the second doped region, thereby improving the stability of the semiconductor structure.
[0095] Continue to refer Fig.10 The second metal silicide layer 255 also contains fluorine ions. By doping fluorine ions and additionally injecting ions of the same type as the doping ions in the second doping region, the concentration of doping ions in the second doping region exposed by the second trench is increased, and the metal / semiconductor contact resistance is reduced.
[0096] Correspondingly, another embodiment of the present application further provides a semiconductor structure, which is substantially the same as the semiconductor structure provided in the aforementioned embodiment, with the main difference that the depth of the first conductive pillar of the semiconductor structure provided in another embodiment of the present application in the first doping region is less than the depth of the first conductive pillar of the semiconductor structure provided in the aforementioned embodiment in the first doping region, and the depth of the second conductive pillar of the semiconductor structure provided in another embodiment of the present application in the second doping region is also less than the depth of the second conductive pillar of the semiconductor structure provided in the aforementioned embodiment in the second doping region. The semiconductor structure provided in another embodiment of the present application will be described in detail below in conjunction with the accompanying drawings.
[0097] Fig. 20 A schematic structural diagram of a semiconductor structure provided in another embodiment of the present application.
[0098] refer to Fig. 20The semiconductor structure includes: a substrate 300, the substrate 300 includes a core region 301 and a peripheral region 302, and the substrate 300 of the core region 301 has a first gate 312, and the substrate 300 on opposite sides of the first gate 312 of the core region 301 has a first doping region 311, the substrate 300 exposes the top surface of the first doping region 311, and the top surface of the first doping region 311 has a dielectric layer 303; the substrate 300 of the peripheral region 302 has a second gate 322, and the substrate 300 on opposite sides of the second gate 322 of the peripheral region 302 has a second doping region 321; the first conductive column 346 is located in the first doping region 311 and protrudes from the surface of the substrate 300; the second conductive column 356 is located in the second doping region 321 and protrudes from the surface of the substrate 300, and the depth of the second conductive column 356 in the second doping region 321 is less than the depth of the first conductive column 346 in the first doping region 311.
[0099] The semiconductor structure provided in another embodiment of the present application is substantially the same as the semiconductor structure provided in the aforementioned embodiment, and will not be described in detail here.
[0100] Since the above-mentioned embodiments correspond to this embodiment, this embodiment can be implemented in conjunction with the above-mentioned embodiments. The relevant technical details mentioned in the above-mentioned embodiments are still valid in this embodiment, and the technical effects that can be achieved in the above-mentioned embodiments can also be achieved in this embodiment. In order to reduce repetition, they are not repeated here. Accordingly, the relevant technical details mentioned in this embodiment can also be applied to the above-mentioned embodiments; ordinary technicians in this field can understand that the above-mentioned embodiments are specific embodiments for implementing the present application, and in actual applications, various changes can be made to them in form and details without departing from the spirit and scope of the present application.
Claims
1. A method for preparing a semiconductor structure, characterized in that: include: A substrate is provided, wherein the substrate comprises a core region and a peripheral region, wherein the substrate in the core region has a first gate, wherein the substrate on two opposite sides of the first gate in the core region has first doped regions, wherein the substrate exposes a top surface of the first doped region, wherein the top surface of the first doped region has a dielectric layer; wherein the substrate in the peripheral region has a second gate, wherein the substrate on two opposite sides of the second gate in the peripheral region has second doped regions; forming a barrier layer on the substrate in the peripheral region, wherein the barrier layer is located on a surface of the second doped region; Forming a mask layer with openings on the substrate in the core area and the peripheral area, wherein the mask layer is also located on the surface of the barrier layer and the dielectric layer, and the material of the mask layer is different from that of the barrier layer; Using the mask layer as a mask, etching the dielectric layer and the first doped region in the core region along the opening to form a first trench in the first doped region, and also etching the barrier layer and the second doped region in the peripheral region along the opening to form a second trench in the second doped region, wherein the depth of the first trench is greater than the depth of the second trench; forming a first conductive column, wherein the first conductive column completely fills the first groove and protrudes from the surface of the substrate; A second conductive column is formed, wherein the second conductive column fills the second trench and protrudes from the surface of the substrate.
2. The method for preparing a semiconductor structure according to claim 1, characterized in that: The blocking layer is also located on the sidewall of the second gate in the peripheral region.
3. The method for preparing a semiconductor structure according to claim 1, characterized in that: The material of the barrier layer includes silicon oxide or silicon nitride.
4. The method for preparing a semiconductor structure according to claim 1, wherein: The process steps for forming the barrier layer include: forming a continuous initial barrier film on the substrate surface in the core region and the peripheral region; The initial barrier film located in the core area is removed, and the remaining initial barrier film serves as the barrier layer.
5. The method for preparing a semiconductor structure according to claim 1, wherein: The second doping region has doping ions, and the doping ions are one of N-type ions or P-type ions. The preparation method further includes: The second trench is pre-processed to increase the concentration of the doping ions in the second doping region exposed by the second trench.
6. The method for preparing a semiconductor structure according to claim 5, characterized in that: The pretreatment includes: a first pretreatment step, in which fluorine ions are doped into the surface of the second doping region exposed by the second groove; a second pretreatment step, in which ions of the same type as the doping ions of the second doping region are doped into the surface of the second doping region exposed by the second groove, and the ions of the same type as the doping ions of the second doping region are N-type ions or P-type ions.
7. The method for preparing a semiconductor structure according to claim 6, characterized in that: The doping ions are P-type ions, and the ions of the same type as the doping ions include boron fluoride ions.
8. The method for preparing a semiconductor structure according to claim 1, wherein: Before forming the first conductive pillar and the second conductive pillar, the method further includes: forming a first metal silicide layer on a surface of the first trench, wherein the first metal silicide layer is located between the first conductive pillar and the first doped region; A second metal silicide layer is formed on the surface of the second trench, and the second metal silicide layer is located between the second conductive pillar and the second doped region.
9. The method for preparing a semiconductor structure according to claim 8, characterized in that: The process steps of forming the first metal silicide layer and the second metal silicide layer include: forming a metal layer, wherein the metal layer is located on a surface of the first groove, a surface of the second groove, and a surface of the barrier layer directly above the second groove; Performing annealing treatment, the metal layer reacts with the first doping region to form the first metal silicide layer, and the metal layer reacts with the second doping region to form the second metal silicide layer; The unreacted metal layer is removed.
10. The method for preparing a semiconductor structure according to claim 1, wherein: The process steps of forming the first conductive pillar and the second conductive pillar include: forming a conductive film that fills the first trench, the second trench, and the opening, and the conductive film is also located on the top surface of the mask layer; The conductive film above the top surface of the mask layer is removed, and the remaining conductive film located in the core area serves as the first conductive column, and the remaining conductive film located in the peripheral area serves as the second conductive column.
11. The method for preparing a semiconductor structure according to claim 1, characterized in that: After forming the first conductive pillar and the second conductive pillar, the method further includes: removing the mask layer.
12. A semiconductor structure, characterized in that: include: A substrate, the substrate comprising a core region and a peripheral region, wherein the substrate in the core region has a first gate, the substrate on opposite sides of the first gate in the core region has first doped regions, the substrate exposes a top surface of the first doped region, the top surface of the first doped region has a dielectric layer; the substrate in the peripheral region has a second gate, the substrate on opposite sides of the second gate in the peripheral region has second doped regions; A first conductive column, the first conductive column is located in the first doping region and protrudes from the surface of the substrate; The second conductive column is located in the second doping region and protrudes from the surface of the substrate, and the depth of the second conductive column in the second doping region is less than the depth of the first conductive column in the first doping region.
13. The semiconductor structure according to claim 12, wherein: Also includes: a first metal silicide layer, wherein the first metal silicide layer is located between the first conductive pillar and the first doped region; A second metal silicide layer is located between the second conductive pillar and the second doped region.
14. The semiconductor structure according to claim 13, wherein: The second metal silicide layer is located on the bottom surface of the second conductive column.
15. The semiconductor structure according to claim 14, wherein: The second metal silicide layer is also located on a side of the second conductive pillar.
16. The semiconductor structure according to claim 13, wherein: The second metal silicide layer further contains fluorine ions.
Citation Information
Patent Citations
Memory structure and forming method thereof
CN106298788A
Semiconductor structure and formation method thereof
CN110211959A