A method for pretreating coal tar raw materials

Through the combination of diluent and adsorbent, coal tar is treated under hydrogen conditions, and the problems of low pretreatment efficiency and environmental pollution in the existing technology are solved, and the effect of efficient removal of impurities and environmental protection is achieved, which is extended. The operation cycle of the hydrogen refueling device.

CN116064158BActive Publication Date: 2024-12-06CHINA PETROLEUM & CHEMICAL CORP +1
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202111273319.8
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2021-10-29
Publication Date
2024-12-06
Estimated Expiration
2041-10-29

AI Technical Summary

Technical Problem

The existing coal tar pretreatment methods are inefficient, have low resource utilization, and the introduction of water causes environmental pollution, making it difficult to meet the operation needs of hydrogen refueling devices.

Method used

After mixing the diluent with coal tar, solid-liquid separation is performed. Combined with adsorption treatment and reaction of pretreatment agent under hydrogen conditions, the metal and ash content in coal tar is effectively reduced and the operation cycle of the hydrogenation device is extended.

Benefits of technology

It has achieved efficient removal of impurities from coal tar, reduced energy consumption and investment, avoided water pollution, met environmental protection requirements, and simplified process flow.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN116064158B_ABST
    Figure CN116064158B_ABST
Patent Text Reader

Abstract

The present invention relates to a method for pretreating coal tar raw materials, the method comprising: S1, mixing the coal tar raw materials with a diluent and performing solid-liquid separation to obtain a solid phase material and a first liquid phase material; wherein the diluent contains hydrogenation product oil and an organic compound solvent; S2, contacting the first liquid phase material with an adsorbent for adsorption treatment to obtain a second liquid phase material; S3, contacting the second liquid phase material with a pretreatment agent under hydrogenation conditions for pretreatment reaction, and performing gas-liquid separation on the obtained pretreatment reaction product. The method of the present invention can effectively reduce the content of metals and ash in coal tar and extend the operation cycle of the hydrogenation device.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to a method for pretreating coal tar raw materials. Background Art

[0002] With the rapid development of social economy, my country's demand for petroleum products is also increasing. However, petroleum is a non-renewable energy source and is facing the crisis of depletion. In contrast, China's coal reserves are relatively abundant. Therefore, making liquid fuel from coal has become a basic direction of coal processing and utilization.

[0003] With the rapid development of modern coal chemical industry, the output of coal tar is increasing, and the clean processing and effective utilization of coal tar are becoming more and more important. At present, the main utilization of coal tar is deep processing to extract chemical products or hydrogenation to produce clean fuels. In recent years, the number of fixed-bed coal tar hydrogenation units in China has increased. Among them, fixed-bed hydrogenation units have the characteristics of simple process, small investment, simple operation and high technical maturity. However, when processing coal tar raw materials with high metal and ash content, it is easy to cause bed blockage, rapid pressure drop and rapid catalyst deactivation, etc., and the unit is forced to shut down, and the start-up time of the unit is shortened, which seriously affects the economic benefits of the enterprise.

[0004] Therefore, in order to extend the operating cycle of the coal tar hydrogenation unit, the coal tar raw materials need to be pretreated to remove metals, ash, etc., and then sent to the fixed bed for hydrogenation to produce clean fuel, etc., which can greatly extend the operating cycle of the unit.

[0005] At present, the pretreatment of coal tar in China mainly adopts centrifugal separation, sedimentation separation, solvent extraction, electric field purification and filtration separation. These methods have the disadvantages of poor pretreatment effect, low efficiency and low utilization rate of coal tar resources.

[0006] CN106701157A discloses a method for demetallizing high-temperature coal tar. Although the method uses diluent oil to dilute, adds alcohol substances and uses a demetallization reactor to pre-treat the high-temperature coal tar to remove metals, water is introduced during the implementation process. The treated water is phenol water, which contains high levels of phenols, ammonia nitrogen, etc., which is difficult to process and does not meet environmental protection requirements.

[0007] CN105713658B discloses a pretreatment process for low-temperature coal tar. The coal tar raw material is pretreated through sedimentation separation, primary electric desalination and secondary electric desalination. The process is complicated and the operation cost is high. In addition, water is introduced during the implementation process, and there is also the problem of difficult treatment of phenol water.

[0008] CN101012385A discloses a method for pretreating coal tar, which utilizes distillate oil and aromatic hydrocarbons to perform two-stage extraction on coal tar to remove ash and the like. Although the solvent extraction separation method has a good purification effect, it uses a large amount of solvent, has a complex process, and has high operating costs. Summary of the invention

[0009] The object of the present invention is to provide a method for pretreating coal tar raw materials, which can effectively reduce the content of metals and ash in coal tar and extend the operating cycle of a hydrogenation unit.

[0010] In order to achieve the above-mentioned purpose, the present invention provides a method for pretreating coal tar raw materials, which comprises: S1, mixing the coal tar raw materials with a diluent and then performing solid-liquid separation to obtain a solid phase material and a first liquid phase material; wherein the diluent contains hydrogenated product oil and an organic compound solvent; S2, contacting the first liquid phase material with an adsorbent for adsorption treatment to obtain a second liquid phase material; S3, contacting the second liquid phase material with a pretreatment agent under hydrogen conditions for pretreatment reaction, and performing gas-liquid separation on the obtained pretreatment reaction product.

[0011] Optionally, the weight ratio of the coal tar raw material to the diluent is 1:(0.005-0.5), preferably 1:(0.01-0.4);

[0012] The weight ratio of the hydrogenated product oil to the organic compound solvent in the diluent is 100:(0.2-3.5), preferably 100:(0.5-2.5).

[0013] Optionally, in step S1, the mixing conditions include: mixing temperature 50-200°C, mixing time 10-90min;

[0014] Preferably, the mixing temperature is 60-160° C. and the mixing time is 30-60 min.

[0015] Optionally, in step S2, the adsorption treatment conditions include: pressure 0.1-3.0 MPa, temperature 120-300°C, gas-to-agent volume ratio 10-500 Nm 3 / m 3 , volume space velocity 0.2-2.0h -1 ;

[0016] Preferably, the pressure is 0.5-2.5 MPa, the temperature is 160-280°C, and the gas-to-agent volume ratio is 30-300 Nm 3 / m 3 , the volume space velocity is 0.2-1.5h -1 .

[0017] Optionally, in step S3, the conditions of the pretreatment reaction include: hydrogen partial pressure of 0.5-3.5 MPa, reaction temperature of 160-340°C, gas-to-agent volume ratio of 10-500 Nm 3 / m 3 The volumetric space velocity of the raw material liquid is 0.2-1.5h -1 ;

[0018] Preferably, the hydrogen partial pressure is 1.0-3.5 MPa, the reaction temperature is 180-300°C, and the gas-to-agent volume ratio is 30-300 Nm 3 / m 3 The raw material liquid volume space velocity is 0.2-1.0h -1 .

[0019] Optionally, in step S1, a separation device is used to perform the solid-liquid separation, and the separation device is selected from a horizontal screw centrifuge, a disc centrifuge, a filter press, a filter or a membrane separator;

[0020] Preferably, the separation device is a horizontal screw centrifuge or a disc centrifuge, and the conditions for solid-liquid separation include: an operating temperature of 60-180° C. and a rotation speed of 3000-8000 rpm.

[0021] Optionally, the organic compound solvent includes one or more of C5-C9 hydrocarbons, C1-C4 alcohols, inorganic acids, organic acids, organic amines and quaternary ammonium salts;

[0022] Preferably, the organic compound solvent includes one or more of n-pentane, n-hexane, n-heptane, benzene, toluene, xylene, methanol, ethanol, formic acid, acetic acid, oxalic acid, phosphoric acid, citric acid, tartaric acid, pyruvic acid, ethanolamine, choline chloride and polyethylene glycol;

[0023] The hydrogenated product oil includes one or more of naphtha, kerosene, diesel, tail oil, light oil, phenol oil, wash oil, naphthalene oil and anthracene oil.

[0024] Optionally, the coal tar raw material includes one or more of low-temperature coal tar, medium-low-temperature coal tar, medium-temperature coal tar and high-temperature coal tar; or,

[0025] The coal tar raw material is a mixture of one or more of low-temperature coal tar, medium-low-temperature coal tar, medium-temperature coal tar and high-temperature coal tar and anthracene oil and / or washing oil.

[0026] Optionally, the adsorbent includes, from upstream to downstream, a first adsorbent, a second adsorbent, a third adsorbent, and optionally a fourth adsorbent;

[0027] The most probable pore diameters of the first adsorbent, the second adsorbent, the third adsorbent and the fourth adsorbent are successively reduced; the most probable pore diameter of the first adsorbent is 15-20 nm, the most probable pore diameter of the second adsorbent is 10-15 nm, the most probable pore diameter of the third adsorbent is 8-10 nm, and the most probable pore diameter of the fourth adsorbent is 6-8 nm;

[0028] The adsorbent is selected from one or more of alumina, silica, alumina-silica, activated carbon and waste catalysts in oil refining equipment.

[0029] Optionally, the pretreatment agent includes a first pretreatment agent and a second pretreatment agent in order from upstream to downstream;

[0030] The first pretreatment agent has an average diameter of 13-15 mm and contains 0.02-0.09 wt % of nickel oxide, 0.15-0.7 wt % of molybdenum oxide, and the balance of silicon oxide;

[0031] The second pretreatment agent has an average diameter of 4.0-5.0 mm and contains 0.03-0.25 wt % of nickel oxide, 0.15-1.2 wt % of molybdenum oxide, and the balance of silicon oxide.

[0032] Optionally, relative to 100 weight of the first pretreatment agent, the amount of the second pretreatment agent is 100-150 weight, the amount of the first adsorbent is 20-50 weight, the amount of the second adsorbent is 20-50 weight, the amount of the third adsorbent is 40-80 weight, and the amount of the fourth adsorbent is 40-80 weight.

[0033] The method of the present invention has the following advantages:

[0034] (1) The diluent used in the present invention contains hydrogenated product oil and an organic compound solvent, and combined with adsorption treatment and pretreatment with a pretreatment agent, can effectively remove impurities such as ash and metals in the coal tar raw material to be pretreated, and the pretreatment effect is good, which can meet the feed requirements of the subsequent hydrogenation reaction unit;

[0035] (2) The method of the present invention has the advantages of low energy consumption, low investment, simple process flow, simple operation and low operating cost;

[0036] (3) The method of the present invention does not introduce water, thus avoiding the environmental pollution problem caused by the difficulty in treating phenol water, and meets environmental protection requirements.

[0037] Other features and advantages of the present invention will be described in detail in the following detailed description. BRIEF DESCRIPTION OF THE DRAWINGS

[0038] The accompanying drawings are used to provide a further understanding of the present invention and constitute a part of the specification. Together with the following specific embodiments, they are used to explain the present invention but do not constitute a limitation of the present invention. In the accompanying drawings:

[0039] Figure 1 The present invention is a schematic flow chart of the method for pretreating coal tar raw materials.

[0040] Description of Reference Numerals

[0041] 1. Coal tar raw material 2. Mixing tank 3. Diluent

[0042] 4. Solid-liquid separator 5. Solid phase material 6. Adsorption tank

[0043] 7. Hydrogen-containing gas 8. Pretreatment tank 9. Gas-liquid separator

[0044] 10. Gas 11. Product tank DETAILED DESCRIPTION

[0045] The specific implementation of the present invention is described in detail below in conjunction with the accompanying drawings. It should be understood that the specific implementation described here is only used to illustrate and explain the present invention, and is not used to limit the present invention.

[0046] The present invention provides a method for pretreating coal tar raw materials, which comprises: S1, mixing the coal tar raw materials with a diluent and performing solid-liquid separation to obtain a solid phase material and a first liquid phase material; wherein the diluent contains hydrogenated product oil and an organic compound solvent; S2, contacting the first liquid phase material with an adsorbent for adsorption treatment to obtain a second liquid phase material; S3, contacting the second liquid phase material with a pretreatment agent under hydrogen conditions for pretreatment reaction, and performing gas-liquid separation on the obtained pretreatment reaction product.

[0047] The method of the present invention uses a diluent containing hydrogenation product oil and an organic compound solvent to dilute the coal tar raw material and then performs solid-liquid separation, and then combines adsorption treatment and pretreatment under the action of a pretreatment agent, which can effectively reduce the content of metals and ash in the coal tar raw material, thereby extending the operation cycle of the hydrogenation device.

[0048] In a specific embodiment of the present invention, the weight ratio of the coal tar feedstock to the diluent can vary within a large range, for example, it can be 1:(0.005-0.5), preferably 1:(0.01-0.4), and the weight ratio of the hydrogenated product oil and the organic compound solvent in the diluent can also vary within a large range, for example, it can be 100:(0.2-3.5), preferably 100:(0.5-2.5).

[0049] In a specific embodiment of the present invention, in step S1, the coal tar feedstock and the diluent can be mixed in any device, for example, in a mixing tank, and the mixing conditions may include: mixing temperature 50-200°C, mixing time 10-90min; preferably, the mixing temperature is 60-160°C, and the mixing time is 30-60min.

[0050] In a specific embodiment of the present invention, in step S2, the adsorption treatment conditions include: pressure 0.1-3.0MPa, temperature 120-300°C, gas-to-agent volume ratio 10-500Nm 3 / m 3 , volume space velocity 0.2-2.0h -1 Preferably, the pressure is 0.5-2.5MPa, the temperature is 160-280°C, and the gas volume ratio is 30-300Nm 3 / m 3 , the volume space velocity is 0.2-1.5h -1 .

[0051] In a specific embodiment of the present invention, the conditions of the pretreatment reaction include: hydrogen partial pressure of 0.5-3.5MPa, reaction temperature of 160-340°C, gas-to-agent volume ratio of 10-500Nm 3 / m 3 The volumetric space velocity of the raw material liquid is 0.2-1.5h -1 Preferably, the hydrogen partial pressure is 1.0-3.5MPa, the reaction temperature is 180-300°C, and the gas-agent volume ratio is 30-300Nm 3 / m 3 The raw material liquid volume space velocity is 0.2-1.0h -1 .

[0052] The present invention pretreats the coal tar raw material under the above reaction conditions, especially pretreating under low hydrogen partial pressure, which can more effectively remove metals and ash from the coal tar raw material and reduce the operating energy consumption of the device.

[0053] According to the present invention, any separation device with solid-liquid separation effect can be used to separate the coal tar raw material into solid and liquid. In a specific embodiment of the present invention, in step S1, a separation device is used to perform the solid-liquid separation, and the separation device can be selected from a horizontal screw centrifuge, a disc centrifuge, a filter press, a filter or a membrane separator. Preferably, the separation device is a horizontal screw centrifuge or a disc centrifuge, and the conditions for the solid-liquid separation include: an operating temperature of 60-180°C and a rotation speed of 3000-8000 rpm.

[0054] In a specific embodiment of the present invention, the organic compound solvent includes one or more of C5-C9 hydrocarbons, C1-C4 alcohols, inorganic acids, organic acids, organic amines and quaternary ammonium salts; the C5-C9 hydrocarbons may include one or more of n-pentane, n-hexane, n-heptane, benzene, toluene and xylene; the C1-C4 alcohols may include one or more of methanol, ethanol, propanol, butanol, isobutanol and polyethylene glycol; the inorganic acid may be selected from one or more of phosphoric acid, hydrochloric acid, nitric acid and sulfuric acid; the organic acid may include one or more of formic acid, acetic acid, oxalic acid, phosphoric acid, citric acid, tartaric acid and pyruvic acid; the organic amine is selected from one or more of ethanolamine, acetamide, tripropylamine and aniline; the quaternary ammonium salt is selected from one or more of alkyl trimethyl ammonium salt, choline chloride, alkyl dimethyl benzyl quaternary ammonium salt and alkyl dimethyl hydroxyethyl quaternary ammonium salt. In a preferred embodiment of the present invention, the organic compound solvent includes one or more of n-pentane, n-hexane, n-heptane, benzene, toluene, xylene, methanol, ethanol, formic acid, acetic acid, oxalic acid, phosphoric acid, citric acid, tartaric acid, pyruvic acid, ethanolamine, choline chloride and polyethylene glycol.

[0055] In a specific embodiment of the present invention, the hydrogenated product oil can be obtained by hydrogenating one or more of petroleum-based raw materials, coal tar raw materials and Fischer-Tropsch synthetic oil, for example, it can include one or more of naphtha, kerosene, diesel and tail oil; the cutting fraction oil of the coal tar raw material can include one or more of light oil, phenol oil, wash oil, naphthalene oil and anthracene oil.

[0056] In a specific embodiment of the present invention, coal tar is well known to those skilled in the art, and refers to coal tar produced by coal pyrolysis or coal gasification or other processes. The coal tar raw material may include low-temperature coal tar produced in the coal gasification process, or may be one or more of low-temperature coal tar, medium-low-temperature coal tar, medium-temperature coal tar and high-temperature coal tar produced in coal pyrolysis or coking process (including low-temperature pyrolysis, medium-temperature pyrolysis and high-temperature coking process), or a mixture of one or more of low-temperature coal tar, medium-low-temperature coal tar, medium-temperature coal tar and high-temperature coal tar with anthracene oil and / or wash oil.

[0057] According to the present disclosure, the distillation range of the low-temperature coal tar can be 50-450°C; the distillation range of the medium-low temperature coal tar can be 50-550°C; the distillation range of the medium-temperature coal tar can be 50-600°C; and the distillation range of the high-temperature coal tar can be 50-650°C.

[0058] According to the present invention, more than two adsorbents are used for adsorption treatment, preferably 3-5 adsorbents are used for adsorption treatment, and more preferably, three adsorbents are used for adsorption treatment. In a specific embodiment of the present invention, the adsorbent includes a first adsorbent, a second adsorbent, a third adsorbent, and optionally a fourth adsorbent from upstream to downstream; the most probable pore sizes of the first adsorbent, the second adsorbent, the third adsorbent and the fourth adsorbent are successively reduced. In one embodiment, the most probable pore size of the first adsorbent is 15-20nm, the most probable pore size of the second adsorbent is 10-15nm, the most probable pore size of the third adsorbent is 8-10nm, and the most probable pore size of the fourth adsorbent is 6-8nm. The present invention does not limit the specific type of adsorbent, which can be a porous material with an adsorption effect, for example, it can be selected from one or more of alumina, silica, alumina-silicon oxide, activated carbon and waste catalysts in oil refining equipment. The present invention does not specifically limit the shape of the adsorbent, which can include but is not limited to Raschig rings, porous spheres, honeycombs or butterfly shapes.

[0059] In a specific embodiment of the present invention, the pretreatment agent includes a first pretreatment agent and a second pretreatment agent from upstream to downstream, and the metal active components of the first pretreatment and the second pretreatment can be independently selected from the metals of Group VIB and / or Group VIII, preferably one or more of Fe, Co, Ni, Mo and W. The average diameter of the first pretreatment agent is 13-15 mm, and it contains 0.02-0.09 wt% of nickel oxide, 0.15-0.7 wt% of molybdenum oxide, and the balance of silicon oxide; the average diameter of the second pretreatment agent is 4.0-5.0 mm, and it contains 0.03-0.25 wt% of nickel oxide, 0.15-1.2 wt% of molybdenum oxide, and the balance of silicon oxide. The present invention does not specifically limit the shape of the pretreatment agent, which can be a catalyst shape well known to those skilled in the art, for example, a porous cylindrical shape, a honeycomb cylindrical shape, a Raschig ring shape, a butterfly shape, etc. In one embodiment, the first pretreatment agent of the present invention is a porous cylindrical shape, and the second pretreatment agent is a honeycomb cylindrical shape.

[0060] In a specific embodiment of the present invention, relative to 100 weight of the first pretreatment agent, the amount of the second pretreatment agent is 100-150 weight, the amount of the first adsorbent is 20-50 weight, the amount of the second adsorbent is 20-50 weight, the amount of the third adsorbent is 40-80 weight, and the amount of the fourth adsorbent is 40-80 weight.

[0061] like Figure 1 As shown, in a specific embodiment disclosed, the coal tar raw material is pretreated by a method comprising the following steps:

[0062] S1, after mixing coal tar raw material 1 and diluent 3 in mixing tank 2, the mixed stream is introduced into solid-liquid separator 4 for solid-liquid separation to obtain solid phase material 5 and first liquid phase material, and the separated solid phase material 5 can be used as fuel or coal gasification raw material for gasification; wherein the diluent contains hydrogenation product oil and organic compound solvent;

[0063] S2, introducing the first liquid phase material into an adsorption tank 6 to contact with an adsorbent for adsorption treatment to obtain a second liquid phase material;

[0064] S3. The second liquid phase material and the hydrogen-containing gas 7 are introduced into a pretreatment tank 8 to contact with a pretreatment agent for a pretreatment reaction. The obtained pretreatment reaction product is introduced into a gas-liquid separator 9 for gas-liquid separation. The separated gas 10 is used as fuel gas. The separated liquid flow enters a product tank 11. The pretreated product is used as a raw material for a subsequent fixed bed hydrogenation device.

[0065] The present invention is further described below by way of examples, but the present invention is not limited thereto. In the following examples, unless otherwise specified, all the raw materials used are commercially available.

[0066] The properties of the coal tar raw material to be pretreated used below are shown in Table 1.

[0067] In Examples 1-5 and the comparative example, along the direction of the reactant flow, the adsorbents in the adsorption tank are the first adsorbent, the second adsorbent and the third adsorbent, respectively. The first adsorbent is honeycomb-shaped silica with a maximum pore size of 18 nm; the second adsorbent is Raschig ring-shaped silica-alumina with a maximum pore size of 14 nm; the third adsorbent is butterfly-shaped alumina with a maximum pore size of 12 nm.

[0068] Along the direction of the reactant flow, the pretreatment agents in the pretreatment tank are respectively the first pretreatment agent and the second pretreatment agent. The first pretreatment agent is a porous cylindrical shape, the carrier is silicon oxide or aluminum oxide, the average diameter is 13-15 mm, and it contains 0.05 wt% nickel oxide, 0.5 wt% molybdenum oxide, and the balance is silicon oxide; the second pretreatment agent is a Raschig ring shape, the average diameter is 4.0-5.0 mm, and it contains 0.15 wt% nickel oxide, 1.0 wt% molybdenum oxide, and the balance is silicon oxide.

[0069] With respect to 100 weight of the first pretreatment agent, the amount of the second pretreatment agent is 130 weight, the amount of the first adsorbent is 30 weight, the amount of the second adsorbent is 40 weight, and the amount of the third adsorbent is 60 weight.

[0070] Example 1

[0071] S1. The diluent and the coal tar raw material 1 to be pretreated in Table 1 are fully mixed in a mixing tank at a weight ratio of 0.1:1, the mixing temperature is 160°C, the mixing time is 50min, and the mixed logistics enters a solid-liquid separator to separate solid slag and liquid to obtain a solid phase material and a first liquid phase material, and the diluent contains coal tar hydrogenation tail oil and toluene in a weight ratio of 100:1;

[0072] S2, allowing the separated first liquid phase material to enter an adsorption tank to contact with an adsorbent for adsorption treatment to obtain a second liquid phase material;

[0073] S3. The second liquid phase material enters the pretreatment tank to contact with the pretreatment agent for pretreatment reaction. The logistics after adsorption treatment enters the gas-liquid separator for gas-liquid separation. The separated liquid logistics is the pretreated product, which is suitable as the raw material for the subsequent coal tar hydrogenation device.

[0074] The specific conditions are shown in Table 2, and the properties of the pretreated coal tar are shown in Table 3.

[0075] Example 2

[0076] S1, the diluent and the coal tar raw material 1 to be pretreated are fully mixed in a mixing tank at a weight ratio of 0.3:1, the mixing temperature is 120°C, the mixing time is 60min, and the mixed logistics enters a solid-liquid separator to separate the solid slag and the liquid to obtain a solid phase material and a first liquid phase material, and the diluent contains wash oil and xylene in a weight ratio of 100:1.5;

[0077] S2, the separated first liquid phase material enters the adsorption tank and contacts with the adsorbent for adsorption treatment to obtain the second liquid phase material;

[0078] S3. The second liquid phase material enters the pretreatment tank to contact with the pretreatment agent for reaction. The logistics coming out of the pretreatment tank enters the gas-liquid separator for gas-liquid separation. The separated liquid logistics is the pretreated product, which is suitable as the raw material for the subsequent coal tar hydrogenation device.

[0079] Example 3

[0080] S1, the diluent and the coal tar raw material 1 to be pretreated are fully mixed in a mixing tank at a weight ratio of 0.01:1, the mixing temperature is 80°C, the mixing time is 30min, and the mixed logistics enters a solid-liquid separator to separate the solid residue and the liquid to obtain a solid phase material and a first liquid phase material, and the diluent contains diesel and acetic acid in a weight ratio of 100:0.5;

[0081] S2, allowing the separated first liquid phase material to enter an adsorption tank to contact with an adsorbent for adsorption treatment to obtain a second liquid phase material;

[0082] S3. The second liquid phase material enters the pretreatment tank to contact with the pretreatment agent for pretreatment reaction. The pretreatment reaction product coming out of the pretreatment tank enters the gas-liquid separator for gas-liquid separation. The separated liquid stream is the pretreated product, which is suitable as the raw material for the subsequent coal tar hydrogenation device.

[0083] The specific adsorption treatment conditions are shown in Table 2, and the properties of the coal tar after adsorption treatment are shown in Table 3.

[0084] Example 4

[0085] S1, the diluent and the coal tar raw material 1 to be pretreated are fully mixed in a mixing tank at a weight ratio of 0.2:1, the mixing temperature is 60°C, the mixing time is 50min, and the mixed logistics enters a solid-liquid separator to separate the solid residue and the liquid to obtain a solid phase material and a first liquid phase material, and the diluent contains phenol oil and methanol at a weight ratio of 100:2.5;

[0086] S2, allowing the separated first liquid phase material to enter an adsorption tank to contact with an adsorbent for adsorption treatment to obtain a second liquid phase material;

[0087] S3. The second liquid phase material enters the pretreatment tank to contact with the pretreatment agent for reaction. The logistics from the gas pretreatment tank enters the gas-liquid separator for gas-liquid separation. The separated liquid logistics is the pretreated product, which is suitable as the raw material for the subsequent coal tar hydrogenation device.

[0088] The specific adsorption treatment conditions are shown in Table 2, and the properties of the coal tar after adsorption treatment are shown in Table 3.

[0089] Example 5

[0090] S1, the diluent and the coal tar raw material 2 to be pretreated are fully mixed in a mixing tank at a weight ratio of 0.15:1, the mixing temperature is 160°C, the mixing time is 50min, and the mixed logistics enters a solid-liquid separator to separate the solid slag and the liquid to obtain a solid phase material and a first liquid phase material, and the diluent contains coal tar hydrogenation tail oil and ethanolamine in a weight ratio of 100:2;

[0091] S2, allowing the separated first liquid phase material to enter an adsorption tank to contact with an adsorbent for adsorption treatment to obtain a second liquid phase material;

[0092] S3. The second liquid phase material enters the pretreatment tank to contact with the pretreatment agent for pretreatment reaction. The logistics after adsorption treatment enters the gas-liquid separator for gas-liquid separation. The separated liquid logistics is the pretreated product, which is suitable as the raw material for the subsequent coal tar hydrogenation device.

[0093] The specific conditions are shown in Table 2, and the properties of the pretreated coal tar are shown in Table 3.

[0094] Example 6

[0095] In this embodiment, a fourth adsorbent is loaded downstream of the third adsorbent in the adsorption tank, and the fourth adsorbent is a waste distillate oil hydrogenation catalyst (based on the carrier, its composition is 10.5% by weight of nickel oxide, 25.7% by weight of molybdenum oxide, and the rest is the carrier).

[0096] With respect to 100 weight of the first pretreatment agent, the amount of the first adsorbent I is 15 weight, the amount of the second adsorbent is 15 weight, the amount of the third adsorbent is 30 weight, and the amount of the fourth adsorbent is 35 weight.

[0097] S1, coal tar hydrogenation tail oil and the coal tar raw material 2 to be pretreated are fully mixed in a mixing tank at a weight ratio of 0.1:1, the mixing temperature is 160°C, the mixing time is 50min, and the mixed logistics enters a solid-liquid separator to separate solid slag and liquid to obtain a solid phase material and a first liquid phase material, and the diluent contains coal tar hydrogenation tail oil and polyethylene glycol in a weight ratio of 100:0.8;

[0098] S2, the separated first liquid phase material enters the adsorption tank and contacts with the adsorbent for adsorption treatment to obtain the second liquid phase material;

[0099] S3. The second liquid phase material enters the pretreatment tank to contact with the pretreatment agent for reaction. The logistics coming out of the pretreatment tank enters the gas-liquid separator for gas-liquid separation. The separated liquid logistics is the pretreated product, which is suitable as the raw material for the subsequent coal tar hydrogenation device.

[0100] Example 7

[0101] The coal tar is pretreated in the same manner as in Example 1, except that in step S1, the diluent is mixed with the coal tar raw material 1 to be pretreated at a weight ratio of 0.005:1.

[0102] Example 8

[0103] The coal tar was pretreated in the same manner as in Example 1, except that in step S1, the diluent contained coal tar hydrogenation tail oil and toluene in a weight ratio of 100:0.3.

[0104] Example 9

[0105] The coal tar was pretreated in the same manner as in Example 1, except that the conditions for the adsorption treatment and the pretreatment were different from those in Example 1.

[0106] Comparative Example 1

[0107] The coal tar was pretreated in the same manner as in Example 1, except that the diluent was coal tar hydrogenation tail oil.

[0108] Comparative Example 2

[0109] The coal tar is pretreated in the same manner as in Example 1, except that step S2 is omitted and the first liquid phase material obtained by separation is directly allowed to enter the pretreatment tank to contact with the pretreatment agent for pretreatment reaction.

[0110]

[0111]

[0112] Table 2

[0113]

[0114]

[0115] Table 3

[0116] Example 1 Example 2 Example 3 Example 4 Example 5 Example 6 <![CDATA[Density (20 °C) / (g / cm 3 )]]> 1.0002 1.0000 1.0001 0.9999 1.1489 1.1496 Total metal content / (μg / g) 9.6 15.1 19.4 8.5 13.2 17.7 Ash content / weight% 0.0022 0.0057 0.0078 0.0038 0.0031 0.0040

[0117] Example 7 Example 8 Example 9 Comparative Example 1 Comparative Example 2 <![CDATA[Density (20 °C) / (g / cm 3 )]]> 1.0001 1.0003 1.0002 1.0002 1.0003 Total metal content / (μg / g) 17.7 35.6 21.3 48.6 55.2 Ash content / weight% 0.0084 0.0060 0.0049 0.022 0.028

[0118] It can be seen from the above that the method of the present invention can more effectively reduce the total metal content and ash content in the coal tar raw material.

[0119] The preferred embodiments of the present invention are described in detail above in conjunction with the accompanying drawings. However, the present invention is not limited to the specific details in the above embodiments. Within the technical concept of the present invention, a variety of simple modifications can be made to the technical solution of the present invention, and these simple modifications all belong to the protection scope of the present invention.

[0120] It should also be noted that the various specific technical features described in the above specific embodiments can be combined in any suitable manner without contradiction. In order to avoid unnecessary repetition, the present invention will not further describe various possible combinations.

[0121] In addition, various embodiments of the present invention may be arbitrarily combined, and as long as they do not violate the concept of the present invention, they should also be regarded as the contents disclosed by the present invention.

Claims

1. A method for pretreating coal tar raw materials, the method include: S1, mixing the coal tar raw material with a diluent and performing solid-liquid separation to obtain a solid phase material and a first liquid phase material; wherein the diluent contains hydrogenated product oil and an organic compound solvent; The weight ratio of the hydrogenated product oil and the organic compound solvent in the diluent is 100:(0.2-3.5); the weight ratio of the coal tar raw material to the diluent is 1:(0.005-0.5); the mixing conditions include: mixing temperature 50-200°C, mixing time 10-90min; The organic compound solvent includes one or more of C5-C9 hydrocarbons, C1-C4 alcohols, organic acids, ethanolamines and polyethylene glycols; The hydrogenated product oil is obtained by hydrogenating one or more of petroleum-based raw materials, coal tar raw materials and Fischer-Tropsch synthetic oil, including one or more of naphtha, kerosene, diesel, tail oil, light oil, phenol oil, wash oil, naphthalene oil and anthracene oil, wherein the light oil, phenol oil, wash oil, naphthalene oil and anthracene oil are cut fraction oils of coal tar raw materials; S2, contacting the first liquid phase material with an adsorbent for adsorption treatment to obtain a second liquid phase material; wherein the conditions of the adsorption treatment include: pressure 0.1-3.0MPa, temperature 120-300°C, gas-to-agent volume ratio of 10-500Nm 3 / m 3 , volume space velocity 0.2-2.0h -1 The adsorbent is selected from one or more of alumina, silica, alumina-silicon oxide, activated carbon and waste catalysts from oil refining equipment; S3. Under hydrogen conditions, the second liquid phase material is contacted with a pretreatment agent to perform a pretreatment reaction, and the obtained pretreatment reaction product is subjected to gas-liquid separation.

2. The method according to claim 1, in, The weight ratio of the coal tar raw material to the diluent is 1:(0.01-0.4); The weight ratio of the hydrogenated product oil to the organic compound solvent in the diluent is 100:(0.5-2.5).

3. The method according to claim 1, in, In step S1, the mixing conditions include: mixing temperature of 60-160°C and mixing time of 30-60 min.

4. The method according to claim 1, in, In step S2, the adsorption treatment conditions include: the pressure is 0.5-2.5MPa, the temperature is 160-280°C, the gas-to-agent volume ratio is 30-300Nm 3 / m 3 , the volume space velocity is 0.2-1.5h -1 .

5. The method according to claim 1, in, In step S3, the pretreatment reaction conditions include: hydrogen partial pressure of 0.5-3.5MPa, reaction temperature of 160-340°C, gas-to-agent volume ratio of 10-500Nm 3 / m 3 The volumetric space velocity of the raw material liquid is 0.2-1.5h -1 .

6. The method according to claim 5, in, In step S3, the conditions of the pretreatment reaction include: the hydrogen partial pressure is 1.0-3.5MPa, the reaction temperature is 180-300°C, the gas-to-agent volume ratio is 30-300Nm 3 / m 3 The raw material liquid volume space velocity is 0.2-1.0h -1 .

7. The method according to claim 1, in, In step S1, a separation device is used to perform the solid-liquid separation, and the separation device is selected from a horizontal screw centrifuge, a disc centrifuge, a filter press, a filter or a membrane separator.

8. The method according to claim 7, in, In step S1, the separation device is a horizontal screw centrifuge or a disc centrifuge, and the conditions for solid-liquid separation include: an operating temperature of 60-180° C. and a rotation speed of 3000-8000 rpm.

9. The method according to claim 1, in, The organic compound solvent includes one or more of n-pentane, n-hexane, n-heptane, benzene, toluene, xylene, methanol, ethanol, formic acid, acetic acid, oxalic acid, citric acid, tartaric acid, pyruvic acid, ethanolamine and polyethylene glycol.

10. The method according to claim 1, in, The coal tar raw material includes one or more of low-temperature coal tar, medium-low-temperature coal tar, medium-temperature coal tar and high-temperature coal tar; or, The coal tar raw material is a mixture of one or more of low-temperature coal tar, medium-low-temperature coal tar, medium-temperature coal tar and high-temperature coal tar and anthracene oil and / or washing oil.

11. The method according to claim 1, in, The adsorbent includes, from upstream to downstream, a first adsorbent, a second adsorbent, a third adsorbent, and optionally a fourth adsorbent; The most probable pore diameters of the first adsorbent, the second adsorbent, the third adsorbent and the fourth adsorbent decrease successively; the most probable pore diameter of the first adsorbent is 15-20nm, the most probable pore diameter of the second adsorbent is 10-15nm, the most probable pore diameter of the third adsorbent is 8-10nm, and the most probable pore diameter of the fourth adsorbent is 6-8nm.

12. The method according to claim 11, in, The pretreatment agent includes a first pretreatment agent and a second pretreatment agent in order from upstream to downstream; The first pretreatment agent has an average diameter of 13-15 mm and contains 0.02-0.09 wt % of nickel oxide, 0.15-0.7 wt % of molybdenum oxide, and the balance of silicon oxide; The second pretreatment agent has an average diameter of 4.0-5.0 mm and contains 0.03-0.25 wt % of nickel oxide, 0.15-1.2 wt % of molybdenum oxide, and the balance of silicon oxide.

13. The method according to claim 12, in, Relative to 100 weight of the first pretreatment agent, the amount of the second pretreatment agent is 100-150 weight, the amount of the first adsorbent is 20-50 weight, the amount of the second adsorbent is 20-50 weight, the amount of the third adsorbent is 40-80 weight, and the amount of the fourth adsorbent is 40-80 weight.