A method for preparing alcohol by hydroformylation of olefins

By using a cobalt-phosphine complex catalyst and two reactors in the hydroformylation reaction, the problem of high alkane selectivity and low alcohol selectivity is solved, which improves alcohol selectivity and reduces waste liquid Emissions have achieved improvements in economic benefits and environmental protection.

CN116063155BActive Publication Date: 2024-12-06CHINA PETROLEUM & CHEMICAL CORP +1
View PDF 9 Cites 0 Cited by

Patent Information

Application Number
CN202111270396.8
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2021-10-29
Publication Date
2024-12-06
Estimated Expiration
2041-10-29

AI Technical Summary

Technical Problem

In the existing hydroformylation reaction, the selectivity of alkanes and the selectivity of alcohols are high, resulting in reduced economic benefits of the device and environmental pollution problems.

Method used

Using cobalt-phosphine complex catalyst, the hydroformylation reaction is carried out in two reactors, and the reaction is participated by separation of the recombinant components, reducing alkane selectivity and improving alcohol selectivity, and processing heavy materials through the second reactor To reduce waste liquid emissions.

Benefits of technology

It significantly improves alcohol selectivity, reduces waste liquid emissions, reduces plant investment and processing costs, and has good industrial application prospects.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure BDA0003328566520000091
    Figure BDA0003328566520000091
Patent Text Reader

Abstract

The present invention relates to the field of hydroformylation reaction, and discloses a method for preparing alcohol by hydroformylation of olefins, the method comprising: (1) in the presence of a cobalt-phosphine complex catalyst, 8 ‑C 30 Olefins and synthesis gas are introduced into a first reactor for a first contact reaction to obtain a first mixture; (2) the synthesis gas and the first mixture are introduced into a second reactor for a second contact reaction to obtain a second mixture; the volume of the second reactor is smaller than the volume of the first reactor; (3) the second mixture is separated to obtain light components and heavy components respectively; (4) the heavy components are recycled. The method has a simple process flow, a high olefin conversion rate, a high target product yield, a low alkane selectivity, and can significantly reduce waste liquid discharge, and has good industrial application prospects.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the field of hydroformylation reaction, and in particular to a method for preparing alcohol by hydroformylation of olefins. Background Art

[0002] Olefins react with carbon monoxide and hydrogen in the presence of a catalyst to undergo hydroformylation. The hydroformylation process includes contacting an olefinic unsaturated compound with carbon monoxide and hydrogen in the presence of a catalyst under reaction conditions to produce one or more aldehydes and alcohols. The catalyst used in the hydroformylation reaction in industrial production is generally a cobalt (Co)-based or rhodium (Rh)-based catalyst.

[0003] CN102123978A discloses a method for hydroformylating alpha-olefins to produce two or more aldehydes comprising normal aldehydes and one or more isomeric aldehydes, wherein the target molar ratio of the normal aldehyde to the one or more isomeric aldehydes is within a selectable range of 3 / 1-60 / 1. The method uses a transition metal-ligand complex catalyst comprising a symmetrical calixarene diphosphite ligand.

[0004] CN108586219A discloses a method for preparing aldehyde by hydroformylation of olefins, and the preparation method is as follows: step 1: C2-C4 olefins are subjected to hydroformylation reaction with carbon monoxide and hydrogen in the presence of a catalyst in a first reactor to continuously prepare aldehyde, while the temperature is 90°C and the pressure is 2.5MPa; step 2: heating is performed in a second reactor at a temperature of 70-80°C, and an inert gas is introduced into the second reactor; step 3: the first reactor is connected to the second reactor, and the aldehyde prepared in the first reactor is introduced into the second reactor; step 4: during the introduction in step 3, the aldehyde is introduced under isobaric and unequal temperature conditions, and a secondary introduction is performed after the introduction; the reaction process of this technology is complicated, and a rhodium-phosphine complex catalyst is used, which is expensive.

[0005] Compared with cobalt catalysts, rhodium complexes have higher reaction activity and can react at milder temperatures and pressures. However, rhodium catalysts are resistant to high temperature differences and are difficult to use for advanced olefin carbonylation. Existing rhodium catalysts have good catalytic effects on terminal olefins, but have low activity on internal olefins. The catalyst is oil-soluble and product separation is also difficult, making post-processing more complicated. Rhodium is a scarce and expensive precious metal resource, and its recovery and reuse costs are high.

[0006] CN1370137A discloses a continuous process for the hydroformylation of olefins having 6 to 20 carbon atoms, wherein: a) an aqueous solution of a cobalt (II) salt is brought into contact with hydrogen and carbon monoxide to form a hydroformylation active cobalt catalyst, and then an aqueous phase containing the cobalt catalyst is brought into contact with olefins and optionally an organic solvent as well as hydrogen and carbon monoxide in at least one reaction zone, wherein the cobalt catalyst is extracted into the organic phase and the olefins are hydroformylated, b) the effluent from the reaction zone is treated with oxygen in the presence of an acidic aqueous solution of a cobalt (II) salt, wherein the cobalt catalyst decomposes to form cobalt (II) salts and these are stripped into the aqueous phase; and the phases are subsequently separated, and c) the aqueous solution of the cobalt (II) salt is recycled to step a in an unchanged form. The process of this process is complex.

[0007] In the hydroformylation reaction process, higher alkane selectivity reduces the economic benefits of the device. Reducing alkane selectivity and increasing isononanol and isononanal selectivity can improve the economic efficiency of the device. Reducing the content of heavy substances in the reaction products can reduce the amount of heavy materials discarded and the amount of waste liquid discarded from the device, which is beneficial to environmental protection. Summary of the invention

[0008] The purpose of the present invention is to overcome the defects of the prior art method for preparing aldols, that is, the alkane selectivity is high but the alcohol selectivity is low.

[0009] In order to achieve the above object, the present invention provides a method for preparing alcohol by hydroformylation of olefins, the method comprising:

[0010] (1) In the presence of a cobalt-phosphine complex catalyst, C8-C 30 The olefin and the synthesis gas are introduced into a first reactor for a first contact reaction to obtain a first mixture;

[0011] (2) introducing the synthesis gas and the first mixture into a second reactor for a second contact reaction to obtain a second mixture; the volume of the second reactor is smaller than the volume of the first reactor, and the volume of the first reactor is 2 to 30 times the volume of the second reactor;

[0012] (3) separating the second mixture to obtain a light component and a heavy component, respectively; the light component contains alcohol, aldehyde and alkane, and the heavy component contains a cobalt-phosphine complex catalyst;

[0013] (4) recycling the heavy components accounting for more than 50 wt % of the total heavy components obtained in step (3) to participate in the first contact reaction.

[0014] The invention provides a process for preparing alcohol by olefin hydroformylation reaction. The method has simple process flow, high olefin conversion rate, high target product yield, low alkane selectivity, can greatly reduce waste liquid discharge, and has good industrial application prospects. DETAILED DESCRIPTION

[0015] The endpoints and any values ​​of the ranges disclosed in this article are not limited to the precise ranges or values, and these ranges or values ​​should be understood to include values ​​close to these ranges or values. For numerical ranges, the endpoint values ​​of each range, the endpoint values ​​of each range and the individual point values, and the individual point values ​​can be combined with each other to obtain one or more new numerical ranges, which should be considered as specifically disclosed in this article.

[0016] As mentioned above, the present invention provides a method for preparing alcohol by hydroformylation of olefins, the method comprising:

[0017] (1) In the presence of a cobalt-phosphine complex catalyst, C8-C 30 The olefin and the synthesis gas are introduced into a first reactor for a first contact reaction to obtain a first mixture;

[0018] (2) introducing the synthesis gas and the first mixture into a second reactor for a second contact reaction to obtain a second mixture; the volume of the second reactor is smaller than the volume of the first reactor, and the volume of the first reactor is 2 to 30 times the volume of the second reactor;

[0019] (3) separating the second mixture to obtain a light component and a heavy component, respectively; the light component contains alcohol, aldehyde and alkane, and the heavy component contains a cobalt-phosphine complex catalyst;

[0020] (4) recycling the heavy components accounting for more than 50 wt % of the total heavy components obtained in step (3) to participate in the first contact reaction.

[0021] In step (4), the heavy components accounting for more than 50 wt% of the total heavy components obtained in step (3) can be recycled back to the inlet of the first reactor.

[0022] The present invention converts olefin into isononanal, isononanol, C9 condensate and ester compounds in a first reactor, and then converts the C9 condensate, ester compounds and isononanal into isononanol in a second reactor.

[0023] The inventors of the present invention have found in their research that according to the above-mentioned two-stage reaction process, the selectivity of alkanes can be reduced and the selectivity of alcohols and aldehydes can be improved. The second reactor can reduce the content of heavy substances such as C9 condensates and ester compounds and aldehydes in the product, further improving the alcohol selectivity.

[0024] Analysis shows that the content of heavy substances such as C9 condensate and ester compounds and aldehydes in the product of the first reactor is significantly increased. The inventors of the present invention propose that this part of the material is sent to a second reactor with a smaller volume, and synthesis gas is introduced but olefins are not introduced, and post-treatment is carried out under the conditions of hydroformylation reaction. Unexpectedly, the heavy substances such as C9 condensate and ester compounds and heavy substances such as aldehydes will be decomposed into products such as alcohols again, which not only further increases the yield of the target product, but also can significantly reduce the amount of external materials, thereby significantly reducing waste liquid discharge and alleviating environmental problems of the hydroformylation process.

[0025] More preferably, the volume of the first reactor is 2-10 times the volume of the second reactor.

[0026] Preferably, the conditions of the first contact reaction are controlled so that the first mixture contains isononanal, isononanol, C9 condensate, and ester compounds.

[0027] According to a preferred specific embodiment, the method further comprises: before the first contact reaction, the cobalt-phosphine complex catalyst is introduced into a pretreatment reactor for a pretreatment reaction, wherein the pretreatment is carried out in the presence of synthesis gas. Catalyst pretreatment is conducive to the formation of active units of the cobalt-phosphine catalyst, reduces catalyst decomposition, improves the activity and stability of the catalyst, and prolongs the service life of the catalyst.

[0028] Preferably, the conditions of the pretreatment reaction include: temperature of 50°C to 150°C, more preferably 75°C to 130°C; pressure of 0.1MPa to 12MPa, preferably 1MPa to 9MPa, more preferably 3MPa to 8MPa; pretreatment time of 0.1 to 10h, more preferably 1 to 3h.

[0029] Preferably, if pretreatment is performed, the material containing the cobalt phosphine complex catalyst can be recycled to the inlet of the pretreatment reactor for reuse. That is, preferably, in step (4), the heavy components accounting for more than 50 wt% of the total heavy components obtained in step (3) are recycled back to the pretreatment reactor.

[0030] According to the method of the present invention, when the material containing the cobalt-phosphine complex catalyst is returned to the hydroformylation reactor (the aforementioned first reactor and / or second reactor) and / or the inlet of the pretreatment reactor, a small amount of new catalyst can be added as needed.

[0031] Preferably, the pretreatment reactor is an autoclave or a tubular reactor.

[0032] According to a preferred embodiment, the initial cobalt mass concentration in the first contact reaction system is 0.01%-3%, preferably 0.2%-2%; more preferably 0.3%-1.5%. The cobalt mass concentration = (mass of cobalt / mass of catalyst solution) × 100%.

[0033] According to a preferred embodiment, the method of the present invention further comprises preparing the cobalt-phosphine complex catalyst in solution by an operation comprising the following steps: mixing a cobalt-containing raw material with a phosphine ligand for reaction in the presence of a solvent.

[0034] Preferably, in the method for preparing the cobalt-phosphine complex catalyst in solution, the contact reaction is carried out in the presence of CO and / or H2.

[0035] Preferably, in the method for preparing the cobalt-phosphine complex catalyst in solution, the contact reaction conditions include: temperature of 80-180°C, more preferably 100-150°C; pressure of 0.1-6MPa, more preferably 1-4MPa; time of 0.5-24h, more preferably 1-15h.

[0036] Preferably, in the method for preparing the cobalt-phosphine complex catalyst in solution, the cobalt-containing raw material is a cobalt salt or a cobalt oxide; more preferably, the cobalt-containing raw material is selected from at least one of cobalt carbonate, cobalt nitrate, cobalt acetate, cobalt levulinate, cobalt formate, dicobalt octacarbonyl and cobalt cyclopentaneate.

[0037] Preferably, in the method for preparing the cobalt-phosphine complex catalyst in solution, the phosphine ligand is selected from at least one of phosphites, triphenylphosphine, trialkylphosphine, di-(triphenylphosphine), and alkylphenylphosphine.

[0038] Preferably, in the method for preparing the cobalt-phosphine complex catalyst in solution, the mass ratio of cobalt element to phosphorus element in the cobalt-phosphine complex catalyst solution is (0.1-3):1, preferably (0.2-2):1, and more preferably (0.3-1):1.

[0039] The solvent in the method for preparing the cobalt-phosphine complex catalyst in solution of the present invention can dissolve the cobalt complex catalyst, and can be a solvent known in the art, such as olefins, alkanes, alcohols, etc., preferably including various types of alcohols of C1 to C20. In addition, the solvent can contain products or raw materials. In addition, the solvent of the cobalt-phosphine complex catalyst can also be the solvent in the catalyst circulating liquid. Specific solvents are exemplified in the examples of the present invention, which should not be construed as limiting the present invention by those skilled in the art.

[0040] Preferably, the cobalt-phosphine complex catalyst in solution is 30The mass ratio of olefin usage is (0.1-10):1, more preferably (2-5):1.

[0041] Preferably, the C8-C 30 The olefin is selected from 2,4,4-trimethyl-1-pentene and 2,4,4-trimethyl-2-pentene. The difficulty of hydroformylation of trimethyl poly-branched olefins is higher than that of less-branched olefins due to their large steric hindrance.

[0042] Preferably, each of the synthesis gases independently contains carbon monoxide and hydrogen in a molar ratio of 4:1 to 1:4. More preferably, each of the synthesis gases independently contains carbon monoxide and hydrogen in a molar ratio of 3:1 to 1:3.

[0043] Preferably, both the first reactor and the second reactor are tubular reactors. Preferably, olefins, synthesis gas and a solution containing a catalyst flow into the lower part of the tubular reactor, and the reaction product flows out from the upper part of the tubular reactor. Alternatively, the olefins flow into the upper part of the tubular reactor, and the reaction product flows out from the lower part of the tubular reactor. After the reaction is completed, part of the alcohol, aldehyde, alkane and olefin raw materials are distilled off from the crude reaction product, and the remaining solution containing the catalyst is circulated to the pre-reactor for pretreatment. After the pretreatment, the catalyst solution is sent to the inlet of the hydroformylation reactor and re-enters the reactor for use.

[0044] The synthesis gas can flow in from the lower part of the pretreatment reactor and / or the hydroformylation reactor, and can also flow in from the lower parts of multiple hydroformylation reactors. In addition, the ratio of CO to H2 in the synthesis gas flowing into different reactors can be the same or different. This can facilitate the adjustment of the ratio between olefins and CO and H2 in each reactor to the optimal ratio, which is conducive to higher conversion rate and better selectivity.

[0045] Preferably, the conditions in the first reactor at least meet the following requirements: the reaction temperature is 60°C to 150°C, preferably 100°C to 145°C; the reaction pressure is 1MPa to 12MPa, preferably 2MPa to 10MPa.

[0046] The present invention has no particular requirement for the average residence time in the first reactor. Exemplarily, the average residence time is 1 to 60 hours, preferably 3 to 25 hours.

[0047] Preferably, the conditions in the second reactor at least meet the following requirements: reaction temperature is 140°C to 200°C, preferably 170°C to 190°C; reaction pressure is 1MPa to 12MPa, preferably 2MPa to 10MPa.

[0048] The present invention has no particular requirements for the average residence time in the second reactor. Exemplarily, the average residence time is 1 to 40 hours, preferably 1 to 25 hours, and more preferably 1 to 8 hours.

[0049] Preferably, in step (1), the synthesis gas and the C8-C 30 The molar ratio of olefins is (1-12):1, more preferably (3-6):1.

[0050] The separation of the present invention can be performed by first performing gas-liquid separation and then performing distillation separation. The gas phase logistics obtained after gas-liquid separation is basically synthesis gas, and after condensation and / or absorption, the remaining synthesis gas can be circulated to at least one inlet of the pretreatment reactor, the first reactor, and the second reactor for repeated use. The liquid phase logistics after gas-liquid separation can be distilled and separated by a distillation device, and the top discharge is a mixed product containing alcohol, alkane and aldehyde, and the bottom obtains a heavy material containing a cobalt-phosphine complex catalyst and / or a solvent.

[0051] Preferably, in step (3), the separation is carried out in a gas-liquid separation tank under conditions of lowering the temperature but not the pressure.

[0052] Preferably, the separation temperature is 0°C-100°C, more preferably 20°C-80°C, more preferably 20°C-40°C.

[0053] Preferably, if the target product is to obtain more alcohol, the obtained mixture of alcohol and aldehyde can also be hydrogenated to convert the aldehyde into alcohol.

[0054] Preferably, the method of the present invention may further include the use of a hydrogenation device, and the alcohol and aldehyde obtained from the product distillation tower and the external feed distillation tower may be further hydrogenated to obtain alcohol with a high yield.

[0055] The present invention has at least the following advantages:

[0056] 1. The price of cobalt catalyst is lower than that of rhodium catalyst, and the hydroformylation reaction temperature in the first reactor is significantly reduced, which is conducive to the stability of the cobalt catalyst.

[0057] 2. The present invention can significantly reduce alkane selectivity, lower aldehyde selectivity and increase alcohol selectivity, thus significantly improving the economic benefits of the process.

[0058] 3. In the scheme of the present invention, a second reactor is used to process materials containing condensates and heavy substances. The condensates and heavy substances can be decomposed into products such as alcohols again, which can improve alcohol selectivity, significantly reduce the amount of external materials, reduce waste liquid discharge, is beneficial to environmental protection, and has industrial prospects.

[0059] 4. The catalyst pretreatment process in the preferred embodiment of the present invention can reduce the decomposition of the cobalt-phosphine catalyst, is conducive to the formation of active units of the cobalt-phosphine catalyst, improves the activity and stability of the catalyst, and prolongs the service life of the catalyst.

[0060] 5. The scheme of the present invention is applicable to a wide range of olefin raw materials, especially to the hydroformylation reaction of multi-branched olefins with large steric hindrance. The reaction pressure is low, and the device investment and processing costs are significantly reduced.

[0061] The present invention will be described in detail below by way of examples. In the following examples, unless otherwise specified, the raw materials used are all common commercially available products.

[0062] The olefin raw material in the example is a commercially available C8 olefin, and the composition is: 75.1 wt % of 2,4,4-trimethyl-1-pentene, 21.2 wt % of 2,4,4-trimethyl-2-pentene, and the rest are multi-branched olefins.

[0063] The following formula for calculating the raw material conversion rate is: [1-(the mass of 2,4,4-trimethyl-1-pentene and 2,4,4-trimethyl-2-pentene in the reaction product) / (the mass of 2,4,4-trimethyl-1-pentene and 2,4,4-trimethyl-2-pentene in the raw material)]×100%

[0064] Catalyst Preparation Example 1

[0065] Cobalt cyclohexanecarboxylate and triphenylphosphine were dissolved in isononanol in such amounts that the cobalt content of the solution was 0.12 wt% and the phosphorus content was 0.09 wt%. The air was replaced with synthesis gas H2 / CO (volume ratio 2:1), and the synthesis gas was introduced to a pressure of 1.7 MPa. The mixture was stirred at 400 rpm and reacted at 140°C for 9 hours to obtain a cobalt-phosphine catalyst solution A1.

[0066] The composition of the catalyst is shown in Table 1.

[0067] Catalyst Preparation Example 2

[0068] Cobalt cyclohexanecarboxylate and triphenylphosphine were dissolved in isononanol in such amounts that the cobalt content in the obtained solution was 0.10 wt% and the phosphorus content was 0.07 wt%. The air was replaced with synthesis gas H2 / CO (volume ratio 2:1), and the synthesis gas was introduced to a pressure of 1.8 MPa. The mixture was stirred at 400 rpm and reacted at 140°C for 9 hours to obtain a cobalt-phosphine catalyst solution A2.

[0069] The composition of the catalyst is shown in Table 1.

[0070] Table 1

[0071]

[0072] Example 1

[0073] The catalyst solution A1 (which has been recycled and reused many times in the olefin hydroformylation process) and the C8 olefin are introduced into the first hydroformylation reactor at a ratio of 83g:30g. The volume of the first hydroformylation reactor is 7 times that of the second hydroformylation reactor. Synthesis gas (CO / H2 molar ratio is 1:2) is added. The temperature of the first hydroformylation reactor is 130°C and the pressure is 8MPa. The reaction discharge is analyzed by chromatography, wherein 3.5wt% of 2.4.4-trimethylpentane, condensation products of at least two C9 molecules and 37.2wt% of ester compounds formed by two C9 molecules are included.

[0074] The material flowing out of the first hydroformylation reactor enters the second hydroformylation reactor. The temperature of the second hydroformylation reactor is 180° C. and the pressure is 8 MPa. 3 wt% (based on the total weight of the material flowing out of the first hydroformylation reactor) of water is added. Compared with the feed to the second hydroformylation reactor, the heavy components of the condensation product of at least two C9 molecules and the ester compound formed by two C9 molecules in the reaction discharge are reduced by 95.3 wt% of the heavy components in the feed to the second hydroformylation reactor, the isononanol in the product is increased by 44.7 wt% of the isononanol in the feed to the second hydroformylation reactor, and the content of 2.2.4-trimethylpentane is basically the same as that in the feed to the second hydroformylation reactor, and the raw materials are almost completely converted.

[0075] Comparative Example 1

[0076] Compared with Example 1, this comparative example only uses the second hydroformylation reactor, the reaction temperature is 180° C., and the rest are the same as Example 1. After the reaction, the raw material conversion rate is lower than that of Example 1, and the proportion of 2.2.4-trimethylpentane in the product is twice that of 2.2.4-trimethylpentane in Example 1.

[0077] Example 2

[0078] The catalyst solution A2 (which has been recycled and reused many times in the olefin hydroformylation process) and the C8 olefin are introduced into the first hydroformylation reactor at a ratio of 83g:30g. The volume of the first hydroformylation reactor is 5 times that of the second hydroformylation reactor. Synthesis gas (CO / H2 molar ratio is 1:2) is added. The temperature of the first hydroformylation reactor is 145°C and the pressure is 8MPa. The reaction discharge is analyzed by chromatography, wherein the content is 4.2wt% of 2.2.4-trimethylpentane, condensation products of at least two C9 molecules and ester compounds formed by two C9 molecules are 20.6wt%.

[0079] The material flowing out of the first hydroformylation reactor enters the second hydroformylation reactor, the temperature of the second hydroformylation reactor is 180° C., and the pressure is 8 MPa. Compared with the feed to the second hydroformylation reactor, the heavy components of the condensation product of at least two C9 molecules and the ester compound formed by two C9 molecules in the product are reduced by 69.1wt% of the heavy components in the feed to the second hydroformylation reactor, the isononanol in the reaction discharge is increased by 13.6% of the isononanol in the feed to the second hydroformylation reactor, the content of 2.2.4-trimethylpentane is basically the same as that in the feed to the second hydroformylation reactor, and the raw materials are almost completely converted.

[0080] Example 3

[0081] The catalyst solution A1 (which has been recycled and reused many times in the olefin hydroformylation process) and the C8 olefin are introduced into the first hydroformylation reactor at a ratio of 83g:30g. The volume of the first hydroformylation reactor is 6 times that of the second hydroformylation reactor. Synthesis gas (CO / H2 molar ratio is 1:2) is added. The temperature of the first hydroformylation reactor is 140°C and the pressure is 8MPa. The reaction discharge is subjected to chromatographic analysis, which shows 3.8wt% of 2.2.4-trimethylpentane, condensation products of at least two C9 molecules and 18.1wt% of ester compounds formed by two C9 molecules.

[0082] The material flowing out of the first hydroformylation reactor enters the second hydroformylation reactor, the temperature of the second hydroformylation reactor is 180° C., and the pressure is 8 MPa. Compared with the feed to the second hydroformylation reactor, the heavy components of the condensation product of at least two C9 molecules and the ester compound formed by two C9 molecules in the product are reduced by 75.1wt% of the heavy components in the feed to the second hydroformylation reactor, the isononanol in the reaction discharge is increased by 21.5% of the isononanol in the feed to the second hydroformylation reactor, the content of 2.2.4-trimethylpentane is basically the same as that in the feed to the second hydroformylation reactor, and the raw materials are almost completely converted.

[0083] It can be seen from the above results that the present invention can significantly reduce alkane selectivity and improve alcohol selectivity.

[0084] The preferred embodiments of the present invention are described in detail above, but the present invention is not limited thereto. Within the technical concept of the present invention, the technical solution of the present invention can be subjected to a variety of simple modifications, including the combination of various technical features in any other suitable manner, and these simple modifications and combinations should also be regarded as the contents disclosed by the present invention and belong to the protection scope of the present invention.

Claims

1. A method for preparing alcohols by hydroformylation of olefins, characterized in that: The method includes: (1) In the presence of a cobalt-phosphine complex catalyst, C8 olefin and synthesis gas are introduced into a first reactor for a first contact reaction to obtain a first mixture; Controlling the conditions of the first contact reaction so that the first mixture contains isononanal, isononanol, C9 condensate, and ester compounds; (2) introducing the synthesis gas and the first mixture into a second reactor for a second contact reaction to obtain a second mixture; the volume of the second reactor is smaller than the volume of the first reactor, and the volume of the first reactor is 2 to 10 times the volume of the second reactor; (3) separating the second mixture to obtain a light component and a heavy component, respectively; the light component contains alcohol, aldehyde and alkane, and the heavy component contains a cobalt-phosphine complex catalyst; (4) recycling the heavy components accounting for more than 50 wt % of the total heavy components obtained in step (3) to participate in the first contact reaction; The conditions in the first reactor at least meet the following requirements: reaction temperature is 100°C to 145°C, reaction pressure is 2MPa to 10MPa; The conditions in the second reactor at least meet the following requirements: reaction temperature is 170° C. to 190° C., and reaction pressure is 2 MPa to 10 MPa.

2. The method according to claim 1, wherein: The method further comprises: before carrying out the first contact reaction, introducing the cobalt-phosphine complex catalyst into a pretreatment reactor for a pretreatment reaction, wherein the pretreatment is carried out in the presence of synthesis gas.

3. The method according to claim 2, wherein: The conditions of the pretreatment reaction include: temperature of 50° C. to 180° C., pressure of 0.1 MPa to 12 MPa, and pretreatment time of 0.1 to 10 h.

4. The method according to claim 3, wherein: The conditions of the pretreatment reaction include: temperature of 50° C. to 150° C., pressure of 1 MPa to 9 MPa, and pretreatment time of 1 to 3 hours.

5. The method according to claim 4, wherein: The conditions of the pretreatment reaction include: a temperature of 75° C. to 130° C. and a pressure of 3 MPa to 8 MPa.

6. The method according to any one of claims 2 to 5, wherein: In step (4), the heavy components accounting for more than 50 wt% of the total heavy components obtained in step (3) are recycled back to the pretreatment reactor.

7. The method according to claim 2, wherein: The pretreatment reactor is an autoclave or a tubular reactor.

8. The method according to any one of claims 1 to 5, wherein: The initial cobalt mass concentration in the system of the first contact reaction is 0.01%-3%.

9. The method according to claim 8, wherein: The initial cobalt mass concentration in the system of the first contact reaction is 0.2% to 2%.

10. The method according to any one of claims 1 to 5, wherein: The mass ratio of the cobalt-phosphine complex catalyst in solution to the C8 olefin is (0.1-10):

1.

11. The method according to claim 10, wherein: The mass ratio of the cobalt-phosphine complex catalyst in solution to the C8 olefin is (2-5):

1.

12. The method according to claim 8, wherein: The method also includes preparing the cobalt-phosphine complex catalyst in solution by adopting the following steps: mixing a cobalt-containing raw material with a phosphine ligand for reaction in the presence of a solvent.

13. The method according to claim 12, wherein: The mixed reaction is carried out in the presence of CO and / or H2.

14. The method according to claim 12, wherein: The conditions of the mixed reaction include: temperature of 80-180° C., pressure of 0.1-6 MPa, and time of 0.5-24 h.

15. The method according to claim 14, wherein: The conditions of the mixed reaction include: temperature of 100-150° C., pressure of 1-4 MPa, and time of 1-15 h.

16. The method according to claim 12, wherein: The cobalt-containing raw material is a cobalt salt or a cobalt oxide.

17. The method according to claim 16, wherein: The cobalt-containing raw material is selected from at least one of cobalt carbonate, cobalt nitrate, cobalt acetate, cobalt levulinate, cobalt formate, dicobalt octacarbonyl and cobalt naphthenate.

18. The method according to claim 12, wherein: The phosphine ligand is selected from at least one of phosphites, triphenylphosphine, trialkylphosphine, di-(triphenylphosphine), and alkylphenylphosphine.

19. The method according to any one of claims 1 to 5, wherein: The C8 olefin is selected from 2,4,4-trimethyl-1-pentene and 2,4,4-trimethyl-2-pentene.

20. The method according to any one of claims 1 to 5, wherein: Each of the synthesis gases independently contains carbon monoxide and hydrogen in a molar ratio of 4:1 to 1:

4.

21. The method according to claim 20, wherein: Each of the synthesis gases independently contains carbon monoxide and hydrogen in a molar ratio of 3:1 to 1:

3.

22. The method according to any one of claims 1 to 5, wherein: The first reactor and the second reactor are both tubular reactors.

23. The method according to any one of claims 1 to 5, wherein: In step (1), the molar ratio of the synthesis gas to the C8 olefin is (1-12):

1.

24. The method according to claim 23, wherein: In step (1), the molar ratio of the synthesis gas to the C8 olefin is (3-6):

1.

25. The method according to any one of claims 1 to 5, wherein: In step (3), the separation is carried out in a gas-liquid separation tank under the condition of lowering the temperature but not the pressure.

26. The method according to any one of claims 1 to 5, wherein: In step (3), the separation temperature is 0°C-100°C.

27. The method according to claim 26, wherein: In step (3), the separation temperature is 20°C-80°C.

Citation Information

Patent Citations

  • Hydroformylation process using a symmetric bisphosphite ligand for improved control over product isomers

    CN102123978A

  • Method for preparing aldehyde through hydroformylation reaction of olefin

    CN108586219A

  • Continuous process for hydroformylating olefins with 6 to 20 carbon atoms

    CN1370137A

  • Hydroformylation process